Method for manufacturing a board having a three-dimensional wood grain on the surface thereof
Patent Information
- Application Number
- MYPI2025006407
- Authority / Receiving Office
- MY · MY
- Patent Type
- Applications
- Current Assignee / Owner
- Priority Date
- 2023-04-18
- Filing Date
- 2024-04-09
- Publication Date
- 2024-10-18
AI Technical Summary
When using existing technology to manufacture boards with three-dimensional wood grain on the surface, it is difficult to match the printed image on the bottom, resulting in poor visual and tactile effects. In addition, the mold wears quickly and the cost is high, making it difficult to meet customization needs.
By obtaining the surface database of natural wood, the underlying wood grain printing data set and the three-dimensional wood grain printing data set are separated, and different printing devices are used to output the underlying wood grain layer and the three-dimensional wood grain respectively. Combined with the shape and depth information of the wood grain, ensure The correspondence between the two simplifies the preparation process and improves flexibility.
It achieves a three-dimensional wood grain effect that is similar to natural wood, improves the accuracy of flower registration, reduces production costs, enhances the flexibility and richness of the product line, and meets customer customization needs.
Smart Images

Figure PI2025006407_DRAWING_001 
Figure PI2025006407_DRAWING_002 
Figure PI2025006407_DRAWING_003
Abstract
Description
Method for manufacturing a board having three-dimensional wood grain on the surface Technical Field The invention relates to the field of surface structure preparation, in particular to a method for manufacturing a board with three-dimensional wood grain on the surface. Background Art Currently in the field of board manufacturing, manufacturers can use advanced technologies and materials to create products that look and feel similar to natural wood based on artificial boards or non-wood boards. These products are expected to have better performance and durability, thus meeting consumers' demand for high-quality, low-maintenance and low-cost products. In addition, these products that are similar to natural wood can also reduce dependence on natural resources, thereby protecting the environment and promoting sustainable development. In order to obtain a texture similar to natural wood on the surface of artificial boards or non-wood boards, manufacturers usually adopt the following methods: 1. Printing technology: Use high-resolution printing technology to print the natural wood texture pattern onto the board surface; 2. Veneer: A thin sheet of wood is glued to the surface of the board to imitate the look and feel of natural wood; 3. Coating technology: Through a special coating process, a texture and color similar to natural wood is formed on the surface of the board. Although these methods can imitate the appearance and texture of natural wood to a certain extent, they also have certain defects. For example, printing technology cannot completely replicate the texture of natural wood; thin wood veneer is easily affected by moisture and cracking; coating technology may have adverse effects on the environment. The patent with publication number CN 101659073 B discloses a wood grain treatment process for the surface of a waterproof floor substrate, which is to print simulated wood grain on the surface of the wood plastic floor, and then add a wear-resistant layer on the simulated wood grain, so that the wood grain pattern is protected and the wood grain texture effect is maintained for a long time. However, this board with only a two-dimensional flat image printed on the surface can no longer meet people's demand for a more realistic visual and tactile combination. Therefore, forming three-dimensional wood grain on the surface of a board material that corresponds to a two-dimensional plane image and has a touch that is closer to that of wood is currently a common concern in the art. In the prior art, a variety of different technical solutions have been proposed to form a three-dimensional structure on the surface of a substrate. Conventional methods generally include a molding method, an upward stacking method, and a downward indentation method. The conventional embossing method is to reproduce the structure to be printed on the sheet by pressing with a mold, roller or belt. The method can be implemented by pressing on an incompletely hardened resin, thermoplastic material, photo-crosslinking resin and simultaneously irradiating and photopolymerizing. The technologies related to the molding method can refer to the following patents: The patent with publication number CN115027117A discloses an enhanced wood texture floor, comprising a foam core having a shell and attachments distributed on the surface of the shell, wherein the shell is formed of a first color resin and the attachments are formed of a second color resin. During the preparation process, the shell is embossed by an embossing roller, so that a part of the second color resin layer is pressed below the shell surface, so that the shell and the second color resin layer present a wood texture together. The patent with publication number CN115122452A discloses a method for producing highly simulated precious tree species wood flooring, which includes using a laser engraving method to engrave a 3D texture on a steel plate of a flat press or on a roller of a roller coater, and then pressing the texture on a blank to produce a beautiful and high-end wood flooring with highly simulated precious tree species wood grain. The upward stacking method is based on resin materials, which are stacked upward layer by layer through printing or printing, so that a floor with a three-dimensional structure is eventually formed in the process of continuous stacking. The following patents can be referenced for technologies related to the upward stacking method: The patent with publication number CN 112455110 A discloses a process for producing wooden floor by inkjet printing. The patent can form convex three-dimensional wood grain on the surface of the pattern texture by continuously printing additive ink on the surface of the printed pattern texture. The downward recess method is to spray a layer of inhibitory substance that can hinder or delay the polymerization of the resin on the surface of the uncured resin. After the subsequent curing treatment of the resin, the part of the resin containing the inhibitory substance remains liquid. It is only necessary to brush off the liquid resin downwards during the subsequent treatment process to form a concave three-dimensional structure. The following patents may be referenced for technologies related to the downward indentation method: Patent publication number CN 110177691 B discloses a method and apparatus for producing embossing on a substrate by means of digital printing technology. This method comprises applying an embossing liquid on a non-polymeric resin layer, and then performing subsequent polymerization of the resin by means of UV curing. The embossing liquid is then removed to form a three-dimensional surface. The patent with publication number CN 112739463 A discloses a new method and device for producing a surface structure, comprising the following steps: A) applying resin A to the surface of a material; B) when the resin A is liquid or partially solidified, applying liquid B to at least a portion of the resin A; C) polymerizing the resin A and the liquid B separately; and D) removing the polymerized liquid B. The patent with publication number CN 112996649 A discloses a method for manufacturing a three-dimensional structure on the surface of a flat substrate, the resulting substrate and an apparatus for producing the substrate according to the method, wherein a material for forming a wood grain seam is dripped onto the surface of the substrate in advance, and then a curable resin is applied to the area of the substrate surface not covered with the material for forming the wood grain seam, and then the resin is cured and the material for forming the wood grain seam is removed, thereby forming the wood grain seam in the cured resin. At present, the dimensions that need to be considered to measure the similarity between three-dimensional wood grain and natural wood grain include: (1) the similarity between the width and depth of the three-dimensional wood grain and the natural wood grain; (2) the correspondence between the three-dimensional wood grain and the bottom two-dimensional plane structure. However, no matter which method is used, the molding method, the upward stacking method or the downward indentation method, there are inevitable defects. For example, the main focus of the above-disclosed prior art is how to form a three-dimensional wood grain with a higher degree of similarity to the natural wood grain, that is, the prior art can only solve the first dimension as mentioned above. As for how to better correspond the three-dimensional wood grain with the bottom two-dimensional plane structure, the above-disclosed prior art does not provide a good solution, so it is easy to cause the defect of misalignment in the manufacturing process of the board, which ultimately leads to the problem of visual and tactile matching. In addition, in the process of using the molding method to prepare a floor with a three-dimensional structure, the mold often wears during the working process, so the service life of the mold is short, the surface structure of the floor between different batches is different, and the manufacturing cost of the floor is higher. Therefore, in order to obtain a three-dimensional wood grain that is more similar to the wood grain of natural wood, it is necessary not only to consider how to prepare a three-dimensional structure that is more similar to the natural wood grain structure, but also to consider how to correspond the three-dimensional structure to the two-dimensional plane image at the bottom. Only by taking into account the molding effect of the three-dimensional structure and the correspondence between the three-dimensional structure and the two-dimensional plane image at the bottom, can the key point be achieved to obtain a texture similar to that of natural wood on the surface of artificial board or non-wood board. However, no relevant precedent has been seen in the currently disclosed technology. Summary of the invention The present invention aims to overcome the defect in the prior art that the three-dimensional wood grain formed on the surface of the board is difficult to match with the printed image at the bottom, and provides a method for manufacturing a board with three-dimensional wood grain on the surface, which effectively solves the problem of inaccurate alignment between the three-dimensional wood grain and the printed image at the bottom. To achieve the above-mentioned purpose, the present invention is implemented by the following technical solutions: In a first aspect, the present invention first provides a method for manufacturing a board having a three-dimensional wood grain on its surface, which comprises at least the following steps: (S.1) obtaining wood grain information and processing it to extract a wood surface database; The database includes at least a bottom wood grain printing data set and a three-dimensional wood grain printing data set; The three-dimensional wood grain printing data set includes a two-dimensional three-dimensional wood grain printing shape data subset corresponding to the bottom wood grain printing data set and a three-dimensional wood grain printing depth data subset corresponding to the three-dimensional wood grain printing shape data subset; (S.2) assigning a bottom wood grain print data set to a first printing device; assigning the three-dimensional wood grain printing data set to a second printing device; (S.3) using the first printing device to output the bottom wood grain printing data set on the surface of the board to obtain a bottom wood grain layer that matches the wood grain information; (S.4) Outputting a wood grain precursor liquid using the three-dimensional wood grain printing data set using the second printing device to obtain a wood grain precursor for forming three-dimensional wood grain and matching the underlying wood grain layer, and the height of the wood grain precursor (i.e., the distance between the upper end surface of the wood grain precursor and the lower end surface of the wood grain precursor) corresponds to different subsets of three-dimensional wood grain printing depth data. The applicant of the present invention has found after extensive and in-depth research on natural wood boards that the color, wood grain shape and three-dimensional structure of the wood surface of natural wood materials will change to varying degrees due to the different wood species and growth environment. As a result, the visual and tactile effects that each natural wood board can present are different. Based on this discovery, in order to form a more realistic three-dimensional wood grain on the surface of the artificial board, it is necessary to consider the visual similarity between the two-dimensional structure of the plane and the natural wood grain, and the visual and tactile similarity between the three-dimensional structure and the natural wood grain. There are many methods in the prior art for forming a two-dimensional bottom wood grain layer on the surface of artificial boards, such as using printing technology, high-precision printing technology, etc. These technologies can well restore the color and wood grain pattern of real natural wood materials, so that these patterns are closer to natural wood grain in visual effect. However, how to obtain a three-dimensional wood grain on the bottom wood grain layer that matches the bottom wood grain layer and feels close to natural wood grain is a difficulty in this field. Generally speaking, in order to form three-dimensional wood grain on the surface of a board, it is first necessary to make a shape reference for the two-dimensional bottom wood grain layer to be printed, and to model the board to be printed through the two-dimensional bottom wood grain layer, so that the printing device can print according to the established three-dimensional model, thereby obtaining a three-dimensional wood grain that corresponds to the target model in the shape of the wood grain and the length, width and depth of the wood grain. Therefore, in this mode, a three-dimensional model can only correspond to a board with a specific two-dimensional bottom wood grain layer. If any variable of the board needs to be changed separately, the model needs to be redrawn and adjusted, resulting in the above method of forming three-dimensional wood grain. The flexibility is poor, it is difficult to adapt the board in a short time, and the production cost is relatively high. Therefore, the product line of enterprises that use this traditional method to prepare boards with three-dimensional wood grain on the surface is usually relatively single, and it is difficult to meet the needs of customization according to customer requirements. In order to overcome the defects existing in the above-mentioned prior art, the applicant of the present invention has conducted further in-depth research on the plane bottom wood grain layer and the three-dimensional wood grain. Among them, after studying the plane bottom wood grain layer, the applicant found that the elements forming the bottom wood grain layer usually include the base color of the wood grain and the shape of the wood grain set on the base color of the wood grain. Usually, only the base color of the wood grain and the shape of the wood grain need to be combined with each other to form a wood grain pattern that matches different wood materials. After conducting in-depth research on the three-dimensional wood grain, the applicant found that the elements forming the three-dimensional wood grain usually include the shape of the wood grain and the corresponding depths of different wood grain shapes. When the shape of the wood grain is combined with different depth information, a three-dimensional wood grain that is closer to the natural wood grain structure can be formed. Therefore, based on the above findings, compared with the prior art, the present invention analyzes and processes the information containing natural wood grain, thereby classifying and regularizing the formation parameters related to natural wood grain, thereby obtaining a bottom wood grain printing data set and a three-dimensional wood grain printing data set. Among them, the bottom wood grain printing data set records the data information used to control the formation of the bottom wood grain layer, and the three-dimensional wood grain printing data set records the data information used to control the formation of three-dimensional wood grain. In addition, the three-dimensional wood grain printing data set in the present application contains a two-dimensional wood grain printing shape data subset corresponding to the bottom wood grain printing data set. Therefore, when the relevant information for printing the bottom wood grain layer is determined, the three-dimensional wood grain shape data that matches the shape and size of the bottom wood grain layer can be selected from the two-dimensional wood grain printing shape data subset, thereby effectively realizing the correspondence between the shape and position of the bottom wood grain layer and the top three-dimensional wood grain, avoiding the problem of inaccurate alignment between the two. In addition, after the shape of the three-dimensional wood grain is determined, by calling the three-dimensional wood grain printing depth data subset, one or more wood grain depths are assigned to each wood grain of different shapes, so that three-dimensional wood grains of different shapes can have different corresponding depths, and the depth can change with the three-dimensional wood grains of different shapes, so as to be more adapted to the structure of natural wood grain, so that the obtained three-dimensional wood grain has a higher similarity with the natural wood grain. Therefore, through the method described in the present application, a three-dimensional wood grain similar to that of a natural wood board can be obtained on the surface of an artificial or non-wood board, and by digitizing the wood grain information, it is possible to achieve strict correspondence between the bottom wood grain layer and the three-dimensional wood grain located above the bottom wood grain layer during printing, thereby overcoming the problem of difficulty in "matching patterns" in the prior art. Finally, this method in the present application also has the advantage of high flexibility. Compared with the prior art, the three-dimensional wood grain in the present application does not require three-dimensional modeling of a single underlying wood grain layer. It only needs to analyze the wood grain shape contained in the underlying wood grain layer, and obtain it by retrieving it from the three-dimensional wood grain printing shape data subset of the three-dimensional wood grain printing data set. The shape data recorded in the three-dimensional wood grain printing shape data subset is matched with the depth data recorded in the three-dimensional wood grain printing depth data subset, thereby creating a three-dimensional wood grain that is closer to natural wood grain, effectively simplifying the construction process of the three-dimensional wood grain, enabling manufacturers to customize the production of products according to customer needs, expanding the richness of the company's product line, effectively reducing production costs and improving production efficiency. Preferably, the wood grain information can be obtained by scanning a natural wood board, wherein the data in the bottom wood grain print data set can be obtained by a high-resolution optical scanner, and the depth information of the wood grain can be obtained by a laser profilometer or other equipment. Preferably, the bottom layer wood grain printing data set includes a plurality of bottom layer wood grain printing base color data subsets and a plurality of bottom layer wood grain printing shape data subsets. The bottom wood grain printing data set in the present invention includes a bottom wood grain printing background color data subset, which is used to print the wood background colors presented by different wood materials. For example, in the process of printing fir and spruce, the background color is slightly yellow, while the background color of basswood, white sauerkraut, yellow tung and other woods is yellow-white, and the background color of locust, pistachio, catalpa, mulberry is brown; the background color of redwood, red pine, cryptomeria, camphor and other woods is reddish brown; the background color of red sandalwood, Indian yellow sandalwood, Indian rosewood is dark purple-red; the background color of ebony is black. Therefore, the data in the bottom wood grain printing background color data subset can be called to simulate the background color of natural wood with different colors. The underlying wood grain printing shape data subset can record information on wood grains of different shapes. For example, the underlying wood grain printing shape data subset can record information including annular growth rings, semi-annular hole structures, strip structures, corrugated structures, burl textures, etc., so the data in the underlying wood grain printing shape data subset can be randomly called to simulate the wood grain structures of natural wood with different shapes. In this way, a huge number of bottom wood grain layer styles can be combined by pairing the wood grain printing background color data subset with the bottom wood grain printing shape data subset, thereby greatly meeting the customer's customizability needs. Preferably, the bottom wood grain printing background color data subset includes multiple background color printing point coordinate data, each background color printing point coordinate data is marked with color information, and the first printing device prints based on the background color printing point coordinate data and the color information corresponding to the background color printing point coordinate data. The background color printing point coordinate data in the bottom wood grain printing background color data subset in the present invention records the color information of each coordinate point located on the surface of the board. Then the first printing device outputs line by line based on the color information of each coordinate point of each point, thereby obtaining a wood grain background color matching the natural wood grain. Preferably, the underlying wood grain printing shape data subset includes multiple sets of multiple two-dimensional plane wood grain printing coordinate data for printing wood grain, each plane wood grain printing coordinate data is marked with color information, and the first printing device prints based on the plane wood grain printing coordinate data and the color information corresponding to the plane wood grain printing coordinate data, and each underlying wood grain printing shape data subset corresponds to an underlying wood grain printing route. The bottom wood grain printing shape data subset of the present invention includes a plurality of two-dimensional plane wood grain printing coordinate data for printing wood grain, which also corresponds to color information, and the color information should be different from the wood grain background color, so that the plane wood grain can be distinguished from the background color, so that the wood grain can be displayed on the surface of the background color. At the same time, since the two-dimensional plane wood grain printing coordinate data records the coordinates of each point constituting the wood grain, the first printing device can print and output the wood grain according to these plane wood grain printing coordinate data. Preferably, the colors in the bottom wood grain printing base color data subset and the bottom wood grain printing shape data subset are obtained by superimposing at least one or more standard colors. Preferably, the standard colors include at least red, blue, light red, yellow, black, and light black. Preferably, the printing resolution of the background color printing point coordinate data and the plane wood grain printing coordinate data is greater than or equal to 100 DPI. The applicant of the present invention has discovered that the printing resolution of the background color printing point coordinate data and the plane wood grain printing coordinate data in the process of being assigned to the first printing device output has a significant impact on the visual effect of the final bottom wood grain layer. When the printing resolution is less than 100 DPI, the display effect after printing is relatively blurred and cannot show the wood grain effect well. Preferably, the three-dimensional wood grain printing shape data subset includes multiple two-dimensional three-dimensional wood grain printing coordinate data for printing wood grain, each three-dimensional wood grain printing shape data subset corresponds to a three-dimensional wood grain printing route, and multiple three-dimensional wood grain printing routes overlap with multiple bottom wood grain printing routes on a two-dimensional plane. The two-dimensional wood grain printing coordinate data contained in the three-dimensional wood grain printing shape data subset in the present application also records the plane coordinates of each point that constitutes the three-dimensional wood grain, and it can correspond to the coordinate information recorded in the underlying wood grain printing shape data subset in the underlying wood grain printing data set on a two-dimensional plane. Therefore, only after determining the plane wood grain coordinate information recorded in the underlying wood grain printing shape data subset and the three-dimensional wood grain printing coordinate data recorded in the three-dimensional wood grain printing shape data subset, the second printing device can output and print along a predetermined printing route, thereby completing the alignment process between the three-dimensional wood grain and the underlying wood grain layer. Preferably, the three-dimensional wood grain printing shape data subset includes printing depth data of each three-dimensional wood grain printing coordinate data. Preferably, in the step (S.1), the wood grain information processing includes at least one of the following operations: Geometric transformations, correction of color and / or brightness and / or contrast, removal of unwanted image elements, image skewing, image distortion. Preferably, the board material includes a wood-plastic board, a stone-plastic board, a wooden board, a metal board or other types of man-made board materials. Preferably, after step (S.4), the following steps are also included: The step of solidifying the wood grain precursor forms a three-dimensional wood grain layer on the surface of the bottom wood grain layer. As described in the background technology, there are many methods for preparing a three-dimensional wood grain layer. In some preferred embodiments of the application, a three-dimensional wood grain layer can be formed on the surface of the bottom wood grain layer by stacking upward. In this way, the curable wood grain precursor liquid can be continuously stacked upward to form a wood grain precursor with different depths, lengths and widths. At this time, it is only necessary to cure the wood grain precursor, and the cured wood grain precursor can become a three-dimensional wood grain layer. The curing method of the wood grain precursor depends on the physicochemical properties of the applied wood grain precursor liquid. If the wood grain precursor liquid contains a thermosetting resin, the wood grain precursor can be cured by a thermosetting method during the curing process. If the wood grain precursor liquid contains a photocatalytic resin, it is only necessary to irradiate the wood grain precursor with ultraviolet light under the condition of the presence of a photoinitiator to initiate the curing of the wood grain precursor. Generally speaking, the light curing method has a higher curing efficiency, which can effectively improve the molding efficiency of the three-dimensional wood grain layer. Preferably, the wood grain precursor comprises at least a photocatalytic resin; and Photoinitiators used to initiate the polymerization of photocatalytic resins. Preferably, the photocatalytic resin contained in the wood grain precursor liquid includes acrylic resin, epoxy resin or other photocurable resin. Preferably, an intermediate step is included between step (S.3) and step (S.4), and the intermediate step includes: - applying a curable liquid resin on the bottom wood grain layer by means of a coating tool, thereby forming a liquid resin layer; In the step (S.4), the wood grain precursor liquid is applied to the upper surface of the liquid resin layer, so that the wood grain precursor liquid and / or at least a portion of the liquid resin mixed with the wood grain precursor liquid and / or at least a portion of the liquid resin covered by the wood grain precursor liquid forms a wood grain precursor. Preferably, the wood grain precursor liquid at least contains an inhibitor for preventing or delaying polymerization of the curable liquid resin. Preferably, after step (S.4), the following steps are also included: - a step of curing the liquid resin except the wood grain precursor formed in the previous step; - A step of removing the wood grain precursor, thereby forming a three-dimensional wood grain layer on the surface of the underlying wood grain layer. As mentioned above, the formation of the three-dimensional wood grain layer includes not only the upward stacking method mentioned above, but also the downward indentation method. Compared with the upward stacking method, the downward indentation method has a controllable width of the texture and a longer depth, so it has a stronger three-dimensional sense. At the same time, there will be no wood grain deformation during the printing process, so the printing accuracy is higher. The prior art has adopted the step of applying a wood grain precursor liquid to an incompletely cured resin layer. However, from the actual test results, due to the high viscosity of the incompletely cured resin layer itself, it is difficult for the wood grain precursor liquid to enter the resin layer. This brings about the following problems: (1) The depth of the wood grain precursor liquid entering the resin layer is low, resulting in a low depth of the final wood grain, making the three-dimensional effect of the overall three-dimensional wood grain layer poor; (2) Due to the high viscosity of the incompletely cured resin layer, the wood grain precursor liquid is more likely to accumulate on the surface of the incompletely cured resin layer after application, making it easier for the wood grain precursor liquid to diffuse on the surface of the resin layer, making it difficult for the shape and width of the final wood grain to match the underlying wood grain layer, thereby causing the problem of misalignment; (3) The incompletely cured resin layer has weak fluidity, so it is difficult to blend with the wood grain precursor liquid in a short period of time, resulting in the formation of The edges of the three-dimensional wood grain layer are more blurred and less sharp, which is significantly different from the structure of natural wood grain; (4) Since the viscosity of the incompletely cured resin layer is relatively high, even after it is mixed with the wood grain precursor liquid, the viscosity of the obtained wood grain precursor is also relatively high. Although the wood grain precursor cannot be completely cured in the subsequent curing process, its viscosity can still be improved to a certain extent. Therefore, these high-viscosity wood grain precursors are difficult to be removed in the subsequent mechanical removal process, so there is often a certain amount of residue, which further leads to the problem of unclear and blurred texture of the wood grain, which further widens the gap between its texture and the actual natural wood material. Therefore, in addition to adopting a pretreatment step in the preparation process, the present invention also adopts a technical solution of applying the wood grain precursor liquid directly to the surface of the uncured liquid resin during the pretreatment step. Compared with applying the wood grain precursor liquid to the semi-cured resin layer, changing this step can bring the following beneficial effects: (1) Since the uncured liquid resin itself has a low viscosity, it has good fluidity. After the wood grain precursor liquid is applied to the uncured liquid resin, it can smoothly enter the uncured liquid resin downward, thereby greatly improving the depth of the prepared wood grain and effectively improving the three-dimensional effect of the three-dimensional wood grain layer. (2) At the same time, since the wood grain precursor liquid can penetrate into the uncured liquid resin, the wood grain precursor liquid is prevented from diffusing on the surface of the uncured liquid resin, so that the shape and width of the wood grain finally formed can match the ink layer below, thereby effectively improving the accuracy of the pattern. (3) Since the uncured liquid resin and the wood grain precursor liquid have a good mixing effect, the wood grain precursor liquid or the wood grain precursor liquid mixed with the uncured liquid resin has a more neat and sharp edge, so the prepared three-dimensional wood grain layer is closer to the natural wood grain. (4) Since the wood grain precursor liquid or the wood grain precursor liquid mixed with the uncured liquid resin still has a low viscosity after curing, it is easier to remove after curing, and no residue will be left after removing the wood grain precursor, so the formed wood grain is cleaner and has sharper edges. Preferably, after step (S.3), a pretreatment step is also performed, and the pretreatment step comprises: The step of covering at least a portion of the surface above the bottom wood grain layer with a curable liquid resin and curing at least a portion of the curable liquid resin on the surface of the bottom wood grain layer to form a three-dimensional wood grain bottom layer. In the process of forming three-dimensional wood grain using the conventional downward indentation method, a portion of the underlying wood grain layer is exposed during the process of removing the wood grain precursor to obtain the three-dimensional wood grain layer. This exposed underlying wood grain layer is easily worn or even peeled off by external forces. Therefore, in the process of mechanically removing the wood grain precursor, the depth of downward removal needs to be considered to prevent the wear of the underlying wood grain layer, which makes it difficult to increase the depth of the three-dimensional wood grain layer. In the process of preparing the three-dimensional structure, the present invention first covers the surface of the bottom wood grain layer with a three-dimensional wood grain bottom layer obtained by curing a curable liquid resin, and then forms a three-dimensional wood grain layer again on the surface of the three-dimensional wood grain bottom layer. Due to the existence of the three-dimensional wood grain bottom layer, in the process of removing the wood grain precursor and forming the three-dimensional wood grain layer, the bottom wood grain layer will not be exposed to the outside, but will be covered by the three-dimensional wood grain bottom layer, so that the bottom wood grain layer will not be worn or peeled off due to the action of external force. Therefore, in the process of mechanically removing the wood grain precursor, it is possible to dig downward to the maximum extent, thereby ensuring that the depth of the three-dimensional wood grain layer can be effectively increased. In addition, in order to make the board containing three-dimensional wood grain prepared by the present invention obtain a texture similar to that of natural wood, in addition to considering the wear of the bottom wood grain layer and the depth of the three-dimensional wood grain layer, it is also necessary to consider the correspondence between the bottom wood grain layer and the upper three-dimensional wood grain layer, that is, the alignment problem between the two. Regarding the alignment problem, the applicant found that the following influencing factors will cause the alignment defect between the bottom wood grain layer and the upper three-dimensional wood grain layer: (1) During the preparation of the upper three-dimensional wood grain layer, the three-dimensional wood grain layer or the bottom wood grain layer is deformed due to the shrinkage of the curable liquid resin material itself during the curing process; (2) During the preparation of the three-dimensional wood grain layer, the compatibility between the wood grain precursor liquid and the curable liquid resin is insufficient, resulting in the depth, width and edge morphology of the three-dimensional wood grain layer not meeting expectations. The applicant found that only after considering the above two factors at the same time can a texture similar to that of natural wood be truly obtained. Regarding the influencing factor (1), the applicant has found that during the curing process of the curable liquid resin, since the energy (UV or heat) used to cure the curable liquid resin is usually input from the top of the liquid resin, the liquid resin at the top will be cured first, while the liquid resin at the bottom will be cured later. Since the liquid resin is often accompanied by a certain volume shrinkage during the curing process, a certain internal stress will be generated. These internal stresses will be superimposed downward, so that a maximum value will be reached at the bottom of the liquid resin. If the liquid resin is directly in contact with the bottom wood grain layer at this time, once the maximum internal stress is greater than the bonding force between the bottom wood grain layer and the surface of the board, it will cause the bottom wood grain layer and the surface of the board to slip, and then make it difficult for the bottom wood grain layer at the bottom to correspond to the three-dimensional wood grain at the top, thereby causing the problem of misalignment, which seriously affects the visual effect of the board. In addition, when the amount of liquid resin applied on the bottom wood grain layer is large, the bottom wood grain layer and the surface of the board may even peel off, which seriously reduces the yield rate of the product. Therefore, in order to overcome the above problems, the present invention first covers at least a portion of the surface of the bottom wood grain layer with liquid resin and solidifies this portion of liquid resin to form a wood grain bottom layer. Since the amount of this portion of liquid resin is small at this time, the internal stress generated after solidification is weak and will not affect the bottom wood grain layer and the surface of the board. Since the liquid resin used to form the three-dimensional wood grain layer is further covered on the wood grain bottom layer and solidified to obtain the three-dimensional wood grain layer, the affinity and bonding force between the wood grain bottom layer and the three-dimensional wood grain layer are strong, so there will be no slippage and peeling problems between the two. And because the wood grain bottom layer has a high mechanical strength after solidification, the internal stress generated by the three-dimensional wood grain layer during solidification is not enough to cause the wood grain bottom layer to deform, and the internal stress generated by the three-dimensional wood grain layer during solidification will not be transferred to the bottom wood grain layer located below the wood grain bottom layer. Therefore, by adding this pretreatment step, it is possible to effectively prevent the problem of misalignment between the three-dimensional wood grain layer and the bottom wood grain layer in the subsequent production process. Preferably, the curing method of the curable liquid resin includes thermal curing or light curing. Preferably, when the curing method of the curable liquid resin is thermal curing, the liquid resin at least includes a thermosetting resin. Preferably, the thermosetting resin includes one or more combinations of epoxy resin, phenolic resin, melamine formaldehyde resin, furan resin, unsaturated polyester resin, silicone resin, and polybutadiene resin. Preferably, the resin solution further includes a curing agent. Preferably, when the curing method of the curable liquid resin is photocuring, the liquid resin at least includes a photocrosslinking resin and a photoinitiator. In another preferred embodiment of the present invention, the photo-crosslinking resin includes any one or more combinations of unsaturated polyester, epoxy resin, acrylic resin, acrylic modified polyurethane resin, acrylic modified silicone resin, acrylic modified epoxy resin, water-based epoxy acrylate, water-based polyurethane acrylate, and water-based polyester acrylate. In another preferred embodiment of the present invention, the photoinitiator includes any one of a free radical polymerization initiator, a cationic polymerization initiator, an energy transfer initiator, and an ion reaction initiator. Preferably, after preparing the three-dimensional wood grain layer, the method further comprises: The step of covering at least a portion of the surface of the three-dimensional wood grain layer with a topcoat and curing the topcoat layer. Preferably, before the step (S.3), the plate further comprises the following steps: The step of covering at least a portion of the surface of the board with a primer and curing it to obtain a primer layer. In a second aspect, the present invention provides a board having three-dimensional wood grain on its surface, which is prepared by the method as described above. In a third aspect, the present invention further provides the use of a board having three-dimensional wood grain on the surface as above in a floor, a decorative wall panel or a ceiling panel. The present invention has the following beneficial effects: The present invention obtains a surface database of natural wood by scanning real natural wood, and further classifies and processes these surface databases, thereby further obtaining a bottom wood grain printing data set for forming a bottom wood grain layer whose base color and pattern match the natural wood grain, and a three-dimensional wood grain printing data set for forming a three-dimensional wood grain with the same feel as the natural wood grain. Through the corresponding matching relationship between the bottom wood grain printing data set and the three-dimensional wood grain printing data set, a three-dimensional wood grain layer that completely corresponds to the bottom wood grain layer can be obtained on the surface of the board, thereby effectively improving the accuracy of the pattern between the two. At the same time, because the present application processes different shapes, colors, and depth information separately, it simplifies the preparation process of the three-dimensional wood grain layer and improves production efficiency. BRIEF DESCRIPTION OF THE DRAWINGS FIG. 1 is a schematic diagram showing a typical structure of natural wood. FIG. 2 shows image data matched to a scanned natural wood image. FIG. 3 is a schematic reproduction diagram of step (S.1) to step (S.11) in Example 1. FIG. 4 is a schematic reproduction diagram of step (S.12) to step (S.13) in Example 1. FIG. 5 is a schematic diagram of the three-dimensional structure of the board with three-dimensional wood grain prepared in Example 1. FIG. FIG. 6 is a schematic diagram of the top view of the board with three-dimensional wood grain prepared in Example 1. FIG. FIG. 7 is a schematic reproduction diagram of step (S.1) to step (S.9) in Example 2. Wherein: board material 10, primer layer 11, color paint layer 12, bottom wood grain layer 13, three-dimensional wood grain bottom layer 14, liquid resin layer 15, wood grain precursor 16, three-dimensional wood grain layer 17, first topcoat layer 18, second topcoat layer 19, conveying equipment 20, first roller coater 21, second roller coater 22, first printing equipment 23, third roller coater 24, fourth roller coater 25, fifth roller coater 26, second printing equipment 27, cleaning device 28, sixth roller coater 29, seventh roller coater 30, wood surface database 100, bottom wood grain printing data set 110, bottom wood grain printing background color data subset 110a, bottom wood grain printing shape data subset 110b, three-dimensional wood grain printing data set 120, three-dimensional wood grain printing shape data subset 120a, three-dimensional wood grain printing depth data subset 120b. DETAILED DESCRIPTION The present invention is further described below in conjunction with the accompanying drawings and specific embodiments of the specification. Those of ordinary skill in the art will be able to implement the present invention based on these descriptions. In addition, the embodiments of the present invention involved in the following description are generally only embodiments of a part of the present invention, rather than all embodiments. Therefore, based on the embodiments of the present invention, all other embodiments obtained by those of ordinary skill in the art without making creative work should fall within the scope of protection of the present invention. In the first embodiment of the present invention, a plurality of different natural woods are first scanned by a scanner (FIG. 1 is a typical structural schematic diagram of natural wood), so as to obtain wood grain information of various natural woods, wherein the wood grain information includes image data of wood grain and three-dimensional depth information of wood grain, and the image data includes background color images displayed by various woods and wood grain shape images that can be displayed on the surface of various woods. Among them, the background color image usually includes the background color that various natural woods can present themselves, for example, the background color images of common natural woods generally include but are not limited to: the background color of fir and spruce is slightly yellow; the background color of basswood, white sauerkraut, yellow tung and other woods is yellow-white; the background color of locust, pistachio, catalpa, mulberry is brown; the background color of redwood, red pine, cryptomeria, camphor and other woods is reddish brown; the background color of red sandalwood, Indian yellow sandalwood, Indian rosewood is dark purple-red; the background color of ebony is black. For example, the shape image of wood grain of common natural wood includes but is not limited to: closed, semi-closed or fully open annual ring texture, semi-ring hole structure, strip structure, corrugated structure, burl texture and other structures. The above-obtained background image and wood grain shape image are processed by image processing software, for example, color and / or brightness and / or contrast correction is performed on the background image, and at least one of the following operations such as geometric transformation, removal of unnecessary image elements, image skew and image distortion is performed on the wood grain shape image, and then the processed wood grain information is analyzed to extract and establish the wood surface database 100. As shown in FIG. 2 , the data in the wood surface database 100 in this embodiment can be divided into at least a bottom wood grain printing data set 110 and a three-dimensional wood grain printing data set 120 . The bottom wood grain print data set 110 is used to record the bottom color information of the wood surface and the shape information of the wood grain on the wood surface. Therefore, in some embodiments, the bottom wood grain print data set 110 can be further classified to divide the bottom wood grain print data set 110 into a plurality of bottom wood grain print bottom color data subsets 110a and a plurality of bottom wood grain print shape data subsets 110b. The bottom wood grain printing background color data subset 110a may include a plurality of background color printing point coordinate data (X, Y), each of which is marked with color information matching the different colors of the wood grain pattern. The color information constituting the background color is obtained by superimposing at least one or more standard colors. The bottom layer wood grain printing shape data subset 110b includes multiple sets of multiple two-dimensional plane wood grain printing coordinate data for printing wood grain, and each plane wood grain printing coordinate data is marked with color information. The color information constituting the wood grain is also obtained by superimposing at least one or more standard colors, and the color information constituting the wood grain can be distinguished from the color information constituting the background color, so that the shape of the bottom layer wood grain can be displayed on the background color. After determining the plane wood grain printing coordinate data, each bottom layer wood grain printing shape data subset 110b can correspond to a bottom layer wood grain printing route. In some preferred embodiments, the standard colors constituting the background color and the wood grain color are at least a series of colors such as red, blue, light red, yellow, black, and light black, which are presented separately or multiple standard colors are superimposed on each other. As an example, these standard colors and their corresponding RGB values are shown in Table 1 below:
[0090] In order to output colored ink on the surface of the board material, thereby forming an underlying wood grain layer that matches the wood grain pattern, in this embodiment, we assign the underlying wood grain printing background color data subset 110a and the underlying wood grain printing shape data subset 110b to the first printing device 200, so that the first printing device 200 prints on the board material surface based on the background color printing point coordinate data and the color information corresponding to the background color printing point coordinate data recorded in the underlying wood grain printing background color data subset 110a, thereby outputting colored ink for forming the required background color on the board material surface, thereby forming the background color. After the base color printing is completed, the first printing device 200 uses the multiple groups of plane wood grain printing coordinate data for printing wood grain recorded in the bottom wood grain printing shape data subset 110b and the color information corresponding to the plane wood grain printing coordinate data to print on the base color surface according to the bottom wood grain printing route corresponding to each bottom wood grain printing shape data subset 110b, thereby outputting the colored ink for forming the wood grain shape on the base color surface and forming the wood grain shape. After the base color and the wood grain shape are printed, the base color and the wood grain shape are superimposed on each other to form a bottom wood grain layer that matches the target wood grain pattern. In order to ensure the clarity of the entire bottom wood grain layer after printing, the first printing device 200 needs to maintain a printing resolution greater than or equal to 100 DPI during the process of printing the plane wood grain printing coordinate data for forming the base color and the plane wood grain printing coordinate data for forming the wood grain shape. The color ink used in the first printing device 200 is preferably a photocurable ink, and the formed bottom wood grain layer is photocured after printing, so as to maintain the stability and wear resistance of the bottom wood grain layer. In order to ensure the photocurable performance of the color ink, in this embodiment, the color ink must include a photocurable resin, a photoinitiator for initiating the curing of the photocurable resin, and pigments for providing different colors. In addition, since the source of the board used in this embodiment can be wood-plastic board, stone-plastic board, wood board, metal board or other types of boards, and since the colors of various boards themselves are different, after the bottom wood grain layer is printed on the surface of different boards, the color of the board itself will cause a certain deviation in the color of the bottom wood grain layer. Therefore, in some preferred embodiments of the present application, it is necessary to first perform a certain surface modification treatment on the board. The surface modification of the board includes the following steps: The SPC board is first coated with a layer of curable primer (for example, the primer may contain: 90% light-curing varnish HYS01-1, 5% photoinitiator 184, 0.5% photoinitiator TPO, 4.5% diluent hydroxyethyl acrylate), and 12g / m 2 The primer is applied to the surface of the SPC sheet using 395nm and 8W / cm 2 The primer is cured by a UV lamp to form a primer layer. The SPC sheet obtained in the previous step is passed through a roller coater, the roller surface of which is coated with a light-curable white paint (for example, the white paint contains: 50% light-curable epoxy HYS01-1, 30% titanium dioxide, 5% photoinitiator 184, 0.5% photoinitiator TPO, 14.5% diluent hydroxyethyl acrylate). During the contact between the SPC sheet and the coating roller, 18g / m 2 The white paint is applied on the surface of the primer, and the 2 After curing with UV lamp, a white paint layer is obtained. The first printing device 200 outputs on the surface of the white paint layer, thereby forming an underlying wood grain layer on the surface of the paint layer to cover up the influence of the color of the SPC board itself on the underlying wood grain layer. 2, the three-dimensional wood grain printing data set 120 is used to record the shape information of the three-dimensional wood grain on the wood surface and the different depth information of the three-dimensional wood grain. Therefore, in some embodiments, the three-dimensional wood grain printing data set 120 can be classified, so that the three-dimensional wood grain printing data set 120 is divided into a plurality of two-dimensional three-dimensional wood grain printing shape data subsets 120a and a plurality of three-dimensional wood grain printing depth data subsets 120b. The 3D wood grain printing shape data subset 120a includes a plurality of 3D wood grain printing coordinate data for printing wood grain, and each 3D wood grain printing shape data subset 120a corresponds to a 3D wood grain printing route. The 3D wood grain printing depth data subset 120b includes the printing depth data of each 3D printing point coordinate data. In order to form three-dimensional wood grain on the surface of the underlying wood grain layer that is compatible with the wood grain shape in the underlying wood grain layer, in this embodiment, the three-dimensional wood grain printing shape data subset 120a and multiple three-dimensional wood grain printing depth data subsets 120b in the three-dimensional wood grain printing data set 120 are respectively allocated to the second printing device 300, thereby forming three-dimensional wood grain during the printing process of the second printing device 300. As described in the background art, there are various methods for forming three-dimensional wood grain, so the method of printing three-dimensional wood grain using the second printing device 300 also needs to be explained separately. The steps of a preferred embodiment of the three-dimensional wood grain formed by the upward stacking method are as follows: (1) Preparation of wood grain precursor liquid: In this embodiment, since the wood grain precursor liquid needs to be stacked upward to form three-dimensional wood grain, the wood grain precursor liquid used must include at least a curable resin and a photoinitiator (as an example, the wood grain precursor liquid used in the upward stacking method may include 90% Dow Corning 65 Additive, 5% photoinitiator 184, 0.5% photoinitiator TPO, and 4.5% diluent hydroxyethyl acrylate). (2) The second printing device 300 prints on the surface of the bottom wood grain layer according to the three-dimensional printing point coordinate data corresponding to the three-dimensional wood grain printing shape data subset 120a and the three-dimensional wood grain printing route corresponding to each three-dimensional wood grain printing shape data subset 120a, thereby outputting wood grain precursor liquid on the bottom color surface. The height of the wood grain precursor liquid can be controlled by the second printing device 300 using the three-dimensional wood grain printing depth data subset 120b, so that the wood grain precursor is finally formed in the process of the wood grain precursor liquid being continuously piled up. In this embodiment, the three-dimensional wood grain printing routes corresponding to the three-dimensional wood grain printing shape data subset 120a overlap with the multiple bottom wood grain printing routes on the two-dimensional plane, thereby completing the alignment between the three-dimensional wood grain and the bottom wood grain. (3) The wood grain precursor was sequentially subjected to 395nm and 8W / cm 2 UV lamp and 160w / cm 2 The Hg lamp irradiates the liquid wood grain precursor to transform into a solidified three-dimensional wood grain layer. The steps of a preferred embodiment of the three-dimensional wood grain formed by the downward indentation method are as follows: (1) Preparation of wood grain precursor liquid: In this embodiment, since the wood grain precursor liquid needs to penetrate downward into the liquid resin layer to form a three-dimensional wood grain, the wood grain precursor liquid used must at least include an inhibitor that hinders or delays the polymerization of the resin liquid layer (as an example, the wood grain precursor liquid used in the upward stacking method contains: 45.5% diacrylate monomer PEG600DA, 20.5% p-hydroxyanisole HQMME, 10% 2-tert-butylhydroquinone MTBHQ, and 24% diethylene glycol butyl ether). (2) With the help of a coating tool, apply a curable liquid resin on top of the bottom wood grain layer. The coating amount of the curable liquid resin can be 50~200g / m 2 When the coating amount of the cured liquid resin is greater than 150g / m 2 When the coating is performed in batches, the liquid resin layer can be formed. (3) The second printing device 300 prints on the surface of the liquid resin layer according to the three-dimensional wood grain printing coordinate data corresponding to the three-dimensional wood grain printing shape data subset 120a and the three-dimensional wood grain printing route corresponding to each three-dimensional wood grain printing shape data subset 120a, thereby outputting the wood grain precursor liquid on the surface of the liquid resin layer. The depth of the wood grain precursor liquid can be controlled by the second printing device 300 using the three-dimensional wood grain printing depth data subset 120b, so that the wood grain precursor liquid and / or at least a portion of the liquid resin mixed with the wood grain precursor liquid and / or at least a portion of the liquid resin covered by the wood grain precursor liquid forms a wood grain precursor. In this embodiment, the three-dimensional wood grain printing routes corresponding to the three-dimensional wood grain printing shape data subset 120a overlap with the multiple bottom wood grain printing routes on the two-dimensional plane, thereby completing the alignment between the three-dimensional wood grain and the bottom wood grain. (4) The liquid resin layer on the surface of the SPC sheet obtained in the previous step was subjected to 395nm and 8W / cm 2 UV lamp and 160w / cm 2 The SPC board is irradiated with a Hg lamp for deep curing, and then the obtained SPC board is conveyed to a cleaning device including a steel brush, so that the wood grain precursor is brushed out by the steel brush, thereby forming a three-dimensional wood grain layer. In some preferred embodiments, in order to improve the wear resistance and scratch resistance of the bottom wood grain layer and make the three-dimensional wood grain layer have better three-dimensional effect and visual effect, a pretreatment step is also performed after obtaining the bottom wood grain layer, and the pretreatment step includes: The step of covering at least a portion of the surface above the bottom wood grain layer with a curable liquid resin and curing it. The amount of the resin liquid applied by roller is about 45g / m 2The photocurable resin liquid (the resin liquid contains: 90% Dow Corning 65 Additive, 5% photoinitiator 184, 0.5% photoinitiator TPO, 4.5% diluent hydroxyethyl acrylate) was sequentially subjected to 395nm and 8W / cm 2 UV lamp and 160w / cm 2 After being cured by Hg lamp, a wood grain bottom layer is formed. Then, a three-dimensional wood grain layer is formed on the top of the wood grain bottom layer. In some preferred embodiments, in order to improve the touch feel of the board and adjust the optical properties, after preparing the three-dimensional wood grain layer, it is necessary to continue to apply at least one layer of topcoat on the surface of the three-dimensional wood grain layer and solidify it to obtain the topcoat layer. Example 1 As shown in FIG3 , a method for manufacturing a board having a three-dimensional wood grain on the surface includes the following steps: (S.1) placing an SPC sheet 10 with a length, width and thickness of 1260 mm*970 mm*4.85 mm on the surface of a conveying device 20 moving in a fixed direction; (S.2) During the conveying process, the SPC sheet 10 first passes through the first roller coater 21. The coating roller surface of the roller coater is adhered with a photocurable primer (the primer contains: 90% photocurable varnish HYS01-1, 5% photoinitiator 184, 0.5% photoinitiator TPO, 4.5% diluent hydroxyethyl acrylate). When the SPC sheet 10 is in contact with the coating roller, 12g / m 2 The primer is applied to the surface of SPC sheet 10, and the surface is heated by 395nm and 8W / cm 2 The primer is cured by a UV lamp to form a primer layer 11; (S.3) The SPC sheet 10 obtained in the previous step is passed through a second roller coater 22. The coating roller surface of the roller coater is adhered with a light-curable white paint (the white paint contains: 50% light-curable epoxy HYS01-1, 30% titanium dioxide, 5% photoinitiator 184, 0.5% photoinitiator TPO, 14.5% diluent hydroxyethyl acrylate). When the SPC sheet 10 is in contact with the coating roller, 18g / m 2 The white paint is applied on the surface of the primer layer 11, and the white paint is heated by 395nm and 8W / cm 2 After curing with a UV lamp, a white paint layer 12 is obtained; (S.4) The SPC board 10 obtained in the previous step is conveyed to the first printing device 23, and the first printing device 50 calls the bottom wood grain printing bottom wood grain printing base color data subset 110a and the bottom wood grain printing shape data subset 110b in the bottom wood grain printing data set 110, so as to spray 6-8 g / m2 of the paint layer 12 through the first printing device 50.2 The ink is cured to form a bottom wood grain layer 13 matching the wood grain information on the surface of the primer layer 11; (S.5) The SPC board 10 obtained in the previous step is conveyed to the third roller coating machine 24, and the surface of the bottom wood grain layer 13 is coated with 45g / m 2 The photocurable resin liquid (the resin liquid contains: 90% Dow Corning 65 Additive, 5% photoinitiator 184, 0.5% photoinitiator TPO, 4.5% diluent hydroxyethyl acrylate) was sequentially subjected to 395nm and 8W / cm 2 UV lamp and 160w / cm 2 After being irradiated and cured by a Hg lamp, a three-dimensional wood grain bottom layer 14 is formed; (S.6) The SPC sheet 10 obtained in the previous step is conveyed to the fourth roller coater 25, so that the coating roller of the fourth roller coater is rolled along the conveying direction of the SPC sheet 10 (the roller rotates clockwise) to coat 80g / m 2 Resin liquid (resin liquid contains: 90% Dow Corning 65 Additive, 5% photoinitiator 184, 0.5% photoinitiator TPO, 4.5% diluent hydroxyethyl acrylate); (S.7) After coating the first layer of the resin liquid, the SPC sheet 10 is conveyed forward along the surface of the conveying device 20, and it is ensured that the fourth roller coater 80 does not apply any force to the resin liquid before conveying to the next roller coater; (S.8) The SPC sheet 10 obtained in the previous step is conveyed to the fifth roller coater 26, so that the coating roller of the fifth roller coater 90 continues to roll-coat 75g / m against the conveying direction of the SPC sheet 10 (the roller itself rotates in a clockwise direction). 2 of resin liquid, thereby obtaining a liquid resin layer 15; (S.9) The SPC board 10 obtained in the previous step is conveyed to the second printing device 27. The second printing device 27 calls the three-dimensional wood grain printing shape data subset 120a and the three-dimensional wood grain printing depth data subset 120b in the three-dimensional wood grain printing data set 120, so as to spray 6-8 g / m 2 The wood grain precursor liquid (the wood grain precursor liquid contains: 45.5% diacrylate monomer PEG600DA, 20.5% p-hydroxyanisole HQMME, 10% 2-tert-butylhydroquinone MTBHQ, 24% diethylene glycol butyl ether), and the wood grain precursor liquid penetrates downward into the liquid resin layer 15 and mixes with the curable liquid resin to form a wood grain precursor 16, and the depth change of the wood grain precursor 16 corresponds to the three-dimensional wood grain printing depth data subset 120b; (S.10) The liquid resin on the surface of the SPC board 10 obtained in the previous step, except for the wood grain precursor 16, is sequentially subjected to 395nm and 8W / cm 2 UV lamp and 160w / cm 2 Hg lamp irradiation for deep curing; (S.11) The SPC board 10 obtained in the previous step is conveyed to a cleaning device 28 including a steel brush, so that the wood grain precursor 16 is brushed out by the steel brush, thereby forming a three-dimensional wood grain layer 17; As shown in FIG. 4 , after the three-dimensional wood grain layer 17 is prepared, the following steps are further performed: (S.12) The SPC sheet 10 obtained in the previous step is passed through the sixth roller coater 29 and 395nm and 8W / cm 2 UV lamp, thus coating the surface of the three-dimensional wood grain layer with 12g / m 2 A first topcoat is formed and cured to obtain a first topcoat layer 18; (S.13) The SPC sheet 10 obtained in the previous step is passed through the seventh roller coater 30 and 395nm and 8W / cm 2 UV lamp, thereby coating the surface of the first topcoat layer 17 with 12g / m 2 The second topcoat is applied and cured to obtain a second topcoat layer 19. The plate material 10 with a three-dimensional structure on the surface prepared in Example 1 was analyzed by laser profilometer analysis to obtain Figures 5 and 6, wherein: Figure 5 is a schematic diagram of the three-dimensional structure of the three-dimensional wood grain, and Figure 6 is a schematic diagram of the top view structure of the three-dimensional wood grain. Example 2 As shown in FIG. 7 , a method for manufacturing a board having a three-dimensional wood grain on the surface includes the following steps: (S.1) placing an SPC sheet 10 with a length, width and thickness of 1260 mm*970 mm*4.85 mm on the surface of a conveying device 20 moving in a fixed direction; (S.2) During the conveying process, the SPC sheet 10 first passes through the first roller coater 21. The coating roller surface of the roller coater is adhered with a photocurable primer (the primer contains: 90% photocurable varnish HYS01-1, 5% photoinitiator 184, 0.5% photoinitiator TPO, 4.5% diluent hydroxyethyl acrylate). When the SPC sheet 10 is in contact with the coating roller, 12g / m 2 The primer is applied to the surface of SPC sheet 10, and the surface is heated by 395nm and 8W / cm 2 The primer is cured by a UV lamp to form a primer layer 11; (S.3) The SPC sheet 10 obtained in the previous step is passed through a second roller coater 22. The coating roller surface of the roller coater is adhered with a light-curable white paint (the white paint contains: 50% light-curable epoxy HYS01-1, 30% titanium dioxide, 5% photoinitiator 184, 0.5% photoinitiator TPO, 14.5% diluent hydroxyethyl acrylate). When the SPC sheet 10 is in contact with the coating roller, 18g / m 2 The white paint is applied on the surface of the primer layer 11, and the white paint is heated by 395nm and 8W / cm 2 After curing with a UV lamp, a white paint layer 12 is obtained; (S.4) The SPC board 10 obtained in the previous step is conveyed to the first printing device 23, and the first printing device 50 calls the bottom wood grain printing bottom wood grain printing base color data subset 110a and the bottom wood grain printing shape data subset 110b in the bottom wood grain printing data set 110, so as to spray 6-8 g / m2 of the paint layer 12 through the first printing device 50. 2 The ink is cured to form a bottom wood grain layer 13 matching the wood grain information on the surface of the primer layer 11; (S.5) The SPC board 10 obtained in the previous step is conveyed to the third roller coating machine 24, and the surface of the bottom wood grain layer 13 is coated with 45g / m 2 The photocurable resin liquid (the resin liquid contains: 90% Dow Corning 65 Additive, 5% photoinitiator 184, 0.5% photoinitiator TPO, 4.5% diluent hydroxyethyl acrylate) was sequentially subjected to 395nm and 8W / cm 2 UV lamp and 160w / cm 2 After being irradiated and cured by a Hg lamp, a three-dimensional wood grain bottom layer 14 is formed; (S.6) The SPC board 10 containing the three-dimensional wood grain bottom layer 14 obtained in the previous step is conveyed to the second printing device 27. The second printing device 27 calls the three-dimensional wood grain printing shape data subset 120a and the three-dimensional wood grain printing depth data subset 120b in the three-dimensional wood grain printing data set 120, so as to spray 6-8 g / m 2 A wood grain precursor liquid (the wood grain precursor liquid contains: 90% Dow Corning 65 Additive, 5% photoinitiator 184, 0.5% photoinitiator TPO, 4.5% diluent hydroxyethyl acrylate) is used to form a wood grain precursor 16, and the depth variation of the wood grain precursor 16 corresponds to the three-dimensional wood grain printing depth data subset 120b; (S.7) The wood grain precursor 16 on the surface of the SPC board 10 obtained in the previous step was subjected to 395nm and 8W / cm 2UV lamp and 160w / cm 2 The Hg lamp is irradiated to achieve deep curing, thereby forming a three-dimensional wood grain layer 17; (S.8) The SPC sheet 10 obtained in the previous step is passed through the sixth roller coater 29 and 395nm and 8W / cm 2 The UV lamp 30 is used to coat the surface of the three-dimensional wood grain layer 17 with 12 g / m 2 A first topcoat is formed and cured to obtain a first topcoat layer 18; (S.9) The SPC sheet 10 obtained in the previous step is passed through the seventh roller coater 30 and 395nm and 8W / cm 2 UV lamp 31 is used to coat 12g / m 2 The second topcoat is applied and cured to obtain a second topcoat layer 19. In summary, through the method described in the present application, a three-dimensional wood grain similar to that of a natural wood board can be obtained on the surface of an artificial or non-wood board, and by digitizing the wood grain information, the bottom wood grain layer and the three-dimensional wood grain above the bottom wood grain layer can be strictly matched during printing, thereby overcoming the problem of difficulty in "matching patterns" in the prior art. At the same time, based on the above principles, this method in the present application also has the advantage of high flexibility. Compared with the prior art, the three-dimensional wood grain in the present application does not require three-dimensional modeling of a single underlying wood grain layer. It only needs to analyze the wood grain shape contained in the underlying wood grain layer, and obtain it by retrieving it from the three-dimensional wood grain printing shape data subset of the three-dimensional wood grain printing data set, and match the shape data recorded in the three-dimensional wood grain printing shape data subset with the depth data recorded in the three-dimensional wood grain printing depth data subset, thereby creating a three-dimensional wood grain that is closer to natural wood grain, thereby effectively simplifying the construction process of the three-dimensional wood grain, so that customized production of products can be carried out according to customer needs, expanding the richness of the company's product line, effectively reducing production costs and improving production efficiency.
Claims
1. A method for manufacturing a board having a three-dimensional wood grain on the surface, characterized in that: It includes at least the following steps: (S.1) obtaining wood grain information and processing it to extract a wood surface database; The database includes at least a bottom wood grain printing data set and a three-dimensional wood grain printing data set; The three-dimensional wood grain printing data set includes a two-dimensional three-dimensional wood grain printing shape data subset corresponding to the bottom wood grain printing data set and a three-dimensional wood grain printing depth data subset corresponding to the three-dimensional wood grain printing shape data subset; (S.2) assigning a bottom wood grain print data set to a first printing device; assigning the three-dimensional wood grain printing data set to a second printing device; (S.3) using the first printing device to output the bottom wood grain printing data set on the surface of the board to obtain a bottom wood grain layer that matches the wood grain information; (S.4) Using the second printing device and the three-dimensional wood grain printing data set to output a wood grain precursor liquid to obtain a wood grain precursor for forming three-dimensional wood grain and matching the underlying wood grain layer, and the height of the wood grain precursor corresponds to different three-dimensional wood grain printing depth data subsets.
2. The method according to claim 1, characterized in that The bottom layer wood grain printing data set includes a plurality of bottom layer wood grain printing base color data subsets and a plurality of bottom layer wood grain printing shape data subsets.
3. The method according to claim 2, characterized in that The bottom wood grain printing background color data subset includes multiple background color printing point coordinate data, each background color printing point coordinate data is marked with color information, and the first printing device prints based on the background color printing point coordinate data and the color information corresponding to the background color printing point coordinate data.
4. The method according to claim 2, characterized in that The bottom layer wood grain printing shape data subset includes multiple sets of multiple two-dimensional plane wood grain printing coordinate data for printing wood grain, each plane wood grain printing coordinate data is marked with color information, and the first printing device prints based on the plane wood grain printing coordinate data and the color information corresponding to the plane wood grain printing coordinate data, and each bottom layer wood grain printing shape data subset corresponds to a bottom layer wood grain printing route.
5. The method according to claim 2, 3 or 4, characterized in that: The marked color information in the bottom wood grain printing base color data subset and the bottom wood grain printing shape data subset is obtained by superimposing at least one or more standard colors.
6. The method according to claim 5, characterized in that The standard colors include at least red, blue, light red, yellow, black, and light black.
7. The method according to claim 6, characterized in that The printing resolution of the background color printing point coordinate data and the plane wood grain printing coordinate data is greater than or equal to 100 DPI.
8. The method according to claim 4, characterized in that The 3D wood grain printing shape data subset includes a plurality of two-dimensional 3D wood grain printing coordinate data for printing wood grains, each 3D wood grain printing shape data subset corresponds to a 3D wood grain printing route, and the plurality of 3D wood grain printing routes respectively overlap with the plurality of bottom wood grain printing routes on a two-dimensional plane.
9. The method according to claim 8, characterized in that The three-dimensional wood grain printing shape data subset includes printing depth data of each three-dimensional wood grain printing coordinate data.
10. The method according to claim 1, characterized in that The wood grain information is obtained by scanning the natural wood board.
11. The method according to claim 1 or 10, characterized in that In the step (S.1), the wood grain information processing includes at least one of the following operations: Geometric transformations, correction of color and / or brightness and / or contrast, removal of unwanted image elements, image skewing, image distortion.
12. The method according to claim 1, characterized in that After step (S.4), the following steps are also included: The step of solidifying the wood grain precursor forms a three-dimensional wood grain layer on the surface of the bottom wood grain layer.
13. The method according to claim 12, characterized in that The wood grain precursor at least includes a photocatalytic resin; and Photoinitiators used to initiate the polymerization of photocatalytic resins.
14. The method according to claim 1, characterized in that There is also an intermediate step between step (S.3) and step (S.4), and the intermediate step includes: - applying a curable liquid resin on top of the underlying wood grain layer by means of a coating tool, thereby forming a liquid resin layer; In the step (S.4), the wood grain precursor liquid is applied to the upper surface of the liquid resin layer, so that the wood grain precursor liquid and / or at least a portion of the liquid resin mixed with the wood grain precursor liquid and / or at least a portion of the liquid resin covered by the wood grain precursor liquid forms a wood grain precursor.
15. The method according to claim 14, characterized in that The wood grain precursor liquid at least contains an inhibitor for preventing or delaying the polymerization of the curable liquid resin.
16. The method according to claim 14, characterized in that After step (S.4), the following steps are also included: - a step of curing the liquid resin except the wood grain precursor formed in the previous step; - A step of removing the wood grain precursor, thereby forming a three-dimensional wood grain layer on the surface of the underlying wood grain layer.
17. The method according to any one of claims 12 to 16, characterized in that After the step (S.3), a pretreatment step is also performed, and the pretreatment step includes: The step of covering at least a portion of the surface above the bottom wood grain layer with a curable liquid resin and curing at least a portion of the resin liquid on the surface of the bottom wood grain layer to form a three-dimensional wood grain bottom layer.
18. The method according to claim 12 or 16, characterized in that After the three-dimensional wood grain layer is prepared, the method further comprises: The step of covering at least a portion of the surface of the three-dimensional wood grain layer with a topcoat and curing the topcoat layer.
19. The method according to claim 1 or 12 or 14, characterized in that Before the step (S.3), the plate further comprises the following steps: The step of covering at least a portion of the surface of the board with a primer and curing it to obtain a primer layer.
20. A board having three-dimensional wood grain on its surface, characterized in that: It is prepared by the method according to any one of claims 1 to 19.
21. Use of the board having three-dimensional wood grain on the surface as claimed in claim 20 in flooring, decorative wall panels or ceiling panels.