Method for producing resin molded product, molding die, and resin molding apparatus

MYPI2025005418A0Undetermined Publication Date: 2024-09-08TOWA
View PDF 0 Cites 0 Cited by

Patent Information

Application Number
MYPI2025005418
Authority / Receiving Office
MY · MY
Patent Type
Applications
Current Assignee / Owner
Priority Date
2023-03-08
Filing Date
2023-10-30
Publication Date
2024-09-08

AI Technical Summary

Technical Problem

In compression molding using a mold release film, existing configurations can lead to wrinkles in the film, causing defects in resin molded products and potentially resulting in protrusions that may fall during transportation, disrupting production and productivity.

Method used

A method and apparatus for manufacturing resin molded products using a mold with a lower mold side member featuring a step of depth equal to or less than the release film thickness, combined with an air vent groove, to suppress film wrinkles and prevent protrusions from forming on the resin product.

Benefits of technology

This configuration effectively prevents film wrinkles and resin protrusions, enhancing product quality and reducing the risk of defects and production interruptions during transportation.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure PI2025005418_DRAWING_001
    Figure PI2025005418_DRAWING_001
  • Figure PI2025005418_DRAWING_002
    Figure PI2025005418_DRAWING_002
  • Figure PI2025005418_DRAWING_003
    Figure PI2025005418_DRAWING_003
Patent Text Reader

Abstract

ABSTRACT METHOD FOR PRODUCING RESIN MOLDED PRODUCT, MOLDING DIE, AND RESIN MOLDING APPARATUS The present disclosure provides a method for producing a resin molded product that suppresses the formation of resin protrusions that may fall off during the conveyance of the resin molded products after resin molding while suppressing the formation of wrinkles in the release film during compression molding using a release film. In the method for producing a resin molded product of the present disclosure, in resin molding, a resin molded product is produced by performing resin molding through compression molding by clamping a molding die in a state where a molding target is placed between an upper die and a lower die (200), a release film is placed on a bottom surface and a side surface of a cavity (200A), and a resin material is placed on the release film, and in conveying, the molding die is opened after the resin molding, and the molded product is taken out of the molding die and then conveyed, and on an upper surface of a lower die side surface member (201), a step (201D) having a depth equal to or less than a thickness of the release film is formed at a position adjacent to an inner peripheral surface of the lower die side surface member (201). (The most illustrative figure: Figure 1)
Need to check novelty before this filing date? Find Prior Art

Description

Manufacturing method of resin molded product, molding die and resin molding device

[0001] The present disclosure relates to a method for manufacturing a resin molded product, a molding die, and a resin molding device.

[0002] Compression molding using a mold is widely used to produce resin molded products. In this compression molding, a release film is sometimes used to prevent resin leakage from the mold.

[0003] Patent Document 1 describes a configuration in which a protrusion is formed on the outer peripheral edge of the upper surface of the bottom member (compression mold) of the lower mold of a molding die used for compression molding using a release film, and a step is formed on the inner peripheral surface of the lower mold side member (frame mold). According to the description in Patent Document 1, this configuration makes it possible to remove wrinkles that occur in the release film when the release film is placed on the upper surface of the lower mold and clamped during compression molding. By preventing wrinkles from occurring in the release film, it is possible to suppress defects in resin molded products caused by the wrinkles.

[0004] JP 2013-180461 A

[0005] However, with the molding die described in Patent Document 1, protrusions corresponding to the steps of the lower die side member remain on the outer periphery of the resin molded product after resin molding. If such protrusions remain, there is a risk that the protrusions will fall off when the resin molded product is removed from the molding die and transported. Such falling protrusions may cause defective products or cause the resin molding device to stop operating, thereby reducing productivity.

[0006] Therefore, the present disclosure aims to provide a method for manufacturing a resin molded product, a molding die, and a resin molding device that, during compression molding using a release film, suppresses the occurrence of wrinkles in the release film while suppressing the formation of resin protrusions that may fall off during transportation of the resin molded product after resin molding.

[0007] In order to achieve this object, the manufacturing method of the resin molded product disclosed herein is a manufacturing method of a resin molded product that uses a molding die to manufacture a resin molded product, wherein the molding die includes an upper die and a lower die, the upper die and the lower die being arranged opposite each other, the lower die including a lower die bottom member and a lower die side member, a cavity is formed by a space surrounded by an upper surface of the lower die bottom member and an inner peripheral surface of the lower die side member, the upper surface of the lower die bottom member forms the bottom surface of the cavity, and the inner peripheral surface of the lower die side member forms the side surface of the cavity, the manufacturing method of the resin molded product includes a resin molding step and a conveying step, the resin molding step is a step in which an object to be molded is placed between the upper die and the lower die, a release film is placed on the bottom and side surfaces of the cavity, and a resin material is placed on the release film, and the molding die is clamped to perform resin molding by compression molding to manufacture the resin molded product, The transporting process is a process of opening the mold after the resin molding process, and removing and transporting the resin molded product from the mold, and this is a method for manufacturing a resin molded product, in which a step having a depth equal to or less than the thickness of the release film is formed on the upper surface of the lower mold side member at a location adjacent to the inner surface of the lower mold side member.

[0008] The first molding die of the present disclosure is the molding die used in the method for producing a resin molded product of the present disclosure.

[0009] a second molding die according to the present disclosure, which is a molding die for compression molding used in a method for manufacturing a resin molded product, the molding die including an upper die and a lower die, the upper die and the lower die being arranged opposite each other, the lower die including a lower die bottom member and a lower die side member, a cavity being formed by a space surrounded by an upper surface of the lower die bottom member and an inner peripheral surface of the lower die side member, the upper surface of the lower die bottom member forming the bottom surface of the cavity, and the inner peripheral surface of the lower die side member forming the side surface of the cavity, and in the method for manufacturing a resin molded product, an object to be molded is placed between the upper die and the lower die, a release film is placed on the bottom and side surfaces of the cavity, and a resin material is placed on the release film, and the molding die is then clamped to perform resin molding by compression molding to manufacture the resin molded product, and a step having a depth equal to or less than the thickness of the release film is formed on the upper surface of the lower die side member at a location adjacent to the inner peripheral surface of the lower die side member. In the following description, the term "the mold of the present disclosure" includes both the first mold of the present disclosure and the second mold of the present disclosure, unless otherwise specified.

[0010] The resin molding apparatus of the present disclosure is a resin molding apparatus including: the molding die of the present disclosure; and a mold clamping mechanism that clamps the upper mold and the lower mold of the molding die.

[0011] According to the present disclosure, it is possible to provide a method for manufacturing a resin molded product, a molding die, and a resin molding device that, in compression molding using a release film, suppress the occurrence of wrinkles in the release film while suppressing the formation of resin protrusions that may fall off during transport of the resin molded product after resin molding.

[0012] FIG. 1 is a diagram showing an example of the configuration of a molding die of the present disclosure. FIG. 1( a) is a plan view. FIG. 1( b) is a cross-sectional view. FIG. 2 is a cross-sectional view illustrating one step in the method for manufacturing a resin molded product of the present disclosure. FIG. 3 is a cross-sectional view illustrating another step in the method for manufacturing a resin molded product of the present disclosure. FIG. 4 is a cross-sectional view illustrating yet another step in the method for manufacturing a resin molded product of the present disclosure. FIG. 5 is a cross-sectional view illustrating yet another step in the method for manufacturing a resin molded product of the present disclosure. FIG. 6 is a cross-sectional view illustrating yet another step in the method for manufacturing a resin molded product of the present disclosure. FIG. 7 is a cross-sectional view illustrating yet another step in the method for manufacturing a resin molded product of the present disclosure. FIG. 8 is a plan view showing an example of the configuration of a resin molding apparatus of the present disclosure.

[0013] In the present disclosure, the molding die is not particularly limited, but may be, for example, a metal mold or a ceramic mold.

[0014] In the present disclosure, when we say "suppressing" phenomena such as the formation of resin protrusions, sagging of the release film, and the occurrence of wrinkles in the release film, unless otherwise specified, it is not limited to minimizing the occurrence of these phenomena, but also includes reducing the occurrence of these phenomena to zero.

[0015] In the present disclosure, the resin molded product is not particularly limited, but may be, for example, an electronic component in which an electronic element such as an IC or semiconductor chip (hereinafter simply referred to as a "chip") is resin-encapsulated. More specifically, for example, by resin-encapsulating a chip, the chip can be made into a resin-encapsulated electronic component (also referred to as a finished electronic component or package, etc.; hereinafter simply referred to as an "electronic component"). Generally, the term "electronic component" can refer to a chip before resin-encapsulation or to a chip in a resin-encapsulated state. However, in the present disclosure, a chip before resin-encapsulation is also referred to as an "electronic element," and a resin-encapsulated chip is referred to as an "electronic component" (a finished electronic component). In other words, in the present disclosure, "chip" and "electronic element" are synonymous, and specific examples include chips such as ICs, semiconductor chips, power control semiconductor elements, resistor elements, and capacitor elements. A "semiconductor element" refers to, for example, a circuit element made from a semiconductor material. The "chip" or "electronic element" in the present disclosure is not particularly limited as long as it is a chip before being sealed with resin, and does not have to be in chip form.

[0016] In the present disclosure, the resin material before molding and the resin after molding are not particularly limited and may be, for example, a thermosetting resin such as an epoxy resin or a silicone resin, or a thermoplastic resin. Furthermore, a composite material containing a thermosetting resin or a thermoplastic resin may also be used. In the present disclosure, examples of the form of the resin material before molding include powdered or granular resin (including granular resin), liquid resin, sheet-like resin, tablet-like resin, etc. In the present disclosure, liquid resin may be liquid at room temperature, or may include molten resin that melts and becomes liquid when heated. The resin may be in any other form as long as it can be supplied to a mold cavity, pot, etc.

[0017] Hereinafter, specific embodiments of the present disclosure will be described with reference to the drawings. For the sake of convenience, the drawings are schematically drawn with appropriate omissions and exaggerations. Embodiment 1

[0018] In this embodiment, an example of a molding die according to the present disclosure and an example of a method for manufacturing a resin molded product using the molding die will be described.

[0019] An example of the configuration of a molding die according to the present disclosure is shown in Figure 1. Figure 1(a) is a plan view (top view). Figure 1(b) is a cross-sectional view taken along the line II in Figure 1(a). However, in Figure 1, for the sake of simplicity, the upper mold of the molding die is omitted, and the lower mold is also shown in a simplified form.

[0020] As shown in Figure 1, this molding die includes a lower die 200. Although not shown, as described above, this molding die also includes an upper die. The upper die and lower die 200 are arranged so that the lower surface of the upper die and the upper surface of the lower die 200 face each other. The configuration of the upper die is not particularly limited, but may be, for example, a configuration in which an object to be molded can be fixed to the lower surface of the upper die, as shown in Figures 2 to 7 described below.

[0021] As shown in the figure, lower mold 200 includes lower mold bottom member 202 and lower mold side member 201. Cavity 200A is formed by the space surrounded by the upper surface of lower mold bottom member 202 and the inner peripheral surface of lower mold side member 201. The upper surface of lower mold bottom member 202 forms the bottom surface of cavity 200A, and the inner peripheral surface of lower mold side member 201 forms the side surface of cavity 200A. As will be described below with reference to Figures 2 to 7, a resin molded product is manufactured by placing an object to be molded between upper mold and lower mold 200, placing release films on the bottom and side surfaces of cavity 200A, and clamping the mold to perform resin molding by compression molding with a resin material placed on the release film.

[0022] In addition, in the lower mold 200 shown in FIG. 1, the outer peripheral edge of the upper surface of the lower mold bottom member 202 is flush with no protrusions.

[0023] A step 201D having a depth equal to or less than the thickness of the release film is formed on the upper surface of the lower mold side surface member 201 at a location adjacent to the inner peripheral surface of the lower mold side surface member 201. The outer end of the step 201D is located inside the outer edge of the area α where the molding object is placed. Furthermore, an air vent groove 201C is formed on the upper surface of the lower mold side surface member 201, extending outward beyond the step 201D. The air vent groove 201C is a groove formed on the upper surface of the lower mold side surface member 201. There are multiple air vent grooves 201C, which are formed radially around a portion of the periphery of the step 201D. In FIG. 1 , the step 201D and the air vent groove 201C are connected. The outer end of the air vent groove 201C is located outside the outer edge of the area α where the molding object is placed. For example, gas (such as air) in the cavity 200A can be released into the air vent groove 201C. It is also possible to suck the release film through the air vent groove 201C, for example.

[0024] The width W1 of the step 201D (the distance from the side in contact with the inner peripheral surface of the lower mold side member 201 to the opposite side) is not particularly limited, but is preferably 0.05 mm or more, for example, from the viewpoint of making it easier to suppress the occurrence of wrinkles in the release film. The upper limit is not particularly limited, and although it depends on the distance from the end face of the object to be molded (e.g., a substrate) to the step 201D, it is, for example, 30 mm or less, 20 mm or less, 10 mm or less, 5 mm or less, 4 mm or less, 3 mm or less, 2 mm or less, 1 mm or less, 0.5 mm or less, 0.4 mm or less, 0.3 mm or less, 0.2 mm or less, or 0.1 mm or less.

[0025] 1, steps 201D are formed on the upper surface of lower mold side member 201 around the entire periphery (all locations) of the portion adjacent to the inner periphery of lower mold side member 201. However, the present disclosure is not limited to this, and steps 201D do not have to be formed around the entire periphery. For example, steps 201D may be formed only in a portion of the upper surface of lower mold side member 201 that is adjacent to the inner periphery of lower mold side member 201, and steps 201D may not be formed in other portions. Specifically, for example, a structure in which steps 201D are not provided in some locations where leakage of even a very small amount of resin material is not permitted may be used.

[0026] Furthermore, through holes 201A and 201B are formed in the upper surface of the lower mold side member 201. Through hole 201A is located partially outside step 201D and air vent groove 201C, penetrating from the upper surface to the lower surface of the lower mold side member 201. As shown in the figure, through hole 201A has a structure in which a groove having a V-shaped cross section when viewed from the side is formed in the upper surface of the lower mold side member 201, and multiple through holes having a circular planar shape are formed at the bottom of the V-shaped groove. Through hole 201B is arranged to surround the entire outer periphery of through hole 201A, penetrating from the upper surface to the lower surface of the lower mold side member 201. As will be described later with reference to Figures 2 to 7, a release film can be sucked through through hole 201A and through hole 201B and adsorbed to the cavity surface of cavity 200A. Furthermore, as will be described later, resin for resin molding can be contained within cavity 200A.

[0027] Next, an example of a method for manufacturing a resin molded product according to the present disclosure using the mold shown in Fig. 1 and the resin molding apparatus according to the present disclosure including the mold will be described with reference to the schematic cross-sectional process views of Fig. 2 to Fig. 7. In Fig. 2 to Fig. 7, the same components as those in Fig. 1 are designated by the same reference numerals. However, for convenience of illustration, the shapes and the like may differ from those in Fig. 1.

[0028] First, the configuration of the resin molding apparatus will be described using FIG. 2. As shown in the figure, the molding mold in this resin molding apparatus includes an upper mold 100 in addition to the lower mold 200 shown in FIG. 1. Furthermore, as shown in FIG. 1, this resin molding apparatus includes, in addition to the molding mold, an outside air blocking member 300 and a release film adsorption mechanism (not shown). The mold surfaces of the upper mold 100 and the lower mold 200 face each other. The upper mold 100 is fixed to the lower surface of an upper mold holding member 110. The lower mold 200 is fixed to the upper surface of a lower mold holding member 210. The upper mold 100 is a mold to which a substrate 10 is fixed, as described below. The substrate 10 corresponds to the "molded object" in this disclosure. The lower mold 200 is a mold in which a cavity is formed on the mold surface, and a release film is adsorbed to this mold surface, as described below. The outside air blocking member 300 is attached to the lower surface of the upper mold holding member 110 and the upper surface of the lower mold holding member 210 so as to surround the periphery of the upper mold 100 and the lower mold 200. As will be described later, the outside air blocking member 300, together with the upper mold holding member 110 and the lower mold holding member 210, surrounds the molding dies (upper mold 100 and lower mold 200) and can block them from the outside air.

[0029] The upper mold 100 is formed by attaching a film holder 103 and a clamper 104 to an upper mold body 102. The film holder 103 is attached to the lower part of the upper mold body 102 via an upper mold elastic member 103s. In this embodiment, a spring is used as the upper mold elastic member. The film holder 103 can move up and down by expanding and contracting the upper mold elastic member 103s. As will be described later, the film holder 103 can press the release film against the lower mold side member 201. As shown in the figure, the clamper 104 can clamp and fix the substrate 10 between the lower surface of the upper mold body 102 and the clamper 104. The arrangement positions of the film holder 103 and the clamper 104 are not limited to those shown in FIG. 2 and can be arbitrary.

[0030] The upper mold body 102 and the upper mold holding member 110 are provided with through-holes 100B and 300B that penetrate from their upper surface to their lower surface. The lower end of the through-hole 100B opens into the fixing surface of the substrate 10 on the lower surface of the upper mold body 102. As will be described later, the substrate 10 can be adsorbed to the upper mold body 102 by suctioning the inside of the through-hole 100B to reduce the pressure. The lower end of the through-hole 300B opens into the outer periphery of the fixing surface of the substrate 10. As will be described later, the space surrounded by the outside air blocking member 300 can be made negative pressure by suctioning the inside of the through-hole 300B to reduce the pressure.

[0031] As described in FIG. 1 , the lower mold 200 has a lower mold bottom surface member 202 and a lower mold side surface member 201. The lower mold side surface member 201 is attached to the peripheral portion of the upper surface of the lower mold bottom surface member 202 via a lower mold elastic member 201s. In this embodiment, a spring is used as the lower mold elastic member. The lower mold side surface member 201 can move up and down by expanding and contracting the lower mold elastic member 201s. As shown in the figure, a cavity 200A is formed by the space surrounded by the central portion of the upper surface of the lower mold bottom surface member 202 (the portion where the lower mold side surface member 201 is not attached) and the inner surface of the lower mold side surface member 201. As will be described later, resin for resin molding can be contained within the cavity 200A.

[0032] As described above, the outer peripheral edge of the upper surface of the lower mold bottom member 202 is flush with no protrusions.

[0033] 1 are formed on the upper surface of the lower mold side surface member 201. The arrangement and configuration of the step 201D and the air vent groove 201C are as described in FIG.

[0034] As described above, the lower mold side surface member 201 has through holes 201A and 201B. The lower mold bottom surface member 202 and the lower mold holding member 210 have through holes 200B. The lower end of the through hole 200B opens from the lower surface of the lower mold bottom surface member 202 to the lower surface of the lower mold holding member 210, and the other end connects to the gap between the lower mold bottom surface member 202 and the lower mold side surface member 201, forming the through hole 200B together with the gap. The through hole 201A penetrates the lower mold holding member 210 and further penetrates from the lower surface of the lower mold bottom surface member 202 to the upper surface of the inner edge of the lower mold side surface member 201. The through hole 201B penetrates the lower mold holding member 210 and further penetrates from the lower surface of the lower mold bottom surface member 202 to the upper surface of the outer edge of the lower mold side surface member 201. As will be described later, the release film can be adsorbed onto the mold surface of the lower mold 200 by suctioning the inside of the through holes 200B, 201A, and 201B using a release film adsorption mechanism to reduce the pressure. Then, as will be described later, resin molding is performed with the release film adsorbed between the mold surfaces of the upper mold 100 and the lower mold 200. Note that the lower mold side surface member 201 may or may not have a through hole for adsorbing the release film, and even if there is a through hole, its arrangement is optional.

[0035] Although not shown, a vacuum pump or the like can be used as the release film suction mechanism. Furthermore, although not shown, this resin molding apparatus further includes a transport mechanism that opens the molding die after resin molding, removes the resin molded product from the molding die, and transports it.

[0036] The outside air blocking member 300 is attached to the peripheral edge of each of the upper mold holding member 110 and the lower mold holding member 210. Elastic O-rings 300A are provided between the upper mold holding member 110 and the upper outside air blocking member 300, between the upper outside air blocking member 300 and the lower outside air blocking member 300, and between the lower outside air blocking member 300 and the lower mold holding member 210.

[0037] Next, an example of a resin molding method using this resin molding apparatus will be described. First, as shown in FIG. 2, the substrate 10 is clamped and fixed between the lower surface of the upper mold body 102 and the clamper 104. As described above, the substrate 10 corresponds to the "molding target" in this disclosure. As shown in the figure, a chip 10a is fixed to the lower surface of the substrate 10 (the surface opposite to the surface fixed to the upper mold body 102). During resin molding, the chip 10a can be resin-encapsulated to produce an electronic component (resin molded product). However, the present disclosure is not limited thereto. For example, components such as chips may not be fixed to the substrate. Furthermore, for example, components other than chips (e.g., wires) may be fixed to the substrate. Furthermore, as shown in the figure, the release film 11, together with the resin material 20a placed thereon, is transported to the mold surface of the lower mold 200. The means and method for placing the resin material 20a on the release film 11 are not particularly limited, and known means and methods such as a feeder may be used as appropriate. The means and method for transporting the release film 11 and the resin material 20a to the position of the mold surface of the lower mold 200 are not particularly limited, and known means and methods such as a loader may be used as appropriate. In addition, although the resin material 20a is a granular resin in this embodiment, it is not limited thereto, and may be, for example, a sheet-like resin, a liquid resin, a tablet-like resin, a semi-solid fluid resin, or the like.

[0038] Next, as shown in FIGS. 3 and 4, a release film adsorption process is performed. First, as shown in FIG. 3, the release film 11 and resin material 20a are transferred to the lower mold 200. Furthermore, as indicated by arrows 201a and 201b, the pressure inside the through-holes 201A and 201B in the lower mold side surface member 201 is reduced by a release film adsorption mechanism (not shown). The release film adsorption mechanism is not particularly limited, but may be, for example, a vacuum pump. As a result, the release film 11 is adsorbed to the upper surface of the lower mold side surface member 201, and tension is applied to the release film 11 placed on the cavity 200A, smoothing out any wrinkles in the release film. At this time, the step 201D formed in the lower mold side surface member 201 stretches the release film by the step 201D, further promoting the stretching of the release film. This suppresses slack in the release film. Therefore, the occurrence of wrinkles in the release film is suppressed, and it is possible to suppress defects in the resin molded product caused by the wrinkles. Furthermore, by forming the air vent grooves 201C in the lower mold side surface member 201, it is possible to further suppress the occurrence of slack and wrinkles in the release film, and it is possible to suppress defects in the resin molded product caused by the wrinkles.

[0039] Furthermore, as shown by arrow 200b in FIG. 4 , the through-hole 200B, which communicates with the gap between the lower mold side surface member 201 and the lower mold bottom surface member 202, is depressurized and suctioned by a release film suction mechanism. This applies further tension to the release film 11, smoothing out any wrinkles, and the release film 11 is adsorbed onto the cavity surface of the cavity 200A. In this manner, the release film 11 is disposed on the bottom and side surfaces of the cavity 200A. As a result, as shown in the figure, the resin material 20a is placed (disposed) in the cavity 200A while being placed (disposed) on the release film 11. At this time, it is preferable to place the release film 11 at least on the upper surface of the step 201D in the lower mold side surface member 201, as shown in the figure. Furthermore, the order in which the release film 11 is adsorbed onto the lower mold 200 is not limited to the above-mentioned order, and can be changed as appropriate depending on the type of release film 11 as long as the release film 11 can be adsorbed onto the cavity surface of the cavity 200A without causing wrinkles.

[0040] As indicated by arrow 100b in Fig. 4, the inside of the through-hole 100B of the upper mold body 102 is depressurized and suctioned by a workpiece suction mechanism (not shown). The workpiece suction mechanism is not particularly limited, but may be, for example, a vacuum pump. As a result, the entire upper surface of the substrate 10 is suctioned to the lower surface of the upper mold body 102, and the substrate 10 is more firmly fixed. Note that suction of the substrate 10 to the upper mold body 102 may begin in this manner at the stage shown in Fig. 2 or 3, for example.

[0041] In this embodiment, the mechanism for holding (fixing) the substrate (molding object) to the upper mold uses suction by reducing pressure in addition to clamping by a clamper. This increases the force for suctioning the substrate and also increases the force for peeling off the release film. However, in the present disclosure, the mechanism for holding the molding object to the upper mold is not limited to this, and may be, for example, clamping only by a clamper.

[0042] In this embodiment, the molding die is constantly preheated by a heater (not shown) provided inside the molding die, and the resin material 20a begins to melt when placed in the cavity 200A together with the release film 11, eventually becoming molten resin 20b. The molten resin 20b corresponds to the molten "resin material." Note that preheating of the molding die may be carried out prior to or simultaneously with the release film adsorption step (FIGS. 3 and 4). Alternatively, preheating of the molding die may begin after the release film adsorption step.

[0043] Next, the resin molding process and the transport process are carried out as shown in Figures 5 to 7. As described above, the resin molding process is a process in which an object to be molded is placed between the upper and lower molds, release films are placed on the bottom and side surfaces of the cavity, and a resin material is placed on the release film, and then the molds are clamped to perform resin molding by compression molding, thereby producing a resin molded product. As described above, the transport process is a process in which the molds are opened after the resin molding process, and the resin molded product is removed from the molds and transported.

[0044] First, the lower mold holding member 210 is raised, and the lower mold 200 is raised together with the outside air blocking member 300. As a result, as shown in Fig. 5 , the upper and lower outside air blocking members 300 are first closed via their respective O-rings 300A, and the molding dies (upper mold 100 and lower mold 200) are blocked from outside air by the upper mold holding member 110, the lower mold holding member 210, and the outside air blocking member 300. Hereinafter, the space S surrounded by the upper mold holding member 110, the lower mold holding member 210, and the outside air blocking member 300 may be referred to as "inside the outside air blocking space." Almost simultaneously with the closing of the outside air blocking member 300, the film holder 103 comes into contact with the lower mold side surface member 201 via the release film 11, and the release film 11 is sandwiched between the lower mold side surface member 201 and the film holder 103. At this time, the upper mold 100 and the lower mold 200 have not yet been clamped, and the substrate 10 and the molten resin 20b have not yet come into contact. In this state, as shown by arrow 300b, the pressure inside the through-hole 300B of the upper mold 100 is reduced by an external air blocking member internal decompression mechanism (not shown). This creates a negative pressure inside the external air blocking space S. The external air blocking member internal decompression mechanism is not particularly limited, and may be, for example, a vacuum pump.

[0045] Thereafter, as shown in FIG. 6 , the lower mold holding member 210 (lower mold 200) is further raised. This causes the chip 10a to be immersed in the molten resin 20b, and the substrate 10 to come into contact with the molten resin 20b. In this manner, the molten resin 20b fills the cavity 200A, and the upper mold 100 and the lower mold 200 are clamped together. At this time, the outer peripheral edge of the upper surface of the lower mold bottom member 202 is flush with no protrusions formed thereon, so the height of the outer peripheral edge of the upper surface of the lower mold bottom member 202 is lower than the height of the step 201D in the lower mold side member 201. As a result, no protrusions corresponding to the protrusions (steps) on the outer peripheral edge of the upper surface of the lower mold bottom member 202 are formed on the manufactured resin molded product. Therefore, such protrusions do not fall off when the resin molded product is removed from the mold and transported. Therefore, there is no risk that the falling of such protrusions could result in defective products or stop the operation of the resin molding device, thereby reducing productivity. Furthermore, since the resin material is not wasted due to the generation of such protrusions, the yield is also good. In addition, since the effective area of ​​the substrate 10 is not reduced, the substrate 10 can be used efficiently.

[0046] Furthermore, as described above, the depth of the step 201D is equal to or less than the thickness of the release film 11. This makes it possible to suppress the phenomenon in which the molten resin 20b penetrates into the portion of the step 201D, hardens, and forms an excess resin portion (resin burr). Furthermore, if the depth of the step 201D is equal to or less than the thickness of the release film 11, even if the molten resin 20b penetrates into the portion of the step 201D, the amount is very small. Therefore, even if an excess resin portion as described above is formed, it will be an extremely thin and lightweight excess resin portion, and problems caused by the excess resin portion falling off are unlikely to occur.

[0047] In this case, it is sufficient that the step 201D is formed inside the edge surface of the substrate 10 in a plan view, and for example, the distance W2 from the outer edge surface of the step 201D to the edge surface of the substrate 10 can be 1 mm or more. The upper limit of the distance W2 is not particularly limited, but is, for example, 50 mm or less, 40 mm or less, 30 mm or less, 20 mm or less, 10 mm or less, 5 mm or less, 4 mm or less, 3 mm or less, or 2 mm or less. The distance W2 can also be expressed as the distance between the outer edge surface of the step 201D and the outer edge of the placement area of ​​the molding object (substrate 10).

[0048] After the mold is closed, the pressure inside the outside air shielding space S is returned to atmospheric pressure. The timing for returning the pressure inside the outside air shielding space S to atmospheric pressure may be any time after the mold is closed and before the hardening of the molten resin 20b is completed.

[0049] Furthermore, as shown in FIG. 7, the molten resin 20b is solidified (cured) to complete the resin molding process, producing a resin molded product, and the release film is peeled off from the resin molded product.

[0050] First, the molten resin 20b is solidified in the mold clamped state as shown in FIG. 6 . For example, if the molten resin 20b is a thermosetting resin, the mold may be further heated by an internal heater to form a cured resin (cured resin 20 shown in FIG. 7 ). Alternatively, if the molten resin 20b is a thermoplastic resin, the mold may be stopped from heating and allowed to cool, or the mold may be rapidly cooled, to solidify the molten resin 20b and form the cured resin 20. Even after the mold is clamped, a force acts on the lower mold holding member 210 to lift the lower mold 200, so the molten resin 20b hardens while being compressed. This allows the production of a resin molded product 30 ( FIG. 7 ) including the substrate 10, the chip 10a, and the cured resin 20.

[0051] Thereafter, the molds are opened, and a conveying step is carried out in which the resin molded article is removed from the molds and conveyed. Specifically, as shown in Figure 7, first, the lower mold holding member 210 is lowered, and the lower mold 200 and the outside air blocking member 300 are lowered, thereby opening the upper mold 100 and the lower mold 200. As a result, as shown in the figure, the release film 11 that has adhered to the cured resin 20 is peeled off from the cured resin 20. Thereafter, the resin molded article 30 is removed from the molds and conveyed by a conveying mechanism (not shown).

[0052] As described above, the method for manufacturing a resin molded product of this embodiment is carried out, and a resin molded product 30 in which one surface of the substrate 10 is resin-molded with the cured resin 20 can be manufactured.

[0053] According to the molding die of the present disclosure, for example, it is possible to improve the releasability between a resin molded product and a release film with an extremely simple configuration, without depending on molding conditions and without providing a resin pool outside the molding area. Embodiment 2

[0054] In this embodiment, an example of the overall configuration of a resin molding apparatus according to the present disclosure and a method for manufacturing a resin molded product using the same will be described.

[0055] Referring to FIG. 8, an example of a resin molding method using the resin molding apparatus 1 will be described. The resin molding apparatus 1 uses granular resin 20a (see FIGS. 2 to 4) as the resin material. First, in the substrate supply / storage module 41, the substrate 10 (see FIGS. 2 to 7) is sent from the substrate supply unit 44 to the substrate placement unit 50. Next, the substrate transfer mechanism 51 is moved in the -Y direction from a predetermined position S1 to receive the substrate 10 from the substrate placement unit 50. The substrate transfer mechanism 51 is then returned to the predetermined position S1. Next, of the three molding modules 42A to 42C provided in the resin molding apparatus 1, for example, the substrate transfer mechanism 51 is moved in the +X direction to a predetermined position P1 of molding module 42B. Next, in molding module 42B, the substrate transfer mechanism 51 is moved in the -Y direction and stopped at a predetermined position C1 above the lower mold 200. Next, the substrate transfer mechanism 51 is raised to secure the substrate 10 to the upper mold 100. Thereafter, the substrate transport mechanism 51 is returned to the predetermined position S1 of the substrate supply / storage module 41.

[0056] As will be described later, the substrate transport mechanism 51 can also be used as a "transport mechanism" for removing and transporting a resin molded product from the opened mold after resin molding.

[0057] Next, the release film 11 stored in the release film supply mechanism 53 is received by the material transport mechanism 56, transported to the lower mold 200 of the molding mold of the molding module 42B, and placed in the cavity 200A of the lower mold 200.

[0058] Next, the XY table 52 is moved in the -Y direction from the predetermined position T1, and stopped at a predetermined position below the resin material containing frame 54. The resin material containing frame 54 is placed on the XY table 52. The XY table 52 on which the resin material containing frame 54 is placed is moved in the +X direction, and the resin material containing frame 54 is stopped at a predetermined position below the resin material supply mechanism 55. By moving the XY table 52 in the X and Y directions, a predetermined amount of resin material 20a (see FIGS. 2 to 4) is supplied from the resin material supply mechanism 55 to the resin material containing frame 54. The XY table 52 on which the resin material containing frame 54 is placed is returned to the predetermined position T1.

[0059] Next, the material conveying mechanism 56 is moved in the -Y direction from the predetermined position M1 to receive the resin material containing frame 54 placed on the XY table 52. The material conveying mechanism 56 is returned to the predetermined position M1. Next, the material conveying mechanism 56 is moved in the -X direction to a predetermined position P1 in the molding module 42B. Next, in the molding module 42B, the material conveying mechanism 56 is moved in the -Y direction and stopped at a predetermined position C1 above the lower mold 200. The material conveying mechanism 56 is lowered to supply the resin material 20a to the upper surface of the release film 11 placed in the cavity 200A. After the supply is completed, the material conveying mechanism 56 is returned to the predetermined position M1.

[0060] Next, in molding module 42B, the "resin molding step" in the manufacturing method of a resin molded product of the present disclosure is performed. In this "resin molding step," a substrate (molding object) 10 is placed between the upper mold and the lower mold, a release film 11 (see FIGS. 2 to 7) is placed on the bottom and side surfaces of cavity 200A, and a resin material is placed on release film 11. The molds are then clamped to perform resin molding by compression molding, thereby producing resin molded product 30. In this embodiment, lower mold 200 is raised by mold clamping mechanism 60, and upper mold 100 and lower mold 200 are clamped together to perform resin molding, producing resin molded product 30. More specifically, this "resin molding step" can be performed, for example, as described with reference to FIGS. 5 to 7.

[0061] After the resin molding step, a "transport step" in the manufacturing method of a resin molded product of the present disclosure is performed. This transport step is a step of opening the molding die and removing and transporting the resin molded product 30 from the molding die. Specifically, first, after resin molding is completed, the upper die 100 and lower die 200 of the molding die are opened. After the molding die is opened, the substrate transport mechanism 51 is moved from a predetermined position S1 of the substrate supply / storage module 41 to a predetermined position C1 on the lower die 200 to receive the resin molded product 30. Next, the substrate transport mechanism 51 is moved to transfer the resin molded product 30 to the substrate placement unit 50. The resin molded product 30 is stored from the substrate placement unit 50 in the resin molded product storage unit 45.

[0062] In this embodiment, three molding modules 42A, 42B, and 42C are installed in a line in the X direction between the substrate supply / storage module 41 and the material supply module 43. However, the number of molding modules is not limited to three and can be any number. Alternatively, the substrate supply / storage module 41 and the material supply module 43 may be combined into a single module, and one molding module 42A may be installed in that module in a line in the X direction. This allows the number of molding modules 42A, 42B, ... to be increased or decreased. Therefore, the configuration of the resin molding apparatus 1 can be optimized according to the production type and production volume, thereby improving productivity.

[0063] In this embodiment, the release film supply mechanism 53 that supplies the release film 11 is provided inside the material supply module 43. However, the present invention is not limited to this, and the release film supply mechanism 53 that supplies the release film 11 may be provided as a new release film supply module instead of inside the material supply module 43. In this case, for example, the release film supply module may be installed between the molding module 42C and the material supply module 43 or next to the material supply module 43 on the opposite side of the molding module 42C. In this way, the resin molding apparatus 1 can be configured simply by adding a release film supply module to a conventional apparatus.

[0064] Furthermore, the present disclosure is not limited to the above-described embodiments, and can be arbitrarily and appropriately combined, modified, or selected and adopted as needed within the scope that does not deviate from the spirit of the present disclosure.

[0065] Some or all of the above embodiments may be described as in the following supplementary notes, but are not limited to the following: (Supplementary Note 1) A method for manufacturing a resin molded product using a molding die, wherein the molding die includes an upper die and a lower die, the upper die and the lower die are arranged opposite each other, the lower die includes a lower die bottom member and a lower die side member, a cavity is formed by a space surrounded by an upper surface of the lower die bottom member and an inner peripheral surface of the lower die side member, the upper surface of the lower die bottom member forms the bottom surface of the cavity, and the inner peripheral surface of the lower die side member forms the side surface of the cavity, the method for manufacturing a resin molded product includes a resin molding step and a conveying step, the resin molding step is a step of manufacturing the resin molded product by clamping the molding die and performing resin molding by compression molding in a state in which an object to be molded is placed between the upper die and the lower die, a release film is placed on the bottom and side surfaces of the cavity, and a resin material is placed on the release film, The transporting step is a step of opening the molding die after the resin molding step, and removing and transporting the resin molded product from the molding die, and the method for manufacturing a resin molded product, wherein a step having a depth equal to or less than the thickness of the release film is formed on the upper surface of the lower mold side member at a location adjacent to the inner peripheral surface of the lower mold side member. (Appendix 2) The method for manufacturing a resin molded product according to Appendix 1, wherein the resin molding step is carried out with the release film placed on at least the upper surface of the step in the lower mold side member. (Appendix 3) The method for manufacturing a resin molded product according to Appendix 1 or 2, wherein the step in the lower mold side member is formed in an annular shape. (Appendix 4) The method for manufacturing a resin molded product according to any of Appendices 1 to 3, wherein the outer end of the step in the lower mold side member is located inside the outer edge of the area where the molding object is placed. (Appendix 5) The method for manufacturing a resin molded product according to any of Appendices 1 to 4, wherein an air vent groove extending outside the step is formed on the upper surface of the lower mold side member. (Supplementary Note 6) The method for manufacturing a resin molded product according to Supplementary Note 5, wherein the step and the air vent groove are connected in the lower mold side surface member. (Supplementary Note 7) The method for manufacturing a resin molded product according to Supplementary Note 5 or 6, wherein an outer end of the air vent groove is located outside an outer edge of an area where the molding object is placed.(Supplementary Note 8) The method for manufacturing a resin molded product according to any one of Supplementary Notes 1 to 7, wherein the object to be molded is placed on a lower surface of the upper mold in the resin molding step. (Supplementary Note 9) The molding mold used in the method for manufacturing a resin molded product according to any one of Supplementary Notes 1 to 8. (Appendix 10) A molding die for compression molding used in a method for manufacturing a resin molded product, wherein the molding die includes an upper die and a lower die, the upper die and the lower die being arranged opposite each other, the lower die including a lower die bottom member and a lower die side member, a cavity being formed by a space surrounded by an upper surface of the lower die bottom member and an inner peripheral surface of the lower die side member, the upper surface of the lower die bottom member forming the bottom surface of the cavity, and the inner peripheral surface of the lower die side member forming the side surface of the cavity, the method for manufacturing a resin molded product, wherein an object to be molded is placed between the upper die and the lower die, a release film is placed on the bottom and side surfaces of the cavity, and a resin material is placed on the release film, and the molding die is clamped to perform resin molding by compression molding, thereby manufacturing the resin molded product, and a step having a depth equal to or less than the thickness of the release film is formed on the upper surface of the lower die side member at a location adjacent to the inner peripheral surface of the lower die side member. (Supplementary Note 11) A resin molding apparatus comprising: the molding die according to Supplementary Note 9 or 10; and a mold clamping mechanism that clamps the upper mold and the lower mold of the molding die. (Supplementary Note 12) The resin molding apparatus according to Supplementary Note 11, further including a transport mechanism that, after the resin molding, removes the resin molded product from the mold that has been opened and transports it.

[0066] This application claims priority based on Japanese Patent Application No. 2023-035729, filed on March 8, 2023, the disclosure of which is incorporated herein in its entirety by reference.

[0067] 1 Resin molding device 10 Substrate (molding object) 10a Chip 11 Release film 20 Cured resin (molded resin) 20a Resin material 20b Molten resin 30 Resin molded product 41 Substrate supply / storage module 42A, 42B, 42C Molding module 43 Material supply module 44 Substrate supply section 45 Resin molded product storage section 50 Substrate placement section 51 Substrate transport mechanism 52 XY table 53 Release film supply mechanism 54 Resin material storage frame 55 Resin material injection mechanism 56 Material transport mechanism 60 Mold clamping mechanism 100 Upper mold 100B Through hole 102 Upper mold body 103 Film holder 103s Upper mold elastic member 104 Clamper 110 Upper mold holding member 200 Lower mold 200A Cavity 200B Through-hole 201A, 201B Through-hole 201C Air vent groove 201D Step 201 Lower mold side surface member 201s Lower mold elastic member 202 Lower mold bottom surface member 210 Lower mold holding member 300 Outside air blocking member 300B Through-hole α Placement area of ​​molding object S Outside air blocking space

Claims

1. A method for manufacturing a resin molded product using a molding die, the molding die including an upper die and a lower die, the upper die and the lower die being arranged opposite each other, the lower die including a lower die bottom member and a lower die side member, a cavity being formed by a space surrounded by an upper surface of the lower die bottom member and an inner peripheral surface of the lower die side member, the upper surface of the lower die bottom member forming the bottom surface of the cavity, and the inner peripheral surface of the lower die side member forming the side surface of the cavity, the method for manufacturing a resin molded product including a resin molding step and a conveying step, the resin molding step being a step of manufacturing the resin molded product by clamping the molding die and performing resin molding by compression molding in a state in which an object to be molded is placed between the upper die and the lower die, a release film is placed on the bottom and side surfaces of the cavity, and a resin material is placed on the release film, The transporting step is a step of opening the mold after the resin molding step, and removing and transporting the resin molded product from the mold, and a step having a depth equal to or less than the thickness of the release film is formed on the upper surface of the lower mold side member at a location adjacent to the inner surface of the lower mold side member.

2. The method for producing a resin molded product according to claim 1, wherein the resin molding step is carried out with the release film placed on at least the upper surface of the step in the lower mold side member.

3. The method for manufacturing a resin molded product according to claim 1 or 2, wherein the step of the lower mold side member is formed in an annular shape.

4. A method for manufacturing a resin molded product according to any one of claims 1 to 3, wherein the outer end of the step in the lower mold side member is located inside the outer edge of the area in which the molded object is placed.

5. A method for manufacturing a resin molded product according to any one of claims 1 to 4, wherein an air vent groove is formed on the upper surface of the lower mold side member, the air vent groove extending beyond the step to the outside.

6. A method for manufacturing a resin molded product according to claim 5, wherein the step and the air vent groove are connected in the lower mold side member.

7. The method for manufacturing a resin molded product according to claim 5 or 6, wherein an outer end of the air vent groove is positioned outside the outer edge of the area in which the molded object is placed.

8. A method for manufacturing a resin molded product according to any one of claims 1 to 7, wherein in the resin molding step, the object to be molded is placed on the lower surface of the upper mold.

9. The molding die used in the method for producing a resin molded product according to any one of claims 1 to 8.

10. A molding die for compression molding used in a manufacturing method for a resin molded product, the molding die includes an upper die and a lower die, the upper die and the lower die being arranged opposite each other, the lower die includes a lower die bottom member and a lower die side member, a cavity is formed by a space surrounded by an upper surface of the lower die bottom member and an inner surface of the lower die side member, the upper surface of the lower die bottom member forms the bottom surface of the cavity, and the inner surface of the lower die side member forms the side surface of the cavity, the manufacturing method for the resin molded product, an object to be molded is placed between the upper die and the lower die, a release film is placed on the bottom and side surfaces of the cavity, and a resin material is placed on the release film, and the molding die is clamped to perform resin molding by compression molding to manufacture the resin molded product, and a step having a depth equal to or less than the thickness of the release film is formed on the upper surface of the lower die side member at a location adjacent to the inner surface of the lower die side member.

11. A resin molding device comprising: the molding die according to claim 9 or 10; and a clamping mechanism for clamping the upper die and the lower die of the molding die.

12. The resin molding apparatus according to claim 11, further comprising a transport mechanism for removing the resin molded product from the opened molding die and transporting it after the resin molding.