Method for pyrolyzing a plastic

MYPI2025006067A0Undetermined Publication Date: 2024-10-18OMV DOWNSTREAM GMBH
View PDF 0 Cites 0 Cited by

Patent Information

Application Number
MYPI2025006067
Authority / Receiving Office
MY · MY
Patent Type
Applications
Current Assignee / Owner
Priority Date
2023-04-18
Filing Date
2024-04-18
Publication Date
2024-10-18

AI Technical Summary

Technical Problem

Current plastic pyrolysis processes have a high carbon footprint and do not effectively utilize a significant portion of the pyrolysis residue, limiting their contribution to the circular economy and sustainability.

Method used

A method involving two pyrolysis steps in separate reactors, with a first pyrolysis reactor followed by separation into solids-rich and solids-poor fractions, and further pyrolysis of the solids-rich fraction in a second reactor, enhancing recycling and reducing environmental impact.

Benefits of technology

This approach significantly reduces greenhouse gas emissions, minimizes waste, and increases resource utilization, thereby strengthening the circular economy and improving economic efficiency by maximizing the use of pyrolysis residues.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure PI2025006067_DRAWING_001
    Figure PI2025006067_DRAWING_001
Patent Text Reader

Abstract

The invention relates to a method for pyrolyzing a plastic, in particular a waste plastic, comprising the steps of (a) pyrolyzing the plastic in a first pyrolysis reactor to obtain a first pyrolysis product, (b) separating a pyrolysis residue from the first pyrolysis product in a first separating unit, (c) separating the pyrolysis residue into a low-solid fraction and a high-solid fraction in a second separating unit, and (d) pyrolyzing the high-solid fraction in a second pyrolysis reactor to obtain a second pyrolysis product. The invention further relates to a device for pyrolyzing a plastic using said method.
Need to check novelty before this filing date? Find Prior Art

Description

[0001] Process for the pyrolysis of a plastic

[0002] The invention relates to a method and a device for the pyrolysis of a plastic, in particular a waste plastic.

[0003] Processes for pyrolyzing a starting material, particularly a plastic, are known in the art. The focus is on separating a gaseous fraction from a pyrolysis product, while the remainder of the pyrolysis product, particularly a solids-rich fraction, is typically utilized for energy recovery.

[0004] For example, EP 1 154 007 A1 discloses a process for the pyrolysis of a waste plastic. The waste plastic is pyrolyzed in a first pyrolysis reactor at a first temperature, whereby a first pyrolysis product comprising a first gaseous fraction and a first pyrolysis residue is obtained. The first pyrolysis residue is then pyrolyzed in a second pyrolysis reactor at a second temperature which is higher than the first temperature, whereby a second pyrolysis product comprising a second gaseous fraction and a second pyrolysis residue is obtained. The second pyrolysis residue is subjected to a magnetic separation process in order to obtain inorganic fillers and waste metals.

[0005] Another process for the pyrolysis of old plastic is described in WO 2016 / 116114 A1. The old plastic is converted in a pyrolysis reactor into a pyrolysis product comprising a gaseous fraction and a solid pyrolysis residue. The pyrolysis residue is then separated in a separation unit, such as a cyclone, into a low-solids fraction and a high-solids fraction. The low-solids fraction is returned to the pyrolysis reactor for further pyrolysis. The high-solids fraction is separated in a settling tank based on its density. A first part of the low-solids fraction with a lower density is returned to the pyrolysis reactor together with the low-solids fraction, while a second part of the high-solids fraction with a higher density can be used as a high-energy fuel.

[0006] Further processes for pyrolyzing starting materials are known from WO 2017 / 168163 Al, US 2022 / 340819 Al, US 2012 / 117860 Al and EP 4 151 702 Al.

[0007] While the pyrolysis product can be at least partially recycled using some of these processes, there is a need for a process with a reduced carbon footprint and a greater contribution to the circular economy and sustainability. One object of this invention is to utilize a larger portion of the pyrolysis residue for material recycling compared to known processes.

[0008] The process according to the invention for the pyrolysis of a plastic comprises the steps

[0009] ( a ) pyrolyzing the plastic in a first pyrolysis reactor to obtain a first pyrolysis product,

[0010] (b) separating a pyrolysis residue from the first pyrolysis product in a first separation unit,

[0011] ( c ) separating the pyrolysis residue into a low solids fraction and a high solids fraction in a second separation unit , and

[0012] (d) pyrolyzing the solids-rich fraction in a second pyrolysis reactor to obtain a second pyrolysis product.

[0013] The invention is further directed to a device for pyrolyzing a plastic, in particular a waste plastic, using the method according to the invention, comprising a first pyrolysis reactor for pyrolyzing the plastic, a first separation unit for separating the pyrolysis residue from the first pyrolysis product, a second separation unit for separating the pyrolysis residue into the low-solids fraction and the high-solids fraction, and a second pyrolysis reactor for pyrolyzing the high-solids fraction.

[0014] By performing two pyrolysis steps in two different pyrolysis reactors and separating the pyrolysis residue between the two pyrolysis steps into a low-solids fraction and a high-solids fraction, this process and device enable particularly good processing of the first and second pyrolysis products and separation into individual components, thus achieving a high degree of recycling. Consequently, the process can reduce environmental impact by lowering greenhouse gas emissions and reducing the amount of waste. Overall, this can significantly reduce resource consumption and strengthen the circular economy, which can also bring economic benefits.

[0015] The plastic preferably comprises a polyolefin and / or a polystyrene (PS), wherein the polyolefin may comprise a polyethylene (PE) and / or a polypropylene (PP). The plastic preferably comprises the polyolefin and / or the polystyrene in an amount of at least 65 wt.%, more preferably at least 70 wt.%, in particular at least 90 wt.%, based on the total weight of the plastic. This makes it possible to obtain a pyrolysis residue that comprises a significant proportion of an aliphatic hydrocarbon (or a mixture of several aliphatic hydrocarbons).

[0016] The plastic preferably comprises at least 20% by weight of the polyolefin, more preferably at least 50% by weight, even more preferably at least 70% by weight, in particular at least 90% by weight, based on the total weight of the plastic. With increasing polyolefin content, the amount of wax obtained using the process according to the invention can be increased, which can improve the economics of the process. The plastic can comprise another polymer from the group consisting of thermoplastics, thermosets and / or elastomers, in particular an acrylonitrile-butadiene-styrene copolymer (ABS), a polyvinyl chloride (PVC), a polyamide (PA) and / or a polyester.

[0017] Before step (a) of the process, the plastic can be plasticized, for example, in a mixer, especially in an extruder. The plastic is preferably heated to a temperature of at least 120°C to plasticize it, more preferably to a temperature of 200 to 500°C, even more preferably 400 to 470°C. The subsequent pyrolysis can then be carried out more energy-efficiently and in a shorter time.

[0018] In the extruder, the plastic can also be degassed to produce a uniform mass without gas inclusions, so that a homogeneous pyrolysis product can be obtained through subsequent pyrolysis.

[0019] Before step (a) of the process, a diluent can be added to the plastic, in particular to the plasticized plastic, to reduce its viscosity. For this purpose, the device can have an introduction device configured to add a diluent to the plastic to reduce its viscosity prior to pyrolysis in the first pyrolysis reactor. The diluent is preferably added to the plastic in an amount of at least 5% by weight, more preferably at least 9% by weight, based on the total weight of the plastic. The ratio of plastic to diluent is preferably at least 1:4, preferably at least 1:9. By adding the diluent to the plastic, the mobility of polymer chains can be increased at a given temperature, so that the heat input into the plastic can be improved during pyrolysis.Furthermore, the risk of overheating of plastic in the wall areas of the pyrolysis reactor can be reduced by reducing the viscosity, as this is usually heated by a heating device located near an outer wall of the pyrolysis reactor. The risk of coking of the plastic during pyrolysis can also be reduced by reducing the viscosity.

[0020] By adding the diluent to the plastic, its viscosity can preferably be reduced by at least 30%, more preferably by at least 50%, particularly preferably by at least 80%, relative to the viscosity of the plastic without diluent under the same measurement conditions, in particular at a temperature in the range of 180 to 240 °C. This can improve the pumpability of the plastic, which can facilitate its processing.

[0021] When the diluent is added, the plastic preferably has a temperature of at least 120 °C, more preferably a temperature of 150 to 300 °C, in particular of 200 to 300 °C. Alternatively or additionally, the diluent can be heated to a temperature of preferably at least 120 °C, more preferably at least 150 °C, in particular to a temperature of 200 to 300 °C before being added to the plastic. By increasing the temperature of the plastic and / or the diluent, the diluent can be mixed into the plastic more quickly and efficiently. The subsequent pyrolysis can also be carried out more quickly and energy-efficiently.

[0022] The diluent can be added to the plastic by means of a adding device. The adding device can have a metering device, such as a metering pump. For example, the plastic, in particular the plasticized plastic, can be fed to a mixer, e.g. a static mixer, and mixed there with the diluent. If the plastic is plasticized in an extruder, the diluent can be added directly in the extruder. For this purpose, the adding device can be arranged, for example, in the compression zone or mixing zone of the extruder.

[0023] The diluent can comprise a hydrocarbon selected from an alkane, a cycloalkane and / or an aromatic. By means of pyrolysis, such a diluent can be converted into a gaseous and / or liquid product which can be at least partially separated from the pyrolysis residue and further utilized. In particular, the diluent can comprise a fraction obtained from crude oil, preferably a heavy oil. The heavy oil can be an oil obtained from petroleum in a petroleum refinery, e.g. a residual oil from a pyrolysis plant. The heavy oil preferably has a proportion of an aromatic hydrocarbon of at least 25% by weight, based on the total weight of the heavy oil.

[0024] Alternatively or additionally, the diluent may comprise a portion of the liquid fraction of the first pyrolysis product and / or a portion of the low-solids fraction. This may enable reuse of the liquid fraction and the low-solids fraction. Preferably, the diluent consists of at least a portion of the liquid fraction of the first pyrolysis product and / or at least a portion of the low-solids fraction. A high degree of recycling can then be achieved.

[0025] The diluent preferably has a boiling point (or a lower end of a boiling range) of at least 300 °C, in particular at least 350 °C. This prevents the diluent from evaporating immediately after the introduction of a mixture of plastic and diluent into the pyrolysis reactor. Instead, evaporation, cleavage, and / or depolymerization of the diluent can only occur with increasing residence time of the mixture in the pyrolysis reactor and the concomitant heating of the mixture. This allows a homogeneous pyrolysis product to be obtained.

[0026] In step (a) of the process, the plastic is pyrolyzed in a first pyrolysis reactor. The first pyrolysis reactor can be a screw reactor, a fluidized bed reactor, a rotary tube reactor, or a coker, preferably a coker.

[0027] In step (a) of the process, the temperature in the first pyrolysis reactor is preferably in the range from 300 to 800 °C, more preferably from 350 to 700 °C. The pressure in the first pyrolysis reactor in step (a) is preferably in the range from 1 to 30 bar, more preferably from 5 to 30 bar, even more preferably from 10 to 25 bar. Furthermore, in step (a), pyrolysis is preferably carried out for a period of 0.3 min, more preferably for a period of 1 to 10 min, in particular 1.5 to 5 min. This allows a good balance between economic viability and process efficiency to be achieved.

[0028] The pyrolysis in step (a) can be thermal pyrolysis (i.e., thermal cracking without the addition of a catalyst) and / or catalytic pyrolysis (i.e., catalytic cracking). Thermal pyrolysis is preferred to avoid any contamination of the wax and / or the solid due to catalyst components.

[0029] The pyrolysis in step (a) can be carried out largely in the absence of oxygen, especially in an inert atmosphere, such as nitrogen. A lack of oxygen or the absence of oxygen can prevent complete combustion and cause a polymer contained in the plastic to be cleaved or depolymerized.

[0030] The first pyrolysis product comprises a pyrolysis residue. Furthermore, the first pyrolysis product comprises a liquid fraction and / or a gaseous fraction. In step (b) of the process, the pyrolysis residue is separated from the first pyrolysis product in a first separation unit. The separation can be carried out by evaporation and / or centrifugal separation (i.e., centrifugation), preferably by centrifugal separation. Accordingly, the first separation unit can comprise an evaporator, a cyclone, and / or a hydrocyclone, in particular a hydrocyclone.

[0031] The temperature in the first separation unit in step (b) is preferably in the range from 300 to 700 °C, more preferably in the range from 330 to 420 °C. The pressure in the first separation unit in step (b) is preferably in the range from 1 to 15 bar, more preferably in the range from 2 to 8 bar. With these process parameters, an efficient and good separation of the pyrolysis residue can be achieved.

[0032] The first separation unit preferably has a hydrocyclone with which the gaseous fraction, the liquid fraction and the pyrolysis residue can be separated from one another in just one process step. Such a hydrocyclone is described in the application WO 2023 / 036751 A1. By introducing the first pyrolysis product via an inlet arranged in an upper region of a jacket of the hydrocyclone, a vortex flow can be generated in the hydrocyclone, as a result of which the gaseous fraction can be separated from the first pyrolysis product and discharged via an outlet arranged in the upper region of the hydrocyclone (e.g. on its ceiling). The remaining part of the first pyrolysis product can then be discharged under gravity towards a base of the hydrocyclone, it being possible for a tangential velocity of a developing vortex flow to increase continuously.As a result, at least part of the pyrolysis residue can be discharged via an outlet arranged in the bottom of the hydrocyclone, while at least part of a liquid fraction of the first pyrolysis product can reach an inner container arranged in the hydrocyclone and from there be discharged via an outlet. This part of the liquid fraction can then be used as a diluent to reduce the viscosity of the plastic before step (a) of the process. The pyrolysis residue discharged via the outlet arranged in the bottom of the hydrocyclone can then be used in step (c) of the process. The hydrocyclone is preferably operated at a temperature in the range from 300 to 450 °C, more preferably from 320 to 420 °C, particularly preferably from 360 to 400 °C.

[0033] The pyrolysis residue separated in step (b) of the process preferably has a boiling point (or a lower end of a boiling range) of at least 250 °C, more preferably at least 300 °C, even more preferably at least 330 °C, particularly preferably at least 350 °C. The boiling point (or boiling range) of the pyrolysis residue can be determined by means of the ASTM D7500-15: 2019 standard (preferably when the pyrolysis residue has a boiling point or boiling range of 100 to 850 °C, in particular 100 to 735 °C) or by means of the ASTM D2887-22: 2022 standard (preferably when the pyrolysis residue has a boiling point or boiling range of 55 to 538 °C).

[0034] The pyrolysis residue separated in step (b) of the process preferably comprises a carbon fraction with at least 14 carbon atoms per molecule, more preferably at least 16 carbon atoms per molecule, and most preferably at least 18 carbon atoms per molecule. The pyrolysis residue can then be readily separated in the subsequent step (c) of the process.

[0035] In step (c) of the process, the pyrolysis residue is separated in a second separation unit into a low-solids fraction and a high-solids fraction. The low-solids fraction preferably has a liquid content of more than 70 wt.%, preferably more than 80 wt.%, more preferably more than 85 wt.%, more preferably more than 90 wt.%, more preferably more than 95 wt.%, more preferably more than 98 wt.%, more preferably more than 99 wt.%. The low-solids fraction preferably has a liquid content in the range of 80 to 100 wt.%, more preferably 90 to 99.9 wt.%, based on the total weight of the low-solids fraction. The low-solids fraction preferably has a density at 20°C and 101325 Pa in the range of 0.600 to 1.100 g / cm 3 preferably 0.750 to 0.990 g / cm 3 .

[0036] The solids-rich fraction preferably has a liquid content of less than 95 wt.%, preferably less than 90 wt.%, more preferably less than 85 wt.%, more preferably less than 80 wt.%, more preferably less than 75 wt.%, more preferably less than 70 wt.%. The solids-rich fraction preferably has a liquid content in the range of 50 to 95 wt.%, more preferably 70 to 90 wt.%, based on the total weight of the solids-rich fraction. The solids-rich fraction preferably has a density at 20°C and 101325 Pa in the range of 0.650 to 1.300 g / cm 3 to , preferably 0 , 800 to 1 , 150 g / cm 3 . Preferably, the solids-rich fraction has a lower liquid content than the solids-poor fraction. It is also preferred if the solids-rich fraction has a higher density at 20 ° C and 101325 Pa than the solids-poor fraction.

[0037] The separation in the second separation unit can comprise gravimetric separation, filtration and / or centrifugal separation, preferably centrifugal separation. The gravimetric separation can comprise sedimentation and / or decanting. Accordingly, the second separation unit can have a device for gravimetric separation, a filter, a centrifuge and / or a hydrocyclone, preferably a hydrocyclone. The device for gravimetric separation can have a sedimentation system and / or a decanter. If the second separation unit comprises a hydrocyclone, this can be constructed and operated in the same or a similar way to the hydrocyclone of the first separation unit, as described above.

[0038] Preferably, the separation in the second separation unit in step (c) comprises centrifugal force separation in combination with filtration or gravimetric separation. The centrifugal force separation can take place before filtration or before gravimetric separation. Accordingly, the second separation unit can have the hydrocyclone in combination with the filter or the device for gravimetric separation. The hydrocyclone can be arranged upstream of the filter or the device for gravimetric separation. In this way, a sharp separation into the low-solids fraction and the high-solids fraction can take place.

[0039] The temperature in the second separation unit in step (c) is preferably in the range of 100 to 700 °C, more preferably 100 to 350 °C, even more preferably 100 to 200 °C. During gravimetric separation or filtration, the temperature is preferably in the range of 180 to 700 °C. During centrifugation, the temperature is preferably 200 °C or below, more preferably in the range of 100 to 180 °C. During centrifugal separation, the temperature is preferably in the range of 200 to 700 °C. If the temperature is selected as indicated depending on the process, the separation into a low-solids fraction and a high-solids fraction can proceed efficiently.

[0040] In step (d) of the process, the solids-rich fraction is pyrolyzed in a second pyrolysis reactor to obtain a second pyrolysis product. The second pyrolysis reactor can be a screw reactor, a fluidized-bed reactor, a rotary tube reactor, or a coker, preferably a coker. The temperature in the second pyrolysis reactor is preferably in the range of 400 to 800 °C, more preferably in the range of 500 to 700 °C. This allows the solids-rich fraction to be efficiently pyrolyzed.

[0041] The temperature during pyrolysis in the second pyrolysis reactor in step (d) may be higher than the temperature during pyrolysis in the first pyrolysis reactor in step (a). The temperature in the second pyrolysis reactor is preferably at least 50°C higher than the temperature in the first pyrolysis reactor, more preferably at least 80°C, even more preferably at least 100°C, even more preferably at least 150°C, especially at least 200°C.

[0042] The pressure in the second pyrolysis reactor is preferably in the range of 1 to 20 bar, more preferably in the range of 2 to 12 bar, in particular 2 to 8 bar. Pyrolysis in the second pyrolysis reactor is preferably carried out for a period of 1 to 90 minutes, in particular 1.5 to 5 minutes. This allows a good balance between economic viability and process efficiency to be achieved.

[0043] The ratio of the volumetric capacity of the first pyrolysis reactor and the second pyrolysis reactor is a maximum of 10:3, more preferably a maximum of 10:2, preferably in the range from 10:0.2 to 10:2, in particular from 10:1 to 10:2. The volumetric capacity is understood to mean the maximum possible filling level of the respective pyrolysis reactor.

[0044] The second pyrolysis product can comprise a solid, a gas, and / or a liquid. The amount of gas is preferably at least 10 wt.%, more preferably at least 20 wt.%, even more preferably at least 40 wt.%, based on the total weight of the second pyrolysis product. The gas preferably comprises a carbon fraction of at least 5 wt.%, more preferably at least 15 wt.%, even more preferably at least 20 wt.%, in particular at least 40 wt.%, based on the total weight of the gas. The carbon fraction of the gas preferably comprises methane, ethane, ethene, propane, propene, butane, butene, butadiene, or a mixture of these components. These components of the gas can be separated from one another, for example by fractional distillation, in order to supply them for further use, for example in other refinery plants.

[0045] The liquid preferably comprises an oil, wherein the oil may comprise a light oil and a heavy oil. The light oil may comprise a carbon fraction of 3 to 14 carbon atoms per molecule, and the heavy oil may comprise a carbon fraction of 11 to 50 carbon atoms per molecule. Separation of individual components of the oil from one another, in particular individual components of the carbon fraction from one another, can be achieved, for example, by fractional distillation, which enables subsequent reuse, for example as fuel. The separation of the gas and the liquid from one another, and the separation of the gas and / or the liquid into individual components, can be achieved in the same distillation apparatus.

[0046] The amount of solid is preferably a maximum of 70 wt%, more preferably a maximum of 55 wt%, even more preferably a maximum of 30 wt%, based on the total weight of the second pyrolysis product. The solid can comprise an inorganic salt, a ceramic raw material, an asphaltene, a tar and / or a coke. In particular, the solid can comprise talc, an iron oxide (e.g. iron (III) oxide), aluminum oxide, titanium dioxide, magnesium oxide and / or calcium carbonate. If the pyrolysis residue provided is obtained by pyrolyzing a plastic, the solid can comprise an additive contained in the plastic. For example, the additive can comprise a filler, a color pigment and / or an additive. A person skilled in the art will know which additives are used depending on the respective plastic and field of application.

[0047] The process may comprise a further step (e): separating at least a portion of the solid from the second pyrolysis product. For this purpose, the device may comprise a solid separation device.

[0048] The separation of the solid from the second pyrolysis product can comprise gravimetric separation, filtration and / or centrifugal separation, preferably filtration. The gravimetric separation can comprise sedimentation and / or decantation. If the separation comprises filtration, this can be carried out using a filter medium, which can comprise activated carbon or bleaching earth. This allows any polar components dissolved together with the wax in the solvent (e.g., a tar or a polyphenol) to be separated and adsorbed by the filter medium. During filtration, even particles with an average particle size (D50) of less than 100 pm, in particular less than 50 pm, can be easily removed (determined by laser diffraction).

[0049] The separation of the solid from the second pyrolysis product can also take place directly in the second pyrolysis reactor. The second pyrolysis reactor is preferably a screw reactor for this purpose. The solid can be discharged directly from the extruder using a discharge device.

[0050] After being separated from the second pyrolysis product, i.e., after step (e) of the process, the solid can be dried, for example in an oven. This makes the solid free-flowing and thus easier to process. The solid is preferably dried at a temperature in the range from 50 to 250°C, more preferably from 100 to 200°C, even more preferably from 130 to 160°C. The drying time is preferably up to 120 minutes, in particular from 5 to 60 minutes. One or more components can be separated from the solid, in particular from the dried solid, and then reused, e.g., as an additive for a plastic.

[0051] The invention particularly relates to the following embodiments:

[0052] 1. A process for the pyrolysis of a plastic, in particular a waste plastic, comprising the steps

[0053] (a) pyrolyzing the plastic in a first pyrolysis reactor to obtain a first pyrolysis product,

[0054] (b) separating a pyrolysis residue from the first pyrolysis product in a first separation unit,

[0055] (c) separating the pyrolysis residue into a low-solids fraction and a high-solids fraction in a second separation unit, and

[0056] (d) pyrolyzing the solids-rich fraction in a second pyrolysis reactor to obtain a second pyrolysis product.

[0057] 2. Method according to embodiment 1, wherein the plastic comprises a polyolefin and / or a polystyrene (PS), wherein the polyolefin preferably comprises a polyethylene (PE) and / or a polypropylene (PP).

[0058] 3. The method according to embodiment 2, wherein the plastic comprises the polyolefin and / or the polystyrene in an amount of at least 65 wt%, more preferably at least 70 wt%, in particular at least 90 wt%, based on the total weight of the plastic.

[0059] 4. Process according to embodiment 2 or 3, wherein the plastic comprises at least 20 wt% of a polyolefin, preferably at least 50 wt%, more preferably at least 70 wt%, in particular at least 90 wt%, based on the total weight of the plastic.

[0060] 5. Process according to one of the preceding embodiments, wherein the plastic is heated to a temperature of at least 120 °C, preferably to a temperature of 200 to 500 °C, more preferably 400 to 470 °C, before step (a).

[0061] 6. Process according to one of the preceding embodiments, wherein a diluent is added to the plastic before step (a) to reduce the viscosity.

[0062] 7. The process according to embodiment 6, wherein the diluent is added to the plastic in an amount of at least 5 wt%, more preferably at least 9 wt%, based on the total weight of the plastic.

[0063] 8. Process according to embodiment 6 or 7, wherein the ratio of plastic to diluent is at least 1:4, preferably at least 1:9.

[0064] 9. The process according to any one of embodiments 6 to 8, wherein the diluent comprises a hydrocarbon selected from an alkane, a cycloalkane and / or an aromatic.

[0065] 10. Process according to one of embodiments 6 to 9, wherein the diluent comprises a fraction obtained from crude oil, preferably a heavy oil, in particular a heavy oil with a proportion of an aromatic hydrocarbon of at least 25% by weight, based on the total weight of the heavy oil.

[0066] 11. The process according to any one of embodiments 6 to 10, wherein the diluent comprises a portion of the liquid fraction of the first pyrolysis product and / or a portion of the solids-free fraction.

[0067] 12. The process according to any one of embodiments 6 to 11, wherein the diluent has a boiling temperature of at least 300 °C, preferably at least 350 °C.

[0068] 13. A process according to any one of embodiments 6 to 12, wherein the diluent and / or the plastic is / are heated to a temperature of at least 120°C, preferably at least 150°C, before the diluent is added to the plastic, preferably to a temperature in the range of 150 to 300°C, more preferably 200 to 300°C.

[0069] 14. Process according to one of the preceding embodiments, wherein the temperature in the first pyrolysis reactor in step (a) is in the range from 300 to 800 °C, preferably from 350 to 700 °C.

[0070] 15. Process according to any one of the preceding embodiments, wherein the pressure in the first pyrolysis reactor in step (a) is in the range from 1 to 30 bar, preferably from 5 to 30 bar, more preferably 10 to 25 bar.

[0071] 16. Process according to one of the preceding embodiments, wherein in step (a) pyrolysis is carried out for a period of at least 0.3 min, preferably for a period of 1 to 10 min, in particular from 1.5 to 5 min.

[0072] 17. Method according to one of the preceding embodiments, wherein the separation in the first separation unit in step (b) comprises evaporation and / or centrifugal separation, preferably centrifugal separation.

[0073] 18. Process according to one of the preceding embodiments, wherein the temperature in the first separation unit in step (b) is in the range from 300 to 700 °C, preferably from 330 to 420 °C.

[0074] 19. Process according to one of the preceding embodiments, wherein the pressure in the first separation unit in step (b) is in the range from 1 to 15 bar, preferably from 2 to 8 bar.

[0075] 20. Process according to one of the preceding embodiments, wherein the pyrolysis residue separated in step (b) has a boiling temperature of at least 250 °C, preferably at least 300 °C, more preferably at least 330 °C, particularly preferably at least 350 °C.

[0076] 21. Process according to one of the preceding embodiments, wherein the pyrolysis residue separated in step (b) comprises a carbon fraction having at least 14 carbon atoms per molecule, preferably at least 16 carbon atoms per molecule, particularly preferably at least 18 carbon atoms per molecule.

[0077] 22. Process according to one of the preceding embodiments, wherein the solids-free fraction has a liquid content of more than 70 wt.%, preferably more than 80 wt.%, more preferably more than 85 wt.%, more preferably more than 90 wt.%, more preferably more than 95 wt.%, more preferably more than 98 wt.%, more preferably more than 99 wt.%.

[0078] 23. Process according to any one of the preceding embodiments, wherein the solids-rich fraction has a liquid content of less than 95 wt.%, preferably less than 90 wt.%, more preferably less than 85 wt.%, more preferably less than 80 wt.%, more preferably less than 75 wt.%, more preferably less than 70 wt.%.

[0079] 24. Process according to one of the preceding embodiments, wherein the low-solids fraction has a liquid content in the range of 80 to 100 wt%, preferably 90 to 99.9 wt%, based on the total weight of the low-solids fraction; and / or wherein the high-solids fraction has a liquid content in the range of 50 to 95 wt%, preferably 70 to 90 wt%, based on the total weight of the high-solids fraction.

[0080] 25. A process according to any one of the preceding embodiments, wherein the solids-free fraction has a density at 20 °C and 101325 Pa in the range of 0.600 to 1.100 g / cm 3 preferably from 0.750 to 0.990 g / cm 3 , based on the total weight of the solids-rich fraction; and / or wherein the solids-rich fraction has a density at 20 °C and 101325 Pa in the range of 0.650 to 1.300 g / cm 3 preferably from 0.800 to 1.150 g / cm 3 , based on the total weight of the solids-rich fraction.

[0081] 26. Process according to any one of the preceding embodiments, wherein the temperature in the second separation unit in step (c) is in the range from 100 to 700 °C, preferably from 100 to 350 °C, more preferably 100 to 200 °C.

[0082] 27. Method according to one of the preceding embodiments, wherein the separation in the second separation unit in step (c) comprises a gravimetric separation, a filtration and / or a centrifugal separation, preferably a centrifugal separation.

[0083] 28. The method according to embodiment 27, wherein the separation in the second separation unit in step (c) comprises centrifugal separation in combination with filtration or gravimetric separation.

[0084] 29. The method according to embodiment 27, wherein the centrifugal separation takes place before the filtration or before the gravimetric separation.

[0085] 30. The process according to any one of embodiments 27 to 29, wherein the temperature during gravimetric separation or filtration is in the range of 180 to 700°C; wherein the temperature during centrifugation is 200°C or below, more preferably in the range of 100 to 180°C; and / or wherein the temperature during centrifugal separation is in the range of 200 to 700°C.

[0086] 31. The process according to any one of the preceding embodiments, wherein the temperature in the second pyrolysis reactor in step (d) is in the range from 400 to 800 °C, preferably in the range from 500 to 700 °C. 32. The process according to any one of the preceding embodiments, wherein the temperature during pyrolysis in the second pyrolysis reactor in step (d) is higher than the temperature during pyrolysis in the first pyrolysis reactor in step (a).

[0087] 33. The process according to embodiment 32, wherein the temperature in the second pyrolysis reactor is at least 50°C higher than the temperature in the first pyrolysis reactor, preferably at least 80°C, more preferably at least 100°C, even more preferably at least 150°C, in particular at least 200°C.

[0088] 34. Process according to any one of the preceding embodiments, wherein the pressure in the second pyrolysis reactor in step (d) is in the range from 1 to 20 bar, preferably from 2 to 12 bar, more preferably from 2 to 8 bar.

[0089] 35. Process according to one of the preceding embodiments, wherein in step (d) pyrolysis is carried out for a period of 1 to 90 minutes, preferably from 1.5 to 5 minutes.

[0090] 36. The process according to any one of the preceding embodiments, wherein a ratio of the volumetric capacity of the first pyrolysis reactor and the second pyrolysis reactor is at most 10:3, preferably in the range from 10:0.2 to 10:2, more preferably from 10:1 to 10:2.

[0091] 37. The method according to any one of the preceding embodiments, wherein the second pyrolysis product comprises a solid, a gas and / or a liquid.

[0092] 38. The process according to embodiment 37, wherein the amount of gas is at least 10 wt%, preferably at least 20 wt%, more preferably at least 40 wt%, based on the total weight of the second pyrolysis product.

[0093] 39. A process according to embodiment 37 or 38, wherein the gas comprises a proportion of a carbon fraction of at least 5 wt%, preferably at least 15 wt%, more preferably at least

[0094] 20% by weight, in particular at least 40% by weight, based on the total weight of the gas.

[0095] 40. The process according to embodiment 39, wherein the carbon fraction comprises methane, ethane, ethene, propane, propene, butane, butene, butadiene or a mixture of these components.

[0096] 41. The method according to any one of embodiments 37 to 40, wherein the liquid comprises an oil, wherein the oil preferably comprises a light oil and a heavy oil.

[0097] 42. The process according to embodiment 41, wherein the light oil preferably comprises a carbon fraction of 3 to 14 carbon atoms per molecule, and / or wherein the heavy oil preferably comprises a carbon fraction of 11 to 50 carbon atoms per molecule.

[0098] 43. Process according to any one of embodiments 37 to 42, wherein the amount of solid is at most 70 wt%, preferably at most 55 wt%, more preferably at most 30 wt%, based on the total weight of the second pyrolysis product.

[0099] 44. The method according to any one of embodiments 37 to 43, wherein the solid comprises an inorganic salt, a ceramic raw material, an asphaltene, a tar and / or a coke.

[0100] 45. The process according to any one of embodiments 37 to 44, further comprising step (e): separating at least a portion of the solid from the second pyrolysis product.

[0101] 46. ​​The method according to embodiment 45, wherein the separation in step (e) comprises a gravimetric separation, a filtration and / or a centrifugal separation, preferably a filtration.

[0102] 47. The method according to embodiment 46, wherein the filtration comprises separation with a filter medium containing activated carbon or bleaching earth.

[0103] 48. A process according to any one of embodiments 45 to 47, wherein the solid is dried after step (e), preferably at a temperature in the range of 50 to 250°C, more preferably 100 to 200°C, in particular 130 to 160°C; and / or for a period of up to 120 minutes, preferably 5 to

[0104] 60 min.

[0105] 49. The process according to any one of embodiments 37 to 48, wherein the gas and / or the liquid are separated from one another by means of fractional distillation.

[0106] 50. The process according to embodiment 49, wherein the gas and / or the liquid are separated into individual components by fractional distillation.

[0107] 51. Apparatus for pyrolyzing a plastic, in particular a waste plastic, with a method according to one of embodiments 1 to 50, comprising a first pyrolysis reactor for pyrolyzing the plastic, a first separation unit for separating the pyrolysis residue from the first pyrolysis product, a second separation unit for separating the pyrolysis residue into the low-solids fraction and the high-solids fraction, and a second pyrolysis reactor for pyrolyzing the high-solids fraction.

[0108] 52. Apparatus according to embodiment 50, further comprising an addition device for adding a diluent to the plastic prior to pyrolysis in the first pyrolysis reactor.

[0109] 53. Device according to embodiment 50 or 52, wherein the first pyrolysis reactor and / or the second pyrolysis reactor is / are a screw reactor, a fluidized bed reactor, a rotary tube reactor or a coker, preferably a coker.

[0110] 54. Device according to one of the embodiments 51 to 53, wherein the first separation unit comprises an evaporator, a cyclone and / or a hydrocyclone, in particular a hydrocyclone.

[0111] 55. Device according to one of the embodiments 51 to 54, wherein the second separation unit comprises a device for gravimetric separation, a filter, a centrifuge and / or a hydrocyclone, preferably a hydrocyclone.

[0112] 56 . Device according to embodiment 55 , wherein the second separation unit comprises the hydrocyclone in combination with the filter or the device for gravimetric separation, wherein the hydrocyclone is preferably arranged upstream of the filter or the device for gravimetric separation.

[0113] 57. Device according to one of the embodiments 51 to 56, further comprising a solid separation device for separating at least a portion of a solid from the second pyrolysis product.

[0114] 58. Device according to one of the embodiments 51 to 57, further comprising a distillation apparatus for separating a gas and / or a liquid from the second pyrolysis product.

[0115] The invention is further explained below with reference to figure descriptions of some embodiments, to which, however, the invention is not limited.

[0116] Fig. 1 shows a flow diagram of a process for the pyrolysis of a plastic.

[0117] As can be seen from Fig. 1, a plastic comprising at least 50 wt.% of a polyolefin is fed to an extruder 1, in which the plastic is plasticized and degassed. The plasticized plastic has a temperature of at least 120°C and is then added to a static mixer 2. In the static mixer 2, a diluent 3 can be added to the plasticized plastic in order to reduce its viscosity. Alternatively or in addition to the diluent 3, a portion of a liquid fraction 4 separated from the first pyrolysis product 6 can be mixed with the plasticized plastic in order to reduce its viscosity. The resulting mixture is then fed to a first pyrolysis reactor 5, in which the plastic is pyrolyzed at a temperature of 350 to 700°C. This produces a first pyrolysis product 6 comprising a gaseous fraction, a liquid fraction, and a pyrolysis residue.The first pyrolysis product 6 is fed to a first separation unit 7, which is connected downstream of the first pyrolysis reactor 5 and has a hydrocyclone. First, the gaseous fraction is at least partially separated in the hydrocyclone. The separated part of the gaseous fraction 8 can then be further separated into a light oil (e.g. with a boiling range of 35 to 225 °C) and a heavy oil (e.g. with a boiling range of 225 to 410 °C) (not shown). Furthermore, the liquid fraction is at least partially separated in the hydrocyclone. The separated part of the liquid fraction 4 can be discharged via an outlet 9 of the hydrocyclone and reused in the process for reducing the viscosity of the plastic, as described above. At least a portion of the pyrolysis residue, which at least partially comprises the pyrolysis residue, is discharged via an outlet 10 arranged in the base of the hydrocyclone.

[0118] As can also be seen in Fig. 1, the pyrolysis residue discharged via the outlet 10 is fed to a second separation unit 11, which has a hydrocyclone 12 and a filter 13, where it is separated into a low-solids fraction 14 and a high-solids fraction 15. The low-solids fraction has a liquid content in the range of 80 to 100 wt%, based on the total weight of the low-solids fraction, and the high-solids fraction has a liquid content in the range of 50 to 95 wt%, based on the total weight of the high-solids fraction. The low-solids fraction 14 can be reused in the process by adding at least a portion of the low-solids fraction 14 to the plasticized plastic in the mixer 2 to reduce the viscosity.The solids-rich fraction 15 is then pyrolyzed in a second pyrolysis reactor 16 at a temperature in the range from 500 to 700 °C, the temperature in the second pyrolysis reactor 16 being at least 80 °C higher than in the first pyrolysis reactor 5, in order to obtain a second pyrolysis product 17. By means of a solids separation device 18 which has a filter, at least a portion of the solid is separated from the second pyrolysis product 17. A filter medium of the filter comprises activated carbon. The separated portion of the solid 19 is dried in an oven 20 at a temperature of 100 to 200 °C. Individual components can then be separated from the solid and reused (not shown). The remaining part of the second pyrolysis product is separated in a distillation apparatus 21 by means of fractional distillation into a gas 22 and a liquid 23.can also be separated into one or more components of a gas and / or one or more components of a liquid.

Claims

Patent claims:

1. A process for the pyrolysis of a plastic, in particular a waste plastic, comprising the steps (a) pyrolyzing the plastic in a first pyrolysis reactor to obtain a first pyrolysis product, (b) separating a pyrolysis residue from the first pyrolysis product in a first separation unit, (c) separating the pyrolysis residue into a low-solids fraction and a high-solids fraction in a second separation unit, and (d) pyrolyzing the solids-rich fraction in a second pyrolysis reactor to obtain a second pyrolysis product.

2. The process according to claim 1, wherein the pyrolysis residue separated in step (b) has a boiling temperature of at least 250 °C.

3. The process according to claim 1 or 2, wherein the low-solids fraction has a liquid content in the range of 80 to 100 wt.%, based on the total weight of the low-solids fraction; and / or wherein the high-solids fraction has a liquid content in the range of 50 to 95 wt.%, based on the total weight of the high-solids fraction.

4. The method according to any one of claims 1 to 3, wherein the separation in the second separation unit in step (c) comprises centrifugal separation.

5. The method according to claim 4, wherein the separation in the second separation unit in step (c) comprises centrifugal separation in combination with filtration or gravimetric separation.

6. The method according to any one of claims 1 to 5, wherein a ratio of the volumetric capacity of the first pyrolysis reactor and the second pyrolysis reactor is at most 10:

3.

7. The process according to any one of claims 1 to 6, wherein the second pyrolysis product comprises a solid, a gas and / or a liquid.

8. The process of claim 7, wherein the gas comprises a proportion of a carbon fraction of at least 20% by weight, based on the total weight of the gas.

9. The process according to claim 7 or 8, wherein the amount of solid is at most 70% by weight, based on the total weight of the second pyrolysis product.

10. The process according to any one of claims 1 to 9, further comprising step (e): separating at least a portion of the solid from the second pyrolysis product.

11. The method according to claim 10, wherein the separation in step (e) comprises filtration, preferably with a filter medium containing activated carbon or bleaching earth.

12. Device for the pyrolysis of a plastic, in particular a waste plastic, with the method according to one of claims 1 to 11, comprising a first pyrolysis reactor (5) for pyrolyzing the plastic, a first separation unit (7) for separating the pyrolysis residue from the first pyrolysis product, a second separation unit (11) for separating the pyrolysis residue into the low-solids fraction and the high-solids fraction, and a second pyrolysis reactor (16) for pyrolyzing the solids-rich fraction.

13. Device according to claim 12, wherein the second separation unit (11) has a hydrocyclone (12).

14. Device according to claim 13, wherein the second separation unit (11) comprises the hydrocyclone (12) in combination with a filter (13) or a device for gravimetric separation.

15. Device according to one of claims 12 to 14, further comprising a solid separation device (18) for separating at least a part of a solid from the second pyrolysis product.