Epitaxial growth detection method

MYPI2025003116A0Undetermined Publication Date: 2024-09-22GUANGDONG TIANYU SEMICON CO LTD
View PDF 0 Cites 0 Cited by

Patent Information

Application Number
MYPI2025003116
Authority / Receiving Office
MY · MY
Patent Type
Applications
Current Assignee / Owner
Priority Date
2023-03-22
Filing Date
2024-03-21
Publication Date
2024-09-22

AI Technical Summary

Technical Problem

The existing technology has the problem of doping concentration drift during the epitaxial growth of silicon carbide single crystal materials, which causes the doping concentration of each furnace of epitaxial materials to increase irregularly. Moreover, the existing detection methods are destructive and costly, and cannot be used in mass production. Promote applications.

Method used

The substrate tray design is adopted, including the main accommodation tank and the secondary accommodation tank. The growth substrate and the reference substrate grow the epitaxial layer at the same time, and the coating parameters of the reference epitaxial layer are tested as the detection parameters of the epitaxial layer of the growth substrate to avoid damage. Product structure, suitable for mass production.

Benefits of technology

It achieves non-destructive detection, reduces production costs, improves detection accuracy and efficiency, is suitable for multi-layer epitaxial growth detection, and reduces waste of production capacity.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure PI2025003116_DRAWING_001
    Figure PI2025003116_DRAWING_001
  • Figure PI2025003116_DRAWING_002
    Figure PI2025003116_DRAWING_002
  • Figure PI2025003116_DRAWING_003
    Figure PI2025003116_DRAWING_003
Patent Text Reader

Abstract

An epitaxial growth detection method, comprising: providing a substrate tray (10), the substrate tray (10) being provided with a main accommodating recess (21) and an auxiliary accommodating recess (22). The growth detection method comprises: step 1, placing a growth substrate in the main accommodating recess (21), and placing a reference substrate in the auxiliary accommodating recess (22); step 2, controlling the substrate tray (10) to rotate at a constant speed and growing an epitaxial layer on the substrate on the substrate tray (10), such that a reference epitaxial layer is formed on the reference substrate while forming the epitaxial layer on the growth substrate; and step 3, testing a coating parameter of the reference epitaxial layer to serve as a detection parameter of the epitaxial layer.
Need to check novelty before this filing date? Find Prior Art

Description

Epitaxial growth detection method Technical Field

[0001] The present invention relates to the technical field of crystal synthesis, and in particular to an epitaxial growth detection method after an epitaxial layer is grown by a high-temperature chemical vapor deposition device. Background Art

[0002] Silicon carbide single crystal material offers advantages such as high thermal conductivity, high breakdown field strength, high saturated electron drift velocity, and high bonding energy. It can effectively meet the application requirements of modern electronic technology in harsh conditions such as high temperature, high power, high voltage, high frequency, and high radiation. Unlike traditional silicon devices, silicon carbide devices cannot be directly fabricated on silicon carbide single crystal material. Instead, high-quality epitaxial layers must be grown on single crystal substrates, and various device structures are then fabricated on the epitaxial layers.

[0003] During the chemical vapor deposition (CVD) growth process, silicon carbide and dopant elements adhering to the graphite components in the furnace cannot be completely removed by high temperatures. They are then reheated and precipitated during the next growth cycle. This results in an erratic increase in the dopant concentration of each batch of epitaxial material, even at the same dopant gas flow rate. This is known in the industry as "dopant concentration drift." During epitaxial growth, laboratory technicians typically adjust the dopant gas flow rate based on the dopant concentration drift of the previous batch of epitaxial wafers. After deposition, samples are typically taken to an offline testing facility to measure parameters such as dopant concentration, thickness, roughness, and stress. However, existing testing methods can damage the epitaxial layers on the product. This is especially true when testing multi-layer epitaxial growth, which inevitably requires the use of secondary ion mass spectrometry (SIMS). This expensive and destructive testing method renders the silicon carbide epitaxial wafers unusable after testing, making it unsuitable for mass production. Multiple wafers must be grown and then re-cut, which is costly and wastes production capacity.

[0004] Therefore, there is an urgent need for an epitaxial growth detection method that can solve the above problems.

[0005] Summary of the Invention

[0006] The purpose of the present invention is to provide an epitaxial growth detection method, which can grow a reference epitaxial layer on a reference substrate while growing an epitaxial layer on a growth substrate, and detect the parameters of the reference epitaxial layer as the parameters of the epitaxial layer on the growth substrate without destroying the epitaxial layer structure on the product.

[0007] In order to achieve the above-mentioned objectives, the present invention discloses an epitaxial growth detection method, providing a substrate tray, wherein the substrate tray has a main receiving groove and a secondary receiving groove; the growth detection method comprises: step 1, placing a growth substrate in the main receiving groove, and placing a reference substrate in the secondary receiving groove; step 2, controlling the substrate tray to rotate at a uniform speed and growing an epitaxial layer on the substrate on the substrate tray, so that while the epitaxial layer is formed on the growth substrate, a reference epitaxial layer is formed on the reference substrate; step 3, testing the coating parameters of the reference epitaxial layer as detection parameters of the epitaxial layer.

[0008] Compared with the prior art, the present invention adds a sub-containing groove for placing the reference substrate on the substrate tray, so that a reference epitaxial layer is grown on the reference substrate while the epitaxial layer is grown on the product. The coating parameters of the reference epitaxial layer are tested as the parameters of the epitaxial layer grown on the product. There is no need to destroy the epitaxial layer on the product, and a variety of testing methods including destructive testing methods can be used, which can be used for epitaxial detection during mass production.

[0009] Preferably, the epitaxial growth detection method is a multi-layer epitaxial growth detection method, wherein multiple layers of single epitaxial layers are grown on the growth substrate, and the sub-receiving groove is divided into a plurality of parts corresponding to the single epitaxial layers on the growth substrate that need to be epitaxially grown; the step 2 comprises: according to the growth order of the epitaxial layers on the growth substrate, using a mask plate to sequentially expose a part of the sub-receiving groove corresponding to the single epitaxial layer to be grown and cover other parts of the sub-receiving groove, controlling the substrate tray to rotate uniformly at a preset speed and growing an epitaxial layer on the substrate on the substrate tray, so that a corresponding single epitaxial layer is formed on the growth substrate, and a corresponding single reference epitaxial layer is formed on the reference substrate of the corresponding part of the sub-receiving groove; the step 3 comprises: detecting the coating parameters of the single reference epitaxial layer on the reference substrate at each part as the detection parameters of the corresponding single epitaxial layer in the epitaxial layer. Compared with the existing technology, this solution switches the shielding sub-capacity groove through the shielding plate to form different single-layer reference epitaxial layers on different reference substrates or different parts of the reference substrate, which are used as detection parameters for different layers of epitaxial layers grown on the product, so as to facilitate the use of single-layer epitaxial material detection methods to detect the epitaxial layer structure on multi-layer epitaxially grown epitaxial wafers. The detection results are accurate and the detection means are diverse.

[0010] Specifically, a double-layer single epitaxial layer is grown on the growth substrate, and the auxiliary receiving groove is divided into a first part and a second part corresponding to the single epitaxial layer on the growth substrate that needs to be tested for epitaxial growth; the step 2 includes: step 21, using a mask plate to cover the first part of the auxiliary receiving groove and expose the second part of the auxiliary receiving groove; step 22, controlling the substrate tray to rotate at a preset speed and growing an epitaxial layer on the substrate on the substrate tray, so that the first single epitaxial layer is formed on the growth substrate, and the first single reference epitaxial layer is formed on the reference substrate in the second part of the auxiliary receiving groove at the same time; step 23 , moving the mask so that it covers the second portion of the auxiliary receiving groove and exposes the first portion of the auxiliary receiving groove; step 24, controlling the substrate tray to rotate uniformly at a preset speed and growing an epitaxial layer on the substrate tray, so that a second single epitaxial layer is formed on the first single epitaxial layer of the growth substrate, and a second single reference epitaxial layer is formed on the reference substrate in the first portion of the auxiliary receiving groove; step 3 includes: testing the coating parameters of the first single reference epitaxial layer as detection parameters of the first single epitaxial layer, and testing the coating parameters of the second single reference epitaxial layer as detection parameters of the second single epitaxial layer. The present invention switches between covering the first and second portions of the auxiliary receiving groove by moving the same mask.

[0011] More preferably, the mask plate is slidably mounted on the substrate tray along a sliding track and can slide under the centrifugal force of the substrate tray to switch between blocking the first and second portions of the auxiliary receiving slot. Step 23 specifically includes controlling the substrate tray to reduce its rotational speed from a preset speed to zero within a preset time, so that the shielding plate switches from blocking the first portion of the auxiliary receiving slot to blocking the second portion of the auxiliary receiving slot. This solution enables the present invention to control the shielding plate to switch between blocking the auxiliary receiving slot through the rotational inertia of the substrate tray, eliminating the need for dedicated control of the shielding plate's switching.

[0012] More specifically, the sliding track is arranged along the centrifugal direction of rotation of the substrate tray and is provided with a limit portion that limits the mask plate from sliding forward to sliding backward of the sliding track. The first and second portions of the auxiliary accommodating groove are arranged from back to front along the sliding track. The mask plate slides along the sliding track between the sliding backward position and the sliding forward position to switch between covering the first portion and the second portion of the auxiliary accommodating groove. The contact surface between the mask plate and the sliding track is a smooth sliding surface, so that the mask plate can slide from back to front on the sliding track under the action of inertia when the substrate tray decelerates. The limit portion can effectively prevent the shielding plate from resetting to the sliding backward position when the substrate tray recovers from 0 to a preset speed.

[0013] Specifically, the position-limiting portion includes a slot provided on the track surface of the sliding track at a position corresponding to the front sliding position and having a concave-convex fit with the support leg of the mask plate. Of course, the structure of the position-limiting portion is not limited thereto.

[0014] Specifically, the substrate tray is controlled to decrease its rotation speed from 600 rpm to 0 within 30 seconds, so that the shielding plate switches from shielding the first part of the auxiliary accommodating groove to shielding the second part of the auxiliary accommodating groove.

[0015] Specifically, the first portion and the second portion are respectively a first auxiliary containing groove and a second auxiliary containing groove arranged at a distance from each other. This solution enables the present invention to form a first single reference epitaxial layer and a second single reference epitaxial layer on two reference substrates, respectively.

[0016] Specifically, a mercury probe CV is used to detect the doping concentration of the reference epitaxial layer on each part of the reference substrate, and FTIR is used to detect the thickness of the reference epitaxial layer on each part of the reference substrate. The coating parameters include doping concentration and / or thickness.

[0017] Preferably, the main accommodating groove is arranged in the middle of the substrate tray, the auxiliary accommodating groove is arranged on one side of the main accommodating groove and adjacent to the edge of the substrate tray, and the notch area of ​​the main accommodating groove is larger than the notch area of ​​the auxiliary accommodating groove.

[0018] Preferably, the growth substrate and the reference substrate are silicon carbide substrates, the substrate tray is made of graphite, and the surface of the substrate tray is covered with a tantalum carbide coating. BRIEF DESCRIPTION OF THE DRAWINGS

[0019] FIG1 is a flow chart of an epitaxial growth detection method according to a first embodiment of the present invention.

[0020] FIG2 is a flow chart of an epitaxial growth detection method according to a second embodiment of the present invention.

[0021] FIG3 is a structural diagram of a substrate tray according to the present invention.

[0022] FIG4 a is a structural diagram of the substrate tray of the present invention after removing the shielding plate.

[0023] FIG4b is an enlarged view of portion a in FIG4a.

[0024] FIG5a and FIG5b are structural diagrams of the mask at different angles.

[0025] 6a and 6b show the connection structure between the auxiliary accommodating groove and the mask plate when the mask plate slides to the second portion.

[0026] 7a and 7b show the connection structure between the auxiliary accommodating groove and the mask plate when the mask plate slides to the first portion.

[0027] FIG. 8 is a connection structure between the auxiliary receiving groove and the mask plate in another embodiment of the present invention. DETAILED DESCRIPTION

[0028] In order to explain the technical content, structural features, achieved objectives and effects of the present invention in detail, the following is a detailed description in conjunction with the embodiments and the accompanying drawings.

[0029] 1 and 3 , in a first embodiment of the present invention, an epitaxial growth detection method is disclosed. A substrate tray 10 is provided, and the substrate tray 10 has a main receiving groove 21 and a secondary receiving groove 22 . The growth detection method includes steps S1 to S3 .

[0030] Step S1 : placing a growth substrate in the main receiving tank 21 , and placing a reference substrate in the auxiliary receiving tank 22 .

[0031] Step S2 , controlling the substrate tray 10 to rotate at a constant speed and growing an epitaxial layer on the substrate on the substrate tray 10 , so that while the epitaxial layer is formed on the growth substrate, a reference epitaxial layer is formed on the reference substrate.

[0032] Step S3 , testing the coating parameters of the reference epitaxial layer to serve as detection parameters of the epitaxial layer.

[0033] In this embodiment, the epitaxial growth can be either single-layer epitaxial growth or multi-layer epitaxial growth. In the case of single-layer epitaxial growth, the epitaxial layer comprises a single epitaxial layer, and the reference epitaxial layer is also a single epitaxial layer. In the case of multi-layer epitaxial growth, the epitaxial side comprises multiple epitaxial layers, and corresponding multiple epitaxial layers can also be formed on the reference epitaxial layer. Alternatively, multiple reference substrates can be used to form multiple single epitaxial layers.

[0034] With reference to Figures 2, 4, and 4a to 5b, in a second embodiment of the present invention, the epitaxial growth detection method is a multi-layer epitaxial growth detection method. Multiple single epitaxial layers are grown on the growth substrate, and the auxiliary receiving groove is divided into a plurality of sections corresponding to the single epitaxial layers on the growth substrate that require epitaxial growth detection. This embodiment is specifically described using a double-layer epitaxial growth detection method as an example:

[0035] Among them, a first single epitaxial layer and a second single epitaxial layer are grown on the growth substrate, and the auxiliary receiving groove 22 is divided into a second part corresponding to the first single epitaxial layer on the growth substrate that needs to be epitaxially grown and a first part corresponding to the second single epitaxial layer that needs to be epitaxially grown.

[0036] The step S2 includes steps S21 to S24.

[0037] In step S21 , a mask plate 13 is used to cover a first portion of the auxiliary receiving groove 22 and expose a second portion of the auxiliary receiving groove 22 .

[0038] In step S22, the substrate tray 10 is controlled to rotate at a preset speed and an epitaxial layer is grown on the substrate on the substrate tray 10, so that a first single epitaxial layer is formed on the growth substrate and a first single reference epitaxial layer is formed on the reference substrate in the second part of the auxiliary receiving groove 22.

[0039] In step S23 , the mask plate 13 is used to cover the second portion of the auxiliary receiving groove 22 and expose the first portion of the auxiliary receiving groove 22 .

[0040] In step S24, the substrate tray 10 is controlled to rotate at a preset speed and an epitaxial layer is grown on the substrate tray 10, so that a second single epitaxial layer is formed on the first single epitaxial layer of the growth substrate, and a second single reference epitaxial layer is formed on the reference substrate of the first part of the auxiliary accommodating groove 22.

[0041] The step S3 includes: testing the coating parameters of the first single reference epitaxial layer to serve as the detection parameters of the first single epitaxial layer, and testing the coating parameters of the second single reference epitaxial layer to serve as the detection parameters of the second single epitaxial layer.

[0042] The epitaxial layer is a single-layer epitaxial structure, and the reference epitaxial layer is also a single-layer epitaxial structure.

[0043] This embodiment is for epitaxial growth detection of a multi-layer epitaxial growth, wherein the epitaxial layers include a first single epitaxial layer and a second single epitaxial layer, and the reference epitaxial layers include a first single reference epitaxial layer and a second single reference epitaxial layer. Of course, this is not limiting. In other embodiments, a mask plate may not be provided, and two reference epitaxial layers may be formed directly on a reference substrate. Then, in step S3, a destructive method (e.g., secondary ion mass spectrometry) is used to detect the coating parameters of the two reference epitaxial layers, which serve as the coating parameters of the two epitaxial layers on the growth substrate.

[0044] More preferably, the mask plate 13 is slidably mounted on the substrate tray 10 along a slide rail 31 and can slide under the centrifugal force of the substrate tray 10 to switch between blocking the first and second portions of the auxiliary receptacle 22. Step S23 specifically includes controlling the substrate tray 10 to reduce its predetermined rotational speed to zero within a predetermined time, so that the shielding plate switches from blocking the first portion of the auxiliary receptacle 22 to blocking the second portion of the auxiliary receptacle 22. Of course, the present invention is not limited to this. The mask plate 13 can also slide or move on the substrate tray 10 under the control of an electric or other control unit to switch between blocking the first and second portions of the auxiliary receptacle 22. For example, the mask plate 13 can be driven to move on the substrate tray by an electric cylinder, solenoid valve, or paddle. In this embodiment, only one mask plate 13 is used to switch between blocking the first and second portions of the auxiliary receptacle 22. In another embodiment, multiple mask plates 13 can be used to independently control blocking of the first and second portions of the auxiliary receptacle 22.

[0045] Among them, this embodiment is used for epitaxial layer detection during double-layer epitaxial growth. In another embodiment, the growth substrate includes N single epitaxial layers that need to be detected for epitaxial growth, N is greater than or equal to 2 (for example, 2, 3, 4), and the N single epitaxial layers constitute the epitaxial layer on the growth substrate. The sub-accommodation groove 22 is divided into N parts. When each single epitaxial layer grows, the mask plate 13 is used to switch the corresponding part of the exposed sub-accommodation groove 22 and block other parts of the sub-accommodation groove 22. When the growth of N single epitaxial layers is completed, N corresponding single reference epitaxial layers will be formed in the N corresponding parts of the sub-accommodation groove 22, so that the coating parameters of the single reference epitaxial layer at each part are detected as the detection parameters of the single epitaxial layer of each single layer in the epitaxial layer.

[0046] Specifically, the substrate tray 10 is controlled to decrease its rotation speed from 600 rpm to 0 within 30 seconds, so that the shielding plate switches from shielding the first part of the auxiliary accommodating groove 22 to shielding the second part of the auxiliary accommodating groove 22 .

[0047] Specifically, a mercury probe CV is used to detect the doping concentration of the first single reference epitaxial layer and the second single reference epitaxial layer respectively, and FTIR is used to detect the thickness of the first single reference epitaxial layer and the second single reference epitaxial layer respectively, and the coating parameters include doping concentration and / or thickness.

[0048] 5a to 5b, the substrate tray 10 has a main accommodating area 11 and a secondary accommodating area 12. The main accommodating area 11 is provided with a main accommodating groove 21 for accommodating a growth substrate, and the secondary accommodating area 12 is provided with a secondary accommodating groove 22 for accommodating a reference substrate. The mask plate 13 is slidably installed on the substrate tray 10 along a sliding track 31 and covers part of the secondary accommodating groove 22. The sliding rail 31 is spaced apart from the rotation center of the substrate tray 10 and is arranged along the centrifugal direction of rotation of the substrate tray 10. The mask plate 13 slides along the sliding rail 31 between the rear sliding position and the front sliding position of the sliding rail, and can switch to cover the first part and the second part of the auxiliary accommodating groove 22. The contact surface between the mask plate 13 and the sliding rail 31 is a smooth sliding surface, so that the mask plate 13 can slide on the sliding rail 31 under the action of inertia when the substrate tray 10 decelerates, and switch from covering the first part of the auxiliary accommodating groove 22 to covering the second part of the auxiliary accommodating groove 22.

[0049] Wherein, the sliding rail 31 is provided with a limiting portion for limiting the sliding of the mask plate 13 from the front sliding position of the sliding rail 31 to the rear sliding position of the sliding rail 31. The limiting portion mainly limits the sliding of the mask plate 13 from the front sliding position of the sliding rail 31 to the rear sliding position of the sliding rail 31 under the action of the centrifugal force when the substrate tray 10 rotates. In this embodiment, the limiting portion includes a clamping groove (313, 314) provided on the track surface of the sliding rail 31 corresponding to the front sliding position and matched with the support feet (132, 133) of the mask plate 13 in a concave-convex manner. Of course, the limiting portion is not limited to this, and can also be other structures, such as a clamping channel located on the sliding rail 31 and extending from the back to the front to gradually become smaller and deeper to clamp the support feet (132, 133), such as a small spring plate provided on the track surface.

[0050] The surface roughness Ra of the contact surface between the mask plate 13 and the sliding rail 31 is less than 10 nm. When the substrate tray 10 rotates in a preset direction and the preset rotational speed decreases to 0 within a preset time, a relatively large swinging force is generated on the mask plate 13, causing the mask plate 13 to slide from the rear sliding position to the front sliding position under the action of inertia, thereby switching the mask plate 13 from covering the first portion of the auxiliary receiving groove 22 to covering the second portion of the auxiliary receiving groove 22. The preset rotational speed is the rotational speed of the tray body when growing an epitaxial layer on the growth substrate, and the preset time is a time designed by technicians based on actual conditions.

[0051] The first and second portions of the secondary accommodating groove 22 are arranged from back to front along the trajectory of the slide track 31. The first and second portions can be spaced apart or directly connected. When the substrate tray 10 is rotated forward during epitaxial layer growth, the first portion is located behind the second portion. This allows the mask 13 to swing from covering the first portion to covering the second portion when the substrate tray is rapidly decelerated.

[0052] The sliding track 31 is an arc-shaped track centered on the rotation center. This solution allows the mask plate 13 to slide along the sliding track 31 more easily under the action of inertia. Of course, it is also possible to have only one end of the sliding track 31 away from the second portion of the secondary accommodating groove 22 be an arc-shaped track centered on the rotation center, with the other parts being connected to the arc-shaped track or a straight line with a smooth transition.

[0053] The fact that the sliding track 31 is arranged along the centrifugal direction of rotation of the substrate tray 10 means that the arc of the sliding track 31 does not face the rotation axis of the substrate tray 10, so that the speed change during the rotation of the substrate tray 10 can drive the mask plate 13 to swing along the sliding track 31. Specifically, the fact that the sliding track 31 is arranged along the centrifugal direction of rotation of the substrate tray 10 includes: the sliding track 31 is arranged along a circle centered on the rotation center of the substrate tray 10, along a tangent of a circle centered on the rotation center of the substrate tray 10, or along a smooth line that combines a circle centered on the rotation center of the substrate tray and a tangent of a circle centered on the rotation center of the substrate tray, or along a spiral track centered on the rotation center of the substrate tray.

[0054] Referring to Figures 3 to 4b, the main accommodating area 11 is provided in the middle of the substrate tray 10, and the secondary accommodating area 12 is provided around the main accommodating area 11 and extends to the edge of the substrate tray 10, so that the secondary accommodating groove 22 is provided adjacent to the edge of the substrate tray 10, thereby increasing the throwing force of the mask plate 13 when the substrate tray 10 is rapidly decelerated, and the notch area of ​​the main accommodating groove 21 is larger than the notch area of ​​the secondary accommodating groove 22. Specifically, the cross section of the main accommodating groove 21 is a circle with straight edges, and the diameter of the circle is 150mm. The secondary accommodating groove 22 has two rectangular or quasi-rectangular cross sections with a length and width of 15mm. The depth of the main accommodating groove 21 and the secondary accommodating groove 22 is 2mm. Of course, the shape of the secondary accommodating groove 22 is not limited to this, and can also be circular, elliptical, fan-shaped, etc.

[0055] The distance between the primary accommodating groove 21 and the secondary accommodating groove 22 is greater than or equal to 0.5 mm and less than or equal to 1.5 mm. The opening of the primary accommodating groove 21 is a circle with straight edges. The opening of the primary accommodating groove 21 is a rhombus or rectangle consisting of two concentric arcs and two parallel straight lines. In this embodiment, the substrate tray 10 is a circular block with a thickness of 8 mm and an outer diameter of 220 mm. The sliding track 31 is composed of arc-shaped segments with a diameter of 166 mm and a diameter of 206 mm. The track arc length is 36 mm, the track width is 1 mm, and the spacing between the two arc-shaped segments is 20 mm.

[0056] Referring to Figures 4b, 6b, and 7b, the sliding track 31 includes a first slide rail 311 corresponding to the first portion and a second slide rail 312 corresponding to the second portion. Referring to Figures 5a to 7b, the mask plate 13 includes a covering body 131, a first support leg 132 that slidably supports the covering body 131 on the first slide rail 311, and a second support leg 133 that slidably supports the covering body 131 on the second slide rail 312. The track surface of the first slide rail 311 is lower than the track surface of the second slide rail 312, forming a stepped blocking surface 3111 between the track surfaces of the first slide rail 311 and the second slide rail 312. This, in conjunction with the end blocking wall of the second slide rail 312, limits the position of the covering body 131. In this embodiment, the covering body 131 has an area of ​​15 mm x 15 mm. The spacing between the first support leg 132 and the second support leg 133 is 16 mm.

[0057] 6b and 7b , the height difference between the first support leg 132 and the second support leg 133 is equal to the height difference between the track surface of the first slide rail 311 and the track surface of the second slide rail 312. The height difference between the track surface of the first slide rail 311 and the track surface of the second slide rail 312 is 1 mm.

[0058] 6b and 7b , a first blocking wall is formed at one end of the first slide rail 311 away from the second slide rail 312 to prevent the first supporting foot 132 from derailing, and a second blocking wall is formed at one end of the second slide rail 312 away from the first slide rail 311 to prevent the second supporting foot 133 from derailing.

[0059] Referring to Figures 4b, 6b, and 7b, a first retaining groove 313 is formed at one end of the first slide rail 311 proximal to the second slide rail 312, which restrains the first support leg 132 of the mask plate 13 when it is switched to the forward sliding position. A second retaining groove 314 is formed at one end of the second slide rail 312 distal from the first slide rail 311, which restrains the second support leg 133 of the mask plate 13 when it is switched to the forward sliding position. The first retaining groove 313 and the second retaining groove 314 are 1mm×1mm×1mm cubic grooves, the first support leg 132 is a cuboid measuring 0.9mm×0.6mm×4mm (height), and the second support leg 133 is a cuboid measuring 0.9mm×0.6mm×5mm (height).

[0060] In this embodiment,

[0061] Referring to Figures 4b, 6a, and 7a, the first portion and the second portion are respectively a first secondary accommodating groove 221 and a second secondary accommodating groove 222, which are spaced apart. A reference substrate 201 is installed in the first secondary accommodating groove 221 corresponding to the first portion, and a reference substrate 201 is installed in the second secondary accommodating groove 222 corresponding to the second portion. The first secondary accommodating groove 221 and the second secondary accommodating groove 222 are arranged around the rotation center spacing. The mask plate 13 can switch between covering the first secondary accommodating groove 221 and the second secondary accommodating groove 222. When covering the first secondary accommodating groove 221, the second secondary accommodating groove 222 is completely exposed. When covering the second secondary accommodating groove 222, the first secondary accommodating groove 221 is exposed.

[0062] In this embodiment, the substrate tray 10 is positioned between the first and second secondary receiving grooves 221, 222. The cross-sections of the first and second secondary receiving grooves 221, 222 are rectangular or quasi-rectangular, with a length and width of 15 mm. The depth of the first and second secondary receiving grooves 221, 222 is 2 mm. Of course, the shapes of the first and second secondary receiving grooves 221, 222 are not limited to this; they may also be circular, elliptical, or fan-shaped.

[0063] Of course, referring to FIG8 , in another embodiment, the auxiliary containing groove 22a can also be one, and the first part and the second part of the auxiliary containing groove 22a are connected, which are the front half and the rear half of the auxiliary containing groove 22a respectively. A reference substrate is installed in the auxiliary containing groove 22a, and the mask plate 13 can switch to cover the front half and the rear half of the auxiliary containing groove 22a. After the epitaxial growth is completed, the concentration and thickness of the epitaxial layer grown on the front half and the rear half of the reference substrate in the auxiliary containing groove 22a can be respectively detected to judge the concentration and thickness of the first single epitaxial layer and the second single epitaxial layer on the growth substrate, wherein the auxiliary containing groove 22a is provided with a reference substrate. The front half and the rear half of 2a are set at a distance or are just connected. If the front half and the rear half of the auxiliary groove 22a are set at a distance, the area between the front half and the rear half of the auxiliary groove 22a can be fully covered or not covered when the mask plate 13 switches to cover the front half and the rear half of the auxiliary groove 22a. When not covered, the epitaxial layer grown between the front half and the rear half of the reference substrate is a double-layer epitaxial layer. The parameters of the double-layer epitaxial layer can be detected to perform separate verification of the two-layer detection data, the parameters between the two epitaxial layers, or the parameters of the overall structure formed by the double-layer epitaxial layer.

[0064] In this embodiment, the method for performing epitaxial growth and epitaxial growth detection using the substrate tray 10 specifically includes:

[0065] Referring to Figures 6a and 6b , the growth substrate is placed in the main receiving groove 21, and the two reference substrates 201 and 202 are placed in the first and second secondary receiving grooves 221 and 222, respectively. The mask plate 13 is moved to the rear sliding position to cover the reference substrate 201 in the first secondary receiving groove 221, while exposing the reference substrate 202 in the second secondary receiving groove 222. At this point, the mask plate 13 is positioned on the first slide rail 311.

[0066] The substrate tray 10 is rotated around its rotation center and installed in the epitaxial growth device. The substrate tray 10 is controlled to rotate in the direction of the arrow in Figure 4b, rotated to a speed of 600 rpm and maintained at a constant speed, and chemical vapor deposition (CVD) is used to grow an epitaxial layer on the substrate on the substrate tray 10, thereby growing a first single epitaxial layer on the growth substrate and growing a first single reference epitaxial layer on the reference substrate 202.

[0067] 7a and 7b , the substrate tray 10 is controlled to decrease its rotation speed from 600 rpm to 0 within 30 seconds, so that the mask plate 13 slides along the sliding rail 31 under the action of inertial centrifugal force, and slides from the first slide rail 311 to the second slide rail 312. The mask plate 13 is inertially swung to the upper part of the sliding front position to cover the reference substrate 202 in the second sub-containing groove 222, and the reference substrate 201 in the first sub-containing groove 221 is exposed.

[0068] The substrate tray 10 is controlled to rotate in the direction of the arrow in Figure 4b, rotated to a speed of 600 rpm and maintained at a constant speed, and the epitaxial layer is started to be grown again on the substrate on the substrate tray 10 using chemical vapor deposition (CVD), thereby growing a second single epitaxial layer on the growth substrate, and growing a second single reference epitaxial layer on the reference substrate 201.

[0069] While the first and second single epitaxial layers are formed on the growth substrate, reference substrate 202 on which the first single reference epitaxial layer is grown and reference substrate 201 on which the second single reference epitaxial layer is grown are obtained. Relevant parameters of the two epitaxial layers on the growth substrate, including doping concentration and thickness, are obtained by testing the first single reference epitaxial layer on reference substrate 202 and the second single reference epitaxial layer on reference substrate 201. The test data of the first single reference epitaxial layer is used as the data of the first single epitaxial layer of the growth substrate, and the test data of the second single reference epitaxial layer is used as the data of the second single epitaxial layer of the growth substrate.

[0070] The reference substrate 201 and the reference substrate 202 are tested for mercury probe CV and FTIR respectively to obtain the doping concentration and thickness of the first single epitaxial layer and the second single epitaxial layer of the growth substrate.

[0071] In this embodiment, the growth substrate and reference substrates 201 and 202 are silicon carbide substrates. The substrate tray 10 is made of graphite and coated with tantalum carbide. Reference substrates 201 and 202, after epitaxial layer growth, are referred to as silicon carbide reference wafers, and the growth substrates after epitaxial layer growth are referred to as double-layer silicon carbide epitaxial wafers. Reference substrate 201 and the growth substrate are made of the same material, differing only in size. The materials of the reference and growth substrates are not limited to silicon carbide.

[0072] The technicians tested the epitaxial layers on the reference substrate 201, reference substrate 202, and growth substrate obtained in the above experiments to verify the accuracy of the testing method of the present invention. Mercury probe CV and FTIR measurements were performed on two silicon carbide reference test wafers, respectively, to obtain the doping concentration and thickness of the first and second single reference epitaxial layers of the dual-layer silicon carbide epitaxial wafer. The data obtained from the first and second single reference epitaxial layers measured on the two silicon carbide reference test wafers were compared with the data obtained from a single measurement of the dual-layer silicon carbide epitaxial wafer using secondary ion mass spectrometry (SIMS). SIMS itself has low accuracy for measuring doping concentration and thickness and can only be used as an estimate. Referring to Table 1 below, the values ​​measured using the reference test wafers in this experiment generally differed from the SIMS data by less than 20%. This confirms that the reference test wafers used in this solution can effectively reflect the doping concentration and thickness of the first and second single epitaxial layers of the dual-layer silicon carbide epitaxial wafer after epitaxial growth.

[0073] Table 1

[0074] The above disclosure is only the preferred embodiment of the present invention, which certainly cannot be used to limit the scope of the present invention. Therefore, equivalent changes made according to the scope of the patent application of the present invention are still within the scope of the present invention.

Claims

1. A method for detecting epitaxial growth, Features: Providing a substrate tray, the substrate tray having a main containing groove and a secondary containing groove; The growth detection method comprises: Step 1, placing a growth substrate in the main containing groove, and placing a reference substrate in the auxiliary containing groove; Step 2, controlling the substrate tray to rotate at a constant speed and growing an epitaxial layer on the substrate on the substrate tray, so that while the epitaxial layer is formed on the growth substrate, a reference epitaxial layer is formed on the reference substrate; Step 3: testing the coating parameters of the reference epitaxial layer to serve as the detection parameters of the epitaxial layer.

2. The epitaxial growth detection method according to claim 1, Features: The epitaxial growth detection method is a multi-layer epitaxial growth detection method, wherein multiple single epitaxial layers are grown on the growth substrate, and the auxiliary containing groove is divided into a plurality of parts corresponding to the single epitaxial layers on the growth substrate that need to be subjected to epitaxial growth detection; The step 2 comprises: according to the growth order of the epitaxial layer on the growth substrate, using a mask plate to sequentially expose a portion of the auxiliary containing groove corresponding to the single epitaxial layer to be grown currently and cover other portions of the auxiliary containing groove, controlling the substrate tray to rotate at a preset speed and growing an epitaxial layer on the substrate on the substrate tray, so that while a corresponding single epitaxial layer is formed on the growth substrate, a corresponding single reference epitaxial layer is formed on the reference substrate of the corresponding portion of the auxiliary containing groove; The step 3 comprises: detecting the coating parameters of the single reference epitaxial layer on the reference substrate at each portion as detection parameters of the corresponding single epitaxial layer in the epitaxial layer.

3. The epitaxial growth detection method according to claim 2, Features: A double-layer single epitaxial layer is grown on the growth substrate, and the auxiliary containing groove is divided into a first part and a second part corresponding to the single epitaxial layer on the growth substrate that needs to be tested for epitaxial growth; The epitaxial growth detection method is a double-layer epitaxial growth detection method; The step 2 comprises: Step 21, using a mask plate to cover the first portion of the auxiliary receiving groove and expose the second portion of the auxiliary receiving groove; Step 22, controlling the substrate tray to rotate uniformly at a preset speed and growing an epitaxial layer on the substrate on the substrate tray, so that while a first single epitaxial layer is formed on the growth substrate, a first single reference epitaxial layer is formed on the reference substrate in the second portion of the secondary receiving groove; Step 23, moving the mask plate so that the mask plate covers the second part of the auxiliary containing groove and exposes the first part of the auxiliary containing groove; Step 24, controlling the substrate tray to rotate uniformly at a preset speed and growing an epitaxial layer on the substrate tray, so that a second single epitaxial layer is formed on the first single epitaxial layer of the growth substrate, and a second single reference epitaxial layer is formed on the reference substrate of the first part of the secondary receiving groove; The step 3 includes: testing the coating parameters of the first single reference epitaxial layer as detection parameters of the first single epitaxial layer, and testing the coating parameters of the second single reference epitaxial layer as detection parameters of the second single epitaxial layer.

4. The epitaxial growth detection method according to claim 3, Features: The mask plate is slidably installed on the substrate tray along a sliding track and can slide under the centrifugal force of the substrate tray to switch between blocking the first part and the second part of the auxiliary containing groove. The step 23 specifically includes: controlling the substrate tray to reduce the preset speed to 0 within a preset time, so that the shielding plate switches from blocking the first part of the auxiliary containing groove to blocking the second part of the auxiliary containing groove.

5. The epitaxial growth detection method according to claim 4, Features: The sliding track is arranged along the centrifugal direction of rotation of the substrate tray and is provided with a limit portion for limiting the mask plate from sliding from the front sliding position of the sliding track to the rear sliding position of the sliding track. The first part and the second part of the auxiliary accommodating groove are arranged from back to front along the sliding track. The mask plate slides along the sliding track between the rear sliding position and the front sliding position to switch between covering the first part of the auxiliary accommodating groove and the second part of the auxiliary accommodating groove. The contact surface between the mask plate and the sliding track is a smooth sliding surface, so that the mask plate can slide from back to front on the sliding track under the action of inertia when the substrate tray decelerates.

6. The epitaxial growth detection method according to claim 5, Features: The limiting portion includes a clamping groove which is arranged on a position on the track surface of the sliding track corresponding to the front sliding position and is concave-convexly matched with the supporting foot of the mask plate.

7. The epitaxial growth detection method according to claim 4, Features: The substrate tray is controlled to decrease its rotation speed from 600 rpm to 0 within 30 seconds, so that the shielding plate switches from shielding the first part of the auxiliary containing groove to shielding the second part of the auxiliary containing groove.

8. The epitaxial growth detection method according to claim 3, Features: The first portion and the second portion are respectively a first auxiliary accommodating groove and a second auxiliary accommodating groove which are spaced apart from each other.

9. The epitaxial growth detection method according to claim 2, Features: A mercury probe CV is used to detect the doping concentration of the reference epitaxial layer on each portion of the reference substrate, and FTIR is used to detect the thickness of the reference epitaxial layer on each portion of the reference substrate. The coating parameters include doping concentration and / or thickness.

10. The epitaxial growth detection method according to claim 2, Features: The main containing groove is arranged in the middle of the substrate tray, the auxiliary containing groove is arranged on one side of the main containing groove and close to the edge of the substrate tray, and the notch area of ​​the main containing groove is larger than the notch area of ​​the auxiliary containing groove.