Circuit board and method for production thereof

MYPI2026002764A0Undetermined Publication Date: 2025-05-10NHK SPRING CO LTD
View PDF 0 Cites 0 Cited by

Patent Information

Application Number
MYPI2026002764
Authority / Receiving Office
MY · MY
Patent Type
Applications
Current Assignee / Owner
Priority Date
2023-11-10
Filing Date
2024-08-30
Publication Date
2025-05-10

AI Technical Summary

Technical Problem

Existing circuit boards for large currents in power devices face challenges in managing heat during the welding of conductive members, which can damage the insulating layer.

Method used

A circuit board design with a circuit pattern on an insulating layer, an additional metal layer laminated and joined to the circuit pattern, and a conductive member laminated on the additional metal layer and joined by welding, with specific thickness ranges to manage heat effectively.

Benefits of technology

The proposed solution effectively suppresses damage to the insulating layer by dispersing heat through the additional metal layer and circuit pattern, ensuring reliable connections in high-current applications.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure PI2026002764_DRAWING_001
    Figure PI2026002764_DRAWING_001
  • Figure PI2026002764_DRAWING_002
    Figure PI2026002764_DRAWING_002
  • Figure PI2026002764_DRAWING_003
    Figure PI2026002764_DRAWING_003
Patent Text Reader

Abstract

Provided is a circuit board capable of performing connection of a conductive material to an additional metal layer by welding. The circuit board includes a circuit pattern 3 provided on an insulating layer 7, an additional metal layer 9 stacked and bonded on the circuit pattern 3, and a lead frame 11 stacked on the additional metal layer 9 and connected to the additional metal layer by welding, wherein a total thickness of the additional metal layer 9 and the circuit pattern 3 in the stacking direction is 1.5mm to 3.0mm, and a thickness of the lead frame 11 in the stacking direction is 0.2mm to 1.2mm. Figure 1
Need to check novelty before this filing date? Find Prior Art

Description

Circuit board and manufacturing method thereof

[0001] The present invention relates to a circuit board used in a power device or the like, and a method for manufacturing the same.

[0002] Some circuit boards for large currents used in power devices and the like have circuit patterns that are partially thickened to reduce thermal resistance. For example, in Patent Document 1, an overlay circuit pattern is laminated on the circuit pattern as an additional metal layer in a portion where an electronic component such as a power semiconductor chip is to be attached. The electronic component is attached to this additional metal layer by soldering.

[0003] On the other hand, there is a demand for attaching conductive members such as lead frames to circuit boards by welding with a laser or soldering with local heating (laser soldering), etc. However, Patent Document 1 assumes that electronic components will be attached by soldering, and is not compatible with welding or laser soldering, which can reach higher temperatures.

[0004] Therefore, for example, when a conductive member is connected to a circuit pattern by welding, heat generated during welding is transferred from the circuit pattern to the interface between the resin insulating layer that supports the circuit pattern, potentially damaging the insulating layer.

[0005] Publication No. 2006-319146

[0006] The problem to be solved is that it is not possible to deal with the large amount of heat generated when connecting the conductive members.

[0007] The present invention provides a circuit board comprising: a circuit pattern provided on an insulating layer; an additional metal layer laminated on and joined to the circuit pattern; and a conductive member laminated on the additional metal layer and joined by welding, wherein the total thickness of the additional metal layer and the circuit pattern in the stacking direction is 1.5 mm to 3.0 mm, and the thickness of the conductive member in the stacking direction is 0.2 mm to 1.2 mm.

[0008] The present invention also provides a method for manufacturing a circuit board, comprising: a circuit pattern provided on an insulating layer; an additional metal layer laminated on and bonded to the circuit pattern; and a conductive member laminated on and bonded to the additional metal layer, wherein the total thickness of the additional metal layer and the circuit pattern in the stacking direction is 1.5 mm to 3.0 mm, and the thickness of the conductive member in the stacking direction is 0.2 mm to 1.2 mm, in which the conductive member is laminated on the additional metal layer and connected by laser welding.

[0009] According to the present invention, damage to the insulating layer due to heat when connecting the conductive member can be suppressed.

[0010] Fig. 1 is a cross-sectional view of a circuit board showing the periphery of a lead frame attachment portion according to a first embodiment of the present invention. Fig. 2 is a plan view of the circuit board of Fig. 1. Fig. 3 is a schematic cross-sectional view of a situation in which an additional metal layer is ultrasonically bonded to a circuit pattern. Fig. 4 is an enlarged cross-sectional view of a portion of the tool of Fig. 3 pressing against the additional metal layer. Fig. 5 is a cross-sectional view showing an experimental method according to the first embodiment. Fig. 6 is a graph plotting the experimental results of Fig. 5.

[0011] The objective of suppressing damage to the insulating layer due to heat when connecting the conductive members was achieved by adjusting the thickness in the stacking direction of the portion of the circuit pattern where the conductive members are connected and the thickness in the stacking direction of the conductive members.

[0012] The circuit board 1 includes a circuit pattern 3, an additional metal layer 9, and a conductive member 11. The circuit pattern 3 is provided on an insulating layer 7. The additional metal layer 9 is laminated and bonded onto the circuit pattern 3. The conductive member 11 is laminated onto the additional metal layer 9 and bonded by welding.

[0013] The total thickness of the additional metal layer 9 and the circuit pattern 3 in the stacking direction is 1.5 mm to 3.0 mm, and the thickness of the conductive member 11 in the stacking direction is 0.2 mm to 1.2 mm.

[0014] In this case, the thicknesses of the additional metal layer 9 and the circuit pattern 3 can be set arbitrarily as long as their total thickness is 1.5 mm to 3.0 mm. In one embodiment, the thickness of the additional metal layer 9 in the stacking direction may be 0.7 mm to 2.7 mm, and the thickness of the circuit pattern 3 in the stacking direction may be 0.3 mm to 0.8 mm.

[0015] In the manufacturing method of the circuit board 1, the conductive member 11 is laminated on the additional metal layer 9 and connected by laser welding.

[0016] In one embodiment, the method for manufacturing the circuit board 1 may include laminating an additional metal layer 9 on the circuit pattern 3, pressing a tool T against the connection surface 12 of the additional metal layer 9 to ultrasonically vibrate it to bond it. In this case, the conductive member 11 is laminated on the surface 12 of the additional metal layer 9 bonded onto the circuit pattern 3, and then connecting it by laser welding.

[0017] [Circuit Board] Fig. 1 is a cross-sectional view of a circuit board showing the periphery of a lead frame attachment portion according to a first embodiment of the present invention. Fig. 2 is a plan view of the circuit board of Fig. 1.

[0018] 1 and 2 is a circuit board for large current applications such as power devices. The circuit board 1 is a metal-based circuit board including a metal substrate 5, an insulating layer 7, a circuit pattern 3, an additional metal layer 9, and a lead frame 11 as a conductive member.

[0019] The metal substrate 5 is a plate-like body made of metal. The shape of the metal substrate 5 can be set appropriately, and a heat sink-shaped metal substrate can also be used.

[0020] The material of the metal substrate 5 can be, for example, a simple metal or an alloy such as aluminum, iron, copper, or stainless steel, and it does not matter whether the metal substrate 5 is flexible or not. The metal substrate 5 may further contain a non-metal such as carbon. The metal substrate 5 may also contain aluminum composited with carbon. The metal substrate 5 may have a single-layer structure or a multi-layer structure.

[0021] The thickness of the metal substrate 5 can be set appropriately, for example, to 2.0 mm. The metal substrate 5 has high thermal conductivity. For example, copper has a thermal conductivity of 370 to 400 W·m -1 ・K -1 , and aluminum materials: 190 to 220 W·m -1 ・K -1 , for iron materials, 60 to 80 W·m -1 ・K -1 It has a thermal conductivity of

[0022] The insulating layer 7 is laminated on the metal substrate 5 and formed in a plate shape. The insulating layer 7 not only serves to electrically insulate the circuit pattern 3 from the metal substrate 5, but also serves as an adhesive that bonds the circuit pattern 3 and the metal substrate 5 together. For this reason, a resin is generally used for the insulating layer 7. The thickness of the insulating layer 7 can be set as appropriate, but is set to, for example, 0.13 mm.

[0023] The insulating layer 7 of this embodiment can be made of epoxy resin, cyanate resin, or the like. Epoxy resin is combined with, for example, an amine-based curing agent, a phenol-based curing agent, an acid anhydride-based curing agent, or an imidazole-based curing agent. Cyanate resin is combined with, for example, dicyandiamide or a phenol resin as a curing agent. Furthermore, the insulating layer 7 may be made of a liquid crystal polymer such as a thermoplastic resin, such as a wholly aromatic polyester, or other thermoplastic resin.

[0024] Preferably, insulating layer 7 further contains an inorganic filler. The inorganic filler contained in insulating layer 7 preferably has excellent electrical insulation properties and high thermal conductivity. Examples of base-free fillers include alumina, silica, aluminum nitride, boron nitride, silicon nitride, and magnesium oxide, and it is preferable to use one or more types selected from these.

[0025] The filling rate of the inorganic filler in the insulating layer 7 can be set appropriately depending on the type of inorganic filler. For example, it is preferably 85% by volume or less, and more preferably 30 to 85% by volume, based on the total volume of the resin contained in the insulating layer 7.

[0026] The insulating layer 7 may further contain, for example, a coupling agent, a dispersant, etc. Note that a semi-cured insulating sheet may also be used as the insulating layer 7.

[0027] The circuit pattern 3 is provided on an insulating layer 7. As a result, the circuit pattern 3 is provided on an insulating substrate in which the insulating layer 7 is provided on a metal substrate 5. The circuit pattern 3 is a plate or foil, and is formed into a predetermined pattern by etching the conductors 3a.

[0028] The circuit pattern 3 of this embodiment is formed of a copper material, which is a conductor for circuits, and has a thickness of 0.3 mm to 0.8 mm, for example 0.5 mm. The circuit pattern 3 has a constant thickness except for the laminated portion of the additional metal layer 9. However, the thickness of the circuit pattern 3 may be varied.

[0029] The circuit pattern 3 may also be made of aluminum or the like. The circuit pattern 3 may be formed in advance by pressing or cutting, rather than by etching, and may be attached to the metal substrate 5 via an insulating layer 7.

[0030] In this embodiment, a lead frame 11, which is another member, is connected to the circuit pattern 3. In the portion of the circuit pattern 3 where the lead frame 11 is connected, an additional metal layer 9 is laminated and bonded, making the portion thicker.

[0031] The additional metal layer 9 is formed in a plate shape. In this embodiment, the additional metal layer 9 is made of copper, but it may be made of other circuit conductors such as aluminum. The planar shape of the additional metal layer 9 is, for example, a 10 mm square. However, the planar shape of the additional metal layer 9 can be set arbitrarily.

[0032] The thickness of the additional metal layer 9 in the stacking direction is 0.7 mm to 2.7 mm. In this embodiment, the thickness of the additional metal layer 9 in the stacking direction is greater than the thickness of the circuit pattern 3 in the stacking direction, but it may be smaller than the thickness of the circuit pattern 3 in the stacking direction. This additional metal layer 9 has a constant thickness. The total thickness of the circuit pattern 3 and the additional metal layer 9 is 1.5 mm to 3.0 mm.

[0033] The additional metal layer 9 has a bonding surface 10 on one side in the stacking direction, which is the bottom surface that faces the circuit pattern 3, and a connection surface 12 on the other side, which is the surface that faces the lead frame 11.

[0034] The bonding surface 10 is bonded to the circuit pattern 3 over the entire area facing the stacking direction. The bonding is performed by ultrasonic welding. The connection surface 12 is the portion that connects the lead frame 11 by laser welding. This connection surface 12 has an uneven portion 17. In this embodiment, the uneven portion 17 is provided on the entire surface of the connection surface 12. The "entire surface" means roughly the entire surface, and also includes cases where part or all of the outer peripheral region of the connection surface 12 is flat.

[0035] This uneven portion 17 is formed by a tool uneven portion 15 (described later in FIG. 5) of a vibration transmission tool T (described later in FIG. 5) for bonding the additional metal layer 9 onto the circuit pattern 3 by ultrasonic vibration in the planar direction.

[0036] The uneven portion 17 can have various planar shapes and cross-sectional shapes, but in any case, it has engaging recesses 17 a and engaging protrusions 17 b. The intervals and sizes of the engaging recesses 17 a and engaging protrusions 17 b are set regularly, but can also be set randomly.

[0037] Each engaging recess 17a of the uneven portion 17 is formed in a quadrangular shape in a plan view and has an inverted square pyramid shape in cross section. The shape of the engaging recess 17a of the uneven portion 17 is not particularly limited, and it may be a recess formed with a curved surface, etc. Each engaging protrusion 17b of the uneven portion 17 has a quadrangular pyramid shape. The uneven portion 17 including the engaging recess 17a and the engaging protrusion 17b is an indentation of the tool uneven portion 15 described below, and can be formed in an appropriate shape depending on the shape of the tool uneven portion 15.

[0038] The lead frame 11 is connected to the connection surface 12 in the stacking direction by laser welding. The lead frame 11 is a rectangular plate and is bent or otherwise formed as needed. The lead frame 11 is pulled out laterally from the connection surface 12 in a direction intersecting the stacking direction. The lead frame 11 has a gap in the intersecting direction between it and the uneven portion 17, excluding the pulled-out portion. The thickness of the lead frame 11 in the stacking direction is 0.2 mm to 1.2 mm. The lead frame 11 is made of a material such as copper, iron, or an alloy thereof.

[0039] The shape of the lead frame 11 can be set arbitrarily. The conductive member connected to the connection surface 12 is not limited to the lead frame 11, and can be made of other conductive materials.

[0040] [Method of Manufacturing Circuit Board] Fig. 3 is a schematic cross-sectional view of a state in which an additional metal layer 9 is ultrasonically bonded to a circuit pattern 3 according to Example 1. Fig. 4 is an enlarged cross-sectional view of a portion of the tool T in Fig. 3 that is pressed against the additional metal layer 9.

[0041] 3 and 4, this manufacturing method uses a tool T. Note that Fig. 3 shows an example in which a tool T having a square shape of 12 mm is used for a 10 mm square additional metal layer 9. It is also possible to use a tool T that is smaller than the additional metal layer 9.

[0042] The tool T has a cross-sectional shape including a tool concave-convex portion 15 that corresponds to the concave-convex portion 17. The tool concave-convex portion 15 has tool concave portions 15a and tool convex portions 15b that are formed to correspond to the engaging convex portions 17b and engaging concave portions 17a of the concave-convex portion 17.

[0043] In the manufacturing method of this embodiment using this tool T, an additional metal layer 9 is laminated on the circuit pattern 3. Then, the tool T is pressed against the connection surface 12 of the additional metal layer 9 and ultrasonic vibrations are applied. As a result, the ultrasonic vibrations are transmitted to bond the additional metal layer 9 onto the circuit pattern 3. This bonding is performed over the entire bonding surface 10 that corresponds in the stacking direction to the portion of the connection surface 12 of the additional metal layer 9 that the tool T pressed against.

[0044] In this embodiment, by pressing the tool T, an uneven portion 17 is formed on the connection surface 12 of the additional metal layer 9 in accordance with the tool uneven portion 15 .

[0045] After bonding the additional metal layer 9 onto the circuit pattern 3 in this manner, the lead frame 11 is connected to the connection surface 12 of the additional metal layer 9, as shown in Figures 1 and 2. This connection is made by positioning the connected portion 14 of the lead frame 11 on the connection surface 12 of the additional metal layer 9. In this state, a laser is irradiated from above the connected portion 14 of the lead frame 11, thereby welding the lead frame 11 and the additional metal layer 9 together.

[0046] At this time, the laser intensity is set according to the thickness of the lead frame 11. In other words, the laser intensity is set to a level that melts the lead frame 11 having a thickness of 0.2 mm to 1.2 mm to the extent that it can be joined to the additional metal layer 9 thereunder. The laser intensity is changed depending on the quality of the conductive material of the lead frame 11, etc., such as the laser absorption rate and melting point of the material.

[0047] Based on this laser intensity setting, the heat generated during welding is dispersed by the additional metal layer 9 having a thickness of 1.5 mm to 3.0 mm and the circuit pattern 3, thereby suppressing the effect on the insulating layer 7. The heat dissipation ability depends on the materials of the additional metal layer 9 and the circuit pattern 3, such as the thermal conductivity of the materials.

[0048] [Experimental Results] Fig. 5 is a cross-sectional view showing the experimental method according to Example 1. As shown in Fig. 5, in the experiment, the additional metal layer 9 was bonded to the surface of the circuit pattern 3 over the entire bonding surface 10. Then, welding was performed by irradiating the lead frame 11 stacked on the connection surface 12 of the additional metal layer 9 with a laser L.

[0049] The temperature of the rear surface of the circuit pattern 3 at this time was measured at a portion TC corresponding to the laser irradiated portion. The rear surface of the circuit pattern 3 is the surface located on the opposite side in the stacking direction from the surface of the lead frame 11 that was irradiated with the laser.

[0050] The lead frame 11 was made of copper and had thicknesses of 0.2 mm, 0.5 mm, and 1.0 mm. The circuit pattern 3 and additional metal layer 9 were made of copper. The total thickness of the circuit pattern 3 and additional metal layer 9 was 0.5 mm to 3.0 mm. The laser intensity was changed to 500 W, 750 W, and 1300 W depending on the thickness of the lead frame 11, and was set so that the additional metal layer 9 melted by 0.2 mm ± 0.1 mm.

[0051] Figure 6 is a graph plotting the experimental results of Figure 5. The vertical axis represents the peak temperature on the back surface of the circuit pattern 3 (peak circuit back surface temperature), and the horizontal axis represents the total thickness of the circuit pattern 3 and the additional metal layer 9 (total circuit thickness). In Figure 6, 0.2 mm 500 W indicates that the thickness of the lead frame 11 is 0.2 mm and the laser intensity is 500 W. The same applies to 0.5 mm 750 W and 1.0 mm 1300 W.

[0052] As shown in Figure 6, when the thickness of the lead frame 11 is 0.2 mm to 1.2 mm (the laser intensity corresponds to the thickness of the lead frame 11) and the total thickness of the additional metal layer 9 and the circuit pattern 3 in the stacking direction is 1.5 mm to 3.0 mm, damage to the insulating layer 7 can be suppressed. If the total circuit thickness is less than 1.5 mm, the peak temperature on the back surface of the circuit will be 105 or higher, which will damage the insulating layer 7. On the other hand, if the total circuit thickness is 1.5 mm or more, the peak temperature on the back surface of the circuit will be within a range that will not damage the insulating layer 7 up to the upper limit of the total thickness of 3.0 mm. Note that if the total thickness exceeds 3.0 mm, the device will become too large, making ultrasonic bonding difficult, and the suppression of the back surface temperature will tend to saturate, resulting in problems such as increased material thermal resistance. For this reason, the upper limit of the total thickness is set to 3.0 mm.

[0053] The insulating layer 7 is made of a liquid crystal polymer and contains boron nitride and alumina. The insulating layer 7 is subject to considerable damage when the peak temperature on the back surface of the circuit reaches approximately 100°C, although the degree of damage varies depending on the heat resistance temperature of the resin. The additional metal layer 9 and the circuit pattern 3 are made of copper, as described above. However, the range of the total thickness does not vary significantly depending on the materials used for the insulating layer 7, circuit pattern 3, and additional metal layer 9 of the circuit board 1.

[0054] The circuit board 1 manufactured in this manner can be a high-quality product in which damage to the insulating layer 7 is suppressed even if the heat rises when joining the lead frame 11, for example, by joining the lead frame 11 to the additional metal layer 9 by laser welding.

[0055] REFERENCE SIGNS LIST 1 Circuit board 3 Circuit pattern 7 Insulating layer 9 Additional metal layer 10 Bonding surface 10a Bonding portion 10b Non-bonding portion 11 Lead frame (conductive member) 12 Connection surface (surface) 13 Connection portion (surface) 17 Concave and recessed portion

Claims

1. A circuit board comprising: a circuit pattern provided on an insulating layer; an additional metal layer laminated and joined onto said circuit pattern; and a conductive member laminated and joined onto said additional metal layer, wherein the total thickness of said additional metal layer and said circuit pattern in said stacking direction is 1.5 mm to 3.0 mm, and the thickness of said conductive member in said stacking direction is 0.2 mm to 1.2 mm.

2. The circuit board according to claim 1, wherein the thickness of said additional metal layer in said stacking direction is 0.7 mm to 2.7 mm, and the thickness of said circuit pattern in said stacking direction is 0.3 mm to 0.8 mm.

3. A method for manufacturing a circuit board comprising: a circuit pattern provided on an insulating layer; an additional metal layer laminated and joined onto the circuit pattern; and a conductive member laminated and joined onto the additional metal layer, wherein the total thickness of the additional metal layer and the circuit pattern in the lamination direction is 1.5 mm to 3.0 mm, and the thickness of the conductive member in the lamination direction is 0.2 mm to 1.2 mm, wherein the conductive member is laminated on the additional metal layer and connected by laser welding.

4. A method for manufacturing a circuit board as claimed in claim 3, comprising the steps of: laminating the additional metal layer on the circuit pattern; pressing a tool against a surface of the additional metal layer and ultrasonically vibrating it to bond the additional metal layer onto the circuit pattern; and laminating the conductive member on the surface of the additional metal layer bonded onto the circuit pattern and connecting them by laser welding.