Conductive paste, electronic component, and multilayered ceramic capacitor
Patent Information
- Application Number
- MYPI2025008363
- Authority / Receiving Office
- MY · MY
- Patent Type
- Applications
- Current Assignee / Owner
- Priority Date
- 2023-07-04
- Filing Date
- 2024-07-02
- Publication Date
- 2025-01-04
Smart Images

Figure PI2025008363_DRAWING_001 
Figure PI2025008363_DRAWING_002 
Figure PI2025008363_DRAWING_003
Abstract
Description
Conductive paste, electronic components, and multilayer ceramic capacitors
[0001] The present invention relates to a conductive paste, an electronic component, and a multilayer ceramic capacitor.
[0002] As electronic devices such as mobile phones and digital devices become smaller and more powerful, there is a demand for smaller electronic components, including multilayer ceramic capacitors, with higher capacitance. Multilayer ceramic capacitors have a structure in which multiple dielectric layers and multiple internal electrode layers are alternately stacked, and by reducing the thickness of these dielectric layers and internal electrode layers, it is possible to achieve smaller size and higher capacitance.
[0003] For example, a multilayer ceramic capacitor is manufactured as follows: First, barium titanate (BaTiO 3 A conductive paste for internal electrodes is printed in a predetermined electrode pattern on the surface of a green sheet containing a dielectric powder such as ethylenediaminetetraacetic acid (EPO) and a binder resin, and then dried to form a dry film (conductive film). The dry film and green sheets are then alternately stacked to obtain a laminate. This laminate is then integrated by heat and pressure to form a pressed body. This pressed body is cut, subjected to an organic binder removal treatment in an oxidizing or inert atmosphere, and then fired to obtain fired chips. A paste for external electrodes is then applied to both ends of the fired chip, and after firing, the surfaces of the external electrodes are nickel-plated or the like to obtain a multilayer ceramic capacitor.
[0004] As multilayer ceramic capacitors become smaller and their capacitances increase, both the internal electrodes and dielectrics are becoming thinner. Accordingly, the particle size of the conductive powder (e.g., nickel powder) used in the conductive paste for the internal electrodes is becoming finer, and nickel powder with an average particle size of 0.4 μm or less is sometimes required. Furthermore, although this depends on the film thickness of the internal electrodes, a particle size that is typically three to five times the number average particle size of the entire conductive powder is used as the reference particle size, and particles larger than this reference particle size are considered coarse particles. Furthermore, with the recent trend toward further miniaturization of multilayer ceramic capacitors and thinner internal electrode layers, a reference particle size that is less than three times the number average particle size of the conductive powder is sometimes required.
[0005] Here, when the conductive powder is mainly composed of primary particles, the coarse particles include not only large particles whose primary particle diameter is equal to or larger than the standard, but also particles that are connected particles in a state where the primary particles are tightly connected and cannot be easily broken down, and have a particle diameter equal to or larger than the standard particle diameter.
[0006] In order to obtain nickel powder that does not contain particles larger than these standard particle sizes, classification treatment using expensive classification equipment is essential. In classification treatment, it is possible to remove coarse particles larger than the classification point, which is an arbitrary value of about 0.6 μm to 2 μm, but there is also the problem that some particles smaller than the classification point are also removed at the same time, which significantly reduces the actual product yield.
[0007] For example, Patent Document 1 discloses a method for producing nickel powder, which is characterized in that the produced nickel particles are disintegrated using a jet mill equipped with a high-speed classification rotor, and coarse particles are removed before re-agglomeration.
[0008] Furthermore, a conventional method for obtaining a conductive paste that does not contain coarse particles is to filter the conductive paste to remove the coarse particles.
[0009] For example, Patent Document 2 discloses a method for removing coarse metal particles having a predetermined particle size or larger by filtering a slurry containing metal particles as the main solid content (hereinafter referred to as "metal particle slurry") through a filter, the method comprising: providing a circulation line for extracting the metal particle slurry from a slurry chamber functioning as a filter front chamber to which the metal particle slurry to be passed through the filter is supplied, circulating the metal particle slurry through a predetermined path, and returning the metal particle slurry to the slurry chamber; filtering the metal particle slurry in the slurry chamber through a filter with a predetermined mesh size while circulating the metal particle slurry through the circulation line to remove the coarse metal particles; and further disclosing a method for recovering the metal particles by distilling off the dispersant and solvent from the metal particle slurry after separating the coarse metal particles from the metal particle slurry.
[0010] JP 2003-089806 A JP 2002-177743 A
[0011] However, even if inorganic particles are classified in advance to remove coarse particles as in Patent Document 1, the inorganic particles may re-aggregate to form coarse particles during the subsequent storage and manufacturing processes.
[0012] Furthermore, in the process of filtering the metal particle slurry while circulating it, as described in Patent Document 2, the dispersion of the metal particle slurry is not sufficiently maintained, and clogging occurs due to aggregates of metal particles, which may prevent accurate removal of coarse particles. Furthermore, an additional process of removing the low-boiling-point dispersant and solvent is required after removing the coarse particles. Particularly with the high-viscosity conductive paste used in multilayer ceramic capacitors, even if a filter with high filtration accuracy is used to remove coarse particles, clogging occurs, making it difficult to sufficiently reduce the number of coarse particles.
[0013] Taking these circumstances into consideration, the present inventors have conducted extensive research and have discovered that in the manufacturing process of a conductive paste containing inorganic particles, by controlling the viscosity of an inorganic particle slurry having a specific composition within a specific range and removing coarse particles using a filter with high filtration accuracy, it is possible to significantly reduce the number of particles (coarse particles) having a standard particle size of about twice the average particle size, even in a highly viscous conductive paste, and have completed the present invention.
[0014] An object of the present invention is to provide a conductive paste that has excellent dispersibility and high viscosity, yet contains a significantly reduced number of coarse particles.
[0015] In a first aspect of the present invention, there is provided a conductive paste containing inorganic particles, a binder resin, a dispersant, and an organic solvent, wherein the inorganic particles contain conductive powder having a number average particle size of 0.05 μm or more and 0.3 μm or less in an amount of 30 mass % or more and 70 mass % or less relative to the entire conductive paste, the binder resin contains a cellulose-based resin, the dispersant contains an acid-based dispersant, and the conductive paste is subjected to a shear rate of 4 s -1The conductive paste has a viscosity of more than 10 Pa s at 2000 kJ / s, and the proportion of conductive powder particles having a particle diameter more than twice the number average particle diameter of the conductive powder particles in the conductive paste is 50 ppm or less relative to the total number of conductive powder particles.
[0016] In a second aspect of the present invention, there is provided a method for producing the above-mentioned conductive paste, comprising: a first step of mixing inorganic particles, a binder resin, a dispersant, and an organic solvent to obtain an inorganic particle slurry; a second step of filtering the inorganic particle slurry through a filter having a filtration accuracy of 1.0 μm or less; and a third step of mixing the filtered inorganic particle slurry with a binder resin and an organic solvent.
[0017] In a third aspect of the present invention, there is provided an electronic component formed using the conductive paste.
[0018] In a fourth aspect of the present invention, there is provided a multilayer ceramic capacitor having at least a laminate in which dielectric layers and internal electrode layers are laminated, the internal electrode layers being formed using the above-mentioned conductive paste.
[0019] The conductive paste of the present invention has excellent dispersibility and high viscosity, but the number of coarse particles is significantly reduced.
[0020] Fig. 1 is a diagram showing an example of a primary particle (single particle) of a conductive powder (inorganic particle). Fig. 2 is a diagram showing an example of a connected particle of a conductive powder (inorganic particle). Fig. 3 is a diagram showing an example of a method for manufacturing a conductive paste according to an embodiment. Fig. 4 is a perspective view and a cross-sectional view showing a multilayer ceramic capacitor according to an embodiment.
[0021] [Conductive Paste] (Paste Viscosity) The conductive paste in this embodiment contains inorganic particles (including conductive powder), a binder resin, a dispersant, and an organic solvent. -1The viscosity at 100 Pa s is greater than 10 Pa s, and may be, for example, greater than 10 Pa s and not greater than 100 Pa s, 15 Pa s or greater and not greater than 50 Pa s, or 20 Pa s or greater and not greater than 40 Pa s. When the viscosity of the conductive paste is within the above range, it can be suitably used, for example, as a paste for screen printing.
[0022] In the case of a conductive paste having a relatively high viscosity as described above, if a filter with high filtration accuracy is used to remove coarse particles having a particle size larger than a predetermined size, clogging occurs, making it difficult to sufficiently reduce the number of coarse particles. In the conductive paste of this embodiment, despite having a relatively high viscosity, the number of coarse particles in the conductive paste can be significantly reduced by using the conductive paste manufacturing method described below.
[0023] FIG. 1 shows an example of a primary particle (single) of the conductive powder contained in the conductive paste, and FIG. 2 shows an example of a connected particle of the conductive powder contained in the conductive paste. In this specification, the term "coarse particles" refers not only to particles in which the particle diameter of the primary particle (single) is larger than the reference particle diameter (e.g., twice the number average particle diameter of the conductive powder), but also to particles in which the particle diameter of connected particles (see FIG. 2) formed by connecting smaller primary particles is larger than the reference particle diameter. Note that the particle diameter of the conductive powder refers to the major axis (the long axis dimension of the circumscribed rectangular parallelepiped) determined from a scanning electron microscope (SEM) image. Each component contained in this embodiment will be described in detail below.
[0024] (Inorganic Particles) The inorganic particles contain conductive powder. The inorganic particles may or may not contain ceramic powder. Each component of the inorganic particles will be described in detail below.
[0025] (a) Conductive Powder The conductive powder is not particularly limited and may be a metal powder, such as one or more powders selected from Ni, Pd, Pt, Au, Ag, Cu, and alloys thereof. Among these, Ni or its alloy powder (hereinafter sometimes referred to as "nickel powder") is preferred from the viewpoints of conductivity, corrosion resistance, and cost. Examples of Ni alloys include alloys of Ni with at least one element selected from the group consisting of Mn, Cr, Co, Al, Fe, Cu, Zn, Ag, Au, Pt, and Pd. The Ni content in the Ni alloy is, for example, 50% by mass or more, preferably 80% by mass or more. The nickel powder may contain several hundred ppm of element S to suppress rapid gas generation due to partial thermal decomposition of the binder resin during debinding.
[0026] Furthermore, when nickel powder is used as the conductive powder, its manufacturing method is not particularly limited, and it can be manufactured using a conventionally known wet method, dry method, or the like. For example, the nickel powder may be nickel powder manufactured by a so-called dry method, such as a CVD method, an evaporation quenching method, or a hydrogen reduction method using nickel salt or nickel hydroxide, or may be nickel powder manufactured by a so-called wet method, such as a wet reduction method using a nickel salt solution with a reducing agent such as hydrazine. Among these, it is preferable to use nickel powder manufactured by a so-called wet method, such as a wet reduction method. For example, the wet reduction method is known to be capable of manufacturing nickel powder with a relatively narrow particle size distribution, but conventional nickel powder manufacturing methods contain a certain proportion of coarse particles, making it difficult to completely remove the coarse particles.
[0027] The number average particle size of the conductive powder is, for example, 0.05 μm or more and 0.3 μm or less, preferably 0.05 μm or more and 0.3 μm or less, and more preferably 0.1 μm or more and 0.2 μm or less. When the average particle size of the conductive powder is within the above range, it can be suitably used as a paste for internal electrodes of thin-film multilayer ceramic capacitors (multilayer ceramic components). In the conductive paste of this embodiment, by using the method described below, the number of coarse particles is sufficiently reduced, and a dry film with high smoothness can be formed, even if the average particle size of the conductive powder is within the above range.
[0028] The average particle size is a value determined by observation with a scanning electron microscope (SEM), and is the average value (SEM average particle size, number average) obtained by measuring the particle size of each of a plurality of particles from an image observed with an SEM at a magnification of 10,000 times.
[0029] The specific surface area of the conductive powder is, for example, 2 m 2 / g or more 50m 2 / g or less, and 2 / g or more 40m 2 / g or less, 2 / g or more 20m 2 When the specific surface area of the conductive powder is large, the surface activity increases, dispersibility decreases, and the powder particles tend to aggregate with each other, or the liquid permeability through the filter decreases. 2 / g or more, or 5m 2 / g or more, the amount of coarse particles can be sufficiently reduced. The specific surface area of the conductive powder can be determined by the BET method using nitrogen gas adsorption.
[0030] The content of the conductive powder is preferably 30% by mass or more and 70% by mass or less, more preferably 40% by mass or more and 60% by mass or less, based on the total amount of the conductive paste. When the content of the conductive powder is within the above range, the conductive paste has excellent conductivity and dispersibility. The content of the conductive powder may also exceed 50% by mass.
[0031] (b) Ceramic Powder The ceramic powder is not particularly limited. For example, in the case of a paste for an internal electrode of a multilayer ceramic capacitor, a known ceramic powder is appropriately selected depending on the type of multilayer ceramic capacitor to be applied. For example, a perovskite-type oxide containing Ba and Ti can be used as the ceramic powder, and preferably barium titanate (BaTiO 3 ) is included.
[0032] The ceramic powder may be a ceramic powder containing barium titanate as a main component and an oxide as a secondary component. Examples of the oxide include oxides of Mn, Cr, Si, Ca, Ba, Mg, V, W, Ta, Nb, and one or more rare earth elements. Examples of the ceramic powder include barium titanate (BaTiO 3 Alternatively, a ceramic powder of a perovskite-type oxide ferroelectric may be used in which the Ba atoms or Ti atoms of the above-mentioned ferroelectric material are substituted with other atoms such as Sn, Pb, or Zr.
[0033] When used as a conductive paste for internal electrodes, the ceramic powder may have the same composition as the dielectric ceramic powder constituting the green sheets of a multilayer ceramic capacitor (electronic component). This prevents cracks from occurring at the interface between the dielectric layer and the internal electrode layer during the sintering process due to a mismatch in shrinkage. Examples of such ceramic powders include, in addition to those mentioned above, ZnO, ferrite, PZT, BaO, and Al. 2 O 3 , Bi 2 O 3 , R (rare earth element) 2 O 3 , TiO 2 , Nd 2 O 3 The ceramic powder may be one type or two or more types.
[0034] The number average particle size of the ceramic powder is, for example, 0.01 μm or more and 0.3 μm or less. The number average particle size of the ceramic powder may be smaller than the number average particle size of the conductive powder, for example, ½ or less of the number average particle size of the conductive powder. When the number average particle size of the ceramic powder is within the above range, when used as an internal electrode paste, a sufficiently fine, thin, and uniform internal electrode can be formed. The number average particle size is a value determined by observation with a scanning electron microscope (SEM), and is the average value (SEM average particle size, number average) obtained by measuring the particle size of each of a plurality of particles from an image observed with the SEM at 50,000x magnification.
[0035] The specific surface area of the ceramic powder is, for example, 5 m 2 / g or more 100m 2 / g or less, and 2 / g or more 80m 2 / g or less, and 2 / g or more 60m 2 The specific surface area of the conductive powder can be determined by the BET method using nitrogen gas adsorption.
[0036] The content of the ceramic powder is preferably 1% by mass or more and 20% by mass or less based on the total amount of the conductive paste, and the upper limit of the content of the ceramic powder may be 15% by mass or less, 10% by mass or less, or 6% by mass or less.
[0037] The content of the ceramic powder is, for example, 2 parts by mass or more and 40 parts by mass or less, per 100 parts by mass of the conductive powder, and may be 30 parts by mass or less, 20 parts by mass or less, or 12 parts by mass or less.
[0038] (Binder Resin) The binder resin preferably contains a cellulose-based resin. The cellulose-based resin is not particularly limited, and a known cellulose-based resin (cellulose derivative) used as a binder resin can be used. Examples of the cellulose-based resin include ethyl cellulose, ethylhydroxyethyl cellulose, nitrocellulose, methyl cellulose, propyl cellulose, and acetyl cellulose. One type of cellulose-based resin may be used alone, or two or more types may be used.
[0039] The cellulose-based resin preferably contains ethyl cellulose resin. When ethyl cellulose resin is contained, the cellulose-based resin has excellent solubility in organic solvents and excellent decomposition by combustion. Furthermore, in the manufacturing process of the conductive paste, when the inorganic particle slurry contains ethyl cellulose resin, the dispersibility of the inorganic particle slurry and the liquid permeability through a filter are improved, and the number of coarse particles can be accurately reduced.
[0040] The weight average molecular weight (Mw) of the cellulose-based resin may be 10,000 or more and 300,000 or less, 30,000 or more and 250,000 or less, or 50,000 or more and 200,000 or less. The hydroxyl value of the cellulose-based resin is not particularly limited, but is preferably 0.1 mgKOH / g or more and 15 mgKOH / g or less, more preferably 0.5 mgKOH / g or more and 7 mgKOH / g or less, and even more preferably 1.5 mgKOH / g or more and 3 mgKOH / g or less. The cellulose-based resin may be used singly or in combination of two or more types.
[0041] The content of the cellulose-based resin may be 0.1% by mass or more and 3.0% by mass or less, 0.5% by mass or more and 2% by mass or less, or 1.0% by mass or more and 2% by mass or less. The higher the content of the cellulose-based resin within the above range, the more improved the liquid permeability of the inorganic particle slurry.
[0042] The binder resin may also contain an acetal-based resin. The acetal-based resin preferably contains a butyral-based resin, and more preferably contains polyvinyl butyral (PVB). When the conductive paste contains an acetal-based resin, the adhesive strength with the green sheet can be further improved. Furthermore, in the manufacturing process of the conductive paste, when the inorganic particle slurry contains an acetal-based resin, the dispersibility of the inorganic particle slurry and its liquid permeability through a filter are improved, and the number of coarse particles can be accurately reduced.
[0043] The weight average molecular weight (Mw) of the acetal resin may be from 30,000 to 300,000, from 50,000 to 200,000, or from 100,000 to 150,000. The glass transition temperature Tg of the acetal resin may be from 50° C. to 90° C., or from 60° C. to 80° C. One type of acetal resin may be used alone, or two or more types may be used in combination.
[0044] The content of the acetal resin may be 0.5% by mass or more and 3% by mass or less, 0.5% by mass or more and 2% by mass or less, or 1% by mass or more and 2% by mass or less. The higher the content of the acetal resin within the above range, the more improved the liquid permeability of the inorganic particle slurry.
[0045] The binder resin may contain a resin other than the cellulose-based resin and the acetal-based resin. The binder resin other than the above is not particularly limited, and any known resin may be used, such as an acrylic resin.
[0046] When the binder resin contains a cellulose-based resin and an acetal-based resin, the cellulose-based resin may be contained in an amount of 20% by mass or more, 40% by mass or more, or 55% by mass or more relative to the total content (100% by mass) of the cellulose-based resin and the acetal-based resin. When the resin content is within the above range, the dispersibility of the inorganic particles can be further improved, and the adhesive strength between the dried film and the green sheet (substrate) can be improved. The binder resin may also contain a resin in which the cellulose-based resin and the acetal-based resin are bonded. In this case, it is preferable that the ratio of each constituent part of the cellulose-based resin and the acetal-based resin satisfies the above-mentioned contents and blending ratios.
[0047] The content of the binder resin is preferably 0.5% by mass or more and 10% by mass or less, more preferably 1% by mass or more and 5% by mass or less, based on the total amount of the conductive paste. When the content of the binder resin is in the above range, the conductive paste has excellent conductivity and dispersibility.
[0048] The content of the binder resin is preferably 1 part by mass or more and 20 parts by mass or less, and more preferably 1 part by mass or more and 10 parts by mass or less, relative to 100 parts by mass of the conductive powder.
[0049] (Organic Solvent) The organic solvent is not particularly limited, and any known organic solvent capable of dissolving the binder resin can be used. The organic solvent can be appropriately selected from known organic solvents so that the viscosity of the inorganic particle slurry and the viscosity of the conductive paste fall within the desired range. Examples of the organic solvent include terpene-based solvents, acetate-based solvents, ether-based solvents, ketone-based solvents, and hydrocarbon-based solvents.
[0050] Examples of the terpene solvent include terpineol, dihydroterpineol, and dihydroterpinyl acetate.
[0051] Examples of acetate solvents include isobornyl acetate, isobornyl propionate, isobornyl butyrate, and isobornyl isobutyrate; glycol ether acetates such as ethylene glycol monobutyl ether acetate, diethylene glycol monobutyl ether acetate, diethylene glycol monoethyl ether acetate, dipropylene glycol methyl ether acetate, 3-methoxy-3-methylbutyl acetate, and 1-methoxypropyl-2-acetate; glycol diacetates such as propylene glycol diacetate, 1,4-butanediol diacetate, 1,3-butylene glycol diacetate, and 1,6-hexanediol diacetate; and cyclohexanol acetate.
[0052] Examples of the ether solvent include propylene glycol monoalkyl ethers such as propylene glycol monomethyl ether, propylene glycol monoethyl ether, propylene glycol monopropyl ether, and propylene glycol monobutyl ether; ethylene glycol ethers such as diethylene glycol mono-2-ethylhexyl ether, ethylene glycol mono-2-ethylhexyl ether, diethylene glycol monohexyl ether, and ethylene glycol monohexyl ether; dipropylene glycol methyl-n-propyl ether, dipropylene glycol methyl-n-butyl ether, and dipropylene glycol dimethyl ether.
[0053] Examples of the ketone solvent include methyl isobutyl ketone, diisobutyl ketone, etc. When a ketone solvent is contained, it is possible to adjust the viscosity and improve the drying property without impairing the dispersibility.
[0054] Examples of hydrocarbon solvents include solvents containing tridecane, nonane, cyclohexane, mineral spirits, naphthenic solvents, etc., with mineral spirits being preferred.
[0055] The organic solvent preferably contains at least one selected from the group consisting of terpineol, dihydroterpineol, dihydroterpinyl acetate, propylene glycol monobutyl ether, and diethylene glycol monobutyl ether acetate. By containing such an organic solvent, excellent compatibility with the binder resin and excellent dispersibility of the filler can be achieved.
[0056] One type of organic solvent may be used, or two or more types may be used. For example, when two or more types of organic solvents are included, the organic solvent may include at least one selected from the group consisting of terpineol, dihydroterpineol, dihydroterpinyl acetate, propylene glycol monobutyl ether, and diethylene glycol monobutyl ether acetate, and a hydrocarbon solvent, or may include dihydroterpineol and a hydrocarbon solvent. Furthermore, the organic solvent may be combined with at least one selected from methyl isobutyl ketone and diisobutyl ketone.
[0057] The total content of the organic solvent is preferably 20% by mass or more and 60% by mass or less, and more preferably 25% by mass or more and 50% by mass or less, based on the total amount of the conductive paste. When the content of the organic solvent is in the above range, the conductive paste has excellent conductivity and dispersibility.
[0058] The content of the organic solvent is preferably 40 parts by mass or more and 120 parts by mass or less, more preferably 50 parts by mass or more and 100 parts by mass or less, relative to 100 parts by mass of the conductive powder. When the content of the organic solvent is within the above range, the conductive powder has excellent conductivity and dispersibility.
[0059] The content of the hydrocarbon solvent may be 10% by mass or more and 50% by mass or less, or may be 20% by mass or more and 40% by mass or less, based on the total amount of the organic solvent.
[0060] (Dispersant) The conductive paste preferably contains a dispersant, more preferably an acid-based dispersant. By containing an acid-based dispersant, the dispersibility of the inorganic particles can be improved, and the liquid permeability of the inorganic particle slurry can be improved. Furthermore, by suppressing re-aggregation of the inorganic particles, the number of coarse particles in the conductive paste can be reduced.
[0061] The acid dispersant may include a carboxylic acid dispersant such as a higher fatty acid, a polycarboxylic acid dispersant, a phosphoric acid dispersant, an acid dispersant having an acidic group such as a polymer surfactant, and the like. Preferably, the dispersant includes at least one of a polycarboxylic acid dispersant and a phosphoric acid dispersant. The polycarboxylic acid dispersant may be a polycarboxylic acid having a graft chain or a polycarboxylic acid having a graft chain polyoxyalkylene. The phosphoric acid dispersant may be a phosphoric acid polyester. The dispersants may be used alone or in combination of two or more.
[0062] The acid dispersant is preferably contained in an amount of 0.01 mass % or more and less than 1.0 mass % based on the entire conductive paste, and may be contained in an amount of 0.05 mass % or more and 0.5 mass % or less.
[0063] The content of the acid-based dispersant is determined based on, for example, the specific surface area (m 2 / g) is 0.02 mg KOH / m 2 0.30mgKOH / m or more 2 or less, preferably 0.05 mg KOH / m 2 0.25mgKOH / m or more 2 or less, more preferably 0.08 mgKOH / m 2 0.20mgKOH / m or more 2 It can be adjusted to the following range:
[0064] In addition, when the acid-based dispersant contains a polycarboxylic acid-based dispersant, the content of the polycarboxylic acid-based dispersant is, for example, determined based on the specific surface area (m 2 / g) is 0.01 mgKOH / m 2 0.10mgKOH / m or more 2 or less, preferably 0.02 mg KOH / m 2 More than 0.07 mgKOH / m 2 or less, more preferably 0.02 mgKOH / m 2 0.06mgKOH / m or more2 It can be adjusted to the following range:
[0065] In addition, when the acid-based dispersant contains a phosphate-based dispersant, the content of the phosphate-based dispersant is, for example, determined based on the specific surface area (m 2 / g) is 0.01 mgKOH / m 2 0.20mgKOH / m or more 2 or less, preferably 0.05 mg KOH / m 2 0.17mgKOH / m or more 2 or less, more preferably 0.08 mgKOH / m 2 0.16mgKOH / m or more 2 It can be adjusted to the following range:
[0066] By adjusting the content of the acid-based dispersant within the above range, the dispersibility of the inorganic particles can be improved, the liquid permeability of the inorganic particle slurry can be further improved, and re-aggregation of the inorganic particles can be further suppressed. The acid value (mg KOH / g) can be determined, for example, by potentiometric titration in accordance with JIS K0070.
[0067] The acid value of the dispersant relative to the specific surface area of the entire inorganic particles can be calculated by the following method: That is, the acid value of the dispersant (for example, X mg KOH / g) is multiplied by the content of the dispersant relative to the entire conductive paste (for example, x mass %) to obtain a value (X × x), which is then multiplied by the specific surface area (for example, A m 2 / g, B m 2 / g) by the content ratio (for example, a mass %, b mass %) relative to the entire conductive paste, and then dividing the result by the sum (A×a+B×b) (i.e., X×y / (A×a+B×b)).
[0068] The conductive paste may also contain a dispersant other than the acid dispersant, such as a basic dispersant, a nonionic dispersant, or an amphoteric dispersant.
[0069] The dispersant is contained in an amount of, for example, 0.01% by mass to 3% by mass of the entire conductive paste. The range including the upper limit of the dispersant content may be 2% by mass or less, 1% by mass or less, or 0.6% by mass or less.
[0070] (Other Additives) The conductive paste of the present embodiment may contain other additives in addition to the above components, as necessary. Examples of other additives that can be used include conventionally known additives such as antifoaming agents, plasticizers, and thickeners.
[0071] (Characteristics of the Conductive Paste) (1) Number of Coarse Particles In the conductive paste of this embodiment, the proportion of conductive powder particles whose particle diameters, as observed by a scanning electron microscope, exceed twice the number average particle diameter of the conductive powder (hereinafter simply referred to as "coarse particles") is, for example, 50 ppm or less relative to the total number of conductive powder particles, thereby significantly reducing the number of coarse particles (including single primary particles and connected particles) contained in the conductive paste. Furthermore, the number of coarse particles may be 40 ppm or less, 20 ppm or less, 10 ppm or less, 5 ppm or less, or even 0 ppm.
[0072] The proportion of coarse particles can be calculated, for example, by the following method.
[0073] First, 5 mg of conductive paste was diluted with an organic solvent (e.g., 4000 times with dihydroterpineol) to prepare a sample solution. The sample solution was filtered through a filter with a pore size no greater than twice the number average particle size of the conductive powder (e.g., a 0.4 μm filter when the number average particle size of the conductive powder is 0.2 μm) to remove some fine particles. Then, using a scanning electron microscope (SEM), the conductive particles on the filter were observed at a magnification of 5000x, and 10 fields of view were photographed. From the photographed images, coarse particles (primary particles and connected particles) were counted, and the number ratio of coarse particles was calculated using the following (Equation 1).
[0074] Ratio of number of coarse particles = (number of counted coarse particles) / (number of conductive powder particles corresponding to the observed field area) (Equation 1)
[0075] The number of conductive powder particles corresponding to the observed field area means the number of conductive powder particles (total) used to count the coarse particles, and is calculated using the following (Equation 2).
[0076] Number of conductive powder particles corresponding to the observed field area=(number of conductive powder particles used in sample preparation)×(observed field area) / (total area of filtration filter) (Equation 2)
[0077] The number of conductive particles used in sample preparation was determined based on the weight of the conductive paste used in sample preparation (a, unit: g), the concentration (weight percent concentration) of the conductive powder in the conductive paste (b, unit: wt%), and the true density of the conductive powder (c, unit: g / cm 3 ) and the number average particle diameter (d, unit: cm) of the conductive powder, is calculated from the following (Equation 3).
[0078] Number of conductive particles used in sample preparation = (a × b / c) ÷ (4 / 3π(1 / 2d) 3 )...(Formula 3)
[0079] When the conductive powder is nickel powder, the true density is 8.9 g / cm 3 The organic solvent used for sample preparation may be the main solvent (the solvent with the highest content) of the conductive paste.
[0080] The amount of conductive paste filtered based on the area of the observed image (area of the observed field of view) may be, for example, 0.02 μg or more of conductive paste. The amount of conductive paste evaluated may be changed depending on the amount of conductive paste, the area of the filter, and the number of fields of view. However, if the amount is small, the number of detected coarse particles may decrease, resulting in greater variation. Therefore, it is preferable to use the above-mentioned amount of conductive paste or more. Furthermore, if the area of the filter can be reduced to observe the entire field of view, the number of coarse particles in the conductive paste used for evaluation can be determined more accurately.
[0081] Alternatively, the number of coarse particles may be directly measured by applying and drying the conductive paste, observing it with an SEM, and then counting the number of coarse particles. For example, ten SEM images at a magnification of 5000 times may be obtained, and the number may be counted using image analysis software. In this case, the number of coarse particles counted may be divided by the total number of particles in the observed conductive powder to calculate the proportion of the number of coarse particles.
[0082] Furthermore, in the conductive paste of this embodiment, the number ratio of conductive powder having a particle diameter of more than 0.4 μm as observed with a scanning electron microscope may be, for example, 40 ppm or less, 20 ppm or less, 10 ppm or less, 5 ppm or less, or 0 ppm.
[0083] (2) Surface Roughness of Dry Film The surface roughness (arithmetic mean height Sa) of the dry film formed by printing the conductive paste is, for example, 0.1 μm or less, or may be 0.08 μm or less, 0.06 μm or less, or 0.05 μm or less. The surface roughness of the conductive paste can be measured, for example, by the method described in the Examples (a method of measuring the arithmetic mean height Sa based on the ISO 25178 standard using an OLS5000 manufactured by Evident).
[0084] The conductive paste according to this embodiment can be suitably used in electronic components such as multilayer ceramic capacitors. The multilayer ceramic capacitor has, for example, dielectric layers formed using dielectric green sheets and internal electrode layers formed using the conductive paste.
[0085] For example, the thickness of the internal electrode layer formed using the conductive paste of this embodiment may be, for example, 1.5 μm or less, 1 μm or less, or 0.7 μm or less. The conductive paste of this embodiment has good dispersibility and a small number of coarse particles, so that thin internal electrode layers can be manufactured with high reliability.
[0086] [Method for manufacturing conductive paste] The method for manufacturing the conductive paste in this embodiment will be described below. Fig. 3 is a diagram showing an example of the method for manufacturing the conductive paste. As shown in Fig. 3, the method for manufacturing the conductive paste in this embodiment includes the following steps (1) to (3).
[0087] (1) A first step (S1) of mixing inorganic particles, a binder resin, a dispersant, and an organic solvent to obtain an inorganic particle slurry; (2) A second step (S2) of filtering the inorganic particle slurry through a filter having a filtration accuracy of 1.0 μm or less; and (3) A third step (S3) of kneading the filtered inorganic particle slurry with a binder resin and an organic solvent.
[0088] 3 shows an example of a method for manufacturing a conductive paste, but the method is not limited to these. The conductive paste of this embodiment is suitable for use in forming internal electrodes of a multilayer ceramic capacitor. Each step will be described in detail below.
[0089] (First Step: S1) In the first step (S1), inorganic particles, a binder resin, a dispersant, and an organic solvent are mixed to obtain an inorganic particle slurry (step S1). The inorganic particle slurry contains, for example, coarse particles (e.g., inorganic particles with a particle diameter exceeding 0.4 μm). The coarse particles are removed from the inorganic particle slurry in the second step (S2) described below.
[0090] The inorganic particle slurry obtained in the first step (S1) is subjected to a shear rate of 4 s at room temperature (25°C). -1 The viscosity of the inorganic particle slurry is 20 Pa·s or less at a shear rate of 4 s -1 The viscosity of the inorganic particle slurry may be, for example, 10 Pa·s or less, or 5 Pa·s or less. -1 The lower limit of the viscosity is not particularly limited, and the lower the viscosity, the more likely it is that the liquid permeability will be improved. -1 The lower limit of the viscosity is, for example, 1 Pa·s or more, or even 2 Pa·s or more, and the number of coarse particles can be sufficiently reduced.
[0091] The inorganic particle slurry obtained in the first step (S1) was subjected to a shear rate of 40 s at room temperature (25°C). -1 The viscosity of the inorganic particle slurry at a shear rate of 40 s may be 5 Pa·s or less, or may be 1 Pa·s or less. -1 The lower limit of the viscosity is not particularly limited, and the lower the viscosity, the more likely it is that the liquid permeability will be improved. -1 The lower limit of the viscosity is, for example, 0.3 Pa·s or more, or even if it is 0.4 Pa·s or more, the number of coarse particles can be sufficiently reduced.
[0092] The viscosity of the inorganic particle slurry can be controlled within the above range by adjusting the type and content of each component contained in the inorganic particle slurry. In the production method of this embodiment, by adjusting the composition and viscosity characteristics of the inorganic particle slurry obtained in the first step (S1), the dispersibility of the inorganic particles is improved while suppressing re-aggregation of the inorganic particles, thereby enabling the use of a filter with high filtration accuracy in the second step (S2).
[0093] The inorganic particles contained in the inorganic particle slurry may include a conductive powder, or may include both a conductive powder and a ceramic powder. The inorganic particles include individual primary particles and connected particles formed by connecting primary particles. The conductive powder used as a raw material may also include coarse particles, for example, particles having a particle diameter more than twice the number average particle diameter of the conductive powder in an amount of more than 50 ppm, 70 ppm or more, or 90 ppm or more. In this specification, the term "coarse particles" refers not only to particles whose particle diameter as individual primary particles is larger than the reference particle diameter, but also to particles whose particle diameter as connected particles (see FIG. 2) formed by connecting smaller primary particles is larger than the reference particle diameter.
[0094] The inorganic particle slurry contains a binder resin. The binder resin contained in the inorganic particle slurry preferably contains a cellulose-based resin, and more preferably contains both a cellulose-based resin and an acetal-based resin. The cellulose-based resin may be contained in an amount of, for example, 0.1% by mass to 3.0% by mass, 0.2% by mass to 2.0% by mass, or 0.2% by mass to 1.5% by mass, based on the total inorganic particle slurry. The acetal-based resin may be contained in an amount of, for example, 0.5% by mass to 3% by mass, or 0.5% by mass to 2% by mass, based on the total inorganic particle slurry.
[0095] The content of the cellulose-based resin contained in the inorganic particle slurry is 0.5 g / m relative to the specific surface area of the inorganic particles. 2 5g / m or more 2 It is preferable that the content is 0.5 g / m or less. 2 3g / m or more 2 It may be less than 1 g / m 2 3g / m or more 2 When the cellulose-based resin is contained in the above range, the dispersibility of the inorganic particles is further improved. In addition, the content of the cellulose-based resin contained in the inorganic particle slurry is 0.5 g / m or less relative to the specific surface area of the conductive powder. 2 5g / m or more 2 It may be 0.5 g / m or less, 2 3g / m or more 2 It may be less than 1 g / m 2 3g / m or more 2 It may be the following:
[0096] The components used for mixing may be the same as those contained in the conductive paste described above. Alternatively, all of the components contained in the final conductive paste, except for a portion of the binder resin and a portion of the organic solvent, may be dispersed (mixed) to obtain an inorganic particle slurry. The binder resin may be dispersed (mixed) using the entire amount of the acetal resin contained in the final conductive paste to obtain an inorganic particle slurry.
[0097] The mixing method is not particularly limited, and known methods can be used. Examples of devices used for mixing include high-pressure homogenizers, mixer stirrers, suction dispersion stirrers, bead mills, ball mills, and three-roll mills. For example, a high-pressure homogenizer may be used. A high-pressure homogenizer utilizes a fine orifice to generate a high-speed jet flow. The orifice diameter of the high-pressure homogenizer is not particularly limited, but may be, for example, 0.05 to 0.2 mm. Furthermore, the conditions for the high-pressure homogenizer (e.g., the number of dispersion passes) can be appropriately selected depending on the required particle size, particle size distribution, and the like. The number of dispersion passes may be determined using a device configured to circulate the paste. Furthermore, if the inorganic particles form aggregates or the like and are difficult to disperse, a three-roll mill may be used for dispersion treatment. In the first step (S1), all components may be mixed in one go to obtain an inorganic particle slurry, or some of the components may be mixed in multiple batches to obtain an inorganic particle slurry. Furthermore, one or more devices may be used for mixing. For example, the components excluding a portion of the organic solvent may be dispersed using a dispersing device (e.g., a three-roll mill), and then the organic solvent may be further added and stirred to obtain an inorganic particle slurry having a viscosity within the above-mentioned range.
[0098] (Second Step: S2) In the second step (S2), the inorganic particle slurry is filtered through a filter having a filtration accuracy of 1.0 μm or less. By using a filter with a relatively high filtration accuracy, it is possible to remove coarse particles that are large relative to the standard particle size. In the method for producing a conductive paste according to this embodiment, by preparing an inorganic particle slurry having the above-described characteristics in the first step (S1), it is possible to suppress clogging and sufficiently reduce the number of coarse particles, even when filtering is performed using a filter with a relatively high filtration accuracy.
[0099] The filtration accuracy of the filter used in the second step may be 1.0 μm or less, 0.8 μm or less, 0.6 μm or less, or 0.4 μm or less. The filtration accuracy can be appropriately selected depending on the particle size of the target inorganic particles. The lower limit of the filtration accuracy of the filter is, for example, 0.1 μm or more. Note that filtration accuracy generally represents the size of particles that can be removed by passing through a filter. For example, it may be expressed as the particle size that can capture 99% or more of particles when the fluid is water and fine dust is filtered through a 10-inch cartridge at a predetermined flow rate. Furthermore, due to its structure, it is also possible to capture particles smaller than the value indicated by the filtration accuracy. Note that the filtration accuracy (μm) of the filter used in the second step (S2) may be, for example, 2 times or more, 2.5 times or more, or 3 times or more the number average particle size of the conductive powder, as long as it is within the above range. Even if the filtration accuracy of the filter is within the above range, coarse particles can be sufficiently removed by preparing an inorganic particle slurry having the above-mentioned properties in the first step (S1).
[0100] In the second step, the amount of liquid passing through the filter may be 50 g / min or more, 100 g / min or more, or 300 g / min or more, for example, when filtering using a filter with a built-in filter total length of 25 mm at a differential pressure of 0.39 MPa. When the amount of liquid passing through the filter is within the above range, the conductive paste can be produced with high productivity.
[0101] (Third Step: S3) In the third step (S3), the filtered inorganic particle slurry is mixed with a binder resin and an organic solvent. After mixing, the conductive paste described above can be obtained with a reduced number of coarse particles. Note that in this step, components other than the binder resin and the organic solvent (e.g., ceramic powder, other additives, etc.) may be added.
[0102] The binder resin added in the third step (S3) may contain a cellulose-based resin, may contain a cellulose-based resin and an acetal-based resin, or may be a cellulose-based resin (e.g., ethyl cellulose) alone.
[0103] The organic solvent added in the third step (S3) is not particularly limited, but may be the same type as the organic solvent added in the first step (S1), and may, for example, contain a terpene-based solvent or may be a terpene-based solvent alone.
[0104] The mixing method is not particularly limited, and any conventionally known method can be used. For example, the mixing can be carried out by stirring and kneading the above components using a three-roll mill, a ball mill, a mixer, or the like.
[0105] [Multilayer Ceramic Capacitor] Hereinafter, embodiments of the multilayer ceramic capacitor of the present invention will be described with reference to the drawings. In the drawings, schematic representations or scale changes may be used as appropriate. Furthermore, the positions and directions of components will be described with reference to an XYZ Cartesian coordinate system shown in FIG. 4 and other figures as appropriate. In this XYZ Cartesian coordinate system, the X and Y directions are horizontal directions, and the Z direction is vertical (up-down direction).
[0106] 4A and 4B are diagrams showing the multilayer ceramic capacitor 1. The multilayer ceramic capacitor 1 includes a ceramic laminate 10 in which dielectric layers 12 and internal electrode layers 11 are alternately stacked, and external electrodes 20.
[0107] A method for manufacturing a multilayer ceramic capacitor using the above-described conductive paste will now be described. First, the conductive paste is printed on a ceramic green sheet and dried to form a dry film. A plurality of ceramic green sheets, each having this dry film on its upper surface, are laminated by pressure bonding to obtain a laminate, which is then fired and integrated to produce a ceramic laminate 10 in which internal electrode layers 11 and dielectric layers 12 are alternately stacked. A pair of external electrodes 20 is then formed on both ends of the ceramic laminate 10 to produce a multilayer ceramic capacitor 1. This method will now be described in more detail.
[0108] First, a green sheet, which is an unfired ceramic sheet, is prepared. For example, this green sheet can be prepared by adding a binder resin such as polyvinyl butyral and a solvent such as terpineol to a predetermined ceramic raw material powder such as barium titanate to form a dielectric layer paste. The paste is then applied to a support film such as a PET film in a sheet form and dried to remove the solvent. The thickness of the dielectric layer made of the green sheet is not particularly limited, but is preferably 0.05 μm or more and 3 μm or less in view of the demand for miniaturization of multilayer ceramic capacitors.
[0109] Next, the conductive paste is printed and applied to one side of the green sheet, and then dried to form a dry film on one side of the green sheet, to prepare a plurality of green sheets. Note that, from the viewpoint of the requirement for thinning of the internal electrode layer 11, it is preferable that the thickness of the dry film formed from the conductive paste is 1 μm or less after drying.
[0110] Next, the green sheets are peeled off from the support film, and the green sheets and the dry film formed on one side thereof are stacked alternately, followed by a heat and pressure treatment to obtain a laminate. Note that a configuration may be adopted in which protective ceramic green sheets not coated with the conductive paste are further placed on both sides of the laminate.
[0111] Next, the laminate is cut to a predetermined size to form green chips, and the green chips are subjected to a binder removal treatment and fired in a reducing atmosphere to produce a fired laminated ceramic body (ceramic laminate 10). The atmosphere in the binder removal treatment is air or N 2 It is preferable to carry out the debinding treatment in a gas atmosphere. The temperature during the debinding treatment is, for example, 200°C or higher and 400°C or lower. Furthermore, it is preferable to hold the above temperature for 0.5 hours or higher and 24 hours or lower during the debinding treatment. Furthermore, the firing is carried out in a reducing atmosphere to suppress oxidation of the metal used in the internal electrode layers, and the temperature during firing of the laminate is, for example, 1000°C or higher and 1350°C or lower, and the temperature holding time during firing is, for example, 0.5 hours or higher and 8 hours or lower.
[0112] By firing the green chip, the organic binder in the ceramic green sheet is completely removed, and the ceramic raw material powder is fired to form the ceramic dielectric layer 12. Also, the organic vehicle in the dried film is removed, and the nickel powder or the alloy powder mainly composed of nickel is sintered or melted and integrated to form the internal electrode layer 11, thereby forming a multilayer ceramic fired body in which a plurality of dielectric layers 12 and internal electrode layers 11 are alternately stacked. Note that, from the viewpoint of taking oxygen into the dielectric layer to increase reliability and suppressing reoxidation of the internal electrodes, the fired multilayer ceramic fired body may be subjected to an annealing treatment.
[0113] A pair of external electrodes 20 is then provided on the produced fired multilayer ceramic body, thereby producing the multilayer ceramic capacitor 1. For example, the external electrodes 20 include an external electrode layer 21 and a plating layer 22. The external electrode layer 21 is electrically connected to the internal electrode layer 11. Suitable materials for the external electrodes 20 include, for example, copper, nickel, or an alloy thereof. Electronic components other than multilayer ceramic capacitors may also be used.
[0114] EXAMPLES The present invention will be described in detail below based on examples and comparative examples, but the present invention is not limited to these examples.
[0115] [Evaluation Method] (Viscosity Measurement) The viscosity of the conductive paste was measured using a rheometer (Rheometer MCR302 manufactured by Anton Paar Japan Co., Ltd.). The viscosity was measured using a cone plate with a cone angle of 1° and a diameter of 25 mm at a shear rate of 4 sec. -1 , shear rate 40 sec -1 The values measured under the conditions above were used.
[0116] (Number of Coarse Particles) The number of coarse particles in the conductive paste was measured by the following method.
[0117] 5 mg of conductive paste was diluted with 20 g of dihydroterpineol, and the solution was passed through a 0.4 μm membrane filter (filter area: 1075 mm 2The coarse particles collected on the filter surface during filtration were observed using a SEM (JSM-IT100 manufactured by JEOL Ltd.) at a magnification of 5000 times and 10 fields of view (total field area 0.0049 mm 2 ) was observed, and primary particles larger than 0.4 μm in particle size and connected particles formed by connecting primary particles were counted as coarse particles. The amount of paste used in the observed field of view was calculated from the amount of conductive paste used in filtration and the ratio of the observed field of view to the total area of the filtration filter, thereby obtaining the number of conductive powder particles with particle sizes exceeding 0.4 μm per 0.023 μg.
[0118] (Number average particle size of conductive powder) The number average particle size of the conductive powder in the conductive paste is the average value obtained by measuring the particle sizes of 100 primary particles of the conductive powder present within a predetermined area of an image observed by SEM. The average particle size of the conductive powder is expressed to one significant digit.
[0119] (Surface roughness of dried film) A sample was applied to a glass substrate (2 inches) (GAP thickness = 10 μm) and dried in an air atmosphere at a maximum temperature of 120 to 150°C in a belt furnace to produce a dried film with a thickness of 1 to 3 μm. If the dispersibility of the conductive paste is good, the surface of the dried film will be smooth. If the dispersibility is poor, aggregation will occur in the conductive paste, causing the surface of the dried film to become rough and its surface smoothness to decrease. Therefore, the surface roughness Sa (arithmetic mean height) of the produced dried film was measured using a laser microscope (OLS5000 manufactured by Evident Co., Ltd.) in accordance with the ISO 25178 standard. The smaller the surface roughness Sa (arithmetic mean height), the smoother the surface of the dried film.
[0120] [Materials Used] (Conductive Powder) Nickel powder a (number average particle size 0.2 μm, specific surface area 4.2 m) was used as the conductive powder. 2 / g), and nickel powder b (number average particle size 0.2 μm, specific surface area 5.4 m 2 / g) was used.
[0121] (Ceramic Powder) As the ceramic powder, barium titanate (BaTiO 3 , number average particle size 0.06μm, specific surface area 23.4m 2 / g) was used.
[0122] (Binder Resin) As the binder resin, polyvinyl butyral resin (PVB) and ethyl cellulose resin (EC) were used.
[0123] (Dispersant) As the acid-based dispersant, a polycarboxylic acid having polyoxyalkylene as a graft chain (acid-based A) and a phosphoric acid polyester (acid-based B), which is a phosphoric acid-based dispersant, were used.
[0124] (Organic Solvent) As the organic solvent, dihydroterpineol (DHT) and mineral spirits (MSA) were used.
[0125] [Example 1] Conductive powder (Ni powder), ceramic powder (BaTiO 3 ), dispersants (acid-based A and acid-based B), binder resins (EC, PVB), and organic solvents (DHT, MA) were mixed in the amounts shown in the first step of Table 2 (total 100% by mass), and the mixture was dispersed using a high-pressure homogenizer to obtain an inorganic particle slurry (first step: S1).
[0126] The obtained inorganic particle slurry was then filtered through a filter with a filtering accuracy of 0.6 μm to remove at least a part of the coarse particles (second step: S2).
[0127] Thereafter, the filtered inorganic particle slurry was blended with a binder resin and an organic solvent in the amounts shown in the third step in Table 4, and mixed using a mixer to prepare a conductive paste (third step: S3).
[0128] The properties of the obtained conductive paste (viscosity, surface roughness, number of coarse particles) were measured. The compounding ratio of each component of the conductive paste and the results are shown in Table 1.
[0129] [Examples 2 to 8] In Examples 2 to 8, conductive pastes were prepared and evaluated in the same manner as in Example 1, except that the type and content of each material used in the first and third steps were changed as shown in Tables 2 and 4. The content of each material in the conductive paste and the evaluation results are shown in Table 1. Table 3 also shows the acid value of the dispersant and the weight of the binder resin relative to the specific surface area of the inorganic particles added in the first step.
[0130] [Comparative Examples 1 to 3] In Comparative Example 1, the components were mixed in the amounts shown in Table 1, and only the dispersion treatment (first step) was carried out using a triple roll mill to prepare a conductive paste, which was then evaluated (the second and third steps were not carried out).
[0131] In Comparative Example 2, in order to confirm the effect of the resin on the state of the inorganic particle slurry prepared in the first step, an inorganic particle slurry was obtained by dispersion treatment using a high-pressure homogenizer under the same conditions as in Example 3, except that the resin used was changed from ethyl cellulose alone to polyvinyl butyral. The obtained inorganic particle slurry had low dispersibility and was difficult to filter, so the second step and subsequent steps were not carried out. For reference, the inorganic particle slurry, which was an intermediate material, was evaluated as a conductive paste.
[0132] In Comparative Example 3, in order to confirm the effect of the resin on the state of the inorganic particle slurry prepared in the first step, an inorganic particle slurry was obtained by dispersion treatment using a high-pressure homogenizer under the same conditions as in Example 1, except that the resin component was omitted in the first step. The obtained inorganic particle slurry had low dispersibility and was difficult to filter, so the second step and subsequent steps were not carried out. The evaluation results of the Examples and Comparative Examples are shown in Table 1.
[0133]
[0134]
[0135]
[0136]
[0137] (Evaluation Results) The conductive pastes of Examples 1 to 8 had a reduced number of coarse particles despite their relatively high viscosity. Furthermore, the surface roughness of the dried film was sufficiently small, demonstrating excellent dispersibility.
[0138] On the other hand, in the conductive pastes of Comparative Examples 1 to 3, the second step (filtration) was not performed, and therefore the number of coarse particles exceeded 50 ppm. Furthermore, in Comparative Example 1, the viscosity of the inorganic particle slurry (conductive paste) obtained after the first step was high, and it was not possible to filter it. In Comparative Example 2, the binder resin was not added in the first step, and therefore the dispersibility of the inorganic particles was poor, and it was not possible to filter it. In Comparative Example 3, the ethyl cellulose resin was not added in the first step, and therefore the paste viscosity was low, but the dispersibility of the inorganic particles was poor, and it was not possible to filter it.
[0139] When the conductive paste of the present invention is used to form internal electrodes of a multilayer ceramic capacitor, a highly reliable multilayer ceramic capacitor can be obtained with high productivity. Therefore, the conductive paste of the present invention is particularly suitable for use as internal electrodes of multilayer ceramic capacitors, which are chip components in electronic devices such as mobile phones and digital devices that are becoming increasingly miniaturized.
[0140] The technical scope of the present invention is not limited to the aspects described in the above-mentioned embodiments. One or more of the requirements described in the above-mentioned embodiments may be omitted. Furthermore, the requirements described in the above-mentioned embodiments may be combined as appropriate. Furthermore, to the extent permitted by law, the disclosures of all documents cited in the above-mentioned embodiments are incorporated by reference into this description. Furthermore, to the extent permitted by law, the contents of Japanese Patent Application No. 2023-110357 are incorporated by reference into this description.
[0141] REFERENCE SIGNS LIST 1 Multilayer ceramic capacitor 10 Ceramic laminate 11 Internal electrode layer 12 Dielectric layer 20 External electrode 21 External electrode layer 22 Plated layer
Claims
1. A conductive paste comprising inorganic particles, a binder resin, a dispersant, and an organic solvent, wherein the inorganic particles comprise conductive powder having a number average particle size of 0.05 μm or more and 0.3 μm or less, in an amount of 30% by mass or more and 70% by mass or less based on the entire conductive paste, the binder resin comprises a cellulose-based resin, the dispersant comprises an acid-based dispersant, and the conductive paste is subjected to a shear rate of 4 s -1 a viscosity at 2000° C. exceeds 10 Pa·s, and a ratio of conductive powder particles having a particle diameter exceeding twice the number average particle diameter of the conductive powder particles in the conductive paste is 50 ppm or less relative to a total number of the conductive powder particles.
2. The conductive paste according to claim 1, wherein the conductive powder contains at least one metal powder selected from the group consisting of Ni, Pd, Pt, Au, Ag, Cu, and alloys thereof.
3. A conductive paste according to claim 1 or 2, wherein the inorganic particles contain ceramic powder having a number average particle size of 0.01 μm or more and 0.3 μm or less in an amount of 1 mass % or more and 20 mass % or less based on the entire conductive paste.
4. The conductive paste of claim 3, wherein said ceramic powder comprises barium titanate.
5. The conductive paste according to claim 1 or 2, wherein the cellulose-based resin is contained in an amount of 0.1% by mass or more and 3.0% by mass or less based on the conductive paste.
6. The conductive paste according to claim 1 or 2, wherein the binder resin contains an acetal-based resin in an amount of 0.5% by mass or more and 3.0% by mass or less based on the entire conductive paste.
7. The conductive paste according to claim 1 or 2, wherein the acid dispersant is contained in an amount of 0.01 mass % or more and less than 1.0 mass % based on the entire conductive paste.
8. A method for producing a conductive paste according to claim 1, comprising: a first step of mixing inorganic particles, a binder resin, a dispersant, and an organic solvent to obtain an inorganic particle slurry; a second step of filtering the inorganic particle slurry through a filter having a filtration accuracy of 1.0 μm or less; and a third step of mixing the filtered inorganic particle slurry with a binder resin and an organic solvent.
9. The method for producing a conductive paste according to claim 8, wherein the binder resin in the inorganic particle slurry contains a cellulose-based resin.
10. The method for producing a conductive paste according to claim 8 or 9, wherein the binder resin in the inorganic particle slurry contains a cellulose-based resin and an acetal-based resin.
11. The inorganic particle slurry obtained in the first step is subjected to a shear rate of 4 s at room temperature (25°C). -1 The method for producing a conductive paste according to claim 8 or 9, wherein the viscosity of the conductive paste is 20 Pa·s or less.
12. The conductive paste according to claim 1 or 2, which is used for internal electrodes of multilayer ceramic parts.
13. An electronic component formed using the conductive paste according to claim 1 or 2.
14. A multilayer ceramic capacitor comprising at least a laminate in which dielectric layers and internal electrode layers are laminated, the internal electrode layers being formed using the conductive paste according to claim 1 or 2.