New tobacco improving sensory evaluation quality, and preparation method for heating section and thick-paste-method sheet thereof
Patent Information
- Application Number
- MYPI2025004721
- Authority / Receiving Office
- MY · MY
- Patent Type
- Applications
- Current Assignee / Owner
- Priority Date
- 2023-10-19
- Filing Date
- 2024-09-30
- Publication Date
- 2025-04-19
AI Technical Summary
The existing new tobacco (heated cigarette) is made of thick slurry thin sheets, which have insufficient tobacco fragrance, plain aroma, poor aroma and temperament, heavy adhesive flavor, and unsatisfactory breathing taste.
By adding the thick slurry containing ammonium dihydrogen phosphate, additive B with a specific compound structure and additive C, and stirring reactions at low pressure and specific temperatures, the pH value of the thick slurry is adjusted to the thick slurry is 3 to 6, and after modifying the thick slurry, the slurry is clothed and dried, to prepare a new tobacco flake using thick slurry method.
It significantly improved the suction taste of the new tobacco thick slurry flakes, the tobacco fragrance is full, the miscellaneous air is reduced, the adhesive is lightened, and the aroma and temperament are coordinated.
Smart Images

Figure PI2025004721_DRAWING_001
Abstract
Description
Novel tobacco with improved sensory smoking quality and preparation method of its heating section and thick pulp method sheet
[0001] This application claims priority to a Chinese patent application filed with the Patent Office of China on October 19, 2023, with application number 202311357207.X and invention name “New tobacco with improved sensory smoking quality and its heating section, and method for preparing thick pulp slices”, the entire contents of which are incorporated by reference into this application. Technical Field
[0002] The present invention relates to the field of new materials in novel tobacco, and in particular to the field of thick pulp method sheet design and production technology for novel tobacco. Background Art
[0003] Tobacco flakes were first introduced in the 1960s as a recombinant process to recycle waste from tobacco processing. However, with growing concern about the health benefits of cigarettes, tobacco flakes have taken on a new role. Because their chemical composition and combustion properties are easier to adjust than those of traditional tobacco leaves, they have been given the ability to reduce tar and reduce harm, becoming a functional carrier or a primary material for improving cigarette combustion and regulating the chemical composition of smoke. Today, with the rise of heated cigarettes (new tobacco), tobacco flakes are being used as a primary new smoking material in the new tobacco industry, and their functionality has been further utilized. The main methods for manufacturing tobacco flakes include the slurry method, roller pressing method, papermaking method, and improved papermaking method (dry method). Currently, 80% of new tobacco flakes in the new tobacco industry use the slurry method or roller pressing method. Both methods require mixing tobacco ash with a binder to create a slurry before producing the flakes. However, flakes produced using traditional slurry or roller pressing methods suffer from quality issues such as insufficient tobacco aroma, bland aroma, poor aroma quality, and a strong binder odor. Especially when used to manufacture new tobacco products (such as heated cigarettes), the above-mentioned quality problems will be more prominent.
[0004] To improve the taste of tobacco sheets, several methods of adding flavors and fragrances have been reported in the prior art. For example, Chinese patent publication CN113508918A describes a method for preparing long-lasting, multi-flavor heat-not-burn tobacco sheets. The method involves adding a mixture of a macromolecular flavor precursor, a thermally conductive adhesive, a thermally conductive colorant, and tobacco powder to a slurry of wood pulp fibers, an atomizer, and water. The method then controls the slurry stirring rate, increases the stirring rate and temperature of the thick slurry, and selects a suitable coating plate and covering film. Freeze-drying is then used to produce a uniform, smooth, and easily peelable tobacco sheet. While this method achieves good technical results, it still suffers from issues such as insufficient aroma, a bland aroma, poor aroma quality, a strong adhesive odor, and an unsatisfactory puffing experience.
[0005] Summary of the Invention
[0006] In response to the problems of insufficient tobacco aroma, bland aroma, poor aroma quality, heavy adhesive odor, and unsatisfactory smoking taste in existing new tobacco (heated cigarettes) made by thick pulp method sheets, the first purpose of the present invention is to provide a method for improving the sensory evaluation quality of new tobacco (heated cigarettes) made by thick pulp method sheets, aiming to improve the smoking taste of the prepared new tobacco (heated cigarettes) made by thick pulp method sheets.
[0007] The second object of the present invention is to provide thick pulp sheet for novel tobacco (heated cigarette) prepared by the preparation method and its application in novel tobacco (heated cigarette).
[0008] The third object of the present invention is to provide a new type of tobacco (heated cigarette) comprising the thick pulp sheet.
[0009] The present invention provides a composition comprising: a binder, a thick slurry of soot, and an additive;
[0010] The additives include additive A, additive B and additive C;
[0011] The additive A is at least one of ammonium dihydrogen phosphate, ammonium phosphate, and diammonium hydrogen phosphate;
[0012] The additive B is a compound having formula 1;
[0013] Said R is H, C1-C6 alkyl, C1-C6 alkyl with substituent or heterocycle;
[0014] The substituent is at least one of a hydroxyl group, a thiol group, an aryl group, a carboxyl group, an amide group, a heterocyclic group, and an amino group;
[0015] The additive C is monosaccharide.
[0016] In the composition of the present invention, the adhesive is at least one of plant gum, starch derivatives, CMC, and sodium alginate;
[0017] Preferably, the plant gum is at least one of xanthan gum, tamarind gum, carrageenan, guar gum, and konjac gum;
[0018] Preferably, the starch derivative is at least one of modified starch, oxidized starch, and etherified starch;
[0019] Preferably, an atomizer is further allowed to be added to the thick slurry, and the atomizer includes at least one of ethylene glycol and glycerol;
[0020] Preferably, the ash contains tobacco raw materials; preferably, the ash is also allowed to contain at least one of tobacco leaf raw materials, stems, papermaking thin sheets, tea leaves, plant roots, stems, leaves, flowers or fruits.
[0021] Preferably, additional plant fibers are allowed to be added to the thick slurry.
[0022] In one aspect, the present invention provides an application of a composition in improving the sensory smoking quality of new tobacco thick pulp method sheets.
[0023] A method for improving the sensory smoking quality of novel tobacco thick pulp sheet comprises obtaining a thick pulp comprising a binder and tobacco ash, adding an additive to the thick pulp and adjusting the pH of the system to 3 to 6, then stirring and reacting the mixture at a temperature of 50 to 95° C. and low pressure (negative pressure) to obtain a modified thick pulp; and subjecting the modified thick pulp to a pulping and drying process to obtain novel tobacco thick pulp sheet.
[0024] The additives include additive A, additive B and additive C;
[0025] The additive A is at least one of ammonium dihydrogen phosphate, ammonium phosphate, and diammonium hydrogen phosphate;
[0026] The additive B is a compound having formula 1;
[0027] Said R is H, C1-C6 alkyl, C1-C6 alkyl with substituent or heterocycle;
[0028] The substituent is at least one of a hydroxyl group, a thiol group, an aryl group, a carboxyl group, an amide group, a heterocyclic group, and an amino group;
[0029] The additive C is monosaccharide.
[0030] The present invention innovatively adds additives including additive A, additive B and additive C to the thick slurry, and cooperates with the low-pressure stirring and the combined control of the temperature to facilitate the chemical synergy of the additives, thereby helping to improve flavor substances, reduce impurities, and improve the smoking taste.
[0031] In the present invention, the components and contents in the thick slurry can be conventional, and can also be obtained based on known means.
[0032] For example, the adhesive is at least one of plant gum, starch derivative, CMC, and sodium alginate. The plant gum is at least one of xanthan gum, tamarind gum, carrageenan, guar gum, and konjac gum. The starch derivative is at least one of modified starch, oxidized starch, and etherified starch.
[0033] In the present invention, the ash contains tobacco raw materials. The ash may also contain at least one of tobacco leaf raw materials (such as tobacco shreds), stems, papermaking thin sheets, tea leaves, plant roots, stems, leaves, flowers or fruits;
[0034] For example, an atomizer may be added to the thick slurry, and the atomizer may include at least one of ethylene glycol and glycerol;
[0035] For example, additional plant fibers are added to the thick slurry.
[0036] The thick slurry may also contain other ingredients permitted in the industry. In addition, the contents of the ingredients in the thick slurry may also be reasonably controlled based on known principles.
[0037] In the present invention, the composition of the additives and the combined control of the low-pressure stirring process and temperature are the key to synergistically improving the mouthfeel of the thick slurry method.
[0038] In the present invention, the additive A is ammonium dihydrogen phosphate. The present invention's research shows that the use of ammonium dihydrogen phosphate as additive A, which can be further combined with additives B and C and an alcoholization process, can further improve the smoking taste of the prepared thin slices.
[0039] In the present invention, in Formula 1, the heterocycle is, for example, a saturated or aromatic ring, wherein the heteroatom is, for example, O or N, preferably N. Furthermore, the heterocycle is a tetrahydropyrrole ring, an indole ring, pyrrole, imidazole, or the like.
[0040] In the present invention, the additive B is a compound with a heterocyclic ring in which R is present, and includes at least one of Formula 1-A to Formula 1-D;
[0041] The present invention has shown that the additive B of formula 1-A to formula 1-D can be further combined with additive A and additive C and an alcoholization process to further improve the smoking taste of the obtained thin slices.
[0042] Preferably, the additive B is a mixture of formula 1-A and formula 1-C in a weight ratio of 1:0.5 to 2. Studies have shown that the use of the preferred additive B can further unexpectedly improve the release effect of the target aroma substance and further improve the smoking effect.
[0043] In the present invention, the monosaccharide is at least one of arabinose, ribose, xylose, lyxose, glucose, mannose, fructose, and galactose, preferably a mixture of ribose and glucose. The preferred monosaccharide can further synergize with the ingredients and the process of the present invention to further improve the content of the target aroma and further enhance the taste of the smoke.
[0044] In the present invention, among the additives, the weight ratio of additive A, additive B and additive C is 1:0.5-10:0.5-10, and can further be 1:1-2:1-10.
[0045] In the present invention, the weight ratio of the additive to the thick slurry is less than or equal to 0.3:1, preferably 0.1 to 0.2:1.
[0046] In the present invention, after the additives are added, the pH of the system is regulated by a pH regulator.
[0047] The pH regulator may be a conventional acid or base. For example, the acid may be phosphoric acid, and the base may be sodium hydroxide, potassium hydroxide, or the like.
[0048] In the present invention, the pH of the thick slurry is controlled to be 3-5 by the pH regulator.
[0049] In the present invention, the thick slurry to which the additives are added and the pH is adjusted is reacted under low pressure, which is beneficial to improving the synergy of the ingredients and further improving the smoking taste of the prepared slices.
[0050] Preferably, the low pressure is less than 0.1 MPa, preferably 0.001 to 0.05 MPa;
[0051] In the present invention, the low-pressure stirring process includes a first holding stage at a temperature of T1 and a second holding stage at a temperature of T2, wherein T1 is 55-65°C and T2 is 75-85°C. Studies have shown that the combination of the synergistic additives and the two-stage gradient low-pressure stirring process can further enhance the chemical synergy of the ingredients and improve the puffing texture of the flakes.
[0052] In the present invention, the low-pressure stirring time is 4 to 30 hours, preferably 4 to 24 hours; when the preferred two-stage low-pressure stirring process is adopted, the time of the first stage low-pressure stirring process is preferably 2 to 15 hours, preferably 2 to 4 hours; the time of the second stage low-pressure stirring process is preferably 2 to 15 hours, preferably 2 to 4 hours.
[0053] The present invention also provides thick pulp method sheets for novel tobacco (heated cigarettes) prepared by the preparation method.
[0054] The present invention also provides a heating section of a novel tobacco (heated cigarette), which is added with a thick pulp method sheet for the novel tobacco (heated cigarette) prepared by the preparation method of the invention.
[0055] The present invention also provides a novel heated cigarette having the heating section described in the present invention. Beneficial effects:
[0056] The present invention innovatively adds additives including additive A, additive B and additive C to the thick slurry, and the combined control of low pressure and temperature thereof helps to facilitate the chemical synergy of the additives, helps to improve flavor substances, reduce impurities, and improve the smoking taste.
[0057] The present invention also shows that the innovative use of the component of formula 1 in which R is a heterocyclic ring as additive B, further combined with ammonium dihydrogen phosphate as an additive and the combination of two low-pressure gradients, can unexpectedly further achieve synergy, help to further improve the content of the target aroma component, reduce impurities, and significantly improve the sensory evaluation effect of the suction. BRIEF DESCRIPTION OF THE DRAWINGS
[0058] FIG1 shows a comparison of the aroma components of the sheets prepared in Example 1 and Comparative Example 1; the upper spectrum is the spectrum of Example 1, and the lower spectrum is the spectrum of Comparative Example 1. DETAILED DESCRIPTION
[0059] The present invention discloses a novel tobacco product with improved sensory smoking quality, as well as a method for preparing a heating section and thick pulp sheet. Those skilled in the art can refer to the contents of this document and appropriately improve the process parameters to achieve this. It should be noted that all similar substitutions and modifications are obvious to those skilled in the art and are considered to be included in the present invention. The methods and applications of the present invention have been described through preferred embodiments, and relevant personnel can obviously modify or appropriately change and combine the methods and applications described herein without departing from the content, spirit, and scope of the present invention to implement and apply the technology of the present invention.
[0060] In the present invention, the initial thick slurry can be obtained based on means known in the industry, for example, it can be obtained by conventional binder components and soot slurry.
[0061] For example, as a typical example, 15 kg of sucrose fiber and 450 kg of water are weighed and placed in a high-speed hydraulic fibrillator for fibrillation for 70 minutes at a stirring speed of 5000 rpm. Then, 3 kg of guar gum, 0.5 kg of xanthan gum, 32 kg of a 10% PEG solution, and 5 kg of glycerol are added to the liquid in the hydraulic fibrillator in that order and stirred at 5000 rpm for 30 minutes before use. Simultaneously, 60 kg of tobacco leaves, 30 kg of tobacco stems, and 10 kg of tea leaves are dry-ground into 300-mesh ash for use.
[0062] In the present invention, the thick slurry modified by the additive and method of the present invention can be formed into thin sheets based on known slurry spreading, drying, and peeling. For example, the drying temperature can be 98°C ± 3.
[0063] The present invention will be further described below in conjunction with the embodiments:
[0064] Example 1
[0065] Step (1):
[0066] 500 kg of the prepared adhesive and 100 kg of the prepared fly ash are mixed according to the batch formula to form a uniformly mixed thick slurry (initial thick slurry). Additive A, which is ammonium dihydrogen phosphate, additive B, which is formula 1-A, and additive C, which is a mixture of ribose and glucose in a weight ratio of 1:1, are sequentially added to the initial thick slurry; the weight ratio of additive A:additive B and additive C is 1:2:1; the weight ratio of additives (referring to the total weight of additives A to C) to the thick slurry is 0.2:1; and the pH value of the thick slurry is then adjusted to 3.5 with phosphoric acid (a pH adjuster) to obtain a mixed thick slurry.
[0067] Step (2):
[0068] The mixed slurry of step (1) was stirred continuously at a speed of 400 rpm for 6 h under low pressure and (85±5)°C under 0.02 MPa conditions to obtain a modified slurry for standby use.
[0069] Step (3):
[0070] The slurry is then applied, dried, and peeled to form thin sheets with a thickness of 0.17 mm and a moisture content of 11.8%.
[0071] The sheets were rolled into a new tobacco product (heated cigarettes), which was then smoked by seven specially trained sensory evaluation experts using the methods outlined in the "Sensory Evaluation Method for Reconstituted Tobacco (Papermaking Process)" (YC / T498-2014). The average quantitative scores are shown in Table 1.
[0072] Comparative Example 1
[0073] Compared with Example 1, the only difference is that the initial thick slurry of step (1) is directly processed in step (3) to obtain a control sheet. The sheet thickness is 0.18 mm and the moisture content of the sheet is 11.5%.
[0074] GC / MS was used to analyze the aroma components of the flue gases from the two different treatments. The gas chromatography parameters were: HP-5MS capillary column (60.0 m × 250 μm × 0.25 μm); inlet temperature 250°C; carrier gas high-purity helium at a flow rate of 1.0 mL / min and a split ratio of 15:1; temperature program: initial temperature 40°C, hold for 2 minutes, then increase to 280°C at 8°C / min and hold for 25 minutes; and mass spectrometry parameters: electron impact (EI) ionization mode, 70 eV ionization energy, 230°C ion source temperature, 150°C quadrupole temperature, full scan mode, and a scanning range of 35-450 amu. A comparison of the aroma components is shown in Figure 1. This demonstrates that the present method can selectively increase the content of target aroma compounds.
[0075] The thin sheets were rolled into a new type of tobacco (heated cigarettes), which were smoked by seven specially trained sensory evaluation experts and evaluated for sensory quality according to the relevant methods in the "Sensory Evaluation Method for Reconstituted Tobacco (Papermaking Method)" (YC / T498-2014).
[0076] The results show that the final slices prepared in Example 1 have significantly improved aroma quality compared to the control slices prepared in Comparative Example 1, with fuller tobacco aroma, less miscellaneous odors, better coordination, and less adhesive odor. The quantitative score averages are shown in Table 1.
[0077] Table 1 Original record of sensory quality evaluation of reconstituted tobacco (papermaking method)
[0078] Table 2 Changes in the main aroma components of smoke samples treated with two different methods
[0079] Figure 1 and Table 2 show that the smoke from the novel tobacco (heated cigarette) rolled with the sheet from Example 1 showed increases in 2-methylpyrazine by 15%, furfural by 38%, furfuryl alcohol by 52.7%, 5-guaiacol by 57.5%, and 2-acetylpyrrole by 80.8%. In addition, other typical target flavor components also increased to varying degrees.
[0080] Example 2
[0081] Compared with Example 1, the only difference is that 5 kg of the above-mentioned binder and 1 kg of soot are mixed to form an initial thick slurry, and on this basis, the components and proportions of additives A, additives B and additives C in the preparation process are changed. The experimental groups are:
[0082] Experimental group A: Additive A is diammonium hydrogen phosphate, and the total amount of additive A remains unchanged.
[0083] Experimental group B: Additive B is formula 1-C, and the total amount of additive B remains unchanged.
[0084] Experimental group C: Additive B is Formula 1-A and Formula 1-C in a weight ratio of 1:1, and the total amount of additive B remains unchanged.
[0085] Experimental group D: Additive B is the compound of formula 1 wherein R1 is benzyl, and the total amount of additive B remains unchanged.
[0086] Experimental group E: Additive C was glucose, and the total amount of additive C remained unchanged.
[0087] Experimental group F: Among the additives, the weight ratio of additive A, additive B and additive C was 1:10:10, and the weight ratio of the additives in the form of thick paste was 0.1:1.
[0088] Example 3
[0089] Compared with Example 2C, the only difference is that in step (2), a low-pressure two-stage gradient treatment is adopted. The difference is that the mixed thick slurry of step (1) is preheated at (60±5)°C for 3 hours under 0.02 MPa conditions, and then at 80±5)°C for 3 hours to obtain a modified thick slurry.
[0090] Comparative Example 2
[0091] Compared with Group B of Example 2, the only difference is that an equal weight of ammonium lactate is used as additive A.
[0092] Comparative Example 3
[0093] Compared with Group B of Example 2, the only difference is that in step 2, the pressure during the reaction is normal pressure.
[0094] According to the national standard method of Example 1, Examples 2 to 3 and Comparative Examples 2 to 3 were subjected to suction. The results are shown in Table 3:
[0095] Table 3 Suction evaluation results of Examples 2-3 and Comparative Examples 2-3:
[0096] As shown in Table 2, the use of ammonium dihydrogen phosphate as Additive A, and the use of Formula 1 (Groups B-D) where R is an aromatic heterocycle, particularly the combination of Formula 1-A and Formula 1-C, can further synergistically improve the release of target aroma compounds and further enhance the inhalation experience. Furthermore, the use of a two-stage low-pressure reaction (Example 3) can further enhance the inhalation experience of the resulting thin film.
[0097] Example 4
[0098] Compared with Example 1, the difference is that the addition ingredients and conditions of the additives are changed, specifically: Step (1):
[0099] Additive A, which is ammonium phosphate, additive B, which is formula 1-B, and additive C, which is mannose, are added to the mixed slurry in sequence; the weight ratio of additive A: additive B and additive C is 1:1:1; the weight ratio of the additives to the thick slurry is 0.2:1; and the pH value of the thick slurry is adjusted to 4.0 with phosphoric acid.
[0100] Step (2):
[0101] The mixed slurry of step (1) was stirred continuously at a speed of 300 rpm for 6 h under low pressure and heat preservation at (60±5)°C under 0.02 MPa conditions and set aside.
[0102] Step (3):
[0103] The slurry is then applied, dried, and peeled to form a sheet with a thickness of 0.16 mm and a moisture content of 11.0%.
[0104] Example 5
[0105] Step (1):
[0106] 500 kg of the prepared adhesive and 100 kg of fly ash were mixed according to the batch formula to form a uniformly mixed thick slurry. Additive A (ammonium dihydrogen phosphate), additive B (formula 1-B), and additive C (lyxose) were added to the mixed slurry in this order; the weight ratio of additives A:additive B and additive C was 1:1:10; the weight ratio of the additives to the thick slurry was 0.15:1; and the pH of the thick slurry was adjusted to 5.0 with phosphoric acid.
[0107] Step (2):
[0108] The mixed slurry of step (1) was stirred continuously at a speed of 300 rpm for 8 h under low pressure and heat preservation at (70±5)°C under 0.02 MPa conditions and set aside.
[0109] Step (3):
[0110] The slurry is then applied, dried, and peeled to form thin sheets with a thickness of 0.17 mm and a moisture content of 11.3%.
[0111] Example 6
[0112] Step (1):
[0113] 500 kg of the prepared adhesive and 100 kg of fly ash were mixed according to the batch recipe to form a uniform thick slurry. Additive A (ammonium dihydrogen phosphate), additive B (formula 1-B), and additive C (arabinose) were added to the mixed slurry in this order; the weight ratio of additives A:additive B:additive C was 1:1:5; the weight ratio of the additives to the thick slurry was 0.10:1. The pH of the thick slurry was adjusted to 4.5 with phosphoric acid.
[0114] Step (2):
[0115] The mixed slurry of step (1) was stirred continuously at a speed of 500 rpm for 8 h under low pressure and heat preservation at (60±5)°C under 0.15 MPa conditions and set aside.
[0116] Step (3):
[0117] The slurry is then applied, dried, and peeled to form thin sheets with a thickness of 0.18 mm and a moisture content of 11.8%.
[0118] Examples 4 to 6 were evaluated by the method of Example 1. The results are shown in Table 4.
[0119] Table 4: Results of smoking tests in Examples 4 to 6
[0120] In summary, the process of the present invention, based on the additives and low-pressure reaction, can unexpectedly improve the release of target aroma substances from the prepared flakes.
[0121] The above describes in detail the novel tobacco provided by the present invention, which has improved sensory smoking quality, as well as its heating section and thick pulp method flake preparation method. This article uses specific examples to illustrate the principles and implementation methods of the present invention. The description of the above examples is only intended to facilitate understanding of the method and core concept of the present invention. It should be noted that those skilled in the art may make various improvements and modifications to the present invention without departing from the principles of the present invention, and such improvements and modifications also fall within the scope of protection of the claims of the present invention.
Claims
1. A composition, characterized in that include: Adhesives, soot slurries and additives; The additives include additive A, additive B and additive C; The additive A is at least one of diammonium phosphate, ammonium phosphate and diammonium hydrogen phosphate; The additive B is a compound having formula 1; The R is H, C1-C6 alkyl, C1-C6 alkyl with substituent or heterocycle; The substituent is at least one of a hydroxyl group, a thiol group, an aryl group, a carboxyl group, an amide group, a heterocyclic group, and an amino group; The additive C is monosaccharide.
2. The composition according to claim 1, characterized in that The adhesive is at least one of plant glue, starch derivatives, CMC and sodium alginate; Preferably, the plant gum is at least one of xanthan gum, tamarind gum, carrageenan, guar gum and konjac gum; Preferably, the starch derivative is at least one of modified starch, oxidized starch and etherified starch; Preferably, an atomizer is allowed to be added to the thick slurry, and the atomizer includes at least one of ethylene glycol and glycerol; Preferably, the ash contains tobacco raw materials; preferably, the ash is also allowed to contain at least one of tobacco leaf raw materials, stems, papermaking thin sheets, tea leaves, plant roots, stems, leaves, flowers or fruits; Preferably, additional plant fibers are allowed to be added to the thick slurry.
3. Use of the composition as claimed in claim 1 or 2 in improving the sensory smoking quality of new tobacco thick pulp sheet.
4. A method for improving the sensory smoking quality of new tobacco thick pulp thin sheets, characterized in that: Obtaining a thick slurry containing a binder and soot, adding an additive to the thick slurry and adjusting the pH value of the system to 3 to 6, and then stirring and reacting at a temperature of 50 to 95° C. and a low pressure to obtain a modified thick slurry; The modified thick pulp is subjected to pulping and drying treatment to obtain a new type of thick pulp sheet for tobacco; The additives include additive A, additive B and additive C; The additive A is at least one of diammonium phosphate, ammonium phosphate and diammonium hydrogen phosphate; The additive B is a compound having formula 1; The R is H, C1-C6 alkyl, C1-C6 alkyl with substituent or heterocycle; The substituent is at least one of a hydroxyl group, a thiol group, an aryl group, a carboxyl group, an amide group, a heterocyclic group, and an amino group; The additive C is monosaccharide.
5. The method according to claim 4, characterized in that The adhesive is at least one of plant glue, starch derivatives, CMC and sodium alginate; Preferably, the plant gum is at least one of xanthan gum, tamarind gum, carrageenan, guar gum and konjac gum; Preferably, the starch derivative is at least one of modified starch, oxidized starch and etherified starch; Preferably, an atomizer is allowed to be added to the thick slurry, and the atomizer includes at least one of ethylene glycol and glycerol; Preferably, the ash contains tobacco raw materials; preferably, the ash is also allowed to contain at least one of tobacco leaf raw materials, stems, papermaking thin sheets, tea leaves, plant roots, stems, leaves, flowers or fruits; Preferably, additional plant fibers are allowed to be added to the thick slurry.
6. The method according to claim 4 or 5, characterized in that The additive A is ammonium dihydrogen phosphate.
7. The method according to any one of claims 4 to 6, characterized in that The additive B is a compound with a heterocyclic ring in R, which includes at least one of Formula 1-A to Formula 1-D; 8. The method according to any one of claims 4 to 7, characterized in that The monosaccharide is at least one of arabinose, ribose, xylose, lyxose, glucose, mannose, fructose and galactose; Preferably, the pH regulator is an acid or a base.
9. The method according to any one of claims 4 to 8, characterized in that Among the additives, the weight ratio of additive A, additive B and additive C is 1:0.5-10:0.5-10.
10. The method according to any one of claims 4 to 9, characterized in that: The weight ratio of the additive to the thick slurry is less than or equal to 0.3:1, preferably 0.1 to 0.2:
1.
11. The method according to any one of claims 4 to 10, characterized in that: The low-pressure stirring process includes a first low-pressure stirring process at a temperature of T1 and a second low-pressure stirring process at a temperature of T2, wherein T1 is 55-65°C and T2 is 75-85°C; Preferably, the low pressure is less than 0.1 MPa, preferably 0.001 to 0.05 MPa; Preferably, the first low-pressure stirring process lasts for 2 to 15 hours, preferably 2 to 4 hours; Preferably, the second low-pressure stirring process lasts for 2 to 15 hours, preferably 2 to 4 hours.
12. A novel thick pulp sheet for tobacco made by the method according to any one of claims 4 to 11.
13. A new type of heating section for heated cigarettes, characterized in that: The thick stock flakes according to claim 12 are added.
14. A novel heated cigarette, characterized in that: A heating section as claimed in claim 13 is provided.