AI Technical Summary
The non-stick coating on the inner pot of existing rice cookers has low hardness, poor scratch resistance, and is easy to fall off, causing food to stick to the pot and making it difficult to clean. Moreover, damage to the coating will cause metal aluminum to precipitate, which affects health and seriously affects the user experience.
The inner pot is designed with a multi-layer structure, including a base body, a transition layer, a non-stick layer and a wear-resistant particle layer. By setting a wear-resistant particle layer on the surface of the non-stick layer, the scratch resistance and wear resistance are improved while maintaining non-stick properties. Continuity and integrity of the adhesive layer.
Without destroying the continuity and corrosion resistance of the non-stick layer, it can significantly improve the scratch resistance of the inner pot, extend its service life, reduce the impact of non-stick performance, and improve production efficiency and yield.
Smart Images

Figure PI2025003398_DRAWING_001 
Figure PI2025003398_DRAWING_002 
Figure PI2025003398_DRAWING_003
Abstract
Description
[0001] Inner Pot, Cooking Utensil, and Method for Preparing an Inner Pot Technical Field This application relates to the technical field of cooking utensils, and more specifically, to an inner pot, cooking utensil, and method for preparing an inner pot. Background Art Currently, the inner pots of commercially available rice cookers commonly use non-stick coatings, such as polytetrafluoroethylene (PTFE) coatings and tetrafluoroethylene-perfluoroalkoxyvinyl aldehyde (PFA) coatings. However, non-stick coatings generally suffer from low hardness and poor scratch resistance. During use, scratches can cause the coating to fall off, rendering the non-stick properties ineffective. This can lead to food sticking to the pot and difficulty cleaning. Damage to the coating can also lead to the release of metallic aluminum, which can affect health and severely impact the customer experience. Therefore, coating shedding and wear on the inner pot of rice cookers are a common problem in the industry and a source of consumer complaints. Therefore, there is a need for an inner pot, cooking utensil, and method for preparing an inner pot to at least partially address these issues. Summary of the Invention: This summary introduces a series of simplified concepts, which will be further explained in the detailed description. This summary of the invention is not intended to limit the key features and essential technical features of the claimed technical solution, nor is it intended to determine the scope of protection of the claimed technical solution. To at least partially address the aforementioned issues, a first aspect of this application provides an inner pot for use in a cooking utensil. The inner pot comprises: a base; a transition layer attached to the inner surface of the base; a non-stick layer attached to the inner surface of the transition layer; and a wear-resistant particle layer composed of a plurality of raised particles spaced apart and attached to the inner surface of the non-stick layer. The inner pot of this application, by disposing the wear-resistant particle layer on the surface of the non-stick layer, can improve the scratch resistance of the inner pot without disrupting the continuity and integrity of the non-stick layer, that is, without affecting the corrosion resistance of the inner pot or significantly affecting its non-stick properties. Optionally, the thickness of the transition layer is 10gm-20gm. o According to this solution, the transition layer can be used as an intermediate transition to improve the firmness of the non-stick layer. Optionally, the thickness of the non-stick layer is 10gm-60gmo Thus, good non-stick performance can be obtained. Optionally, the height of the protruding particles of the wear-resistant particle layer protruding from the inner surface of the non-stick layer is 10gm-500gm o This can improve the wear resistance and the number of scratch resistance. Optionally, the height of the protruding particles of the wear-resistant particle layer protruding from the inner surface of the non-stick layer is 20gm-200gm o According to this solution, the scratch resistance can be further improved. Optionally, the height of the protruding particles of the wear-resistant particle layer protruding from the inner surface of the non-stick layer is 50gm-100gm o According to this solution, the scratch resistance can be further improved. Optionally, the diameter of the protruding particles in the wear-resistant particle layer is 10gm-500gm o Thus, the wear resistance of the wear-resistant particle layer can be improved, while the non-stick property of the non-stick layer is less affected. Optionally, the diameter of the protruding particles of the wear-resistant particle layer is 50gm-300gm o According to this solution, the scratch resistance of the wear-resistant particle layer can be further improved. Optionally, the diameter of the protruding particles in the wear-resistant particle layer is 100gm-200gm. oAccording to this solution, the scratch resistance of the wear-resistant particle layer can be further increased. Optionally, the ratio of the total contact area of the raised particles in the wear-resistant particle layer with the non-stick layer to the inner surface area of the non-stick layer is 5%-50%. This configuration can improve the wear resistance of the inner pot while minimizing the impact on non-stick properties. Optionally, the ratio of the total contact area of the raised particles in the wear-resistant particle layer with the non-stick layer to the inner surface area of the non-stick layer is 10%-30%. According to this solution, the scratch resistance of the inner pot can be improved while further minimizing the impact on non-stick properties. Optionally, the ratio of the total contact area of the raised particles in the wear-resistant particle layer with the non-stick layer to the inner surface area of the non-stick layer is 15%-25%. According to this solution, the scratch resistance of the inner pot can be improved while further minimizing the impact on non-stick properties. Optionally, the material polarity of the transition layer is less than that of the substrate, and the material polarity of the transition layer is greater than that of the non-stick layer. According to the above configuration, the material polarity of the transition layer lies between that of the substrate and the non-stick layer, enabling good adhesion between the transition layer and both the substrate and the non-stick layer, ensuring secure adhesion of the non-stick layer and reducing the likelihood of it falling off. Optionally, the material polarity of the wear-resistant particle layer is greater than that of the non-stick layer. According to this solution, the wear-resistant particle layer is made of a different material from the non-stick layer, ensuring excellent scratch resistance. Optionally, the transition layer and the non-stick layer are heat-fused. Optionally, the non-stick layer and the raised particles in the wear-resistant particle layer are heat-fused. This configuration further enhances the secure connection between the layers and improves the durability of the inner pot. Optionally, the raised particles in the wear-resistant particle layer are formed by shrinking molten wear-resistant material onto molten non-stick material, followed by cooling and solidification. This configuration ensures secure adhesion of the wear-resistant particle layer to the surface of the non-stick layer without compromising the integrity of the non-stick layer. Optionally, the interface material of the transition layer includes a material similar to the non-stick material of the non-stick layer; and the interface material of the transition layer further includes a material such that the material polarity of the transition layer is less than the material polarity of the substrate and greater than the material polarity of the non-stick layer.Optionally, the interface material of the transition layer includes polyamide-imide and at least one of polytetrafluoroethylene and tetrafluoroethylene-perfluoroalkoxyvinyl aldehyde copolymer. According to this solution, the materials are readily available, which helps improve production efficiency and reduce costs. Optionally, the non-stick material of the non-stick layer includes at least one of polytetrafluoroethylene and tetrafluoroethylene-perfluoroalkoxyvinyl aldehyde copolymer. According to this solution, the materials are readily available, which helps improve production efficiency and reduce costs. Optionally, the non-stick material is polytetrafluoroethylene, and the thickness of the non-stick layer is 10 μm to 30 μm; alternatively, the non-stick material is tetrafluoroethylene-perfluoroalkoxyvinyl aldehyde copolymer, and the thickness of the non-stick layer is 20 μm to 60 μm. o According to this solution, an excellent non-stick effect can be achieved. Optionally, the wear-resistant material of the wear-resistant particle layer includes at least one of polyols and polyarylaldehyde. According to this solution, the material is readily available, which helps improve production efficiency and reduce costs. It also allows the wear-resistant particle layer to adhere smoothly to the non-stick layer and form. Optionally, the wear-resistant material of the wear-resistant particle layer is a mixture of polyols and polyarylaldehyde, with the polyols comprising no less than 50% by weight. According to this solution, costs can be reduced. A second aspect of the present application provides a cooking utensil comprising: a pot body; an inner pot as described in the first aspect above, the inner pot being insertable and removable; and a lid, the lid being retractably attached to the pot body. When the inner pot is placed in the pot body and the lid is closed, a cooking space is formed between the lid and the inner pot. The cooking utensil according to this application includes the inner pot of the first aspect above, and thus can achieve similar technical effects as the inner pot of the first aspect. A third aspect of the present application provides a method for preparing an inner pot, for preparing the inner pot as described in the first aspect above, the method comprising:
[0002] S1: preparing the substrate;
[0003] S2: preparing a transition layer on the substrate;
[0004] S3: Preparing a non-stick layer and a wear-resistant particle layer, said S3 includes: spraying a non-stick material on the inner side of the transition layer to form a non-stick material film, spraying a wear-resistant material on the inner side of the non-stick material film to form a wear-resistant material film, heating the non-stick material film and the wear-resistant material film until they are melted together, and causing the molten wear-resistant material to shrink on the molten non-stick material, and forming a non-stick layer attached to the transition layer and a plurality of raised particles attached to the non-stick layer after cooling and solidification. According to the third aspect of the preparation method of the inner pot of the present application, it is possible to firmly attach the wear-resistant particle layer to the surface of the non-stick layer without destroying the continuity and integrity of the non-stick layer, thereby achieving the technical effect of improving the scratch resistance of the inner pot without affecting the corrosion resistance of the inner pot and without significantly affecting the non-stick property; and the non-stick layer and the wear-resistant particle layer are sintered and formed in one step, reducing the processing steps and facilitating improved production efficiency. The fourth aspect of the present application provides a preparation method of an inner pot, which is used to prepare the inner pot described in the first aspect above, and the preparation method of the inner pot includes:
[0005] S1: Prepare substrate;
[0006] S2: preparing a transition layer on the substrate;
[0007] S3: Preparing a non-stick layer and a wear-resistant particle layer, wherein S3 includes:
[0008] S31: spraying a non-stick material on the inner side of the transition layer to form a non-stick material film, heating the non-stick material film until it melts, and cooling and solidifying it to form the non-stick layer.
[0009] S32: Spraying a wear-resistant material on the inner side of the non-stick layer to form a wear-resistant material film, heating the wear-resistant material film and the non-stick layer until they are melted together, so that the molten wear-resistant material shrinks on the molten non-stick material, and after cooling and solidification, a non-stick layer attached to the transition layer and a plurality of raised particles attached to the non-stick layer are formed. According to the fourth aspect of the preparation method of the inner pot of the present application, it is possible to firmly attach a wear-resistant particle layer to the surface of the non-stick layer without destroying the continuity and integrity of the non-stick layer, thereby achieving the technical effect of improving the scratch resistance of the inner pot without affecting the corrosion resistance of the inner pot and without significantly affecting the non-stick property; and the non-stick layer and the wear-resistant particle layer are sintered and formed twice, which improves the success rate of the preparation, is conducive to improving the yield rate, and reduces production costs. Optionally, the heating temperature is 350-440°C and the heating time is 3-30 minutes. o According to this solution, it is beneficial to improve production efficiency and reduce production costs. At the same time, the above conditions are beneficial to regulating the surface tension of the molten wear-resistant material and the molten non-stick material, so that the molten wear-resistant material can better shrink on the molten non-stick material to form a firmly adhered wear-resistant particle layer. Optionally, the thickness of the non-stick material film is 10-60 rms. Optionally, the thickness of the wear-resistant material film is 5-100 rms. This facilitates the formation of raised particles with a predetermined height and diameter. Optionally, the thickness of the wear-resistant material film is 10-50 rms. This further facilitates the formation of raised particles with a predetermined height and diameter. Optionally, S1 also includes: sandblasting and / or degreasing the substrate to increase the roughness of the substrate. According to the above settings, the adhesion of the transition layer can be improved. Optionally, S2 also includes:
[0010] S21: spraying the interface material on the substrate to form an interface material film, the thickness of the interface material film is 10-20gm;
[0011] S22: Heating the interface material film at 80-200°C for 5-20 minutes to form the transition layer. According to this solution, the process is simple and the cost is low. Optionally, the wear-resistant material is constructed as a powder or an aqueous dispersion with a solid content of 20%-50%, and the particles of the wear-resistant material have a particle size of 1-5 μm. The wear-resistant material film is formed by electrostatic spraying or pressure spraying. According to the above arrangement, the process is simple, the cost is low, and the yield is high. [Note: The following figures are provided as part of the present application and are provided for understanding the present application.] The figures illustrate embodiments of the present application and their descriptions to explain the principles of the present application. In the figures: FIG1 is an enlarged schematic diagram of the structure of an inner pot according to a preferred embodiment of the present application; FIG2 is a schematic flow chart of a method for preparing an inner pot according to a preferred embodiment of the present application; and FIG3 is a schematic flow chart of a method for preparing an inner pot according to another preferred embodiment of the present application. Explanation of the Figures:
[0012] 100: Inner pot
[0013] 110: Matrix
[0014] 120: Transition layer
[0015] 130: Non-stick layer
[0016] 140: Wear-resistant particle layer
[0017] 141: Specific Implementation Methods of Raised Particles The following description provides numerous specific details to provide a more thorough understanding of the present application. However, it will be apparent to those skilled in the art that the present application can be practiced without one or more of these details. In other instances, certain technical features known in the art are not described to avoid confusion with the present application. It should be noted that the terminology used herein is intended only to describe specific embodiments and is not intended to limit the exemplary embodiments according to the present application. As used herein, unless the context clearly indicates otherwise, the singular is intended to include the plural. Furthermore, it should be understood that when the terms "comprising" and / or "including" are used in this specification, they indicate the presence of the described features, integers, steps, operations, elements, and / or components, but do not preclude the presence or addition of one or more other features, integers, steps, operations, elements, components, and / or combinations thereof. Ordinal numbers such as "first" and "second" cited in this application are merely identifiers and do not have any other meaning, such as a specific order. Moreover, for example, the term "first component" itself does not imply the presence of a "second component," and the term "second component" itself does not imply the presence of a "first component." It should be noted that the terms "upper," "lower," "front," "rear," "left," "right," "inner," "outer," and similar expressions used herein are for illustrative purposes only and are not limiting. Now, exemplary embodiments according to the present application will be described in more detail with reference to the accompanying drawings. One aspect of the present application provides a cooking appliance, which generally includes a pot body and a lid body. The pot body is substantially in the shape of a rounded rectangular parallelepiped. The pot body consists of a middle plate and an outer shell connected to the underside of the middle plate. Both can be integrally injection molded. The middle plate defines a cylindrical inner pot cavity, allowing the inner pot to be freely inserted and removed for easy cleaning. The inner pot typically has a circular opening on its top surface for holding ingredients to be heated, such as rice or soup. The pot body includes a heating device for heating the inner pot. The lid has a shape that essentially mirrors the pot body.The lid is mounted on the pot body in an openable and closable manner. Specifically, it is pivotally connected to the pot body via a pivot shaft and can freely pivot about a pivot axis on which the pivot shaft is located between a closed position and an open position relative to the pot body, facilitating closing and opening of the pot body. When the lid is closed on the pot body, it covers the inner pot and forms a cooking space between the lid and the inner pot. The cooking appliance may also include a temperature sensor, such as an upper temperature sensor disposed in the lid body and / or a lower temperature sensor disposed below the inner pot accommodating cavity. The cooking appliance may also include a lid opening button mechanism, preferably mounted on the pot body. The lid opening button mechanism is connected to a locking mechanism that locks the lid to the pot body via a transmission mechanism. When the lid opening button mechanism is pressed, the lid automatically opens. The cooking appliance includes a control device and a heating device. The control device is used to control cooking operations of the cooking appliance and may be an MCU (Micro Control Unit). The heating device is used to heat the inner pot and may be a coil. The control device is electrically connected to the heating device to control heating. Both the upper and lower temperature sensing devices are electrically connected to the control device of the cooking appliance. After sensing the temperature of the inner pot, they feed the sensed temperature signal back to the control device, enabling the control device to more accurately control the cooking process based on the temperature signal. When the inner pot is placed in the inner pot holding cavity of the pot body, the lower temperature sensing device can sense the temperature of the inner pot's bottom. For example, the lower temperature sensing device can be in direct or indirect contact with the bottom of the inner pot. Another aspect of the present application provides an inner pot 100 for a cooking appliance. Referring to Figure 1 , the inner pot 100 includes a base 110, a transition layer 120, a non-stick layer 130, and a wear-resistant particle layer 140. The transition layer 120 is attached to the inner surface of the base 110. The non-stick layer 130 is attached to the inner surface of the transition layer 120. The wear-resistant particle layer 140 is composed of a plurality of raised particles 141 spaced apart and attached to the inner surface of the non-stick layer 130. According to the inner pot 100 of the present application, by arranging multiple raised particles 141 of the wear-resistant particle layer 140 on the outer surface of the non-stick layer 130, the scratch resistance of the inner pot 100 can be improved without destroying the continuity and integrity of the non-stick layer 130, that is, without affecting the corrosion resistance of the inner pot 100 and without causing a significant impact on the non-stick property.The substrate 110 can be made of materials such as aluminum and iron, thereby providing high structural strength. The non-stick material of the non-stick layer 130 can be selected from at least one of polytetrafluoroethylene and a tetrafluoroethylene-perfluoroalkoxyvinyl aldehyde copolymer, thereby providing excellent non-stick properties. The thickness of the non-stick layer 130 is preferably 10 gm to 60 gm to achieve good non-stick properties. In an alternative embodiment, when the non-stick material is polytetrafluoroethylene, the thickness of the non-stick layer 130 is 10 gm to 30 gm. oAlternatively, when the non-stick material is tetrafluoroethylene-perfluoroalkoxyvinyl aldehyde copolymer, the thickness of the non-stick layer 130 is 20 Å-60 Å. The interface material of the transition layer 120 can be selected from at least one of polyamide-imide (PM), polytetrafluoroethylene, and tetrafluoroethylene-perfluoroalkoxyvinyl aldehyde copolymer. Selecting a material similar to the non-stick layer 130 can improve the compatibility between the transition layer 120 and the non-stick layer 130. Furthermore, the addition of polyamide-imide increases the material polarity of the transition layer 120, placing it between the polarities of the substrate 110 and the non-stick layer 130. Specifically, the material polarity of the transition layer 120 is less than that of the substrate 110, and greater than that of the non-stick layer 130. As a result, the material polarity of the transition layer 120 is between that of the substrate 110 and the non-stick layer 130, enabling good adhesion between the transition layer 120 and both the substrate 110 and the non-stick layer 130. This ensures that the non-stick layer 130 adheres securely, reducing the likelihood of detachment. Preferably, water and colorant can be added to the interface material to enhance its sprayability and assist in adjusting the material polarity. The thickness of the transition layer 120 is preferably 10 μm to 20 μm. The material polarity of the wear-resistant particle layer 140 is preferably greater than that of the non-stick layer 130. Thus, the wear-resistant particle layer 140 is made of a different material than the non-stick layer 130, ensuring that the raised particles 141 of the wear-resistant particle layer 140 have excellent scratch resistance. For example, the wear-resistant material of the wear-resistant particle layer 140 can be at least one of polyethersulfone (PES) and polyetherketoneketone (PAEK). When a mixture of PES and PAEK is used as the wear-resistant material, the proportion of PES is preferably no less than 50%. Due to the low polarity of the non-stick layer 130, it is generally difficult to place other components or parts on the non-stick layer 130. Therefore, the raised particles 141 of the wear-resistant particle layer 140 are formed by shrinking the molten wear-resistant material onto the molten non-stick material and then cooling and solidifying. This ensures that the raised particles 141 of the wear-resistant particle layer 140 are firmly attached to the surface of the non-stick layer 130 without damaging the integrity of the non-stick layer 130.In other words, the transition layer 120 and the non-stick layer 130 are thermally fused together, and the non-stick layer 130 is thermally fused together with the raised particles 141 of the wear-resistant particle layer 140. Specifically, the non-stick material has a low material polarity, while the wear-resistant material has a relatively high material polarity. In other words, the non-stick material has a low surface energy, while the wear-resistant material has a high surface energy. During preparation, after both the non-stick and wear-resistant materials are melted, the surface tension of the molten non-stick material is lower than that of the molten wear-resistant material. The molten wear-resistant material has difficulty wetting and spreading on the surface of the molten non-stick material. Consequently, the molten wear-resistant material shrinks on the surface of the molten non-stick material, forming small protrusions or spherical protrusions with smooth transition curves. After both the molten non-stick and wear-resistant materials cool and solidify, the wear-resistant particle layer 140 with multiple raised particles 141 is thermally bonded to the surface of the non-stick layer 130. The magnitude of the aforementioned material polarity can be characterized in various ways. For example, characterization can be performed by differences in the surface energy of solid materials, or by differences in their solubility parameters, or by differences in the surface tension of liquid materials, as described above. For example, contact angles can be used to characterize material polarity, surface energy, and the like. For example, if the contact angle of water on a non-stick material is greater than that on a wear-resistant material, this indicates that the surface energy of the non-stick material is less than that of the wear-resistant material. Conversely, if the contact angle of water on a non-stick material is less than that on a wear-resistant material, this indicates that the surface energy of the non-stick material is greater than that of the wear-resistant material. During testing, it is preferred that the surfaces of the non-stick material and the wear-resistant material have similar roughness. Furthermore, the height h (see FIG. 1 ) of the protruding particles 141 of the wear-resistant particle layer 140 protruding from the non-stick layer 130 is 10 gm to 500 gm, preferably 20 to 200 gm, and more preferably 50 to 100 gm. oThe diameter d (see Figure 1) of the raised particles 141 of the wear-resistant particle layer 140 is 10-500 gm, preferably 50-300 gm, and more preferably 100-200 gm. This improves wear resistance and the number of scratches. The ratio of the total contact area between the raised particles 141 of the wear-resistant particle layer 140 and the non-stick layer 130 to the inner surface area of the non-stick layer 130 is 5%-50%, preferably 10%-30%, and more preferably 15%-25%. This solution improves the scratch resistance of the inner pot 100 while further reducing the impact on non-stick properties. The wear resistance of the inner pot 100 of this application will be illustrated below using the experiments shown in Table 1. The comparative example does not include a non-stick layer 130 or a wear-resistant particle layer 140. Examples 1-8 each have different heights h and diameters d of the raised particles 141. The test procedure was as follows: The specimen was mounted on an abrasion tester, a pressure of 45 N was applied, a 0.5% detergent solution was added to the friction surface, and the friction test was repeated using a 3M-7447C scouring pad. The pad was replaced every 500 abrasions. The test was terminated when 10 white spots appeared on the substrate, large scratches were observed, or the entire substrate fell off. The maximum number of abrasions was recorded. Table 1 Another aspect of the present application further provides a method for preparing the inner pot 100, which is used to prepare the inner pot 100. The method for preparing the inner pot 100 includes:
[0018] S1: Preparing a substrate 110. Step S1 specifically includes sandblasting and / or degreasing the substrate 110 to increase its roughness. This arrangement can improve the adhesion of the transition layer 120. S2: Preparing the transition layer 120 on the substrate 110. Step S2 specifically includes: S21: Spraying an interface material onto the substrate 110 to form an interface material film having a thickness of 10-20 μm; S22: Heating the interface material film at 80-200°C for 5-20 minutes to form the transition layer 120. This solution provides a simple process and low cost.
[0019] S3: preparing a non-stick layer 130 and a wear-resistant particle layer 140. In an optional embodiment of the method for preparing the inner pot 100 of the present application, step S3 includes spraying a non-stick material on the inner side of the transition layer 120 to form a non-stick material film, spraying a wear-resistant material on the inner side of the non-stick material film to form a wear-resistant material film, heating the non-stick material film and the wear-resistant material film until they are melted together, causing the molten wear-resistant material to shrink on the molten non-stick material, and cooling and solidifying to form a non-stick layer 130 attached to the transition layer 120 and a plurality of raised particles 141 attached to the non-stick layer 130. According to the method for preparing the inner pot 100 of this optional embodiment of the present application, the wear-resistant particle layer 140 can be firmly attached to the surface of the non-stick layer 130 without destroying the continuity and integrity of the non-stick layer 130, thereby achieving the technical effect of improving the scratch resistance of the inner pot 100 without affecting the corrosion resistance of the inner pot 100 and without significantly affecting the non-stick property. In addition, the non-stick layer 130 and the wear-resistant particle layer 140 are sintered and formed in one step, reducing the processing steps and facilitating improved production efficiency. In another optional embodiment of the method for preparing the inner pot 100 of the present application, step S3 includes:
[0020] S31: spraying a non-stick material on the inner side of the transition layer 120 to form a non-stick material film, heating the non-stick material film until it melts, and cooling and solidifying it to form the non-stick layer 130.
[0021] S32: Spraying a wear-resistant material on the inner side of the non-stick layer 130 to form a wear-resistant material film, heating the wear-resistant material film and the non-stick layer 130 until they are melted together, so that the molten wear-resistant material shrinks on the molten non-stick material, and after cooling and solidification, the non-stick layer 130 attached to the transition layer 120 and the plurality of raised particles 14L attached to the non-stick layer 130 are formed. According to the preparation method of the inner pot 100 of this alternative embodiment of the present application, the wear-resistant particle layer 140 can be firmly attached to the surface of the non-stick layer 130 without destroying the continuity and integrity of the non-stick layer 130, thereby achieving the technical effect of improving the scratch resistance of the inner pot 100 without affecting the corrosion resistance of the inner pot 100 and without significantly affecting the non-stick property. In addition, the non-stick layer 130 and the wear-resistant particle layer 140 are sintered and formed twice, which improves the success rate of the preparation, is conducive to improving the yield rate, and reduces production costs. In the two preparation methods described above, the heating (or sintering) temperature is 350-440°C, and the heating (or sintering) time is 3-30 minutes. This can improve production efficiency and reduce production costs. Furthermore, these conditions facilitate adjusting the surface tension of the molten wear-resistant material and the molten non-stick material, allowing the molten wear-resistant material to shrink more effectively on the molten non-stick material to form a firmly adhered wear-resistant particle layer 140. In S3, the thickness of the sprayed non-stick material film is 10-60 μm, and the thickness of the sprayed wear-resistant material film is 5-100 μm. oThis facilitates the formation of a wear-resistant particle layer 140 with a predetermined height and diameter. The wear-resistant material is in the form of a powder or an aqueous dispersion with a solids content of 20%-50%, and the wear-resistant material particles have a particle size of 1-5 μm. The wear-resistant material film is preferably formed by electrostatic spraying or pressure spraying. This results in a simple process, low cost, and high yield. The two preparation routes described above will be described in more detail below with reference to Figures 2 and 3. Referring to Figure 2, in this preferred embodiment according to one preparation route, the substrate 110 is first pre-treated, such as by sandblasting and degreasing. The interface material is then sprayed onto the surface of the substrate 110 to form a uniform interface material film with a thickness between 10 and 20 μm. The interface material film is then dried to prepare for the next step. Preferred drying conditions include a temperature of 80°C to 200°C for 5 to 20 minutes. This forms the transition layer 120. A non-stick material is then sprayed onto the surface of the transition layer 120 to form a non-stick film of a certain thickness. When PTFE is used as the non-stick material, the preferred thickness of the non-stick film is between 10 and 30 microns. When PFA is used as the non-stick material, the preferred thickness of the non-stick film is between 20 and 60 microns. The non-stick material can be a powder coating or a liquid coating, and the spraying method can be powder electrostatic spraying, air pressure spraying, liquid electrostatic spraying, etc. Next, a primary sintering process is performed to form a dense non-stick layer 130. Preferred sintering conditions include: when PTFE is used as the non-stick material, a sintering temperature of 380°C to 440°C and a sintering time of 3 to 5 minutes; when PFA is used as the non-stick material, a sintering temperature of 380°C to 420°C and a sintering time of 5 to 30 minutes. A wear-resistant material, such as PES, is then sprayed onto the surface of the formed non-stick layer 130 to form a wear-resistant film of a certain thickness, ranging from 5 to 100 microns, preferably from 10 to 50 microns. The wear-resistant material can be a powder coating or a liquid coating, and the spraying method can be powder electrostatic spraying, liquid air pressure spraying, liquid electrostatic spraying, etc. Finally, a secondary sintering process is performed to simultaneously melt the non-stick layer (e.g., PFA) and the wear-resistant film (e.g., PES).Due to the difference in surface tension (molten PFA has a lower surface tension than molten PES), the melted PES condenses on the PFA surface, forming particles with certain protrusions. Simultaneously, the PFA and PES fuse together at the interface, forming a thermally bonded interface with strong bonding strength. As a result, the PES protrusions resist easy detachment after cooling and solidification. The secondary sintering conditions are: a sintering temperature of 350°C to 430°C and a sintering time of 3 to 20 minutes. Preferred sintering conditions are: a sintering temperature of 380°C to 400°C and a sintering time of 5 to 10 minutes. Referring to Figure 3 , in this preferred embodiment according to another preparation route, substrate 110 is first pretreated, such as by sandblasting and degreasing. Then, an interface material is sprayed onto the surface of substrate 110 to form a uniform film of the interface material, with a thickness of between 10 and 20 microns. The interface material film is then dried to prepare for the next step. Preferred drying conditions include a temperature of 80°C to 200°C for 5 to 20 minutes. This forms the transition layer 120. A non-stick material is then sprayed onto the surface of the transition layer 120 to form a non-stick film of a certain thickness. When PTFE is used as the non-stick material, the preferred film thickness is between 10 and 30 microns. When PFA is used as the non-stick material, the preferred film thickness is between 20 and 60 microns. The non-stick material can be a powder coating or a liquid coating, and the spraying method can be powder electrostatic spraying, air pressure spraying, or liquid electrostatic spraying. A wear-resistant material is then sprayed directly onto the surface of the non-stick film to form a wear-resistant film of a certain thickness, ranging from 5 to 100 microns, preferably between 10 and 50 microns. The wear-resistant material can be powder coating or liquid coating, and the spraying method can be powder electrostatic spraying, liquid air pressure spraying, liquid electrostatic spraying, etc. Finally, a single sintering process is performed to simultaneously melt the non-stick material film (such as PTFE) and the wear-resistant material film (such as PES). Due to the difference in surface tension (molten PTFE has a lower surface tension, while molten PES has a relatively higher surface tension), the melted PES condenses on the PTFE surface, forming a particle shape with certain protrusions.At the same time, the PTFE and PES fuse together at the contact surface, forming a thermally bonded interface with strong bonding strength. As a result, the PES protruding particles will not easily detach after cooling and solidification. The sintering conditions are: a sintering temperature of 380°C to 430°C, and a sintering time of 3 to 20 minutes. It should be understood that although the inner pot described herein is that of a cooking utensil, the concepts of the present invention can also be appropriately applied to other types of non-stick pans, such as non-stick woks and frying pans. The processes and steps described in all the preferred embodiments above are merely examples. Unless adverse effects occur, various processing operations may be performed in a different order from the above processes. Steps in the above processes may also be added, combined, or deleted as needed. Unless otherwise defined, technical and scientific terms used herein have the same meanings as commonly understood by those skilled in the art to which this application relates. The terms used herein are for purposes of describing specific implementations only and are not intended to limit this application. Features described in one embodiment herein may be applied alone or in combination with other features in another embodiment, unless such features are not applicable in the other embodiment or otherwise indicated. The present application has been described through the above-mentioned embodiments, but it should be understood that the above-mentioned embodiments are only for the purpose of example and explanation. The present application is not limited to the above-mentioned embodiments. According to the teachings of the present application, more variations and modifications can be made, and these variations and modifications all fall within the scope of protection claimed by the present application.
Claims
Claims 1. An inner pot (100) for a cooking utensil, characterized in that: The inner pot (100) comprises: a base (110); a transition layer (120), the transition layer (120) being attached to the inner surface of the base (110); a non-stick layer (130), the non-stick layer (130) being attached to the inner surface of the transition layer (120); and a wear-resistant particle layer (140), the wear-resistant particle layer (140) being composed of a plurality of protruding particles (141) attached to the inner surface of the non-stick layer (130) at intervals.
2. The inner pot (100) according to claim 1, characterized in that: The thickness of the transition layer (120) is 10|im-20|imo 3. The inner pot (100) according to any one of claims 1 to 2, characterized in that: The thickness of the non-stick layer (130) is 10gm-60gm o 4. The inner pot (100) according to any one of claims 1 to 3, characterized in that: The height (h) of the protruding particles (141) of the wear-resistant particle layer (140) protruding from the inner surface of the non-stick layer (130) is 10|im-500|imo 5. The inner pot (100) according to claim 4, characterized in that The height (h) of the protruding particles (141) of the wear-resistant particle layer (140) protruding from the inner surface of the non-stick layer (130) is 20 (im-200|im.
6. The inner pot (100) according to claim 5, characterized in that The height (h) of the protruding particles (141) of the wear-resistant particle layer (140) protruding from the inner surface of the non-stick layer (130) is 50|im-100|imo 7. The inner pot (100) according to any one of claims 1 to 6, characterized in that: The diameter (d) of the protruding particles (141) of the wear-resistant particle layer (140) is 10|im-500|imo 8. The inner pot (100) according to claim 7, characterized in that The diameter (d) of the protruding particles (141) of the wear-resistant particle layer (140) is 50gm-300gm o 9. The inner pot (100) according to claim 8, characterized in that The wear-resistant The diameter (d) of the protruding particles (141) of the particle layer (140) is 100gm-200gm o 10. The inner pot (100) according to any one of claims 1 to 9, characterized in that: The protruding particles (141) of the wear-resistant particle layer (140) and the non-stick layer The ratio of the total area of the contact surface of (130) to the inner surface area of the non-stick layer (130) is 5%-50%. o 11. The inner pot (100) according to claim 10, characterized in that The ratio of the total contact area of the protruding particles (141) of the wear-resistant particle layer (140) and the non-stick layer (130) to the inner surface area of the non-stick layer (130) is 10%-30%. o 12. The inner pot (100) according to claim 11, characterized in that The ratio of the total contact area of the raised particles (141) of the wear-resistant particle layer (140) and the non-stick layer (130) to the inner surface area of the non-stick layer (130) is 15%-25%.
13. The inner pot (100) according to any one of claims 1 to 12, characterized in that the material polarity of the transition layer (120) is smaller than the material polarity of the base (110), and the material polarity of the transition layer (120) is greater than the material polarity of the non-stick layer (130).
14. The inner pot (100) according to claim 13, characterized in that The transition layer (120) and the non-stick layer (130) are connected by hot melt.
15. The inner pot (100) according to any one of claims 1 to 14, characterized in that the material polarity of the wear-resistant particle layer (140) is greater than the material polarity of the non-stick layer (130).
16. The inner pot (100) according to claim 15, characterized in that The non-stick layer (130) is thermally melt-connected to the protruding particles (141) of the wear-resistant particle layer (140).
17. The inner pot (100) according to claim 16, characterized in that The raised particles (141) of the wear-resistant particle layer (140) are formed by shrinking the molten wear-resistant material on the molten non-stick material and cooling and solidifying.
18. The inner pot (100) according to any one of claims 1 to 17, characterized in that the interface material of the transition layer (120) comprises a material similar to the non-stick material of the non-stick layer (130); and the interface material of the transition layer (120) further comprises The material polarity of the transition layer (120) is smaller than the material polarity of the substrate (110) and larger than the material polarity of the non-stick layer (130).
19. The inner pot (100) according to claim 18, characterized in that The interface material of the transition layer (120) includes polyamide-imide, and at least one of polytetrafluoroethylene and tetrafluoroethylene-perfluoroalkoxyvinyl aldehyde copolymer.
20. The inner pot (100) according to any one of claims 1 to 19, characterized in that the non-stick material of the non-stick layer (130) includes at least one of polytetrafluoroethylene and tetrafluoroethylene-perfluoroalkoxyvinyl aldehyde copolymer.
21. The inner pot (100) according to claim 20, characterized in that The non-stick material is polytetrafluoroethylene, and the thickness of the non-stick layer (130) is 10|im-30|im; or the non-stick material is tetrafluoroethylene-perfluoroalkoxyvinyl aldehyde copolymer, and the thickness of the non-stick layer (130) is 20|im-60|im 22. The inner pot (100) according to any one of claims 1 to 21, characterized in that the wear-resistant material of the wear-resistant particle layer (140) includes at least one of polyols and polyarylaldehyde.
23. The inner pot (100) according to claim 22, characterized in that The wear-resistant material of the wear-resistant particle layer (140) is a mixture of polyols and polyarylaldehyde, wherein the mass proportion of the polyols is not less than 50%.
24. A cooking utensil, characterized in that: include: pot body; According to the inner pot (100) according to any one of claims 1 to 23, the inner pot (100) can be placed in and taken out of the pot body; the cover body can be opened and closed on the pot body, and when the inner pot (100) is placed in the pot body and the cover body covers the pot body, a cooking space is formed between the cover body and the inner pot (100).
25. A method for preparing an inner pot (100), for preparing the inner pot (100) according to any one of claims 1 to 23, characterized in that: The preparation method of the inner pot (100) comprises: S1: preparing a substrate (110); 18 S2: preparing a transition layer (120) on the substrate (110); S3: preparing a non-stick layer (130) and a wear-resistant particle layer (140), said S3 comprising: spraying a non-stick material on the inner side of the transition layer (120) to form a non-stick material film, spraying a wear-resistant material on the inner side of the non-stick material film to form a wear-resistant material film, heating the non-stick material film and the wear-resistant material film until they are melted together, and allowing the melted wear-resistant material to shrink on the melted non-stick material, and forming a non-stick layer (130) attached to the transition layer (120) and a plurality of protruding particles (141) attached to the non-stick layer (130) after cooling and solidification.
26. A method for preparing an inner pot (100), for preparing the inner pot (100) according to any one of claims 1 to 23, characterized in that: The preparation method of the inner pot (100) comprises: S1: preparing a substrate (110); S2: preparing a transition layer (120) on the substrate (110); S3: preparing a non-stick layer (130) and a wear-resistant particle layer (140), said S3 comprising: S31: spraying a non-stick material on the inner side of the transition layer (120) to form a non-stick material film, heating the non-stick material film until it melts, and cooling and solidifying it to form the non-stick layer (130). S32: spraying a wear-resistant material on the inner side of the non-stick layer (130) to form a wear-resistant material film, heating the wear-resistant material film and the non-stick layer (130) until they are melted together, so that the melted wear-resistant material shrinks on the melted non-stick material, and after cooling and solidification, forming a non-stick layer (130) attached to the transition layer (120) and a plurality of protruding particles (141) attached to the non-stick layer (130) 27. The method for preparing the inner pot (100) according to claim 25 or 26, characterized in that: The heating temperature is 350-440°C and the heating time is 3-30 minutes.
28. The method for preparing the inner pot (100) according to any one of claims 25 to 27, characterized in that: The thickness of the non-stick material film is 10-60 ^ 1; the thickness of the wear-resistant material film is 5-100gm o 29. The method for preparing the inner pot (100) according to claim 28, characterized in that: The thickness of the wear-resistant material film is 10-50mm.
30. The method of manufacturing the inner pot (100) according to any one of claims 25 to 29 19 Preparation method, characterized in that, Said S1 further comprises: performing sandblasting and / or degreasing treatment on said substrate (110) to increase the roughness of said substrate (110).
31. The method for preparing the inner pot (100) according to any one of claims 25 to 30, characterized in that: Said S2 further comprises: S21: spraying an interface material on said substrate (110) to form an interface material film, wherein the thickness of said interface material film is 10-20 μm; S22: heating the interface material film at 80-200° C. for 5-20 minutes to form the transition layer (120).
32. The method for preparing the inner pot (100) according to any one of claims 25 to 31, characterized in that: The wear-resistant material is in the form of powder or a water dispersion with a solid content of 20%-50%, and the particle size of the wear-resistant material particles is 1-5 μm. The wear-resistant material film is formed by electrostatic spraying or pressure spraying. 20