Raw material composition of thermoplastic product mixed with microalgae, product thereof and preparation method therefor

MYPI2025002395A0Undetermined Publication Date: 2024-04-19ECO RESEARCH SDN BHD
View PDF 0 Cites 0 Cited by

Patent Information

Application Number
MYPI2025002395
Authority / Receiving Office
MY · MY
Patent Type
Applications
Current Assignee / Owner
Priority Date
2022-10-19
Filing Date
2023-10-17
Publication Date
2024-04-19

AI Technical Summary

Technical Problem

Existing biodegradable plastics decompose at inconsistent rates in the environment, oxidatively degradable plastics are banned, naturally derived starch-based composites may compete with food sources, and there is a lack of efficient bioplastics that meet biodegradability, water solubility, mechanical and thermal properties. .

Method used

Using protein-rich microalgae as filler, combined with polyvinyl alcohol, compatibilizer, plasticizer, cross-linking agent, reaction aid and lubricant, the mixture is prepared through specific proportions and process steps to form a thermoplastic product, including drying, Pellets and molding process.

Benefits of technology

Comprehensive bioplastics that achieve biodegradability, water solubility, good mechanical and thermal properties are suitable for plastic production and reduce the problem of plastic waste.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure PI2025002395_DRAWING_001
    Figure PI2025002395_DRAWING_001
Patent Text Reader

Abstract

A raw material composition of a thermoplastic product mixed with microalgae, a product thereof and a preparation method therefor. The composition comprises polyvinyl alcohol, microalgae, a compatilizer, a plasticizer, a cross-linking agent, a reaction aid and a lubricating agent, wherein the weight percentage of the microalgae on the basis of the weight of the polyvinyl alcohol is between 10% and 30%; the weight percentage of the compatilizer on the basis of the weight of the polyvinyl alcohol is between 2% and 5%; the weight percentage of the plasticizer on the basis of the weight of the polyvinyl alcohol is between 20% and 30%; the weight percentage of the cross-linking agent on the basis of the weight of the polyvinyl alcohol is between 0% and 1.5%; the weight percentage of the reaction aid on the basis of the weight of the polyvinyl alcohol is between 1% and 5%; and the weight percentage of the lubricating agent on the basis of the weight of the polyvinyl alcohol is between 0.1% and 0.5%. Fig. 1
Need to check novelty before this filing date? Find Prior Art

Description

[0001] Raw material composition of thermoplastic product mixed with microalgae, product thereof and preparation method

[0002] [Technical Field] The present invention relates to a raw material composition of a thermoplastic product mixed with microalgae, and more particularly to a raw material composition of a thermoplastic product mixed with microalgae, the product thereof, and a preparation method thereof.

[0003] [Prior Art] Reducing and eliminating plastic waste is a global goal and challenge, and the use of biodegradable plastics is a major solution. However, oxo-degradable plastics, due to their specific degradation conditions and lack of consistent evidence regarding their environmental decomposition rates, have recently been banned by authorities including the European Union. Meanwhile, naturally derived plastics, such as starch-based composites, hold great potential for widespread application but may compete with food sources. Therefore, the development of functional bioplastics and composites that meet the requirements of biodegradability, water solubility, and good mechanical and thermal properties is a key issue. Among the raw materials for biodegradable plastics, algae are abundant and offer advantages such as rapid production, simple cultivation, and minimal impact on the food chain, making them suitable for use as polymer fillers in plastic production.

[0004] [Summary of the Invention] The present invention provides a raw material composition for a thermoplastic product mixed with microalgae. The weight percentage of the crosslinking agent based on the weight of the polyvinyl alcohol (PVA) is between 20% and 30%, the weight percentage of the crosslinking agent based on the weight of the PVA is between 0% and 1.5%, the weight percentage of the reaction aid based on the weight of the PVA is between 1% and 5%, and the weight percentage of the lubricant based on the weight of the PVA is between 0.1% and 0.5%. In one embodiment, the composition further includes a toughening agent, the weight percentage of which is between 0.2% and 0.5%, based on the weight of the PVA. In one embodiment, the degree of polymerization of the PVA is between 300 and 2400. In one embodiment, the hydrolysis rate of the PVA is between 88% and 99%. In one embodiment, the protein content of the microalgae is not less than 30%. In one embodiment, the microalgae is Spirulina sp., Chlorella sp., Nannochloropsis sp., Dunaliella sp., Tetraselmis sp., or a combination thereof. In one embodiment, the plasticizer is a polyol. In one embodiment, the polyol is glycerol, polyethylene glycol, sorbitol, xylitol, mannitol, or a combination thereof. In one embodiment, the compatibilizer is gum rosin. In one embodiment, the crosslinking agent is boric acid, citric acid, adipic acid, succinic acid, or suberic acid. In one embodiment, the reaction aid is a lubricant. In one embodiment, the lubricant comprises alkali metal stearic acid. According to one aspect, the present invention also provides a thermoplastic product mixed with microalgae, which is made from the above raw materials.According to one aspect, the present invention further provides a method for preparing a thermoplastic product mixed with microalgae, comprising the steps of: mixing polyvinyl alcohol, microalgae, a compatibilizer, a plasticizer, a crosslinking agent, a reaction aid, and a lubricant to obtain a mixture, wherein the weight percentage of the microalgae, based on the weight of the polyvinyl alcohol, is between 10% and 30%, the weight percentage of the compatibilizer, based on the weight of the polyvinyl alcohol, is between 2% and 5%, the weight percentage of the plasticizer, based on the weight of the polyvinyl alcohol, is between 20% and 30%, the weight percentage of the crosslinking agent, based on the weight of the polyvinyl alcohol, is between 0% and 1.5%, the weight percentage of the reaction aid, based on the weight of the polyvinyl alcohol, is between 1% and 5%, and the weight percentage of the lubricant, based on the weight of the polyvinyl alcohol, is between 0.1% and 0.5%; drying the mixture; forming the mixture into pellets; and shaping the pellets into a product.

[0005] [Brief Description of the Figures] The designated representative figures are: [Figure 1], which is a flow chart of the steps of an embodiment of the present invention.

[0006] [Implementation Methods] Although some embodiments herein perform steps in a specific order, these steps may be performed in another reasonable order. Certain features described below may be replaced or eliminated for different embodiments or examples. It should be understood that additional operations may be performed before, during, or after the described method, and that certain operations may be replaced or omitted in other embodiments of the method. Unless otherwise indicated, all numerical values ​​for dimensions, quantities, and physical properties used herein and in the claims should be understood to be modified in all instances by the term "about." Therefore, unless otherwise indicated, the numerical parameters listed herein and in the claims are approximate values, and those skilled in the art will be able to appropriately modify these approximate values ​​to achieve the desired properties using the disclosure herein. The use of numerical ranges expressed as endpoints includes all values ​​within that range and any range within that range. For example, 1 to 5 includes values ​​such as 1, 1.2, 1.5, 1.7, 2, 2.75, 3, 3.80, 4, and 5. The present invention discloses a raw material composition for a thermoplastic product mixed with microalgae. The composition primarily uses protein-rich microalgae as a filler. The composition also includes a water-soluble additive, including polyvinyl alcohol, which can be soluble in cold or hot water. In one example, the composition includes polyvinyl alcohol, microalgae, a compatibilizer, a plasticizer, a crosslinking agent, a processing aid, and a slipping agent. In another example, the composition may optionally include a toughening agent.In terms of proportions, the weight percentage of the microalgae, based on the weight of the polyvinyl alcohol, is between 10% and 30%, the weight percentage of the compatibilizer, based on the weight of the polyvinyl alcohol, is between 2% and 5%, the weight percentage of the plasticizer, based on the weight of the polyvinyl alcohol, is between 20% and 30%, the weight percentage of the cross-linking agent, based on the weight of the polyvinyl alcohol, is between 0% and 1.5%, the weight percentage of the reaction aid, based on the weight of the polyvinyl alcohol, is between 1% and 5%, the weight percentage of the lubricant, based on the weight of the polyvinyl alcohol, is between 0.1% and 0.5%, and the weight percentage of the toughening agent, based on the weight of the polyvinyl alcohol, is between 0.2% and 0.5%.In one example, the weight percentage of the microalgae based on the weight of the polyvinyl alcohol is 10%±0.5%, 12%±0.5%, 15%±0.5%, or 18%±0.5%, the weight percentage of the compatibilizer based on the weight of the polyvinyl alcohol is 2%±0.5%, 3%±0.5%, 4%±0.5%, or 5%±0.5%, the weight percentage of the plasticizer based on the weight of the polyvinyl alcohol is 16%±0.5%, 20%±0.5%, 24%±0.5%, or 25%±0.5%, and the weight percentage of the cross-linking agent based on the weight of the polyvinyl alcohol is 0% (i.e., no cross-linking agent is added), 0.2%±0.1%, 0.3%±0.1%, or 0.5%±0.1%. The weight percentage of the reaction aid, based on the weight of the polyvinyl alcohol, is 3.4%±0.5%, 3.6%±0.5%, 4%±0.5%, or 5%±0.5%. The weight percentage of the lubricant, based on the weight of the polyvinyl alcohol, is 0.2%±0.1%, 0.3%±0.1%, or 0.4%±0.1%. The weight percentage of the toughening agent, based on the weight of the polyvinyl alcohol, is 0.2±0.1% or 0.4±0.1%. The protein-rich microalgae used is a microalgae having a protein content of at least 30%, such as Spirulina sp., Chlorella sp., Nannochloropsis sp., Dunaliella sp., Tetraselmis sp., or a combination thereof. In terms of properties, in one example, the degree of polymerization of the polyvinyl alcohol is between 300 and 2400. If the degree of polymerization of the polyvinyl alcohol is relatively low, the melting point temperature and melt viscosity are relatively low, resulting in a lower Young's modulus and tensile strength of the final product, but a higher elongation at break. If the degree of polymerization of the polyvinyl alcohol is relatively high, the melting point temperature and melt viscosity are relatively high, resulting in a higher Young's modulus and tensile strength of the final product, but a lower elongation at break. Therefore, the degree of polymerization of the polyvinyl alcohol needs to be within an appropriate range.The hydrolysis rate of the polyvinyl alcohol is between 88% and 99%. For example, polyvinyl alcohols with hydrolysis rates of 88% (such as PVA-0588, PVA-1788, PVA-2088, PVA-2288, and PVA-2488) or 99% (such as PVA-0599, PVA-1799, PVA-2099, PVA-2299, and PVA-2499) can be used. If the hydrolysis rate of the polyvinyl alcohol is higher, such as 99%, the final product will need to be dissolved in water at a higher temperature (around 50°C), but will have better heat resistance during use. If the hydrolysis rate of the polyvinyl alcohol is too low, such as 88%, the final product will dissolve in water at room temperature, but will have poor heat resistance during use. Therefore, the hydrolysis rate of the polyvinyl alcohol needs to be within an appropriate range. Because the melting point of polyvinyl alcohol (PVA) is close to its decomposition temperature, thermal processing of PVA is generally difficult. Therefore, the addition of a plasticizer is necessary to widen the processing window and improve the processability and flexibility of the product. Plasticizers can be polyols, such as glycerol, polyethylene glycol, sorbitol, xylitol, and mannitol. In some cases, low-molecular-weight polyols can be selected. These have good penetrating power and can help fill the gaps between molecular chains. To facilitate compatibility and melt mixing between PVA and microalgae, a compatibilizer is added. This compatibilizer can be a natural material, such as gum rosin, to improve interfacial adhesion between PVA and microalgae, resulting in better mechanical and thermal properties for the product.Cross-linking agents can be selected from those with multifunctional groups that react with polyvinyl alcohol and microalgae, such as boric acid, citric acid, adipic acid, succinic acid, or suberic acid. The reaction aid can be a lubricant, such as stearic acid and / or polyethylene oxide, or an internal lubricant such as myristic acid, palmitic acid, or stearic acid, or an external lubricant such as polyethylene oxide. The lubricant can be, for example, an alkali metal stearic acid, such as sodium stearate or potassium stearate. Depending on the embodiment, the raw material composition can contain one or more components. For example, the polyvinyl alcohol may be selected from a single species or a combination of two or more species, such as a combination of PVA-0588 and PVA-1788 or a combination of PVA-0599 and PVA-1799. The microalgae may be selected from a single genus or a combination of two or more species, such as a combination of Spirulina and Chlorophytum. Similarly, the compatibilizer, plasticizer, crosslinker, reaction aid, and lubricant may be selected from a single species or a combination of two or more species.

[0007] Figure 1 is a flow chart of a preparation method according to one embodiment of the present invention, comprising the following steps. Polyvinyl alcohol, microalgae, a compatibilizer, a plasticizer, a crosslinking agent, a reaction aid, and a lubricant are first mixed to obtain a mixture (step S1). The raw materials are composed in the proportions described above. The mixture is then dried (step S2). The mixture is then formed into pellets (step S3). Finally, the pellets are formed into a product (step S4). In one example, a toughening agent may be further added to the mixture. The present invention is described in more detail below through experimental examples. However, the experimental examples of the present invention are not limited to the following and may be appropriately varied. Table 1 shows the raw materials and proportions used in Experimental Examples 1 to 6, and Table 2 shows the raw materials and proportions used in Experimental Examples 7 to 12. In Experiments 1 to 8, the raw materials were first mixed in a mixer at 300 rpm for approximately 3 minutes, then at 800 rpm for approximately 5 minutes. The resulting mixture was then dried at 55°C for approximately 24 hours. The dried mixture was then formed into pellets using an extrusion pelletizing machine, and then into plastic films using a blown film machine. In Experimental Example 1, the temperature profile of the extrusion process from zone 1 to the die head was 165°C, 165°C, 180°C, 185°C, 190°C, 185°C, 180°C, 170°C, and 165°C, and the temperature profile of the film blowing process from zone 1 to the die head was 185°C, 193°C, 205°C, 205°C, and 185°C, respectively. In Experimental Example 2, the temperature profile of the extrusion process from zone 1 to the die head was 175°C, 175°C, 190°C, 195°C, 200°C, 195°C, 190°C, 180°C, and 175°C, and the temperature profile of the film blowing process from zone 1 to the die head was 185°C, 193°C, 205°C, 205°C, and 185°C, respectively. The temperature to the die is 195 °C, 203 °C, 215 °C, 215 °C, and 195 °C in sequence.In Experimental Example 3, the temperature profile of the extrusion process from zone 1 to the die head was 175°C, 175°C, 190°C, 195°C, 200°C, 195°C, 190°C, 180°C, and 175°C, and the temperature profile of the film blowing process from zone 1 to the die head was 190°C, 198°C, 210°C, 210°C, and 190°C. In Experimental Example 4, the temperature profile of the extrusion process from zone 1 to the die head was 185°C, 185°C, 200°C, 205°C, 210°C, 205°C, 200°C, 190°C, and 185°C, and the temperature profile of the film blowing process from zone 1 to the die head was 195°C, 203°C, 215°C, 215°C, and 195°C. In Experimental Examples 5 to 7, the temperature profile of the extrusion process from zone 1 to the die head was 165°C, 165°C, 180°C, 185°C, 190°C, 185°C, 180°C, 170°C, and 165°C, respectively. The temperature profile of the film blowing process from zone 1 to the die head was 185°C, 193°C, 205°C, 205°C, and 185°C, respectively. In Experimental Example 8, the temperature profile of the extrusion process from zone 1 to the die head was 175°C, 185°C, 200°C, 205°C, 210°C, 205°C, 200°C, 190°C, and 185°C, respectively. The temperature profile of the film blowing process from zone 1 to the die head was 185°C, 193°C, 205°C, 205°C, and 185°C, respectively.

[0008] 185°C, 193°C, 205°C, 205°C, and 185°C. In Experiments 9 to 12, the raw materials were first mixed in a blender at 300 rpm for approximately 5 minutes, then at 800 rpm for approximately 3 minutes. The resulting mixture was then dried at 55°C for approximately 24 hours. The dried mixture was formed into pellets using a twin-screw extruder, and then into dumbbell-shaped plastic products using a BOY 22M injection molding machine. In Experimental Example 9, the temperature profile of the extrusion process from zone 1 to the die head is 165°C, 165°C, 180°C, 185°C, 190°C, 185°C, 180°C, 170°C, and 165°C. The temperature profile of the injection molding process from zone 1 to zone 3 is 165°C, 175°C, and 175°C. The nozzle temperature is 170°C. The pressure is maintained at 150°C.

[0009] The holding pressure was set sequentially between 30-40-50 bar, and the back pressure was set sequentially between 40-60 bar. In Experimental Example 10, the temperature profile of the extrusion process from Zone 1 to the die was 175°C, 175°C, 190°C, 195°C, 200°C, 195°C, 190°C, 180°C, and 175°C. The temperature profile of the injection molding process from Zone 1 to Zone 3 was 185°C, 195°C, and 195°C. The nozzle temperature was 190°C. The holding pressure was set sequentially between 65-75-85 bar, and the back pressure was set sequentially between 80-100 bar. In Experimental Example 11, the temperature profile of the extrusion process from zone 1 to the die was 175°C, 175°C, 190°C, 195°C, 200°C, 195°C, 190°C, 180°C, and 175°C, respectively. The temperature profile of the injection molding process from zone 1 to zone 3 was 185°C, 195°C, and 195°C, respectively. The nozzle temperature was 190°C. The holding pressure was set to 30-40-50 (bar), and the back pressure was set to 40-60 (bar). In Experimental Example 12, the extrusion process temperature profile from Zone 1 to the die was 185°C, 195°C, 210°C, 215°C, 220°C, 215°C, 210°C, 200°C, and 195°C, respectively. The injection molding process temperature profile from Zone 1 to Zone 3 was 185°C, 205°C, and 205°C, respectively. The nozzle temperature was 195°C. The holding pressure was set to 40-50-60 bar, and the back pressure was set to 60-80 bar. The plastic film products of Experimental Example 8 were tested for tensile strength using ASTM D882, while the products of Experimental Examples 9 to 12 were tested for tensile strength using ASTM D638. The results are shown in Table 3. The mechanical properties test results demonstrate that, based on the raw material composition disclosed herein, by appropriately adjusting the proportions, materials with varying mechanical properties can be produced, allowing for diverse applications. For example, the film product of Experimental Example 8 exhibits excellent ductility and moderate strength, while the plastic product of Experimental Example 12 exhibits good mechanical strength.

[0010] Replacement Page (Article 26 of the Regulations) Replacement Sheet (Article 26 of the Regulations) Table 3 -

Claims

Claims [Patent Application Scope] A raw material composition of a thermoplastic product mixed with microalgae, characterized in that: The composition includes: polyvinyl alcohol; microalgae, the weight percentage of which is between 10% and 30% based on the weight of the polyvinyl alcohol; a compatibilizer, the weight percentage of which is between 2% and 5% based on the weight of the polyvinyl alcohol; a plasticizer, the weight percentage of which is between 20% and 30% based on the weight of the polyvinyl alcohol; a cross-linking agent, the weight percentage of which is between 0% and 1.5% based on the weight of the polyvinyl alcohol; a reaction aid, the weight percentage of which is between 1% and 5% based on the weight of the polyvinyl alcohol; and a lubricant, the weight percentage of which is between 0.1% and 0.5% based on the weight of the polyvinyl alcohol. The raw material composition according to claim 1, characterized in that The composition further includes a toughening agent, the weight percentage of which is between 0.2% and 0.5% based on the weight of the polyvinyl alcohol. The raw material composition according to claim 1, characterized in that The degree of polymerization of the polyvinyl alcohol is between 300 and 2400. The raw material composition according to claim 1, characterized in that The hydrolysis rate of the polyvinyl alcohol is between 88% and 99%. The raw material composition according to claim 1, characterized in that The protein content of the microalgae is not less than 30%. The raw material composition according to claim 1, characterized in that The microalgae is of the genus Spirulina, Chlorella, Nannochloropsis, Dunaliella, Tetraselmis, or a combination thereof. The raw material composition according to claim 1, characterized in that The plasticizer is a polyol. The raw material composition according to claim 7 is characterized in that the polyol (polyol) is glycerol, polyethylene glycol, sorbitol, xylitol, mannitol, or a combination thereof. The raw material composition according to claim 1, characterized in that The compatibilizer is gum rosin. The raw material composition according to claim 1, characterized in that The cross-linking agent is boric acid, citric acid, adipic acid, succinic acid or suberic acid. The raw material composition according to claim 1, characterized in that The reaction aid is a lubricant. The raw material composition according to claim 1, characterized in that Such lubricants include alkali metal stearic acid. A thermoplastic product mixed with microalgae, characterized in that: The invention is prepared from the raw materials according to any one of claims 1 to 12. A method for preparing a thermoplastic product mixed with microalgae, characterized in that: The invention comprises the following steps: mixing polyvinyl alcohol, microalgae, a compatibilizer, a plasticizer, a cross-linking agent, a reaction aid and a lubricant to obtain a mixture, wherein the weight percentage of the microalgae based on the weight of the polyvinyl alcohol is between 10% and 30%, and the mixture is 16, the weight percentage of the solvent based on the weight of the polyvinyl alcohol is between 2% and 5%, the weight percentage of the plasticizer based on the weight of the polyvinyl alcohol is between 20% and 30%, the weight percentage of the cross-linking agent based on the weight of the polyvinyl alcohol is between 0% and 1.5%, the weight percentage of the reaction aid based on the weight of the polyvinyl alcohol is between 1% and 5%, and the weight percentage of the lubricant based on the weight of the polyvinyl alcohol is between 0.1% and 0.5%; drying the mixture; forming the mixture into pellets; and shaping the pellets into a product.