Device and method for splitting a semiconductor wafer

MYPI2025004310A0Undetermined Publication Date: 2024-07-20INFINEON TECHNOLOGIES AG
View PDF 0 Cites 0 Cited by

Patent Information

Application Number
MYPI2025004310
Authority / Receiving Office
MY · MY
Patent Type
Applications
Current Assignee / Owner
Priority Date
2023-01-20
Filing Date
2024-01-17
Publication Date
2024-07-20

AI Technical Summary

Technical Problem

The existing methods for splitting semiconductor wafers, such as sawing, result in significant material loss and surface damage, and handling polymer films can be challenging, especially for costly materials like silicon carbide (SiC).

Method used

A device comprising a polymer and a frame, where the polymer undergoes a partial glass transition when cooled below a critical temperature, is used to attach and split semiconductor workpieces. The polymer is configured to be elastic above the critical temperature and has a surface for attaching the workpiece, with a second region that remains above the critical temperature to mitigate forces on the frame, reducing material loss and surface damage.

Benefits of technology

This method effectively reduces material loss and surface damage during wafer splitting, allowing for efficient production of semiconductor wafers with improved handling and processing capabilities.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure PI2025004310_DRAWING_001
    Figure PI2025004310_DRAWING_001
  • Figure PI2025004310_DRAWING_002
    Figure PI2025004310_DRAWING_002
  • Figure PI2025004310_DRAWING_003
    Figure PI2025004310_DRAWING_003
Patent Text Reader

Abstract

A device for holding a semiconductor work piece in a splitting process is disclosed. The device comprises a polymer and a frame. The frame is connected with the polymer and surrounding the polymer. The polymer is configured to undergo at least a partial glass transition when being cooled below a critical temperature, and to be elastic when having a temperature above the critical temperature. The polymer comprises a first region having a surface to which a semiconductor work piece can be attached.
Need to check novelty before this filing date? Find Prior Art

Description

[0001] DEVICE AND METHOD FOR SPLITTING A SEMICONDUCTOR WAFER

[0002] BACKGROUND

[0003] Wafer costs make up a significant ratio of the overall production costs of silicon carbide (SiC) semiconductor devices. Typically, wafers are obtained from a solid-state material in the form of a block, which is referred to as a boule or ingot Pieces can be obtained from such ingots (or boules), for example, by means of a sawing method. These pieces may already constitute a wafer, or the pieces obtained are divided further until they have the desired thickness of a wafer to be produced. In the sawing method, wire saws (e.g., made of diamond) are typically used, which can result in loss of a portion of up to 50% of the original solid-state material referred to as “kerf loss”, which may be disadvantageous in the case of costly starting solid- state materials.

[0004] Moreover, the sawing operation can cause damages on the wafer surface, which may need to be remedied, e.g., by additional process steps for surface treatment such as lapping or polishing steps. As an alternative, a splitting method can be used for the division of a boule into a wafer and a smaller boule (i.e., a wafer can be directly split from the boule) and / or for the division of a thick wafer into two thin wafers. In examples, a polymer film is used to facilitate the splitting. However, in some applications, handling the polymer film may be challenging.

[0005] SUMMARY

[0006] According to an embodiment, a device for holding a semiconductor work piece in a splitting process comprises the polymer and a frame. The semiconductor work piece may comprise or may be a semiconductor boule or a semiconductor wafer. The frame may be connected with the polymer. The frame surrounds the polymer. The polymer may be configured to undergo at least a partial glass transition when being cooled below a critical temperature, and to be elastic when having a temperature above the critical temperature. The polymer comprises a first region having a surface to which a semiconductor work piece can be attached.

[0007] According to an embodiment, the frame and / or the polymer comprises at least one attachment element, wherein the polymer is directly attached to the frame via the at least one attachment element. Thereby, the polymer and the frame may be connected.

[0008] According to an embodiment, the device may further comprise a foil, wherein the foil is fixedly attached to the polymer and the frame thereby connecting the polymer and the frame. The frame may be a wafer ring (sometimes also referred to as “wafer frame”), and the foil may be a dicing foil. The foil may be attached to the polymer at a surface of the polymer opposite to the surface to which a semiconductor work piece can be attached.

[0009] According to some embodiments, a thickness of the polymer in the first region is at least 2 mm, or at least 2.5 mm. For example, a thickness of the polymer in the first region may be in between at least 2 mm and at most 4 mm, or in between at least 2.5 mm and at most 3.5 mm.

[0010] In some embodiments, the polymer is directly attached to the frame thereby connecting the polymer and the frame.

[0011] According to an embodiment, the polymer comprises a second region which does not overlap with the first region of the polymer and which surrounds the first region of the polymer.

[0012] In some embodiments, the surface of the polymer to which a semiconductor work piece can be attached (so-called “functional surface”) may have a surface roughness of at least 0.1 pm and at most 2 pm (or at least 0.1 pm and at most 1 pm or at least 0.2 pm and at most 0.8 pm). The surface roughness may generally be the arithmetical mean height (Sa). A surface of the polymer opposite to the functional surface (e.g., a backside surface of the polymer and / or, if applicable, the surface to which the foil is attached) may have the same surface roughness as the functional surface or may have a higher surface roughness, For example, the surface roughness of the surface of the polymer opposite to the functional surface may be at least 1 pm and at most 10 pm (or at least 2 pm and at most 8 pm or at least 2 pm and at most 5 pm). If the polymer comprises a second region, the surface of the polymer in the second region adjoining the functional surface may have the same surface roughness as the functional surface or may have a higher surface roughness. For example, the surface roughness of the surface of the polymer in the second region adjoining the functional surface may be at least 1 pm and at most 10 pm (or at least 2 pm and at most 8 pm or at least 2 pm and at most 5 pm).

[0013] In some embodiments, a surface of the second region has substantially a ring shape or a loop shape. The inner circle of the ring may be given by the surface of the first region. The diameter of the outer circle of the ring may be at least 16 cm or at least 18 cm or at least 22 cm.

[0014] In general, a diameter of the polymer, e.g. an outer circle of the second region or the diameter of the first region in the case of no second region, may be at least 95% or at least 105% and / or at most 110% or at most 120% of a diameter of the semiconductor work piece. In some examples, the diameter of the polymer may be at least 3 mm or at least 4 mm or at least 5 mm larger than the diameter of the semiconductor work piece. In an embodiment, the frame comprises a flexible ring wherein the flexible ring substantially has a circular shape with a first diameter. In one or more embodiments, the flexible ring comprises three or more ring elements and corresponding three or more flexible attachment elements, each flexible attachment element connects two respective ring elements of the three or more ring elements with each other to form the flexible ring. When a force is applied to the flexible ring that points towards the center of the flexible ring, the flexible attachment elements are contracted so that the flexible ring substantially has a circular shape with a second diameter, the second diameter being smaller than the first diameter.

[0015] In an embodiment, the frame further comprises an outer ring. The flexible ring may be removably attached to the outer ring. In this context, “removably attached” may refer to a connection that can be released (e.g., mechanically released) without destroying the outer ring and the flexible ring.

[0016] In some embodiments the device for attaching the polymer to the semiconductor work piece is used in a splitting process.

[0017] According to an embodiment, a method of splitting a semiconductor work piece comprises attaching the semiconductor work piece to a first region of a surface of a device. Optionally, a separation region may be formed within the semiconductor work piece. The device comprises a polymer and a frame, wherein the frame is connected with the polymer and surrounding the polymer. The polymer is configured to undergo at least a partial glass transition when being cooled below a critical temperature and to be elastic when having a temperature above the critical temperature. The polymer comprises the surface. The method further comprises cooling the work piece together with the first region of the device to a temperature below the critical temperature.

[0018] In an embodiment, the surface of the polymer comprises a second region which does not overlap with the first region of the surface. During the cooling, at least a portion of the second region remains at a temperature that is above the critical temperature

[0019] In one or more embodiments, the semiconductor work piece is attached to the device such that an outer surface of the boule is placed on the device, the outer surface having a smaller distance to a separation region within the semiconductor work piece as compared to a surface of the semiconductor work piece opposite the outer surface.

[0020] In an embodiment, a device for holding a semiconductor work piece in a splitting process, comprises a polymer and a frame, wherein the frame is directly connected with the polymer and surrounding the polymer, the polymer is configured to undergo at least a partial glass transition when being cooled below a critical temperature, and to be elastic when having a temperature above the critical temperature, wherein the polymer comprises a surface to which a semiconductor work piece can be attached, and wherein the polymer having a diameter of at least 16 cm or at least 18 cm.

[0021] Those skilled in the art will recognize additional features and advantages upon reading the following detailed description, and upon viewing the accompanying drawings.

[0022] BRIEF DESCRIPTION OF THE DRAWINGS

[0023] The present disclosure is illustrated by way of example, and not by way of limitation, in the figures of the accompanying drawings in which like reference numerals refer to similar or identical elements. The elements of the drawings are not necessarily to scale relative to each other. The features of the various illustrated examples can be combined unless they exclude each other.

[0024] Figures 1A through 1 E illustrate cross-sectional views of a semiconductor wafer during different stages of a wafer splitting process, according to an embodiment.

[0025] Figure 2 illustrates a portion of a separation region formed within the semiconductor substrate and which includes microscopic cracks that are at least partially disconnected from one another within the separation region.

[0026] Figure 3A illustrates a plot of storage modulus versus temperature for a polymer used during the wafer splitting process and which does not contain fillers.

[0027] Figure 3B illustrates a plot of storage modulus versus temperature for the polymer in Figure 3A with one or more fillers contained in the polymer.

[0028] Figure 4A illustrates a side view of a device that can be used during the process of wafer splitting, according to an embodiment.

[0029] Figures 4B and 4C illustrate a top view of embodiments of the device shown in Figure 4A.

[0030] Figure 5A illustrates a side of a device that can be used during the process of wafer splitting, according to an embodiment.

[0031] Figure 5B illustrates a side view of a device that can be used during the process of wafer splitting according to an embodiment. Figure 5C illustrates a top view of the devices shown in Figures 5A and 5B.

[0032] Figure 6 illustrates a further embodiment regarding the frame shown in Figures 4A to 5C.

[0033] Figure 7 illustrates a semiconductor wafer or boule placed on a device as shown in Figures 4A to 6.

[0034] Figure 8 illustrates a method in which the device according to Figures 4A to 7 can be used.

[0035] DETAILED DESCRIPTION

[0036] Notably, modifications and other embodiments of the disclosed invention(s) will come to mind to one skilled in the art having the benefit of the teachings presented in the foregoing descriptions and the associated drawings. Therefore, it is to be understood that the invention(s) is / are not to be limited to the specific embodiments disclosed and that modifications and other embodiments are intended to be included within the scope of this disclosure. Although specific terms may be employed herein, they are used in a generic and descriptive sense only and not for purposes of limitation.

[0037] The present disclosure relates to a splitting process of a semiconductor work piece and to devices that may be used in such a process. A semiconductor work piece may be or may comprise a semiconductor boule (also called “ingot”) or a semiconductor wafer. While emphasis is placed on work pieces comprising or consisting of SiC as a material (and SiC devices produced using SiC wafers), the embodiments described herein are not intended to be limited to SiC wafers and may be used with other semiconductor wafer technologies such as silicon (Si), gallium arsenide (GaAs), gallium nitride (GaN), sapphire, etc.

[0038] In some embodiments, the splitting techniques described herein may be applied to splitting semiconductor wafers from a semiconductor boule. The splitting techniques described herein may be applied to splitting semiconductor wafers from a semiconductor boule by forming a separation region within a semiconductor boule, the separation region having at least one altered physical property which increases thermo-mechanical stress within the separation region relative to the remainder of the semiconductor boule. For example, thermo-mechanical stress may be increased within the separation region by focusing laser radiation at a targeted position within the semiconductor boule. An external force may then be applied to the semiconductor boule such that at least one crack propagates along the separation region and a wafer splits from the semiconductor boule. For example, an external force is applied to the semiconductor boule by applying a polymer to the semiconductor boule, the polymer having a CTE different from a CTE of the semiconductor boule. The polymer and the semiconductor boule are subjected to a temperature process during which the polymer imparts mechanical stress to the semiconductor boule. The process may be applied multiple times to yield a plurality of wafers from a single semiconductor boule.

[0039] In other embodiments, device structures are produced in a base semiconductor wafer and the base wafer is subsequently split into a thinner device wafer, which includes the device structures, and a thinner reclaimed wafer. The reclaimed wafer may be processed and further devices may be produced within the reclaimed wafer.

[0040] The wafer splitting technique described herein includes at least two main steps: (i) forming a separation region within a semiconductor work piece (e.g. a boule or a wafer) and which has at least one altered physical property which increases thermo-mechanical stress within the separation region relative to the remainder of semiconductor work piece; and (ii) applying an external force to the semiconductor work piece such that at least one crack propagates along the separation region and a semiconductor wafer splits from the semiconductor work piece (or the semiconductor work piece splits into two separate wafers or a thinner semiconductor wafer splits from the semiconductor work piece).

[0041] In some embodiments, forming the separation region includes forming microscopic cracks that are at least partially disconnected from one another within the separation region. The microscopic cracks connect to one another in response to the external force applied to the semiconductor workpiece (such as a boule or a semiconductor wafer), forming the at least one crack which propagates along the separation region and which splits the semiconductor wafer from the boule (or splits the semiconductor wafer into two separate pieces). The external force applied to the semiconductor workpiece may involve application of a polymer layer.

[0042] Described next are various embodiments of the semiconductor splitting process. The following disclosure is directed to splitting a semiconductor wafer into two separate semiconductor wafers. The same process may be applied for splitting a semiconductor wafer from a boule if not indicated otherwise. In that case, the semiconductor wafer 100 shown in the following Figures corresponds to the boule.

[0043] Figures 1A through 1 E illustrate cross-sectional views of a semiconductor workpiece 100 during different stages of the splitting process, according to an embodiment. As explained above, the semiconductor workpiece 100 may be any type of wafer used to produce semiconductor devices. For example, the semiconductor workpiece may be a SiC wafer or SiC boule such as 4H-SiC and may have a thickness (T_wafer) which may vary depending on wafer diameter. Typically, 4 inch and 6 inch (150 mm) SiC wafers have a thickness of 350 pm (microns) with an accuracy of, e.g., at most ± 40 pm or at most ±25 pm. For larger SiC wafer diameters (e.g. an 200 mm and / or 8 inch SiC wafer), the thickness may be higher. For example, the thickness of a 200 mm wafer may be 500 pm (± 40pm or ±25pm). The wafer splitting process described herein may also be used with other SiC polytypes and / or other semiconductor materials, as explained above (e.g., Si, GaAs, GaN, sapphire, etc.), with corresponding adaptations of the process parameters.

[0044] Figure 1 A is an optional processing step that might not be present according to the present disclosure. In particular, Figure 1A shows the semiconductor workpiece 100 after one or more epitaxial layers 102 are formed on the semiconductor workpiece 100, device structures 104 are formed in the one or more epitaxial layers 102, a metallization layer and / or a passivation layer 106 (e.g., at least one passivation layer) is formed over the device structures 104, and a carrier 108 is attached to the semiconductor workpiece 100 with the one or more epitaxial layers 102. Layer 106 is shown in the cross-sectional view as a continuous layer, but instead may be discontinuous. For example, in the case of a passivation layer, layer 106 may be present only above the device structures 104. In the case of a metallization layer, layer 106 may be patterned. The carrier 108 protects the device structures 104 from damage and mechanically stabilizes the semiconductor workpiece 100 during and / or after the splitting process. In some examples, an additional layer 118 may be foreseen between the layer 106 and the carrier 108.

[0045] Doping regions 110, 112, 114 of the device structures 104 are produced by implantation with subsequent annealing steps or by doping during the epitaxial process. For example, a first deposited epitaxial layer 114 may be an n-doped drain or emitter layer with a thickness ranging, e.g., between 10 pm and 50 pm for power MOSFET (metal-oxide-semiconductor field effect transistors) or power diode devices, or a p-doped emitter layer for IGBT (insulated gate bipolar transistor) devices. A second epitaxially deposited layer (not shown) may be deposited as a buffer layer for preventing punch-through of the space charge layer towards the emitter I drain layer 114. The thickness of the buffer layer is typically 1 pm to 40 pm or 2 pm to 30 pm. A n- type drift zone layer 112 may then be deposited by an epitaxial technique. The thickness of the drift zone layer 112 depends on the target breakdown voltage (for 1200 V devices typically in the range between 8 pm and 12 pm and for 3.3. kV devices between 25 pm and 35 pm). The doping level of the drift zone layer 112 also may be adjusted according to the desired breakdown voltage (for 1200 V devices typically about 1016 cm-3 and for 3.3 kV devices a few times 1015 cm-3). Front side device structures 110, such as p-body and source regions for power MOSFETs or IGBTs or p-emitter for power diodes, may be formed by masked ion implantation with subsequent annealing steps. For switchable devices, a gate structure is also realized in the form of planar or trench-based gates.

[0046] After device formation, the semiconductor workpiece 100 has a front side with the device structures 104 and a front side metallization layer and / or passivation layers 106. The device structures 104 may be structures of a semiconductor device, for example a MEMS (microelectromechanical systems) and / or a MOEMS (micro-opto-electro-mechanical system) device, a diode such as an MPS (merged-pin-Schottky) diode, Schottky diode, MOS-gated diode, etc. or a transistor device such as a MOSFET, JFET (junction FET), IGBT, fin-FET, thyristor, etc. or a combination thereof. If the device structures 104 include a Schottky contact, the front side metallization layer 108 may include a Schottky contact metal. In addition, or as an alternative in the case of no Schottky contact, the front side metallization layer 108 may include an Ohmic contact metal.

[0047] In another embodiment, the semiconductor workpiece 100 may not be processed according to the above disclosure before the splitting and the process may start with forming the separation region 116, as disclosed in the following in connection with Figures 1 B to 1 E. In that case, the semiconductor workpiece 100 does not include the one or more epitaxial layers 102, the device structures 104, the layer 106, the carrier 108, the doping regions 110, 112, 114, and the additional layer 118 before the splitting starts. In other words, in this embodiment, the raw semiconductor workpiece may be split into two semiconductor pieces. The same holds for splitting a semiconductor wafer from a boule, where the boule may not be processed according the disclosure given with respect to Figure 1A. In this case, the splitting process may directly start with Figure 1 B, as described in the following.

[0048] Figure 1 B shows the semiconductor workpiece 100 after forming a separation region 116 within the semiconductor workpiece 100. The separation region 116 has at least one altered physical property which increases thermo-mechanical stress within the separation region 116 relative to the remainder of the semiconductor workpiece 100. The separation region 116 allows for splitting of the semiconductor workpiece 100 at a defined position. The separation region 116 may extend along horizontal directions of the wafer. Otherwise, the splitting would take place at a random position that may be influenced by crystal damages, etc. . The well- defined separation region 116 may reduce material losses (also referred to as kerf loss) during wafer splitting. A thickness (t_sep) of the separation region 116 may define the kerf loss. For example, losses may originate from the vertical extent of the microscopic cracks and additional losses due to chemical, mechanical, electrochemical and / or plasma material removal. In case the front side of the semiconductor workpiece is processed, as, e.g., shown in Figure 1A, the position of the separation region 116 may be chosen such that, after defining the device structures 104, the distanceed 1 ’ to the front side of the semiconductor workpiece 100 with the one or more epitaxial layers 102 is sufficiently high to allow for mechanical handling of the thinner device wafer which results from the splitting process, and such that the distance d1 to the front side is sufficiently low and therefore the distance ‘d2’ to the backside is sufficiently high so that the reclaimed wafer which results from the splitting process may still be processed. In case the semiconductor workpiece 100 is processed according to Figure 1A, the separation region 116 is close to the interface between the wafer 100 and the first deposited epitaxial layer 114 (substrate / drain layer for power MOSFETs or substrate / emitter layer for diodes). Typically, the distance between the separation region 116 and the interface between the wafer 100 and the first deposited epitaxial layer 114 is less than 10 pm or even less than 4 pm or even less than 2 pm. In case the semiconductor workpiece is not processed according to Figure 1A, the distances ‘dT and ‘d2’ may be chosen according to need, e.g., ‘dT and ‘d2’ are equal. In particular, the distances ‘dT and ‘d2’ may define the thickness of the two semiconductor pieces after the splitting. In case a semiconductor wafer is split from a boule, the distance ‘d may be chosen to be substantially the thickness of the semiconductor wafer that is to be split from the boule (taking into account the losses that arise during the splitting). The thickness of the semiconductor wafer may vary according to circumstances and may depend on the future use of the semiconductor wafer (typical thicknesses are, e.g., 100 pm to 500 pm or 50 pm to 600 pm).

[0049] In general, thermo-mechanical stress may be increased within the separation region 116 compared to the remainder of the semiconductor workpiece 100, thus simplifying splitting of the semiconductor workpiece 110 into a device wafer and a reclaimed wafer, e.g., by applying mechanical force

[0050] In one embodiment, the separation region 116 is formed by damaging the material of the semiconductor workpiece 100 at a targeted position. For example, in the case of SiC as the wafer material, the SiC material may be damaged. In some cases, SiC may be at least partially decomposed, for instance, into Si and C. This may be done, e.g., by creating a plasma in the SiC material at the targeted position within the semiconductor workpiece 100. At least some of the atoms in the plasma may reform to carbon clusters and silicon material, e.g., in the form of amorphous carbon and / or amorphous silicon. In addition or as an alternative, at least some of the atoms may re-crystal I ize, semi-crystallize and / or re-organize, for example to at least one polytype of SiC (e.g., 4H-SiC, 6H-SiC, or 3C-SiC) or amorphous SiC where both Si and C phases are amorphous. In some examples, the separation region 106 may comprise at least one of crystalline portions of at least one polytype of SiC or silicon or carbon (e.g., in the form of microcrystalline), amorphous portions of SiC or silicon or carbon, and / or cavities.

[0051] In one embodiment, a plasma is created in the material at the targeted position within the semiconductor workpiece 100 by focusing laser radiation at the targeted position within the semiconductor workpiece 100. The semiconductor workpiece 100 may be irradiated through the backside opposite the device structures 104 or through the front side with (or without) the device structures 104, and focused to a well-defined region within the wafer 100 to ignite a plasma within the wafer 100 and which decomposes the laser irradiated semiconductor material into its constituent components. For example, in the case of SiC, laser irradiated SiC decomposes as follows: SiC — > Si + C. The interaction with the laser radiation may result in a different material phase, e.g., as described above, and / or in microscopic cracks within the semiconductor workpiece 100. In case the device structures 104 are already present (such as when the process begins with Figure 1A), irradiating the semiconductor workpiece 100 with laser radiation through the front side may be done before producing the front side metallization 106, since the metallization 106 may not be transparent for laser radiation.

[0052] If the separation region 116 has already been pre-defined, e.g., by implantation as explained above briefly and as explained below in more detail, the laser radiation that is applied to the separation region 116 may be in a resonant regime where single-photon processes (e.g., single-photon absorption) dominate, i.e., a probability of multi-photon processes is small (e.g. at least ten times smaller than the probability of a single-photon process). In the resonant regime, the band gap of the material within the separation region 116 may be, e.g., in the range of the photon energy of the laser radiation (e.g. with a detuning of at most ±5% or at most ±1 % or at most ±0.1% or at most ±0.01% of the band gap, depending on the laser energy). The laser radiation may be absorbed in the separation region 116 and may lead to further damage of the separation region 116 (e.g. decomposition of SiC in the case of a SiC wafer 100), such that no or only a small mechanical force is needed to split the semiconductor workpiece 100 at the separation region 116.

[0053] The separation region 116 may be defined, or in the case of a pre-defined layer previously formed, e.g., by ion implantation, further defined, by focusing laser radiation to a well-defined region such as a region with at most the targeted thickness, e.g. at most 50% of the targeted thickness, of the separation region 116 within the semiconductor workpiece 100. In this case, the laser radiation may be in an off-resonant regime such that a probability of single-photon processes in the separation region 116 is small and mostly multi-photon processes (in particular, multi-photon absorption) may have to be accounted for. For example, the off- resonant regime may be achieved if the band gap of the separation region 116 is larger than (e.g., at least twice of or at least ten times of) the photon energy of the laser radiation. In the case of a multi-photon process, damage creation may be further supported by a pre-defined layer (e.g., formed by ion implantation) that increases absorption within the region where the focal point of the laser radiation is positioned.

[0054] The laser radiation may be pulsed laser radiation. The parameters of the laser radiation such as pulse duration, repetition rate, pulse energy, intensity, wavelength, pulse shape, polarization, etc. are interconnected and may be optimized according to a specific application or requirement. For example, the laser radiation may have a pulse duration of 100 fs to 100 ns (e.g. 50 ps to 10 ns), a repetition rate of 10 kHz to 10 MHz, a pulse energy of 100nJ to 50pJ, and a peak wavelength of 400nm to 2100nm (e.g., 900 nm to 1200 nm).

[0055] The laser radiation may be applied along laser lines (also referred to as scribe lines) that run essentially parallel to one another. For each laser line, a laser beam is scanned along the line. The speed of the laser scanning may be so fast that neighboring single laser shots can be distinguished, e.g. do not overlap. Here, a single laser shot may correspond to the damage created by a single pulse of laser radiation as shown in Figure 2.

[0056] In Figure 2, which shows a small section of the separation region 116, the dashed ovals labelled ‘A’ correspond to locations of individual I single laser shots. At each single laser shot location ‘A’, material of the separation region 116 is decomposed and microscopic cracks appear that extend along a crystal plane of the material of the wafer as indicated by the additional microscopic cracks labelled ‘B’ and ‘C’. The microscopic cracks ‘A’, ‘B’, ‘C’ formed within the separation region 116 are at least partially disconnected from one another. The microscopic crack labelled ‘C’ is produced by tensions between other microscopic cracks ‘A’ and not directly formed by a laser shot. For 4H-SiC, the growth direction of the semiconductor workpiece 100, which corresponds to the vertical direction along which the wafer 100 has a thickness T_wafer, may be slightly tilted to the main crystal axis, typically by 4° (also referred to as off-axis angle). Therefore, the crystal planes are tilted.

[0057] If the separation region 116 were to have only a single large crack, which would be planar but tilted, the separation region 116 would be tilted by 4° with respect to the lateral directions (i.e. , the directions perpendicular to the vertical direction). Along the entire diameter of the semiconductor workpiece 100 this would result in rather large losses. Accordingly, for SiC, the splitting process may be useful for 4H-SiC if the separation plane is not planar but has a zig- zag shape I saw-tooth shape. The microscopic cracks ‘A’, ‘B’, ‘C’ are subsequently connected to enable splitting of the semiconductor workpiece 100, as described in more detail further below.

[0058] In addition or alternatively to damaging the semiconductor workpiece 100 by laser radiation to form the separation region 116, the material of the semiconductor workpiece 100 may be damaged at the targeted position by implanting ions into the semiconductor workpiece 100 at a depth corresponding to the targeted position within the wafer 100 to produce and / or predefine the separation region 116. The ions may result directly in higher absorption, e.g., due to higher absorption rate in the separation region 116 where the majority of implanted ions reside. In the case of SiC as the material of the semiconductor workpiece 100, the ions may lead to conversion of the crystal structure of the SiC wafer into a different material, for example into a different poly-type (e.g., from 4H-SiC to 3C-SiC) and / or into a different crystallinity and / or into amorphous SiC and / or into silicon and carbon (amorphous or crystalline), such that the absorption coefficient at the wavelength of the laser radiation is increased in the separation region 116. The ions may also result in decomposition of the material of the semiconductor workpiece 100 in the separation region 116.

[0059] In one embodiment, the ions may be selected from the group consisting of nitrogen ions, phosphorus ions, hydrogen ions, and helium ions. For example, atoms such as nitrogen and / or phosphorus atoms may be implanted into the separation region 116, with an implantation dose resulting in an amorphous layer and / or or cavities being created. In addition or alternatively, helium ions or protons may be implanted to create a local damaged layer within the separation region 116. Light ions such as helium and hydrogen penetrate more deeply in the semiconductor workpiece 100 as compared to heavier ions for the same energy, increasing the depth of the separation region 116 if desired. Light ions like helium and hydrogen may create vacancy clusters and damaged layers preferentially in the end-of-range of the implantation so that the splitting process can be facilitated in this region. Phosphorous and / or nitrogen are suitable for realizing highly damaged layers in SiC. In the case of phosphorous and / or nitrogen, the implantation dose may be chosen such that an amorphous layer and / or cavities are created in the separation region 116. Optionally, channelling may be exploited during implantation which results in a lower surface damage of the surface into which the implantation is performed. The ions may be implanted before the one or more epitaxial layers 102 are formed. For example, the ions may be implanted through the surface of the semiconductor workpiece 100 onto which the one or more epitaxial layers 102 are to be formed. In case the device structure is produced before the splitting (e.g., according to the disclosure given by Figure 1A), the device structures 104 may be produced after ion implantation. After or before producing the device structures 104, laser radiation as described above may be irradiated through the semiconductor workpiece 100, with the focal point being roughly positioned at the implantation layer. The ions and / or the semiconductor material that has been converted by the ions will have an increased absorption compared to the rest of the wafer 100, thus improving the decomposition of, e.g., SiC into Si and C by an enhanced local heating of the wafer 100. For example, a combination of a multi-photon and single-photon processes may take place within the pre-defined ion implantation layer in order to increase the thermomechanical stress within the separation region 116 relative to the remainder of the semiconductor workpiece 100.

[0060] In one embodiment, the separation region 116 is formed by both laser irradiation and ion implantation of the semiconductor workpiece 100. Particularly, the material of the semiconductor workpiece 100 may be damaged at the targeted position within the semiconductor workpiece 100 by implanting ions into the semiconductor workpiece 100 at a depth corresponding to the targeted position within the wafer 100. After the ions are implanted, laser radiation is then focussed at the targeted position within the semiconductor workpiece 100. According to this embodiment, the implanted ions increase an absorption coefficient in the separation region 116 at a wavelength of the laser radiation which further increases the thermo-mechanical stress within the separation region 116 relative to the remainder of the semiconductor workpiece 100.

[0061] After formation of the separation region 116, an external force is applied to the semiconductor workpiece 100 such that at least one large crack propagates along the separation region 116 and the semiconductor workpiece 100 splits into two separate pieces. The force equilibrium of surface energy, bonding forces and (optional) external pressure are shifted in favor of the external force such that internal binding forces still present within the semiconductor workpiece 100 are overcome at the separation region 116, thus resulting in crack propagation. Alternatively, the laser radiation propagates enough cracks along the separation region 116 such that application of an external force is not necessarily required to split the semiconductor workpiece 100. However, an external force may still be applied to aid the lift-off process of the split wafer pieces and / or the wafer splitting.

[0062] The separation region 116 has at least one altered physical property which increases thermomechanical stress within the separation region 116 relative to the remainder of the semiconductor workpiece 100, as explained above. For example, laser radiation and / or ion implantation may be used to alter at least one physical property of the separation region 116. Laser radiation may form microscopic cracks ‘A’, ‘B’, ‘C’ in the separation region 116 whereas implanted ions may increase the absorption coefficient in the separation region 116 at a wavelength of the laser radiation. The localized increase in thermo-mechanical stress restricts crack propagation to the separation region 116 in a controlled and reproducible manner.

[0063] Figures 1C through 1 E illustrate an embodiment of applying the external force to the semiconductor workpiece 100 for splitting the wafer 100 along the separation region 116. According to this embodiment, a polymer 120 is applied to the semiconductor workpiece 100 (such as from below as indicated in Figure 1C). A polymer may also optionally be applied to the carrier 108 as shown in Figure 1C (such as from above as indicated in Figure 1C).

[0064] Figure 1C shows the device structures (such as epitaxial layers 102, the device structures 104, the layer 106, the carrier 108, the doping regions 110, 112, 114, and the additional layer 118). As discussed, the devices structures are optional and do not need to be present. The polymer 120 has a CTE (coefficient of thermal expansion) different from a CTE of the semiconductor workpiece 100. The polymer 120 and semiconductor workpiece 100 are then subjected to a temperature process during which the polymer 120 imparts mechanical stress to the semiconductor workpiece 100 as indicated by the dashed arrows in Figure 1 D. The mechanical stress causes at least one large crack 122 to propagate along the separation region 116 such that the semiconductor workpiece splits 100 into two separate pieces 124, 126 as shown in Figure 1 E. One piece 124 retains the device structures 104 (if present) or is available for subsequent processing (if the device structures are not present). The other piece 126 is available for subsequent device processing. In case a semiconductor wafer is split from a boule, the polymer 120 may be applied to the surface of the boule that is closer to the separation region 116.

[0065] In the case of the separation region 116 including microscopic cracks ‘A’, ‘B’, ‘C’ as explained above in connection with Figure 2, the mechanical stress imparted to the semiconductor workpiece 100 causes the microscopic cracks ‘A’, ‘B’, ‘C’ to connect to one another to form the large crack 122 which splits the wafer 100. That is, the individual microscopic cracks ‘A’, ‘B’, ‘C’ shift with respect to one another in response to the external force. The separation region 116 may thus not be viewed as a single layer within the semiconductor workpiece 100, but rather a combination of several microscopic cracks ‘A’, ‘B’, ‘C’ that are only combined during the splitting. In the case of SiC as the material of the semiconductor workpiece 100, combining the microscopic cracks ‘A’, ‘B’, ‘C’ results in both separate pieces 124, 126 having a separation surface 128, 130 with a saw-tooth pattern. The resulting device piece 124 and the reclaimed piece 126 thus do not have a smooth planar surface in the case of SiC. In one embodiment, after the semiconductor workpiece 100 is split into the two separate pieces 124, 126, each separation surface 128, 130 which results from the large crack 122 propagating along the separation region 116 is smoothed. Residual decomposed material may be present at the separation surface 128, 130 of each piece 124, 126 split from the wafer 100, and may be removed by a cleaning process.

[0066] The polymer 120 may be attached to the semiconductor workpiece 100 with the carrier 108 already attached to the wafer 100 (if the device structures are present). The polymer 120 may be attached at the backside 132 of the semiconductor workpiece 100 that faces away from the front side and the carrier 108. The polymer 120 may also be attached to an outer side 134 of the carrier 108 which faces away from the semiconductor workpiece 100 (if present). In case the device structures 104 are not present, the polymer may be attached on the frontside of the semiconductor workpiece 100 (not indicated in Figure 1C). In general, a further layer (e.g., a bonding layer, such as an adhesive, and / or a layer that simplifies later removal of the polymer 120) may be applied between the polymer 120 and the side at which the polymer 120 is applied. The polymer 120 may also be applied only to the backside 132 of the semiconductor workpiece 100 or only to the front side of the wafer 100.

[0067] The polymer 120 may be selected based not only CTE, but also by taking into account multiple parameters. The CTE of the polymer 120 should be different from the CTE of the semiconductor workpiece 100. For example, the CTE of the polymer 120 is preferably larger than the CTE of the semiconductor workpiece 100. In addition to the CTE difference, the linear course of the CTE in the polymer 120 over a wide temperature range may be advantageous for successful separation.

[0068] Furthermore, the polymer 120 should have sufficiently high thermal conductivity. In one embodiment, one or more fillers such as ZnO and / or carbon black are added to the polymer 120 before the temperature process. The filler(s) may increase the thermal conductivity of the polymer 120 and may reduce a slope of a storage modulus of the polymer 120, extending the linear course of the CTE in the polymer 120 over a smaller temperature range. By adding ZnO and / or carbon black to the polymer 120, percolation chains that form can increase thermal conductivity in the polymer 120. If a filler material is used, the polymer material may be chosen such that the filler material is homogeneously distributed throughout the polymer 120. One example for the polymer 120 is PDMS (polydimethylsiloxane), usually with at least one filler. PDMS may generate high adhesion to a surface. Attaching may thus require some pre- processing or conditioning to allow for damage-free polymer removal. For example, a foil may be positioned between the polymer and the surface to which the polymer is attached.

[0069] Attaching the polymer 120 is typically performed at higher temperatures (e.g., above room temperature but below 300°C). A binding process may be applied to allow for a firm bond throughout the entire temperature process. For example, before applying the polymer 120, the application surface of the polymer 120 and / or the semiconductor workpiece 100 and / or carrier 108 may undergo chemical and / or physical surface treatment (for example, with a plasma) to allow for firm bonding. An indirect temporary cold plasma activation process may be used to ensure subsequent easy removal of the polymer 120.

[0070] Another additional or alternative approach is to apply a binding (sacrificial) layer between the semiconductor workpiece 100 and the polymer 120. The binding layer may be chosen such that adhesion to the polymer 120 can be reduced, e.g., with chemicals or with thermal treatment. The polymer 120 may not be produced directly on the semiconductor workpiece 100 and / or directly on the carrier 108. Rather, the polymer 120 may be pre-produced and subsequently attached to the semiconductor workpiece 100 and / or carrier 108.

[0071] After attaching the polymer 120 to the semiconductor workpiece 100 (and / or carrier 108, if applicable), the temperature process is carried out. In one embodiment, the temperature process is selected such that the polymer 120 undergoes a partial glass transition and a partial crystallization during the temperature process. This may include a first phase during which the polymer 120 and the semiconductor workpiece 100 undergo a temperature gradient from a starting temperature down to room temperature, the starting temperature being 300°C or less but above room temperature, and a second phase during which the polymer 120 and the semiconductor workpiece 100 are further cooled down to a lower temperature. For example, the lower temperature may correspond to ±40°C of a boiling temperature of a cooling liquid (e.g., liquid nitrogen) used for cooling. The lower temperature may be, for example, -170°C, in particular for the entire wafer 100. In some examples, the lower temperature may be below a glass transition temperature (Tg) of the polymer 120, depending on the cooling conditions (e.g., the cooling liquid).

[0072] Figures 3A and 3B illustrate the storage modulus (modulus of elasticity) in MPa over temperature in °C for the same polymer 120 without fillers (Figure 3A) and with one or more fillers (Figure 3B). During the second phase of the temperature process, the polymer 120 may undergo a partial glass transition and a partial crystallization process as shown in Figures 3A and 3B. The definition of glass transition Tg is not standardized. There are several methods to determine Tg which is not a constant material property but rather depends on the method used to define Tg and also on parameters used during this method. For example, if using the DMA (dynamic mechanical analyzing) method, which measures the viscoelastic moduli, the dynamic glass transition temperature must be stated and also what parameters are used for the measurement (e.g., frequency of the external load, ramping speed, ramping direction, measurement accuracy, etc.). In Figure 3A, the glass transition temperature Tg is found at the turning point (at least for some methods of defining Tg). In Figure 3B, the crystallization starts at higher temperatures (slower slope between T 1 and T2) than the glass transition (higher slope below T2) where T3 is below T2 and T2 is below T1. A turning point, and thus Tg, can no longer be clearly determined as compared to the same polymer in Figure 3A but without fillers. By adding one or more fillers to the polymer 120, the degrees of freedom in the used polymer crystallize earlier than those of a polymer without fillers.

[0073] During the wafer splitting process, pressure may be applied to the semiconductor workpiece 100. For example, a piston may apply pressure to the semiconductor workpiece 100 with the one or more epitaxial layers 102. The piston may be pushed in the direction of the wafer 100 with pressurized air, or only the weight force of the piston may be applied to the wafer 100.

[0074] After the splitting of the semiconductor workpiece 100, the piece 124 which retains the device structures 104 may be thinner than the other piece 126. For example, the piece 124 which retains the device structures 104 may have a thickness of at most 100 pm (e.g., at most 70 pm or at most 50 pm) and at least the required thickness of the drift zone as described above (or at least 10 pm more than the required thickness) and the other piece 126 may have a thickness of at least 150 pm (e.g., at least 190 pm). In case a semiconductor wafer is split from a boule, the thickness of the semiconductor wafer may be at least 150 pm (e.g., at least 190 pm) or thicker, depending on for what the semiconductor wafer will be used later.

[0075] Afterwards, the polymer 120 may be removed by mechanical means both on the device side separation surface 128 (if applicable) and on the reclaimed side separation surface 130.

[0076] After the wafer splitting, the separation surfaces 128, 130 of the split wafer pieces 124, 126 on which piece 124, 126 is being processed (or the separation surfaces of the split wafer piece and the remainder of the boule). For the backside of the piece 124 with the device structures 104, a damage removal, e.g., by mechanical grinding and / or chemical mechanical polish and / or etching may be performed. The final roughness of the separation surface 128 after damage removal may have a root-mean-square (rms) value below 5 pm or even below 2 pm. Further processing may then follow. In the case of the piece 126 without the device structures 104, the separation surface 130 may need processing to be ready for subsequent epitaxial growth. In this case, the rms value of the separation surface 130 may be below 500nm or even below 300 nm. The thickness of the piece 126 without the device structures 104 may be adapted to the original thickness of the wafer 100, e.g., by means of deposition techniques such as CVD-epitaxial techniques, so that the same procedure as described above can be repeated several times for the thickened pieces 126.

[0077] The wafer splitting as described above can also be performed with the arrangement being turned upside down. In other words, in the wafer splitting shown in Figures 1 D and 1 E, the reclaimed wafer (which corresponds to the remainder of the boule in case the semiconductor wafer is split from a boule) may be located on top of the semiconductor wafer that corresponds to piece 124.

[0078] According to the present disclosure, a semiconductor work piece (e.g. a semiconductor boule or a semiconductor wafer, both being indicated by the reference sign 100 in Figures 1A to 1 E) may be placed on a device which may be configured to hold the polymer 120. In this context, “placed on” may mean that the semiconductor work piece is positioned above the device and the semiconductor work piece may be brought in contact (e.g. in direct contact) with the device (in particular the polymer) or “placed on” may mean that the device is positioned above the semiconductor work piece and the device (in particular the polymer) may be brought in contact (e.g. in direct contact) with the semiconductor work piece. The device may comprise a frame surrounding the polymer that is connected with the polymer. The boule (or semiconductor wafer) 100 can then be attached to the polymer, e.g., after the separation region 160 is formed and before the temperature process starts. The frame may have the form of a wafer ring that is typically used for processing a semiconductor wafer, e.g., for dicing the semiconductor wafer. For example, the wafer ring may be a metal frame. This may allow that the device (with or without the boule attached to it) can be handled by typical semiconductor manufacturing devices, which are configured to handle a typical semiconductor frame. The boule can then be attached to the polymer, e.g., with the side from which the semiconductor wafer is to be split. The device together with the boule attached to it can then be subjected to the thermal process in order to split the semiconductor wafer from the boule (as described above).

[0079] Figures 4A and 4B illustrate an exemplary device 10 that can be used for holding a work piece during a splitting process. In the example, the work piece is a boule 100. In other examples, the work piece may be a semiconductor wafer. For example, the device may be used for attaching a polymer to the boule 100. In particular, Figure 4A illustrates a side view of the device 10 and Figure 4B illustrates a top view of the device 10. The device 10 may comprise a polymer 20 and a frame 30. The polymer 20 may have the same properties (or is the same polymer) as the polymer 120 discussed above with regard to Figures 1 to 3. In addition, the device 10 may comprise a foil 40 that is fixedly attached (such as laminated) to the frame 30. The polymer 20 may be disposed on the foil 40 thereby providing a connection between the frame 30 and the polymer 20. The frame 30 is connected with the polymer 20, 120 and surrounds the polymer 20, 120. In one example, the foil 40 is a dicing foil that is typically used when dicing a semiconductor wafer.

[0080] The frame 30 may have an inner diameter 30d, an outer diameter 30D and a width 30w. The width may be at least 10 mm or at least 20 mm. The width may be at most 100 mm or at most 80 mm or at most 50 mm. The outer diameter 30D may be at least 20 cm or at least 26 cm or at least 28 cm. The outer diameter 30D may be at most 40 cm or at most 35 cm or at most 31 cm. The inner diameter may be at least 18 cm or at least 20 cm or at least 25 cm. The inner diameter may be at most 35 cm or at most 30 cm or at most 29 cm.

[0081] The device 10 may allow an efficient handling of the polymer 20, 120 that avoids manually placing the polymer 20, 120 on the boule 100. In one example, the frame 30 may be a wafer ring (e.g. a so-called dicing ring or dicing frame) that is typically used (e.g., in conjunction with a dicing foil) for handling wafers in typical semiconductor manufacturing machines. This may allow using the same semiconductor manufacturing machines to handle the boule 100 that is placed on foil 40 connected to the wafer ring. The polymer 20, 120 may be fixedly attached to the foil 40. This can be achieved by the adhesion of the polymer 20, 120 itself or by an additional adhesion step (such as laminating the polymer 20, 120 to the foil 40).

[0082] Figure 4B depicts the frame 30 as an ideal ring with an inner circle and an outer circle and a constant width along the circumference of the frame 30. The shape of the frame 30 may, however, deviate from an ideal ring shape. An example for a non-regular shape for the frame 30 is depicted in Fig. 4C. The outer rim of the frame 30 may comprise regions 301 ,302 that deviate from a circle or an ellipsoid. The width 30w1 ,30w2 of the frame 30 along the circumference may be changing. For example, the frame 30 may comprise regions with a larger first width 30w1 compared to regions with a narrower second width 30w2. The frame 30 may comprise flattened regions 301 (i.e. , the outer rim follows a straight line in regions). The flattened regions 301 may adjoin rounded regions 302. A first outer diameter 30D2 of the frame 30 in the flattened regions 301 may be smaller than a second outer diameter 30D1 of the frame 30 in the rounded regions 302. The frame 30 may comprise further regions 303, e.g. an indentation. The contour of the outer rim though usually still follows a ring shape, in particular given by the rounded regions 302. Likewise, the inner rim of the frame 30 may deviate from a circle or an ellipsoid in regions, but usually the shape inner rim is closer to a ring. The frame 30 depicted in Fig. 4C may be a so-called dicing frame. The frame 30 may be a so-called 8 inch dicing frame. This may allow for easier handling with standardized manufacturing equipment. An 8 inch dicing frame may be used for a boule or a wafer with a 150 mm diameter as well as a 200 mm diameter. The first outer diameter 30D1 may be 296±1 mm and the second outer diameter 30D2 may be 276±1 mm. An inner diameter 30d of the frame 30 may be 250±1 mm (as for the standard 8 inch dicing frame). In other examples, the inner diameter 30d of the frame 30 may be at least the outer diameter of the polymer, e.g. at least 160 mm for a 150 mm boule or wafer or at least 210 mm for a 200 mm boule or wafer. The first outer diameter 30D1 and the second outer diameter 30D2 in this case may still be the same as for a standard 8 inch dicing frame to allow for easier handling with standardized manufacturing equipment.

[0083] As discussed above, the polymer 20, 120 may undergo a partial glass transition when being cooled below a critical temperature while the polymer 20, 120 may be elastic when having a temperature above the critical temperature. The polymer 20, 120 comprises a first region 21A with a surface 22A to which a boule 100 can be attached. In some examples, the first region is equal to the entire polymer 20, 120. In other examples, the polymer may comprise additional regions that are not attached to a semiconductor work piece. For example, the polymer 20, 120 may have a diameter of about 15 cm or about 20 cm. When the boule 100 is attached to the surface 22A of the polymer 20, 120 of device 10, cooling the polymer 20, 120 below the critical temperature may apply a force to the boule 100 that causes the boule 100 to split (as described above with respect to Figures 1 B to 1 E). For example, the first region 21 A of the polymer 20, 120 may be contracted due to the partial glass transition. This force (which may arise due to the contraction) may not only apply to the boule 100, but also to the foil 40. This force may cause the foil 40 to pull the frame 30 towards the polymer 20, 120, which is located in the center of the frame 30 (due to the foil 40 being fixedly attached to the polymer 20, 120 and to the frame 30). In some cases, this may cause deformation of the frame, so that the frame 30 may be damaged after the cooling.

[0084] Figure 5A to 5C illustrates a further exemplary device 10 that can be used for holding a boule 100 during a splitting process. In particular, Figures 5A and 5B each illustrate a side view of an embodiment of the device 10 and Figure 5C illustrates an exemplary top view of the device 10. The device 10 may comprise a frame 30 and a polymer 20. The frame 30 may have an ideal ring shape as depicted in Fig. 5C or it may deviate from an ideal ring shape, for example as shown in connection with the embodiment of Fig. 4C. The polymer 20 may have the same properties (or is the same polymer) as the polymer 120 discussed above with regard to Figures 1 to 4. The polymer 20, 120 may have a surface 22A of a first region 21 A onto which a boule 100 can be attached and which will be cooled below the critical temperature of the polymer 20, 120 in order to perform a partial glass transition to split the boule 100 (as discussed above). Optionally, the polymer 20, 120 may additionally have a second region 21 B that will not undergo a transition during the cooling (e.g., by not cooling the second region 21 B below the critical temperature). As such, the second region 21 B may remain its elastic properties while the first region 21A of the polymer 20, 120 undergoes a transition and contracts (due to being cooled below the critical temperature). This may allow the second region 21 B of the polymer 20, 120 to mitigate the force that is applied to the frame 30 so that the frame 30 may not be deformed due to the force that is exerted by the first region 21A of the polymer during the transition. The surface 22A of the first region has substantially a circular shape with a diameter of about 15 cm or about 20 cm (depending on the size of the work piece). For example, the diameter of the surface 22A may correspond to a diameter (with a deviation of at most ±20% or at most ±10% or at most ±5%) of the semiconductor work piece 100 to which the polymer 20, 120 can be attached. The diameter of the surface 22A may, for instance, correspond to at least 105% or at least 110% of the diameter of the semiconductor work piece.

[0085] The second region 21 B may not overlap with the first region 21 A of the polymer 20, 120 and may surround the first region 21 A of the polymer. A surface of the second region 21 B may have substantially a ring shape, wherein the inner circle of the ring is substantially given by the surface 22A of the first region 21 A and wherein the diameter of the outer circle of the ring is at least 18 cm or at least 20 cm or at least 25 cm or at least 30 cm more. This may ensure that the second region 21 B may not undergo a partial glass transition when the first region 21 A is cooled below the critical temperature (or that at least parts of the second region 21 B may not undergo the partial glass transition). In particular, by cooling only substantially the first region 21A of the polymer 20, 120 and by not cooling the second region 21 B of the polymer 20, 120, a temperature gradient may be established within the polymer 20, 120 with a temperature that is above the critical temperature at least in parts of the second region 21 B. Then, the part of the second region 21 B of the polymer may remain elastic and may mitigate the forces that are applied by the first region 21A of the polymer 20, 120 when the first region 21A of the polymer 20, 120 undergoes the partial glass transition. This may mitigate the forces that are applied to the frame so that the frame 30 may not be damaged (or at least be less damaged). It may be possible that a thickness of the polymer 20, 120 perpendicular to the surface 22A is larger in the first region 21 A than in the second region 21 B. In this case, there may be a transition region between the first region 21 A and the second region 21 B, where the thickness is reduced. Separately or in combination, a surface roughness of at least one surface of the polymer may be larger in the first region 21 A compared to the second region 21 B. A reduced thickness and / or a higher surface roughness in the second region may reduce manufacturing costs of the polymer.

[0086] The polymer 20, 120 may be directly attached to the frame 30, e.g., by attachment elements 31 (such as hooks or holes, e.g. within the material of the frame) that protrude from the frame 30, as illustrated in Figure 5A. For example, the attachment elements 31 may protrude towards the polymer 20, 120. The attachment elements 31 may be part of the frame 30 or may be fixedly connected to the frame. The polymer 20, 120 may be molded (e.g., injection molded) onto the attachment elements 31 in order to form a firm connection between the polymer 20, 120 and the frame 30. For example, part of the polymer 20, 120 may be molded around the attachment elements 31. A distance of the attachment elements 31 (e.g., a center of the attachment elements 31) to an upper surface of the frame 30 may differ from a distance of the attachment elements 31 (e.g., a center of the attachment elements 31) to an opposite lower surface of the frame 30 by at most + / -20%, e.g. at most + / -10%. The attachment elements 31 may be positioned symmetrically with respect to the upper and the lower surface of the frame 30.

[0087] Alternatively, the polymer 20, 120 may have attachment elements 23, such as protrusions and / or fingers and / or hooks, that may be disposed (e.g., via molding) in voids of the frame 30 in order to form a firm connection between the polymer 20, 120 and the frame 30 (as illustrated in Figure 5B). For example, the polymer 20, 120 may be molded into the voids of the frame. The voids may be positioned symmetrically with respect to the upper and the lower surface of the frame 30. For example, a distance of a center of the voids to an upper surface of the frame 30 may differ from a distance of the center of the voids to an opposite lower surface of the frame 30 by at most + / -20%, e.g. at most + / -10%.

[0088] The first region 21 A of the polymer 20, 120A and the second region 21 B of the polymer 20, 120 may be formed of the same piece of polymer 20, 120. The first region 21A and the second region 21 B may have the same thickness or the thickness of the second region 21 B may be smaller than the thickness of the first region 21A. The entire polymer 20, 120 may have a diameter of at least 120% of the diameter of the semiconductor work piece (e.g. at least 20 cm for a semiconductor work piece, e.g. a boule 100 or a wafer, with a diameter of 150 mm).

[0089] The (optional) second region 21 B may form substantially a ring with an inner diameter that is at most 120% of or equal to the diameter of the semiconductor workpiece 100 that is attached to the first surface 21A and an outer diameter of about at least 120% of the diameter of the semiconductor workpiece 100 (e.g. an inner diameter of 150mm or 160 mm or 170 mm and an outer diameter of 18 cm). In the case of an outer diameter of 18 cm, the ring may have a width of at most 1 .5 cm when a semiconductor workpiece 100 with a diameter of 150 mm (such as a 6 inch SiC boule) is attached to the first surface 21A. This may ensure that at least a part of the second region 21 B may not undergo the partial glass transition when the first region 21 A is cooled below the critical temperature and may remain elastic to mitigate the forces (as discussed above). In other examples, the outer diameter of the second region 210B may be at least 20 cm or at least 25 cm or at least 30 cm or at least 40 cm or at least 50 cm or at least 60 cm or at least 70 cm or at least 80 cm or at least 100 cm. As a general rule, the larger the diameter of the semiconductor workpiece 100 is, the larger the outer diameter of the polymer 20, 120 should be chosen. In some examples, a thermal insulator may be provided between the first region 21 A and the second region 21 B of the polymer 20, 120. In some examples, the polymer 20, 120 may be formed of a single part.

[0090] Figure 6 illustrates another embodiment of the present disclosure. In particular, the frame 30 may be an assembly of a plurality of parts. In particular, the frame 30 may comprise an outer ring 34 that is removably attached to a flexible ring. The flexible ring may comprise three or more ring elements 32 and respective three or more flexible attachment elements 33. Each flexible attachment element 33 may connect two respective ring elements 32 of the three or more ring elements with each other to form the flexible ring. Figure 6 shows an example with six ring elements and respective six flexible attachment elements 33. Of course, other embodiments are possible, e.g., with three ring elements 32 and respective three flexible attachment elements 33 (or four, five, seven, eight, nine, ten, and so on). As discussed above, the polymer 20, 120 may be connected with the frame 30 by directly attaching the polymer 20, 120 to the frame 30, e.g., by attachment elements 31 (such as hooks or holes) that protrude from the frame 30, as illustrated in Figure 5A or by attachment elements 23, such as protrusions and / or fingers and / or hooks, that may be disposed (e.g., via molding) in voids of the frame in order to form a firm connection between the polymer 20, 120 and the frame 30 (as illustrated in Figure 5B). In the exemplary disclosure of Figure 6, the attachment elements 31 may protrude from the ring elements 32 1 the voids may be formed in the ring elements 32. The flexible ring formed by the ring elements 32 and the flexible attachment elements 33 may have an inner diameter that substantially equals the outer diameter of the second region 21 B of the polymer 20, 120 in case the polymer is directly attached to the flexible ring of the frame 30. In another embodiment, the polymer 20, 120 may be connected with the flexible ring of the frame 30 via the foil 40 disclosed in context with Figures 4A and 4B. As discussed above, the polymer may be attached to the foil 40 (e.g., by laminating the polymer 20, 120 to the foil) and the foil 40 may be attached to the flexible ring of the frame 30 (e.g. by lamination). The flexible attachment elements 33 may firmly connect the ring elements 32 to each other. In addition, the flexible attachment elements 33 may allow the flexible ring to have a first inner diameter when no external force is applied to the flexible ring, and, when an external force that points towards the center of the flexible ring is applied, the flexible attachment elements 33 may allow the flexible ring to have a second inner diameter, the second inner diameter of the flexible ring being smaller than the first inner diameter of the flexible ring. This may allow the flexible ring to mitigate the force that may arise from the contraction of the polymer 20, 120 when the polymer undergoes the partial glass transition. For example, the flexible attachment elements 33 may comprise springs or suspension components that may contract (e.g., shrink) under pressure. For example, when no external force is applied to the flexible ring, two neighboring ring elements 32 may have a gap between each other. When an external force is applied to the ring elements 32 that points towards the center of the flexible ring, the flexible attachment elements may be contracted so that the gap between the ring elements 32 becomes smaller. This may allow the flexible ring to contract from a first diameter (when no external force is applied to a smaller diameter (when a force is applied to the ring elements that points towards the center of the flexible ring, e.g., from the polymer 20, 120 that contracts when undergoing the partial glass transition). When the external force reaches a threshold force, the gap may vanish or may reach a minimal size of the gap. For example, the ring elements 32 may comprise voids where the flexible ring elements can slip into when the external force is applied. The ring elements 32 each may span an angle of the flexible ring. The ring elements 32 may all have the same size and can also have different sizes, e.g., one ring element having a greater length than the remaining ring elements. The ring elements 32, when assembled together with the flexible attachment elements 33 (and when no external force is applied) may form a ring with an inner diameter of, e.g., 18 cm 20 cm, 25 cm or larger (the inner diameter may depend on the diameter of the polymer 20, 120) and an outer diameter of, e.g., 23 cm, 25 cm, 30 cm (e.g., 5 cm greater than the inner diameter of the flexible ring). The flexible ring may be removably attached (such as mounted) to an outer ring 34 of the frame 30. The outer ring 34 may be a rigid frame that may provide stability to the flexible ring.

[0091] Figure 7 illustrates the use of a device 10 in accordance with the disclosure herein in a process of splitting a semiconductor workpiece 100. The semiconductor workpiece 100 (such as a boule or a semiconductor wafer) may be attached to the surface 22A of the first region 21 A of the polymer 20, 120 after the separation region 116 has been formed within the boule 100. The semiconductor work piece 100 may be attached to the device 10 such that the surface of the boule is placed on the device 10 that has less distance to the separation region 116 within the semiconductor work piece 100 as compared to the other surface of the semiconductor work piece.

[0092] Figure 8 illustrates a method of splitting a semiconductor work piece according to embodiments of the present disclosure. As discussed above in context with Figure 1A the method may optionally comprise forming one or more epitaxial layers on the semiconductor work piece, forming a plurality of device structures in the one or more epitaxial layers, forming a metallization layer and / or a passivation layer over the plurality of device structures, and attaching a carrier with the one or more epitaxial layers on top of the device structures, the carrier protecting the plurality of device structures.

[0093] The method may then comprise the step 810 of forming a separation region within the boule or within the semiconductor wafer. The separation region may have at least one altered physical property which may increase thermo-mechanical stress within the separation region relative to the remainder of the semiconductor work piece. In some examples, forming the separation region within the semiconductor work piece comprises damaging a material of the semiconductor work piece at a targeted position within the semiconductor work piece. In an embodiment, damaging the material of the semiconductor work piece at the targeted position within the semiconductor work piece may comprise creating a plasma in the material at the targeted position within the semiconductor work piece. For instance, creating the plasma in the material at the targeted position comprises focusing laser radiation at the targeted position. In addition or as an alternative, damaging the material of the boule or of the semiconductor wafer at the targeted position may comprise implanting ions into the semiconductor work piece at a depth corresponding to the targeted position. An implantation does of the ions may be selected such that the material of the semiconductor work piece damaged by the implanted ions is amorphous or cavities are created. For instance, the ions are selected from the group consisting of nitrogen ions, phosphorus ions, hydrogen ions, and helium ions. In some embodiments, damaging the material of the boule or of the semiconductor wafer at the targeted position may comprise implanting ions into the semiconductor work piece at a depth corresponding to the targeted position; and after the ions are implanted, focusing laser radiation at the targeted position, wherein the implanted ions increase an absorption coefficient in the separation region at a wavelength of the laser radiation.

[0094] Then, the method may proceed to the step 820 of attaching the semiconductor work piece to a first region of a surface of a polymer. The polymer is included in a device for holding a semiconductor work piece during splitting. The device comprises the polymer and a frame, wherein the frame is connected with the polymer and surrounding the polymer, wherein the polymer is configured to undergo at least a partial glass transition when being cooled below a critical temperature and to be elastic when having a temperature above the critical temperature, wherein the polymer comprises the surface. The device may be the device described in context with Figures 4A to 6. The polymer may comprise a second region which does not overlap with the first region of the surface. The second region may surround the first region of the polymer and may be dimensioned such that during the subsequent step of cooling (as further described below), at least a part of the second region of the polymer remains above the critical temperature. This may ensure that the second region of the polymer may remain elastic and can be stretched while the first region of the polymer is contracted during the glass transition of the first region of the polymer. As such, the diameter of the first region of the polymer may be substantially equal to the diameter of the semiconductor work piece that is placed on the polymer (such as 15 cm, 20 cm, or 30 cm). The second region second region may have substantially a ring shape, wherein the inner circle of the ring is given by the surface of the first region and wherein the diameter of the outer circle is chosen such that at least a portion of the second region does not undergo a glass transition when the semiconductor work piece is cooled down (such as the diameter of the outer circle being at least 18 cm, 20 cm, 25 cm, 30 cm, 40 cm, 50 cm, 60 cm, 700 cm or more). In some examples, the second region of the polymer can reach to the frame of the device and can directly be connected with the frame. The semiconductor work piece may be attached to the device such that the surface of the boule is placed on the device that has less distance to the separation region within the semiconductor work piece as compared to the other surface of the semiconductor work piece. In some examples, the semiconductor work piece may not be disposed directly on the polymer and a binding (sacrificial) layer may be disposed between the semiconductor wafer 100 and the polymer 120. 17. In addition, before the surface of the first region of the polymer is attached to the semiconductor work piece, the surface of the first region of the polymer and / or a surface of the boule (or the semiconductor wafer) may be chemically and / or physically treated.

[0095] In a subsequent step, the method may comprise cooling 830 the boule or the semiconductor together with the first region of the device to a temperature below the critical temperature. This may be performed in order to apply an external force to the semiconductor work piece such that at least one crack propagates along the separation region and the semiconductor work piece splits into two separate pieces. For example, the polymer attached to the boule or to the semiconductor wafer may have a CTE (coefficient of thermal expansion) different from a CTE of the semiconductor work piece. Cooling the first region of the polymer and the boule (or the first region of the polymer and the semiconductor wafer) to a temperature below the critical temperature may impart mechanical stress to the boule (or to the semiconductor wafer). The polymer may comprise a second region which does not overlap with the first region of the surface. The second region may surround the first region of the polymer and may be dimensioned such that during the cooling, at least a part of the second region of the polymer remains above the critical temperature so that the second region of the polymer remains elastic. This may reduce the forces that are applied to the frame of the device. In one example, the semiconductor work piece together with the first region of the polymer are cooled with a cooling stamp that is not in direct contact with the second region of the polymer and / or only partially in contact with the second region.

[0096] During the wafer splitting process, pressure may be applied to the semiconductor wafer 100. For example, a piston may apply pressure to the semiconductor wafer 100 with the one or more epitaxial layers 102. The piston may be pushed in the direction of the wafer 100 with pressurized air, or only the weight force of the piston may be applied to the wafer 100.

[0097] The cooling may be part of a temperature process that includes a first phase during which the polymer and the semiconductor work piece undergo a temperature gradient from a starting temperature down to room temperature, the starting temperature being 300°C or less but above room temperature, and a second phase during which cooling 830 is performed. Before the temperature process, one or more fillers (such as ZnO and / or carbon black) may be added to the polymer which may increase the thermal conductivity of the polymer and reduce a slope of a storage modulus of the polymer. During a partial crystallization of the first region of the polymer, at least one crack propagates through the semiconductor work piece along the separation region. In addition, an additional external force may be applied to the semiconductor work piece by applying pressure to the semiconductor wafer during the splitting of the semiconductor wafer into the two separate pieces.

[0098] Optionally in a subsequent step, after the semiconductor work piece is split into the two separate pieces, a surface roughness of a separation surface of both pieces may be reduced, each separation surface being a surface formed as the at least one crack propagates along the separation region.

[0099] The boule and the semiconductor wafer, as described in the above disclosure may be a SiC boule I SiC semiconductor wafer. Nevertheless, the embodiments described herein are not intended to be limited to SiC boules and SiC wafers and may be used with other semiconductor wafer technologies such as silicon (Si), gallium arsenide (GaAs), gallium nitride (GaN), sapphire, etc. Although the present disclosure is not so limited, the following numbered examples demonstrate one or more aspects of the disclosure.

[0100] Example 1 : A device for attaching a polymer to a semiconductor work piece in a splitting process, the device comprising a polymer and a frame, wherein the frame is connected with the polymer and surrounding the polymer, the polymer is configured to undergo at least a partial glass transition when being cooled below a critical temperature, and to be elastic when having a temperature above the critical temperature, and the polymer comprises a first region having a surface to which a semiconductor work piece can be attached.

[0101] Example 2: The device according to example 1 , further comprising a foil, wherein the foil is fixedly attached to the polymer and to the frame thereby connecting the polymer and the frame.

[0102] Example 3: The device according to example 2, wherein the frame is a wafer ring, and wherein the foil is a dicing foil.

[0103] Example 4: The device according to example 1 , wherein the polymer is directly attached to the frame thereby connecting the polymer and the frame.

[0104] Example 5: The device according to example 1 , wherein the polymer comprises a second region which does not overlap with the first region of the polymer and which surrounds the first region of the polymer.

[0105] Example 6: The device according to example 5, wherein the surface of the first region has substantially a circular shape with a diameter of one of: about 15 cm, about 20 cm, or about 30 cm.

[0106] Example 7: The device according to example 5 or 6, wherein a surface of the second region has substantially a ring shape, wherein the inner circle of the ring is given by the surface of the first region and wherein the diameter of the outer circle of the ring is at least 16 cm or at least 18 cm.

[0107] Example 8: The device according to any of the preceding examples, wherein the frame comprises a flexible ring wherein the flexible ring substantially has a circular shape with a first diameter, wherein the flexible ring comprises three or more ring elements and corresponding three or more flexible attachment elements, wherein each flexible attachment element connects two respective ring elements of the three or more ring elements with each other to form the flexible ring, wherein when a force is applied to the flexible ring that points towards the center of the flexible ring, the flexible attachment elements are contracted so that the flexible ring substantially has a circular shape with a second diameter, the second diameter being smaller than the first diameter.

[0108] Example 9: The device according to example 8, wherein the frame further comprises an outer ring, and wherein the flexible ring is removably attached to the outer ring.

[0109] Example 10: Use of a device according to any one of examples 1 to 9 in a splitting process.

[0110] Example 11 :. A method of splitting a semiconductor work piece, the method comprising: attaching the semiconductor work piece to a first region of a surface of a polymer of a device, wherein the device comprises the polymer and a frame, wherein the frame is connected with the polymer and surrounding the polymer, wherein the polymer is configured to undergo at least a partial glass transition when being cooled below a critical temperature and to be elastic when having a temperature above the critical temperature, wherein the polymer comprises the surface; and cooling the boule together with the first region of the device to a temperature below the critical temperature.

[0111] Example 12: The method according to example 11 , wherein the surface of the polymer comprises a second region which does not overlap with the first region of the surface, and wherein during the cooling, at least a portion of the second region remains at a temperature that is above the critical temperature

[0112] Example 13: The method according to examples 11 or 12, wherein the semiconductor work piece is attached to the device such that an outer surface of the semiconductor work piece is placed on the device, the outer surface having a smaller distance to a separation region within the semiconductor work piece as compared to a surface of the semiconductor work piece opposite the outer surface..

[0113] Example 14: The method according to any one of examples 10 to13, wherein the separation region has at least one altered physical property which increases thermo-mechanical stress within the separation region relative to the remainder of the semiconductor work piece.

[0114] Example 15: The method according to any one of examples 10 to 14; wherein cooling the boule together with the first region of the device to a temperature below the critical temperature causes an external force to be applied to the semiconductor work piece such that at least one crack propagates along the separation region and the semiconductor work piece splits into two separate pieces. Example 16. The method according to any one of examples 10 to 15, wherein forming the separation region within the semiconductor work piece comprises: damaging a material of the semiconductor work piece at a targeted position within the semiconductor work piece.

[0115] Example 17. The method according to example 16, wherein damaging the material of the semiconductor work piece at the targeted position within the semiconductor work piece comprises: creating a plasma in the material at the targeted position within the semiconductor work piece.

[0116] Example 18: The method according to example 17, wherein creating the plasma in the material at the targeted position within the semiconductor work piece comprises: focusing laser radiation at the targeted position within the semiconductor work piece.

[0117] Example 19 The method according to example 16, wherein damaging the material of the semiconductor work piece at the targeted position within the semiconductor work piece comprises: implanting ions into the semiconductor work piece at a depth corresponding to the targeted position within the semiconductor work piece.

[0118] Example 20: The method according to example 19, wherein the ions are selected from the group consisting of nitrogen ions, phosphorus ions, hydrogen ions, and helium ions.

[0119] Example 21 : The method according to example 19, wherein an implantation does of the ions is selected such that the material of the semiconductor work piece damaged by the implanted ions is amorphous or cavities are created.

[0120] Example 22. The method according to example 16, wherein damaging the material of the semiconductor work piece at the targeted position within the semiconductor work piece comprises: implanting ions into the semiconductor work piece at a depth corresponding to the targeted position within the semiconductor work piece; and after the ions are implanted, focusing laser radiation at the targeted position within the semiconductor work piece, wherein the implanted ions increase an absorption coefficient in the separation region at a wavelength of the laser radiation.

[0121] Example 23: The method according to example 15, wherein the external force is applied to the semiconductor work piece by attaching the semiconductor work piece to the polymer, and wherein the polymer has a CTE (coefficient of thermal expansion) different from a CTE of the semiconductor work piece. Example 24: The method according to example 15, the cooling causes the polymer to undergo a partial glass transition and / or a partial crystallization.

[0122] Example 25: The method according to any one of examples 11 to 24, wherein the cooling is part of a temperature process, wherein the temperature further includes a first phase during which the polymer and the semiconductor work piece undergo a temperature gradient from a starting temperature down to room temperature, the starting temperature being 300°C or less but above room temperature before the cooling.

[0123] Example 26. The method according to any one of examples 11 to 25, wherein fillers are added to the polymer.

[0124] Example 27: The method according to example 26, wherein the one or more fillers comprises ZnO and / or carbon black.

[0125] Example 28: The method according to any one of examples 11 to 27, further comprising: before attaching the semiconductor work piece to the polymer, chemically and / or physically treating a surface of the polymer and / or a surface of the semiconductor work piece.

[0126] Example 29. The method according to example 15, wherein the at least one crack propagates during a partial crystallization of the polymer which occurs during the temperature process.

[0127] Example 30: The method according to example 15, wherein an additional external force is applied to the semiconductor work piece by applying pressure to the semiconductor work piece during the splitting of the semiconductor work piece into the two separate pieces.

[0128] Example 31. The method according to any of examples 11 to 30, the method further comprising: after the semiconductor work piece is split into the two separate pieces, reducing a surface roughness of a separation surface of the two pieces, each separation surface being a surface formed as the at least one crack propagates along the separation region.

[0129] Example 32: The method according to example 15, wherein the at least one altered physical property of the separation region comprises a plurality of microscopic cracks that are at least partially disconnected from one another within the separation region, and wherein the plurality of microscopic cracks connect to one another in response to the external force, to form the at least one crack which propagates along the separation region.

[0130] Example 33: A device for attaching a polymer to a semiconductor work piece in a splitting process, the device comprising a polymer and a frame, wherein the frame is directly connected with the polymer and surrounding the polymer, the polymer is configured to undergo at least a partial glass transition when being cooled below a critical temperature, and to be elastic when having a temperature above the critical temperature, wherein the polymer comprises a surface to which a semiconductor work piece can be attached, and wherein the polymer having a diameter of at least 16 cm or at least 18 cm.

[0131] Example 34: The device of example 33, wherein the polymer has a diameter of at least 20 cm.

[0132] Example 35 The device of example 33, wherein the polymer has a diameter of at least 23 cm.

[0133] Example 36 The device of example 33, wherein the polymer has a diameter of at least 25 cm.

[0134] Example 37 The device of example 33, wherein the polymer has a diameter of at least 30 cm.

[0135] Example 38: The device or method according to any of the preceding examples, wherein the boule is a SiC boule, and / or wherein the semiconductor wafer is a SiC semiconductor wafer.

[0136] Although specific examples have been illustrated and described herein, it will be appreciated by those of ordinary skill in the art that a variety of alternate and / or equivalent implementations may be substituted for the specific examples shown and described without departing from the scope of the present invention. This application is intended to cover any adaptations or variations of the specific examples discussed herein. Therefore, it is intended that this invention be limited only by the claims and the equivalents thereof.

[0137] It should be noted that the methods and devices including its preferred embodiments as outlined in the present document may be used stand-alone or in combination with the other methods and devices disclosed in this document. In addition, the features outlined in the context of a device are also applicable to a corresponding method, and vice versa. Furthermore, all aspects of the methods and devices outlined in the present document may be arbitrarily combined. In particular, the features of the claims may be combined with one another in an arbitrary manner.

[0138] It should be noted that the description and drawings merely illustrate the principles of the proposed methods and systems. Those skilled in the art will be able to implement various arrangements that, although not explicitly described or shown herein, embody the principles of the invention and are included within its spirit and scope. Furthermore, all examples and embodiments outlined in the present document are principally intended expressly to be only for explanatory purposes to help the reader in understanding the principles of the proposed methods and systems. Furthermore, all statements herein providing principles, aspects, and embodiments of the invention, as well as specific examples thereof, are intended to encompass equivalents thereof.

Claims

CLAIMS1 . A device for attaching a polymer to a semiconductor work piece in a splitting process, the device comprising the polymer and a frame, wherein the frame surrounds the polymer, the polymer is configured to undergo at least a partial glass transition when being cooled below a critical temperature, and to be elastic when having a temperature above the critical temperature, the polymer comprises a first region having a surface to which a semiconductor work piece can be attached, and the frame and / or the polymer comprises at least one attachment element, wherein the polymer is directly attached to the frame via the at least one attachment element, thereby connecting the polymer and the frame.

2. The device of claim 1 , wherein a thickness of the polymer in the first region is at least 2 mm.

3. The device of any of the preceding claims, wherein the frame comprises at least one attachment element that protrudes from the frame towards the polymer.

4. The device of any of the preceding claims, wherein the at least one attachment element comprises or consists of a hook and / or a hole within the material of the frame.

5. The device of any of the preceding claims, wherein the frame comprises at least one attachment element and wherein the polymer is molded to the at least one attachment element of the frame.

6. The device of any of the preceding claims, wherein the polymer comprises a second region which does not overlap with the first region of the polymer and which surrounds the first region of the polymer.

7. The device of the previous claim, wherein a surface of the second region has substantially a ring shape, wherein the inner circle of the ring is given by the surface of the first region and wherein the diameter of the outer circle of the ring is at least 16 cm.

8. The device of any of the preceding claims, wherein the frame comprises a flexible ring wherein the flexible ring substantially has a first inner diameter, wherein the flexible ring comprises three or more ring elements and corresponding three or more flexible attachment elements, wherein each flexible attachment element connects two respective ring elements of the three or more ring elements with each other to form the flexible ring, wherein when a force is applied to the flexible ring that points towards the center of the flexible ring, the flexible attachment elements are contracted so that the flexible ring substantially has a second inner diameter, the second inner diameter being smaller than the first inner diameter.

9. A method of splitting a semiconductor work piece, the method comprising: attaching the semiconductor work piece to a surface of a first region of a polymer of a device, wherein the device comprises the polymer and a frame, wherein the frame is connected with the polymer and surrounding the polymer, wherein the polymer is configured to undergo at least a partial glass transition when being cooled below a critical temperature and to be elastic when having a temperature above the critical temperature, wherein the polymer comprises the surface; and cooling the boule or the semiconductor together with the first region of the device to a temperature below the critical temperature.

10. The method according to the previous claim, wherein the surface of the polymer comprises a second region which does not overlap with the first region of the surface, and wherein during the cooling, at least a portion of the second region remains at a temperature that is above the critical temperature11. The method according to any of the two previous claims, wherein the semiconductor work piece is attached to the device such that an outer surface of the semiconductor work piece is placed on the device, the outer surface having a smaller distance to a separation region within the semiconductor work piece as compared to a surface of the semiconductor work piece opposite the outer surface.

12. A device for holding a semiconductor work piece in a splitting process, the device comprising a polymer and a frame, whereinthe frame is directly connected with the polymer and surrounding the polymer, the polymer is configured to undergo at least a partial glass transition when being cooled below a critical temperature, and to be elastic when having a temperature above the critical temperature, the polymer comprises a surface to which a semiconductor work piece can be attached, and the polymer having a diameter of at least 16 cm.