Agent for adjusting wettability of surface of rock for carbon dioxide storage, and method for storing carbon dioxide

MYPI2025004606A0Undetermined Publication Date: 2024-07-31NISSAN CHEM CORP
View PDF 0 Cites 0 Cited by

Patent Information

Application Number
MYPI2025004606
Authority / Receiving Office
MY · MY
Patent Type
Applications
Current Assignee / Owner
Priority Date
2023-06-02
Filing Date
2024-01-31
Publication Date
2024-07-31

AI Technical Summary

Technical Problem

Current methods for enhancing carbon dioxide storage in rocks, such as using silica particles, face challenges due to particle size limitations that prevent effective injection into underground rock formations, leading to reduced storage capacity and potential clogging of pores.

Method used

A rock surface wettability modifier comprising a silica sol with silica particles of 5 to 100 nm in diameter, coated with silane compounds, is used to create a hydrophilic surface, allowing for increased carbon dioxide storage by improving wettability and preventing particle aggregation.

Benefits of technology

The wettability modifier increases carbon dioxide storage capacity by adjusting the rock surface to be more hydrophilic, allowing for better penetration and retention of CO2 within the rock, enhancing storage efficiency and preventing clogging.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure PI2025004606_DRAWING_001
    Figure PI2025004606_DRAWING_001
Patent Text Reader

Abstract

[Problem] To provide a wettability control agent for rock surfaces to increase an amount of carbon dioxide stored in bedrocks. [Solution] To provide a wettability control agent for rock surfaces, which makes rock surfaces hydrophilic to increase an amount of carbon dioxide stored in bedrocks, comprising a silica sol containing silica particles (a) having an average primary particle diameter of 5 to 100 nm and an aqueous medium (b), and a method for controlling surface wettability of underground rocks using the wettability control agent. FIG. 1
Need to check novelty before this filing date? Find Prior Art

Description

Rock surface wettability adjuster for carbon dioxide gas storage, and carbon dioxide gas storage method

[0001] The present invention relates to a rock surface wettability control agent for increasing the amount of carbon dioxide stored in rock masses by making the rock surface hydrophilic, and a method for evaluating the wettability of a surface after application of the wettability control agent.

[0002] CO 2 Carbon dioxide Capture and Storage (CCS) is a technology that captures and stores CO2 emitted from sources such as power plants and steel mills. 2 In order to prevent CO from being released directly into the atmosphere, 2 This technology separates and captures CO2 and injects it underground or underwater for storage, and is considered an important option for global warming countermeasures. 2 Deep underground aquifers (such as sandstone layers containing many voids) are considered to be promising storage locations for CO, and a geological storage system has been proposed, for example, as shown in Patent Document 1. Patent Document 2 also proposes the storage of CO in an unstructured reservoir that does not have a sealed structure as an underground storage target layer. 2 Proposals have been made for underground carbon dioxide storage facilities to achieve this.

[0003] CO injected into a saline aquifer (reservoir) deep underground 2 CO displaces the formation water in the reservoir and spreads, and is trapped by four mechanisms: structural traps, residual gas traps, dissolution traps, and mineral traps. 2 Since silica is non-polar, its movement can be restricted by its surroundings being hydrophilic (water-wet layer), and it is thought that this hydrophilicity works advantageously to improve the trapping ability. Non-Patent Document 1 discloses a technology that attempts to wet rock surfaces using an aqueous solution in which silica particles are dispersed in water.

[0004] JP 2008-307483 A JP 2011-147869 A International Publication No. 2007 / 111147

[0005] International Journal of Greenhouse Gas Control 66 (2017) 97-105Journal of Colloid and Interface Science 508 (2017) 222-229

[0006] Although Non-Patent Document 1 discloses that the wettability of the calcite substrate was changed by silica particle treatment, 2 The silica particles disclosed in Non-Patent Documents 1 and 2 have an average particle size of 84 nm (as determined by dynamic light scattering) and also contain many coarse particles of 1 μm or larger, which poses a problem when they are injected into underground bedrock.

[0007] The present invention provides a wettability modifier for rock surfaces, which hydrophilizes rock surfaces to increase the amount of carbon dioxide stored in rock masses, and includes a silica sol containing silica particles (a) and an aqueous medium (b). The present invention also aims to provide the wettability modifier and a method for adjusting the surface wettability of underground rocks using the wettability modifier.

[0008] The present invention provides, as a first aspect, a rock surface wettability adjuster for increasing the amount of carbon dioxide stored in rock mass by hydrophilizing the rock surface, the rock surface wettability adjuster comprising a silica sol containing silica particles (a) having an average primary particle size of 5 to 100 nm and an aqueous medium (b); as a second aspect, the rock surface wettability adjuster according to the first aspect, in which the silica particles in the silica sol have an average particle size of 5 to 70 nm as measured by a dynamic light scattering method; as a third aspect, the rock surface wettability adjuster according to the first or second aspect, in which the silica particles are at least partially coated with a silane compound (c) having a hydrophilic organic group, and the hydrophilic organic group is an epoxy group-containing organic group, an amino group-containing organic group, a hydroxy group-containing organic group, or a carboxy group-containing organic group; As a fourth aspect, the wettability adjuster for a rock surface according to any one of the first to third aspects, wherein a cumulative particle size distribution D90 of average particle diameters of silica particles in the silica sol measured by a dynamic light scattering method is 5 to 200 nm; As a fifth aspect, the wettability adjuster for rock surfaces according to any one of the first to fourth aspects, wherein, in a test in which 6 μL of saltwater is dropped onto a rock slab at an inclination angle of 15° placed in a container filled with carbon dioxide at a pressure of 10 MPa and a temperature of 50°C, at a distance of 3.5 to 4.0 mm from a direction perpendicular to the bottom of the container, and the receding contact angle and advancing contact angle of the droplet formed on the rock slab are measured, after the surface of the rock slab has a receding contact angle and an advancing contact angle of 70 to 110°, the wettability adjuster for rock surfaces according to any one of the first to fourth aspects is coated on the surface of the rock slab, and the receding contact angle on the coated surface becomes 5 to 70°, and the advancing contact angle can be adjusted to 5 to 70°; as a sixth aspect, the wettability adjuster for rock surfaces according to the fifth aspect, wherein the saltwater has a salt concentration of 0.1 to 30 mass%; As a seventh aspect, the wettability control agent for a rock surface according to any one of the first to sixth aspects, wherein when a droplet of the wettability control agent diluted with 3 mass % salt water so that the silica particle concentration is 0.1 to 0.5 mass % is dropped from a vertically installed needle having a diameter of 1.5 mm at a flow rate of 0.5 mL / min in a container filled with carbon dioxide at a pressure of 10 MPa and a temperature of 50°C, the interfacial tension calculated from the shape of the largest droplet that does not fall is 1 to 35 mN / m;As an eighth aspect, the wettability adjuster for a rock surface according to any one of the first to seventh aspects, wherein, in a measurement of a carbon dioxide storage amount obtained when an internal pressure is reached by injecting a wettability adjuster diluted with 3 mass% brine to a silica particle concentration of 0.5 mass%, 10 MPa carbon dioxide, and 3 mass% brine into rock under a temperature condition of 50°C, the residual carbon dioxide saturation rate (with application of the wettability adjuster) calculated from the CT value of carbon dioxide remaining inside the rock after the 3 mass% brine injection (second time) is increased by 10% or more compared to the residual carbon dioxide saturation rate (without application of the wettability adjuster) calculated from the CT value of carbon dioxide remaining inside the rock after the 3 mass% brine injection (second time) under a temperature condition of 50°C, the wettability adjuster diluted with 3 mass% brine to a silica particle concentration of 0.5 mass%. As a ninth aspect, the wettability adjuster for a rock surface according to any one of the first to eighth aspects, wherein, in a measurement of a carbon dioxide storage amount obtained by injecting a wettability adjuster diluted with 3 mass % brine to a silica particle concentration of 0.5 mass %, 10 MPa carbon dioxide, and 3 mass % brine into a rock in this order under a temperature condition of 50°C and setting the internal pressure to 10 MPa, an initial carbon dioxide saturation rate (with application of the wettability adjuster) calculated from the CT value of the carbon dioxide remaining inside the rock after the carbon dioxide injection increases by 10% or more compared to the initial carbon dioxide saturation rate (without application of the wettability adjuster) calculated from the CT value of the carbon dioxide remaining inside the rock after the carbon dioxide injection, in a measurement of a carbon dioxide storage amount obtained by injecting 3 mass % brine (first time), 10 MPa carbon dioxide, and 3 mass % brine (second time) into a rock in this order under a temperature condition of 50°C and setting the internal pressure to 10 MPa; As a tenth aspect, a method for adjusting the surface wettability of an underground rock surface, the method comprising: adjusting the wettability adjuster for a rock surface according to any one of the first to ninth aspects in an aqueous medium to a silica particle concentration of 0.001 to 30 mass %; and injecting the resulting mixture into an underground formation.As an eleventh aspect, the present invention relates to a method for storing carbon dioxide in a subterranean layer, the method including: a step of adjusting the wettability adjuster for a rock surface according to any one of the first to ninth aspects to a silica particle concentration of 0.001 to 30 mass% in an aqueous medium, and injecting the resultant into a subterranean layer; and a step of injecting carbon dioxide into the subterranean layer at 10 to 300°C and under a pressure of 0.1 to 100 MPa. Furthermore, the present invention encompasses, as a twelfth aspect, an embodiment of the wettability evaluation method, which is a method for evaluating the wettability of a rock surface, comprising the steps of placing a rock slab having a surface coated with the rock surface wettability adjuster according to any one of the first to ninth aspects at an inclination angle of 15° in a container filled with carbon dioxide at a pressure of 10 MPa and a temperature of 50°C, dropping 0.1 to 10 μL of salt water onto the coated surface of the rock slab at a distance of 1.0 to 10.0 mm from the vertical direction to the bottom of the container, and measuring the receding contact angle and the advancing contact angle of the droplet formed on the coated surface.

[0009] The rock surface wettability modifier of the present invention can hydrophilize rock surfaces, and is therefore expected to be useful as an agent for increasing the amount of carbon dioxide stored in rock. In a preferred embodiment, the rock surface wettability modifier of the present invention contains silica particles with a cumulative particle size distribution D90 of 5 to 200 nm, i.e., does not contain coarse particles. Therefore, even when injected into underground rock, it can penetrate without blocking pores, and is expected to hydrophilize the rock surfaces that make up the pores, thereby contributing to an increase in the amount of carbon dioxide stored in rock. Furthermore, according to a wettability evaluation method included in the present invention, the wettability of rock surfaces imparted by the wettability modifier can be evaluated.

[0010] Fig. 1 shows the shapes of droplets (salt water) on aged substrates A and B of Examples 1 to 5, which were coated with nanofluids prepared by diluting the wettability modifiers of Examples 1 to 5 so that the silica concentration was 0.5% by mass, and the shapes of droplets (salt water) on the (uncoated) substrate of Comparative Example 1. Fig. 2 is a schematic diagram of droplet contact angle measurement using the inclined plate contact angle method, showing the advancing angle (θa) and receding angle (θr) of the droplet.

[0011] [Rock Surface Wettability Adjuster] The present invention relates to a rock surface wettability adjuster (hereinafter simply referred to as a wettability adjuster) for increasing the amount of carbon dioxide stored in rock by hydrophilizing the rock surface. Examples of rocks that can be hydrophilized with the wettability adjuster of the present invention include sedimentary rocks and igneous rocks. Sedimentary rocks include conglomerate, sandstone, siltstone, mudstone, limestone, carbonate rock, and chert. Igneous rocks include basalt, andesite, dacite, rhyolite, dolerite, porphyrite, quartz porphyry, gabbro, diorite, and granite. Minerals that make up these rocks (quartz, calcite, olivine, pyroxene, amphibole, mica, feldspar, etc.) and glass can also be hydrophilized with the wettability adjuster of the present invention. For convenience, these are also considered to be rocks in the broad sense of the term in the present invention. Furthermore, the physical properties of the rock are not particularly limited, but rocks having a pore volume of 5% to 50%, 5% to 30%, or 10% to 30%, more preferably 10% to 30%, and liquid permeability of 0.1 mD to 100 D, 0.1 mD to 10 D, 0.1 mD to 1 D, 0.1 mD to 500 mD, 1 mD to 500 mD, 10 mD to 500 mD, or 10 mD to 300 mD, more preferably 10 mD to 300 mD, can be used. Note that in this specification, the liquid permeability refers to absolute permeability, i.e., the permeability evaluated by placing rock under a steady flow of saltwater or the like and judging from the pressure difference between the inlet and outlet sides.

[0012] The wettability control agent of the present invention comprises a silica sol containing (a) silica particles having an average primary particle size of 5 to 100 nm and (b) an aqueous medium. At least a portion of the (a) silica particles may be coated with (c) a silane compound having a hydrophilic organic group.

[0013] As the silica sol containing (a) silica particles and (b) aqueous medium, for example, aqueous silica sol can be used. Aqueous silica sol refers to a colloidal dispersion system in which an aqueous solvent (i.e., (b) aqueous medium) is used as a dispersion medium and colloidal silica particles (i.e., (a) silica particles) are used as a dispersoid, and can be produced by a known method using water glass (aqueous sodium silicate solution) as a raw material. The average primary particle size of aqueous silica sol refers to the average primary particle size of the colloidal silica particles, which are the dispersoid.

[0014] In the present invention, the average primary particle diameter of the aqueous silica sol (colloidal silica particles) refers to the specific surface area diameter or the Sears particle diameter measured by the nitrogen adsorption method (BET method) unless otherwise specified. The specific surface area diameter (average particle diameter (specific surface area diameter) D (nm)) measured by the nitrogen adsorption method (BET method) is the specific surface area S (m 2 From the particle size (D / g), the particle size is given by the formula D(nm) = 2720 / S. The Sears particle size refers to the average particle size measured based on the method described in the literature as "A rapid method for measuring colloidal silica particle size" by G. W. Sears, Anal. Chem. 28(12), 1981, p. 1956. In detail, when 1.5 g of SiO 2 The equivalent diameter (specific surface area diameter) is calculated from the specific surface area of ​​the colloidal silica, which is determined from the amount of 0.1 N NaOH required to titrate colloidal silica equivalent to 100% of the total weight of the colloidal silica from pH 4 to pH 9. In the present invention, the average primary particle diameter of the (a) silica particles, i.e., for example, aqueous silica sol (colloidal silica particles), as determined by the nitrogen adsorption method (BET method) or the Sears method is 5 to 100 nm, and can be, for example, 5 to 70 nm, 5 to 60 nm, 5 to 50 nm, or 5 to 30 nm.

[0015] In addition, (a) silica particles in a silica sol containing silica particles, i.e., (a) silica particles in a wettability modifier, or (a) silica particles in a fluid sample obtained by mixing a wettability modifier with salt water or the like, can be measured by dynamic light scattering to determine their average particle size (DLS average particle size) and their dispersion state (whether the silica particles are in a dispersed or aggregated state). The DLS average particle size represents the average value of secondary particle diameters (dispersed particle diameters), and the DLS average particle diameter in a completely dispersed state is said to be about twice the average primary particle diameter (the specific surface area diameter obtained by measurement using the nitrogen adsorption method (BET method) or the Sears method, and represents the average value of primary particle diameters). The larger the DLS average particle size, the more it can be determined that the silica particles in the medium are in an aggregated state. For example, an example of an aqueous silica sol is the aqueous silica sol Snowtex (trade name) ST-O manufactured by Nissan Chemical Industries, Ltd., which has an average primary particle size (BET method) of 10 to 11 nm and a DLS average particle size of 15 to 20 nm. As shown in the examples described below, the silica sol (wettability modifier) ​​of a synthetic example prepared using this aqueous silica sol and the test fluid (nanofluid) containing it have a DLS average particle size of 25 nm or less, indicating that the silica particles are substantially dispersed in the medium. In the present invention, the average particle size (DLS particle size) of the (a) silica particles can be, for example, 1 to 100 nm, 1 to 50 nm, 3 to 30 nm, 5 to 15 nm, or 5 to 70 nm. By making the DLS particles larger than 1 nm, the particles do not aggregate in the aqueous silica sol and become more stable, and by making the DLS particles smaller than 100 nm, they can easily penetrate into the pores of sandstone and carbonate rock present in underground oil field layers.

[0016] Particles with a DLS average particle size larger than 100 nm are not preferred because they do not penetrate the gaps in the underground layer and clog the gaps. Therefore, it is preferable to use an aqueous silica sol that does not contain coarse particles, for example, a silica sol in which the cumulative particle size distribution D90 of the average particle size (DLS average particle size) measured by dynamic light scattering is 5 to 200 nm, 5 to 150 nm, 5 to 100 nm, or 5 to 70 nm. Furthermore, it is preferable that the silica particles contained in the aqueous silica sol have salt resistance such that, when they come into contact with saltwater contained in the underground layer, the silica particles do not aggregate to an extent that exceeds the DLS particle size or D90 range. The D90 is the particle size that represents the cumulative 90% of the cumulative particle size distribution from the fine particle side. The cumulative particle size distribution can be obtained, for example, by dynamic light scattering or image analysis. In the present invention, the cumulative particle size distribution value can be measured using a dynamic light scattering particle size analyzer. Methods for analyzing the D value include the number distribution method and the volume distribution method. The number distribution method regards particles as perfect circles of the same area as the particle itself, and measures the percentage of particles having a specific particle diameter. The volume distribution method, on the other hand, assumes that if the particle density is constant, volume and weight are proportional, and measures the mass percentage of particles of a specific particle diameter in a given amount of sample. In the present invention, it is preferable to determine the D value (D90) using the volume distribution method.

[0017] The aqueous silica sol can be a commercially available product. Aqueous silica sols with a silica concentration of 5 to 50% by mass are generally commercially available, which is preferred because they are easily available. Aqueous silica sols include alkaline aqueous silica sols and acidic aqueous silica sols, and both can be used, but acidic aqueous silica sols are preferred. Examples of commercially available acidic aqueous silica sols include Snowtex (trade name) ST-OXS, ST-OS, and ST-O.

[0018] In the wettability adjuster of the present invention, the (a) silica particles may be at least partially coated with (c) a silane compound having a hydrophilic organic group.

[0019] In the present invention, "coated with a silane compound" refers to an embodiment in which the surface of a silica particle is coated with a silane compound, and also includes an embodiment in which a silane compound is bonded to the surface of a silica particle. "An embodiment in which a silane compound is coated on the surface of a silica particle" may refer to an embodiment in which a silane compound coats at least a portion of the surface of a silica particle, i.e., an embodiment in which the silane compound covers a portion of the surface of a silica particle, and an embodiment in which the silane compound covers the entire surface of a silica particle. This embodiment does not require bonding between the silane compound and the surface of a silica particle. Furthermore, "an embodiment in which a silane compound is bonded to the surface of a silica particle" may refer to an embodiment in which a silane compound is bonded to at least a portion of the surface of a silica particle, i.e., an embodiment in which the silane compound is bonded to a portion of the surface of a silica particle and covers at least a portion of the surface, and an embodiment in which the silane compound is bonded to the entire surface of a silica particle and covers the entire surface.

[0020] The (c) silane compound may be a silane compound having a hydrophilic organic group such as an epoxy group-containing organic group, an amino group-containing organic group, a hydroxy group-containing organic group, or a carboxy group-containing organic group. In addition to the hydrophilic organic group, the (c) silane compound preferably has a hydrolyzable group such as an alkoxy group, an acyloxy group, or a halogen group.

[0021] Specific examples of these (c) silane compounds include silane coupling agents having an epoxy group-containing organic group or an amino group-containing organic group. Examples of the silane coupling agent having an epoxy group-containing organic group include 3-glycidoxypropyltrimethoxysilane, 3-glycidoxypropyltriethoxysilane, 3-glycidoxypropylmethyldimethoxysilane, 3-glycidoxypropylmethyldiethoxysilane, 3-glycidoxypropyltriethoxysilane, 2-(3,4-epoxycyclohexyl)propyltrimethoxysilane, 2-(3,4-epoxycyclohexyl)propyltriethoxysilane, 2-(3,4-epoxycyclohexyl)ethyltrimethoxysilane, 2-(3,4-epoxycyclohexyl)ethyltriethoxysilane, 2-(3,4-epoxycyclohexyl)methyltrimethoxysilane, 2-(3,4-epoxycyclohexyl)methyltriethoxysilane, 1-(3,4-epoxycyclohexyl)methyltrimethoxysilane, and 1-(3,4-epoxycyclohexyl)methyltriethoxysilane. Examples of the silane coupling agent having the amino group-containing organic group include 3-(2-(2-aminoethylamino)ethylamino)propyltriethoxysilane, N-2-(aminoethyl)-3-aminopropylmethyldimethoxysilane, N-2-(aminoethyl)-3-aminopropyltrimethoxysilane, 3-aminopropyltrichlorosilane, 3-aminopropyltrimethoxysilane, 3-aminopropyltriethoxysilane, 3-aminopropylmethyldimethoxysilane, 3-aminopropylmethyldiethoxysilane, 3-triethoxysilyl-N-(1,3-dimethylbutylidene)propylamine, N-phenyl-3-aminopropyltrimethoxysilane, and N-phenyl-3-aminopropyltriethoxysilane.

[0022] The silica particles according to the present invention, at least a portion of which is coated with a silane compound having a hydrophilic organic group (also referred to as "silica particles surface-treated with a silane compound"), can be obtained, for example, by adding a silane compound to an aqueous silica sol, followed by heat treatment at 50 to 100°C for about 1 to 20 hours. In this case, the amount of silane compound added relative to the silica particles (silica solid content) in the aqueous silica sol can be, for example, a mass ratio of silane compound / silica particles = 0.1 to 10.0. The amount of surface treatment with the silane compound, i.e., the amount of silane compound bonded to the silica particle surface, is determined based on the amount of silane compound bonded to the silica particle surface within 1 nm of the silica particle surface. 2 It is preferable that the number of particles is, for example, about 0.1 to 12 per particle.

[0023] The hydrophilization of rock surfaces (rock surface wettability) due to the wettability modifier of the present invention can be evaluated using the inclined plate contact angle method. The detailed procedure for the rock surface wettability evaluation method encompassed by the present invention is as follows. First, a rock slab to be tested is placed at an inclination angle of 15° in a container filled with carbon dioxide at a pressure of 10 MPa and a temperature of 50°C. The rock slab can have a surface coated with the wettability modifier of the present invention. 0.1 to 10 μL of saltwater is dropped onto the rock slab (coated surface) from a distance of 1.0 to 10.0 mm perpendicular to the bottom of the container. The receding and advancing contact angles of the droplet formed on the rock slab (coated surface) are then measured. This method for evaluating the wettability of rock surfaces is also within the scope of the present invention. Figure 2 shows a schematic diagram of droplet contact angle measurement using the inclined plate contact angle method. The inclination angle α is 15°, and in Figure 2, θa represents the advancing contact angle (also referred to as the advancing angle), and θr represents the receding contact angle (also referred to as the receding angle). In general, a contact angle of less than 50° can be evaluated as having strong water wettability, 50° or more and less than 70° as having weak water wettability, and 70° or more and less than 110° as having intermediate wettability (wettability intermediate between water wettability and oil wettability).

[0024] In the above-mentioned evaluation method, the wettability adjuster of the present invention can adjust the hydrophilicity of a rock surface by coating the surface of a rock slab (without a coated surface) with a receding contact angle and an advancing contact angle of 70 to 110° under the condition that 6 μL of saltwater is dropped from a distance of 3.5 to 4.0 mm from the vertical direction to the bottom of the container. The wettability adjuster of the present invention can adjust the hydrophilicity of the rock surface so that the receding contact angle on the coated surface is 5 to 70° and the advancing contact angle is 5 to 70°. In other words, the wettability adjuster of the present invention adjusts a rock surface with intermediate wettability to one with strong to weak water wettability. The receding contact angle is preferably 5 to 70°, 10 to 60°, 10 to 50°, or 10 to 40°. The advancing contact angle is preferably 5 to 70°, 15 to 65°, 15 to 50°, or 20 to 50°. By adjusting the contact angles within the above ranges, the rock surface becomes strongly to weakly wettable, and hydrophobic CO 2 As a result, CO 2 is more likely to be bound in the voids inside the rock, 2 Storage volume increases.

[0025] The saltwater used for measuring the contact angle may have a salt concentration of 0.1 to 30% by mass, or 0.1 to 20% by mass, 0.1 to 10% by mass, or 1 to 5% by mass. For example, the saltwater may contain calcium ions and magnesium ions, with sodium ions as the main component, and have a salt concentration of 0.1 to 30% by mass.

[0026] The wettability modifier of the present invention makes the rock surface hydrophilic (the wettability of the rock surface) and reduces CO 2The effect of increasing the underground storage volume of carbon dioxide can also be evaluated by measuring interfacial tension. As an example, interfacial tension can be measured by the hanging drop method in a container filled with carbon dioxide at a pressure of 10 MPa and a temperature of 50°C. The hanging drop method is a method in which a liquid is dropped from the tip of a vertically placed thin tube (needle) and the surface tension of the liquid is calculated from the shape of the largest hanging drop that does not fall. Specifically, first, the wettability modifier according to the present invention is diluted with salt water (e.g., 3 mass% salt water) so that the silica particle concentration becomes a predetermined concentration (e.g., 0.1 to 0.5 mass%), thereby preparing a nanofluid (sample) for interfacial tension measurement. As an example of a measurement system, a Pendant Drop Interfacial Tension Cell (MODEL IFT-05 / 10 / 20) manufactured by Corelab is used, which is sealed and a CO accumulator filled with the nanofluid (sample) and a CO 2 detector are installed. 2 All the equipment involved in the contact angle measurement, including the ISCO pump filled with CO, is heated to 50°C. 2 is injected into the measurement chamber to a pressure of 10 MPa. Then, the nanofluid (sample) and CO 2 The nanofluid (sample) is contacted with the 2 After dissolving the nanofluid, one drop (6-7 μL) of the nanofluid is discharged at a flow rate of 0.5 mL / min from a needle with a diameter of 1.5 mm placed at the top of the measurement chamber, and the interfacial tension is evaluated from the obtained shape. Methods for analyzing the interfacial tension from the droplet shape include the d / D method and the Young-Lapiace method (curve fitting method), and either method can be used for evaluation. In the present invention, the wettability modifier (CO 2 The interfacial tension of the nanofluid (nanofluid having CO dissolved therein) can be, for example, 1 to 35 mN / m, 5 to 35 mN / m, 10 to 35 mN / m, 25 to 35 mN / m, or 20 to 35 mN / m. By using a wettability control agent having an interfacial tension in the above range, CO can be easily transported into the narrower flow paths in the core. 2 can enter, and CO 2 On the other hand, if the interfacial tension becomes too low, such as 1 mN / m or less, CO2 will leak through the gaps in the rock. 2 This is not preferable because it makes the material more susceptible to leakage.

[0027] CO by the wettability preparation of the present invention 2 The effect of increasing underground storage capacity is 2 This can be assessed by measuring the CO 2 For example, the storage volume was measured by applying nanofluid (e.g., a wettability adjuster adjusted to a silica particle concentration of 0.5 mass% in 3 mass% salt water) and CO 2 CO is injected in this order, followed by salt water. 2 In assessing storage capacity, residual CO calculated from CT values ​​after saltwater injection 2 It can be evaluated from the saturation rate. 2 Residual CO in storage volume evaluation 2 The saturation percentage can be 10 to 100% by volume, 10 to 90% by volume, 25 to 100% by volume, 25 to 70% by volume, 25 to 60% by volume, 25 to 50% by volume, or 25 to 45% by volume. 2 In assessing the storage volume, the aforementioned residual CO 2 The saturation rate (with wettability modifier applied) was significantly higher when salt water was used instead of nanofluid (salt water (first run), CO 2 , saltwater (second injection), and the residual CO calculated after the second saltwater injection. 2 The increase can be 10% or more, 10% to 500%, 10% to 300%, 10% to 200%, 10% to 100%, 10% to 80%, or 20% to 80% compared to the value of the saturation rate (without the application of a wettability modifier). Furthermore, a nanofluid (for example, a wettability modifier adjusted to a silica particle concentration of 0.5% by mass in 3% by mass salt water), CO 2 CO is injected in this order, followed by salt water. 2 In assessing storage capacity, CO 2 Initial CO from CT value after injection 2 The saturation rate can be evaluated. 2 Initial CO storage volume evaluation 2 The saturation percentage can be 10 to 100% by volume, 10 to 90% by volume, 20 to 90% by volume, 30 to 90% by volume, 30 to 80% by volume, 45 to 80% by volume, or 45 to 70% by volume. 2 In assessing the storage volume, the initial CO 2The saturation rate (with wettability modifier applied) was significantly higher when salt water was used instead of nanofluid (salt water (first run), CO 2 , salt water (second time) and CO 2 Initial CO calculated after injection 2 The increase can be 10% or more, 10% to 500%, 10% to 300%, 10% to 200%, 10% to 100%, 10% to 80%, 10% to 70%, 10% to 60%, 10% to 50%, 20% to 80%, 20% to 70%, or 25% to 70% compared to the saturation rate (without application of a wettability control agent).

[0028] The CT value is calculated by dividing the X-ray absorption value of a substance by 2000, with air being -1000 HU (Hounsfield Unit) and water being 0 HU. The higher the CT value, the whiter the CT image will appear. Carbon dioxide (CO 2 The saturation rate of carbon dioxide (what percentage of the fluid inside the rock has been replaced by carbon dioxide / how much carbon dioxide remains inside the rock after the brine injection) can be calculated using this CT value. In addition, since the obtained CT value can be converted into image data, calculations can also be made by converting image data reconstructed from the CT value back into a CT value. Note that the CT value depends on the amount of X-ray absorption by the substance filled inside the sample, so by acquiring the CT value of each pure substance in advance, it is possible to identify the substance contained inside the sample and calculate its volume fraction. Specifically, after injecting the nanofluid or brine into the rock, CO 2 At this time, CO is injected into the rock. 2 The average CT value of the entire rock before and after injection is obtained by CT scanning, and the CO 2 Calculate the volume ratio of the initial CO 2 Calculate the saturation percentage, e.g., CO after nanofluid injection. 2 is injected (CO 2 Initial CO after partial replacement of nanofluid with 2 Saturation (1) and CO after brine injection 2 is injected (CO 2 Initial CO after partial replacement of salt water with 2The saturation rate (2) is defined as follows: Initial CO 2 Saturation rate (1) = (CT nano -CT CO2ni ) / (CT nano -CT CO2 ) Initial CO 2 Saturation rate (2) = (CT brine -CT CO2bi ) / (CT brine -CT CO2 ) CO 2 CT value (at saturation): CT CO2 CT value of nanofluid (at saturation): CT nano CT value of saltwater (saturated): CT brine After nanofluid saturation, CO 2 CT value after press-fitting: CT CO2ni , CO after salt water saturation 2 CT value after press-fitting: CT CO2bi

[0029] Following the above operation, CO 2 The operation of injecting brine into the injected rock is carried out, and the average CT value of the entire rock after brine injection (with / without application of nanofluid) is obtained by CT scanning. The CT value when the rock is filled with brine (the CT value in the brine saturated state) and the CT value when CO 2 CO from the difference in CT value after injection and saltwater injection 2 Calculate the volume ratio of residual CO 2 Calculate the saturation rate. For example, apply the nanofluid first (nanofluid saturation) and 2 Residual CO after brine injection via injection 2 Saturation rate (1), and salt water was applied first (saturated salt water) and CO 2 Residual CO after brine injection via injection 2 The saturation rate (2) is defined as follows: 2 Saturation rate (1) = (CT nano -CT CO2nr ) / (CT nano -CT CO2 ) ・Residual CO 2 Saturation rate (2) = (CT brine -CT CO2br ) / (CT brine -CTCO2 ) CO 2 CT value (at saturation): CT CO2 CT value of nanofluid (at saturation): CT nano CT value of saltwater (saturated): CT brine After nanofluid saturation, CO 2 CT value after saltwater injection: CT CO2nr , CO after salt water saturation 2 CT value after saltwater injection: CT CO2br

[0030] As shown in the above formula, CO 2 Nanofluids, CO as a reference value for assessing storage capacity 2 The CT values ​​of the salt water and the CO contained in the sample must be measured in advance before the test begins. 2 , salt water, and nanofluid. 2 , saltwater, and nanofluid ratios can be expressed as volume percentages.

[0031] CO 2 The initial saturation rate of the nanofluid (or saltwater) and CO 2 In the evaluation, CO 2 The CT value of the nanofluid (or saline) filled state before the injection of CO 2 After injection of CO 2 The initial CO is calculated as the ratio of the CT value at the time when the CO is injected and reaches an equilibrium state. 2 The saturation rate of 30% by volume is CO 2 % of the area occupied by the nanofluid (or brine) before the injection of CO 2 By injecting 30% by volume of CO 2 This means that it has been replaced by CO 2 The calculation of the residual saturation rate is based on the aforementioned nanofluid (or saltwater), CO 2 In the evaluation, when the total pore volume of the rock is taken as 100% by volume, after the injection of salt water, CO 2 That is, the remaining CO 2A saturation rate of 30% by volume means that CO is added to 30% of the pore volume of the rock by injecting salt water. 2 This means that there is a residual

[0032] The present invention also relates to a method for adjusting the surface wettability of an underground rock surface, comprising the steps of: adjusting the rock surface wettability adjuster in an aqueous medium to a silica particle concentration of 0.001 to 30% by mass; and injecting the rock surface wettability adjuster into an underground formation. The present invention also relates to a method for storing carbon dioxide in an underground formation, comprising the steps of: adjusting the rock surface wettability adjuster in an aqueous medium to a silica particle concentration of 0.001 to 30% by mass; and injecting carbon dioxide into the underground formation at 10 to 300°C and under a pressure of 0.1 to 100 MPa.

[0033] The wettability adjuster of the present invention can be diluted as desired with an aqueous medium such as salt water, groundwater, or river water to set the silica particle concentration at 0.001 to 30 mass %, and then used for surface treatment of rocks (adjusting the wettability of the surface). For example, when the rock is underground, the wettability adjuster can be coated on the rock surface by injecting it into the bedrock underground using an underground injection well pipe, and the wettability can be adjusted by CO 2 This will increase the amount of CO stored underground. 2 CO reaches a supercritical state at 31.1°C and 7.28 MPa or higher. 2 There is no limitation on the form of injection, but CO can be used in the gas phase, liquid phase, or supercritical fluid. 2 There are no particular limitations on the underground reservoir into which CO is injected, but the method can be applied to underground reservoirs having temperatures of 10°C to 300°C, 10°C to 200°C, 10°C to 150°C, 20°C to 150°C, or 30°C to 150°C and pressures of 0.1 MPa to 200 MPa, 0.1 MPa to 100 MPa, 0.1 to 50 MPa, 0.1 to 20 MPa, 0.1 to 10 MPa, 0.1 to 5 MPa, 0.2 to 5 MPa, 7 MPa to 100 MPa, 7 MPa to 50 MPa, 7 MPa to 20 MPa, or 7 MPa to 100 MPa. 2 When used at temperatures and pressures where CO is in the liquid phase or supercritical state, more CO is released underground. 2 The wettability adjuster of the present invention is preferably used to store CO in underground formations. 2When storing the wettability adjuster and CO 2 The order and steps of injecting the wettability adjuster into the ground are not limited at all. For example, the wettability adjuster may be injected first, followed by CO 2 Injecting CO 2 After injecting the wettability adjuster, CO 2 After injecting the wettability modifier, a buffer such as salt water is injected, and then CO 2 After the wettability adjuster, CO 2 There are no particular limitations on the type of injection method as long as it is capable of injecting CO. 2 The underground storage area is not limited in any way, but may be an oil field, a gas field, an oil and gas field, a depleted oil field, a depleted gas field, a depleted oil and gas field, or an aquifer.

[0034] The present invention will be described in further detail below based on synthesis examples, examples, and comparative examples, but it should be understood that the present invention is not limited to these examples in any way.

[0035] (Measuring Instruments) DLS average particle size (dynamic light scattering particle size): A dynamic light scattering particle size measuring instrument, trade name Zetasizer Nano (manufactured by Spectris K.K., Malvern Division), was used. D90: The particle size at which the frequency is 90% of the volume distribution of particles detected by a dynamic light scattering particle size measuring instrument, trade name Zetasizer Nano (manufactured by Spectris K.K., Malvern Division), was used. Silica specific surface area: Calculated from the amount of nitrogen gas adsorption measured by a trade name MONOSORB (manufactured by Quantachrome Instruments). pH: A pH meter (manufactured by DKK Toa Corporation, trade name MM43X) was used. Electrical conductivity: An electrical conductivity meter (manufactured by DKK Toa Corporation, trade name CM-30R) was used. Contact angle and interfacial tension: A product manufactured by Corelab, trade name: Pendant Drop Interfacial Tension Cell (MODEL IFT-05 / 10 / 20) was used. 2 Evaluation of retention volume: An X-ray core holder (manufactured by Corelab, trade name FCH Series) and a CT scanning device (manufactured by SIEMENS, trade name SOMATOM Definition AS) were used.

[0036] (Removal of silane not bonded to silica particles) 2 g of the aqueous silica sol prepared in the synthesis example described below and 4 g of pure water were placed in a 15 ml centrifugal filter unit (trade name: Amicon Ultra-15, manufactured by Merck Ltd.), and centrifuged for 20 minutes at a centrifugal force of 2770 G. After centrifugation, the liquid discharged to the bottom of the unit was discarded, and the same mass of pure water as the discarded liquid was added to the aqueous silica sol concentrated on the filter to redisperse it, and then centrifuged again for 20 minutes at a centrifugal force of 2770 G. The above procedure was repeated a total of four times to obtain an aqueous silica sol from which silane not bonded to silica particles had been removed.

[0037] (Measurement of silica specific surface area) The aqueous silica sol or the aqueous silica sol from which the silane not bonded to the silica particles has been removed was dried on a hot plate at 80°C to obtain silica gel, which was then pulverized in a mortar and further dried at 60°C for 3 hours under vacuum to obtain a dried silica powder. The specific surface area (m2) of this powder was measured by the nitrogen adsorption method based on the BET theory. 2 / g) was measured (BET method, i.e., nitrogen gas BET method).

[0038] Synthesis Example 1: Preparation of Wettability Adjuster of Example 1 A 2,000 mL glass recovery flask was charged with 1,000 g of aqueous silica sol (Snowtex (trade name) ST-OXS, manufactured by Nissan Chemical Industries, Ltd., silica concentration = 10.4 mass%, average particle size measured by BET method: 5.1 nm, average particle size measured by DLS method: 8.6 nm) and a magnetic stirrer. Then, while stirring with the magnetic stirrer, 40.6 g of 3-glycidoxypropyltrimethoxysilane (manufactured by Evonik, trade name Dynasylan GLYMO) was added so that the mass ratio of silane compound to silica (colloidal silica particles) in the aqueous silica sol was 0.39. Subsequently, a cooling tube through which tap water was flowing was placed on top of the recovery flask, and the aqueous silica sol was heated to 60°C while refluxing, maintained at 60°C for 4 hours, and then cooled. After cooling to room temperature, the aqueous silica sol was removed. This aqueous silica sol was placed in a crucible, heated on a hot plate at 100°C to remove the solvent, and then calcined in an electric furnace at 1000°C for 30 minutes, and the resulting calcination residue was calculated as the silica solid content. An aqueous silica sol of Synthesis Example 1 was obtained, which was surface-treated with a silane compound, with a silane compound to silica mass ratio of 0.39, silica solid content = 11.2 mass%, pH = 2.9, electrical conductivity = 427 μS / cm, DLS average particle size = 18.4 nm, and D90 = 23 nm. The aqueous silica sol of Synthesis Example 1 was used as the wettability adjuster of Example 1 and in the following tests.

[0039] Synthesis Example 2: Preparation of Wettability Adjuster of Example 2 Into a 2,000 mL glass recovery flask, 1,000 g of aqueous silica sol (Snowtex (trade name) ST-O, manufactured by Nissan Chemical Industries, Ltd., silica concentration = 20.5 mass%, average particle size by BET method 11.0 nm, average particle size by DLS method 17.2 nm) and a magnetic stirrer were placed. Then, while stirring with the magnetic stirrer, 39.8 g of 3-glycidoxypropyltrimethoxysilane (manufactured by Evonik, trade name Dynasylan GLYMO) was added so that the mass ratio of silane compound to silica (colloidal silica particles) in the aqueous silica sol was 0.19. Next, a cooling tube through which tap water was flowing was placed on top of the recovery flask, and the aqueous silica sol was heated to 60°C while refluxing, maintained at 60°C for 4 hours, and then cooled. After cooling to room temperature, the aqueous silica sol was removed. In addition, pure water was added to adjust the silica solid content concentration of the extracted aqueous silica sol to 20.5% by mass.This aqueous silica sol was placed in a crucible, heated on a hot plate at 100 ° C to remove the solvent, and then calcined in an electric furnace at 1000 ° C for 30 minutes, and the resulting calcination residue was calculated as the silica solid content.An aqueous silica sol of Synthesis Example 2 was obtained, which was surface-treated with a silane compound, with a silane compound-to-silica ratio of 0.19, silica solid content = 20.5% by mass, pH = 2.8, electrical conductivity = 573 μS / cm, DLS average particle size = 19.8 nm, and D90 = 24 nm.The aqueous silica sol of Synthesis Example 2 was used as the wettability adjuster of Example 2 and was used in the following tests.

[0040] Synthesis Example 3: Preparation of Wettability Adjuster of Example 3 Into a 2,000 mL glass recovery flask, 1,000 g of aqueous silica sol (Snowtex (trade name) ST-O, manufactured by Nissan Chemical Industries, Ltd., silica concentration = 20.5 mass%, average particle size by BET method 11.0 nm, average particle size by DLS method 17.2 nm) and a magnetic stirrer were placed. Then, while stirring with the magnetic stirrer, 159.2 g of 3-glycidoxypropyltrimethoxysilane (manufactured by Evonik, trade name Dynasylan GLYMO) was added so that the mass ratio of silane compound to silica (colloidal silica particles) in the aqueous silica sol was 0.78. Subsequently, a cooling tube through which tap water was flowing was placed on top of the recovery flask, and the aqueous silica sol was heated to 60°C while refluxing, maintained at 60°C for 4 hours, and then cooled. After cooling to room temperature, the aqueous silica sol was removed. In addition, pure water was added to adjust the silica solid content concentration of the extracted aqueous silica sol to 20.5% by mass.This aqueous silica sol was placed in a crucible, heated on a hot plate at 100 ° C to remove the solvent, and then calcined in an electric furnace at 1000 ° C for 30 minutes, and the resulting calcination residue was calculated as the silica solid content.The aqueous silica sol of Synthesis Example 3 was obtained, which was surface-treated with a silane compound, with a silane compound-to-silica ratio of 0.78, silica solid content = 20.5% by mass, pH = 2.7, electrical conductivity = 417 μS / cm, DLS average particle size = 20.9 nm, and D90 = 23 nm.The aqueous silica sol of Synthesis Example 3 was used as the wettability adjuster of Example 3 and was used in the following tests.

[0041] Synthesis Example 4: Preparation of Wettability Adjuster of Example 4 Into a 2,000 mL glass recovery flask, 1,000 g of aqueous silica sol (Snowtex (trade name) ST-O-40, manufactured by Nissan Chemical Industries, Ltd., silica concentration = 40.5 mass%, average particle size by BET method 21.0 nm, average particle size by DLS method 35.8 nm) and a magnetic stirrer were placed, and then, while stirring with the magnetic stirrer, 41.7 g of 3-glycidoxypropyltrimethoxysilane (manufactured by Evonik, trade name Dynasylan GLYMO) was added so that the mass ratio of silane compound to silica (colloidal silica particles) in the aqueous silica sol was 0.20. Subsequently, a cooling tube through which tap water was flowing was placed on top of the recovery flask, and the aqueous silica sol was heated to 60°C while refluxing, maintained at 60°C for 4 hours, and then cooled. After cooling to room temperature, the aqueous silica sol was removed. In addition, pure water was added to adjust the silica solid content concentration of the extracted aqueous silica sol to 20.5% by mass. This aqueous silica sol was placed in a crucible, heated on a hot plate at 100 ° C to remove the solvent, and then calcined in an electric furnace at 1000 ° C for 30 minutes, and the resulting calcination residue was calculated as the silica solid content. The aqueous silica sol of Synthesis Example 4 was surface-treated with a silane compound, with a silane compound-to-silica ratio of 0.20, silica solid content = 20.5% by mass, pH = 3.0, electrical conductivity = 513 μS / cm, DLS average particle size = 35.8 nm, and D90 = 41 nm. The aqueous silica sol of Synthesis Example 4 was used as the wettability preparation of Example 4 and in the subsequent tests.

[0042] (Wettability Adjuster of Example 5) An aqueous silica sol (Snowtex (trade name) ST-O manufactured by Nissan Chemical Industries, Ltd., silica solid content = 20.5 mass%, average particle size measured by BET method: 11.0 nm, average particle size measured by DLS method: 17.2 nm, D90 = 21 nm) was adopted as the wettability adjuster of Example 5 and used in the subsequent tests.

[0043] Reference Example 1 To 0.098 g of anionic surfactant sodium dodecyl sulfate (Shinoline (trade name) 90TK-T, manufactured by New Japan Chemical Co., Ltd.), 3% by mass brine prepared in (Preparation Example 1) described below was added so that the total volume was 100 g, and the mixture was dissolved by stirring with a magnetic stirrer for 2 hours, thereby obtaining a sodium dodecyl sulfate aqueous solution-1. 0.05 g of fumed silica (Silicon Dioxide, manufactured by Sigma-Aldrich, average particle size by BET method: 10-20 nm) was weighed out, and the sodium dodecyl sulfate aqueous solution-1 was added to make a total volume of 50 g. The resulting solution was subjected to ultrasonic treatment for 15 minutes, thereby obtaining a fumed silica dispersion-1. The DLS average particle size of the obtained fumed silica dispersion-1 was 1400 nm. Furthermore, when the mixture was stored at 50°C for 5 hours, the silica component aggregated and settled, resulting in separation into two layers.

[0044] Reference Example 2 To 0.245 g of anionic surfactant sodium dodecyl sulfate (Shinoline (trade name) 90TK-T, manufactured by New Japan Chemical Co., Ltd.), 3% by mass brine prepared in (Preparation Example 1) described below was added so that the total volume was 100 g, and the mixture was dissolved by stirring with a magnetic stirrer for 2 hours, thereby obtaining a sodium dodecyl sulfate aqueous solution-2. 0.05 g of fumed silica (Silicon Dioxide, manufactured by Sigma-Aldrich, average particle size measured by the BET method: 10-20 nm) was weighed out, and the sodium dodecyl sulfate aqueous solution-2 was added to make a total volume of 50 g. The resulting solution was subjected to ultrasonic treatment for 15 minutes, thereby obtaining a fumed silica dispersion-2. The DLS average particle size of the resulting fumed silica dispersion-2 was 1974 nm. Furthermore, when the mixture was stored at 50°C for 5 hours, the silica component aggregated and settled, resulting in separation into two layers.

[0045] (Reference Example 3) 176.7 g of 1 mm diameter glass beads, 0.1 g of fumed silica (Sigma-Aldrich Silicon Dioxide, average particle size by BET method 10-20 nm), and 99.9 g of deionized water were placed in this order in a 250 cc polyethylene wide-mouth bottle (body diameter 62 mm), and the container was sealed. The container was ball milled in a universal mill at 190 rpm for 24 hours, and the resulting fluid was separated and recovered. The DLS average particle size was measured and found to be 128 nm, confirming that the dispersion was uniformly dispersed without two-layer separation. 50 g of the resulting dispersion was diluted with 50 g of 3 mass% salt water prepared in (Preparation Example 1) described below, and the dispersion stability at 50 ° C. was confirmed. The DLS particle size after 1 hour was 415 nm, and after 5 hours, the silica component aggregated and settled, resulting in two-layer separation.

[0046] Reference Example 4: 176.7 g of glass beads with a diameter of 1 mm, 0.1 g of fumed silica (Sigma-Aldrich Silicon Dioxide, average particle size measured by the BET method: 10-20 nm), and 99.9 g of aqueous sodium dodecyl sulfate solution were placed in a 250 cc polyethylene wide-mouth bottle (body diameter: 62 mm) in this order, and the bottle was sealed. The bottle was subjected to a ball milling treatment in a universal mill at 190 rpm for 24 hours, and the resulting fluid was separated and recovered. The DLS average particle size was measured and found to be 1648 nm.

[0047] Reference Example 5: 176.7 g of glass beads with a diameter of 1 mm, 0.1 g of fumed silica (Sigma-Aldrich Silicon Dioxide, average particle size measured by the BET method: 10-20 nm), and 99.9 g of aqueous sodium dodecyl sulfate solution-2 were placed in a 250 cc polyethylene wide-mouth bottle (body diameter: 62 mm) in this order, and the bottle was sealed. The bottle was subjected to a ball milling treatment in a universal mill at 190 rpm for 24 hours, and the resulting fluid was separated and recovered. The DLS average particle size was measured and found to be 1295 nm.

[0048] The above Reference Examples 1 to 5 evaluate the dispersion stability in saltwater containing divalent cations simulating seawater of nanofluids of silica nanopowder (fumed silica) using an anionic surfactant, as shown in Non-Patent Document 2. Non-Patent Document 2 shows that silica powder disperses in a sodium chloride solution, but as shown in the above results, the silica powder aggregates and settles in saltwater containing divalent cations simulating seawater, resulting in separation into two layers. In other words, it was confirmed that silica powder has poor dispersibility in the saltwater, making it difficult to inject into underground bedrock as envisioned by the present invention, and that even if injected, it is expected that the silica powder will aggregate and block pores in the bedrock.

[0049] (Preparation Example 1) Marine Art SF-1 (trade name, manufactured by Osaka Yaken Co., Ltd.) was added to pure water to dilute it to a salt concentration of 3% by mass, to prepare salt water (containing sodium chloride as the main component, and also containing anhydrous sodium sulfate, calcium chloride, magnesium chloride, sodium bicarbonate, and potassium bromide).

[0050] (Preparation Example 2) A 20 mm x 20 mm x 10 mm square quartz substrate was prepared and washed by pouring solvents onto the substrate surface in the following order: acetone, methanol, and pure water. The quartz substrate was then subjected to ozone plasma treatment for 15 minutes to remove contamination from the substrate. To simulate underground conditions, hydrochloric acid was added dropwise to the 3% by mass salt water prepared in (Preparation Example 1) to adjust the pH to 4, and the quartz substrate from which the contamination had been removed was immersed in this 3% by mass salt water adjusted to pH 4. After 30 minutes, the quartz substrate was removed and dried with pure nitrogen. The resulting quartz substrate was transferred to a sealable container, and lauric acid was added to 10% by mass with normal decane. -2 The diluted solution was poured into M, and a quartz substrate was immersed in it. After sealing the container, the quartz substrate was subjected to aging treatment by being kept at 50°C for 7 days, and after being removed from the container, the quartz substrate was dried by blowing pure nitrogen onto it, thereby obtaining an aged substrate A with improved wettability.

[0051] (Preparation Example 3) An aged substrate B with improved wettability was obtained in the same manner as in (Preparation Example 2), except that stearic acid was used instead of lauric acid.

[0052] (Preparation Example 4) An aged substrate C with improved wettability was obtained in the same manner as in (Preparation Example 2), except that a 20 mm x 20 mm x 10 mm square carbonate rock (manufactured by WARD'S Natural Science, trade name CALCITE-ICELAND SPAR (TEST Chips)) was used instead of the quartz substrate.

[0053] [Contact Angle Measurement] <Preparation of Nanoparticle-Coated Substrates> The wettability modifiers of Examples 1, 3, and 5 were diluted with the 3% by mass salt water prepared in (Preparatory Example 1) to a silica concentration of 0.5% by mass, and the wettability modifier of Example 2 was diluted to a silica concentration of 0.5%, 0.3%, or 0.1% by mass, to prepare the nanofluids. The aged substrates A, B, and C were immersed in the resulting nanofluids for 5 hours at room temperature, removed, and then dried with pure nitrogen to obtain substrates coated with the nanofluids. In the following description of [Contact Angle Measurement], the wettability modifier example number will also be used as the coated substrate number, nanofluid number, and example number for each evaluation. The aged substrates A, B, and C (none of which were coated with nanofluid) were used as the substrates for Comparative Example 1 and subjected to the contact angle measurements described below.

[0054] <Measurement> A pedestal for tilting the substrate at an angle of 15° from the horizontal was installed in a Pendant Drop Interfacial Tension Cell (Model IFT-05 / 10 / 20) manufactured by Corelab, and the substrates of Examples 1 to 5 and Comparative Example 1 were placed on the pedestal (see Figure 2), and the measurement space was sealed. Then, the salt water or CO2 prepared in (Preparation Example 1) was added to the cell. 2 All the equipment involved in the contact angle measurement, including the ISCO pump filled with CO, was heated to 50°C. 2The pressure was then pressed into the measurement space to 10 MPa. Then, a drop of saltwater (Preparation Example 1) was ejected (approximately 6 μL) from a distance of 3.5 to 4.0 mm from the vertical direction relative to the bottom of the container onto a rock slab placed in the measurement space at an inclination angle of 15° at a flow rate of 0.4 mL / min from a 1.5 mm diameter needle installed at the top of the measurement space. The angle formed by the droplet (saltwater) and the substrate (see Figure 2) was measured, and the contact angle (advancing angle and receding angle) was evaluated. In Figure 2, θa is the advancing angle and θr is the receding angle. Generally, a contact angle of less than 50° can be evaluated as strong water wettability, 50° to less than 70° as weak water wettability, and 70° to less than 110° as intermediate water wettability. The results are shown in Table 1. Figure 1 also shows the shapes of droplets (salt water) on the substrates of Examples 1 to 5, which were aged substrates A and B and coated with a nanofluid prepared by diluting the wettability adjuster of Examples 1 to 5 so that the silica concentration was 0.5% by mass, and the shapes of droplets (salt water) on the substrate (uncoated) of Comparative Example 1.

[0055] [Interfacial Tension Measurement] The wettability modifiers of Examples 1, 3, and 5 were diluted with the 3 mass % saltwater prepared in (Preparatory Example 1) so that the silica concentration was 0.5 mass %, and the wettability modifier of Example 2 was diluted so that the silica concentration was 0.5 mass %, 0.3 mass %, or 0.1 mass %, to prepare the respective nanofluids. Furthermore, the 3 mass % saltwater prepared in (Preparatory Example 1) was used as is as Comparative Example 2. A Corelab product, product name Pendant Drop Interfacial Tension Cell (MODEL IFT-05 / 10 / 20), was sealed, and an accumulator filled with each nanofluid having the above-mentioned predetermined silica concentration or 3 mass % saltwater and a CO 2 All the equipment involved in the interfacial tension measurement, including the ISCO pump filled with CO, was heated to 50°C. 2 was injected into the measurement chamber to a pressure of 10 MPa. Then, the nanofluid or salt water and CO 2 The nanofluid or saltwater was contacted with CO for 5 minutes. 2After dissolving the nanofluid, a drop of the nanofluid was discharged at a flow rate of 0.5 mL / min from a 1.5 mm diameter needle placed at the top of the measurement chamber, and the interfacial tension was evaluated by the suspension method. The results obtained by analysis using the Young-Laplace method are shown in Table 1.

[0056] [CO 2 Evaluation of storage volume] A Fontainebleau sandstone sample (hereinafter referred to as "core") measuring 1.5 inches in diameter and 2 inches in length, with a porosity of 9 to 12% by volume and a quartz content of 99% by mass or more, was prepared. The core was placed in an X-ray core holder, and the air and moisture in the core were removed by evacuating it using a vacuum pump for 1 hour. Thereafter, lauric acid was diluted with normal heptane for 10 minutes. -2 The synthetic oil diluted to M was introduced into an X-ray core holder using an ISCO pump, and the inside of the device was pressurized to 10 MPa. After the pressure stabilized, the device was left at room temperature for two days to obtain an oil-saturated core. The obtained oil-saturated core was transferred to a heat-resistant beaker, placed in a vacuum dryer, and vacuum-dried at 105 °C for one day to obtain an aged core.

[0057] The aging core was placed in an X-ray core holder, and the device was evacuated at room temperature for one hour with the valve downstream of the core holder closed to remove air from inside the device. 2 was injected into the aging core in a vacuum state at a rate of 3 cc / min, and the injection was continued until the pressure inside the core holder stabilized at 50°C and 10 MPa. 2 The resulting CO 2 CT scan of the aging core saturated with CO 2 The saturated CT value was obtained (CT CO2 ).

[0058] The wettability control agents of Examples 1 to 3 and Example 5 were each diluted with the 3 mass % salt water prepared in (Preparation Example 1) so that the silica concentration was 0.5 mass %, to prepare each nanofluid.

[0059] The aforementioned CO 2Each nanofluid obtained by the above procedure was injected into an aging core saturated with each nanofluid, while the valve downstream of the core holder was opened, while gradually increasing the flow rate at 1, 2, 3, and 4 cc / min. Injection was continued until the differential pressure at each flow rate became constant, and the liquid permeability at each flow rate was measured. The liquid permeability of the aging core measured at this time was 100 to 200 mD. Thereafter, the valve downstream of the core holder was closed, and each nanofluid was injected so that the internal pressure became 10 MPa. After the pressure stabilized, the aging core was held for 3 hours. By performing a CT scan of the aging core (in a state where the aging core was saturated with each nanofluid) after holding for 3 hours, the CT value (CT nano After that, CO was added to the aging core at 50°C to a pressure of 10 MPa. 2 After the pressure stabilized, the pressure was maintained for 2 hours to allow CO to enter the nanofluid in the aging core. 2 This process involves dissolving or saturating the CO 2 In the injection process, the nanofluid is injected with CO 2 The purpose is to eliminate the influence of CO 2 The pressure was 10 MPa applied from the upstream side of the core holder. 2 At 3 cc / min, 10 PV (Pore Volume: the total void volume in the total volume of the core) was injected, and part of the nanofluid in the aging core was replaced by CO 2 It was replaced by CO 2 By continuing to perform CT scans during the injection period, CO 2 The change in the saturation rate was observed, and the CT value (CO 2 The CT value when the pressure is pressed in and reaches equilibrium was obtained (CT CO2ni ).

[0060] The aforementioned CO 2The 3 mass % saltwater prepared in (Preparation Example 1) was injected into an aging core saturated with saltwater, while the flow rate was increased stepwise to 1, 2, 3, and 4 cc / min, with the valve downstream of the core holder open. At this time, the injection was continued until the differential pressure became constant at each flow rate, and the liquid permeability at each flow rate was measured. The liquid permeability of the aging core measured at this time was 100 to 200 mD. Thereafter, the valve downstream of the core holder was closed, and 3 mass % saltwater was injected so that the internal pressure became 10 MPa. After the pressure stabilized, the aging core was held for 3 hours. The CT value of the saltwater saturated state was obtained by CT scanning the aging core after holding for 3 hours (CT brine Then, CO was added to the aging core at 50°C to a pressure of 10 MPa. 2 After the pressure stabilized, the pressure was maintained for 2 hours, and CO was added to the 3 mass % salt water in the aging core. 2 This process involves dissolving or saturating the CO 2 During the injection process, CO is injected into the brine. 2 The purpose is to eliminate the influence of CO 2 The pressure was 10 MPa applied from the upstream side of the core holder. 2 At 3cc / min, 10 PV (Pore Volume: the total volume of voids in the total volume of the core) was injected, and part of the salt water in the aging core was replaced with CO 2 It was replaced by CO 2 By continuing to perform CT scans during the injection period, CO 2 The change in the saturation rate was observed, and the CT value (CO 2 The CT value when the pressure is pressed in and reaches equilibrium was obtained (CT CO2bi ).

[0061] From each CT value obtained by the above procedure, the initial CO 2 The saturation rate [volume %] was calculated. Examples 1 to 3, 5 (nanofluid application): Initial CO 2 Saturation rate (1) = (CT nano -CT CO2ni ) / (CT nano -CT CO2 ) Comparative Example 3 (no nanofluid applied): Initial CO2 Saturation rate (2) = (CT brine -CT CO2bi ) / (CT brine -CT CO2 )

[0062] The 3 mass % salt water prepared in (Preparation Example 1) was filled into an ISCO pump, and 10 MPa of CO 2 is introduced and held for more than 2 hours to dissolve it sufficiently. 2 This process produces saturated brine. In the subsequent brine injection process, CO 2 present in the system is removed. 2 The purpose of this is to eliminate the effect of the CT being dissolved in the injected saltwater. CO2ni or CT CO2bi In the system after the acquisition of this CO 2 Saturated salt water is added to the CO 2 The core holder was pressurized with 10 MPa at 3 cc / min for 10 PV, and the CO 2 During the saltwater injection period, CT scans were continued to be performed to measure the CO2 concentration calculated from the CT values. 2 The change in saturation rate was observed, and the CT value after 10 PV injection was obtained (nanofluid was applied first: CT CO2nr , without application of nanofluids: CT CO2br From each CT value obtained by the above procedure, the residual CO 2 The saturation rate [volume %] was calculated. Examples 1 to 3, 5 (nanofluid application): Residual CO 2 Saturation rate (1) = (CT nano -CT CO2nr ) / (CT nano -CT CO2 ) Comparative Example 3 (no nanofluid applied): residual CO 2 Saturation rate (2) = (CT brine -CT CO2br ) / (CT brine -CT CO2 )

[0063] <[(Initial CO in Examples 1 to 3 and 5 2 Saturation rate / initial CO in Comparative Example 3 2 saturation rate)−1×100> as the initial CO 2Increase in saturation rate (%), <[(Residual CO in Examples 1 to 3 and 5 2 Saturation rate / residual CO in Comparative Example 3 2 Saturation rate) - 1 × 100 > residual CO 2 The results are shown in Table 1 as the increase in saturation rate (%).

[0064]

[0065] As shown in Table 1, the substrate (blank) of Comparative Example 1, which was not coated with nanofluid, had intermediate wettability, with all contact angles of the saltwater droplets ranging from 70° to less than 110°. On the other hand, for the substrates of Examples 1 to 5, the contact angles of the saltwater droplets (advancing angle and receding angle for each of the two substrates) on Aged Substrate A and Aged Substrate B were all less than 50°, and on Aged Substrate C, the contact angles were less than 70° in Example 2 and less than 50° in Example 3. These results confirmed that the wettability of the substrate surface can be adjusted from intermediate wettability to very strong to weak wettability by applying a wettability adjuster.

[0066] Furthermore, as shown in Table 1, the interfacial tension in Comparative Example 2, which used 3 mass% salt water, was 39 mN / m, but when the nanofluids using the wettability modifiers prepared in Examples 1 to 3 and 5 were used, the interfacial tension was 29 to 34 mN / m, which was lower than the comparative examples. This is because the nanofluid and supercritical CO2 were more easily reacted with each other than with 3 mass% salt water. 2 This result suggests that the nanofluid obtained by diluting the wettability modifier with brine has a moderately low interfacial tension, allowing CO2 to enter narrower channels in the core that could not be injected with brine alone. 2 can penetrate into the initial CO 2 The saturation rate is increased, resulting in CO 2 This suggests that it has the effect of increasing storage volume.

[0067] Furthermore, as shown in Table 1, the residual CO 2 The saturation rate was 23% by volume, but the residual CO in Examples 1 to 3 and 5 after injecting the nanofluid obtained by diluting the wettability modifier with salt water was 2The saturation rate is high at 28 to 41% by volume, and the residual CO 2 The increase in saturation rate reached 22-78%. 2 The increase in saturation rate is due to the nanofluid changing the surface inside the core from intermediate wettability to very strong wettability to weak wettability, as inferred from the contact angle results mentioned above, and CO 2 As can be inferred from the results of the interfacial tension, CO 2 Nanofluids with moderately reduced interfacial tension against CO 2 This allows CO to exist as smaller supercritical fluids, droplets or bubbles, and allows CO to enter narrower channels within the core. 2 By allowing the entry of 2 The saturation rate was improved (Comparative Example 3: 41% by volume, Examples 1 to 3, 5: 53 to 67% by volume, initial CO 2 This is thought to be due to the influence of the increase in the saturation rate (29-63%). As described above, the results obtained suggest that the rock surface wettability adjuster of the present invention can make rock surfaces hydrophilic, and thus can be expected to be useful as an agent for increasing the amount of carbon dioxide stored within rock masses.

Claims

1. A rock surface wettability adjuster for increasing the amount of carbon dioxide stored within rock by making the rock surface hydrophilic, the rock surface wettability adjuster comprising a silica sol containing silica particles (a) having an average primary particle size of 5 to 100 nm and an aqueous medium (b).

2. A wettability adjuster for rock surfaces as described in claim 1, wherein the average particle size of the silica particles in the silica sol is 5 to 70 nm as determined by dynamic light scattering method.

3. A wettability adjuster for a rock surface according to claim 1 or 2, wherein the silica particles are at least partially coated with a silane compound (c) having a hydrophilic organic group, and the hydrophilic organic group is an epoxy group-containing organic group, an amino group-containing organic group, a hydroxyl group-containing organic group, or a carboxyl group-containing organic group.

4. A rock surface wettability adjuster according to any one of claims 1 to 3, wherein the cumulative particle size distribution D90 of the average particle size of the silica particles in the silica sol measured by dynamic light scattering method is 5 to 200 nm.

5. A rock surface wettability adjuster as claimed in any one of claims 1 to 4, in which, in a test in which 6 μL of salt water is dropped onto a rock slab at a distance of 3.5 to 4.0 mm from the vertical direction to the bottom of the container, the rock slab is placed at an inclination angle of 15° and is placed in a container filled with carbon dioxide at a temperature of 50°C under a pressure of 10 MPa, and the receding contact angle and advancing contact angle of the droplet formed on the rock slab are measured, the surface of the rock slab having receding and advancing contact angles of 70 to 110° is coated with a wettability adjuster, and the receding contact angle on the coated surface becomes 5 to 70°, and the advancing contact angle can be adjusted to 5 to 70°.

6. The wettability adjuster for rock surfaces according to claim 5, wherein the salt water has a salt concentration of 0.1 to 30 mass %.

7. A rock surface wettability control agent according to any one of claims 1 to 6, in which when a droplet of the wettability control agent diluted with 3 mass% salt water to give a silica particle concentration of 0.1 to 0.5 mass% is dropped at a flow rate of 0.5 mL / min from a vertically installed needle with a diameter of 1.5 mm in a container filled with carbon dioxide at a pressure of 10 MPa and a temperature of 50°C, the interfacial tension calculated from the shape of the largest droplet that does not fall is 1 to 35 mN / m.

8. A wettability adjuster for a rock surface as claimed in any one of claims 1 to 7, wherein, in a measurement of the amount of carbon dioxide stored in a state where an internal pressure is reached by injecting 3 mass% salt water (first time), 10 MPa carbon dioxide, and 3 mass% salt water into a rock in that order at a temperature condition of 50°C, the residual carbon dioxide saturation rate (with application of wettability adjuster) calculated from the CT value of the carbon dioxide remaining inside the rock after 3 mass% salt water is injected (second time), is increased by 10% or more compared to the residual carbon dioxide saturation rate (without application of wettability adjuster) calculated from the CT value of the carbon dioxide remaining inside the rock after 3 mass% salt water is injected (second time) in a measurement of the amount of carbon dioxide stored in a state where an internal pressure is reached by injecting 3 mass% salt water (first time), 10 MPa carbon dioxide, and 3 mass% salt water (second time) into a rock in that order at a temperature condition of 50°C, the residual carbon dioxide saturation rate (without application of wettability adjuster) calculated from the CT value of the carbon dioxide remaining inside the rock after 3 mass% salt water is injected (second time).

9. A wettability adjuster for a rock surface as claimed in any one of claims 1 to 8, wherein, in a measurement of the amount of carbon dioxide stored in a state where an internal pressure is reached by injecting 3 mass% salt water (first time), 10 MPa carbon dioxide, and 3 mass% salt water (second time) into a rock in that order under a temperature condition of 50°C, the initial carbon dioxide saturation rate (with wettability adjuster applied) calculated from the CT value of the carbon dioxide remaining in the rock after carbon dioxide injection is increased by 10% or more compared to the initial carbon dioxide saturation rate (without wettability adjuster applied) calculated from the CT value of the carbon dioxide remaining in the rock after carbon dioxide injection, in a measurement of the amount of carbon dioxide stored in a state where an internal pressure is reached by injecting 3 mass% salt water (first time), 10 MPa carbon dioxide, and 3 mass% salt water (second time) into a rock in that order under a temperature condition of 50°C, the initial carbon dioxide saturation rate (without wettability adjuster applied) calculated from the CT value of the carbon dioxide remaining in the rock after carbon dioxide injection.

10. A method for adjusting the surface wettability of an underground rock surface, comprising the steps of: adjusting the wettability adjuster for a rock surface according to any one of claims 1 to 9 in an aqueous medium to a silica particle concentration of 0.001 to 30 mass %; and injecting the resulting mixture into an underground layer.

11. A method for storing carbon dioxide in an underground layer, comprising the steps of: adjusting the wettability adjuster for rock surfaces according to any one of claims 1 to 9 in an aqueous medium to a silica particle concentration of 0.001 to 30 mass %; and injecting carbon dioxide into the underground layer at 10 to 300°C and under a pressure of 0.1 to 100 MPa.