Adhesive paste@ground tobacco ash composite material, preparation thereof, and uses thereof in novel tobacco product and tobacco sheet

MYPI2025006152A0Undetermined Publication Date: 2025-04-27CHINA TOBACCO HUNAN IND CORP
View PDF 0 Cites 0 Cited by

Patent Information

Application Number
MYPI2025006152
Authority / Receiving Office
MY · MY
Patent Type
Applications
Current Assignee / Owner
Priority Date
2023-10-27
Filing Date
2024-08-28
Publication Date
2025-04-27

AI Technical Summary

Technical Problem

Existing heated cigarette sheets are prone to moisture absorption during production and storage, resulting in macular, quality problems and difficult processing in high humidity environments.

Method used

The preparation method of sticky paste and soot composite material is adopted. The atomizer and inorganic material are coated in the sticky paste through a three-stage coating process and mixed with the soot to form a hydrophobic sticky paste and soot composite material to reduce the moisture absorption rate and improve the uniformity of the atomizer release.

Benefits of technology

It realizes the reduction of the moisture absorption rate of the flakes in a high humidity environment, prevents macular and quality problems, and improves the uniform release and suction taste of the atomizer.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure PI2025006152_DRAWING_001
    Figure PI2025006152_DRAWING_001
  • Figure PI2025006152_DRAWING_002
    Figure PI2025006152_DRAWING_002
  • Figure PI2025006152_DRAWING_003
    Figure PI2025006152_DRAWING_003
Patent Text Reader

Abstract

The present application relates to the field of preparation of novel tobacco sheets, and in particular to a preparation method for an adhesive paste @ ground tobacco ash composite material. The preparation method comprises: performing first-stage coating on a vaporizing agent and an inorganic material in an adhesive paste preparation tank to prepare an adhesive paste; then mixing the adhesive paste with a hydrophobic agent, so as to achieve second-stage coating, and then performing third-stage coating on the adhesive paste obtained by the second-stage coating and ground tobacco ash in a trough mixer to prepare the adhesive paste @ ground tobacco ash composite material. The present application further comprises the composite material prepared by means of the preparation method, and uses of the composite material in a novel tobacco and a tobacco sheet. In the present application, the preparation method can effectively mitigate the problem of moisture absorption of the sheet, and can promote the uniform and effective release of the vaporizing agent. Figure 1
Need to check novelty before this filing date? Find Prior Art

Description

Adhesive paste@ash composite material and its preparation and application in new tobacco products and its sheets

[0001] This application claims priority to Chinese patent application number 2023114095167, publication number CN118020990A, and entitled “Adhesive paste@ash composite material, its preparation and application in new tobacco products and their sheets” filed on October 27, 2023, the entire text of which is hereby incorporated by reference. Technical Field

[0002] The present application relates to the field of novel tobacco technology, and in particular to the field of thin sheet technology for novel tobacco products. Background Art

[0003] With the development of society, people are paying more and more attention to their health. A product that reduces the harm of cigarettes - heated cigarettes has emerged. However, in order to make this product meet consumers' requirements for smoke volume and improve consumers' experience, it is usually adopted to add 5-20% by weight of glycerin, propylene glycol and other smoking agents directly to the surface of tobacco cuts and stems, or add them to the viscose of reconstituted tobacco leaves by thick pulp method, rolling method or extrusion molding method, or spray them on the surface of dry reconstituted tobacco leaves, or coat them on the sheet base of reconstituted tobacco leaves by papermaking method. The smoking materials of heated cigarettes manufactured by the above methods have the following disadvantages: due to the large amount of smoking agent used, a large amount of smoking agent will remain on the surface of the carrier. Because the smoke-generating agent is a highly hygroscopic material, the smoke-generating material manufactured using the above method is prone to moisture absorption, resulting in quality problems such as clumping, material blockage, and water-soaked lumps during the silk-making process. During the cigarette-rolling process, the cigarette-rolling machine gun may be blocked, resulting in poor rolling, and quality defects such as nozzle twisting, air leakage, low cigarette hardness, and wrinkled cigarettes. During the packaging and storage stages, quality problems such as moisture absorption, yellow spots, and mildew may occur. During the consumer's inhalation process, the amount of smoke per puff may be uneven, the smoke temperature may increase, the cigarette may become soft due to moisture absorption, and the cigarette may become yellow spots. At the same time, the subsequent processing of the smoke-generating material manufactured using the above method requires the humidity of the processing environment to be controlled at no more than 42%. In such an environment, not only huge energy consumption is incurred, but also producers may feel uncomfortable.

[0004] In response to the problem of yellow spots caused by moisture absorption in tobacco slices, a Chinese patent document with publication number CN111165870A discloses a long-shelf-life, low-hazard smoke-enhancing cigarette, including cigarette paper, a filter tip, and an aerosol-generating matrix. The aerosol-generating matrix includes tobacco slices treated with smoke enhancement and / or tobacco shreds treated with smoke enhancement. The tobacco slice raw materials for manufacturing tobacco slices treated with smoke enhancement include traditional tobacco slice slurry and a smoke enhancer. The tobacco shreds treated with smoke enhancement include traditional tobacco shreds and a smoke enhancer. The smoke enhancer has low deliquescent properties, which fundamentally solves the problem that cigarettes with a large amount of atomizer added are prone to moisture absorption and thus produce yellow spots. While improving the smoking effect of cigarettes, it also tries to extend the shelf life of cigarettes. A Chinese patent document with publication number CN112493528A discloses a composite functional tobacco slice, which has a core-shell structure, wherein the core is a tobacco slice, and the shell is a compound having the structural formula 1. At least one barrier functional material; said n is an integer not less than 2.

[0005] Although traditional technical solutions provide some moisture-proof ideas for different thin sheets, the moisture absorption rate of traditional technical solutions during the production of heated cigarettes using heated cigarette sheets is too fast, making it difficult to successfully process them into qualified heated cigarettes under environmental humidity conditions greater than 45% to 70%. It is also difficult to solve problems such as yellow spots and mildew that may occur during the storage of heated cigarettes. In addition, traditional technical solutions find it difficult to balance the effects of moisture-proofing and uniform release of atomizers.

[0006] The above information disclosed in the background of this application is only used to understand the background of the concept of this application, and may contain information that does not constitute a traditional technical solution.

[0007] Summary of the Invention

[0008] In view of the common problems of existing thin slices, especially thick slurry method thin slices, such as easy moisture absorption, yellow spots, uneven smoke release, unsatisfactory smoking taste, low humidity required during the thin slice preparation stage, and easy blockage and shutdown of equipment, the first purpose of this application is to provide a preparation method of a viscous paste@ash composite material, aiming to provide a viscous paste@ash composite material with many advantages such as high loading rate, low moisture absorption, uniform atomization, rich smoking flavor, and the ability to be assembled into tobacco products under ambient humidity.

[0009] The second object of the present application is to provide a paste@soot composite material prepared by the preparation method and its application in the preparation of thin sheets, especially thick slurry thin sheets.

[0010] The third object of the present application is to provide a thick pulp sheet and a new tobacco product comprising the adhesive paste@ash composite material.

[0011] The preparation process of existing heated cigarette sheets inevitably uses more than 5-20% atomizer, which has good hygroscopicity and easily leads to moisture absorption and yellow spots during the production and storage processes. In particular, for thick slurry method sheets, a large amount of solvent water needs to be introduced during the production process, which will increase the difficulty of subsequent moisture-proofing to a certain extent. In addition, in order to circumvent the moisture absorption problem of the atomizer, there are some encapsulation methods in the existing technology. However, these methods are difficult to avoid affecting the release of the atomizer while achieving the moisture-proof effect, making it difficult to take into account both moisture absorption and atomizer release effects. In response to the above problems, this application provides the following solutions:

[0012] A method for preparing a viscous paste@soot composite material comprises: performing a first coating step on an atomizer and an inorganic material in a viscous paste preparation tank to produce a viscous paste; then mixing the viscous paste with a hydrophobic agent to produce a second coating step; and then performing a third coating step on the second coated viscous paste and soot in a tank mixer to produce the viscous paste@soot composite material.

[0013] The inorganic material is a material having at least one pore structure of nanopores, mesopores and macropores, and its D50 particle size is 50 meshes to 300 meshes. The D50 particle size of the soot is 100 meshes to 300 meshes.

[0014] Existing heated cigarette smoking materials that add a large proportion of atomizers require cigarette processing under low-humidity conditions, which requires relatively high costs and is difficult to truly and effectively solve problems such as moisture resistance and yellow spot prevention. To address the technical difficulties faced by this approach, the present application innovatively uses a paste preparation tank to pre-coat the atomizer and inorganic material in a first stage, and then uses a hydrophobic agent to coat the surface of the first-coated paste and the openings of the inorganic material to form a hydrophobic paste. A trough mixer is then used to coat and seal the ash on the surface of the hydrophobic paste. Furthermore, combined with the three-stage coating concept, structure, and particle size control, this allows the atomizer to effectively fill the inorganic material in a water-free environment and the ash to efficiently block the pore structure on the paste surface. This reduces the replacement rate of the atomizer water in the coating material during the thick slurry preparation process, reduces the moisture absorption rate of the finished thin sheet, improves the atomization uniformity of the heated cigarette prepared using the materials of the present application, and improves the stable release of flavor substances, thereby improving the smoking taste. In addition, the heated cigarette core (smoking material) prepared using the present application has loose requirements on the cigarette rolling and storage environment, which can be relaxed to a humidity level not higher than 65%.

[0015] In the present application, the adhesive paste preparation tank, the tank mixer equipment, the coating concept, and the combined control of particle size, modification of the inorganic porous material, and the hydrophobic agent are the key to synergistically achieving coating, reducing the replacement rate of the atomizer and water in the wrapping material, reducing the moisture absorption rate of the sheet, improving the atomization uniformity of the heated cigarette prepared using the materials of the present application, and effectively releasing the flavor substances, thereby improving the puffing taste and other effects.

[0016] In one embodiment, the atomizer can be a component applicable to new tobacco known in the industry, for example, a substance that can emit smoke at a temperature of 150 to 250° C.; including but not limited to at least one of glycerol, propylene glycol, polyols, esters, and sugar compounds.

[0017] In one embodiment, the inorganic material is at least one of activated carbon, diatomaceous earth, sepiolite, zeolite, silica, vermiculite, foamed aluminum, foamed nickel, foamed carbon, porous silicon carbide, porous ceramics, carbon molecular sieve, and zeolite molecular sieve.

[0018] In one embodiment, the inorganic material comprises a mixture of diatomaceous earth and vermiculite and a modified mixture thereof;

[0019] In one embodiment, the weight ratio of diatomaceous earth to vermiculite in the mixture is 50-80:20-50;

[0020] In one embodiment, the modified mixture is a product obtained by mixing the mixture (comprising a mixture of diatomaceous earth and vermiculite) with a pore-forming agent and then subjecting the mixture to a gradient calcination treatment.

[0021] In one embodiment, the pore-forming agent includes but is not limited to at least one of CMC, glucose solution, proline and starch.

[0022] In one embodiment, the gradient calcination treatment stage includes two heat treatment platforms, wherein the temperature of the first heat treatment platform is 150-300°C, and the temperature of the second heat treatment platform is 900-1100°C.

[0023] In the present application, the first heat treatment stage may last for 30 to 120 minutes, and the second heat treatment stage may last for 30 to 90 minutes.

[0024] The research of this application found that the innovative use of the combined inorganic material, further combined with the pretreatment of the special temperature control mechanism, can unexpectedly achieve synergy and give the material an atomizer-adaptive interface. Not only that, it is also conducive to the construction of a special hierarchical pore structure. More importantly, the combination of the combined inorganic material and the modification process can unexpectedly induce the atomizer to penetrate into the pore structure, improve its stability and loading capacity, and reduce its moisture absorption rate, yellow spots and other problems.

[0025] In one embodiment, the porosity of the inorganic material is greater than 10%, and may further be 50-90%.

[0026] In one embodiment, the weight ratio of the atomizer to the inorganic material is 0.1 to 0.5:1, and can further be 0.3 to 0.4:1.

[0027] In one embodiment, the first coating period is more than 10 minutes, and considering the processing efficiency, it can be further extended to 10 to 120 minutes.

[0028] In one embodiment, the first coating stage is performed under positive pressure.

[0029] In one embodiment, the positive pressure is above 1.1 atm, preferably above 1.5 atm (the atm refers to standard atmospheric pressure).

[0030] In one embodiment, the paste preparation tank includes a tank body (1), wherein a frame-type scraping and stirring device is provided in the tank body, wherein the frame-type scraping and stirring device includes a rotating shaft (3) and a rotating frame body (4), wherein an axial hole is provided on the top of the rotating frame body, wherein the rotating shaft (3) passes through the axial hole and is rotatably connected to the rotating frame body (4), wherein a plurality of stirring rods (5) are radially mounted on the rotating shaft, wherein a plurality of stirring rods (5) are provided on the inner side of the rotating frame body, wherein a plurality of stirring scrapers (2) are provided on the outer side of the rotating frame body (4), and further comprising a first motor (6), a second motor (12) and a main controller (13), wherein the output end of the first motor is connected to the rotating shaft, and the output end of the second motor is connected to the rotating frame body via a bevel gear, wherein the tank body is provided with a temperature control device (9), and the first motor, the second motor and the temperature control device are all electrically connected to the main controller.

[0031] In this application, an innovative method is adopted to prepare a can using a sticky paste so that the atomizer can penetrate and fill the pore structure of the inorganic material. This can solve the problems of difficulty in filling and poor filling stability caused by the poor interface compatibility between the atomizer and the inorganic material, thereby helping to improve the moisture resistance of the composite material and the release effect and uniformity of the atomizer.

[0032] In one embodiment, in the paste preparation tank, the temperature control device (9) includes an insulating shell and a hot water pipeline arranged in the insulating shell, and temperature sensors are provided in the insulating shell and the tank body (1), and the temperature sensors are electrically connected to the main controller.

[0033] In one embodiment, the bottom end of the rotating shaft is fixedly connected to a dispersion rotating disk (7), and the dispersion rotating disk has a plurality of teeth alternately distributed up and down around it.

[0034] In one embodiment, the tank body has a cover (8), and the cover (8) is also fixedly connected with a sight light and a vacuum sight glass with a scraper, a CIP cleaning head and a vacuum pressure gauge.

[0035] In one embodiment, a lifting platform is further included, wherein the bottom of the lifting platform (10) is connected to an electric push rod (11), the electric push rod is electrically connected to the main controller, the motor is fixedly connected to the lifting platform, and the cover is fixedly connected to the lifting platform; when the lifting platform is raised or lowered, the motor, the frame-type scraping and stirring device and the cover are raised or lowered together with the lifting platform.

[0036] In one embodiment, the tank body (1) is a three-layer structure, and the material of the innermost layer of the tank body is stainless steel.

[0037] In one embodiment, the innermost layer of the tank body (1) is mirror-polished.

[0038] In the present application, the adhesive paste coated in the first stage is coated in the second stage with a hydrophobic agent, wherein the hydrophobic agent is at least one of glycidyl methacrylate and organopolysiloxane.

[0039] In one embodiment, the weight ratio of the adhesive paste to the hydrophobic agent is 1:0.1-0.8. Considering the cost and effect, the weight ratio can be further 1:0.1-0.3, and further 1:0.15-0.25.

[0040] In one embodiment, after the second coating, the material is combined with soot to perform the third coating.

[0041] In one embodiment, the particle size of the soot is 200-500 mesh, which is conducive to the sealing of the adhesive surface when combined with the process and equipment.

[0042] In one embodiment, the raw materials in the ash at least include tobacco raw materials, and the tobacco raw materials include at least one of tobacco leaves, tobacco stems, fragments, and tobacco dust.

[0043] In one embodiment, the raw materials in the ash further include auxiliary plant ingredients, which preferably include but are not limited to at least one of tea leaves, clove leaves, mint leaves, and roses.

[0044] In one embodiment, the soot is obtained by crushing and grinding the raw materials at a temperature below 50°C.

[0045] In one embodiment, the ash is transported by air conveying or conveyed by belt or screw.

[0046] In one embodiment, the weight ratio of the second coating paste to the soot is 1:1-20, and can further be 1:4-6.

[0047] In one embodiment, the tank mixer includes a base (14), a first motor (15), a fixed column (24) and a second motor are fixedly connected to the base (14), the output end of the first motor (15) is connected to a stirring rod (19), the stirring rod (19) is rotatably connected to a mixing tank body (22), the stirring rod (19) is provided with a stirring blade on the shaft section in the mixing tank body (22), the other end of the stirring rod (19) is rotatably connected to the fixed column (24), one side of the mixing tank body (22) is fixedly connected to a first gear (25), the output end of the second motor is connected to a second gear (26), the first gear (25) and the second gear (26) are transmission-connected, and at least one feeding pipe (29) is provided on the inner top of the mixing tank body, the feeding pipe is provided with a plurality of feeding holes, and the adhesive paste enters the mixing tank body (22) through the feeding holes.

[0048] In one embodiment, the soot is used to coat the surface of the paste with the aid of the trough mixer, thereby improving the surface pore blocking effect and making it a material that is conducive to the preparation of thick slurry sheets.

[0049] In one embodiment, in the tank mixer, the first motor (15) and the stirring rod (19) are connected via a first reducer (16).

[0050] In one embodiment, the second motor is connected to the second gear (26) via a second reducer (27);

[0051] In one embodiment, through holes for the stirring rod (19) to pass through are provided at both ends of the mixing tank body (22), a bearing seat (17) is fixedly connected to the through hole, a bearing is matched and installed in the bearing seat (17), and the stirring rod (19) is rotatably installed through the bearing.

[0052] In one embodiment, a top cover (21) is provided at the open top of the mixing tank body (22).

[0053] In one embodiment, the invention further comprises a first bracket (18) and a second bracket (23), and both ends of the top cover (21) are fixedly mounted on the first bracket (18) and the second bracket (23), respectively.

[0054] In one embodiment, it further comprises a sealing strip (20), wherein the sealing strip (20) is provided at the contact portion after the top cover (21) and the mixing tank body (22) are covered.

[0055] In one embodiment, the top cover (21) is provided with an ash inlet.

[0056] In one embodiment, the diameter of the feed hole is selected to be 0.5mm-3mm.

[0057] In one embodiment, the D50 particle size of the adhesive paste@soot composite material is 50 mesh to 300 mesh.

[0058] In one embodiment, there is no particular requirement for the duration of each coating stage, for example, it can be more than 10 minutes, and considering the processing efficiency, it can be further 10 to 120 minutes.

[0059] In one embodiment, there is no special requirement for the temperature and humidity of each coating stage, which can be a normal ambient temperature and humidity. Furthermore, the temperature can be 10-45° C. and the humidity can be relaxed to 60%.

[0060] The present application also provides a paste@soot composite material prepared by the preparation method.

[0061] In the present application, thanks to the preparation method, a composite material with special results can be obtained, and the composite material can unexpectedly take into account both excellent moisture-proof performance and atomizer release effect.

[0062] The present application also provides an application of the adhesive paste@ash composite material obtained by the preparation method, which is used to prepare tobacco sheets for new tobacco, more preferably thick pulp method sheets.

[0063] This application also provides a novel tobacco product comprising a tobacco sheet comprising the adhesive paste and ash composite material produced by the aforementioned preparation method, preferably a thick slurry-based sheet. The tobacco sheet can be a sheet comprising the adhesive paste and ash composite material produced by any preparation method. Given the composite material's excellent moisture resistance and uniform release of the smoking agent, it is particularly suitable for thick slurry-based sheets, thereby providing greater applicability.

[0064] A novel tobacco product comprises a paste@ash composite material obtained by the preparation method described in the present application and tobacco sheets containing the paste@ash composite material.

[0065] The preferred novel tobacco product is a heat-not-burn cigarette, the heating section of which is added with the thick pulp sheet. The present application also provides a heat-not-burn novel tobacco, the heating section of which is added with the thick pulp sheet.

[0066] The present application also provides a method for preparing the novel tobacco product, which can be obtained by rolling the thick pulp sheet described in the present application based on known equipment and methods.

[0067] In one embodiment, the humidity during the preparation process is 45-70%, and can further be 60±5%.

[0068] In the present application, thanks to the excellent performance of the composite material, the humidity of the sheet formed therefrom can be relaxed to 45-70% of the ambient humidity for preparing tobacco products compared to existing conventional sheets. However, the humidity of existing conventional sheets during the preparation time of the cigarette forming process usually needs to be specially controlled to be below 45%.

[0069] This application provides a method for preparing a paste-to-ash composite material, which can reduce the exchange of atomizer and water, slow the moisture absorption rate of the prepared smoking material, and eliminate the generation of yellow smoke. Furthermore, it can improve the atomization loading rate, atomization uniformity, and flavor release, thereby improving the puff taste.

[0070] The present application adopts a special diatomaceous earth and vermiculite combination inorganic material and its special calcination process to pretreat the modified mixture in combination with a pore-forming agent, as well as improved processes such as the first stage coating under pressurized conditions (positive pressure conditions). This can be further combined with the equipment and material structure of the present application to help further improve the atomizer loading rate, reduce the replacement of the atomizer and water, reduce the moisture absorption rate of the prepared smoking material, eliminate the generation of yellow smoke, and improve the atomization uniformity and the smoking taste.

[0071] The heated cigarette core (smoking material) prepared using the present application has loose requirements for the cigarette rolling and storage environment, which can be relaxed to a humidity level not higher than 65%. The production process cost is low, and the atomization uniformity and smoking taste of the produced thin sheets are better. BRIEF DESCRIPTION OF THE DRAWINGS

[0072] In order to more clearly illustrate the embodiments of the present application or the technical solutions in the conventional technology, the following briefly introduces the drawings required for use in the embodiments or the conventional technology descriptions. Obviously, the drawings described below are only some embodiments of the present application. For ordinary technicians in this field, other drawings can be obtained based on these drawings without creative work.

[0073] FIG1 is a schematic diagram of the main structure of the adhesive paste preparation tank of the present application.

[0074] FIG2 is a side view of the structure of the adhesive paste preparation tank after the lifting platform is raised.

[0075] FIG3 is a schematic diagram of the top view of the paste preparation tank.

[0076] FIG4 is a front view of a trough mixer for uniformly mixing the paste and the soot.

[0077] FIG5 is a side view of a mixing tank body of a tank mixer for uniformly mixing paste and soot after rotation.

[0078] Reference numerals:

[0079] 1. Tank body; 2. Stirring scraper; 3. Rotating shaft; 4. Frame body; 5. Stirring rod; 6. First motor; 7. Dispersion turntable; 8. Cover body; 9. Temperature control device; 10. Lifting platform; 11. Electric push rod; 12. Second motor; 13. Main controller; 14. Base; 15. First motor; 16. First reducer; 17. Bearing seat; 18. First bracket; 19. Stirring rod; 20. Sealing strip; 21. Top cover; 22. Mixing tank body; 23. Second bracket; 24. Fixed column; 25. First gear; 26. Second gear; 27. Second reducer; 28 Second motor; 29. ​​Feed pipe. DETAILED DESCRIPTION

[0080] The following will be combined with the drawings in the embodiments of this application to clearly and completely describe the technical solutions in the embodiments of this application. Obviously, the embodiments described are only part of the embodiments of this application, not all of the embodiments. Based on the embodiments in this application, all other embodiments obtained by ordinary technicians in this field without making creative efforts are within the scope of protection of this application.

[0081] As shown in Figures 1-3, the present invention discloses a paste preparation tank, comprising a tank body 1, wherein the tank body 1 is provided with a frame-type scraping and stirring device, wherein the frame-type scraping and stirring device comprises a rotating shaft 3 and a rotating frame body 4, wherein the top of the rotating frame body 4 is provided with an axial hole, wherein the rotating shaft 3 passes through the axial hole and is rotatably connected to the rotating frame body 4, wherein a plurality of stirring rods 5 are radially mounted on the rotating shaft 3, wherein the inner side of the rotating frame body 4 is provided with a plurality of stirring rods 5, wherein the outer side of the rotating frame body 4 is provided with a plurality of stirring scrapers 2, and further comprising a first motor 6, a second motor 12, and a main controller 13, wherein the output end of the first motor 6 is connected to the rotating shaft 3, and the output end of the second motor 12 is connected to the rotating frame body 4 via a bevel gear, wherein the tank body 1 is provided with a temperature control device, wherein the first motor 6, the second motor 12, and the temperature control device are all electrically connected to the main controller 13. Specifically, the main controller has a stepless frequency converter, which changes the speed of the first motor and the second motor by the stepless frequency converter to adjust the stirring impact force, and can adjust the speed within the speed range of 0 to 60 rpm. It can make the material roll naturally in the pot and eliminate dead corners, so that the material can obtain higher quality stirring effect.

[0082] In some embodiments, the temperature control device 9 includes an insulating outer shell and a hot water pipe disposed within the insulating outer shell. Both the insulating outer shell and the tank body 1 are provided with temperature sensors, which are electrically connected to the main controller 13. The temperature control device maintains the temperature within the tank body at 50-60°C, thereby increasing the fluidity of the high-viscosity paste and resolving the problem of poor discharge of the high-viscosity paste.

[0083] In some embodiments, the bottom end of the rotating shaft is fixedly connected to a dispersion turntable 7, which has a plurality of teeth alternately distributed up and down around it. The dispersion turntable with teeth can further disperse the material at the bottom of the tank body and improve the stirring effect.

[0084] In some embodiments, the tank body has a cover body 8, and a sight light and a vacuum sight glass with a scraper, a CIP cleaning head and a vacuum pressure gauge are fixedly connected to the cover body. Specifically, when the sight light is turned on, the state of the interior of the tank body can be seen through the vacuum sight glass with a scraper. The scraper can scrape off the material attached to the vacuum sight glass to avoid blocking the line of sight. The CIP cleaning system belongs to the prior art. The CIP cleaning head is connected to the cover body to facilitate the cleaning of the tank body. The vacuum pressure gauge is used to detect the pressure value in the tank body. A feed port is provided on the cover body, and feeding is achieved through a vacuum feeding pipe. A discharge port is provided at the bottom of the tank body. The size of the discharge port can be selected according to actual needs. In this embodiment, the diameter of the discharge port is 51 mm, which is conducive to discharging materials.

[0085] Some embodiments further include a lifting platform. The bottom of the lifting platform 10 is connected to an electric push rod 11, which is electrically connected to a main controller. The motor is fixedly connected to the lifting platform, and the cover is fixedly connected to the lifting platform. When the lifting platform is raised or lowered, the motor, the frame-type scraping and stirring device, and the cover rise and fall with the lifting platform. Opening the cover via the lifting platform facilitates the cleaning of residual materials.

[0086] In some embodiments, the tank body 1 has a three-layer structure, with the innermost layer being made of stainless steel and mirror-polished. Specifically, a multi-layered tank body provides improved thermal insulation, and the mirror-polished stainless steel reaches a 300EMSH sanitary grade, preventing contamination of the contents. The outer insulation layer utilizes a PU polyurethane foaming process to reduce energy consumption.

[0087] In the present application, the rotation of the frame-type scraping stirring device is realized by the first motor and the second motor, and the stepless frequency converter of the main controller is used to realize the stepless speed change of the motor for sufficient stirring, and multiple radially arranged stirring rods can improve the uniformity of stirring and mixing. The dispersion turntable arranged at the bottom of the rotating shaft can make the material at the bottom more evenly dispersed. The temperature inside the tank is maintained at 50-60°C by the temperature control device, which increases the fluidity of the high-viscosity paste and solves the problem of poor discharge of the high-viscosity paste. The cover can be automatically opened by the lifting platform to facilitate the cleaning of residual materials in the tank. In the present application, the paste preparation tank can achieve good infiltration of inorganic materials and penetration of the pore structure by the atomizer in the absence of water.

[0088] As shown in Figures 4 and 5, the present invention discloses a trough mixer for uniformly mixing adhesive paste and cigarette ash, including a base 14, to which a first motor 15, a fixed column 24, and a second motor are fixedly connected. The output end of the first motor 15 is connected to a stirring rod 19, which is rotatably connected to a mixing trough body 22. The stirring rod 19 is provided with stirring blades on a shaft section in the mixing trough body 22. The other end of the stirring rod 19 is rotatably connected to the fixed column 24. A first gear 25 is fixedly connected to one side of the mixing trough body 22, and a second gear 26 is connected to the output end of the second motor. The first gear 25 is transmission-connected to the second gear 26. The number of teeth on the first gear 25 is greater than the number of teeth on the second gear 26, so that a larger transmission torque can be obtained, which is more conducive to rotating the mixing trough body 22.

[0089] At least one feed pipe 29 is provided at the top of the mixing tank body. This feed pipe is provided with multiple small holes through which the paste enters the mixing tank body 22. The paste is squeezed externally through the holes in the feed pipe and enters the mixing tank body. Extrusion of the paste can be accomplished by using an electric push rod to push a piston, or other equivalent methods. The diameter of the small holes is selected to be 0.5 mm to 3 mm. After extrusion, the paste flows out in a thin, filamentous form, facilitating even mixing with the ash.

[0090] In some embodiments, the first motor 15 is connected to the stirring rod 19 via a first reducer 16, and the second motor is connected to the second gear 26 via a second reducer 27. Specifically, by selecting appropriate first reducer 16 and second reducer 27, the transmission ratio and transmission torque can be controlled to achieve a better stirring and mixing effect. The second motor can be selected as a stepper motor or a servo motor to better control the tilting angle of the mixing tank 22.

[0091] In some embodiments, through-holes are formed at both ends of the mixing tank body 22 for the stirring rod 19 to pass through. Bearing blocks 17 are fixedly connected to the through-holes. Bearings are matched and installed in the bearing blocks 17. The stirring rod 19 is rotatably installed through the bearings. Specifically, the bearing blocks 17 are fixed to the through-holes at both ends of the mixing tank body 22 by bolts. The bearings are installed in the bearing blocks 17. The stirring rod 19 passes through the bearings at both ends. The stirring rod 19 can rotate in the mixing tank body 22 to stir and mix.

[0092] In some embodiments, the open top of the mixing tank body 22 is provided with a top cover 21, and further includes a first bracket 18 and a second bracket 23. The two ends of the top cover 21 are fixedly mounted on the first bracket 18 and the second bracket 23 respectively. The top cover 21 is provided with an ash inlet and further includes a sealing strip 20. The sealing strip 20 is provided at the contact portion after the top cover 21 and the mixing tank body 22 are covered. Specifically, the material to be mixed is put into the mixing tank body 22 through the feed port on the top cover 21. During the stirring process of the stirring rod 19, the top cover 21 acts as a seal to prevent the internal material from overflowing. The top cover 21 is fixedly mounted by the first bracket 18 and the second bracket 23. When the mixing tank body 22 needs to be rotated to pour out the material therein, the top cover 21 will not move with the mixing tank body 22.

[0093] To sum up, the present application uses the trough mixer to mix and stir the materials in the mixing trough body by driving the stirring rod through the first motor. When the material mixing is completed, the mixing trough body is driven to rotate by the second motor to pour out the material. The entire mixing process does not require manual intervention, which effectively improves work efficiency and avoids the safety hazards that may be caused by manual operation. On the other hand, the diameter of the viscous paste entering the mixing trough body through the feed hole is smaller, and it is more uniform after mixing with the ash. Not only that, it is also beneficial for the ash to effectively block the pore structure on the surface of the viscous paste.

[0094] In the present application, the viscose used to form the thick slurry can be any conventional adhesive in the industry. For example, as an exemplary embodiment, the viscose is prepared by weighing 18 kg of sucrose fiber and 450 kg of water, placing them in a high-speed hydraulic fibrillator for 80 minutes while stirring at 5000 rpm. Then, 3 kg of guar gum, 1 kg of xanthan gum, and 5 kg of glycerin are added to the liquid in the hydraulic fibrillator in sequence and stirred at 5000 rpm for 30 minutes before use (adhesive).

[0095] The weight ratio of the paste@soot particles to the binder may be 1:3-10, and further may be 1:4-6.

[0096] In the present application, the preparation method of the thick slurry method sheet can be conventional. For example, the adhesive and the adhesive paste@ash particles can be evenly mixed to form a thick slurry, and then the slurry is spread, dried, and peeled based on conventional means to form a sheet.

[0097] In this application, the humidity of the preparation process is based on excellent tolerance and can be prepared under any environmental humidity conditions.

[0098] Example 1

[0099] Step (1): One stage of coating

[0100] 3000 g of inorganic material (diatomaceous earth, D50 is 200 mesh) and 1000 g of atomizer (glycerin) are stirred and coated in a paste preparation tank. Stirring is continued for 20 to 30 minutes, the stirring rotor speed is controlled at 1200 rpm, and the stirring tank temperature is controlled at 50°C ± 5°C. After meeting the process requirements, mixture 1 (paste) is obtained and set aside.

[0101] Step (2): Second stage coating

[0102] Add glycidyl methacrylate (0.2 times the weight of the paste) to the paste of step 1, mix and perform the second coating (time is 20 to 30 minutes) to obtain a modified paste;

[0103] Step (3): Three-stage coating

[0104] The ash raw materials (tobacco leaves, tobacco stems and tea leaves in a weight ratio of 6:3:1) are crushed at a temperature below 50° C. to obtain ash with a mesh size of 200 to 500.

[0105] The modified paste and soot were mixed in a tank mixer at a weight ratio of 1:5 (for 20 to 30 minutes) to obtain paste@soot particles.

[0106] Step (4): Conventional slurry and sheet preparation

[0107] The prepared adhesive paste@cigarette ash particles and viscose (weight ratio of 1:4) are evenly mixed, and then thick pulp sheet for heated cigarette is produced according to the manufacturing process of thick pulp sheet.

[0108] The thick slurry flakes produced using this method are then cut into shreds and rolled into heated cigarettes. (This process is based on known techniques and equipment, differing in that the humidity during the production stages of heated cigarettes, including cutting and rolling, is relaxed to 60±5%). This effectively prevents moisture absorption, clumping, clogging, and water-soaked lumps in the flakes or heated cigarettes. Furthermore, no clogging of the cigarette-rolling machine occurred during the production process.

[0109] Comparative Example 1

[0110] Compared with Example 1, steps 1 to 3 are combined into one mixing process. Specifically, the inorganic material, atomizer, glycidyl methacrylate and soot are mixed together using the mixing equipment of Figure 1 (total mixing time is 1.5 hours) to obtain a composite material, which is used to replace the sticky paste @ soot particles in Example 1 and is processed in step 4 to obtain a thick slurry and a thin sheet.

[0111] Example 2:

[0112] Compared with Example 1, the only difference is that the inorganic material is changed. Other operations and parameters are the same as Example 1. The experimental groups are:

[0113] A: The inorganic material is vermiculite (D50 is 200 mesh)

[0114] B: The inorganic material is diatomaceous earth (D50 is 200 mesh) and vermiculite (D50 is 200 mesh) in a weight ratio of 1:1; the amount of the total inorganic material is the same as that in Example 1.

[0115] C: The inorganic material is a modified material, and its preparation process is as follows: 2000 grams of diatomaceous earth (D50 is 200 mesh), 1000 grams of vermiculite (D50 is 200 mesh) and 1000 grams of starch are treated by the following program heating process

[0116] Example 3:

[0117] Compared with Example 1, the only difference is that in step 1, the atomizer and the inorganic material are stirred and coated at 1.5 atmospheres.

[0118] Comparative Example 2

[0119] Compared with Example 1, the only difference is that step 2 is missing, and other operations and parameters are the same as Example 1.

[0120] Comparative Example 3

[0121] Compared with Example 1, a conventional thick slurry preparation process is adopted, the only difference being that steps 1 to 3 are omitted, and instead the inorganic material, smoke generating agent, and glycidyl methacrylate used in these steps are directly mixed with the adhesive in step 4 to form a thick slurry and a thin sheet.

[0122] Comparative Example 4

[0123] Compared with Example 1, the only difference is that Step 3 is directly performed after Step 1, followed by Step 2, and then Step 4. Other operations and parameters are the same as in Example 1.

[0124] Example 4

[0125] Compared with Example 1, the difference is that in step 1, the inorganic material is activated carbon. The atomizer is glycerol. The weight ratio of the atomizer to the inorganic material is 0.4:1;

[0126] In step 2, the hydrophobic agent is organopolysiloxane, and the weight ratio of the adhesive paste to the hydrophobic agent is 1:0.15.

[0127] In step 3, the weight ratio of the second coating paste to the soot is 1:4.

[0128] Other operations and parameters are the same as in Example 1.

[0129] Example 5

[0130] Compared with Example 1, the difference is that in step 1, the inorganic material is porous ceramic. The atomizer is glycerol. The weight ratio of the atomizer to the inorganic material is 0.3:1;

[0131] In step 2, the hydrophobic agent is organopolysiloxane, and the weight ratio of the adhesive paste to the hydrophobic agent is 1:0.25.

[0132] In step 3, the weight ratio of the second coating paste to the soot is 1:6.

[0133] Other operations and parameters are the same as in Example 1.

[0134] Example 6

[0135] Compared with Example 1, the only difference is that in step 4, the thin sheet is produced using a papermaking method. The mixture (adhesive paste and ash particles) processed in steps 1, 2, and 3 is mixed with a coating liquid (adhesive) at a ratio of 1:2. This mixture is then coated on a substrate using the papermaking thin sheet production process, dried, and sliced. The resulting mixture is then shredded to produce heated cigarettes.

[0136] Example 7

[0137] Compared with Example 1, the only difference is that step 4 uses a roller pressing method to produce thin sheets. First, 18 kg of sucrose fiber and 120 kg of water are weighed and placed in a high-speed hydraulic fiberizer for fiberization for 60 minutes at a stirring speed of 5000 rpm. 3 kg of guar gum, 1 kg of xanthan gum, and 5 kg of glycerin are sequentially added to the liquid in the hydraulic fiberizer and stirred at 5000 rpm for 30 minutes before use (adhesive). The mixture (adhesive paste and ash particles) processed in steps 1, 2, and 3 is mixed in a 1:1 ratio. Roller pressing is used to produce thin sheets for heated cigarettes, which are then dried and shredded to produce heated cigarettes.

[0138] Example 8

[0139] Compared with Example 1, the only difference is that step 4 uses a substrate coating method to produce the sheet, and the mixture (paste @ ash particles) treated in steps 1, 2, and 3 is mixed with a coating liquid (adhesive) in a ratio of 1:1 to form a coating slurry, and the above-mentioned coating slurry is coated on a substrate (which can be a papermaking tobacco sheet or a plant fiber substrate made of other fibers), and then dried, sliced, and shredded to make heated cigarettes.

[0140] Example 9

[0141] Compared with Example 1, the only difference is that step 4 uses a dry method to produce thin sheets. The mixture (adhesive paste @ ash particles) processed in steps 1, 2, and 3 is mixed with a binder in a ratio of 1:5 to form a spray slurry. The above-mentioned spray slurry is repeatedly sprayed 6 times using a nozzle onto a substrate pre-manufactured using a non-woven fabric production process. Thereafter, the substrate is dried, sliced, and shredded to produce heated cigarettes.

[0142] Example 10

[0143] Compared with Example 1, the only difference is that step 4 uses extrusion molding to produce thin slices. First, 15 kilograms of sucrose fiber and 100 kilograms of water are weighed and placed in a high-speed hydraulic fiberizer for fiberization for 60 minutes at a stirring speed of 5000 rev / min. 3 kilograms of guar gum, 1 kilogram of xanthan gum, and 1 kilogram of angle glue are sequentially put into the liquid in the above-mentioned hydraulic fiberizer and continued to stir at 5000 rev / min for 30 minutes for standby use (adhesive). The mixture (adhesive paste @ ash particles) processed by steps 1, 2, and 3 is mixed in a 1:1 ratio. Thin slices for heating cigarettes are manufactured by the extrusion molding process, dried, and shredded to make heating cigarettes.

[0144] The puff-by-puff method of heated cigarettes is tested according to conventional industry methods. For example, the heating operating temperature of the heating device during the puffing stage is 220℃±5℃.

[0145] The release uniformity of the atomizer of glycerol 1 to 7 puffs and the 24-hour weight gain data at a humidity of 45 to 60 ± 3% detected in the Examples and Comparative Examples are shown in Table 2:

[0146] Table 2

[0147] In summary, the present invention can effectively improve the moisture-proof effect, and even under high humidity conditions, it can show excellent moisture-proof effect. Not only that, not only will the atomizer release effect not be sacrificed for moisture-proofing, but it can also improve the atomizer release amount and release uniformity of the sheet to a certain extent. Moreover, the preparation process of the present invention is flexible in conditions and can tolerate high humidity preparation conditions. For example, it can be rolled into cigarettes unexpectedly at high ambient humidity (about 60%). In addition, it can also be applied to different sheet preparation processes, the process conditions are easy to achieve, and the process has good universality.

[0148] In the description of this application, it should be understood that if the terms "first" and "second" appear, these terms are used for descriptive purposes only and should not be understood as indicating or implying relative importance or implicitly indicating the number of technical features indicated. Therefore, a feature defined as "first" or "second" may explicitly or implicitly include at least one of such features. In the description of this application, if the term "plurality" appears, "plurality" means at least two, for example, two, three, etc., unless otherwise clearly and specifically defined.

[0149] In this application, unless otherwise specified or limited, the terms "connected" and "fixed" should be interpreted broadly. For example, they can refer to fixed connections, removable connections, or integration; mechanical connections or electrical connections; direct connections or indirect connections through an intermediary; and internal communication between two components or interaction between two components, unless otherwise specified. Those skilled in the art will understand the specific meanings of these terms in this application based on the specific circumstances.

[0150] The technical features of the above-mentioned embodiments can be combined arbitrarily. In order to make the description concise, not all possible combinations of the technical features in the above-mentioned embodiments are described. However, as long as there is no contradiction in the combination of these technical features, they should be considered to be within the scope of this specification.

[0151] The above-described embodiments merely represent several implementation methods of the present application. While the descriptions are relatively specific and detailed, they should not be construed as limiting the scope of the patent application. It should be noted that a person of ordinary skill in the art may make various modifications and improvements without departing from the spirit of the present application, and these modifications and improvements fall within the scope of protection of the present application. Therefore, the scope of protection of the present patent application shall be determined by the appended claims.

Claims

1. A method for preparing a viscous paste@soot composite material, comprising: coating an atomizer and an inorganic material in a viscous paste preparation tank in a first stage to obtain a viscous paste; then mixing the viscous paste with a hydrophobic agent to achieve a second stage of coating; and then coating the viscous paste and soot in a tank mixer in a third stage to obtain the viscous paste@soot composite material; The inorganic material is a material having at least one pore structure of nanopores, mesopores and macropores, and its D50 particle size is 50-300 meshes. The D50 particle size of the soot is 100-300 meshes.

2. The preparation method according to claim 1, wherein the atomizer refers to a substance that can emit smoke at a temperature of 150 to 250° C.; including but not limited to at least one of glycerol, propylene glycol, polyols, esters, and sugar compounds.

3. The preparation method according to claim 1, wherein the inorganic material is at least one of activated carbon, diatomaceous earth, sepiolite, zeolite, silica, vermiculite, foamed aluminum, foamed nickel, foamed carbon, porous silicon carbide, porous ceramics, carbon molecular sieve, and zeolite molecular sieve.

4. The preparation method according to claim 3, wherein the inorganic material comprises a mixture of diatomaceous earth and vermiculite and a modified mixture thereof; The modified mixture is a product obtained by mixing the mixture and the pore-forming agent and then subjecting the mixture to a gradient calcination treatment; The pore-forming agent includes but is not limited to at least one of CMC, glucose solution, proline and starch; The gradient calcination treatment stage includes two heat treatment platforms, wherein: The temperature of the first stage heat treatment platform is 150-300°C, and the temperature of the second stage heat treatment platform is 900-1100°C.

5. The preparation method according to claim 1, wherein the weight ratio of the atomizer to the inorganic material is 0.1 to 0.5:1; The first coating stage is carried out under positive pressure; The positive pressure is above 1.1 atm, preferably above 1.5 atm.

6. The preparation method according to any one of claims 1 to 5, wherein the paste preparation tank comprises a tank body (1), wherein a frame-type scraping and stirring device is provided in the tank body, wherein the frame-type scraping and stirring device comprises a rotating shaft (3) and a rotating frame body (4), wherein an axial hole is provided at the top of the rotating frame body, wherein the rotating shaft (3) passes through the axial hole and is rotatably connected to the rotating frame body (4), wherein a plurality of stirring rods (5) are radially mounted on the rotating shaft, wherein a plurality of stirring rods (5) are provided on the inner side of the rotating frame body, wherein a plurality of stirring scrapers (2) are provided on the outer side of the rotating frame body (4), wherein the first motor (6), a second motor (12) and a main controller (13), wherein the output end of the first motor is connected to the rotating shaft, wherein the output end of the second motor is connected to the rotating frame body via a bevel gear, wherein the tank body is provided with a temperature control device (9), wherein the first motor, the second motor and the temperature control device are all electrically connected to the main controller; In the paste preparation tank, the temperature control device (9) comprises a heat-insulating shell and a hot water pipeline arranged in the heat-insulating shell, and the heat-insulating shell and the tank body (1) are both provided with temperature sensors, and the temperature sensors are electrically connected to the main controller; The bottom end of the rotating shaft is fixedly connected with a dispersion rotating disk (7), and the dispersion rotating disk has a plurality of teeth alternately distributed up and down around it; The tank body has a cover body (8), and the cover body (8) is also fixedly connected with a sight light, a vacuum sight glass with a scraper, a CIP cleaning head and a vacuum pressure gauge; It also comprises a lifting platform, wherein the bottom of the lifting platform (10) is connected to an electric push rod (11), the electric push rod is electrically connected to a main controller, the motor is fixedly connected to the lifting platform, and the cover is fixedly connected to the lifting platform; when the lifting platform is raised or lowered, the motor, the frame-type wall scraping and stirring device, and the cover are raised or lowered together with the lifting platform; The tank body (1) has a three-layer structure, and the innermost layer of the tank body is made of stainless steel; The innermost layer of the tank body (1) is subjected to mirror polishing treatment.

7. The preparation method according to claim 1, wherein the hydrophobic agent is at least one of glycidyl methacrylate and organopolysiloxane; The weight ratio of the adhesive paste to the hydrophobic agent is 1:0.1-0.

8.

8. The preparation method according to claim 1, wherein the particle size of the soot is 200 to 500 mesh; The raw materials in the ash at least include tobacco raw materials, and the tobacco raw materials include at least one of tobacco leaves, tobacco stems, fragments, and tobacco dust; The raw materials in the ash also include auxiliary plant ingredients, which preferably include but are not limited to at least one of tea leaves, clove leaves, mint leaves and roses.

9. The preparation method according to claim 8, wherein the smoke ash is obtained by crushing and grinding the raw materials at a temperature below 50°C.

10. The preparation method according to claim 1, 8 or 9, wherein the weight ratio of the second coating paste to the soot is 1:1-20.

11. The preparation method according to claim 1, wherein the tank mixer comprises a base (14), a first motor (15), a fixed column (24) and a second motor are fixedly connected to the base (14), a stirring rod (19) is connected to the output end of the first motor (15), the stirring rod (19) is rotatably connected to a mixing tank body (22), a stirring blade is provided on the shaft section of the stirring rod (19) in the mixing tank body (22), the other end of the stirring rod (19) is rotatably connected to the fixed column (24), a first gear (25) is fixedly connected to one side of the mixing tank body (22), a second gear (26) is connected to the output end of the second motor, the first gear (25) is transmission-connected to the second gear (26), at least one feeding pipe (29) is provided on the inner top of the mixing tank body, the feeding pipe is provided with a plurality of feeding holes, and the adhesive paste enters the mixing tank body (22) through the feeding holes; In the tank mixer, the first motor (15) and the stirring rod (19) are connected via a first reducer (16); The second motor is connected to the second gear (26) via a second reducer (27); Through holes for the stirring rod (19) to pass through are formed at both ends of the mixing tank body (22), a bearing seat (17) is fixedly connected to the through hole, a bearing is matched and installed in the bearing seat (17), and the stirring rod (19) is rotatably installed through the bearing; The open top of the mixing tank body (22) is provided with a top cover (21); It also includes a first bracket (18) and a second bracket (23), and the two ends of the top cover (21) are fixedly mounted on the first bracket (18) and the second bracket (23) respectively; It also includes a sealing rubber strip (20), wherein the sealing rubber strip (20) is arranged at the contact position after the top cover (21) and the mixing tank body (22) are covered; The top cover (21) is provided with an ash inlet; The diameter of the feed hole is selected to be 0.5mm-3mm.

12. The preparation method according to claim 1, wherein the D50 particle size of the adhesive paste@soot composite material is 50 mesh to 300 mesh.

13. An adhesive paste@soot composite material obtained by the preparation method according to any one of claims 1 to 12.

14. Use of the adhesive paste@cigarette ash composite material obtained by the preparation method according to any one of claims 1 to 12, wherein the composite material is used to prepare tobacco sheets of new tobacco, more preferably thick slurry sheets.

15. A tobacco sheet of a novel tobacco product, comprising the adhesive paste@cigarette ash composite material obtained by the preparation method according to any one of claims 1 to 12.

16. A novel tobacco product, comprising the adhesive paste@cigarette ash composite material obtained by the preparation method according to any one of claims 1 to 12; It comprises the thick pulp flakes as claimed in claim 15.

17. The novel tobacco product according to claim 16, which is a heat-not-burn cigarette, wherein the thick pulp sheet is added to the heating section.

18. A method for preparing the novel tobacco product according to any one of claims 16 to 17, which is obtained by rolling the thick pulp sheet; The humidity during the preparation process is 45-70%.