Limited solid-solution-type phase with a scheelite-type structure and method for producing said phase

PL452105A1Pending Publication Date: 2026-11-23ZACHODNIOPOMORSKI UNIWERSYTET TECHNOLOGICZNY W SZCZECINIE
View PDF 0 Cites 0 Cited by

Patent Information

Application Number
PL2025452105
Authority / Receiving Office
PL · PL
Patent Type
Applications
Current Assignee / Owner
Filing Date
2025-05-21
Publication Date
2026-11-23
Patent Text Reader

Abstract

The subject of the application is a confined solid solution phase with a scheelite-type structure, doped with a d-electron trivalent metal ion and a rare-earth metal ion with the general formula Ca1-3(x+y)x+yFe2xRE2yWO4, where the d-electron metal is iron and the rare-earth metal is neodymium or europium, 0 <x≤0,025, 0<y≤0,06, a oznacza luki w sieci krystalicznej roztworu.The application also covers a method for producing a phase of a confined solid solution type with a scheelite-type structure, doped with a d-electron trivalent metal ion and a rare-earth metal ion, consisting in mixing, homogenizing, annealing and cooling, characterized in that calcium carbonate in an amount of not less than 41.89 mol% and less than 47.96 mol% is mixed with a rare-earth metal oxide in an amount of not more than 3.24 mol%, tungsten(VI) oxide in an amount of more than 51.02 mol% and not more than 54.06 mol% and iron(III) oxide in an amount of not more than 1.30 mol%. The mixture is heated at a temperature of 900°C to 1175°C, then cooled to obtain a product with the general formula Ca1-3(x+y) x+yFe2xRE2yWO4, where RE is neodymium or europium, 0 <x≤0,025, 0<y≤0,06, a oznacza luki w sieci krystalicznej roztworu.
Need to check novelty before this filing date? Find Prior Art