Composition for electrode formation, additive, and gelation inhibitor

MYPI2025002864A0Undetermined Publication Date: 2024-07-13NISSAN CHEM CORP
View PDF 0 Cites 0 Cited by

Patent Information

Application Number
MYPI2025002864
Authority / Receiving Office
MY · MY
Patent Type
Applications
Current Assignee / Owner
Priority Date
2023-09-29
Filing Date
2024-01-12
Publication Date
2024-07-13

AI Technical Summary

Technical Problem

Lithium-ion secondary battery electrode slurries face issues with thickening and gelation due to alkaline components, leading to uniformity problems, increased battery resistance, and reduced lifespan, with existing solutions either complicating the manufacturing process or introducing environmental and cost burdens.

Method used

A composition for forming electrodes that includes a positive electrode active material, a binder, and a solvent, with a heterocycle-containing compound having a nitrogen-containing 5-membered ring without oxygen atoms, which suppresses thickening and gelation, improving storage stability and battery characteristics.

Benefits of technology

The solution effectively prevents electrode slurry thickening and gelation, enhancing the quality and yield of energy storage devices, reducing manufacturing costs, and improving battery performance by forming a protective film on the positive electrode active material.

✦ Generated by Eureka AI based on patent content.
Patent Text Reader

Abstract

Provided is a composition for electrode formation with which it is possible to suppress thickening and gelation, improve shelf life and increase the concentration of solid matter by a simple method. The composition for electrode formation contains a positive electrode active substance, a binder, a solvent, and a heterocyclic compound, where the heterocyclic compound has a nitrogen-containing 5-membered ring, does not have an oxygen atom in the 5-membered ring, and has a carbonyl structure on the 5-membered ring.
Need to check novelty before this filing date? Find Prior Art

Description

Electrode-forming composition, additive, and gelation inhibitor

[0001] The present invention relates to an electrode-forming composition, an additive, and a gelation inhibitor.

[0002] Lithium-ion secondary batteries have a high energy density per unit weight and volume, which contributes to the miniaturization and lightening of electronic devices. In recent years, the spread of electric vehicles has accelerated as part of efforts to achieve zero-emissions automobiles, and there is a demand for batteries with even lower resistance, longer life, higher capacity, safety, and lower cost.

[0003] Lithium-ion secondary batteries generally have a three-layer structure consisting of a positive electrode, a separator, and a negative electrode, each containing an electrolyte. The positive electrode and the negative electrode are manufactured, for example, by coating a current collector with an electrode slurry, which is a mixture of an active material, a conductive material, and a binder. Currently, the most common method for manufacturing a negative electrode is to coat a copper foil current collector with the negative electrode slurry and then dry it. The most common method for manufacturing a positive electrode is to prepare a positive electrode slurry using an organic solvent such as N-methyl-2-pyrrolidone as a solvent, and then coat the aluminum foil current collector with the positive electrode slurry.

[0004] As positive electrode active materials for lithium ion secondary batteries, inorganic compounds such as transition metal oxides and transition metal chalcogens containing alkali metals are known as materials capable of obtaining a battery voltage of around 4 V. Among these, highly alkaline positive electrode active materials containing large amounts of nickel and manganese are used in order to obtain high-capacity lithium ion secondary batteries.

[0005] For example, Li x High-nickel positive electrode active materials, such as NiO2, have a high discharge capacity and are attractive positive electrode materials. However, alkaline components such as LiOH, Li2O, LiHCO3, and Li2CO3 are generated on the surface through proton exchange reactions with raw material residues or moisture, and reactions with moisture and carbon dioxide in the air.

[0006] When such a positive electrode active material is used, the electrode slurry may thicken or gel, gradually losing its fluidity, which not only makes it difficult to achieve a uniform coating thickness but also makes it impossible to apply the electrode slurry, resulting in waste of material.

[0007] The main cause of this is thought to be that, in the process of producing the positive electrode, alkaline components present on the surface of the positive electrode active material, in the presence of a trace amount of moisture, promote the dehydrofluorination reaction of the fluorine-based binder, such as polyvinylidene fluoride (PVdF) having a vinylidene fluoride structure, used as a binder.

[0008] Furthermore, alkaline components corrode the aluminum foil commonly used as a current collector for the positive electrode, thereby increasing the resistance of the battery, and may also react with the electrolyte in the battery, increasing the resistance of the battery and shortening its lifespan.

[0009] The thickening and gelation described above can be suppressed by handling the raw materials and the electrode slurry in a dry environment and controlling the water content. However, this requires large-scale facilities for a series of mass production processes from the preparation of the electrode slurry to the manufacture of the battery, and also poses problems of increased costs and increased environmental load due to the use of large amounts of electricity.

[0010] To solve this problem, for example, Patent Document 1 discloses a technique for suppressing gelation of an electrode slurry by preparing an electrode slurry (cathode material slurry) so that it does not exhibit strong alkalinity even when dispersed in water. However, preparing an electrode slurry so that it does not exhibit strong alkalinity using the method described in Patent Document 1 not only requires strict pH control, but also requires a process in which the cathode active material is first dispersed in water, filtered from the dispersion to extract the cathode active material, and then dried. As a result, this process leads to cumbersome operations and reduced yield. Furthermore, such a process may cause a decrease in the performance of the cathode active material itself.

[0011] Furthermore, Patent Document 2 reports a technology that uses a compound such as ultra-high molecular weight (weight average molecular weight of 2.2 million or more) polyethylene oxide to bind water through interactions with water (e.g., hydrogen bonding), thereby suppressing the reaction between the alkaline component of the positive electrode active material and water, thereby suppressing thickening and gelation. However, ultra-high molecular weight polymers with strong thickening effects have handling issues, such as the time and cost required for uniform dissolution in a solvent and the difficulty of producing a high-concentration solution. Furthermore, because the above-mentioned ultra-high molecular weight polymers have a high ability to bind water, there is a concern that the polymer itself may bring in water, and strict control over pre-drying is required to prevent this.

[0012] Patent Documents 3 and 4 propose adding an organic or inorganic acid to the positive electrode of a lithium-ion secondary battery to suppress gelation of the electrode slurry (positive electrode mixture slurry). Patent Document 3 uses maleic acid, citraconic acid, and malonic acid in the positive electrode mixture, while Patent Document 4 uses acetic acid, phosphoric acid, sulfuric acid, etc. in the electrode slurry (positive electrode paste). However, neutralizing the alkali with an acid requires the addition of a large amount of acid, which may result in a decrease in the battery's energy density and an increase in battery resistance. Furthermore, there is a problem that the acid corrodes the equipment used to fabricate the electrode. Furthermore, with this method, the high acidity of the organic or inorganic acid may cause a neutralization reaction with the lithium ions in the active material, potentially leading to a deterioration in battery performance.

[0013] Patent Document 5 reports a method of treating a positive electrode active material with fluorine gas and immobilizing the remaining LiOH as LiF, thereby preventing gelation and suppressing gas generation. However, fluorine gas is highly toxic and difficult to handle, and LiF produced as a by-product increases the internal resistance of the battery, reducing capacity. Furthermore, corrosion of the positive electrode active material by fluorine gas also reduces capacity. Furthermore, there is a problem in that the residual fluorine reacts with traces of moisture present in the active material and electrolyte to produce hydrogen fluoride, which easily causes cycle deterioration.

[0014] Patent Document 6 reports that unreacted lithium hydroxide and impurities derived from raw materials are removed by washing with an aqueous solution containing a lithium salt. However, there are issues with this method, such as increased environmental load due to wastewater generated during washing and the cost associated with treating the wastewater.

[0015] JP 2000-90917 A JP 2019-121471 A JP 9-306502 A JP 10-79244 A JP 2006-286240 A International Publication No. 2017-034001

[0016] In view of the above circumstances, the present invention aims to provide an electrode-forming composition that can suppress thickening and gelation of an electrode slurry by a simple method, thereby improving storage stability, increasing the solid content concentration, and suppressing battery deterioration, as well as an additive for an electrode slurry containing a positive electrode active material, a binder, and a solvent, and a method for suppressing gelation.

[0017] The present inventors have conducted extensive research to achieve the above-mentioned object, and have found that adding a specific heterocycle-containing compound having a nitrogen-containing five-membered ring and not containing an oxygen atom to an electrode slurry containing at least a positive electrode active material, a binder, and a solvent can suppress thickening and gelation of the composition and improve storage stability. Furthermore, electrodes fabricated using the electrode-forming composition of the present invention can suppress deterioration in batteries caused by alkaline components and can also improve battery performance.

[0018] That is, the present invention provides the following electrode-forming compositions, additives, and gelation inhibitors. 1. An electrode-forming composition comprising a positive electrode active material, a binder, a solvent, and a heterocycle-containing compound, wherein the heterocycle-containing compound has a nitrogen-containing five-membered ring, does not contain an oxygen atom in the five-membered ring, and has a carbonyl structure on the five-membered ring. 2. The electrode-forming composition of 1, in which the heterocycle-containing compound is attached to the positive electrode active material. 3. The electrode-forming composition of 1, in which the heterocycle-containing compound is a non-fused nitrogen-containing five-membered heterocyclic compound. 4. The electrode-forming composition of 1, in which the carbonyl structure exhibits proton tautomerism. 5. The electrode-forming composition of 4, in which the proton tautomerism is keto-enol tautomerism. 6. The electrode-forming composition of 1, in which the heterocycle-containing compound is represented by any of the following formulas (3) to (4): (In formulas (3) to (4), R a ~R c are each independently a hydrogen atom, a halogen atom, a carboxy group, a hydroxy group, a thiol group, an amino group, an alkyl group having 1 to 6 carbon atoms which may have a substituent, an alkenyl group having 2 to 6 carbon atoms which may have a substituent, or an aryl group having 6 to 12 carbon atoms which may have a substituent, and R a and R b may be bonded to each other to form a ring having 4 to 12 carbon atoms which may have a substituent; each L is independently a single bond, a carbonyl group, an ether bond, an ester bond or an amide bond; X a and X b are each independently a hydrogen atom, a lithium atom, a sodium atom, an alkyl group having 1 to 6 carbon atoms which may have a substituent, an aryl group having 6 to 12 carbon atoms which may have a substituent, or —CHNR d 2, and R d are each independently an alkyl group having 1 to 10 carbon atoms, an alkanol group having 1 to 10 carbon atoms, an alkenyl group having 2 to 10 carbon atoms, or an aryl group having 6 to 12 carbon atoms.) 7. a ~R c , X a and X b7. The electrode-forming composition of claim 1, wherein the substituent group of the heterocycle-containing compound is at least one selected from the group consisting of a carboxy group, a hydroxy group, an aldehyde group, an ester group, a ketone group, an amino group, a phenyl group, a halogen atom, an alkoxysilyl group, an epoxy group, a carboxylic acid chloride group, and a thiol group. (In the formula, R a ~R c is the same as above, and R e is a hydrogen atom, a carboxy group, a hydroxy group, an aldehyde group, an ester group, a ketone group, an amino group, a phenyl group, a halogen atom, an alkoxysilyl group, an epoxy group, a carboxylic acid chloride group, or a thiol group. 9. The electrode-forming composition of 1, wherein the heterocycle-containing compound is solid at room temperature. 10. The electrode-forming composition of 1, further comprising a conductive assistant. 11. The electrode-forming composition of 1, wherein the positive electrode active material contains 30% by mass or more of Ni. 12. The electrode-forming composition of 1, wherein the positive electrode active material contains 40% by mass or more of Ni. 13. The electrode-forming composition of 1, wherein the positive electrode active material contains 50% by mass or more of Ni. 14. The electrode-forming composition of 1, further comprising a nonionic polymer. 15. The electrode-forming composition of 14, wherein the nonionic polymer is a polymer having a pyrrolidone structure or a nitrile group. 16. 15. The electrode-forming composition of 15, wherein the nonionic polymer is at least one selected from the group consisting of polyvinylpyrrolidone and polyacrylonitrile. 17. The electrode-forming composition of 1, wherein the content of the heterocycle-containing compound is 0.001 to 0.5 mass% of the solid content. 18. An electrode-forming composition comprising a positive electrode active material, a binder, a solvent, and a heterocycle-containing compound, wherein the heterocycle-containing compound is represented by any one of the following formulas (1) or (2): (In formula (1), R a and R b are each independently a hydrogen atom, a carboxy group, a hydroxy group, a thiol group, an alkyl group having 1 to 6 carbon atoms which may have a substituent, an alkenyl group having 2 to 6 carbon atoms which may have a substituent, or an aryl group having 6 to 12 carbon atoms which may have a substituent,a and R b may be bonded to each other to form a ring having 4 to 12 carbon atoms which may have a substituent, each L is independently a single bond, a carbonyl group, an ether bond, an ester bond or an amide bond, Z is N or C-L-R c and R c is a hydrogen atom, a halogen atom, a carboxy group, a hydroxy group, a thiol group, an alkyl group having 1 to 6 carbon atoms which may have a substituent, an alkenyl group having 2 to 6 carbon atoms which may have a substituent, or an aryl group having 6 to 12 carbon atoms which may have a substituent, and X a is a hydrogen atom, a lithium atom, a sodium atom, an alkyl group having 1 to 6 carbon atoms which may have a substituent, an aryl group having 6 to 12 carbon atoms which may have a substituent, or —CHNR d 2, and R d are each independently an alkyl group having 1 to 10 carbon atoms, an alkanol group having 1 to 10 carbon atoms, an alkenyl group having 2 to 10 carbon atoms, or an aryl group having 6 to 12 carbon atoms. a and R b are each independently a hydrogen atom, a halogen atom, a carboxy group, a hydroxy group, a thiol group, an alkyl group having 1 to 6 carbon atoms which may have a substituent, an alkenyl group having 2 to 6 carbon atoms which may have a substituent, or an aryl group having 6 to 12 carbon atoms which may have a substituent; each L is independently a single bond, a carbonyl group, an ether bond, an ester bond, or an amide bond; X a is a hydrogen atom, a lithium atom, a sodium atom, an alkyl group having 1 to 6 carbon atoms which may have a substituent, an aryl group having 6 to 12 carbon atoms which may have a substituent, or —CHNR d 2, and R d are each independently an alkyl group having 1 to 10 carbon atoms, an alkanol group having 1 to 10 carbon atoms, an alkenyl group having 2 to 10 carbon atoms, or an aryl group having 6 to 12 carbon atoms.) 19. An electrode-forming composition according to 18, in which the heterocycle-containing compound is adhered to the positive electrode active material. 20. The R a ~R c , X aand X b 20. The electrode-forming composition of 18, wherein the substituent group of the formula (I) is at least one selected from the group consisting of a carboxy group, a hydroxy group, an aldehyde group, an ester group, a ketone group, a phenyl group, a halogen atom, an alkoxysilyl group, an epoxy group, a carboxylic acid chloride group, and a thiol group. 21. The electrode-forming composition of 18, wherein the heterocycle-containing compound is a heterocycle-containing compound represented by the following formula (5): (In the formula, Ar 1 Z, X are an aromatic ring having 4 to 12 carbon atoms which may have a substituent, or an aliphatic ring having 4 to 10 carbon atoms which may have a substituent. a are the same as above.) 22. The electrode-forming composition of 21, wherein the heterocycle-containing compound is a heterocycle-containing compound represented by any one of the following formulas (6) to (7): (Wherein Z and X aare the same as above.) 23. The electrode-forming composition of 18, wherein Z is N. 24. The electrode-forming composition of 18, further comprising a conductive additive. 25. The electrode-forming composition of 18, wherein the positive electrode active material contains 30% by mass or more of Ni. 26. The electrode-forming composition of 18, wherein the positive electrode active material contains 40% by mass or more of Ni. 27. The electrode-forming composition of 18, wherein the positive electrode active material contains 50% by mass or more of Ni. 28. The electrode-forming composition of 18, further comprising a nonionic polymer. 29. The electrode-forming composition of 28, wherein the nonionic polymer is a polymer having a pyrrolidone structure or a nitrile group. 30. The electrode-forming composition of 29, wherein the nonionic polymer is at least one selected from the group consisting of polyvinylpyrrolidone and polyacrylonitrile. 31. The electrode-forming composition of 18, wherein the content of the heterocycle-containing compound is 0.001 to 0.5 mass% of the solid content. 32. An electrode layer obtained from the electrode-forming composition of any one of 1 to 31. 33. An electrode comprising the electrode layer of 32. 34. A secondary battery comprising the electrode of 33. 35. A method for producing the electrode-forming composition of 1, comprising the steps of mixing a positive electrode active material, a binder, and a solvent to prepare a dispersion, and mixing the dispersion with a heterocycle-containing compound. 36. A method for producing the electrode-forming composition of 35, wherein a conductive assistant is further mixed in the step of preparing the dispersion. 37. A method for producing the electrode-forming composition of 18, comprising the steps of mixing a positive electrode active material, a binder, and a solvent to prepare a dispersion, and mixing the dispersion with a heterocycle-containing compound. 38. A method for producing the electrode-forming composition of 37, wherein a conductive assistant is further mixed in the step of preparing the dispersion. 39. An additive for an electrode slurry containing a positive electrode active material, a binder, and a solvent, the additive comprising a heterocycle-containing compound having a nitrogen-containing five-membered ring, the five-membered ring not containing an oxygen atom, and the five-membered ring having a carbonyl structure. 40. The additive of 39, wherein the heterocycle-containing compound is a non-fused nitrogen-containing five-membered heterocyclic compound. 41. The additive of 39, wherein the carbonyl structure exhibits proton tautomerism.42. The additive of 41, wherein the proton tautomerism is keto-enol tautomerism. 43. The additive of 39, wherein the heterocycle-containing compound is represented by any one of the following formulas (3) to (4): (In the formula, R a ~R c are each independently a hydrogen atom, a halogen atom, a carboxy group, a hydroxy group, a thiol group, an amino group, an alkyl group having 1 to 6 carbon atoms which may have a substituent, an alkenyl group having 2 to 6 carbon atoms which may have a substituent, or an aryl group having 6 to 12 carbon atoms which may have a substituent, and R a and R b may be bonded to each other to form a ring having 4 to 12 carbon atoms which may have a substituent; each L is independently a single bond, a carbonyl group, an ether bond, an ester bond or an amide bond; X a and X b are each independently a hydrogen atom, a lithium atom, a sodium atom, an alkyl group having 1 to 6 carbon atoms which may have a substituent, an aryl group having 6 to 12 carbon atoms which may have a substituent, or —CHNR d 2, and R d are each independently an alkyl group having 1 to 10 carbon atoms, an alkanol group having 1 to 10 carbon atoms, an alkenyl group having 2 to 10 carbon atoms, or an aryl group having 6 to 12 carbon atoms.) 44. a ~R c , X a and X b 45. The additive of 43, wherein the substituent group is at least one selected from the group consisting of a carboxy group, a hydroxy group, an aldehyde group, an ester group, a ketone group, an amino group, a phenyl group, a halogen atom, an alkoxysilyl group, an epoxy group, a carboxylic acid chloride group, and a thiol group. 46. The additive of 43, wherein the heterocycle-containing compound is represented by the following formula (4b): (In the formula, R a ~R c is the same as above, and R eis a hydrogen atom, a carboxy group, a hydroxy group, an aldehyde group, an ester group, a ketone group, an amino group, a phenyl group, a halogen atom, an alkoxysilyl group, an epoxy group, a carboxylic acid chloride group, or a thiol group. 46. The additive of 39, wherein the heterocycle-containing compound is solid at room temperature. 47. The additive of 39, wherein the positive electrode active material contains 30 mass% or more of Ni. 48. The additive of 39, further comprising a nonionic polymer. 49. The additive of 48, wherein the nonionic polymer is a polymer having a pyrrolidone structure or a nitrile group. 50. The additive of 49, wherein the nonionic polymer is at least one selected from the group consisting of polyvinylpyrrolidone and polyacrylonitrile. 51. The additive of 39, further comprising a solvent. 52. An additive for electrode slurry, comprising a positive electrode active material, a binder, and a solvent, the additive comprising a heterocycle-containing compound represented by any one of the following formulas (1) or (2): (In formula (1), R a and R b are each independently a hydrogen atom, a carboxy group, a hydroxy group, a thiol group, an alkyl group having 1 to 6 carbon atoms which may have a substituent, an alkenyl group having 2 to 6 carbon atoms which may have a substituent, or an aryl group having 6 to 12 carbon atoms which may have a substituent, a and R b may be bonded to each other to form a ring having 4 to 12 carbon atoms which may have a substituent, each L is independently a single bond, a carbonyl group, an ether bond, an ester bond or an amide bond, Z is N or C-L-R c and R c is a hydrogen atom, a halogen atom, a carboxy group, a hydroxy group, a thiol group, an alkyl group having 1 to 6 carbon atoms which may have a substituent, an alkenyl group having 2 to 6 carbon atoms which may have a substituent, or an aryl group having 6 to 12 carbon atoms which may have a substituent, and X a is a hydrogen atom, a lithium atom, a sodium atom, an alkyl group having 1 to 6 carbon atoms which may have a substituent, an aryl group having 6 to 12 carbon atoms which may have a substituent, or —CHNR d 2, and R dare each independently an alkyl group having 1 to 10 carbon atoms, an alkanol group having 1 to 10 carbon atoms, an alkenyl group having 2 to 10 carbon atoms, or an aryl group having 6 to 12 carbon atoms. a and R b are each independently a hydrogen atom, a halogen atom, a carboxy group, a hydroxy group, a thiol group, an alkyl group having 1 to 6 carbon atoms which may have a substituent, an alkenyl group having 2 to 6 carbon atoms which may have a substituent, or an aryl group having 6 to 12 carbon atoms which may have a substituent; each L is independently a single bond, a carbonyl group, an ether bond, an ester bond, or an amide bond; X a is a hydrogen atom, a lithium atom, a sodium atom, an alkyl group having 1 to 6 carbon atoms which may have a substituent, an aryl group having 6 to 12 carbon atoms which may have a substituent, or —CHNR d 2, and R dare each independently an alkyl group having 1 to 10 carbon atoms, an alkanol group having 1 to 10 carbon atoms, an alkenyl group having 2 to 10 carbon atoms, or an aryl group having 6 to 12 carbon atoms.) 53. The additive of 52, wherein the positive electrode active material contains 30 mass% or more of Ni. 54. The additive of 52, further comprising a nonionic polymer. 55. The additive of 54, wherein the nonionic polymer is a polymer having a pyrrolidone structure or a nitrile group. 56. The additive of 55, wherein the nonionic polymer is at least one selected from the group consisting of polyvinylpyrrolidone and polyacrylonitrile. 57. The additive of 52, further comprising a solvent. 58. A gelation inhibitor for an electrode slurry containing a positive electrode active material, a binder, and a solvent, the gelation inhibitor comprising a heterocycle-containing compound having a nitrogen-containing five-membered ring and not containing an oxygen atom in the nitrogen-containing five-membered ring. 59. The gelation inhibitor of 58, wherein the nitrogen-containing five-membered ring contains only nitrogen atoms as heteroatoms. 60. The gelation inhibitor of 59, wherein the nitrogen-containing five-membered ring contains two or three nitrogen atoms. 61. The gelation inhibitor of 58, wherein the heterocycle-containing compound has a carbonyl structure on the five-membered ring. 62. The gelation inhibitor of 61, wherein the heterocycle-containing compound is a non-fused nitrogen-containing five-membered heterocyclic compound. 63. The gelation inhibitor of 61, wherein the carbonyl structure exhibits proton tautomerism. 64. The gelation inhibitor of 63, wherein the proton tautomerism is keto-enol tautomerism. 65. The gelation inhibitor of 58, consisting of a heterocycle-containing compound represented by any one of the following formulas (3) to (4): (In the formula, R a ~R c are each independently a hydrogen atom, a halogen atom, a carboxy group, a hydroxy group, a thiol group, an amino group, an alkyl group having 1 to 6 carbon atoms which may have a substituent, an alkenyl group having 2 to 6 carbon atoms which may have a substituent, or an aryl group having 6 to 12 carbon atoms which may have a substituent, and R a and R b may be bonded to each other to form a ring having 4 to 12 carbon atoms which may have a substituent; each L is independently a single bond, a carbonyl group, an ether bond, an ester bond or an amide bond; Xa and X b are each independently a hydrogen atom, a lithium atom, a sodium atom, an alkyl group having 1 to 6 carbon atoms which may have a substituent, an aryl group having 6 to 12 carbon atoms which may have a substituent, or —CHNR d 2, and R d are each independently an alkyl group having 1 to 10 carbon atoms, an alkanol group having 1 to 10 carbon atoms, an alkenyl group having 2 to 10 carbon atoms, or an aryl group having 6 to 12 carbon atoms.) 66. a ~R c , X a and X b 65. The gelation inhibitor of 65, wherein the substituent group is at least one selected from the group consisting of a carboxy group, a hydroxy group, an aldehyde group, an ester group, a ketone group, an amino group, a phenyl group, a halogen atom, an alkoxysilyl group, an epoxy group, a carboxylic acid chloride group, and a thiol group. 67. The gelation inhibitor of 65, wherein the heterocycle-containing compound is represented by the following formula (4b): (In the formula, R a ~R c is the same as above, and R e is a hydrogen atom, a carboxy group, a hydroxy group, an aldehyde group, an ester group, a ketone group, an amino group, a phenyl group, a halogen atom, an alkoxysilyl group, an epoxy group, a carboxylic acid chloride group, or a thiol group.) 68. The gelation inhibitor of 58, wherein the heterocycle-containing compound is solid at room temperature. 69. The gelation inhibitor of 58, wherein the positive electrode active material contains 30 mass% or more of Ni. 70. The gelation inhibitor of 58, further comprising a nonionic polymer. 71. The gelation inhibitor of 70, wherein the nonionic polymer is a polymer having a pyrrolidone structure or a nitrile group. 72. The gelation inhibitor of 71, wherein the nonionic polymer is at least one selected from the group consisting of polyvinylpyrrolidone and polyacrylonitrile. 73. The gelation inhibitor of 58, further comprising a solvent. 74. A gelation inhibitor for an electrode slurry containing a positive electrode active material, a binder, and a solvent, the gelation inhibitor comprising a heterocycle-containing compound represented by any one of the following formulas (1) and (2): (In formula (1), Ra and R b are each independently a hydrogen atom, a carboxy group, a hydroxy group, a thiol group, an alkyl group having 1 to 6 carbon atoms which may have a substituent, an alkenyl group having 2 to 6 carbon atoms which may have a substituent, or an aryl group having 6 to 12 carbon atoms which may have a substituent, a and R b may be bonded to each other to form a ring having 4 to 12 carbon atoms which may have a substituent, each L is independently a single bond, a carbonyl group, an ether bond, an ester bond or an amide bond, Z is N or C-L-R c and R c is a hydrogen atom, a halogen atom, a carboxy group, a hydroxy group, a thiol group, an alkyl group having 1 to 6 carbon atoms which may have a substituent, an alkenyl group having 2 to 6 carbon atoms which may have a substituent, or an aryl group having 6 to 12 carbon atoms which may have a substituent, and X a is a hydrogen atom, a lithium atom, a sodium atom, an alkyl group having 1 to 6 carbon atoms which may have a substituent, an aryl group having 6 to 12 carbon atoms which may have a substituent, or —CHNR d 2, and R d are each independently an alkyl group having 1 to 10 carbon atoms, an alkanol group having 1 to 10 carbon atoms, an alkenyl group having 2 to 10 carbon atoms, or an aryl group having 6 to 12 carbon atoms. a and R b are each independently a hydrogen atom, a halogen atom, a carboxy group, a hydroxy group, a thiol group, an alkyl group having 1 to 6 carbon atoms which may have a substituent, an alkenyl group having 2 to 6 carbon atoms which may have a substituent, or an aryl group having 6 to 12 carbon atoms which may have a substituent; each L is independently a single bond, a carbonyl group, an ether bond, an ester bond, or an amide bond; X a and X b are each independently a hydrogen atom, a lithium atom, a sodium atom, an alkyl group having 1 to 6 carbon atoms which may have a substituent, an aryl group having 6 to 12 carbon atoms which may have a substituent, or —CHNR d 2, and R dare each independently an alkyl group having 1 to 10 carbon atoms, an alkanol group having 1 to 10 carbon atoms, an alkenyl group having 2 to 10 carbon atoms, or an aryl group having 6 to 12 carbon atoms.) 75. a ~R c , X a and X b 76. The gelation inhibitor of 74, wherein the substituent group of formula (I) is at least one selected from the group consisting of a carboxy group, a hydroxy group, an aldehyde group, an ester group, a ketone group, a phenyl group, a halogen atom, an alkoxysilyl group, an epoxy group, a carboxylic acid chloride group, and a thiol group. 77. The gelation inhibitor of 74, wherein the heterocycle-containing compound is a heterocycle-containing compound represented by the following formula (5): (In the formula, Ar 1 Z, X are an aromatic ring having 4 to 12 carbon atoms which may have a substituent, or an aliphatic ring having 4 to 10 carbon atoms which may have a substituent. a are the same as above.) 77. The gelation inhibitor of 76, wherein the heterocycle-containing compound is a heterocycle-containing compound represented by any one of the following formulas (6) to (7): (Wherein Z and X a are the same as above.) 78. The gelation inhibitor of 74, wherein Z is N. 79. The gelation inhibitor of 74, wherein the positive electrode active material contains 30 mass% or more of Ni. 80. The gelation inhibitor of 74, further comprising a nonionic polymer. 81. The gelation inhibitor of 80, wherein the nonionic polymer is a polymer having a pyrrolidone structure or a nitrile group. 82. The gelation inhibitor of 81, wherein the nonionic polymer is at least one selected from the group consisting of polyvinylpyrrolidone and polyacrylonitrile. 83. The gelation inhibitor of 74, further comprising a solvent.

[0019] The electrode-forming composition of the present invention is resistant to thickening and gelation and has high storage stability, making it suitable for use in forming positive electrodes for energy storage devices. When an energy storage device is manufactured using the composition, benefits such as improved quality and yield due to the improved storage stability of the composition, cost reduction and reduced environmental impact due to a high solids concentration, and suppression of deterioration within the battery caused by alkaline components can be expected, contributing to reduced manufacturing costs for the energy storage device and improved battery characteristics.

[0020] In the present invention, the above-mentioned thickening and gelation suppression effect is achieved by adding a specific heterocycle-containing compound to an electrode slurry containing a positive electrode active material, a binder, and a solvent, whereby a majority of the heterocycle-containing compound adheres to the positive electrode active material, forming a protective coating on the surface of the positive electrode active material. This protective coating suppresses the proton exchange reaction between the active material and water and suppresses the reaction between alkaline components derived from the positive electrode active material and the binder, particularly a fluorine-based binder. As a result, thickening and gelation of the composition can be suppressed, improving storage stability. It is known that electrode slurries containing a positive electrode active material, a binder, and a solvent, are prone to gelation when using a Ni-rich positive electrode active material, for example, a positive electrode active material containing 30% by mass or more of Ni. Adding the additive or gelation suppressor of the present invention to the electrode slurry significantly suppresses gelation of the electrode slurry. According to the present invention, suppressing thickening and gelation of the electrode slurry enables the formation of a homogeneous positive electrode layer. It also makes it possible to improve the solids concentration in the electrode slurry, thereby reducing the cost and environmental impact of producing energy storage devices. Furthermore, it is possible to suppress corrosion of aluminum foil, which is commonly used as a current collector foil, and deterioration of battery characteristics due to reaction with the electrolyte, which are caused by alkaline components. Therefore, according to the present invention, gelation of the electrode slurry can be effectively suppressed, regardless of the type of conductive additive or binder. However, the present invention is not limited to these mechanisms.

[0021] [Electrode-Forming Composition] The present invention is characterized in that when an additive containing a heterocycle-containing compound or a gelation inhibitor containing a heterocycle-containing compound is added to an electrode slurry containing a positive electrode active material, a binder, and a solvent, a majority of the additive or gelation inhibitor adheres to the positive electrode active material. The form of adhesion is not limited here, and it may be physical adsorption, chemical adsorption, or chemical bonding such as ionic bonding or hydrogen bonding. Preferably, 60% by mass or more of the additive containing a heterocycle-containing compound or the gelation inhibitor containing a heterocycle-containing compound contained in the electrode-forming composition adheres to the positive electrode active material, more preferably 70% by mass or more, even more preferably 75% by mass or more, and particularly preferably 80% by mass or more. In the present invention, terms related to gelation inhibition, such as "gelation inhibition," refer to the suppression of gelation of the electrode-forming composition compared to when the additive or gelation inhibitor of the present invention is not included.

[0022] <Heterocycle-Containing Compound> The electrode-forming composition of the present invention comprises a positive electrode active material, a binder, a solvent, and a heterocycle-containing compound, wherein the heterocycle-containing compound has a nitrogen-containing five-membered ring and does not contain an oxygen atom in the five-membered ring. The heterocycle-containing compound of the present invention is different from the solvent of the present invention and is preferably solid at room temperature. In the present invention, "solid at room temperature" means that the melting point at 1 atmosphere is 25°C or higher. "Not containing an oxygen atom in the five-membered ring" means that none of the five atoms constituting the five-membered ring are oxygen atoms. "Having a carbonyl structure (carbonyl group) on the ring" means that at least one carbon atom of the five atoms constituting the five-membered ring is bonded to an oxygen atom by a double bond. For example, furan contains an oxygen atom in the five-membered ring but does not have a carbonyl structure (carbonyl group) on the ring. For example, pyrazolone contains two nitrogen atoms in a five-membered ring, no oxygen atoms in the five-membered ring, and a carbonyl structure (carbonyl group) on the ring, whereas oxazoline contains one oxygen atom and one nitrogen atom in the five-membered ring, and no carbonyl structure (carbonyl group) on the ring.

[0023] The heterocycle-containing compound is preferably one in which the nitrogen-containing five-membered ring contains only a nitrogen atom as a heteroatom, and more preferably one in which the nitrogen-containing five-membered ring contains two or three nitrogen atoms.

[0024] Furthermore, the heterocycle-containing compound preferably has a carbonyl structure (carbonyl group) on the nitrogen-containing five-membered ring, and in this case, it is more preferable that the nitrogen-containing five-membered ring is not a condensed ring. Furthermore, it is even more preferable that the carbonyl structure exhibits proton tautomerism, and even more preferably exhibits keto-enol tautomerism. Note that keto-enol tautomerism refers to the tautomerism between keto (ketone, aldehyde) and enol.

[0025] In the present invention, it is preferable that the heterocycle-containing compound does not contain two or more bonds selected from the group consisting of amide bonds and sulfide bonds in the nitrogen-containing five-membered ring.

[0026] Furthermore, it is preferable that the heterocycle-containing compound does not have a partial structure represented by the following formula:

[0027] (* represents a bond.)

[0028] Specific examples of the heterocycle-containing compound include those represented by any of the following formulas (1) to (4).

[0029] (In formula (1), R a and R b are each independently a hydrogen atom, a carboxy group, a hydroxy group, a thiol group, an amino group, an alkyl group having 1 to 6 carbon atoms which may have a substituent, an alkenyl group having 2 to 6 carbon atoms which may have a substituent, or an aryl group having 6 to 12 carbon atoms which may have a substituent, and R a and R b are bonded to each other to form a ring having 4 to 12 carbon atoms which may have a substituent; each L is independently a single bond, a carbonyl group, an ether bond, an ester bond or an amide bond; Z is N or C-L-R c and R c is a hydrogen atom, a halogen atom, a carboxy group, a hydroxy group, a thiol group, an amino group, an alkyl group having 1 to 6 carbon atoms which may have a substituent, an alkenyl group having 2 to 6 carbon atoms which may have a substituent, or an aryl group having 6 to 12 carbon atoms which may have a substituent, and X a are each independently a hydrogen atom, a lithium atom, a sodium atom, an alkyl group having 1 to 6 carbon atoms which may have a substituent, an aryl group having 6 to 12 carbon atoms which may have a substituent, or —CHNR d 2, and R d are each independently an alkyl group having 1 to 10 carbon atoms, an alkanol group having 1 to 10 carbon atoms, an alkenyl group having 2 to 10 carbon atoms, or an aryl group having 6 to 12 carbon atoms. a ~R care each independently a hydrogen atom, a halogen atom, a carboxy group, a hydroxy group, a thiol group, an amino group, an alkyl group having 1 to 6 carbon atoms which may have a substituent, an alkenyl group having 2 to 6 carbon atoms which may have a substituent, or an aryl group having 6 to 12 carbon atoms which may have a substituent, and R a and R b may be bonded to each other to form a ring having 4 to 12 carbon atoms which may have a substituent; each L is independently a single bond, a carbonyl group, an ether bond, an ester bond or an amide bond; X a and X b are each independently a hydrogen atom, a lithium atom, a sodium atom, an alkyl group having 1 to 6 carbon atoms which may have a substituent, an aryl group having 6 to 12 carbon atoms which may have a substituent, or —CHNR d 2, and R d are each independently an alkyl group having 1 to 10 carbon atoms, an alkanol group having 1 to 10 carbon atoms, an alkenyl group having 2 to 10 carbon atoms, or an aryl group having 6 to 12 carbon atoms.

[0030] The above formulas (2), (3), and (4) may be structural isomers. Specifically, isomers of the heterocycle-containing compound represented by formula (2) include heterocycle-containing compounds represented by the following formulas (2-A) to (2-C), isomers of the heterocycle-containing compound represented by formula (3) include heterocycle-containing compounds represented by the following formulas (3-A) to (3-E), and isomers of the heterocycle-containing compound represented by formula (4) include heterocycle-containing compounds represented by the following formulas (4-A) to (4-G).

[0031] X a and X b are each a hydrogen atom, a lithium atom, or a sodium atom, the tautomers are preferred among the structural isomers. a and X b are hydrogen atoms, the tautomers are also called proton tautomers.

[0032] (In the formula, R a ~R c , L, Xa , X b is the same as above.)

[0033] R a ~R c The alkyl group having 1 to 6 carbon atoms, represented by the formula (I), may be any of linear, branched, and cyclic, and specific examples thereof include linear or branched alkyl groups having 1 to 6 carbon atoms, such as a methyl group, an ethyl group, an n-propyl group, an isopropyl group, an n-butyl group, an isobutyl group, an s-butyl group, a t-butyl group, an n-pentyl group, and an n-hexyl group; and cyclic alkyl groups having 3 to 6 carbon atoms, such as a cyclopropyl group, a cyclobutyl group, a cyclopentyl group, and a cyclohexyl group.

[0034] R a ~R c Examples of the alkenyl group having 2 to 6 carbon atoms represented by the formula (I) include ethenyl group, n-1-propenyl group, n-2-propenyl group, 1-methylethenyl group, n-1-butenyl group, n-2-butenyl group, n-3-butenyl group, 2-methyl-1-propenyl group, 2-methyl-2-propenyl group, 1-ethylethenyl group, 1-methyl-1-propenyl group, 1-methyl-2-propenyl group, and n-1-pentenyl group.

[0035] R a ~R c Examples of the aryl group having 6 to 12 carbon atoms represented by the formula (I) include a phenyl group, a tolyl group, a 1-naphthyl group, and a 2-naphthyl group.

[0036] The above R a and R b Examples of the ring having 4 to 12 carbon atoms formed by bonding together include a cyclopentane ring, a cyclohexane ring, a benzene ring, a naphthalene ring, a triazole ring, a pyridine ring, and a pyrazine ring.

[0037] The above R a ~R cmay have a substituent. Examples of the substituent include a carboxy group, a hydroxy group, an aldehyde group, an ester group, a ketone group, an amino group, a phenyl group, a halogen atom, an alkoxysilyl group, an epoxy group, a carboxylic acid chloride group, and a thiol group. Examples of the alkoxysilyl group include a trimethoxysilyl group, a dimethoxymethylsilyl group, a methoxydimethylsilyl group, a triethoxysilyl group, a diethoxymethylsilyl group, and an ethoxydimethylsilyl group. In the present invention, a carboxy group is preferred. a ~R c When has a substituent, the number of the substituents is preferably 1 to 6, and more preferably 1 to 3.

[0038] The above R a ~R c Examples of the alkyl group include a hydrogen atom, a carboxy group, an alkyl group having 1 to 6 carbon atoms which may have a substituent, an aryl group having 6 to 12 carbon atoms which may have a substituent, and R a and R b are preferably bonded to each other to form a ring having 4 to 12 carbon atoms which may have a substituent.

[0039] In addition, the above R a ~R c Examples of the alkyl group include a hydrogen atom, a carboxy group, an alkyl group having 1 to 6 carbon atoms, an aryl group having 6 to 12 carbon atoms, and R a and R b However, it is more preferable that they are bonded to each other to form an aromatic ring having 4 to 12 carbon atoms which may have a substituent.

[0040] Furthermore, the above R a ~R c Examples of the alkyl group include a hydrogen atom, a carboxy group, an alkyl group having 1 to 3 carbon atoms, an aryl group having 6 to 10 carbon atoms, and R a and R b are bonded to each other to form an aromatic ring having 6 to 10 carbon atoms which may have a substituent.

[0041] Furthermore, the above R a ~R c Examples of the aryl group include a hydrogen atom, a carboxy group, a methyl group, a phenyl group, and R a and Rb More preferred is an optionally substituted benzene ring formed by bonding together:

[0042] L is preferably a single bond, an ester bond or an amide bond, and more preferably a single bond.

[0043] Z is preferably N.

[0044] X a and X b The alkyl group having 1 to 6 carbon atoms, represented by the formula (I), may be any of linear, branched, and cyclic, and specific examples thereof include linear or branched alkyl groups having 1 to 6 carbon atoms, such as a methyl group, an ethyl group, an n-propyl group, an isopropyl group, an n-butyl group, an isobutyl group, an s-butyl group, a t-butyl group, an n-pentyl group, and an n-hexyl group; and cyclic alkyl groups having 3 to 6 carbon atoms, such as a cyclopropyl group, a cyclobutyl group, a cyclopentyl group, and a cyclohexyl group.

[0045] X a and X b Examples of the aryl group having 6 to 12 carbon atoms represented by the formula (I) include a phenyl group, a tolyl group, a 1-naphthyl group, and a 2-naphthyl group.

[0046] Above X a and X b may have a substituent. Examples of the substituent include a carboxy group, a hydroxy group, an aldehyde group, an ester group, a ketone group, an amino group, a phenyl group, a halogen atom, an alkoxysilyl group, an epoxy group, a carboxylic acid chloride group, and a thiol group. Examples of the alkoxysilyl group include a trimethoxysilyl group, a dimethoxymethylsilyl group, a methoxydimethylsilyl group, a triethoxysilyl group, a diethoxymethylsilyl group, and an ethoxydimethylsilyl group. In the present invention, a carboxy group and an alkoxysilyl group are preferred, and a carboxy group and a trimethoxysilyl group are more preferred.

[0047] R dThe alkyl group having 1 to 10 carbon atoms and represented by the formula (I) may be linear, branched or cyclic, and specific examples thereof include linear or branched alkyl groups having 1 to 10 carbon atoms such as methyl, ethyl, n-propyl, isopropyl, cyclopropyl, n-butyl, isobutyl, s-butyl, t-butyl, n-pentyl, neopentyl, n-hexyl, n-octyl, n-nonyl and n-decyl groups; and cyclic alkyl groups having 3 to 10 carbon atoms such as cyclopropyl, cyclobutyl, cyclopentyl, cyclohexyl and 1-adamantyl groups.

[0048] R d Examples of the alkanol group having 1 to 10 carbon atoms represented by the formula (I) include a hydroxymethyl group, a hydroxyethyl group, a hydroxypropyl group, a hydroxybutyl group, a hydroxypentyl group, a hydroxyhexyl group, a hydroxyoctyl group, a hydroxynonyl group, and a hydroxydecyl group.

[0049] R d Examples of the alkenyl group having 2 to 10 carbon atoms represented by the formula (I) include ethenyl group, n-1-propenyl group, n-2-propenyl group, 1-methylethenyl group, n-1-butenyl group, n-2-butenyl group, n-3-butenyl group, 2-methyl-1-propenyl group, 2-methyl-2-propenyl group, 1-ethylethenyl group, 1-methyl-1-propenyl group, 1-methyl-2-propenyl group, n-1-pentenyl group, and n-1-decenyl group.

[0050] R d Examples of the aryl group having 6 to 12 carbon atoms represented by the formula (I) include a phenyl group, a tolyl group, a 1-naphthyl group, and a 2-naphthyl group.

[0051] Above X a and X b Examples of the alkyl group include a hydrogen atom, a lithium atom, a sodium atom, an alkyl group having 1 to 6 carbon atoms which may have a substituent, an aryl group having 6 to 12 carbon atoms which may have a substituent, and —CHNR d 2 is preferred.

[0052] In addition, the above X a and X bExamples of the alkyl group include a hydrogen atom, a lithium atom, a sodium atom, an alkyl group having 1 to 4 carbon atoms, an aryl group having 6 to 10 carbon atoms, and —CHNR d 2 is preferred.

[0053] Furthermore, the above X a and X b Examples of the alkyl group include a hydrogen atom, a lithium atom, a sodium atom, an alkyl group having 1 to 3 carbon atoms, an aryl group having 6 to 8 carbon atoms, and —CHNR d 2 is more preferred.

[0054] Furthermore, the above X a and X b Examples of the —CHNR group include a hydrogen atom, a lithium atom, a sodium atom, a methyl group, a phenyl group, and —CHNR d 2 is even more preferred.

[0055] The above R d As the alkyl group, an alkyl group having 1 to 3 carbon atoms and an aryl group having 6 to 10 carbon atoms are preferred, and a methyl group and a phenyl group are more preferred.

[0056] As the heterocycle-containing compounds represented by the above formulas (1) to (4), heterocycle-containing compounds represented by the following formulas (1a) to (4a) are preferred.

[0057] (In the formula, R a ~R c , Z, X a , X b is the same as above.)

[0058] Furthermore, the heterocycle-containing compound is more preferably a heterocycle-containing compound represented by the following formula (5).

[0059] (In the formula, Ar 1 Z, X are an aromatic ring having 4 to 12 carbon atoms which may have a substituent, or an aliphatic ring having 4 to 10 carbon atoms which may have a substituent. a is the same as above.)

[0060] The heterocycle-containing compound is more preferably a heterocycle-containing compound represented by any one of the following formulas (6) to (7).

[0061] (Wherein Z and X a is the same as above.)

[0062] In addition to the heterocycle-containing compound represented by the above formula (5), the heterocycle-containing compound represented by the following formula (4b) is more preferred.

[0063] (In the formula, R a ~R c is the same as above, and R e is a hydrogen atom, a carboxy group, a hydroxy group, an aldehyde group, an ester group, a ketone group, an amino group, a phenyl group, a halogen atom, an alkoxysilyl group, an epoxy group, a carboxylic acid chloride group, or a thiol group.

[0064] In the above formula (4b), R e When is a hydrogen atom, X in the above formula (4) a corresponds to an embodiment in which no substituent is present. e is other than a hydrogen atom, e is X in the above formula (4). a The substituent corresponds to the substituent possessed by X a and X b The substituents are the same as those described in the description of the substituents possessed by the group.

[0065] Furthermore, the heterocycle-containing compound is more preferably a heterocycle-containing compound represented by the following formula (8).

[0066] (In the formula, R a ~R c is the same as above.)

[0067] Specific examples of the heterocycle-containing compound represented by the above formula (1) include heterocycle-containing compounds represented by the following formulas (1-1) to (1-15).

[0068] *The structure of the heterocycle-containing compound represented by formula (1-6) is the structure of the compound manufactured by Shin-Etsu Chemical Co., Ltd. as X-12-1214A and described in the catalog of the company.

[0069] Specific examples of the heterocycle-containing compound represented by the above formula (2) include heterocycle-containing compounds represented by the following formulas (2-1) to (2-7).

[0070]

[0071] Specific examples of the heterocycle-containing compound represented by the above formula (3) include heterocycle-containing compounds represented by the following formulas (3-1) to (3-13).

[0072]

[0073] Specific examples of the heterocycle-containing compound represented by the above formula (4) include heterocycle-containing compounds represented by the following formulas (4-1) to (4-14).

[0074]

[0075] The content of the heterocycle-containing compound is preferably 0.001 to 4 mass% of the solid content, more preferably 0.001 to 2 mass%, even more preferably 0.001 to 0.5 mass%, even more preferably 0.001 to 0.3 mass%, and particularly preferably 0.001 to 0.2 mass%. An even more preferable lower limit of the content of the heterocycle-containing compound is 0.01 mass% of the solid content. By keeping the content of the heterocycle-containing compound within this range, gelation of the electrode-forming composition can be effectively suppressed, and the battery characteristics of the resulting battery can be maintained. In this specification, the term "solid content" refers to the components other than the solvent that constitute the composition (the same applies hereinafter).

[0076] The content of the heterocycle-containing compound is preferably 0.001 to 4 parts by mass, more preferably 0.001 to 2 parts by mass, even more preferably 0.001 to 0.5 parts by mass, even more preferably 0.001 to 0.3 parts by mass, and particularly preferably 0.001 to 0.2 parts by mass, relative to 100 parts by mass of the positive electrode active material. By setting the content of the heterocycle-containing compound within the above range, gelation of the electrode-forming composition can be effectively suppressed, and the battery characteristics of the resulting battery can be maintained.

[0077] The content of the heterocycle-containing compound is preferably 0.1 to 50 parts by mass, more preferably 0.1 to 30 parts by mass, and even more preferably 0.1 to 20 parts by mass, relative to 100 parts by mass of the binder. By setting the content of the heterocycle-containing compound within the above range, gelation of the electrode-forming composition can be effectively suppressed, and the battery characteristics of the resulting battery can be maintained.

[0078] <Positive Electrode Active Material> The positive electrode active material can be appropriately selected from various active materials conventionally used in electrodes for energy storage devices such as secondary batteries, and can be selected from those that satisfy the above conditions. For example, in the case of lithium secondary batteries or lithium ion secondary batteries, chalcogen compounds or lithium ion-containing chalcogen compounds capable of adsorbing and desorbing lithium ions, polyanionic compounds, elemental sulfur and its compounds, etc. can be used. In order to further improve battery capacity, reduce the amount of rare metal used, and reduce cost, a positive electrode active material containing 30% by mass or more of Ni is preferred. In the present invention, in order to further reduce the amount of rare metal used and obtain a battery with even greater capacity, a positive electrode active material containing 35% by mass or more of Ni is more preferred, a positive electrode active material containing 40% by mass or more of Ni is even more preferred, a positive electrode active material containing 50% by mass or more of Ni is even more preferred, and a positive electrode active material containing 55% by mass or more of Ni is particularly preferred. The upper limit is not particularly limited, but is typically 65% ​​by mass or less.

[0079] Examples of lithium ion-containing chalcogen compounds include LiNiO2, Li x Ni y M 1-y O2 (M represents at least one metal element selected from Co, Mn, Ti, Cr, V, Al, Sn, Pb, and Zn, and 0.05≦x≦1.10, 0.3≦y≦1.0), Li a Ni (1-x-y) Co x M 1 y M 2 z O2 (M 1 is at least one selected from the group consisting of Mn and Al; 2represents at least one element selected from the group consisting of Zr, Ti, Mg, B, Zr, W, and V, and 1.00≦a≦1.50, 0.00≦x≦0.50, 0≦y≦0.50, 0.000≦z≦0.020). Examples of polyanion compounds include LiFePO 4、 Li a Mn b Fe c D d PO4 (wherein 1.00≦a≦1.15, 0.01≦b≦0.99, 0.01≦c≦0.99, 0.00≦d≦0.10, and D is selected from Co, Mn, Ti, Cr, V, Al, Sn, Pb, and Zn, and at least a portion of the positive electrode active material has an olivine structure). Examples of sulfur compounds include sulfur, Li2S, FeS2, TiS2, MoS2, and rubeanic acid. These positive electrode active materials can be used alone or in combination of two or more.

[0080] In the present invention, among the above positive electrode active materials, Li a Ni (1-x-y) Co x M 1 y M 2 z X w O2 (M 1 is at least one selected from the group consisting of Mn and Al; 2 represents at least one selected from the group consisting of Zr, Ti, Mg, W, and V, and preferably 1.00≦a≦1.50, 0.00≦x≦0.50, 0≦y≦0.50, 0.000≦z≦0.020, 0.000≦w≦0.020). These active materials can be used singly or in combination of two or more.

[0081] The content of the positive electrode active material is preferably 88.0 to 99.949 mass % of the solid content, more preferably 88.0 to 99.899 mass %, and even more preferably 95.0 to 99.0 mass %.

[0082] The binder can be appropriately selected from known materials and is not particularly limited. Specific examples include fluorine-based binders such as polyvinylidene fluoride (PVdF), polytetrafluoroethylene, copolymers containing at least one monomer selected from the group consisting of vinylidene fluoride, tetrafluoroethylene, and hexafluoropropylene, and non-aqueous binders such as polyimide, ethylene-propylene-diene terpolymer, styrene-butadiene rubber, polyethylene, and polypropylene. In the present invention, the use of a fluorine-based binder is preferable from the viewpoint of improving the storage stability of the composition. Furthermore, the fluorine-based binder is preferably modified with a polar functional group such as a carboxy group or a hydroxyl group. The polar functional group can be confirmed by the presence or absence of a clear peak detected in the range of 10 to 15 ppm in measurement using a nuclear magnetic resonance (NMR) spectrometer. The binders can be used alone or in combination of two or more.

[0083] The weight-average molecular weight (Mw) of the binder is 600,000 to 3,000,000, preferably 700,000 to 2,000,000, and more preferably 700,000 to 1,500,000, from the viewpoint of improving the adhesion between the current collector and the electrode layer. The weight-average molecular weight is a polystyrene-equivalent value determined by gel permeation chromatography (GPC).

[0084] From the viewpoints of reducing costs and obtaining a high energy density, the content of the binder is preferably 0.05 to 8 mass %, more preferably 0.05 to 5 mass %, even more preferably 0.05 to 4 mass %, still more preferably 0.1 to 3 mass %, particularly preferably 0.2 to 2 mass %, and most preferably 0.3 to 1.5 mass %, based on the solid content.

[0085] <Conductive Aid> The electrode-forming composition of the present invention may further contain a conductive aid to improve electrical conductivity. Examples of the conductive aid include carbon materials such as graphite, carbon black, acetylene black (AB), vapor-grown carbon fiber, carbon nanotubes (CNT), carbon nanohorns, and graphene, and conductive polymers such as polyaniline, polypyrrole, polythiophene, polyacetylene, and polyacene. From the viewpoints of conductivity and ease of preparation of the electrode-forming composition, it is preferable that the composition does not contain graphene. It is preferable to use carbon black, acetylene black, vapor-grown carbon fiber, carbon nanotubes, or carbon nanohorns, and it is more preferable to use carbon black, acetylene black, or carbon nanotubes. The conductive aids can be used alone or in combination of two or more. It is most preferable to use carbon black or acetylene black in combination with carbon nanotubes.

[0086] When the conductive additive is contained, its content is not particularly limited, but is preferably 0.05 to 5 mass % of the solid content, more preferably 0.05 to 4 mass %, even more preferably 0.1 to 3 mass %, and even more preferably 0.2 to 2 mass %. By setting the content of the conductive additive within the above range, good electrical conductivity can be obtained.

[0087] <Other Components> The electrode-forming composition of the present invention may further contain other components. For example, a dispersant may be included to improve the dispersibility of the active material and conductive additive. The dispersant can be selected from those conventionally used as dispersants for conductive carbon materials such as CNTs. However, from the viewpoint of stability within the battery, a nonionic polymer is preferred. Examples of the nonionic polymer include polyvinylpyrrolidone (PVP) and polymers having at least one group selected from the group consisting of a nitrile group, a hydroxy group, a carbonyl group, an amino group, a sulfonyl group, and an ether group. Specific examples of the polymer include polyvinyl alcohol, polyacrylonitrile, polylactic acid, polyester, polyimide, polyphenyl ether, polyphenylsulfone, polyethyleneimine, and polyaniline. In the present invention, polymers having a pyrrolidone structure or a nitrile group are preferred, and polyvinylpyrrolidone and polyacrylonitrile are more preferred. The dispersants may be used alone or in combination of two or more. The dispersant may be added simultaneously with an additive or gelation inhibitor comprising a specific heterocycle-containing compound, or the additive or gelation inhibitor comprising a heterocycle-containing compound and the dispersant may be added separately. In addition, the addition of a nonionic polymer is expected to improve the dispersibility of the active material and conductive additive as well as the adhesion to the current collector foil.

[0088] When the dispersant is contained, its content is not particularly limited, but is preferably 0.001 to 0.5 mass% of the solid content, more preferably 0.001 to 0.3 mass%, and even more preferably 0.001 to 0.2 mass%. An even more preferable lower limit of the content of the dispersant is 0.01 mass% of the solid content. Furthermore, in consideration of the adhesion between the resulting electrode layer and the current collector, the total amount of the heterocycle-containing compound and the dispersant is preferably 0.001 to 1 mass%, more preferably 0.01 to 1 mass%, of the solid content.

[0089] <Solvent> The electrode-forming composition of the present invention contains a solvent. The solvent is not particularly limited as long as it is one that has conventionally been used in preparing electrode-forming compositions, and examples thereof include water; ethers such as tetrahydrofuran (THF), diethyl ether, and 1,2-dimethoxyethane (DME); halogenated hydrocarbons such as methylene chloride, chloroform, and 1,2-dichloroethane; amides such as N,N-dimethylformamide (DMF), N,N-dimethylacetamide (DMAc), and N-methyl-2-pyrrolidone (NMP); ketones such as acetone, methyl ethyl ketone, methyl isobutyl ketone, and cyclohexanone; and alcohols such as methanol, ethanol, n-propanol, isopropanol, n-butanol, and t-butanol. Examples of suitable solvents include alcohols, aliphatic hydrocarbons such as n-heptane, n-hexane, and cyclohexane, aromatic hydrocarbons such as benzene, toluene, xylene, and ethylbenzene, glycol ethers such as ethylene glycol monoethyl ether, ethylene glycol monobutyl ether, and propylene glycol monomethyl ether, glycols such as ethylene glycol and propylene glycol, carbonates such as ethylene carbonate, propylene carbonate, dimethyl carbonate, diethyl carbonate, and methyl ethyl carbonate, and organic solvents such as γ-butyrolactone, dimethyl sulfoxide (DMSO), dioxolane, and sulfolane. These solvents may be used alone or in combination of two or more.

[0090] The binder may be used by dissolving or dispersing it in these solvents as needed. Suitable solvents in this case include water, NMP, DMSO, ethylene carbonate, propylene carbonate, dimethyl carbonate, diethyl carbonate, methyl ethyl carbonate, γ-butyrolactone, THF, dioxolane, sulfolane, DMF, DMAc, etc., and may be appropriately selected depending on the type of binder. NMP is suitable for water-insoluble binders such as PVdF, and water is suitable for water-soluble binders.

[0091] The solids concentration of the electrode-forming composition of the present invention is appropriately set taking into consideration the coatability of the composition, the thickness of the electrode to be formed, and the like, but is usually about 60 to 92 mass %, preferably about 65 to 90 mass %, and more preferably about 70 to 85 mass %.

[0092] The viscosity of the electrode-forming composition of the present invention is set appropriately taking into consideration the coating method, the thickness of the electrode to be formed, and the like, but is usually about 100 to 2,000,000 mPa·s, preferably about 300 to 1,000,000 mPa·s, and more preferably about 400 to 800,000 mPa·s. The above viscosity is a value measured at 25°C using an E-type viscometer.

[0093] The electrode-forming composition of the present invention can be obtained by mixing the above-mentioned components. When the composition contains optional components other than the additive (heterocycle-containing compound), the positive electrode active material, and the binder of the present invention, the additive and the positive electrode active material may be mixed together with the optional components, or both components may be mixed in advance and then mixed with the optional components. Either method can achieve the effects of the present invention.

[0094] [Method for producing an electrode-forming composition] Examples of a method for producing an electrode-forming composition include, but are not limited to, a method comprising the steps of: mixing a positive electrode active material, a binder, and a solvent to prepare a dispersion; and mixing the dispersion with a heterocycle-containing compound. In addition, when a conductive additive is used, it is preferable to mix it in the step of preparing the dispersion.

[0095] Here, the heterocycle-containing compound may be mixed alone, or may be mixed as an additive in which the heterocycle-containing compound is combined with at least one selected from the group consisting of a polymer having a pyrrolidone structure or a nitrile group, and a solvent.

[0096] Examples of the polymer having a pyrrolidone structure or a nitrile group include the same polymers as those exemplified in the description of the dispersant, with polyvinylpyrrolidone and polyacrylonitrile being preferred.

[0097] When the heterocycle-containing compound is mixed with a solvent, examples of the solvent that can be used include the same solvents as those exemplified above. Among these, NMP, propylene carbonate, ethylene carbonate, diethyl carbonate, dimethyl carbonate, and ethyl methyl carbonate are particularly suitable for use in the present invention.

[0098] [Electrode] The electrode of the present invention comprises an electrode layer made of the electrode-forming composition described above on at least one surface of a substrate, which is a current collector. Examples of methods for forming the electrode layer on the substrate include a method in which the prepared electrode-forming composition is applied to the substrate to form a coating film, which is then dried. This method is not particularly limited, and various conventionally known methods can be used. Specific examples of coating methods include various printing methods such as offset printing and screen printing, blade coating, dip coating, spin coating, bar coating, slit coating, inkjet printing, and die coating.

[0099] When drying the coating film, either natural drying or heat drying may be used, but heat drying is preferred from the viewpoint of production efficiency. When heat drying is performed, the temperature is preferably about 50 to 400°C, and more preferably about 70 to 150°C.

[0100] Examples of substrates used for the electrodes include metal substrates such as platinum, gold, iron, stainless steel, copper, aluminum, and lithium, alloy substrates made of any combination of these metals, oxide substrates such as indium tin oxide (ITO), indium zinc oxide (IZO), and antimony tin oxide (ATO), and carbon substrates such as glassy carbon, pyrolytic graphite, and carbon felt. In particular, the thickness of the substrate is not particularly limited, but in the present invention, it is preferably 1 to 100 μm, more preferably 3 to 30 μm, and most preferably 5 to 25 μm.

[0101] The thickness of the electrode layer is not particularly limited, but is preferably about 0.01 to 1,000 μm, more preferably about 5 to 300 μm. When the electrode layer is used alone as an electrode, the thickness is preferably 10 μm or more.

[0102] The electrode may be pressed as necessary. A commonly used pressing method can be used, but mold pressing and roll pressing are particularly preferred. The pressing pressure is not particularly limited, but is preferably 1 kN / cm or more, more preferably 2 kN / cm or more, and more preferably 5 kN / cm or more. The upper limit of the pressing pressure is not particularly limited, but is preferably 50 kN / cm or less.

[0103] [Secondary Battery] The secondary battery of the present invention is provided with the above-described electrodes, more specifically, is provided with at least one pair of positive and negative electrodes, a separator interposed between the electrodes, and an electrolyte, and the positive electrode is formed from the above-described electrode. Other constituent members of the battery element may be appropriately selected from conventionally known components.

[0104] Examples of materials used for the separator include glass fiber, cellulose, porous polyolefin, polyamide, and polyester.

[0105] The electrolyte may be either liquid or solid, and may be either aqueous or non-aqueous. However, from the viewpoint of easily achieving practically sufficient performance, an electrolytic solution composed of an electrolyte salt, a solvent, etc. may be preferably used.

[0106] Examples of the electrolyte salt include LiPF, LiBF, and LiN(SOF). 2、 Examples of the electrolyte salt include lithium salts such as LiN(CFSO), LiAsF, LiSbF, LiAlF, LiGaF, LiInF, LiClO, LiN(CFSO), LiCFSO, LiSiF, and LiN(CFSO)(CFSO), metal iodides such as LiI, NaI, KI, CsI, and CaI, iodide salts of quaternary imidazolium compounds, iodide salts and perchlorates of tetraalkylammonium compounds, and metal bromides such as LiBr, NaBr, KBr, CsBr, and CaBr. These electrolyte salts can be used alone or in combination of two or more.

[0107] The solvent is not particularly limited as long as it does not corrode or decompose the materials constituting the battery, thereby deteriorating performance, and dissolves the electrolyte salt. For example, non-aqueous solvents include cyclic esters such as ethylene carbonate, propylene carbonate, butylene carbonate, and γ-butyrolactone; ethers such as tetrahydrofuran and dimethoxyethane; chain esters such as methyl acetate, dimethyl carbonate, diethyl carbonate, and ethyl methyl carbonate; and nitriles such as acetonitrile. These solvents can be used alone or in combination of two or more.

[0108] In addition, as the solid electrolyte, inorganic solid electrolytes such as sulfide-based solid electrolytes and oxide-based solid electrolytes, and organic solid electrolytes such as polymer-based electrolytes can be suitably used. By using these solid electrolytes, an all-solid-state battery can be obtained that does not require an electrolytic solution.

[0109] The sulfide-based solid electrolyte may be a Li2S-SiS2-lithium compound (wherein the lithium compound is Li3PO 4、 At least one selected from the group consisting of LiI and LiSiO 、 Li2S-PO 5、 Li2S-B2S 5、 Examples include thiolithium-based materials such as Li2S-P2S5-GeS2.

[0110] The oxide-based solid electrolyte is Li5La3M2O, an oxide having a garnet structure. 12 (M = Nb, Ta) and Li7La3Zr2O 12 , oxyacid salt compounds based on the γ-Li3PO4 structure, collectively known as LISICON, perovskite-type, Li, 3.3 P.O. 3.8 N 0.22, sodium / alumina, etc. Examples of the polymer solid electrolyte include polyethylene oxide materials and polymer compounds obtained by polymerizing or copolymerizing monomers such as hexafluoropropylene, tetrafluoroethylene, trifluoroethylene, ethylene, propylene, acrylonitrile, vinylidene chloride, acrylic acid, methacrylic acid, methyl acrylate, ethyl acrylate, methyl methacrylate, styrene, and vinylidene fluoride. The polymer solid electrolyte may contain a supporting salt and a plasticizer.

[0111] The supporting salt contained in the polymer solid electrolyte may include lithium (fluorosulfonylimide), and the plasticizer may include succinonitrile.

[0112] A battery manufactured using the electrode-forming composition of the present invention has high battery characteristics even though it contains less fluorine binder than a typical secondary battery.

[0113] The type of secondary battery and the type of electrolyte are not particularly limited, and any type of battery such as a lithium ion secondary battery, a nickel-metal hydride battery, a manganese battery, or an air battery may be used, but a lithium ion secondary battery is preferred. The lamination method and production method are also not particularly limited.

[0114] When applied to a coin cell, the electrode of the present invention described above may be punched into a predetermined disk shape for use. For example, a lithium-ion secondary battery can be produced by placing one electrode on a coin cell lid to which a washer and spacer are welded, placing a separator of the same shape impregnated with an electrolyte solution on top of that, placing the electrode of the present invention on top with the electrode layer facing downwards, placing a case and a gasket on top, and sealing the battery with a coin cell crimping machine.

[0115] [Additive] The present invention also provides an additive for an electrode slurry containing a positive electrode active material, a binder, and a solvent, the additive comprising a heterocycle-containing compound having a nitrogen-containing five-membered ring and not containing an oxygen atom in the nitrogen-containing five-membered ring. The additive can be suitably used as a gelation inhibitor for an electrode slurry containing a positive electrode active material, a binder, and a solvent. Furthermore, the present invention can be suitably applied as a method for suppressing gelation of an electrode slurry by adding the heterocycle-containing compound to the electrode slurry.

[0116] The heterocycle-containing compound is preferably a solid at room temperature, as described above in the description of the electrode-forming composition.

[0117] The heterocycle-containing compound is preferably one in which the nitrogen-containing five-membered ring contains only a nitrogen atom as a heteroatom, and more preferably one in which the nitrogen-containing five-membered ring contains two or three nitrogen atoms.

[0118] The heterocycle-containing compound preferably has a carbonyl structure (carbonyl group) on a nitrogen-containing five-membered ring, and in this case, it is more preferable that the nitrogen-containing five-membered ring is not a condensed ring. Furthermore, it is even more preferable that the carbonyl structure exhibits proton tautomerism, and even more preferably exhibits keto-enol tautomerism.

[0119] Specific examples of the heterocycle-containing compound include additives made of heterocycle-containing compounds represented by any one of the following formulas (1) to (4).

[0120] (In formula (1), R a and R b are each independently a hydrogen atom, a carboxy group, a hydroxy group, a thiol group, an alkyl group having 1 to 6 carbon atoms which may have a substituent, an alkenyl group having 2 to 6 carbon atoms which may have a substituent, or an aryl group having 6 to 12 carbon atoms which may have a substituent, a and R bmay be bonded to each other to form a ring having 4 to 12 carbon atoms which may have a substituent, each L is independently a single bond, a carbonyl group, an ether bond, an ester bond or an amide bond, Z is N or C-L-R c and R c is a hydrogen atom, a halogen atom, a carboxy group, a hydroxy group, a thiol group, an alkyl group having 1 to 6 carbon atoms which may have a substituent, an alkenyl group having 2 to 6 carbon atoms which may have a substituent, or an aryl group having 6 to 12 carbon atoms which may have a substituent, and X a is a hydrogen atom, a lithium atom, a sodium atom, an alkyl group having 1 to 6 carbon atoms which may have a substituent, an aryl group having 6 to 12 carbon atoms which may have a substituent, or —CHNR d 2, and R d are each independently an alkyl group having 1 to 10 carbon atoms, an alkanol group having 1 to 10 carbon atoms, an alkenyl group having 2 to 10 carbon atoms, or an aryl group having 6 to 12 carbon atoms. a and R b are each independently a hydrogen atom, a halogen atom, a carboxy group, a hydroxy group, a thiol group, an alkyl group having 1 to 6 carbon atoms which may have a substituent, an alkenyl group having 2 to 6 carbon atoms which may have a substituent, or an aryl group having 6 to 12 carbon atoms which may have a substituent; each L is independently a single bond, a carbonyl group, an ether bond, an ester bond, or an amide bond; X a is a hydrogen atom, a lithium atom, a sodium atom, an alkyl group having 1 to 6 carbon atoms which may have a substituent, an aryl group having 6 to 12 carbon atoms which may have a substituent, or —CHNR d 2, and R d are each independently an alkyl group having 1 to 10 carbon atoms, an alkanol group having 1 to 10 carbon atoms, an alkenyl group having 2 to 10 carbon atoms, or an aryl group having 6 to 12 carbon atoms. a ~R care each independently a hydrogen atom, a halogen atom, a carboxy group, a hydroxy group, a thiol group, an amino group, an alkyl group having 1 to 6 carbon atoms which may have a substituent, an alkenyl group having 2 to 6 carbon atoms which may have a substituent, or an aryl group having 6 to 12 carbon atoms which may have a substituent, and R a and R b may be bonded to each other to form a ring having 4 to 12 carbon atoms which may have a substituent; each L is independently a single bond, a carbonyl group, an ether bond, an ester bond or an amide bond; X a and X b are each independently a hydrogen atom, a lithium atom, a sodium atom, an alkyl group having 1 to 6 carbon atoms which may have a substituent, an aryl group having 6 to 12 carbon atoms which may have a substituent, or —CHNR d 2, and R d are each independently an alkyl group having 1 to 10 carbon atoms, an alkanol group having 1 to 10 carbon atoms, an alkenyl group having 2 to 10 carbon atoms, or an aryl group having 6 to 12 carbon atoms.

[0121] In the above formulas (1) to (4), R a ~R c , L, X a , X b , R d Specific examples of the above are the same as those given in the description of the electrode-forming composition.

[0122] The additive may further include a non-ionic polymer.

[0123] Examples of the nonionic polymer include the same dispersants as those exemplified in the description of other components of the electrode-forming composition, and polymers having a pyrrolidone structure or a nitrile group are preferred, with polyvinylpyrrolidone and polyacrylonitrile being more preferred.

[0124] When the additive contains the polymer, its content is not particularly limited, but is preferably 0.001 to 0.5 mass % of the solid content, more preferably 0.001 to 0.3 mass %, and even more preferably 0.001 to 0.2 mass %. An even more preferable lower limit of the polymer content is 0.01 mass % of the solid content.

[0125] The additive may further contain a solvent. Examples of the solvent include those exemplified in the description of the electrode-forming composition. In the present invention, NMP, propylene carbonate, ethylene carbonate, diethyl carbonate, dimethyl carbonate, and ethyl methyl carbonate are particularly suitable.

[0126] When the additive contains a solvent, the heterocycle-containing compound represented by any one of the above formulas (1) to (4) is preferably dissolved or dispersed in the solvent, and more preferably dissolved in the solvent.

[0127] When the additive of the present invention contains a solvent, the solid content concentration of the additive is appropriately set taking into consideration the saturated solubility in the solvent, storage stability, etc., but is usually about 1 to 60 mass %, preferably about 3 to 55 mass %, and more preferably about 3 to 50 mass %.

[0128] The positive electrode active material and binder of the electrode slurry are also the same as those described in the explanation of the electrode-forming composition.

[0129] [Gelation Inhibitor] The present invention further provides a gelation inhibitor for electrode slurries containing a positive electrode active material, a binder, and a solvent, the gelation inhibitor comprising a heterocycle-containing compound having a nitrogen-containing five-membered ring and not containing an oxygen atom in the nitrogen-containing five-membered ring. The gelation inhibitor of the present invention can more effectively inhibit gelation of electrode slurries containing a positive electrode active material, a binder, and a solvent.

[0130] The heterocycle-containing compound is different from the solvent in the present invention in that it is a solid at room temperature, as described above in the description of the electrode-forming composition.

[0131] The heterocycle-containing compound is preferably one in which the nitrogen-containing five-membered ring contains only a nitrogen atom as a heteroatom, and more preferably one in which the nitrogen-containing five-membered ring contains two or three nitrogen atoms.

[0132] The heterocycle-containing compound preferably has a carbonyl structure (carbonyl group) on a nitrogen-containing five-membered ring, and in this case, it is more preferable that the nitrogen-containing five-membered ring is not a condensed ring. Furthermore, it is even more preferable that the carbonyl structure exhibits proton tautomerism, and even more preferably exhibits keto-enol tautomerism.

[0133] Specific examples of the heterocycle-containing compound include those represented by any of the following formulas (1) to (4). (In formula (1), R a and R b are each independently a hydrogen atom, a carboxy group, a hydroxy group, a thiol group, an alkyl group having 1 to 6 carbon atoms which may have a substituent, an alkenyl group having 2 to 6 carbon atoms which may have a substituent, or an aryl group having 6 to 12 carbon atoms which may have a substituent, a and R b may be bonded to each other to form a ring having 4 to 12 carbon atoms which may have a substituent, each L is independently a single bond, a carbonyl group, an ether bond, an ester bond or an amide bond, Z is N or C-L-R c and R c is a hydrogen atom, a halogen atom, a carboxy group, a hydroxy group, a thiol group, an alkyl group having 1 to 6 carbon atoms which may have a substituent, an alkenyl group having 2 to 6 carbon atoms which may have a substituent, or an aryl group having 6 to 12 carbon atoms which may have a substituent, and X a is a hydrogen atom, a lithium atom, a sodium atom, an alkyl group having 1 to 6 carbon atoms which may have a substituent, an aryl group having 6 to 12 carbon atoms which may have a substituent, or —CHNR d 2, and R dare each independently an alkyl group having 1 to 10 carbon atoms, an alkanol group having 1 to 10 carbon atoms, an alkenyl group having 2 to 10 carbon atoms, or an aryl group having 6 to 12 carbon atoms. a and R b are each independently a hydrogen atom, a halogen atom, a carboxy group, a hydroxy group, a thiol group, an alkyl group having 1 to 6 carbon atoms which may have a substituent, an alkenyl group having 2 to 6 carbon atoms which may have a substituent, or an aryl group having 6 to 12 carbon atoms which may have a substituent; each L is independently a single bond, a carbonyl group, an ether bond, an ester bond, or an amide bond; X a is a hydrogen atom, a lithium atom, a sodium atom, an alkyl group having 1 to 6 carbon atoms which may have a substituent, an aryl group having 6 to 12 carbon atoms which may have a substituent, or —CHNR d 2, and R d are each independently an alkyl group having 1 to 10 carbon atoms, an alkanol group having 1 to 10 carbon atoms, an alkenyl group having 2 to 10 carbon atoms, or an aryl group having 6 to 12 carbon atoms. a ~R c are each independently a hydrogen atom, a halogen atom, a carboxy group, a hydroxy group, a thiol group, an amino group, an alkyl group having 1 to 6 carbon atoms which may have a substituent, an alkenyl group having 2 to 6 carbon atoms which may have a substituent, or an aryl group having 6 to 12 carbon atoms which may have a substituent, and R a and R b may be bonded to each other to form a ring having 4 to 12 carbon atoms which may have a substituent; each L is independently a single bond, a carbonyl group, an ether bond, an ester bond or an amide bond; X a and X b are each independently a hydrogen atom, a lithium atom, a sodium atom, an alkyl group having 1 to 6 carbon atoms which may have a substituent, an aryl group having 6 to 12 carbon atoms which may have a substituent, or —CHNR d 2, and R dare each independently an alkyl group having 1 to 10 carbon atoms, an alkanol group having 1 to 10 carbon atoms, an alkenyl group having 2 to 10 carbon atoms, or an aryl group having 6 to 12 carbon atoms.

[0134] In the above formulas (1) to (4), R a ~R c , L, X a , X b , R d Specific examples of the above are the same as those given in the description of the electrode-forming composition.

[0135] The gelation inhibitor may further contain a nonionic polymer.

[0136] Examples of the nonionic polymer include the same dispersants as those exemplified in the description of other components of the electrode-forming composition, and polymers having a pyrrolidone structure or a nitrile group are preferred, with polyvinylpyrrolidone and polyacrylonitrile being more preferred.

[0137] When the gelation inhibitor contains the polymer, its content is not particularly limited, but is preferably 0.001 to 0.5 mass %, more preferably 0.001 to 0.3 mass %, and even more preferably 0.001 to 0.2 mass % of the solid content. An even more preferable lower limit of the polymer content is 0.01 mass % of the solid content.

[0138] The gelation inhibitor may further contain a solvent. Examples of the solvent include those exemplified in the description of the electrode-forming composition. In the present invention, NMP, propylene carbonate, ethylene carbonate, diethyl carbonate, dimethyl carbonate, and ethyl methyl carbonate are particularly suitable.

[0139] When the gelation inhibitor contains a solvent, the heterocycle-containing compound represented by any one of the above formulas (1) to (4) is preferably dissolved or dispersed in the solvent, and more preferably dissolved in the solvent.

[0140] When the gelation inhibitor of the present invention contains a solvent, the solids concentration of the gelation inhibitor is appropriately set taking into consideration the saturated solubility in the solvent, storage stability, etc., but is usually about 1 to 60 mass %, preferably about 3 to 55 mass %, and more preferably about 3 to 50 mass %.

[0141] The positive electrode active material and binder of the electrode slurry are also the same as those described in the explanation of the electrode-forming composition.

[0142] The present invention will be described in more detail below with reference to examples and comparative examples, but the present invention is not limited to the following examples. The apparatus used is as follows.

[0143] (1) Rotation / revolution type mixer: Thinky Corporation, Awatori Rentaro, atmospheric pressure type, ARE-310 (2) Dry mixer: Nippon Spindle Mfg. Co., Ltd. (3) E-type viscometer: Toki Sangyo Co., Ltd., VISCOMETER TV-22, measurement temperature: 25°C, rotor: 1°34' x R24. The viscosity was measured 5 minutes after the start of measurement under the following measurement conditions. The rotor rotation speed was selected from 0.1 to 10 rpm, and an appropriate value was selected for the viscosity of the sample to be measured. The viscosity on the day of slurry preparation was measured within 0.5 to 6 hours after preparation. (4) Liquid Chromatography-Mass Spectrometry (LC / MS) Liquid Chromatography Apparatus: NexeraX2 (Shimadzu), manufactured by Shimadzu Corporation; Mass Spectrometer (MS): Q-Exactive, manufactured by Thermo Fisher Scientific; Column: XBridge C18 2.1 x 150 mm (5 μm); Eluent: Acetonitrile with formic acid added at a concentration of 0.1% (vol / vol) / Pure water with formic acid added at a concentration of 0.1% (vol / vol) = 20 / 80 - 95 / 5 (12 min) - 95 / 5 (13 min); Ionization Method: ESI+

[0144] The raw materials used are as follows: <Active material> NCA: Lithium nickel oxide (LiNi 0.88 Co 0.11 Al 0.01O2, NCA-034H, Ni content: 55% by mass, Ecopro NCM811: lithium nickel manganese cobalt oxide (LiNi 0.8 Co 0.1 Mn 0.1O2, Ningbo Ronbay New Energy Technology Co. , Ltd. S-800, Ni content: 50% by mass) <Binder> Solef-5130: polyvinylidene fluoride (PVdF), manufactured by SOLVAY Solef-5140: polyvinylidene fluoride (PVdF), manufactured by SOLVAY <Conductive additive> AB: Denka Black (registered trademark) Li100 (high-purity acetylene black), manufactured by Denka Company, Limited <Solvent> NMP: manufactured by Nippon Refine Co., Ltd. Tetrahydrofuran: manufactured by Asahi Rika Seisakusho Co., Ltd. 2-Propanol: manufactured by Junsei Chemical Co., Ltd. Hexane: manufactured by Junsei Chemical Co., Ltd. <Additive A> [Additives used in the examples] A1: 1H-1,2,3-Benzotriazole-5-carboxylic acid monohydrate (CBT-1), manufactured by Johoku Chemical Industry Co., Ltd. (corresponding to the monohydrate of formula (1-1)) A2: 1H-Benzotriazole, manufactured by Fujifilm Wako Pure Chemical Industries, Ltd. (corresponding to formula (1-2)) A3: 1H-1,2,3-Triazole, manufactured by Fujifilm Wako Pure Chemical Industries, Ltd. (corresponding to formula (1-3)) A4: 1H-1,2,4-Triazole, manufactured by Tokyo Chemical Industry Co., Ltd. (corresponding to formula (2-1)) A5: 2,A6: 3-Dimethyl-1-phenyl-5-pyrazolone, manufactured by Tokyo Chemical Industry Co., Ltd. (corresponding to formula (3-1)) A7: Benzimidazole, manufactured by Tokyo Chemical Industry Co., Ltd. (corresponding to formula (1-4)) A8: 5-Benzimidazolecarboxylic acid, manufactured by Tokyo Chemical Industry Co., Ltd. (corresponding to formula (1-5)) A9: X-12-1214A, manufactured by Shin-Etsu Chemical Co., Ltd. (corresponding to formula (1-6)) A10: CBT-1 neutralized with 99 mol% LiOH (synthetic product) (corresponding to the monohydrate of formula (1-15)) A11: 3-Methyl-1-p-tolyl-5-pyrazolone, manufactured by Tokyo Chemical Industry Co., Ltd. (Corresponding to formula (3-9)) A12: 1-(4-Chlorophenyl)-3-methyl-5-pyrazolone, manufactured by Tokyo Chemical Industry Co., Ltd. (Corresponding to formula (3-13)) A13: 3-Amino-1-phenyl-2-pyrazolin-5-one, manufactured by Tokyo Chemical Industry Co., Ltd. (Corresponding to formula (4-10)) A14: 3-Methyl-1-phenyl-5-pyrazolone Li salt (synthetic product) (Corresponding to formula (3-5)) A15: Hydantoin, manufactured by Tokyo Chemical Industry Co., Ltd. A16: 5,5-Dimethylhydantoin, manufactured by Tokyo Chemical Industry Co., Ltd. A17: 1,2-Benzisothiazol-3(2H)-one, manufactured by Tokyo Chemical Industry Co., Ltd. A18: 2-Mercaptobenzimidazole, manufactured by Tokyo Chemical Industry Co., Ltd. A19: 5-Mercapto-1-methyltetrazole, manufactured by Tokyo Chemical Industry Co., Ltd. A20: 7-Hydroxy-5-methyl-[1,2,4]triazolo[1,5-a]pyrimidine, manufactured by Tokyo Chemical Industry Co., Ltd. A21: Bis(3-methyl-1-phenyl-5-pyrazolone), manufactured by Tokyo Chemical Industry Co., Ltd. [Additives used in Comparative Examples] a1: 2-(2-Hydroxyphenyl)pyridine, manufactured by Fujifilm Wako Pure Chemical Industries Co., Ltd. a2: 1,10-Phenanthroline, manufactured by Tokyo Chemical Industry Co., Ltd. a3: 1,a4: 8-Naphthyridine, manufactured by Tokyo Chemical Industry Co., Ltd. a5: Pyridine, manufactured by Fujifilm Wako Pure Chemical Industries, Ltd. a6: Poly(4-vinylpyridine), manufactured by Sigma-Aldrich a7: WS-700 (oxazoline group-containing polymer), manufactured by Nippon Shokubai Co., Ltd., Mw: 40,000, reactive crosslinker a8: 2-(1,3-Phenylene)bis-2-oxazoline (PBO), manufactured by Fujifilm Wako Pure Chemical Industries, Ltd., reactive crosslinker a9: Polyacrylic acid, Toagosei Co., Ltd., Aron AC-10P, Mw: 5,000 a10: Oxalic acid, manufactured by Fujifilm Wako Pure Chemical Industries, Ltd. a11: Phenylboronic acid, Cangzhou Pure Chemical Industries, Ltd. a12: Benzoic acid, manufactured by Fujifilm Wako Pure Chemical Industries, Ltd. a13: Tannic acid, manufactured by Fujifilm Wako Pure Chemical Industries, Ltd. a14: Water-soluble methylolmelamine (Nikaresin S176 (triazine structure)), manufactured by Nippon Carbide Industries Co., Ltd. a15: Isobam18 (copolymer of isobutylene and maleic anhydride), manufactured by Kuraray Co., Ltd., Mw: 300,000 to 350,000 a16: Anthranil, manufactured by Tokyo Chemical Industry Co., Ltd. <Other additives> PVP: Pitzcol K90, manufactured by Daiichi Kogyo Seiyaku Co., Ltd., Mw: 1.2 million, dispersant PAN: H-PAN, manufactured by Dolan GmbH, Mw: 200,000, dispersant

[0145] Synthesis Example 1 Synthesis of Additive A10 (CBT-1 Neutralized with 99 mol% LiOH) A solution of 4.43 g of 1H-1,2,3-Benzotriazole-5-carboxylic acid (CBT-1) dissolved in 22.72 g of NMP and a solution of 111 g of NMP and 0.58 g of LiOH (manufactured by Tokyo Chemical Industry Co., Ltd.) dissolved in 23.69 g of pure water were mixed, stirred and mixed for 1 hour, and then allowed to stand for 24 hours for neutralization. Using a vacuum distillation apparatus and an oil bath, this was subjected to vacuum distillation at 85°C / 20 Torr for 0.5 hour and then at 110-120°C / 50-20 Torr for 1 hour to obtain a 5 mass % NMP solution of a LiOH-neutralized product of CBT-1.

[0146] Synthesis Example 2 Synthesis of Additive A14 (Li Salt of 3-Methyl-1-phenyl-5-pyrazolone) 1.76 g of 3-Methyl-1-phenyl-5-pyrazolone was dissolved in 60.14 g of tetrahydrofuran, and 6.25 mL of BuLi in hexane (ca. 15% in hexane, ca. 1.6 mol / L) (Tokyo Chemical Industry Co., Ltd.) was added to the solution and stirred at room temperature for 1 hour. 5 g of 2-propanol was added to the solution and stirred for 1 hour. The solution was poured into 240 g of hexane to cause reprecipitation, and the resulting precipitate was collected using a Kiriyama funnel. This was then vacuum dried at 80°C for 3 hours to obtain the Li salt of 3-Methyl-1-phenyl-5-pyrazolone.

[0147] The amount of heterocycle-containing compound (additive or gelation inhibitor) attached to the active material can be confirmed, for example, by dissolving each compound in a solvent, dispersing the active material in the resulting solution, filtering the solution, quantifying the compound concentration in the filtrate, and confirming the concentration decrease from the initial concentration. The concentration of the heterocycle-containing compound in the filtrate can be determined by any of the common quantitative analysis methods, such as liquid chromatography-mass spectrometry (LC / MS) or NMR. The adsorption rate (%) can also be calculated using the following formula: Adhesion rate (%) = (charged concentration of each compound - concentration of each compound in the filtrate) / charged concentration of each compound.

[0148] The positive electrode active material, additive (gelling inhibitor), and NMP were mixed in a dry mixer to the composition ratio shown in Table 1, and the mixture was mixed for 1 hour using a mixer rotor. The mixture was filtered through a 0.2 μm filter to remove the active material, and the filtrate was collected. The resulting filtrate was diluted with methanol as needed. Evaluation Example 1 was diluted 1,100 times, Examples 2 and 3 were diluted 110 times, and Example 4 was diluted 11 times. Examples 5 and 6 were not diluted. Extracted ion chromatograms were plotted for each of these samples using LC / MS measurement. The additive concentrations were quantified from the peak areas on the resulting chromatograms and a previously prepared calibration curve, and the adsorption rates of each additive were calculated.

[0149]

[0150] Preparation of Positive Electrode Composition (Electrode Slurry) [Examples 1-1 to 1-35, Comparative Examples 1-1 to 1-19] A 5% by mass NMP solution was prepared for each additive. A 7% by mass NMP solution of PVdF was prepared. The positive electrode active material, binder solution, conductive additive, additive A solution, additive B solution, NMP, and water were mixed in a dry mixer to obtain the composition ratios shown in Tables 2, 3, and 5, and then mixed using a rotation-revolution mixer to obtain electrode slurries. The total amount of each slurry prepared was 20 g, the solids content was 71% by mass, and the solvent composition of the slurry was adjusted to NMP / HO = 97 / 3 (mass ratio). Note that the water was added to intentionally create a high moisture content in the slurry. The preparation method is described in more detail below. A 5% by mass NMP solution was prepared for each additive. A 7% by mass NMP solution of PVdF was prepared. The conductive additive and binder solution were weighed in a dry mixer to achieve the composition ratios shown in Tables 2, 3, and 5, and mixed for 5 minutes at 2,000 rpm using a rotation / revolution mixer. Half of the positive electrode active material was added to the mixture, and the mixture was mixed for 5 minutes at 2,000 rpm. The remaining half of the positive electrode active material was added to the mixture, and the mixture was mixed for 5 minutes at 2,000 rpm. The additive A solution, additive B solution, NMP, and water were added, and the mixture was mixed for 5 minutes at 2,000 rpm. The mixture was stirred with a spatula and mixed for 5 minutes at 2,000 rpm to obtain electrode slurries. The total amount of each slurry prepared was 20 g, with a solids content of 71% by mass. The solvent composition of the slurry was adjusted to NMP / HO = 97 / 3 (by mass). The water was added to intentionally create a high moisture content in the slurry.

[0151] Examples 1-36 to 1-41: An NMP solution containing 7% by mass of PVdF was prepared. The positive electrode active material, binder solution, conductive additive, additive A, NMP, and water were mixed in a dry oven to obtain the composition shown in Table 4, and then mixed using a rotation / revolution mixer to obtain an electrode slurry. The total amount of each slurry prepared was 20 g, the solids content was 71% by mass, and the solvent composition of the slurry was adjusted to NMP / HO = 97 / 3 (mass ratio). Note that the water was added to intentionally create a high water content in the slurry. The preparation method is described in more detail below. An NMP solution containing 7% by mass of PVdF was prepared. The conductive additive and binder solution were weighed in a dry oven to obtain the composition shown in Table 4, and then mixed for 5 minutes using a rotation / revolution mixer at 2,000 rpm. To this, half of the positive electrode active material was added, and the mixture was mixed at 2,000 rpm for 5 minutes. The remaining half of the positive electrode active material was added, and the mixture was mixed at 2,000 rpm for 5 minutes. Additive A, NMP, and water were added, and the mixture was mixed at 2,000 rpm for 5 minutes. The whole was stirred using a spatula, and the mixture was mixed at 2,000 rpm for 5 minutes to obtain an electrode slurry. The total amount of the prepared slurries was 20 g each, the solid content was 71 mass%, and the solvent composition of the slurry was adjusted to NMP / HO = 97 / 3 (mass ratio). Note that the water was added to intentionally create a high moisture content in the slurry.

[0152] [Examples 1-42, Comparative Examples 1-20] An NMP solution containing 7% by mass of PVdF was prepared. The positive electrode active material, binder solution, additive A, NMP, and water were mixed in a dry oven to obtain the composition ratios shown in Tables 4 and 5, and then mixed using a rotation / revolution mixer to obtain an electrode slurry. The total amount of each slurry prepared was 19.76 g, the solids content was 79.76% by mass, and the solvent composition of the slurry was adjusted to NMP / HO = 97 / 3 (mass ratio). Note that the water was added to intentionally create a high water content in the slurry. The preparation method is described in more detail below. An NMP solution containing 7% by mass of PVdF was prepared. The binder solution and additive A solution were weighed in a dry oven to obtain the composition ratios shown in Tables 4 and 5, and then mixed for 5 minutes using a rotation / revolution mixer at 2,000 rpm. To this, half of the positive electrode active material was added and mixed at 2,000 rpm for 5 minutes. The remaining half of the positive electrode active material was added to this and mixed at 2,000 rpm for 5 minutes. The conductive additive, NMP, and water were added to this and mixed at 2,000 rpm for 5 minutes. The entire mixture was stirred using a spatula and mixed at 2,000 rpm for 5 minutes to obtain electrode slurries. The total amount of the prepared slurries was 19.76 g, the solid content was 79.76 mass%, and the solvent composition of the slurries was adjusted to NMP / HO = 97 / 3 (mass ratio). Note that the water was added to intentionally create a high moisture content in the slurry.

[0153] [Examples 1-43 to 1-49, Comparative Example 1-21] A 5% by mass NMP solution was prepared for each additive. A 7% by mass NMP solution of PVdF was prepared. The positive electrode active material, binder solution, conductive additive, additive A solution, NMP, and water were mixed in a dry mixer to obtain the composition ratios shown in Tables 4 and 5, and then mixed using a rotation / revolution mixer to obtain electrode slurries. The total amount of each slurry prepared was 20 g, the solids content was 80% by mass, and the solvent composition of the slurry was adjusted to NMP / HO = 97 / 3 (mass ratio). Note that the water was added to intentionally create a high moisture content in the slurry. The preparation methods are described in more detail below. A 5% by mass NMP solution was prepared for each additive. A 7% by mass NMP solution of PVdF was prepared. The binder solution and additive A solution were weighed in a dry mixer to achieve the composition ratios shown in Tables 4 and 5, and mixed for 5 minutes at 2,000 rpm using a rotation / revolution mixer. Half of the positive electrode active material was added to the mixture, and the mixture was mixed for 5 minutes at 2,000 rpm. The remaining half of the positive electrode active material was added to the mixture, and the mixture was mixed for 5 minutes at 2,000 rpm. The conductive additive, NMP, and water were added to the mixture, and the mixture was mixed for 5 minutes at 2,000 rpm. The mixture was stirred with a spatula and mixed for 5 minutes at 2,000 rpm to obtain electrode slurries. The total amount of each slurry prepared was 20 g, the solids content was 80% by mass, and the solvent composition of the slurry was adjusted to NMP / HO = 97 / 3 (mass ratio). The water was added to intentionally create a high moisture content in the slurry.

[0154] The viscosity of the slurry obtained above was measured using an E-type viscometer immediately after preparation. Furthermore, after storing for 24 hours at 40°C, the presence or absence of gelation was confirmed visually. For those that had not gelled, the viscosity was similarly measured using an E-type viscometer to check for thickening and a tendency to gel, and the results were judged based on the following criteria. These evaluations are also summarized in each table. <Judgment criteria> A: No gelation, viscosity change rate less than 200% B: No gelation, but viscosity change rate of 200% or more, with significant thickening C: The composition gelled and could not be used to form electrodes Viscosity change rate (%) = ((viscosity after storage - initial viscosity) / initial viscosity) x 100

[0155]

[0156]

[0157]

[0158]

[0159] The results in Tables 2 to 5 confirm that the electrode-forming composition of the present invention, to which a specific heterocycle-containing compound was added, suppressed thickening and gelation and improved storage stability. Therefore, the electrode-forming composition does not lose its coatability even after a long time has passed since its preparation, and can be suitably used in the industrial production of lithium-ion secondary batteries.

[0160] Examples 1-50 to 1-53: An NMP solution containing 7% by mass of PVdF was prepared. The positive electrode active material, binder solution, conductive additive, additive A, additive B, NMP, and water were mixed in a dry oven to obtain the composition shown in Table 6, and then mixed using a rotation / revolution mixer to obtain an electrode slurry. The total amount of each slurry prepared was 20 g, the solids content was 71% by mass, and the solvent composition of the slurry was adjusted to NMP / HO = 97 / 3 (mass ratio). Note that the water was added to intentionally create a high water content in the slurry. The preparation method is described in more detail below. An NMP solution containing 7% by mass of PVdF was prepared. The conductive additive and binder solution were weighed in a dry oven to obtain the composition shown in Table 6, and then mixed for 5 minutes using a rotation / revolution mixer at 2,000 rpm. To this, half of the positive electrode active material was added and mixed at 2,000 rpm for 5 minutes. The remaining half of the positive electrode active material was added to this, and mixed at 2,000 rpm for 5 minutes. A 5% by mass NMP solution containing additives A and B, NMP, and water were added, and mixed at 2,000 rpm for 5 minutes. The entire mixture was stirred using a spatula and mixed at 2,000 rpm for 5 minutes to obtain an electrode slurry. The total amount of the prepared slurries was 20 g each, the solid content was 71% by mass, and the solvent composition of the slurry was adjusted to NMP / HO = 97 / 3 (mass ratio). Note that the water was added to intentionally create a high moisture content in the slurry.

[0161] The slurries obtained above were subjected to viscosity measurement using an E-type viscometer immediately after preparation in the same manner as in Example 1-1. Furthermore, after storage at 40°C for 24 hours, the presence or absence of gelation was confirmed visually. For those that did not gel, viscosity was similarly measured using an E-type viscometer to confirm the presence or absence of a tendency for thickening and gelation. The evaluation criteria and the method for calculating the viscosity change rate were the same as above. These evaluations are also summarized in Table 6.

[0162]

[0163] The results in Table 6 above confirm that the electrode-forming composition of the present invention, to which the specific heterocycle-containing compound was added, suppressed thickening and gelation and improved storage stability. Therefore, the electrode-forming composition does not lose its coatability even after a long time has passed since its preparation, and can be suitably used in the industrial production of lithium-ion secondary batteries.

Claims

1. An electrode-forming composition comprising a positive electrode active material, a binder, a solvent, and a heterocycle-containing compound, wherein the heterocycle-containing compound has a nitrogen-containing five-membered ring, does not contain an oxygen atom in the five-membered ring, and has a carbonyl structure on the five-membered ring.

2. The electrode-forming composition according to claim 1, wherein said heterocycle-containing compound is attached to said positive electrode active material.

3. The electrode-forming composition according to claim 1, wherein said heterocycle-containing compound is a non-condensed nitrogen-containing five-membered heterocycle.

4. The electrode-forming composition according to claim 1, wherein said carbonyl structure exhibits proton tautomerism.

5. The electrode-forming composition according to claim 4, wherein the proton tautomerism is keto-enol tautomerism.

6. The electrode-forming composition according to claim 1, wherein the heterocycle-containing compound is represented by any one of the following formulas (3) to (4): (In formulas (3) to (4), R a ~R c are each independently a hydrogen atom, a halogen atom, a carboxy group, a hydroxy group, a thiol group, an amino group, an alkyl group having 1 to 6 carbon atoms which may have a substituent, an alkenyl group having 2 to 6 carbon atoms which may have a substituent, or an aryl group having 6 to 12 carbon atoms which may have a substituent, and R a and R b may be bonded to each other to form a ring having 4 to 12 carbon atoms which may have a substituent; each L is independently a single bond, a carbonyl group, an ether bond, an ester bond or an amide bond; X a and X b are each independently a hydrogen atom, a lithium atom, a sodium atom, an alkyl group having 1 to 6 carbon atoms which may have a substituent, an aryl group having 6 to 12 carbon atoms which may have a substituent, or —CHNR d 2, and R d are each independently an alkyl group having 1 to 10 carbon atoms, an alkanol group having 1 to 10 carbon atoms, an alkenyl group having 2 to 10 carbon atoms, or an aryl group having 6 to 12 carbon atoms.

7. The above R a ~R c , X a and X b 2. The electrode-forming composition according to claim 1, wherein the substituent of is at least one selected from the group consisting of a carboxy group, a hydroxy group, an aldehyde group, an ester group, a ketone group, an amino group, a phenyl group, a halogen atom, an alkoxysilyl group, an epoxy group, a carboxylic acid chloride group, and a thiol group.

8. The electrode-forming composition according to claim 6, wherein the heterocycle-containing compound is represented by the following formula (4b): (In the formula, R a ~R c is the same as above, and R e is a hydrogen atom, a carboxy group, a hydroxy group, an aldehyde group, an ester group, a ketone group, an amino group, a phenyl group, a halogen atom, an alkoxysilyl group, an epoxy group, a carboxylic acid chloride group, or a thiol group.

9. The electrode-forming composition according to claim 1, wherein said heterocycle-containing compound is solid at room temperature.

10. The electrode-forming composition according to claim 1, further comprising a conductive additive.

11. The electrode-forming composition according to claim 1, wherein the positive electrode active material contains 30% by mass or more of Ni.

12. The electrode-forming composition according to claim 1, wherein the positive electrode active material contains 40 mass % or more of Ni.

13. The electrode-forming composition according to claim 1, wherein the positive electrode active material contains 50 mass % or more of Ni.

14. The electrode-forming composition according to claim 1, further comprising a nonionic polymer.

15. The electrode-forming composition according to claim 14, wherein the nonionic polymer is a polymer having a pyrrolidone structure or a nitrile group.

16. The electrode-forming composition according to claim 15, wherein said nonionic polymer is at least one selected from the group consisting of polyvinylpyrrolidone and polyacrylonitrile.

17. The electrode-forming composition according to claim 1, wherein the content of the heterocycle-containing compound is 0.001 to 0.5% by mass based on the solid content.

18. An electrode-forming composition comprising a positive electrode active material, a binder, a solvent, and a heterocycle-containing compound, wherein the heterocycle-containing compound is represented by any one of the following formulas (1) and (2): (In formula (1), R a and R b are each independently a hydrogen atom, a carboxy group, a hydroxy group, a thiol group, an alkyl group having 1 to 6 carbon atoms which may have a substituent, an alkenyl group having 2 to 6 carbon atoms which may have a substituent, or an aryl group having 6 to 12 carbon atoms which may have a substituent, a and R b may be bonded to each other to form a ring having 4 to 12 carbon atoms which may have a substituent, each L is independently a single bond, a carbonyl group, an ether bond, an ester bond or an amide bond, Z is N or C-L-R c and R c is a hydrogen atom, a halogen atom, a carboxy group, a hydroxy group, a thiol group, an alkyl group having 1 to 6 carbon atoms which may have a substituent, an alkenyl group having 2 to 6 carbon atoms which may have a substituent, or an aryl group having 6 to 12 carbon atoms which may have a substituent, and X a is a hydrogen atom, a lithium atom, a sodium atom, an alkyl group having 1 to 6 carbon atoms which may have a substituent, an aryl group having 6 to 12 carbon atoms which may have a substituent, or —CHNR d 2, and R d are each independently an alkyl group having 1 to 10 carbon atoms, an alkanol group having 1 to 10 carbon atoms, an alkenyl group having 2 to 10 carbon atoms, or an aryl group having 6 to 12 carbon atoms. a and R b are each independently a hydrogen atom, a halogen atom, a carboxy group, a hydroxy group, a thiol group, an alkyl group having 1 to 6 carbon atoms which may have a substituent, an alkenyl group having 2 to 6 carbon atoms which may have a substituent, or an aryl group having 6 to 12 carbon atoms which may have a substituent; each L is independently a single bond, a carbonyl group, an ether bond, an ester bond, or an amide bond; X a is a hydrogen atom, a lithium atom, a sodium atom, an alkyl group having 1 to 6 carbon atoms which may have a substituent, an aryl group having 6 to 12 carbon atoms which may have a substituent, or —CHNR d 2, and R d are each independently an alkyl group having 1 to 10 carbon atoms, an alkanol group having 1 to 10 carbon atoms, an alkenyl group having 2 to 10 carbon atoms, or an aryl group having 6 to 12 carbon atoms.

19. The electrode-forming composition according to claim 18, wherein the heterocycle-containing compound is attached to the positive electrode active material.

20. The above R a ~R c , X a and X b The electrode-forming composition according to claim 18, wherein the substituent of is at least one selected from the group consisting of a carboxy group, a hydroxy group, an aldehyde group, an ester group, a ketone group, a phenyl group, a halogen atom, an alkoxysilyl group, an epoxy group, a carboxylic acid chloride group, and a thiol group.

21. The electrode-forming composition according to claim 18, wherein the heterocycle-containing compound is a heterocycle-containing compound represented by the following formula (5): (In the formula, Ar 1 Z, X are an aromatic ring having 4 to 12 carbon atoms which may have a substituent, or an aliphatic ring having 4 to 10 carbon atoms which may have a substituent. a is the same as above.) 22. The electrode-forming composition according to claim 21, wherein the heterocycle-containing compound is a heterocycle-containing compound represented by any one of the following formulas (6) to (7): (Wherein Z and X a is the same as above.) 23. The electrode-forming composition according to claim 18, wherein Z is N.

24. The electrode-forming composition according to claim 18, further comprising a conductive additive.

25. The electrode-forming composition according to claim 18, wherein the positive electrode active material contains 30% by mass or more of Ni.

26. The electrode-forming composition according to claim 18, wherein the positive electrode active material contains 40% by mass or more of Ni.

27. The electrode-forming composition according to claim 18, wherein the positive electrode active material contains 50% by mass or more of Ni.

28. The electrode-forming composition according to claim 18, further comprising a nonionic polymer.

29. The electrode-forming composition according to claim 28, wherein the nonionic polymer is a polymer having a pyrrolidone structure or a nitrile group.

30. The electrode-forming composition according to claim 29, wherein said nonionic polymer is at least one selected from the group consisting of polyvinylpyrrolidone and polyacrylonitrile.

31. The electrode-forming composition according to claim 18, wherein the content of the heterocycle-containing compound is 0.001 to 0.5% by mass based on the solid content.

32. An electrode layer obtained from the electrode-forming composition according to any one of claims 1 to 31.

33. An electrode comprising the electrode layer of claim 32.

34. A secondary battery comprising the electrode according to claim 33.

35. A method for producing an electrode-forming composition according to claim 1, comprising the steps of: mixing a positive electrode active material, a binder, and a solvent to prepare a dispersion; and mixing the dispersion with a heterocycle-containing compound.

36. The method for producing an electrode-forming composition according to claim 35, wherein a conductive additive is further mixed in the step of preparing the dispersion.

37. A method for producing an electrode-forming composition according to claim 18, comprising the steps of: mixing a positive electrode active material, a binder, and a solvent to prepare a dispersion; and mixing the dispersion with a heterocycle-containing compound.

38. The method for producing an electrode-forming composition according to claim 37, wherein a conductive additive is further mixed in the step of preparing the dispersion.

39. An additive for an electrode slurry containing a positive electrode active material, a binder, and a solvent, the additive comprising a heterocycle-containing compound having a nitrogen-containing five-membered ring, containing no oxygen atoms in the five-membered ring, and having a carbonyl structure on the five-membered ring.

40. The additive according to claim 39, wherein said heterocycle-containing compound is a non-fused nitrogen-containing five-membered heterocycle.

41. The additive according to claim 39, wherein the carbonyl structure exhibits proton tautomerism.

42. The additive of claim 41, wherein the proton tautomerism is keto-enol tautomerism.

43. The additive according to claim 39, wherein the heterocycle-containing compound is represented by any one of the following formulas (3) to (4): (In the formula, R a ~R c are each independently a hydrogen atom, a halogen atom, a carboxy group, a hydroxy group, a thiol group, an amino group, an alkyl group having 1 to 6 carbon atoms which may have a substituent, an alkenyl group having 2 to 6 carbon atoms which may have a substituent, or an aryl group having 6 to 12 carbon atoms which may have a substituent, and R a and R b may be bonded to each other to form a ring having 4 to 12 carbon atoms which may have a substituent; each L is independently a single bond, a carbonyl group, an ether bond, an ester bond or an amide bond; X a and X b are each independently a hydrogen atom, a lithium atom, a sodium atom, an alkyl group having 1 to 6 carbon atoms which may have a substituent, an aryl group having 6 to 12 carbon atoms which may have a substituent, or —CHNR d 2, and R d are each independently an alkyl group having 1 to 10 carbon atoms, an alkanol group having 1 to 10 carbon atoms, an alkenyl group having 2 to 10 carbon atoms, or an aryl group having 6 to 12 carbon atoms.

44. Above R a ~R c , X a and X b The additive according to claim 43, wherein the substituent on said compound is at least one selected from the group consisting of a carboxy group, a hydroxy group, an aldehyde group, an ester group, a ketone group, an amino group, a phenyl group, a halogen atom, an alkoxysilyl group, an epoxy group, a carboxylic acid chloride group, and a thiol group.

45. The additive according to claim 43, wherein the heterocycle-containing compound is represented by the following formula (4b): (In the formula, R a ~R c is the same as above, and R e is a hydrogen atom, a carboxy group, a hydroxy group, an aldehyde group, an ester group, a ketone group, an amino group, a phenyl group, a halogen atom, an alkoxysilyl group, an epoxy group, a carboxylic acid chloride group, or a thiol group.

46. ​​The additive according to claim 39, wherein said heterocycle-containing compound is solid at room temperature.

47. The additive according to claim 39, wherein the positive electrode active material contains 30% by mass or more of Ni.

48. The additive of claim 39, further comprising a nonionic polymer.

49. The additive according to claim 48, wherein the nonionic polymer is a polymer having a pyrrolidone structure or a nitrile group.

50. The additive according to claim 49, wherein said nonionic polymer is at least one selected from the group consisting of polyvinylpyrrolidone and polyacrylonitrile.

51. The additive of claim 39, further comprising a solvent.

52. An additive for an electrode slurry containing a positive electrode active material, a binder, and a solvent, the additive containing a heterocycle-containing compound represented by any one of the following formulas (1) and (2): (In formula (1), R a and R b are each independently a hydrogen atom, a carboxy group, a hydroxy group, a thiol group, an alkyl group having 1 to 6 carbon atoms which may have a substituent, an alkenyl group having 2 to 6 carbon atoms which may have a substituent, or an aryl group having 6 to 12 carbon atoms which may have a substituent, a and R b may be bonded to each other to form a ring having 4 to 12 carbon atoms which may have a substituent, each L is independently a single bond, a carbonyl group, an ether bond, an ester bond or an amide bond, Z is N or C-L-R c and R c is a hydrogen atom, a halogen atom, a carboxy group, a hydroxy group, a thiol group, an alkyl group having 1 to 6 carbon atoms which may have a substituent, an alkenyl group having 2 to 6 carbon atoms which may have a substituent, or an aryl group having 6 to 12 carbon atoms which may have a substituent, and X a is a hydrogen atom, a lithium atom, a sodium atom, an alkyl group having 1 to 6 carbon atoms which may have a substituent, an aryl group having 6 to 12 carbon atoms which may have a substituent, or —CHNR d 2, and R d are each independently an alkyl group having 1 to 10 carbon atoms, an alkanol group having 1 to 10 carbon atoms, an alkenyl group having 2 to 10 carbon atoms, or an aryl group having 6 to 12 carbon atoms. a and R b are each independently a hydrogen atom, a halogen atom, a carboxy group, a hydroxy group, a thiol group, an alkyl group having 1 to 6 carbon atoms which may have a substituent, an alkenyl group having 2 to 6 carbon atoms which may have a substituent, or an aryl group having 6 to 12 carbon atoms which may have a substituent; each L is independently a single bond, a carbonyl group, an ether bond, an ester bond, or an amide bond; X a is a hydrogen atom, a lithium atom, a sodium atom, an alkyl group having 1 to 6 carbon atoms which may have a substituent, an aryl group having 6 to 12 carbon atoms which may have a substituent, or —CHNR d 2, and R d are each independently an alkyl group having 1 to 10 carbon atoms, an alkanol group having 1 to 10 carbon atoms, an alkenyl group having 2 to 10 carbon atoms, or an aryl group having 6 to 12 carbon atoms.

53. The additive according to claim 52, wherein the positive electrode active material contains 30% by mass or more of Ni.

54. The additive of claim 52, further comprising a nonionic polymer.

55. The additive according to claim 54, wherein the nonionic polymer is a polymer having a pyrrolidone structure or a nitrile group.

56. The additive according to claim 55, wherein the nonionic polymer is at least one selected from the group consisting of polyvinylpyrrolidone and polyacrylonitrile.

57. The additive of claim 52, further comprising a solvent.

58. A gelation inhibitor for an electrode slurry containing a positive electrode active material, a binder, and a solvent, the gelation inhibitor comprising a heterocycle-containing compound having a nitrogen-containing five-membered ring and not containing an oxygen atom in the nitrogen-containing five-membered ring.

59. The gelation inhibitor according to claim 58, wherein the only heteroatom contained in said nitrogen-containing five-membered ring is a nitrogen atom.

60. The gelation inhibitor according to claim 59, wherein the nitrogen-containing five-membered ring contains two or three nitrogen atoms.

61. The gelation inhibitor according to claim 58, wherein said heterocycle-containing compound has a carbonyl structure on the five-membered ring.

62. The gelation inhibitor according to claim 61, wherein said heterocycle-containing compound is a non-fused nitrogen-containing five-membered heterocycle.

63. The gelation inhibitor according to claim 61, wherein the carbonyl structure exhibits proton tautomerism.

64. The gelation inhibitor of claim 63, wherein the proton tautomerism is keto-enol tautomerism.

65. The gelation inhibitor according to claim 58, which comprises a heterocycle-containing compound represented by any one of the following formulas (3) to (4): (In the formula, R a ~R c are each independently a hydrogen atom, a halogen atom, a carboxy group, a hydroxy group, a thiol group, an amino group, an alkyl group having 1 to 6 carbon atoms which may have a substituent, an alkenyl group having 2 to 6 carbon atoms which may have a substituent, or an aryl group having 6 to 12 carbon atoms which may have a substituent, and R a and R b may be bonded to each other to form a ring having 4 to 12 carbon atoms which may have a substituent; each L is independently a single bond, a carbonyl group, an ether bond, an ester bond or an amide bond; X a and X b are each independently a hydrogen atom, a lithium atom, a sodium atom, an alkyl group having 1 to 6 carbon atoms which may have a substituent, an aryl group having 6 to 12 carbon atoms which may have a substituent, or —CHNR d 2, and R d are each independently an alkyl group having 1 to 10 carbon atoms, an alkanol group having 1 to 10 carbon atoms, an alkenyl group having 2 to 10 carbon atoms, or an aryl group having 6 to 12 carbon atoms.

66. Above R a ~R c , X a and X b The gelation inhibitor according to claim 65, wherein the substituent is at least one selected from the group consisting of a carboxy group, a hydroxy group, an aldehyde group, an ester group, a ketone group, an amino group, a phenyl group, a halogen atom, an alkoxysilyl group, an epoxy group, a carboxylic acid chloride group, and a thiol group.

67. The gelation inhibitor according to claim 65, wherein the heterocycle-containing compound is represented by the following formula (4b): (In the formula, R a ~R c is the same as above, and R e is a hydrogen atom, a carboxy group, a hydroxy group, an aldehyde group, an ester group, a ketone group, an amino group, a phenyl group, a halogen atom, an alkoxysilyl group, an epoxy group, a carboxylic acid chloride group, or a thiol group.

68. The gelation inhibitor according to claim 58, wherein the heterocycle-containing compound is solid at room temperature.

69. The gelation inhibitor according to claim 58, wherein the positive electrode active material contains 30% by mass or more of Ni.

70. The gelation inhibitor of claim 58, further comprising a nonionic polymer.

71. The gelation inhibitor according to claim 70, wherein the nonionic polymer is a polymer having a pyrrolidone structure or a nitrile group.

72. The gelation inhibitor according to claim 71, wherein the nonionic polymer is at least one selected from the group consisting of polyvinylpyrrolidone and polyacrylonitrile.

73. The gelation inhibitor of claim 58, further comprising a solvent.

74. A gelation inhibitor for an electrode slurry containing a positive electrode active material, a binder, and a solvent, the gelation inhibitor comprising a heterocycle-containing compound represented by any one of the following formulas (1) and (2): (In formula (1), R a and R b are each independently a hydrogen atom, a carboxy group, a hydroxy group, a thiol group, an alkyl group having 1 to 6 carbon atoms which may have a substituent, an alkenyl group having 2 to 6 carbon atoms which may have a substituent, or an aryl group having 6 to 12 carbon atoms which may have a substituent, a and R b may be bonded to each other to form a ring having 4 to 12 carbon atoms which may have a substituent, each L is independently a single bond, a carbonyl group, an ether bond, an ester bond or an amide bond, Z is N or C-L-R c and R c is a hydrogen atom, a halogen atom, a carboxy group, a hydroxy group, a thiol group, an alkyl group having 1 to 6 carbon atoms which may have a substituent, an alkenyl group having 2 to 6 carbon atoms which may have a substituent, or an aryl group having 6 to 12 carbon atoms which may have a substituent, and X a is a hydrogen atom, a lithium atom, a sodium atom, an alkyl group having 1 to 6 carbon atoms which may have a substituent, an aryl group having 6 to 12 carbon atoms which may have a substituent, or —CHNR d 2, and R d are each independently an alkyl group having 1 to 10 carbon atoms, an alkanol group having 1 to 10 carbon atoms, an alkenyl group having 2 to 10 carbon atoms, or an aryl group having 6 to 12 carbon atoms. a and R b are each independently a hydrogen atom, a halogen atom, a carboxy group, a hydroxy group, a thiol group, an alkyl group having 1 to 6 carbon atoms which may have a substituent, an alkenyl group having 2 to 6 carbon atoms which may have a substituent, or an aryl group having 6 to 12 carbon atoms which may have a substituent; each L is independently a single bond, a carbonyl group, an ether bond, an ester bond, or an amide bond; X a and X b are each independently a hydrogen atom, a lithium atom, a sodium atom, an alkyl group having 1 to 6 carbon atoms which may have a substituent, an aryl group having 6 to 12 carbon atoms which may have a substituent, or —CHNR d 2, and R d are each independently an alkyl group having 1 to 10 carbon atoms, an alkanol group having 1 to 10 carbon atoms, an alkenyl group having 2 to 10 carbon atoms, or an aryl group having 6 to 12 carbon atoms.

75. Above R a ~R c , X a and X b The gelation inhibitor according to claim 74, wherein the substituent is at least one selected from the group consisting of a carboxy group, a hydroxy group, an aldehyde group, an ester group, a ketone group, a phenyl group, a halogen atom, an alkoxysilyl group, an epoxy group, a carboxylic acid chloride group, and a thiol group.

76. The gelation inhibitor according to claim 74, wherein the heterocycle-containing compound is a heterocycle-containing compound represented by the following formula (5): (In the formula, Ar 1 Z, X are an aromatic ring having 4 to 12 carbon atoms which may have a substituent, or an aliphatic ring having 4 to 10 carbon atoms which may have a substituent. a is the same as above.) 77. The gelation inhibitor according to claim 76, wherein the heterocycle-containing compound is a heterocycle-containing compound represented by any one of the following formulas (6) to (7): (Wherein Z and X a is the same as above.) 78. The gelation inhibitor of claim 74, wherein Z is N.

79. The gelation inhibitor according to claim 74, wherein the positive electrode active material contains 30% by mass or more of Ni.

80. The gelation inhibitor of claim 74, further comprising a nonionic polymer.

81. The gelation inhibitor according to claim 80, wherein the nonionic polymer is a polymer having a pyrrolidone structure or a nitrile group.

82. The gelation inhibitor according to claim 81, wherein the nonionic polymer is at least one selected from the group consisting of polyvinylpyrrolidone and polyacrylonitrile.

83. The gelation inhibitor of claim 74, further comprising a solvent.