Clad plate for lead frames,lead frame using the same, and method of manufacturing the lead frame

MYPI1999004199A0Inactive Publication Date: 2000-03-30TOYO KOHAN CO LTD
View PDF 0 Cites 0 Cited by

Patent Information

Application Number
MYPI1999004199
Authority / Receiving Office
MY · MY
Patent Type
Applications
Current Assignee / Owner
Filing Date
1999-09-28
Publication Date
2000-03-30
Estimated Expiration
Not applicable · inactive patent

AI Technical Summary

Technical Problem

Existing methods for manufacturing lead frames using clad sheets face challenges such as difficult chemical etching control due to the absence of an etching stopper layer, unflat bonding surfaces, and high production costs, particularly with the cold rolling method and vapor deposition techniques.

Method used

A clad sheet is manufactured by press-bonding copper or aluminum foils to nickel foils at a reduction rate of 0.1 to 3%, with nickel plating on one or both sides, and an activation treatment in a vacuum chamber using hyper low-pressure inert gas and glow discharge, enabling selective etching and reducing manufacturing costs.

Benefits of technology

This method produces lead frames with excellent selective etchability and reduced production costs, avoiding pore generation and alloy layer formation, while maintaining flatness and eliminating the need for heat treatment.

✦ Generated by Eureka AI based on patent content.
Patent Text Reader

Abstract

THE PRESENT INVENTION OFFERS A CLAD SHEET (31) FOR LEAD FRAME WHICH CAN MANUFACTURE ECONOMICALLY AND HAS EXCELLENT CHARACTERISTICS, LEAD FRAME USING THEREOF AND MANUFACTURING METHOD THEREOF. A CLAD SHEET (31) FOR LEAD FRAME IS MANUFACTURED BY PRESS-BONDING COPPER FOIL (24) TO NICKEL FOIL (21) AT THE REDUCTION RATE OF 0.1 TO 3%. OR, IT IS MANUFACTURED BY PRESS-BONDING COPPER FOIL HAVING NICKEL PLATING (22) ON ONE OR BOTH SIDES OF IT TO THE OTHER COPPER FOIL (24) AT THE REDUCTION RATE OF 0.1 TO 3%. FURTHER, IT IS ALSO MANUFACTURED BY PRESS-BONDING COPPER FOIL HAVING NICKEL PLATING (22) ON ONE SIDE OF IT TO ALUMINUM FOIL (20) AT THE REDUCTION RATE OF 0.1 TO 3%. CLAD SHEET (31) IS COMPRISING THREE LAYERS OF COPPER / NICKEL / COPPER OR COPPER / NICKEL / ALUMINUM.(FIG. 5)
Need to check novelty before this filing date? Find Prior Art

Description

CLAD PLATE FOR LEAD FRAMES, LEAD FRAME USING THESAME, AND METHOD OF MANUFACTURING THE LEAD FRAMEDetailed description of the invention [Technological field the invention involving]The present invention relates to the method of manufacturing a lead frame, particularly that can be manufactured using a clad sheet formed by cold press-bonding method.[Prior art]Recently, accompanied with semiconductor device being more highly accumulated, having more pins and being smaller sized, and electronic equipment being smaller sized and lighter weighted, high density mount board is required.In the method for connecting semiconductor chips to lead frames, a metal lead having bumps, which could minimize the assembly process, the size of package and the cost compared to the conventional wire-bonding method, has been researched and developed. In this method, jutting bumps are formed at the edge portion of a lead and the lead connects to semiconductor chip intervening theses bumps, which can make a package thin.And now, as a method for forming bumps, a three layered clad sheet is tried to be used as a metallic material for manufacturing lead frame.Japanese laid open publication No. Hei 9-115965 discloses a method of manufacturing a lead frame by using such three layer clad sheet.In this manufacturing method, a clad sheet is manufactured by holding a high hardness copper sheet between pure copper sheets.[Problems which is to be solved by the invention]However, in the method mentioned above, any etching stopper layer does not exist in the clad sheet, which causes a problem that the control of the chemical etching is extremely difficult.There is also a method of manufacturing lead frame using three layer clad sheets in which aluminum or ferrous alloy is used as an etching stopper layer. But these clad sheets are formed by a usual cold rolling method using a higher reduction rate, which-3produce unflat bonding surface or form an alloy layer on a surface between a copper sheet and etching stopper layer during heat treatment, which causes inferior selective etching.In addition, there is the other method of manufacturing a lead frame, in which thin metal film is formed by a vapor deposition method. However, there was a problem, that is, in case that the formed film is thin (several pm), pores are easily generated, while in case that the formed film is thick (10 pm or more), the productability is deteriorated and the cost becomes io high.The present invention is aimed to solve such problems, and the objective of the present invention is to produce a clad sheet for lead frame which can be manufactured at low cost and has an excellent selective etchability, a lead frame using thereof, and a manufacturing method thereof.[Means to solve problems]The clad sheet for lead frame is characterized in that it is manufactured by press bonding a copper foil to nickel foil at the reduction rate of 0.1 to 3%.The copper foil has a nickel plating on one or both sides.The clad sheet for lead frame is characterized in that it is manufactured by press bonding an aluminum foil to a nickel foil at the reduction rate of 0.1 to 3%.According to still another feature, the clad sheet for a lead frame is characterized in that it is composed of a three-layer construction comprising copper / nickel / copper.According to a further feature, the lead frame is characterized in that bumps are formed by selectively etching the clad sheet.-4The method of manufacturing the lead frame is preferably characterized in that:said clad sheet for lead frame is formed by previously practicing an activation treatment of the bonding surface of said copper foil or aluminum foil and the bonding surface of said nickel foil or nickel plating in a vacuum chamber, laminating said copper foil or aluminum foil to said nickel foil and nickel plating, and then press-bonding at the reduction rate of 0.1 to 3%, wherein io said activation treatment is practiced (1) in a hyper low pressure inert gas atmosphere of 13.3 to 0.013 Pa (1 X 10'1 2 3to 1 X 10’4Torr), (2) by glow discharging charging an alternate current of 1 to 50 MHz between one electrode A comprising said copper foil or aluminum foil having bonding surface and said nickel foil or nickel plating respectively electrically ground and the other electrode B insulatingly supported, and (3) by sputter-etching (4) in the manner that the electrode area exposed in plasma generated by said glow discharging is not more than % the area of electrode B.-5[The best manner to practice the invention]Hereafter, the present invention is concretely explained referring to an embodiment shown in an attached figures.First of all, the structure of a lead frame relating to a embodiment of the present invention is explained referring to Figure 7.As shown in Figure, etching stopper layers 11 (thickness of 0.5 to 3 pm) comprising nickel foil (thickness of 5 to 10 pm ) or nickel plating is connected to one side of outer lead layer 10 (thickness of 10 to 100 pm) io comprising copper foil or aluminum foil 20, which forms a lead. Further, bump 12 (thickness of 10 to 100 pm) comprising copper foil 24 which is inner lead layer and external terminal 13 are formed. And, a lead frame is formed by connecting semiconductor chip 14 to bump 12.Next, a manufacturing method of the above-mentioned lead frame is 15 explained. First of all, nickel plating 21 (thickness of 0.5 to 3 pm) which is to be etching stopper layer 11 is given to one side of copper foil 20 (thickness of 10 to 100 pm) which is to be outer lead layer 10 when a lead frame is manufactured. Thus, nickel plated copper foil 22 is manufactured (referred toFigure I).Nickel plated copper foil 22 is wound around pay-off reel 23 of a clad sheet manufacturing equipment shown in Figure 8, while copper foil 24 which is to be inner lead layer is wound around pay-off reel 25.Nickel plated copper foil 22 and copper foil 24 are rewound from pay-off 5 reel 23 and 25 respectively at the same time. And portions of them are wound around electrode roll 27 and 28 which are projecting in etching chamber 26. After that, they are activated by sputter etching treatment in etching chamber 26.In this case, the activation treatment is practiced by the following condition as disclosed in Japanese laid open patent number Hei 1-224184, namely φ in a hyper low pressure inert gas atmosphere of 1 X 10-1 to 1 X 10-4Torr, ® by glow discharging charging an alternate current of 1 to 50 MHz between one electrode A comprising said copper foil or aluminum foil having bonding surface and said nickel foil or nickel plating respectively electrically ground and the other electrode B insulatingly supported, and ® by sputter-etching @ in the manner that the electrode area exposed in plasma generated by said glow discharging is not more than 1 / 3 the area of electrode B. After that, they are cold press-bonded by rolling unit 30 installed in vacuum chamber 29, and then clad sheet for 20 lead frame having three layered structure is rewound around rewinding roll 32. Thus, clad sheet for lead frame is manufactured.While the case of press-bonding a copper foil which is previously nickel plated is explained in the above-mentioned, a copper foil or an aluminum foil to which a nickel foil is press bonded using the above-mentioned equipment can also be available in place of nickel plating. In this case, three layered clad sheet intervened by a nickel layer as an intermediate layer in the order of copper / nickel / copper or copper / nickel / aluminum can be manufactured by repeating the press-bonding using the above-mentioned equipment.The manufacturing method in this case is described below.First of all, copper foil or aluminum foil 20 (thickness of 10 to 100 H m) which is to be outer lead layer when lead frame is manufactured (referred to Figure l) is wound around pay-off reel 23 of clad sheet manufacturing equipment shown in Figure 8. Nickel foil 21 (thickness of 5 to 10 M m) which is to be etching stopper layer 11 is wound around pay-off reel 25.Copper foil or aluminum foil 20 and nickel foil 21 are rewound from pay-off reel 23 and 25 respectively at the same time. And portions of them are wound around electrode roll 27 and 28 which are projecting in etching chamber 26. And then, the bonding surfaces are activated by sputter etching treatment in etching chamber 26. After that, they are cold press-bonded by rolling unit 30 in the manner that the activated surfaces are bonding surfaces. Thus copper foil or aluminum foil 22 with nickel foil and having two layered structure is manufactured. After that, this two layered clad sheet is wound around winding roll 32.Next, copper foil or aluminum foil 22 with nickel foil having two layered structure is wound again around pay-off reel 23. Copper foil 24 which is to be inner lead layer is wound around pay-off reel 25.Copper foil or aluminum foil 22 with nickel foil and copper fill 24 are rewound from pay-off reel 23 and 25 respectively at the same time. And portions of them are wound around electrode roll 27 and 28 which are projecting in etching chamber 26.After that, they are activated by sputter etching treatment in etching chamber 26.-8In this case, the activation treatment is also practiced by the following condition, namely (1) in a hyper low pressure inert gas atmosphere of 13.3 to0.013 Pa (1 X 10’1to 1 X 10-4Torr), (2) by glow discharging charging an alternate current of 1 to 50 MHz between one electrode A comprising said copper foil or aluminum foil 22 with nickel foil having bonding surface and said nickel foil or nickel plating respectively electrically ground io and the other electrode B insulatingly supported, and (3) by sputter-etching (4) in the manner that the electrode area exposed in plasma generated by said glow discharging is not more than1 / 3the area of electrode B. Thus clad sheet 31 for lead frame having three layered structure is manufactured as shown in Figure 1.In addition, it is also possible to manufacture a multi-layered clad sheet in single press-bonding by installing three or more of the above-mentioned pay-off reels, setting copper foil or aluminum foil and nickel foil on these payoff reels, and simultaneously supplying foils from three or more of pay-off reels.Next, after clad sheet 31 for lead frame is cut into desired size, lead frame and bump are manufactured through the following processes as explained referring to Figure 2 to 7.First of all, after photo resist is coated on the surface of copper foil 24 25 as shown in Figure 2, photo resist film 40 is formed by exposing and printing.Then, copper foil 24 is removed by selective etching using a solution of sulfuric acid plus hydrogen peroxide so that bump 12 and external terminal 13 are left as shown in Figure 3. It takes about four minutes, for instance, for etching. In the case where aluminum foil is etched, sodium hydroxide solution is used.Then, photo resist film 41 is formed on the surface of bump 12 and external terminal 13, and further, after photo resist is coated on the surface of copper foil or aluminum foil 20 which is to be outer lead layer 10, photo resist film 42 is formed by exposing and printing as shown in Figure 4.Next, copper foil 20 and nickel plating or nickel foil 21 which are to be outer lead layer 10 is etched using ferric chloride, cupric chloride or the like, after that, conductor circuit 43 is formed by removing photo resist film 41 and 42 as shown in Figure 5.Moreover, in the case where aluminum foil 20 is etched, 5 % solution of sodium hydroxide or potassium hydroxide (50 G) is used as etchant. It takes about two minutes, for instance, for etching. After that, conductor circuit 43 is formed by etching nickel plating or nickel foil 21 using ferric chloride, cupric chloride or the like.Or, instead of selective etching from the side of outer lead layer as shown inFigure 4, photo resist film 41 can be formed on the top surface and the side surface of bump 12 and external terminal 13 so that photo resist film 41 is not formed on the bottom portions between bumps, and further, photo resist film 42 can be formed on the surface of copper foil or aluminum foil 20 which is to be outer lead layer 10 as shown in Figure 6.In this case, etching can be processed from the side of nickel plating or nickel foil 21 toward copper foil 20 on the side of outer lead layer using ferric chloride, cupric chloride or the like.And, in the case where aluminum foil 20 is formed, nickel plating or nickel foil 21 is first etched using ferric chloride, cupric chloride or the like. After that, aluminum foil 20 is etched using 5% solution of sodium hydroxide or potassium hydroxide (50 X3).And then, semiconductor chip 14 is connected to bump 12 as shown in Figure7.[effect of invention]As mentioned above, in the clad sheet for lead frame of Claim 1 to 6, clad sheet for lead frame is manufactured by press-bonding copper foil or aluminum foil to 10 nickel foil, or press-bonding copper foil having nickel plating on one or both sides of it to the other copper foil in the state that both foils are laminated. Therefore, the generation of pore caused in the vapor deposition method can be avoided and the quality can be improved. And, since it can merely be manufactured by laminating and press-bonding, the manufacturing cost of the clad sheet for lead frame can be reduced.Moreover, the flatness on the bonding surface can be maintained by suppressing the stress on the bonding surface to low since the press-bonding is practiced at the low reduction rate of 0.1 to 3 %. And further, heat treatment for the recovery of formability is also unnecessary, and the alloy layer is not caused on the interface. Therefore, lead frame excellent in the selective etching can be manufactured by using this clad sheet for lead frame.In the lead frame of Claim 7, bump is formed by selectively etching the above-mentioned clad sheet for lead frame. Therefore, a thin lead frame can be manufactured efficiently and economically.In the method of manufacturing the lead frame of Claim 8, clad sheet for lead frame is formed by laminating and press-bonding copper foil or aluminum foil which forms lead layer to nickel plating or nickel foil which forms etching stopper layer. After that, lead frame is manufactured by selectively etching the above-manufactured multi-layered clad sheet and forming bump comprising copper or aluminum. Therefore, a thin lead frame having uniform bumps can be manufactured efficiently and economically.In the manufacturing method of lead frame of Claim 9, after bonding surfaces of copper foil or aluminum foil and nickel plating or nickel foil are previously activated in a vacuum chamber, the copper foil or aluminum foil is laminated to the nickel plating or nickel foil and press-bonded at the reduction rate of 0.1 to 3 %. Thus the clad sheet for lead frame is formed. Therefore, the flatness of the bonding surface can be maintained by suppressing the stress on the bonding surface to low. Moreover, heat treatment for the recovery of formability is also unnecessary, and the alloy is not caused on the interface. Therefore, lead frame excellent in the selective etching can be manufactured by using this multi-layered clad sheet.[Brief explanation of drawings]Figure 1 is process explanatory drawing of the manufacturing method of lead frame relating to one embodiment of the present invention.Figure 2 is process explanatory drawing of the manufacturing method of lead frame relating to one embodiment of the present invention.Figure 3 is process explanatory drawing of the manufacturing method of lead frame relating to one embodiment of the present invention.Figure 4 is process explanatory drawing of the manufacturing method of lead frame relating to one embodiment of the present invention.Figure 5 is process explanatory drawing of the manufacturing method of lead frame relating to one embodiment of the present invention.Figure 6 is process explanatory drawing of the manufacturing method of lead frame relating to one embodiment of the present invention.Figure 7 is process explanatory drawing of the manufacturing method of lead frame relating to one embodiment of the present invention.Figure 8 is sectional front elevation of manufacturing equipment of clad metal sheet.[Explanation of symbols]10 * · · outer lead layer · · · etching stopper layer · · bump · · · external terminal · · · semiconductor chip20 ·' · copper foil or aluminum foil · · · nickel plating or nickel foil ' · · nickel plated copper foil, copper foil having nickel foil or aluminum foil having nickel foil · · * pay-off reel24 · · copper foil · · · pay-off reel · · · etching chamber * · · electrode roll · · · electrode roll29 ·' · vacuum chamber · · · rolling unit · · · clad sheet for lead frame · · winding roll40, 41, and 42 ' ·' photo resist film · · · conductor circuit

Claims

CLAIMS 1. A clad sheet (31) comprising Cu / Ni / AI for lead frame manufactured by pressbonding a copper foil having nickel plating (22) on one side of it to an aluminum foil (20) at the reduction rate of 0.1 to 3%.

52. A lead frame in which bumps (12) are formed by selectively etching the clad sheet (31) according to claim 1.

3. A manufacturing method of lead frame comprising: a. forming a clad sheet (31) comprising Cu / Ni / AI or Ni / Cu / Ni / Cu for lead frame by press-bonding a copper foil or an aluminum foil (20) to a nickel io foil or a nickel plated copper foil (22) which serve as etching stopper layer (11), and then; b. forming bumps (12) of copper or aluminum by selectively etching the clad sheet (31).

4. The method according to claim 3 wherein the clad sheet (31) for lead frame is 15 formed by previously activating the bonding surface of the copper foil or the aluminum foil (20) and the bonding surface of the nickel foil or nickel plating (21) in a vacuum chamber (29), laminating the copper foil or aluminum foil (20) to the nickel foil or nickel plating (21), and press-bonding at a reduction rate of 0.1 to 3%; -15wherein the activation treatment is practiced a. in a hyper low pressure inert gas atmosphere of 13.3 to 0.013 Pa (1 X 10'1 to 1 X 10'4 Torr);5 b. by glow discharging charging an alternate current of 1 to 50 MHz between one electrode A comprising the copper foil or aluminum foil (20) having bonding surface and the nickel foil or nickel plating (21), respectively, electrically grounded, and another electrode, electrode B, insulatingly supported, and io c. by sputter-etching d. in the manner that the electrode area exposed in a plasma generated by the glow discharging is not more than % the area of electrode B.