Method for manufacturing non-stick pan liner

MYPI2025004665A0Undetermined Publication Date: 2024-08-14JOYOUNG CO LTD
View PDF 0 Cites 0 Cited by

Patent Information

Application Number
MYPI2025004665
Authority / Receiving Office
MY · MY
Patent Type
Applications
Current Assignee / Owner
Priority Date
2023-02-14
Filing Date
2023-11-15
Publication Date
2024-08-14

AI Technical Summary

Technical Problem

The non-stick performance of existing non-stick pans is affected by deformation during the molding process, and the non-stick coating cannot effectively prevent contact with hard particles, affecting the service life and performance.

Method used

Composite metal plates are used to form an anti-stick array through etching or engraving, and the stretching rate and expansion rate are controlled to make the pot. This ensures that the deformation of the anti-stick array is within the preset range and reduces the difference in thickness ratio between the side wall and the bottom wall of the pot. , to maintain the non-stick effect of the pan.

Benefits of technology

It effectively controls the thickness ratio between the side wall and the bottom wall of the pot, ensuring that the anti-stick array is within a controllable range, improving the non-stick performance of the pot, extending its service life, and avoiding the problem of non-stick coating falling off and sticking to the pot.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure PI2025004665_DRAWING_001
    Figure PI2025004665_DRAWING_001
  • Figure PI2025004665_DRAWING_002
    Figure PI2025004665_DRAWING_002
  • Figure PI2025004665_DRAWING_003
    Figure PI2025004665_DRAWING_003
Patent Text Reader

Abstract

A method for manufacturing a non-stick pan liner (30), comprising: providing a metal plate compounded with at least an outer metal layer (321), a heat equalizing layer (322) and an inner metal layer (323), and etching, engraving or pressing one side of the inner metal layer (323) to form an anti-stick array (33), wherein the anti-stick array (33) comprises a plurality of grooves or protrusions (S01); controlling an elongation to stretch the metal plate provided with the anti-stick array (33), and forming the pan liner (30) (S03); or controlling the elongation to form a pan liner blank first by stretching (S04), and then controlling an expansion ratio to expand the pan liner blank to form the pan liner (30) (S06). A thickness ratio of a side wall of the prepared pan liner (30) to a bottom wall of the pan liner (30) is 0.9 to 1.1, and a thickness ratio of the outer metal layer (321) to the inner metal layer (323) is 0.6 to 1.4, such that the grooves or protrusions that are subjected to stretching deformation in the anti-stick array (33) satisfy a preset range, and an area change of a region where the grooves or protrusions are located is then within a controllable range, such that rice and the anti-stick array (33) on the side wall of the pan liner (30) are kept in a preferable contact state. Fig. 2
Need to check novelty before this filing date? Find Prior Art

Description

A method for making a non-stick pan

[0001] This application claims priority to the Chinese patent application filed with the Patent Office of China on February 14, 2023, with application number CN202310112004.8 and invention name “A method for making a non-stick pan core”, the entire contents of which are incorporated by reference into this application. Technical Field

[0002] The present application belongs to the technical field of kitchen appliances, and in particular relates to a method for manufacturing a non-stick pan. Background Art

[0003] An existing non-stick pan has protrusions or grooves on its inner surface. By applying a non-stick coating within the grooves, the spatula is less likely to scrape the non-stick coating within the grooves when scraping the pan surface during cooking, thereby extending the service life of the non-stick coating. However, during the pot body forming process, the blank is often deformed using processing methods such as stamping and bulging to form the pot body structure. The pot body structure can be divided into a straight pot or a spherical pot structure based on the shape of the pot body sidewall. Specifically, for a straight pot body, the shape of the pot body can be stamped in a single step, while a spherical pot body requires a single stamping and a secondary bulging step. During the process of blank elongation and extrusion, the metal sheet in the center of the mold forms the bottom wall of the pot body, while the metal sheet in the outer portion forms the sidewalls of the pot body. When grooves and protrusions are formed on the surface of the metal sheet, the stretched part of the metal sheet will cause deformation of the grooves and protrusions. Excessive deformation will affect the non-stick performance of the pot. If the deformation is to be eliminated, the manufacturing cost and difficulty will be increased, the production efficiency will be low, and the defective rate will be high. The deformation mainly occurs at the side walls of the pot. Generally, the side walls of woks and frying pans are not the main cooking area, so the non-stick performance requirements of woks and frying pans are relatively lower, and the impact of deformation can be ignored. However, the side walls of the pot, which mainly serves as a container, are often in contact with food, and the impact of deformation needs to be considered. In addition, the non-stick coating set in the groove cannot guarantee that hard and fine particles will not contact the non-stick coating in the groove. If this problem occurs, its non-stick performance cannot be guaranteed. For this reason, zero coating non-stick is a common pursuit in the industry.

[0004] Summary of the Invention

[0005] The present application provides a method for manufacturing a non-stick pan inner shell to solve at least one of the above-mentioned technical problems.

[0006] The technical solutions adopted in this application are:

[0007] A method for making a non-stick pan inner shell comprises providing a metal sheet composited with at least an outer metal layer, a heat-uniform layer, and an inner metal layer; etching, engraving, or pressing one side of the inner metal layer to form an anti-sticking array, wherein the anti-sticking array comprises a plurality of grooves or protrusions; controlling the stretching rate to stretch the metal sheet provided with the anti-sticking array to form a pan inner shell; or controlling the stretching rate to first stretch the metal sheet into a pan inner shell blank, and then controlling the bulging rate to bulge the pan inner shell into the pan inner shell; the thickness ratio of the side wall of the manufactured pan inner shell to the bottom wall is 0.9 to 1.1, and the thickness ratio of the outer metal layer to the inner metal layer is 0.6 to 1.4, so that the grooves or protrusions in the anti-sticking array that are deformed by stretching are within a preset range.

[0008] As a preferred embodiment of the present application, the grooves or protrusions in the anti-sticking array that are subjected to tensile deformation are located on the side wall, and the deformation ratio along the axial direction of the side wall of the pot is 1.1 to 1.8 times.

[0009] As a preferred embodiment of the present application, the grooves or protrusions in the anti-sticking array that are subjected to tensile deformation are located on the side wall, and the deformation ratio along the circumferential direction of the side wall of the pot is 0.5 times to 1.01 times.

[0010] As a preferred embodiment of the present application, the equivalent diameter D of the groove or protrusion on the bottom wall of the pot and the thickness H1 of the inner metal layer satisfy the following relationship: 0.08≤D / H1≤3.

[0011] As a preferred embodiment of the present application, the grooves or protrusions in the anti-sticking array that are subjected to tensile deformation are located on the side walls, and the maximum diameter of the grooves on the side walls of the pot after deformation is no more than 1620 microns.

[0012] As a preferred embodiment of the present application, the grooves or protrusions in the anti-sticking array that are subjected to tensile deformation are located on the side wall, and the minimum diameter of the side wall of the pot after deformation is not less than 50 microns.

[0013] As a preferred embodiment of the present application, the ratio of the outer metal layer to the thickness of the metal sheet is 0.2 to 0.4.

[0014] As a preferred embodiment of the present application, the ratio of the inner metal layer to the thickness of the metal sheet is 0.1 to 0.4.

[0015] As a preferred embodiment of the present application, the ratio of the uniform heat layer to the thickness of the metal plate is 0.2 to 0.7.

[0016] As a preferred embodiment of the present application, the grooves in the anti-sticking array are independent single pits that are not interconnected, and the anti-sticking array in the middle of the bottom wall of the gallbladder covers the temperature measuring device.

[0017] Due to the adoption of the above technical solution, the beneficial effects achieved by this application are as follows:

[0018] In some embodiments of the present invention, in order to make the deformation of the anti-stick array within a preset range, the thickness ratio of the side wall of the pot and the bottom wall of the pot is made to be 0.9 to 1.1, and the thickness ratio of the outer and inner metal layers can be 0.6 to 1.4, thereby making the area deformation ratio of the area formed by the circumferential and axial directions between 1.1-0.9, thereby making the area change of the area where the grooves or protrusions are located within a controllable range, so that the rice maintains a better contact state with the anti-stick array on the side wall of the pot. BRIEF DESCRIPTION OF THE DRAWINGS

[0019] The drawings described herein are used to provide a further understanding of the present application and constitute a part of the present application. The illustrative embodiments of the present application and their descriptions are used to explain the present application and do not constitute an improper limitation on the present application. In the drawings:

[0020] FIG1 is a cross-sectional view of a cooking utensil provided in an embodiment of the present application;

[0021] FIG2 is a cross-sectional view of a pot provided in an embodiment of the present application;

[0022] FIG3 is a top view of the pot structure provided in an embodiment of the present application;

[0023] FIG4-1 is an electron microscope image of a cross section in the thickness direction of the bottom wall of the pot in a specific embodiment of the present application;

[0024] FIG4-2 is an electron microscope image of a cross section in the thickness direction of the side wall of the pot in a specific embodiment of the present application;

[0025] FIG5-1 is an electron microscope image of the anti-sticking array on the bottom wall of a pot in a specific embodiment of the present application;

[0026] FIG5-2 is an electron microscope image of the anti-sticking array on the side wall of the pot in a specific embodiment of the present application;

[0027] FIG6 is a regional distribution diagram of an anti-sticking array formed on a metal sheet in accordance with the second embodiment of the present application;

[0028] FIG7-1 is a partial enlarged view of the groove in region S1 provided in Example 2 of the present application;

[0029] FIG7-2 is a partial enlarged view of the groove in region S2 provided in Example 2 of the present application;

[0030] Among them, 10 pot body; 105 heating device; 20 pot cover; 30 pot inner lining; 31 bottom wall; 32 side wall; 33 anti-stick array; 301 cooking cavity; 321 outer metal layer; 322 uniform heat layer; 323 inner metal layer. DETAILED DESCRIPTION

[0031] In order to more clearly illustrate the overall concept of the present application, a detailed description is given below in an illustrative manner in conjunction with the accompanying drawings.

[0032] In the following description, many specific details are set forth to facilitate a full understanding of the present application. However, the present application may also be implemented in other ways different from those described herein. Therefore, the scope of protection of the present application is not limited to the specific embodiments disclosed below.

[0033] In addition, in the description of the present application, it should be understood that the terms "top", "bottom", "inside", "outside", "axial", "radial", "circumferential", etc., indicating orientations or positional relationships, are based on the orientations or positional relationships shown in the accompanying drawings. They are only for the convenience of describing the present application and simplifying the description, and do not indicate or imply that the device or element referred to must have a specific orientation, be constructed and operated in a specific orientation. Therefore, they cannot be understood as limitations on the present application.

[0034] In this application, unless otherwise expressly specified or limited, terms such as "installed," "connected," "connect," and "fixed" should be understood in a broad sense. For example, they may refer to fixed connection, detachable connection, or integration; mechanical connection, electrical connection, or communication; direct connection or indirect connection through an intermediate medium; and internal communication between two components or interaction between two components. Those skilled in the art will understand the specific meanings of the above terms in this application based on specific circumstances.

[0035] In this application, unless otherwise expressly specified and limited, a first feature "above" or "below" a second feature may be that the first and second features are in direct contact, or the first and second features are in indirect contact through an intermediate medium. In the description of this specification, the description with reference to the terms "one embodiment", "some embodiments", "example", "specific example", or "some examples" means that the specific features, structures, materials or characteristics described in conjunction with the embodiment or example are included in at least one embodiment or example of the present application. In this specification, the schematic representation of the above terms does not necessarily refer to the same embodiment or example. Moreover, the specific features, structures, materials or characteristics described may be combined in an appropriate manner in any one or more embodiments or examples.

[0036] This application proposes a method for making a non-stick pot lining, and more particularly, a method for making a zero-coating rice pot lining. This pot lining is primarily used in rice cooking utensils, such as electric rice cookers or pressure cookers. In other embodiments, it can be other cooking utensils with rice cooking functions. This application also proposes a zero-coating rice cooking pot lining, which can be made using the above-mentioned method.

[0037] The cooking utensil uses a zero-coating or zero-coating pot to cook rice. Most existing pots have coated pots, that is, a Teflon coating (scientific name polytetrafluoroethylene, English abbreviation PTFE) is provided on the inner surface of the pot. The zero-coating pot of the present application is different from the above-mentioned coated pot. The coating is no longer provided on the base material of the pot, so the inner side wall of the pot is a metal layer that can come into contact with food. The metal layer can be stainless steel. When cooking, food is directly contacted and cooked through the metal layer of the pot, thereby eliminating the coating shedding of the coated pot and the dietary health problems caused by the coating itself.

[0038] Referring to Figure 1, an electric rice cooker is shown. The electric rice cooker includes a pot body 10, a lid 20, and a pot inner 30. The pot inner 30 is disposed within the pot body 10. The inner side of the pot inner 30 contacts the rice via an inner metal layer 323. The lid 20 covers the pot body 10. The pot body 10 is provided with a heating device 105 for heating the pot inner 30. During the cooking process, a rice-water mixture is added to a cooking cavity 301 within the pot inner 30. The rice is cooked under the heating of the heating device 105 at the bottom of the pot inner 30.

[0039] The pot inner shell of the present invention is formed by etching, engraving, or pressing to form an anti-stick array, thereby achieving a non-stick effect. The anti-stick array has multiple grooves or protrusions. When rice contacts the protrusions, the presence of the protrusions and grooves reduces the contact area between the rice and the pot inner shell, changing the contact angle between the rice and the pot inner shell, thereby achieving a non-stick effect. In the manufacture of the pot inner shell, the grooves or protrusions are first formed on a metal sheet, and then the sheet is stretched into a cylindrical structure through a mold.

[0040] The inner pot of the present application adopts a metal plate with a composite structure, as shown in Figures 4-1 and 4-2. The metal plate includes at least an outer metal layer 321, a uniform heat layer 322, and an inner metal layer 323 that are composited together. The inner metal layer 323 is located on the side of the inner pot used to hold rice, which can meet the requirements of food hygiene. The base material of the inner metal layer 323 can be made of stainless steel. The uniform heat layer 322 uses a base material with a large thermal conductivity coefficient, which facilitates the rapid conduction of heat and achieves uniform heating of the inner pot. The uniform heat layer 322 can be made of aluminum. The outer metal layer 321 is located on the outside of the inner pot and can be used to self-heat under the action of a magnetic field, or to protect the uniform heat layer 322. The outer metal layer 321 can be made of stainless steel. In some other embodiments, the metal plate may include at least a uniform heat layer 322 and an inner metal layer 323 that are composited together.

[0041] In a specific embodiment of the present application, as shown in Figures 1, 2, and 3, the inner pot 30 includes a bottom wall 31, a side wall 32, and a cooking cavity 301. The cooking cavity 301 is open at the top, and the side wall 32 has a depth direction extending from one side of the bottom wall 31 to the open side of the cooking cavity 301, and a circumferential direction extending along the circumference of the bottom wall 31. One side of the inner metal layer 323 of the inner pot 30 is etched, engraved, or pressed to form an anti-stick array 33, and the anti-stick array 33 includes a plurality of grooves or protrusions; etching is a processing technology that uses the erosion effect on the surface of the inner metal layer 323 to remove metal from the stainless steel surface; engraving can be laser engraving or mechanical engraving, among which laser engraving processing technology is based on CNC technology and uses laser as a medium. The processing material is physically transformed by instantaneous melting and vaporization under the irradiation of laser engraving to achieve the processing purpose; pressing is to apply external force to the plate through stamping equipment, so that the plate is directly subjected to deformation force and deformed in the mold; etching and engraving are material removal manufacturing methods, and pressing is a deformation manufacturing method.

[0042] In a specific embodiment of the present application, in order to control the deformation of the grooves and protrusions to meet the preset range, the following method for manufacturing a non-stick pot inner shell is proposed. The manufacturing method is mainly achieved by controlling the change in the thickness of the pot inner shell, as follows:

[0043] Embodiment 1: It includes providing a metal plate that is at least composited with an outer metal layer 321, a uniform heat layer 322 and an inner metal layer 323, and etching, engraving or pressing one side of the inner metal layer 323 to form an anti-sticking array 33, wherein the anti-sticking array 33 includes a plurality of grooves or protrusions; controlling the stretching rate to stretch the metal plate provided with the anti-sticking array 33 to form a pot inner shell; or controlling the stretching to first stretch it into a pot inner shell blank, and then controlling the bulging rate to bulge the pot inner shell blank to form a pot inner shell; the thickness ratio of the side wall of the pot inner shell to the bottom wall of the pot inner shell is 0.9 to 1.1, and the thickness ratio of the outer metal layer 321 to the inner metal layer 323 is 0.6 to 1.4, so that the grooves or protrusions in the anti-sticking array 33 that are subjected to stretching deformation meet the preset range.

[0044] In Examples 1 and 2, as well as other specific embodiments of the present application, the percentage of the length of the material's plastic elongation to the original sample length is called the elongation, elongation, or extension. For example, 304 stainless steel has an elongation exceeding 40%, meaning a 1mm piece of stainless steel can be stretched at least 0.4mm. The present invention's manufacturing method ensures the smooth production of the inner pot. During the stretching process, the elongation should be controlled to not exceed the maximum elongation of the metal material used, thereby avoiding material breakage and necking. While ensuring these basic requirements, and in the presence of the anti-sticking array 33, further consideration should be given to the weakening of the anti-sticking effect of the anti-sticking array 33 due to tensile deformation. During the stretching process, the expansion of the metal sheet causes the anti-sticking array 33 to deform, specifically manifesting as the grooves in the anti-sticking array 33 becoming larger in the axial direction and potentially shrinking or expanding in the circumferential direction. In this case, the grooves deviate from their original, undeformed configuration, changing the optimal contact configuration between the rice and the inner pot surface, resulting in poor rice non-sticking effect on the sidewalls of the inner pot.

[0045] In Examples 1 and 2 of the present application and some other specific embodiments, based on the basic principle that the density of a metal material remains unchanged after plastic deformation, it is known that the mass remains unchanged before and after deformation. To maintain the consistency of density before and after deformation, the volume must also be consistent before and after deformation. Volume = length * width * thickness. Specifically, the length direction is the axial direction of the side wall of the inner pot, the width direction is the circumferential direction of the side wall of the inner pot, and the thickness direction is the wall thickness direction of the side wall of the inner pot. Therefore, the deformation relationship of the side wall of the inner pot in the axial, circumferential, and left-right directions is obtained; the magnitude of the deformation in the thickness direction depends on how the axial and circumferential directions are deformed. In other words, the magnitude of the deformation in the thickness direction can be used to indirectly reflect the magnitude of the deformation in the axial and circumferential directions, and then the deformation of the anti-sticking array 33 in the circumferential and axial directions can be obtained, thereby preventing the anti-sticking array 33 from being deformed too much.

[0046] In Examples 1 and 2 of the present application and some other specific embodiments, in the stamping manufacturing process, the deformation size in the wall thickness direction can be controlled by the size and shape of the cavity between the front and rear molds of the mold, or by the expansion pressure. Compared with directly controlling the circumferential and axial deformation rates of the anti-sticking array 33, controlling the deformation of the anti-sticking array 33 by the size in the thickness direction is in line with the control logic of the key parameters of the mold in the stamping manufacturing process. The control is simple and convenient, which can ensure the consistency of product molding and high product manufacturing quality. It is convenient to control the deformation amount of the anti-sticking array 33, avoid excessive deformation, and ensure the non-stick effect of the side wall of the pot. Specifically, in Example 1 of the present application, in order to keep the deformation of the anti-sticking array 33 within a preset range, the thickness ratio of the side wall of the pot to the bottom wall of the pot is made to be 0.9 to 1.1, and the area deformation ratio of the area formed by the circumferential and axial directions is between 1.1-0.9, so that the area change of the area where the grooves or protrusions are located is within a controllable range, thereby maintaining a better contact state between the rice and the anti-sticking array 33 on the side wall of the pot. Preferably, the thickness ratio a of the side wall of the pot to the bottom wall of the pot is between 1.01-1.1. Assuming that the ratio of shrinkage and expansion in the circumferential and axial directions is the same, the relationship between the deformation rate X and a can be obtained as follows: 1-X 2 =1 / a, and the solution is X∈[10%,30%], which can make the circumferential reduction rate at a minimum of 10% and a maximum of about 30%, thereby avoiding the formation of slits in the groove.

[0047] In Example 1 of the present application, the thickness ratio a of the side wall of the pot to the bottom wall of the pot can also be 0.9, 0.91, 0.92, 0.93, 0.94, 0.95, 0.96, 0.97, 0.98, 0.99, 1, 1.02, 1.3, 1.04, 1.05, 1.06, 1.07, 1.08, or 1.09; thereby ensuring that the area variation of the region where the grooves or protrusions are located is within a reasonable range. Figure 4-1 shows an enlarged cross-sectional view of the bottom wall of the pot under an electron microscope, where the bottom wall thickness is 1.243 mm. Figure 4-2 shows an enlarged cross-sectional view of the side wall of the pot under an electron microscope, where the side wall thickness is 1.295 mm. The ratio is 1.04.

[0048] In the first and second embodiments of the present application and some other specific implementations, during the stamping process, in the interior of the deformed material, any area that is subjected to excessive tensile stress will cause the material to be locally severely thinned or even torn; in any area that is subjected to excessive compressive stress, if the compressive stress exceeds the critical stress, the material will lose stability and wrinkle; in the composite metal sheet, relatively speaking, in the deformation of the pot, the outer metal layer 321 close to the inside is more subjected to tensile stress and tends to become thinner, while the inner metal layer 323 is more subjected to compressive stress and tends to become thicker. Therefore, in order to avoid excessive deformation of the thickness of the composite metal sheet, in the first embodiment of the present application, the inner The thickness of the outer metal layer 321 should not vary significantly, and should be kept as consistent as possible to avoid excessive compressive stress in the thickness direction of the inner metal layer 323, which could lead to excessive groove depth. The thickness ratio of the outer metal layer 323 to the inner metal layer 323 can be between 0.6 and 1.4. If the inner metal layer 323 is too thick and the outer metal layer 321 is too thin, the outer metal layer 321 will be more ductile than the inner metal layer 323, resulting in a deeper groove in the inner metal layer 323. If the inner metal layer 323 is too thin and the outer metal layer 321 is too thick, the inner metal layer 323 will be more ductile than the outer metal layer 321, resulting in a shallower groove in the inner metal layer 323. Increasing or decreasing the groove depth affects the optimal contact between the rice and the anti-stick array 33. Maintaining the grooves of the anti-stick array 33 within a reasonable deformation range ensures the non-stick properties of the pot sidewall.

[0049] In Example 1 of the present application, the thickness ratio of the outer metal layer 323 can be 0.6, 0.7, 0.8, 0.9, 1, 1.1, 1.2, 1.3, or 1.4. The specific value of the inner metal layer 323 can be 0.35-0.8 mm. The ratio of the outer metal layer to the inner metal layer shown in Figure 4-1 is 464.5 μm / 428.1 μm = 1.08; the ratio of the outer metal layer to the inner metal layer shown in Figure 4-2 is 463.6 μm / 463.6 μm = 1.

[0050] In Examples 1 and 2 of the present application, as well as in some other specific embodiments, the pot bottom wall is the substantially flat portion of the pot bottom; the pot sidewall is the portion of the pot wall connected to the flat portion of the pot bottom and extending toward the pot opening; these include, but are not limited to, curved sidewalls transitioning upward into an arc; if the pot is a straight pot (referred to as a straight pot), they also include vertical sidewalls extending toward the pot opening; if the pot is a spherical pot (referred to as a spherical pot), they also include spherical pot wall portions extending toward the pot opening and protruding outward from the pot. The pot shown in FIG2 is a spherical pot.

[0051] In the first embodiment of the present application, different production processes are used depending on the shape of the inner pot. For a straight inner pot, the production process is as follows:

[0052] S01: Etching, engraving or pressing one side of the inner metal layer to form an anti-sticking array;

[0053] S03: controlling the stretching rate to stretch the metal sheet provided with the anti-sticking array to form a pot inner shell;

[0054] For the bladder, the production process is as follows:

[0055] S02: etching, engraving or pressing one side of the inner metal layer to form an anti-sticking array;

[0056] S04: Control stretching to form a pot core embryo;

[0057] S06: Control the expansion rate to expand the pot core blank to form the pot core.

[0058] The pot core blank can be punched once by a punching machine, and then expanded twice by a water expansion machine.

[0059] In Example 1 of the present application, in order to make the grooves or protrusions in the anti-sticking array 33 that are subjected to tensile deformation meet the preset range, it can be the area change rate of the area where the grooves or protrusions are located, it can be the size change rate of the grooves or protrusions in the circumferential direction, or it can be the size change rate of the grooves or protrusions in the axial direction.

[0060] Specifically, in the first embodiment of the present application, the preset range may be:

[0061] The grooves or protrusions in the anti-sticking array 33 that are deformed by tension are located on the sidewalls, and their deformation ratio b along the axial direction of the pot sidewall is 1.1 to 1.8 times; the deformation ratio is the ratio of the axial dimension of the anti-sticking array 33 on the pot sidewall after stretching to the corresponding dimension (pre-axial dimension) of the anti-sticking array 33 on the pot bottom wall;

[0062] The axial dimension will increase during the stretching process. The axial deformation should not be too large, otherwise the groove width will be too large and the rice non-stick effect will be poor.

[0063] As described above, in this embodiment, the grooves or protrusions in the anti-sticking array 33 that are subjected to tensile deformation are located on the sidewalls, and the deformation ratio c along the circumferential direction of the sidewalls of the inner pot is 0.5 to 1.01 times; the deformation ratio is the ratio of the circumferential dimension of the anti-sticking array 33 on the inner pot sidewall to the corresponding dimension (pre-circumferential dimension) of the anti-sticking array 33 on the inner pot bottom wall after stretching;

[0064] According to the principle of inconvenience in volumetric deformation in front and back, when the thickness direction deforms by ±10%, the deformation in the axial direction should not exceed 1.8 to avoid a circumferential shrinkage rate of no more than 50%. If the circumferential shrinkage rate is too large and the axial elongation is too large, the grooves on the side walls will become elongated, forming slits. This will make it easier for starch particles or other food residues to get stuck in the grooves, making it impossible to clean the gallbladder wall, which will harbor dirt and grime, affecting food hygiene, facilitating flavor transfer, and affecting the experience. The axial direction should not be less than 1.1, so that the circumferential elongation is no more than 1%, so that the circumferential and axial dimensions of the grooves are not too large. If rice grains are easily stuffed into the grooves, the rice grains will be heated three-dimensionally in the grooves. At this time, the starch in the rice will be more easily gelatinized, causing stickiness and difficulty in taking off, resulting in poor non-stick effect.

[0065] In the first embodiment of the present application, the value of the deformation ratio b can be specifically 1.1, 1.2, 1.3, 1.4, 1.5, 1.6, 1.7, 1.8; the value of the deformation ratio c can be specifically 0.5, 0.6, 0.7, 0.8, 0.9, 1, 1.01. The anti-sticking array 33 on the bottom wall of the pot can be the anti-sticking array 33 covering the temperature measuring device in the middle of the bottom wall of the pot. Figure 5-1 is an electron microscope image of the anti-sticking array at the bottom wall of the pot, and the diameter of the groove is 455.2μm. Figure 5-2 is an electron microscope image of the anti-sticking array at the side wall of the pot, and the axial dimension of the groove is 585.9μm and the circumferential dimension is 324.6μm. Therefore, the specific value of the deformation ratio b is 585.9 / 455.2=1.287, and the specific value of the deformation ratio c is 324.6 / 455.2=0.713.

[0066] In another specific embodiment of the present application, in order to control the deformation of the grooves and protrusions to meet the preset range, a method for manufacturing a zero-coating rice pot is also proposed. The manufacturing method is mainly achieved through the principle of pre-deformation, as follows:

[0067] Embodiment 2: It includes providing a metal plate that is at least composited with an inner metal layer 323 and a uniform heat layer 322; etching, engraving or pressing one side of the inner metal layer 323 to form an anti-sticking array 33, wherein the anti-sticking array 33 includes a plurality of grooves and protrusions; stretching the metal plate provided with the anti-sticking array 33 to form a pot inner shell; or first stretching it into a pot inner shell blank, and then expanding the pot inner shell blank to form a pot inner shell; when etching, engraving or pressing the anti-sticking array, the grooves and protrusions on the metal plate portion used to form the side wall of the pot inner shell are compared with the metal plate portion used to form the bottom wall of the pot inner shell, the pre-axial size of the grooves of the former is smaller than the pre-axial size of the grooves of the latter, and the pre-circumferential size of the former is larger than the pre-circumferential size of the grooves of the latter, so that the grooves and protrusions in the anti-sticking array 33 that are subjected to tensile deformation meet the preset range.

[0068] The second embodiment of the present application is similar to the first embodiment. Different manufacturing processes are used depending on the shape of the inner pot. For a straight inner pot, the manufacturing process is as follows:

[0069] S01: Etching, engraving or pressing one side of the inner metal layer to form an anti-sticking array;

[0070] S03: forming a pot inner shell by stretching a metal plate provided with an anti-sticking array;

[0071] For the bladder, the production process is as follows:

[0072] S02: etching, engraving or pressing one side of the inner metal layer to form an anti-sticking array;

[0073] S04: First stretch it into a pot embryo;

[0074] S06: The pot core blank is then expanded to form the pot core.

[0075] The pot core blank can be punched once by a punching machine, and then expanded twice by a water expansion machine.

[0076] During the plastic deformation of the metal, the grooves and protrusions on the side wall of the pot will be deformed. After deformation, the anti-sticking array 33 will change the optimal contact state between the rice and the anti-sticking array 33, resulting in poor non-stick effect of the rice on the side wall of the pot.

[0077] First, the thickness of the side wall of the pot can be controlled to remain within a controllable range before and after deformation, thereby obtaining the area deformation ratio of the regions in the other two directions of the anti-sticking array 33. Based on possible deformation parameters, before stretching, the shape and size of the grooves and protrusions of the anti-sticking array 33 are pre-deformed in the reverse direction so that the deformation of the grooves on the side wall of the manufactured pot can be controlled within a preset range.

[0078] Specifically, when etching, engraving, or pressing the anti-sticking array, the grooves and protrusions on the metal sheet portion used to form the side wall of the pot are compared with the metal sheet portion used to form the bottom wall of the pot, and the pre-axial dimension of the grooves of the former is smaller than the pre-axial dimension of the grooves of the latter, and the pre-circumferential dimension of the former is larger than the pre-circumferential dimension of the grooves of the latter;

[0079] The pre-axial dimension refers to the axial dimension of the pot's sidewall surface after the pot is formed. The pre-circumferential dimension refers to the circumferential dimension of the pot's sidewall surface after the pot is formed. For example, before stretching, based on the center point of the sheet material, the radial dimension of each groove passing through the center point is generally the pre-axial dimension, and the dimension perpendicular to this radial direction is the pre-circumferential dimension.

[0080] As shown in FIG6 , when performing step S01 or S02 on the metal sheet before stretching, assuming that area S2 is the part that will form the bottom wall of the pot after subsequent stretching, and S1 is the part that will form the side wall of the pot after subsequent stretching, the groove shape of area S1 is pre-deformed. As shown in FIG7-1 and FIG7-2 , taking a circular groove as an example, a circular groove is made in area S2 that will form the bottom wall of the pot, and its dimensions W2 and L2 are both diameters, while an elliptical groove is made in area S1 that will form the side wall of the pot. At this time, the major axis of the ellipse is approximately in the pre-circumferential direction, and the minor axis of the ellipse is approximately in the pre-axial direction.

[0081] When the inner pot is manufactured, the groove is pre-deformed into an ellipse, and its pre-axial dimension L1 will become longer, and the pre-circumferential dimension W1 will become shorter, so that the axial dimension and circumferential dimension of the groove at the side wall of the inner pot are not significantly different from the groove dimension (W2, L2) of the bottom wall of the inner pot, so that the deformation of the side wall groove is controlled within the preset range, ensuring the non-stick effect.

[0082] In the second embodiment of the present application, the preset range is the ratio of the axial groove size at the side wall of the pot to the groove size at the bottom wall of the pot after stretching, and the ratio range is 0.9-1.25.

[0083] The axial dimension will increase during the stretching process, and the axial deformation should not be too large, otherwise it will easily lead to a groove width that is too large and a poor non-stick effect for rice. After pre-deformation treatment, the groove on the side wall of the pot can be made to have a shape similar to that of the groove at the bottom of the pot, thereby ensuring that the non-stick effect of rice in the pot is good.

[0084] The preset range is the ratio of the size of the groove in the circumferential direction at the side wall of the pot to the size of the groove at the bottom wall of the pot after stretching, and the ratio range is 0.8-1.01.

[0085] The circumferential dimension is likely to shrink during the deformation process. Similarly, after pre-deformation treatment, the circumferential dimension can also make the grooves on the side wall of the pot and the grooves on the bottom wall of the pot not much different, thereby ensuring a good non-stick effect for rice.

[0086] In embodiment 2 of the present application, the ratio of the groove size in the axial direction to the groove size at the bottom wall of the pot can be specifically 0.9, 0.95, 1, 1.05, 1.1, 1.15, 1.2, or 1.25; the ratio of the groove size in the circumferential direction to the groove size at the bottom wall of the pot can be specifically 0.8, 0.85, 0.9, 0.95, 1, 1.05, 1.1, 1.15, 1.2, or 1.25.

[0087] Similarly, the thickness of the side wall of the pot is kept within a controllable range before and after deformation, which facilitates pre-deformation of the pre-axial and pre-circumferential dimensions of the anti-sticking array 33 before stretching;

[0088] To this end, before stretching, the grooves and protrusions on the metal sheet part used to form the side wall of the pot are equal in depth to the groove depth of the metal sheet part used to form the bottom wall of the pot.

[0089] By making the groove depth before stretching equal to the groove depth after stretching, the thickness is not pre-deformed, thereby facilitating pre-deformation of the axial and circumferential dimensions and reducing the difficulty of pre-deformation;

[0090] The preset range is the ratio of the groove depth at the side wall of the pot to the groove depth at the bottom wall of the pot after stretching, and the ratio range is 0.9-1.1.

[0091] In the stamping process, the deformation size in the groove depth direction can be controlled by the size and shape of the cavity between the front and rear dies of the mold, or by the bulging pressure, which is convenient, simple and efficient to control.

[0092] In Example 2 of the present application, the ratio of the groove depth of the side wall to the groove depth at the bottom wall of the pot can be specifically 0.9, 0.95, 1, 1.05, or 1.1; as shown in Figures 4-1 and 4-2, the groove depth of the bottom wall of the pot is 428.1-327.9=100.2μm, and the groove depth of the side wall of the pot is 463.6-354.5=109.1μm; the specific ratio of the two is 1.08.

[0093] The following are further technical solutions of Examples 1 and 2 of this application and some other specific implementation methods:

[0094] The equivalent diameter D of the groove or protrusion on the bottom wall of the pot and the thickness H1 of the inner metal layer 323 satisfy the following relationship: 0.08≤D / H1≤3.

[0095] The ratio of equivalent diameter D to thickness H1 represents the number of grooves per unit thickness. If there are too many grooves per unit thickness, the overhead ratio per unit thickness will be too high. Given a certain amount of heat per unit thickness, excessive overhead means lower heat transfer efficiency. If there are too few grooves per unit thickness, the overhead ratio per unit thickness is too low, causing the rice to lie close to the pot wall, receiving more heat and making it more likely to stick to the pot. Therefore, in the specific embodiments of this application, the number of grooves per unit thickness is no less than 0.08 and no more than 3, thus balancing low heat transfer efficiency and sticking.

[0096] In Examples 1 and 2 of the present application and some other specific embodiments, the specific value of D / H1 can also be 0.08, 0.53, 0.98, 1.43, 1.88, 2.33, 2.78, or 3. Referring to Figures 4-1 and 5-1 , the equivalent diameter D is 455.2 μm, H1 is 428.1 μm, and the ratio is 1.06;

[0097] In addition to the deformation of the anti-sticking array 33 between the side wall and the bottom wall of the pot being within a preset ratio range, the preset range also includes:

[0098] In some specific embodiments of the present application, the grooves or protrusions in the anti-sticking array 33 that are deformed by tension are located on the sidewalls, and the maximum diameter of the grooves on the sidewalls of the pot after deformation is no greater than 1620 μm. As shown in FIG5-2 , the maximum diameter of the grooves after deformation is 585.9 μm.

[0099] Generally, the width of rice grains is about 2mm, and the water absorption expansion rate is about 1.5-2 times. Therefore, the width of the rice after absorbing water should not be less than about 3mm. In order to achieve the non-stick effect of rice and prevent rice sticking, the maximum diameter after deformation should not be greater than 1620 microns. When the groove is stretched, the groove will be larger than the original size, which may exceed the size of the rice grain. If so, the rice grain will be more easily stuck in the deformed groove. As mentioned above, the pot core is generally elongated in the axial direction and shortened in the circumferential direction, so the groove after deformation is prone to form a slit. On this basis, if the deformation size exceeds the upper limit, rice sticking is likely to occur. The rice grains stuck in the groove are heated in three dimensions, and the starch in the rice is easily burnt, causing the problem of sticking to the pot.

[0100] The grooves or protrusions in the anti-sticking array 33 that are deformed by tension are located on the sidewalls, and the minimum diameter of the deformed sidewalls of the pot is no less than 50 μm. As shown in FIG5-2 , the minimum diameter of the grooves after deformation is 324.6 μm.

[0101] In order to achieve the non-stick effect, there must be a minimum actual value after lateral reduction, for example, greater than 100 microns. If it is not greater than this actual value, the groove is too narrow and cannot achieve the anti-stick effect. The narrow gap formed is not easy to clean, and dirt and grime are hidden inside, affecting food hygiene. The inner surface of the pot is prone to blackening, the odor is heavy, and it is easy to transfer flavors.

[0102] The equivalent diameter D of the grooves or protrusions on the bottom wall of the pot is not more than 900 microns at most and not less than 100 microns at least. This ensures that during the cooking process of the cooking utensil, the deformation of the grooves or protrusions of the anti-stick array 33 on the side wall of the pot is neither too large nor too small, and is within a reasonable range, thereby ensuring the non-stick effect of the pot.

[0103] In the embodiment of the present application, the thickness of the metal sheet is 1 to 5 mm, and the thickness variation of the sheet is controlled to be approximately ±10%. For example, a 3 mm metal sheet has a thickest point of 3.32 mm after stretching.

[0104] As the thickness of the metal sheet increases, its mass also increases. Accordingly, the thickness of the outer metal layer 321 can also be increased, thereby improving the pot's protective ability. In some specific embodiments of the present application, the ratio of the outer metal layer 321 to the thickness of the metal sheet is 0.2 to 0.4. This ratio can be 0.2, 0.25, 0.3, 0.35, or 0.4. For example, the ratio of the pot bottom wall in Figure 4-1 is 464.5 / 1243 = 0.37; and the ratio of the pot side wall in Figure 4-2 is 463.6 / 1295 = 0.36.

[0105] As the thickness of the metal sheet increases, the inner metal layer 323 can also increase, but it can be thinner than the outer metal layer 321. The ratio of the inner metal layer 323 to the thickness of the metal sheet is 0.1 to 0.4. Specifically, this ratio can be 0.1, 0.15, 0.2, 0.25, 0.3, 0.35, or 0.4. For example, the ratio of the pot bottom wall in Figure 4-1 is 428.1 / 1243 = 0.34; for the pot side wall in Figure 4-2, the ratio is 463.6 / 1295 = 0.36.

[0106] Generally, as metal sheets become thicker, their capacity increases, placing higher demands on heat conduction. In this case, the uniform heat layer 322 will be thicker than usual. The ratio of the uniform heat layer 322 to the thickness of the metal sheet can be between 0.2 and 0.7. This ratio can be 0.2, 0.25, 0.3, 0.35, 0.4, 0.45, 0.5, 0.55, 0.6, or 0.65. For the pot bottom wall in Figure 4-1, the ratio is 355.2 / 1243 = 0.28; for the pot side wall in Figure 4-2, the ratio is 372.7 / 1295 = 0.28.

[0107] For a 1.5 mm thick metal sheet, the thicknesses of the inner metal layer 323 , the uniform heat layer 322 , and the outer metal layer 321 are 0.5 mm, 0.5 mm, and 0.5 mm, respectively. For a 3 mm thick metal sheet, the thicknesses of the inner metal layer 323 , the uniform heat layer, and the outer metal layer 321 are 0.8 mm, 1.6 mm, and 0.6 mm, respectively.

[0108] In some specific embodiments of the present application, the grooves in the anti-sticking array 33 are independent single pits that are not interconnected, and the anti-sticking array 33 in the middle of the bottom wall of the pot covers the temperature measuring device. The grooves are independent single pits that are not interconnected, so that the grooves have a certain water-locking ability, thereby being able to maintain a water film, and thus having non-stick ability. The anti-sticking array 33 in the middle of the bottom wall of the pot covers the temperature measuring device, and the place where the temperature measuring device is located is basically horizontal to ensure the accuracy of temperature measurement. Therefore, the pot wall here must be the bottom wall of the pot, and the deformation of the anti-sticking array 33 on this is relatively small, and its size can be used as a source of pre-axial size and pre-circumferential size before deformation. It can also be used as a source of the size of the grooves of the manufactured pot before deformation. For example, the size of the side wall of the pot is obtained, and the size of the groove covering the temperature measuring device is obtained. By comparing the two, the desired data can be obtained.

[0109] In some embodiments of the present application, the grooves have basic shapes, such as circular, hexagonal, square, rectangular, etc., and the arrangement of the grooves in the inner pot has a basic array, such as a rectangular array, an annular array, etc. The array of the grooves and protrusions in the anti-sticking array 33 is a rectangular array or an annular array. With respect to the embodiments provided above, it should be understood by those skilled in the art that the basic shape of the grooves can also be other shapes, and the array arrangement can also be other arrangements. Different shapes and array arrangements can be freely combined, for example, a circular rice slurry groove can also be arranged in a rectangular array.

[0110] Anything not described in this application can be achieved by adopting or drawing on existing technologies.

[0111] The various embodiments in this specification are described in a progressive manner, and the same or similar parts between the various embodiments can be referred to each other. Each embodiment focuses on the differences from other embodiments.

[0112] The foregoing is merely an embodiment of the present application and is not intended to limit the present application. For those skilled in the art, the present application may have various changes and variations. Any modifications, equivalent replacements, improvements, etc. made within the spirit and principles of the present application should all be included within the scope of the claims of the present application.

Claims

1. A method for making a non-stick pan, characterized in that: The invention comprises providing a metal sheet material which is at least composited with an outer metal layer, a uniform heat layer and an inner metal layer, etching, engraving or pressing one side of the inner metal layer to form an anti-sticking array, wherein the anti-sticking array comprises a plurality of grooves or protrusions; controlling the stretching rate to stretch the metal sheet material provided with the anti-sticking array to form a pot core; or controlling the stretching to first stretch it into a pot core embryo, and then controlling the bulging rate to bulge the pot core embryo to form the pot core; the thickness ratio of the side wall of the pot core to the bottom wall of the pot core is 0.9 to 1.1, and the thickness ratio of the outer metal layer to the inner metal layer is 0.6 to 1.4, so that the grooves or protrusions in the anti-sticking array which are subjected to stretching deformation meet a preset range, and the preset range comprises: the grooves or protrusions in the anti-sticking array which are subjected to stretching deformation are located on the side wall, and the deformation ratio along the axial direction of the side wall of the pot core is 1.1 to 1.8 times.

2. The method for making a non-stick pot as claimed in claim 1, characterized in that: The grooves or protrusions in the anti-sticking array that are subjected to tensile deformation are located on the side wall, and the deformation ratio along the circumferential direction of the side wall of the pot is 0.5 times to 1.01 times.

3. The method for making a non-stick pot as claimed in claim 1, characterized in that: The equivalent diameter D of the groove or protrusion on the bottom wall of the pot, the thickness H1 of the inner metal layer, and the equivalent diameter D satisfy the following relationship: 0.08≤D / H1≤3.

4. The method for making a non-stick pot as claimed in claim 1, characterized in that: The grooves or protrusions in the anti-sticking array that are deformed by tension are located on the side wall, and the maximum diameter of the grooves on the side wall of the pot after deformation is no more than 1620 microns.

5. The method for making a non-stick pot as claimed in claim 1, characterized in that: The grooves or protrusions in the anti-sticking array that are subjected to tensile deformation are located on the side wall, and the minimum diameter of the side wall of the pot after deformation is not less than 50 microns.

6. The method for making a non-stick pot as claimed in claim 1, characterized in that: The ratio of the outer metal layer to the thickness of the metal sheet is 0.2 to 0.

4.

7. The method for making a non-stick pot as claimed in claim 1, characterized in that: The ratio of the inner metal layer to the thickness of the metal sheet is 0.1 to 0.

4.

8. The method for making a non-stick pot as claimed in claim 1, characterized in that: The ratio of the uniform heat layer to the thickness of the metal plate is 0.2 to 0.