Method for preparing high-pressure leaching solution and method for preparing nickel cobalt hydroxide

PH12025050203A1Pending Publication Date: 2026-09-28ZHEJIANG HUAYOU COBALT CO LTD
0 Cites 0 Cited by

Patent Information

Application Number
PH12025050203
Authority / Receiving Office
PH · PH
Patent Type
Applications
Current Assignee / Owner
Filing Date
2025-03-28
Publication Date
2026-09-28
Patent Text Reader

Abstract

Provided are a method for preparing a high-pressure leaching solution and a method for preparing nickel cobalt hydroxide. The method includes: performing a high-pressure acid leaching treatment on a reductive nickel laterite slurry to obtain a high-pressure leaching solution. The reductive nickel laterite slurry is mixed with an oxidant prior to the high-pressure acid leaching treatment, and / or the reductive nickel laterite slurry is added with the oxidant during the high-pressure acid leaching treatment. The method has a simple production process, and reduces the smelting cost of reductive nickel laterite.
Need to check novelty before this filing date? Find Prior Art