Catalyst for Hydrogen Peroxide Activation
A titanium-silicon-oxygen catalyst with tailored water adsorption and µ2η2-peroxy bridging species concentrations addresses the lack of catalytic activity and selectivity in hydrogen peroxide activation, enhancing epoxide addition reactions.
Patent Information
- Application Number
- SA1120242925
- Authority / Receiving Office
- SA · SA
- Patent Type
- Patents
- Current Assignee / Owner
- Filing Date
- 2024-05-28
- Publication Date
- 2026-10-04
- Estimated Expiration
- 2042-11-29
AI Technical Summary
Existing catalysts for hydrogen peroxide activation lack a high correlation between catalytic activity and selectivity, limiting their effectiveness in processes such as epoxide addition reactions.
A catalyst composed of titanium, silicon, and oxygen, with specific water adsorption and µ2η2-peroxy bridging species concentrations, determined by 17O NMR quantitative spectroscopy, is developed to enhance catalytic activity and selectivity.
The catalyst exhibits improved catalytic activity and selectivity in hydrogen peroxide activation, particularly for epoxide addition reactions like the conversion of propylene to propylene oxide, with optimized water adsorption and bridging species concentrations.
Abstract
Description
Detailed description: Therefore, the objective of the present invention is to provide an improved catalyst for hydrogen peroxide activation. Specifically, the aim of the present invention is to provide a catalyst that exhibits a specific activating factor with a high correlation between both catalytic activity and catalytic selectivity, and thus can be considered a material in light of its improved catalytic performance. Furthermore, the objective of the present invention is to provide an improved process for hydrogen peroxide activation, utilizing a catalyst that exhibits a specific activating factor. Surprisingly, it was found that the improved catalysts that could be provided exhibit unique activation factors. Specifically, it was found that the water adsorption doubling product and the bridging concentration of µ2η2-peroxygenated species for each metal in the hydrogen peroxide-activated catalyst, as determined by 17O NMR quantitative spectroscopy, provide the innovative catalyst with a unique activation factor that is not only related to its catalytic activity but also distinguishes it from the aforementioned innovative catalysts. Furthermore, it was found that an improved hydrogen peroxide activation process could be provided in light of this activation factor, thus providing improved catalysts according to the present invention. Therefore, it was found that a catalyst with unique physical and chemical properties could be provided, and that the aforementioned catalyst allows for improved catalytic activity, specifically in hydrogen peroxide activation for oxidation, and specifically for epoxide addition reactions such as the conversion of propylene and hydrogen peroxide to propylene oxide. Therefore, the present invention relates to a catalyst containing titanium, silicon, and oxygen, where the catalyst exhibits water adsorption, preferentially determined according to Reference Example 1.1, a concentration (c) of µ2η2-peroxy bridging species per titanium in the hydrogen peroxide-activated catalyst as determined by 17O NMR quantitative spectroscopy, preferentially determined according to Reference Example 1.3, and an activation factor (a) according to Formula I, where the activation factor is in the range of 15 to 80 mM mol / mol; According to formula I, the activation factor is the product of the water adsorption multiplication and the bridging concentration of µ2η2-peroxy species per titanium in the hydrogen peroxide-activated catalyst: A=WxC(I). Ideally, the catalyst should exhibit water adsorption in the range of 1 to 10 wt%, with 1.5 to 9.5 wt% being best, 2 to 9 wt% best, 2.5 to 8.5 wt% best, 3 to 8 wt% best, 3.2 to 7.9 wt% best, 3.5 to 7.5 wt% best, 4 to 7 wt% best, 4.5 to 6.5 wt% best, and 5 to 6 wt% best. It has been observed that for water adsorption of x wt%, this value corresponds to x% g / g = (x / 100) g / g = W. Therefore, for example, water adsorption of 1 wt% = 1% g / g = 0.01 g / g = W. In addition to the above and independently of it, the catalyst should preferably exhibit a concentration of µ2η2-peroxy-type bridging per titanium in the hydrogen peroxide-activated catalyst in the range of 200 to 1,200 mmol / mol, better than 300 to 1,000 mmol / mol, better than 350 to 950 mmol / mol, better than 400 to 900 mmol / mol, better than 450 to 850 mmol / mol, better than 500 to 800 mmol / mol, better than 550 to 750 mmol / mol, and better than 600 to 700 mmol / mol.In addition to the above and independently of it, the concentration (c) for bridging µ2η2-peroxy species per titanium in the hydrogen peroxide-activated catalyst, as determined by 17O NMR quantitative spectroscopy, is the concentration determined at a time point T after the catalyst comes into contact with H217O2, where T is in the range of 1 to 720 mins after the catalyst comes into contact with H217O2, best of all 2 mins to 480 mins, best of all 4 to 240 mins, best of all 6 to 120 mins, best of all 8 to 60 mins, best of all 10 to 30 mins, best of all 12 to 20 mins, and best of all 14 to 16 mins, where T is best of all 15 mins. In addition to the above and independently of it, the activating factor should preferably be in the range of 16 to 70 mmol / mol, better than 18 to 60 mmol / mol, better than 20 to 55 mmol / mol, better than 23 to 50 mmol / mol, better than 25 to 45 mmol / mol, better than 26 to 44 mmol / mol, better than 27 to 42 mmol / mol, better than 28 to 40 mmol / mol, better than 29 to 37 mmol / mol, and better than 30 to 35 mmol / mol. Alternatively, the catalyst should ideally exhibit a 200–825 mM / mol concentration for bridging µ2η2-peroxy-tetanium species in the hydrogen peroxide-activated catalyst. The µ2η2-peroxy-tetanium bridging concentration in the hydrogen peroxide-activated catalyst, as determined by quantitative 17O NMR spectroscopy, is the concentration determined at a time point T after the catalyst comes into contact with H₂₁₇O₂, where T is in the range of 65–175 minutes. Furthermore, and independently of the above, the catalyst should ideally exhibit water adsorption in the range of 1–7.9 wt%, 3–7.5 wt%, 4–7 wt%, 4.5–6.5 wt%, and 5–6 wt%. In addition to the above and independently of it, the catalyst should preferably exhibit a concentration of µ2η2-peroxy bridging species per titanium in the hydrogen peroxide-activated catalyst as determined by 17O NMR quantitative spectroscopy, as best determined according to Reference Example 1.3, in the range of 300 to 822 mmol / mol, better than 350 to 800 mmol / mol, better than 400 to 780 mmol / mol, better than 450 to 760 mmol / mol, better than 500 to 740 mmol / mol, better than 550 to 720 mmol / mol, and better than 600 to 700 mmol / mol. In addition to the above and independently of it, T is preferably in the range of 75 to 165 minutes, better than 85 to 155 minutes, better than 95 to 145 minutes, better than 105 to 135 minutes, better than 112 to 128 minutes, better than 116 to 124 minutes, better than 118 to 122 minutes, and better than 119 to 121 minutes, where T is best at 120 minutes.In addition to the above and independently of it, the activating factor should preferably be in the range of 16 to 75 mmol / mol, better than 18 to 67 mmol / mol, better than 20 to 65 mmol / mol, better than 22 to 60 mmol / mol, better than 24 to 55 mmol / mol, better than 26 to 50 mmol / mol, better than 27 to 45 mmol / mol, better than 28 to 40 mmol / mol, better than 29 to 37 mmol / mol, and better than 30 to 34 mmol / mol. The catalyst preferably exhibits an X-ray absorption spectrum near the edge structure (XANES) with a signal intensity ratio at 4987 eV to a signal intensity ratio at 4992 eV in the range of 0.95:1 to 1.07:1, better than 0.97:1 to 1.07:1, better than 0.99:1 to 1.07:1, better than 1.01:1 to 1.07:1, better than 1.03:1 to 1.07:1, and best than 1.05:1 to 1.07:1, where the X-ray absorption spectrum near the edge structure is best defined according to Reference Example 1.2. The catalyst, according to the present invention, should preferably include a Brunauer, Emmett, and Teller (BET) specific surface area in the range of 350 to 475 m² / g, preferably 370 to 455 m² / g, preferably 390 to 435 m² / g, where the Brunauer, Emmett, and Teller specific surface area is preferred according to Reference Example 1.5. The catalyst, according to the present invention, should preferably contain 0.5 to 2.5% by weight, better than 0.8 to 2.0% by weight, better than 1.0 to 1.9% by weight, better than 1.0 to 1.8% by weight, better than 1.1 to 1.3% by weight of titanium, calculated by element and based on the total weight of the catalyst. The catalyst, according to the present invention, should preferably contain 0 to 1% by weight, preferably 0 to 0.1% by weight, preferably 0 to 0.01% by weight, preferably 0 to 0.001% by weight of B, calculated by element and based on the total weight of the catalyst. The catalyst, according to the present invention, should preferably contain 0 to 1% by weight, preferably 0 to 0.1% by weight, preferably 0 to 0.01% by weight, preferably 0 to 0.001% by weight of Na, calculated by element and based on the total weight of the catalyst. The catalyst, according to the present invention, should preferably contain 0 to 1% by weight, preferably 0 to 0.1% by weight, preferably 0 to 0.01% by weight, preferably 0 to 0.001% by weight of Ge, calculated by element and based on the total weight of the catalyst. The catalyst, according to the present invention, should preferably contain 0 to 1% by weight, preferably 0 to 0.5% by weight, better still 0 to 0.2% by weight, better still 0 to 0.1% by weight of C, calculated by element and based on the total weight of the catalyst. The catalyst, according to the present invention, should preferably exhibit propylene oxide activity of at least 2.0% wt%, preferably in the range of 3.0 to 15.0% wt%, best in the range of 9.0 to 13.0% wt%, preferably defined as shown in Reference Example 1.6. The catalyst should preferably also include one or more selected metals from the group consisting of Zinc (Zn), Cadmium (Cd), Tin (Sn), Lanthanum (La), and Barium (Ba), which includes mixtures of two or more of them. It is preferable that 95 to 100% by weight of the catalyst be composed of titanium, silicon, and oxygen, better than 97 to 100% by weight, better than 98 to 100% by weight, better than 99 to 100% by weight, better than 99.5 to 100% by weight, and better than 99.9 to 100% by weight. It is preferable that 95 to 100% by weight of the catalyst be composed of titanium, silicon, oxygen, and hydrogen, better than 97 to 100% by weight, better than 98 to 100% by weight, better than 99 to 100% by weight, better than 99.5 to 100% by weight, and better than 99.9 to 100% by weight. Ideally, the catalyst should include, or better yet consist of, a zeolite material with a framework structure that includes silicon, titanium, and oxygen. In the case where the catalyst includes a zeolite material with a framework structure that includes silicon, titanium, and oxygen, it is preferable that the zeolite material has a silicon:titanium molar ratio in the range of 1 to 250, better in the range of 10 to 150, better in the range of 20 to 95, better in the range of 30 to 75, better in the range of 35 to 70, better in the range of 40 to 65, better in the range of 45 to 60, and better in the range of 50 to 55. Furthermore, and independently, where the catalyst contains a zeolite with a framework structure including silicon, titanium, and oxygen, it is preferable that the zeolite incorporate a framework structure type selected from the group consisting of MFI, MEL, MWW, ITH, IWR, IMF, SVY, FER, SVR, and intergrowth structures of two or more of these, or preferably from the group consisting of MFI, MEL, MWW, ITH, and IWR, and intergrowth structures of two or more of these, or preferably from the group consisting of MFI, MEL, and intergrowth structures, where the zeolite incorporates an MFI framework structure. Furthermore, and independently, it is preferable that the zeolite be a titanium-1 silicate zeolite. Furthermore, and independently of it, it is preferable that the zeolite material also includes one or more selected metals from the group consisting of zinc, cadmium, tin, lanthanum, and barium, which includes mixtures of two or more of them, since one or more of the metals are better contained in the pores of the zeolite material. Furthermore, and independently of it, it is preferable that 95 to 100% by weight of the zeolite material be composed of titanium, silicon, and oxygen, better than 97 to 100% by weight, better than 98 to 100% by weight, better than 99 to 100% by weight, better than 99.5 to 100% by weight, and better than 99.9 to 100% by weight. Furthermore, and independently of it, it is preferable that 95 to 100% by weight of the zeolite material be composed of titanium, silicon, oxygen, and hydrogen, better than 97 to 100% by weight, better than 98 to 100% by weight, better than 99 to 100% by weight, better than 99.5 to 100% by weight, and better than 99.9 to 100% by weight. Furthermore, and independently of it, it is preferable that the zeolite material includes crystallization in the range of 50 to 100% by weight, better than 75 to 100% by weight, better than 80 to 100% by weight, and better than 90 to 100% by weight, where crystallization has been determined preferentially as shown in Reference Example 1.4. The present invention also relates to a method for preparing catalyst molds, which includes (a) To provide in accordance with any of the embodiments specified and preferred in accordance with the present invention; (b) Mix the catalyst provided in step (a) with one or more binding materials; (c) Optionally knead the mixture obtained in step (b); (d) Molding the mixture obtained in step (b) or (c) to obtain one or more molds; (e) Optionally, dry one or more of the molds obtained in step (d); and (f) Toasting the molds obtained in step (d) or (e). The catalyst should preferably be provided in (a) the selection of a catalyst from among those that include titanium, silicon, and oxygen, and exhibit water adsorption (W), preferably determined according to Reference Example 1.1, and Concentration (c) of µ2η2-peroxy bridging species per titanium in hydrogen peroxide-activated catalyst as determined by 17O quantitative NMR spectroscopy, preferably according to reference example 1.3; The catalyst is selected by calculating the activation factor (A) according to the formula I for each of the catalysts, and selecting a catalyst that exhibits an activation factor in the range of 15 to 80 mM mol / mol, where the activation factor is the product of the water adsorption multiplication and the bridging concentration of the µ2η2-peroxy species per titanium in the hydrogen peroxide-activated catalyst: A=WxC(I). In the case where the provision of the catalyst in (a) involves choosing the catalyst from among catalysts that include titanium, silicon, and O, it is preferable to provide the catalyst in (a) choosing the catalyst from among catalysts that exhibit water adsorption in the range of 1 to 10% by weight, preferably 1.5 to 9.5% by weight, better than 2 to 9% by weight, better than 2.5 to 8.5% by weight, better than 3 to 8% by weight, better than 3.2 to 7.9% by weight, better than 3.5 to 7.5% by weight, better than 4 to 7% by weight, better than 4.5 to 6.5% by weight, and better than 5 to 6% by weight. Furthermore, and independently of it, it is preferable to provide the catalyst in (a) the selection of the catalyst from among the catalysts that exhibit a concentration for bridging µ2η2-peroxy species per titanium in the hydrogen peroxide-activated catalyst in the range of 200 to 1,200 mL mol / mol, better than 300 to 1,000 mL mol / mol, better than 350 to 950 mL mol / mol, better than 400 to 900 mL mol / mol, better than 450 to 850 mL mol / mol, better than 500 to 800 mL mol / mol, better than 550 to 750 mL mol / mol, and better than 600 to 700 mL mol / mol.Furthermore, and independently of it, it is preferable that the catalyst be selected by calculating the activation factor (A) for each of the catalysts, and selecting a catalyst that exhibits an activation factor in the range of 16 to 70, better than 18 to 60 mmol / mol, better than 20 to 55 mmol / mol, better than 23 to 50 mmol / mol, better than 25 to 45 mmol / mol, better than 26 to 44 mmol / mol, better than 27 to 42 mmol / mol, better than 28 to 40 mmol / mol, better than 29 to 37 mmol / mol, and better than 30 to 35 mmol / mol.Furthermore, and independently of it, the concentration (c) for bridging µ2η2-peroxy species per titanium in the hydrogen peroxide-activated catalyst, as determined by 17O NMR quantitative spectroscopy, is the concentration determined at a time point T after the catalyst comes into contact with H217O2, where T is in the range of 1 to 720 mins after the catalyst comes into contact with H217O2, best of all 2 mins to 480 mins, best of all 4 to 240 mins, best of all 6 to 120 mins, best of all 8 to 60 mins, best of all 10 to 30 mins, best of all 12 to 20 mins, and best of all 14 to 16 mins, where T is best of all 15 mins. Alternatively, it is preferable to provide the catalyst in (a) the selection of the catalyst from among those that exhibit a concentration (c) of µ2η2-peroxy-type bridging per titanium in the hydrogen peroxide-activated catalyst as determined by the 17O NMR quantitative spectrometer in the range of 200 to 825 mM mol / mol, where the concentration (c) of µ2η2-peroxy-type bridging per titanium in the hydrogen peroxide-activated catalyst as determined by the 17O NMR quantitative spectrometer is the concentration determined at a time point T after the catalyst comes into contact with H217O2, where T is in the range of 65 to 175 min. In addition to the above and independently of it, it is preferable to provide the catalyst in (a) choosing the catalyst from among the catalysts that show water adsorption in the range of 1 to 7.9% by weight, better than 3 to 7.5% by weight, better than 4 to 7% by weight, better than 4.5 to 6.5% by weight, and better than 5 to 6% by weight.In addition to the above and independently of it, it is preferable to provide the catalyst in (a) the selection of the catalyst from among the catalysts that exhibit a concentration of (c) for bridging µ2η2-peroxy species per titanium in the hydrogen peroxide-activated catalyst as determined by the 17O NMR quantitative spectroscopy, as best determined according to Reference Example 1.3, in the range of 300 to 822 mmol / mol, best of 350 to 800 mmol / mol, best of 400 to 780 mmol / mol, best of 450 to 760 mmol / mol, best of 500 to 740 mmol / mol, best of 550 to 720 mmol / mol, and best of 600 to 700 mmol / mol. In addition to the above and independently of it, T is preferably in the range of 75 to 165 minutes, better than 85 to 155 minutes, better than 95 to 145 minutes, better than 105 to 135 minutes, better than 112 to 128 minutes, better than 116 to 124 minutes, better than 118 to 122 minutes, and better than 119 to 121 minutes, where T is best at 120 minutes.In addition to the above and independently of it, the activation factor (A) should preferably be in the range of 16 to 75 mmol / mol, better than 18 to 67 mmol / mol, better than 20 to 65 mmol / mol, better than 22 to 60 mmol / mol, better than 24 to 55 mmol / mol, better than 26 to 50 mmol / mol, better than 27 to 45 mmol / mol, better than 28 to 40 mmol / mol, better than 29 to 37 mmol / mol, and better than 30 to 34 mmol / mol. In (a) the selection of catalysts, it is preferable to provide the catalyst in (a) the selection of the catalyst among catalysts that include 0 to 1% by weight, better than 0 to 0.1% by weight, better than 0 to 0.01% by weight, better than 0 to 0.001% by weight than B, calculated by element and based on the total weight of the catalyst. It is preferable to provide the catalyst in (a) choosing the catalyst from among catalysts that include 0 to 1% by weight, better than 0 to 0.1% by weight, better than 0 to 0.01% by weight, better than 0 n lang="ar-SA">to 0.001% by weight of Na, calculated by element and based on the total weight of the catalyst. It is preferable to provide the catalyst in (a) choosing the catalyst from among catalysts that include 0 to 1% by weight, better than 0 to 0.1% by weight, better than 0 to 0.01% by weight, better than 0 to 0.001% by weight of Ge, calculated by element and based on the total weight of the catalyst. It is preferable to provide the catalyst in (a) choosing the catalyst from among catalysts that include 0 to 1% by weight, better than 0 to 0.5% by weight, better than 0 to 0.2% by weight, better than 0 to 0.1% by weight of C, calculated by element and based on the total weight of the catalyst. The catalyst should preferably be provided in (a) the selection of the catalyst from among catalysts that exhibit propylene oxide activity of at least 2.0% wt%, best in the range of 3.0 to 15.0% wt%, best in the range of 9.0 to 13.0% wt%, as best defined as shown in Reference Example 1.6. It is preferable to select one or more of the binders in (b) from the group of inorganic binders, where one or more of the binders better include one or more sources of metal oxide and / or metalloid oxide, or better yet one or more sources of metal oxide and / or metalloid oxide selected from the group consisting of silica, alumina, titania, zirconia, lanthana, magnesia, and mixtures thereof and / or mixtures of two or more of these, rather than from the group consisting of silica, alumina, titania, zirconia, magnesia, mixtures of silica-alumina, mixtures of silica-titania, mixtures of silica-zirconia, mixtures of silica-lanthana, mixtures of Silica-zirconia-lanthanum, alumina-titania mixed oxides, alumina-zirconia mixed oxides, alumina-lanthanum mixed oxides, alumina-zirconia-lanthanum mixed oxides, titania-zirconia mixed oxides, and mixtures thereof and / or mixtures of two or more of these, better than the groupConsisting of silica, alumina, silica-alumina mixed oxides, and mixtures thereof of two or more of them, where preferably one or more of the binding materials in (b) include one or more silica sources, where preferably one or more of the binding materials in (b) are composed of one or more silica sources, where preferably one or more of the silica sources include one or more of the selected compounds from the group consisting of fumed silica, colloidal silica, silica-alumina, colloidal-alumina silica, and mixtures thereof of two or more of them, preferably one or more of the selected compounds from the group consisting of fumed silica, colloidal silica, and mixtures thereof, where preferably one or more of the binding materials in (b) are colloidal silica. It is preferable that step (b) also includes mixing the zeolite material and one or more binding materials with a solvent system, where the solvent system includes one or more solvents, preferably hydrophilic solvents, preferably selected from the group consisting of polar solvents, rather than the group consisting of polar protic solvents, preferably including one or more polar protic solvents selected from the group consisting of water, alcohols, carboxylic acids, and mixtures of two or more of them, rather than the group consisting of water, C1-C5 alcohols, C1-C5 carboxylic acids, and mixtures of two or more of them, rather than the group consisting of water, C1-C4 alcohols, C1-C4 carboxylic acids, and mixtures of two or more of them, rather than the group consisting of water. C1-C3 alcohols, C1-C3 carboxylic acids, and mixtures of two or more of them, are better than the group consisting of water, methanol,Ethanol, propanol, formic acid, acetic acid, and mixtures of two or more of these, are better than the combination of water, ethanol, acetic acid, and mixtures of two or more of these, where the solvent system better includes water and / or ethanol, where the solvent system better includes water, where even better the solvent system consists of water. Step (b) should preferably also include mixing the zeolite material and one or more binders with one or more pore-forming agents and / or lubricants and / or plasticizers, where one or more of the pore-forming agents and / or lubricants and / or plasticizers are better selected from the group consisting of polymers, carbohydrates, graphite, plant additives, and mixtures of two or more of these, rather than from the group consisting of polymeric vinyl compounds, polyalkylene oxides, polyacrylates, polyolefins, polyamides, polyesters, cellulose and cellulose derivatives, sugars, sesbania cannabina, and mixtures of two or more of these, rather than from the group consisting of poly Polystyrene, C2-C3 polyalkyne oxides, cellulose derivatives, sugars, and mixtures of two or more of these, are better than the group consisting of polystyrene, polyethylene oxide, and cellulose derivatives.Treated with C1-C2 hydroxyalkylates and / or C1-C2 alkylates, sugars, and mixtures of two or more of them, better than the group consisting of polystyrene, polyethylene oxide, hydroxyethyl methyl cellulose, and mixtures of two or more of them, where better one or more of the porosizing agents and / or lubricants and / or plasticizers are composed of one or more selected from the group consisting of polystyrene, polyethylene oxide, hydroxyethyl methyl cellulose, and mixtures of two or more of them, and better one or more of the porosizing agents and / or lubricants and / or plasticizers are composed of a mixture of polystyrene, polyethylene oxide, and hydroxyethyl methyl cellulose. It is preferable to carry out the roasting of the dried blocks obtained in step (e) at a temperature ranging from 350 to 850°C, better than 400 to 700°C, better than 450 to 650°C, and better than 475 to 600°C. The present invention also relates to catalyst molds which include, in accordance with any of the embodiments specified and preferred in accordance with the present invention, catalyst molds which are preferred to be obtained by a preferred manner or obtained by a process in accordance with any of the embodiments specified and preferred in accordance with the present invention. The present invention also relates to a process for activating hydrogen peroxide that includes: (1) To provide a reactor that incorporates, in accordance with any of the embodiments specified and preferred according to the present invention, Or catalyst molds according to any of the specified and preferred embodiments according to the present invention; (2) Contact of the catalyst or catalyst molds supplied in (1) with hydrogen peroxide. The catalyst in (1) should preferably be chosen from among catalysts that include titanium, silicon, and oxygen, and exhibit water adsorption (W), ideally determined according to Reference Example 1.1, and Concentration (c) of µ2η2-peroxy bridging species per titanium in hydrogen peroxide-activated catalyst as determined by 17O quantitative NMR spectroscopy, preferably according to reference example 1.3; The catalyst is selected by calculating the activation factor (A) according to the formula I for each of the catalysts, and selecting a catalyst that exhibits an activation factor in the range of 15 to 80 mM mol / mol, where the activation factor is the product of the water adsorption multiplication and the bridging concentration of the µ2η2-peroxy species per titanium in the hydrogen peroxide-activated catalyst: A=WxC(I). In the case where the provision of the catalyst in (1) involves the selection of the catalyst from among catalysts that include titanium, silicon, and oxygen, where the catalyst is selected by calculating the activation factor (A) according to Formula I for each of the catalysts, the catalyst in (1) is preferred from among the catalysts that exhibit water adsorption in the range of 1 to 10% by weight, better than 1.5 to 9.5% by weight, better than 2 to 9% by weight, better than 2.5 to 8.5% by weight, better than 3 to 8% by weight, better than 3.2 to 7.9% by weight, better than 3.5 to 7.5% by weight, better than 4 to 7% by weight, better than 4.5 to 6.5% by weight, and better than 5 to 6% by weight.Furthermore, and independently of the above, in the case where the provision of the catalyst in (1) involves selecting the catalyst from among catalysts containing titanium, silicon, and oxygen, where the catalyst is selected by calculating the activation factor (A) according to Formula I for each catalyst, the catalyst in (1) is preferably selected from among those catalysts exhibiting a concentration of µ2η2-peroxy-bridging species per titanium in the hydrogen peroxide-activated catalyst in the range of 200 to 1,200 mM / mol, better than 300 to 1,000 mM / mol, better than 350 to 950 mM / mol, better than 400 to 900 mM / mol, better than 450 to 850 mM / mol, better than 500 to 800 mM / mol, better than 550 to 750 mM / mol, and better than 600 to 700 ml mol / mol.Furthermore, and independently of it, in the case where the provision of the catalyst in (a) involves the selection of the catalyst from among catalysts that include titanium, silicon, and oxygen, where the catalyst is selected by calculating the activation factor (a) according to formula I for each of the catalysts, it is preferable that the catalyst be selected by calculating the activation factor (a) for each of the catalysts, and selecting a catalyst that exhibits an activation factor in the range of 16 to 70 mmol / mol, better than 18 to 60 mmol / mol, better than 20 to 55 mmol / mol, better than 23 to 50 mmol / mol, better than 25 to 45 mmol / mol, better than 26 to 44 mmol / mol, better than 27 to 42 mmol / mol, better than 28 to 40 mmol / mol, better than 29 to 37 mmol / mol, and better than 30 to 35 mmol / mol. Furthermore, and independently of it, in the case where the provision of the catalyst in (a) involves the selection of the catalyst from among catalysts containing titanium, silicon, and oxygen, where the catalyst is selected by calculating the activation factor (a) according to the formula I for each of the catalysts, the preferred concentration (c) for bridging the µ2η2-peroxy species per titanium in the hydrogen peroxide-activated catalyst, as determined by quantitative 17O NMR spectroscopy, is the concentration determined at a time point T after the catalyst has been exposed to H217O2, where T is in the range of 1 to 720 min after the catalyst has been exposed to H217O2, better 2 to 480 min, better 4 to 240 min, better 6 to 120 min, better 8 to 60 min, better 10 to 30 min, better 12 to 20 min, and better 14 Up to 16 minutes, where T is better at 15 minutes. Alternatively, in the case where the provision of the catalyst in (1) involves the selection of the catalyst from among catalysts that include titanium, silicon, and oxygen, where the catalyst is selected by calculating the activation factor (A) according to the formula I for each of the catalysts, it is preferable to select the catalyst in (1) from among the catalysts that exhibit a concentration (C) of µ2η2-peroxy-type bridging per titanium in the hydrogen peroxide-activated catalyst as determined by the 17O NMR quantitative spectrometer in the range of 200 to 825 mM mol / mol, where the concentration (C) of µ2η2-peroxy-type bridging per titanium in the hydrogen peroxide-activated catalyst as determined by the 17O NMR quantitative spectrometer is the concentration determined at a time point T after the catalyst comes into contact with H217O2, where T is in the range of 65 to 175 min. In addition to the above and independently of it, in the case where the provision of the catalyst in (1) involves the selection of the catalyst from among catalysts that include titanium, silicon, and oxygen, where the catalyst is selected by calculating the activation factor (A) according to the formula I for each of the catalysts, it is preferable to select the catalyst in (1) from among the catalysts that exhibit water adsorption in the range of 1 to 7.9% by weight, better than 3 to 7.5% by weight, better than 4 to 7% by weight, better than 4.5 to 6.5% by weight, and better than 5 to 6% by weight. Furthermore, and independently of the foregoing, in the case where the provision of the catalyst in (1) involves the selection of the catalyst from among catalysts containing titanium, silicon, and oxygen, where the catalyst is selected by calculating the activation factor (A) according to Formula I for each of the catalysts, the catalyst in (1) is preferably selected from among those catalysts exhibiting a concentration (C) of µ2η2-peroxy-bridging species per titanium in the hydrogen peroxide-activated catalyst, as determined by quantitative 17O NMR spectroscopy, preferably determined according to Reference Example 1.3, in the range of 300 to 822 mM mol / mol, better than 350 to 800 mM mol / mol, better than 400 to 780 mM mol / mol, better than 450 to 760 mM mol / mol, better than 500 to 740 mM mol / mol, and better than 550 to 720 mM mol / mol. Mol / mol, and ideally 600 to 700 ml mol / mol.In addition to the above and independently of it, in the case where the provision of the catalyst in (1) involves the selection of the catalyst from among catalysts that include titanium, silicon, and oxygen, where the catalyst is selected by calculating the activation factor (A) according to the formula I for each of the catalysts, according to the second alternative, it is preferable that T be in the range of 75 to 165 minutes, better than 85 to 155 minutes, better than 95 to 145 minutes, better than 105 to 135 minutes, better than 112 to 128 minutes, better than 116 to 124 minutes, better than 118 to 122 minutes, and better than 119 to 121 minutes, where T is best 120 minutes.In addition to the above and independently of it, in the case where the provision of the catalyst in (1) involves the selection of the catalyst from among catalysts that include titanium, silicon, and oxygen, where the catalyst is selected by calculating the activation factor (A) according to the formula I for each of the catalysts, the activation factor (A) is preferably in the range of 16 to 75 mmol / mol, better than 18 to 67 mmol / mol, better than 20 to 65 mmol / mol, better than 22 to 60 mmol / mol, better than 24 to 55 mmol / mol, better than 26 to 50 mmol / mol, better than 27 to 45 mmol / mol, better than 28 to 40 mmol / mol, better than 29 to 37 mmol / mol, and better than 30 to 34 mmol / mol. The catalyst in (1) is preferably chosen from among catalysts that include 0 to 1% by weight, better than 0 to 0.1% by weight, better than 0 to 0.01% by weight, better than 0 to 0.001% by weight of B, calculated by element and based on the total weight of the catalyst. The catalyst in (1) is preferably chosen from among catalysts that include 0 to 1% by weight, better than 0 to 0.1% by weight, better than 0 to 0.01% by weight, better than 0 to 0.001% by weight of Na, calculated by element and based on the total weight of the catalyst. The catalyst in (1) is preferably chosen from among catalysts that include 0 to 1% by weight, better than 0 to 0.1% by weight, better than 0 to 0.01% by weight, better than 0 to 0.001% by weight of Ge, calculated by element and based on the total weight of the catalyst. The catalyst in (1) is preferably chosen from among catalysts that include 0 to 1% by weight, preferably 0 to 0.5% by weight, better than 0 to 0.2% by weight, better than 0 to 0.1% by weight of C, calculated by element and based on the total weight of the catalyst. The catalyst in (1) is preferably chosen from among catalysts that exhibit propylene oxide activity of at least 2.0% wt%, preferably in the range of 3.0 to 15.0% wt%, preferably in the range of 9.0 to 13.0% wt%, preferably defined as shown in Reference Example 1.6. In (2) it is preferable that hydrogen peroxide be included in the liquid feed stream that is fed into the reactor, where the liquid feed stream also includes one or more unsaturated organic compounds, preferably with one or more olefin compounds, preferably with one or more C2-C5 alkene compounds, preferably with one or more C2-C4 alkene compounds, preferably with one or more C2 or C3 alkene compounds, preferably propylene. In the case where (2) hydrogen peroxide is included in the liquid feed stream fed into the reactor, and the liquid feed stream also includes one or more unsaturated organic compounds, it is preferable that the liquid feed stream also includes a solvent system, where the solvent system includes one or more solvents, where preferably the solvent system includes one or more hydrophilic solvents, preferably hydrophilic solvents selected from the group consisting of polar solvents, preferably from the group consisting of polar protonized solvents, where preferably the solvent system includes one or more polar protonized solvents selected from the group consisting of water, alcohols, and mixtures of two or more of them, preferably from the group consisting of water, C1-C5 alcohols, and mixtures of two or more of them, preferably from the group consisting of water, C1-C4 alcohols, and mixtures of two or more of them, preferably from the group consisting of water, C1-C3 alcohols, and mixtures of two or more of them More than that, and better than the group consisting of water, methanol, ethanol, propanol, and mixtures thereofFor two or more of them, better than the combination of water, methanol, and mixtures thereof, where the solvent system best includes water, preferably water and methanol, where the solvent system best consists of water and methanol. Furthermore, and independently of it, the liquid feed stream should ideally contain hydrogen peroxide at a concentration in the range of 1 to 75% by weight, better than 3 to 50% by weight, 5 to 30% by weight, better than 7 to 25% by weight, better than 8 to 20% by weight, better than 9 to 15% by weight, and better than 10 to 12% by weight, based on the total weight of the liquid feed stream. Furthermore, and independently of it, the feed stream of the liquid being fed into the reactor in (2) should ideally be in a temperature range of 0 to 60 °C, preferably 25 to 50 °C. Furthermore, and independently of it, the feed stream of the liquid being fed into the reactor in (2) should preferably be at a pressure in the range of 5 to 100 bar, better than 10 to 50 bar, and better than 15 to 25 bar. Furthermore, and independently of it, contact is best carried out in (2) at a temperature in the range of 10 to 100 °C, better than 25 to 80 °C, better than 30 to 75 °C, better than 40 to 65 °C. Furthermore, and independently of it, contact in (2) is preferably performed at a pressure in the range of 5 to 100 bar, better than 10 to 50 bar, better than 14 to 32 bar, and better than 15 to 25 bar, where the pressure is determined by the pressure at the reactor outlet. Furthermore, and independently of it, the catalyst loading in reactor (1) is preferably in the range of 0.05 to 5 S-1, better than 0.1 to 4 S-1, better than 0.2 to 3.5 S-1, better than 0.7 to 3 S-1, better than 1 to 2.75 S-1, better than 1.25 to 2.5 S-1, better than 1.5 to 2.25 S-1, and better than 1.75 to 2 S-1, where the catalyst loading is determined by the ratio of the mass flow rate in kg / hr of hydrogen peroxide included in the feed fluid stream divided by the amount in kg of catalyst included in reactor (1). Furthermore and independently of it, the process should preferably also include (3) the removal of a flux from the reactor. The flux should include an oxidized organic compound, preferably an epoxidized organic compound, preferably an alkylene oxide, preferably a selected alkylene oxide from the C2-C5 alkylene oxides, preferably from the C2-C4 alkylene oxides, preferably from the C2 or C3 alkylene oxides, preferably from the C3 alkylene oxides, where the flux should preferably include propylene oxide. The present invention relates to the use of the catalyst, according to any of the embodiments specified and preferred in accordance with the present invention, or the catalyst molds, according to any of the embodiments specified and preferred in accordance with the present invention, as a catalyst and / or catalytic component in a reaction involving the formation and / or conversion of a CC bond, and preferably as a catalyst and / or catalytic component in an isomerization reaction, in an ammonia oxidation reaction, in an amination reaction, in a hydrocracking reaction, in an alkylation reaction, in an acylation reaction, in a reaction for the conversion of alkanes to olefin compounds, or in a reaction for the conversion of one or more olefin oxygenates and / or aromatic compounds, in a hydrogen peroxide synthesis reaction, in an aldol substitution reaction, in an isomer formation reaction of epoxides, in a transesterification reaction, in a hydroxylation reaction, in a Baeyer-Villiger oxidation reaction, in a reaction Of the Dakin type, or in an epoxide addition reaction, preferably as a catalyst and / or catalytic component in a hydroxyl addition reaction, inBaeyer-Villiger type oxidation reaction, in a Dakin type reaction, or in an epoxide addition reaction to olefin compounds, best in an epoxide addition reaction to olefin compounds, best in an epoxide addition reaction to C2-C5 alkene compounds, best in an epoxide addition reaction to C2-C4 alkene compounds, in an epoxide addition reaction to C2 or C3 alkene compounds, best for adding epoxide to C3 alkene compounds, and best as a catalyst or catalytic component for converting propylene to propylene oxide. The present invention is further clarified by the following set of incarnations and sets of incarnations resulting from dependencies and references, as specified. In particular, it should be noted that in every instance where the range of incarnations is mentioned, for example, in the context of a term such as "catalyst according to any one of incarnations 1 to 4," each incarnation within that range is assumed to be expressly disclosed to the skilled person; that is, the formulation of this term should be understood by the skilled person as synonymous with "catalyst for any of incarnations 1, 2, 3, and 4." Furthermore, it is clearly stated that the following set of incarnations is not the set of elements of protection that defines the scope of protection, but rather represents a suitably structured part of the description directed at the general and preferred aspects of the present invention. Moreover, it has been found that a process for preparing such an improved catalyst can be provided. In addition, it has been found that a process for activating hydrogen peroxide can be provided, whereby any specified catalyst is used. Incarnations 1. The catalyst includes titanium, silicon, and oxygen, where the catalyst exhibits water adsorption (W), preferably determined according to reference example 1.1, the concentration (C) of µ2η2-peroxy bridging species per titanium in the hydrogen peroxide-activated catalyst as determined by 17O NMR quantitative spectroscopy, preferably determined according to reference example 1.3, and an activation factor (A) according to formula I, where the activation factor is in the range of 15 to 80 mM mol / mol; According to formula I, the activation factor is the product of the water adsorption multiplication and the bridging concentration of µ2η2-peroxy species per titanium in the hydrogen peroxide-activated catalyst: A=WxC(I). 2. The catalyst according to embodiment 1, where the catalyst exhibits water adsorption in the range of 1 to 10% by weight, preferably 1.5 to 9.5% by weight, better than 2 to 9% by weight, better than 2.5 to 8.5% by weight, better than 3 to 8% by weight, better than 3.2 to 7.9% by weight, better than 3.5 to 7.5% by weight, better than 4 to 7% by weight, better than 4.5 to 6.5% by weight, and better than 5 to 6% by weight. 3. The catalyst according to embodiment 1 or 2, where the catalyst exhibits a concentration for bridging µ2η2-peroxy species per titanium in the hydrogen peroxide-activated catalyst in the range of 200 to 1,200 mL mol / mol, preferably 300 to 1,000 mL mol / mol, better than 350 to 950 mL mol / mol, better than 400 to 900 mL mol / mol, better than 450 to 850 mL mol / mol, better than 500 to 800 mL mol / mol, better than 550 to 750 mL mol / mol, and better than 600 to 700 mL mol / mol. 4. The catalyst according to any of the embodiments 1 to 3, where the concentration (c) of the µ2η2-peroxy bridging species per titanium in the hydrogen peroxide-activated catalyst as determined by the 17O NMR quantitative spectrometer is the concentration determined at a time point T after the catalyst comes into contact with H217O2, where T is in the range of 1 to 720 mins after the catalyst comes into contact with H217O2, preferably 2 mins to 480 mins, better 4 to 240 mins, better 6 to 120 mins, better 8 to 60 mins, better 10 to 30 mins, better 12 to 20 mins, and better 14 to 16 mins, where T is best 15 mins. 5. The catalyst according to any of the embodiments 1 to 4, where the activation factor is in the range of 16 to 70 mM mol / mol, preferably 18 to 60 mM mol / mol, better than 20 to 55 mM mol / mol, better than 23 to 50 mM mol / mol, better than 25 to 45 mM mol / mol, better than 26 to 44 mM mol / mol, better than 27 to 42 mM mol / mol, better than 28 to 40 mM mol / mol, better than 29 to 37 mM mol / mol, and better than 30 to 35 mM mol / mol. 6. The catalyst according to embodiment 1, where the catalyst exhibits a concentration of µ2η2-peroxy-peroxy-types bridging per titanium in the hydrogen peroxide-activated catalyst in the range of 200 to 825 mM mol / mol, where the concentration of µ2η2-peroxy-peroxy-types bridging per titanium in the hydrogen peroxide-activated catalyst as determined by the 17O NMR quantitative spectrometer is the concentration determined at a time point T after the catalyst comes into contact with H217O2, where T is in the range of 65 to 175 min. 7. The catalyst according to embodiment 6, where the catalyst exhibits water adsorption in the range of 1 to 7.9% by weight, preferably 3 to 7.5% by weight, better 4 to 7% by weight, better 4.5 to 6.5% by weight, and better 5 to 6% by weight. 8. The catalyst according to embodiment 6 or 7, where the catalyst exhibits a concentration of µ2η2-peroxy bridging species per titanium in the hydrogen peroxide-activated catalyst as determined by 17O NMR quantitative spectroscopy, preferredly determined according to reference example 1.3, in the range of 300 to 822 mmol / mol, preferably 350 to 800 mmol / mol, preferably 400 to 780 mmol / mol, preferably 450 to 760 mmol / mol, preferably 500 to 740 mmol / mol, preferably 550 to 720 mmol / mol, and preferably 600 to 700 mmol / mol. 9. a For a catalyst according to any of the incarnations 6 to 8, where T is in the range of 75 to 165 minutes, preferably 85 to 155 minutes, better 95 to 145 minutes, better 105 to 135 minutes, better 112 to 128 minutes, better 116 to 124 minutes, better 118 to 122 minutes, and better 119 to 121 minutes, where T is best 120 minutes. 10. The catalyst according to any of the embodiments 6 to 9, where the activation factor is in the range of 16 to 75 mmol / mol, preferably 18 to 67 mmol / mol, better than 20 to 65 mmol / mol, better than 22 to 60 mmol / mol, better than 24 to 55 mmol / mol, better than 26 to 50 mmol / mol, better than 27 to 45 mmol / mol, better than 28 to 40 mmol / mol, better than 29 to 37 mmol / mol, and better than 30 to 34 mmol / mol. 11. The catalyst, according to any of the embodiments 1 to 10, exhibits an X-ray absorption spectrum near the edge structure that has a signal intensity ratio at 4987 eV to a signal intensity at 4992 eV in the range of 0.95:1 to 1.07:1, preferably from 0.97:1 to 1.07:1, better in the range of 0.99:1 to 1.07:1, better in the range of 1.01:1 to 1.07:1, better in the range of 1.03:1 to 1.07:1, and best in the range of 1.05:1 to 1.07:1, where X-ray absorption spectra near the edge structure are preferred to be determined according to the reference example 1.2. 12. The catalyst, according to any of the embodiments 1 to 11, with a Brunauer, Emmett, and Teller specific surface area in the range of 350 to 475 m² / g, preferably 370 to 455 m² / g, and even better 390 to 435 m² / g, where the Brunauer, Emmett, and Teller specific surface area was determined preferentially according to Reference Example 1.5. 13. The catalyst, according to any of the embodiments 1 to 12, includes 0.5 to 2.5% by weight, preferably 0.8 to 2.0% by weight, better than 1.0 to 1.9% by weight, better than 1.0 to 1.8% by weight, better than 1.1 to 1.3% by weight of titanium, calculated by element and based on the total weight of the catalyst. 14. The catalyst, according to any of the incarnations 1 to 13, includes 0 to 1% by weight, preferably 0 to 0.1% by weight, better than 0 to 0.01% by weight, better than 0 to 0.001% by weight of B, calculated by element and based on the total weight of the catalyst. 15. The catalyst, according to any of the incarnations 1 to 14, includes 0 to 1% by weight, preferably 0 to 0.1% by weight, better than 0 to 0.01% by weight, better than 0 to 0.001% by weight of Na, calculated by element and based on the total weight of the catalyst. 16 The catalyst, according to any of the incarnations 1 to 15, includes 0 to 1% by weight, preferably 0 to 0.1% by weight, better than 0 to 0.01% by weight, better than 0 to 0.001% by weight of Ge, calculated by element and based on the total weight of the catalyst. 17. The catalyst, according to any of the embodiments 1 to 16, includes 0 to 1% by weight, preferably 0 to 0.5% by weight, better than 0 to 0.2% by weight, better than 0 to 0.1% by weight of C, calculated by element and based on the total weight of the catalyst. 18. The catalyst, according to any of the embodiments 1 to 17, exhibits propylene oxide activity of at least 2.0% wt%, preferably in the range of 3.0 to 15.0% wt%, best in the range of 9.0 to 13.0% wt%, preferably defined as shown in Reference Example 1.6. 19. The catalyst according to any of the incarnations 1 to 18, where the catalyst also includes one or more selected metals from the group consisting of zinc, cadmium, tin, lanthanum, and barium, which includes mixtures of two or more of them. 20. The catalyst according to any of the embodiments 1 to 19, where 95 to 100% by weight of the catalyst is composed of titanium, silicon, and oxygen, preferably 97 to 100% by weight, better than 98 to 100% by weight, better than 99 to 100% by weight, better than 99.5 to 100% by weight, and better than 99.9 to 100% by weight. 21. The catalyst according to any of the embodiments 1 to 20, where 95 to 100% by weight of the catalyst is composed of titanium, silicon, oxygen, and hydrogen, preferably 97 to 100% by weight, better than 98 to 100% by weight, better than 99 to 100% by weight, better than 99.5 to 100% by weight, and better than 99.9 to 100% by weight. 22. The catalyst according to any of the embodiments 1 to 21, where the catalyst includes, preferably consists of, a zeolite material with a framework structure that includes silicon, titanium, and oxygen. 23. The catalyst according to the embodiment 22, the zeolite material has a silicon:titanium molar ratio in the range of 1 to 250, preferably in the range of 10 to 150, better in the range of 20 to 95, better in the range of 30 to 75, better in the range of 35 to 70, better in the range of 40 to 65, better in the range of 45 to 60, better in the range of 50 to 55. 24. The catalyst according to embodiment 22 or 23, where the zeolite material includes a selected frame structure type from the group consisting of MFI, MEL, MWW, ITH, IWR, IMF, SVY, FER, SVR, and intergrowth structures of two or more of them, preferably selected from the group consisting of MFI, MEL, MWW, ITH, and IWR, and intergrowth structures of two or more of them, better selected from the group consisting of MFI, MEL, and intergrowth structures of it, where the zeolite material best includes a frame structure of type MFI. 25. The catalyst according to any of the embodiments 22 to 24, where the zeolite material is titanium silicate zeolite-1. 26. The catalyst according to any of the embodiments 22 to 25, where the zeolite material also includes one or more selected metals from the group consisting of zinc, cadmium, tin, lanthanum, and barium, which includes mixtures of two or more of them, where one or more metals are preferentially included in the pores of the zeolite material. 27. The catalyst according to any of the embodiments 22 to 26, where 95 to 100% by weight of the zeolite material is composed of titanium, silicon, and oxygen, preferably 97 to 100% by weight, better than 98 to 100% by weight, better than 99 to 100% by weight, better than 99.5 to 100% by weight, and better than 99.9 to 100% by weight. 28. The catalyst according to any of the embodiments 22 to 27, where 95 to 100% by weight of the zeolite material is composed of titanium, silicon, oxygen, and hydrogen, preferably 97 to 100% by weight, better than 98 to 100% by weight, better than 99 to 100% by weight, better than 99.5 to 100% by weight, and better than 99.9 to 100% by weight. 29. The catalyst according to any of the embodiments 22 to 28, where the zeolite material includes crystallization in the range of 50 to 100% by weight, preferably 75 to 100% by weight, better than 80 to 100% by weight, and best than 90 to 100% by weight, where crystallization has been determined preferentially as described in Reference Example 1.4. 30. A method for preparing catalyst molds, including (a) Provided according to any of the incarnations 1 to 29; (b) Mix the catalyst provided in step (a) with one or more binding materials; (c) Optionally knead the mixture obtained in step (b); (d) Molding the mixture obtained in step (b) or (c) to obtain one or more molds; (e) Optionally, dry one or more of the molds obtained in step (d); and (f) Toasting the molds obtained in step (d) or (e). 31. The method according to embodiment 30, where the provision of the catalyst in (a) involves selecting the catalyst from among catalysts that include titanium, silicon, and O, and exhibit water adsorption (W), preferentially determined according to reference example 1.1, and Concentration (c) of µ2η2-peroxy bridging species per titanium in hydrogen peroxide-activated catalyst as determined by 17O quantitative NMR spectroscopy, preferably according to reference example 1.3; The catalyst is selected by calculating the activation factor (A) according to the formula I for each of the catalysts, and selecting a catalyst that exhibits an activation factor in the range of 15 to 80 mM mol / mol, where the activation factor is the product of the water adsorption multiplication and the bridging concentration of the µ2η2-peroxy species per titanium in the hydrogen peroxide-activated catalyst: A=WxC(I). 32. The method according to the embodiment 30 or 31, where the provision of the catalyst in (a) involves the selection of the catalyst from among the catalysts that exhibit water adsorption in the range of 1 to 10% by weight, preferably 1.5 to 9.5% by weight, better than 2 to 9% by weight, better than 2.5 to 8.5% by weight, better than 3 to 8% by weight, better than 3.2 to 7.9% by weight, better than 3.5 to 7.5% by weight, better than 4 to 7% by weight, better than 4.5 to 6.5% by weight, and better than 5 to 6% by weight. 33. The method according to any of the embodiments 30 to 32, where the provision of the catalyst in (a) involves the selection of the catalyst from among the catalysts that exhibit a concentration for bridging µ2η2-peroxy-types per titanium in the hydrogen peroxide-activated catalyst in the range of 200 to 1,200 mL mol / mol, preferably 300 to 1,000 mL mol / mol, better than 350 to 950 mL mol / mol, better than 400 to 900 mL mol / mol, better than 450 to 850 mL mol / mol, better than 500 to 800 mL mol / mol, better than 550 to 750 mL mol / mol, and better than 600 to 700 mL mol / mol. 34. The method according to any of the embodiments 30 to 33, where the catalyst is selected by calculating the activation factor (A) for each of the catalysts, and selecting a catalyst that exhibits an activation factor in the range of 16 to 70, preferably 18 to 60 mmol / mol, better than 20 to 55 mmol / mol, better than 23 to 50 mmol / mol, better than 25 to 45 mmol / mol, better than 26 to 44 mmol / mol, better than 27 to 42 mmol / mol, better than 28 to 40 mmol / mol, better than 29 to 37 mmol / mol, and better than 30 to 35 mmol / mol. 35. The method according to any of the embodiments 30 to 34, where the concentration (c) of the µ2η2-peroxy bridging species per titanium in the hydrogen peroxide-activated catalyst as determined by the 17O NMR quantitative spectrometer is the concentration determined at a time point T after the catalyst comes into contact with H217O2, where T is in the range of 1 to 720 mins after the catalyst comes into contact with H217O2, preferably 2 mins to 480 mins, better 4 to 240 mins, better 6 to 120 mins, better 8 to 60 mins, better 10 to 30 mins, better 12 to 20 mins, and better 14 to 16 mins, where T is best 15 mins. 36. The method according to the embodiment 31, where the provision of the catalyst in (a) involves selecting the catalyst from among the catalysts that exhibit a concentration (c) of µ2η2-peroxy-type bridging per titanium in the hydrogen peroxide-activated catalyst as determined by the 17O NMR quantitative spectrometer in the range of 200 to 825 mM mol / mol, where the concentration (c) of µ2η2-peroxy-type bridging per titanium in the hydrogen peroxide-activated catalyst as determined by the 17O NMR quantitative spectrometer is the concentration determined at a time point T after the catalyst comes into contact with H217O2, where T is in the range of 65 to 175 min. 37. The method according to the embodiment 36, where the provision of the catalyst in (a) involves selecting the catalyst from among the catalysts that exhibit water adsorption in the range of 1 to 7.9% by weight, preferably 3 to 7.5% by weight, better than 4 to 7% by weight, better than 4.5 to 6.5% by weight, and better than 5 to 6% by weight. 38. The method according to the embodiments s 36 or 37, where the provision of the catalyst in (a) involves the selection of the catalyst from among the catalysts that exhibit a concentration of (c) for bridging the µ2η2-peroxy species of each titanium in the hydrogen peroxide-activated catalyst as determined by the 17O quantitative NMR spectrometer, preferredly determined according to the reference example 1.3, in the range of 300 to 822 mmol / mol, preferably 350 to 800 mmol / mol, preferably 400 to 780 mmol / mol, preferably 450 to 760 mmol / mol, preferably 500 to 740 mmol / mol, preferably 550 to 720 mmol / mol, and preferably 600 to 700 mmol / mol. 39. The method according to any of the incarnations 36 to 38, where T is in the range of 75 to 165 minutes, preferably 85 to 155 minutes, better 95 to 145 minutes, better 105 to 135 minutes, better 112 to 128 minutes, better 116 to 124 minutes, better 118 to 122 minutes, and better 119 to 121 minutes, where T is best 120 minutes. 40. The method according to any of the incarnations 36 to 39, where the activation factor (A) is in the range of 16 to 75 mM mol / mol, preferably 18 to 67 mM mol / mol, better than 20 to 65 mM mol / mol, better than 22 to 60 mM mol / mol, better than 24 to 55 mM mol / mol, better than 26 to 50 mM mol / mol, better than 27 to 45 mM mol / mol, better than 28 to 40 mM mol / mol, better than 29 to 37 mM mol / mol, and better than 30 to 34 mM mol / mol. 41. The method according to any of the embodiments 30 to 40, where the provision of the catalyst in (A) involves the selection of the catalyst from among catalysts that include 0 to 1% by weight, preferably 0 to 0.1% by weight, better than 0 to 0.01% by weight, better than 0 to 0.001% by weight of B, calculated by element and based on the total weight of the catalyst. 42. The method according to any of the embodiments 30 to 41, where the provision of the catalyst in (a) involves the selection of the catalyst from among catalysts that include 0 to 1% by weight, preferably 0 to 0.1% by weight, better than 0 to 0.01% by weight, better than 0 to 0.001% by weight of Na, calculated by element and based on the total weight of the catalyst. 43. The method according to any of the embodiments 30 to 42, where the provision of the catalyst in (a) involves the selection of the catalyst from among catalysts that include 0 to 1% by weight, preferably 0 to 0.1% by weight, better than 0 to 0.01% by weight, better than 0 to 0.001% by weight of Ge, calculated by element and based on the total weight of the catalyst. 44. The method according to any of the embodiments 30 to 43, where the provision of the catalyst in (a) involves the selection of the catalyst from among catalysts that include 0 to 1% by weight, preferably 0 to 0.5% by weight, better than 0 to 0.2% by weight, better than 0 to 0.1% by weight of C, calculated by element and based on the total weight of the catalyst. 45. The method according to any of the embodiments 30 to 44, where the provision of the catalyst in (a) involves the selection of the catalyst from among catalysts that exhibit propylene oxide activity of at least 2.0 wt%, preferably in the range of 3.0 to 15.0 wt%, best in the range of 9.0 to 13.0 wt%, determined preferentially as described in Reference Example 1.6. 46. The method according to any of the embodiments 30 to 45, where one or more of the binders in (b) are chosen from the group consisting of inorganic binders, where one or more of the binders preferentially include one or more sources of metal oxide and / or metal oxide, preferably one or more sources of metal oxide and / or metal oxide chosen from the group consisting of silica, alumina, titania, zirconia, lanthanum, magnesia, mixtures thereof and / or mixtures of two or more of them, preferably from the group consisting of silica, alumina, titania, zirconia, magnesia, mixtures of silica-alumina, mixtures of silica-titania, mixtures of silica-zirconia, mixtures of silica-lanthanum, mixtures of silica-zirconia-lanthanum. Mixed oxides of alumina-titanium, mixed oxides of alumina-zirconia, mixed oxides of alumina-lanthanum, mixed oxides of alumina-zirconia-lanthanum, mixed oxides of titania-zirconia, and mixtures thereof and / or mixtures of two or more of them, better than the group consisting of silica, alumina, mixed oxides ofSilica-alumina, and mixtures thereof of two or more, where preferably one or more of the binding materials in (b) include one or more sources of silica, where preferably one or more of the binding materials in (b) are composed of one or more sources of silica, where preferably one or more of the silica sources include one or more of the selected compounds from the group consisting of fumed silica, colloidal silica, silica-alumina, colloidal silica-alumina, and mixtures thereof of two or more, preferably one or more of the selected compounds from the group consisting of fumed silica, colloidal silica, and mixtures thereof, where preferably one or more of the binding materials in (b) are composed of colloidal silica. 47. The method according to any of the embodiments 30 to 46, where step (b) also involves mixing the zeolite material and one or more binders with a solvent system, where the solvent system includes one or more solvents, preferably hydrophilic solvents, preferably selected from the group consisting of polar solvents, rather than the group consisting of polar protonized solvents, where the solvent system preferably includes one or more polar protonized solvents selected from the group consisting of water, alcohols, carboxylic acids, and mixtures of two or more of them, rather than the group consisting of water, C1-C5 alcohols, C1-C5 carboxylic acids, and mixtures of two or more of them, rather than the group consisting of water, C1-C4 alcohols, C1-C4 carboxylic acids, and mixtures of two or more of them, rather than the group consisting of Water, C1-C3 alcohols, C1-C3 carboxylic acids, and mixtures of two or more of them, are better suited than the combination of water, methanol, ethanol, propanol, formic acid, and carboxylic acid.Acetic acid, and mixtures of two or more of them, are better than the combination of water, ethanol, acetic acid, and mixtures of two or more of them, where the solvent system better includes water and / or ethanol, where the solvent system better includes water, where even better the solvent system consists of water. 48. The method according to any of the embodiments 30 to 47, where step (b) also involves mixing the zeolite material and one or more binders with one or more porosizing agents and / or lubricants and / or plasticizers, where one or more porosizing agents and / or lubricants and / or plasticizers are preferably chosen from the group consisting of polymers, carbohydrates, graphite, vegetable additives, and mixtures thereof of two or more, better than the group consisting of vinyl polymers, polyalkylene oxides, polyacrylates, polyolefin compounds, polyamides, polyester compounds, cellulose and cellulose derivatives, sugars, sesbania canabina, and mixtures thereof of two or more, better than the group consisting of polystyrene, C2-C3 polyalkylene oxides, cellulose derivatives, sugars, and mixtures thereof of two or more, better than the group consisting of polystyrene, poly Ethylene oxide, C1-C2 hydroxyalkylated and / or C1-C2 alkylated cellulose derivatives, sugars, and mixtures thereof of two or more, are better than the group consisting of polystyrene, polyethylene oxide, and hydroxyethylMethyl cellulose, and mixtures thereof of two or more of them, whereby one or more of the porosizing agents and / or lubricants and / or plasticizers are best formed from one or more selected from the group consisting of polystyrene, polyethylene oxide, hydroxyethyl methyl cellulose, and mixtures thereof of two or more of them, best formed from one or more of the porosizing agents and / or lubricants and / or plasticizers are best formed from a mixture of polystyrene, polyethylene oxide, and hydroxyethyl methyl cellulose. 49. The method according to any of the embodiments 30 to 49, whereby the roasting of the dried blocks obtained in step (e) is carried out at a temperature ranging from 350 to 850°C, preferably from 400 to 700°C, better from 450 to 650°C, and best from 475 to 600°C. 50. Catalyst molds that include, according to any of the incarnations 1 to 29, where the catalyst molds are preferred to be obtained or obtained by a process according to any of the incarnations 30 to 49. 51. A process for activating hydrogen peroxide involves: (1) Provision of a reactor that includes, according to any of the incarnations 1 to 29, catalyst templates according to incarnation 48; (2) Contact of the catalyst or catalyst templates provided in (1) with hydrogen peroxide. 52. The process, according to embodiment 51, involves providing the catalyst in (1) selecting the catalyst from among those containing titanium, silicon, and O, and exhibiting water adsorption (W), preferentially determined according to Reference Example 1.1, and Concentration (c) of µ2η2-peroxy bridging species per titanium in hydrogen peroxide-activated catalyst as determined by 17O quantitative NMR spectroscopy, preferably according to reference example 1.3; The catalyst is selected by calculating the activation factor (A) according to the formula I for each of the catalysts, and selecting a catalyst that exhibits an activation factor in the range of 15 to 80 mM mol / mol, where the activation factor is the product of the water adsorption multiplication and the bridging concentration of the µ2η2-peroxy species per titanium in the hydrogen peroxide-activated catalyst: A=WxC(I). 53. The process according to the embodiment 52, where the provision of the catalyst involves (1) selecting the catalyst from among the catalysts that exhibit water adsorption in the range of 1 to 10% by weight, preferably 1.5 to 9.5% by weight, better than 2 to 9% by weight, better than 2.5 to 8.5% by weight, better than 3 to 8% by weight, better than 3.2 to 7.9% by weight, better than 3.5 to 7.5% by weight, better than 4 to 7% by weight, better than 4.5 to 6.5% by weight, and better than 5 to 6% by weight. 54. The process according to the embodiment 52 or 53, where the provision of the catalyst in (1) involves the selection of the catalyst from among the catalysts that exhibit a concentration for bridging µ2η2-peroxy-types per titanium in the hydrogen peroxide-activated catalyst in the range of 200 to 1,200 mL mol / mol, preferably 300 to 1,000 mL mol / mol, better than 350 to 950 mL mol / mol, better than 400 to 900 mL mol / mol, better than 450 to 850 mL mol / mol, better than 500 to 800 mL mol / mol, better than 550 to 750 mL mol / mol, and better than 600 to 700 mL mol / mol. 55. The process is according to any of the embodiments 52 to 54, where the catalyst is selected by calculating the activation factor (A) for each of the catalysts, and selecting a catalyst that exhibits an activation factor in the range of 16 to 70 mmol / mol, better than 18 to 60 mmol / mol, better than 20 to 55 mmol / mol, better than 23 to 50 mmol / mol, better than 25 to 45 mmol / mol, better than 26 to 44 mmol / mol, better than 27 to 42 mmol / mol, better than 28 to 40 mmol / mol, better than 29 to 37 mmol / mol, and better than 30 to 35 mmol / mol. 56. The process is according to either of the embodiments 52 to 55, where the concentration (C) of the µ2η2-peroxy-bridging species per titanium in the hydrogen peroxide-activated catalyst, as determined by quantitative 17O NMR spectroscopy, is the concentration determined at time point T after the catalyst comes into contact with H₂O₂, where T is in the range of 1 to 720 minutes after the catalyst comes into contact with H₂O₂. 217O2, preferably from 2 minutes to 480 minutes, better from 4 to 240 minutes, better from 6 to 120 minutes, better from 8 to 60 minutes, better from 10 to 30 minutes, better from 12 to 20 minutes, and better from 14 to 16 minutes, where T is best 15 minutes. 57. The process according to the embodiment 52, where the provision of the catalyst in (1) involves selecting the catalyst from among the catalysts that exhibit a concentration (C) for bridging µ2η2-peroxy-types per titanium in the hydrogen peroxide-activated catalyst as determined by the 17O NMR quantitative spectrometer in the range of 200 to 825 mM mol / mol, where the concentration (C) for bridging µ2η2-peroxy-types per titanium in the hydrogen peroxide-activated catalyst as determined by the 17O NMR quantitative spectrometer is the concentration determined at a time point T after the catalyst comes into contact with H217O2, where T is in the range of 65 to 175 min. 58. The process according to the embodiment 57, where the provision of the catalyst involves (1) selecting the catalyst from among the catalysts that exhibit water adsorption in the range of 1 to 7.9% by weight, preferably 3 to 7.5% by weight, better than 4 to 7% by weight, better than 4.5 to 6.5% by weight, and better than 5 to 6% by weight. 59. The process according to the embodiment 57 or 58, where the provision of the catalyst in (1) involves the selection of the catalyst from among the catalysts that exhibit a concentration (c) for bridging the µ2η2-peroxy species of each titanium in the hydrogen peroxide-activated catalyst as determined by the 17O NMR quantitative spectrometer, preferredly determined according to the reference example 1.3, in the range of 300 to 822 mmol / mol, preferably 350 to 800 mmol / mol, preferably 400 to 780 mmol / mol, preferably 450 to 760 mmol / mol, preferably 500 to 740 mmol / mol, preferably 550 to 720 mmol / mol, and preferably 600 to 700 mmol / mol. 60. The process according to any of the incarnations 57 to 59, where T is in the range of 75 to 165 minutes, preferably 85 to 155 minutes, better 95 to 145 minutes, better 105 to 135 minutes, better 112 to 128 minutes, better 116 to 124 minutes, better 118 to 122 minutes, and better 119 to 121 minutes, where T is best 120 minutes. 61. The process according to any of the incarnations 57 to 60, where the activation factor (A) is in the range of 16 to 75 mM mol / mol, preferably 18 to 67 mM mol / mol, better than 20 to 65 mM mol / mol, better than 22 to 60 mM mol / mol, better than 24 to 55 mM mol / mol, better than 26 to 50 mM mol / mol, better than 27 to 45 mM mol / mol, better than 28 to 40 mM mol / mol, better than 29 to 37 mM mol / mol, and better than 30 to 34 mM mol / mol. 62. The process according to any of the embodiments 51 to 61, where the provision of the catalyst in (1) involves the selection of the catalyst among catalysts that include 0 to 1% by weight, preferably 0 to 0.1% by weight, better than 0 to 0.01% by weight, better than 0 to 0.001% by weight of B, calculated by element and based on the total weight of the catalyst. 63. The process according to any of the embodiments 51 to 62, where the provision of the catalyst involves (1) choosing the catalyst from among catalysts that include 0 to 1% by weight, preferably 0 to 0.1% by weight, better than 0 to 0.01% by weight, better than 0 to 0.001% by weight of Na, calculated by element and based on the total weight of the catalyst. 64. The process according to any of the embodiments 51 to 63, where the provision of the catalyst involves (1) choosing the catalyst from among catalysts that include 0 to 1% by weight, preferably 0 to 0.1% by weight, better than 0 to 0.01% by weight, better than 0 to 0.001% by weight of Ge, calculated by element and based on the total weight of the catalyst. 65. The process according to any of the embodiments 51 to 64, where the provision of the catalyst in (1) involves the selection of the catalyst from among catalysts that include 0 to 1% by weight, preferably 0 to 0.5% by weight, better than 0 to 0.2% by weight, better than 0 to 0.1% by weight of C, calculated by element and based on the total weight of the catalyst. 66. The process according to any of the embodiments 51 to 65, where the provision of the catalyst in (1) involves the selection of the catalyst from among catalysts that exhibit propylene oxide activity of at least 2.0% wt%, preferably in the range of 3.0 to 15.0% wt%, best in the range of 9.0 to 13.0% wt%, determined preferentially as described in Reference Example 1.6. 67. The process according to any of the embodiments 51 to 66, where in (2) hydrogen peroxide is included in the liquid feed stream which is fed into the reactor, where the liquid feed stream also includes one or more unsaturated organic compounds, preferably one or more olefin compounds, preferably one or more C2-C5 alkene compounds, preferably one or more C2-C4 alkene compounds, preferably one or more C2 or C3 alkene compounds, preferably propylene. 68. The process according to embodiment 67, where the liquid feed stream also includes a solvent system, where the solvent system includes one or more solvents, where preferably the solvent system includes one or more hydrophilic solvents, preferably selected from the group consisting of polar solvents, better than the group consisting of polar protonized solvents, where preferably the solvent system includes one or more polar protonized solvents selected from the group consisting of water, alcohols, and mixtures thereof of two or more, better than the group consisting of water, C1-C5 alcohols, and mixtures thereof of two or more, better than the group consisting of water, C1-C4 alcohols, and mixtures thereof of two or more, better than the group consisting of water, C1-C3 alcohols, and mixtures thereof of two or more, better than the group consisting of water, methanol, ethanol, propanol, and mixtures thereof of two or more. Better than a combination of water, methanol, and mixtures thereof, where the solvent system best includes water, preferably water and methanol, whereIdeally, the solvent system consists of water and methanol. 69. The process according to embodiment 67 or 68, whereby the liquid feed stream contains hydrogen peroxide at a concentration in the range of 1 to 75% by weight, preferably 3 to 50% by weight, 5 to 30% by weight, preferably 7 to 25% by weight, preferably 8 to 20% by weight, preferably 9 to 15% by weight, preferably 10 to 12% by weight, based on the total weight of the liquid feed stream. 70. The process according to any of the embodiments 67 to 69, whereby the feed stream of the liquid being fed into the reactor is involved at (2) a temperature in the range of 0 to 60 °C, preferably 25 to 50 °C. 71. The process according to any of the embodiments 67 to 70, where the feed stream of liquid being fed into the reactor in (2) is at a pressure in the range of 5 to 100 bar, preferably 10 to 50 bar, better still 15 to 25 bar. 72. The process according to any of the embodiments 67 to 71, where contact is carried out in (2) at a temperature in the range of 10 to 100 °C, preferably 25 to 80 °C, better 30 to 75 °C, better 40 to 65 °C. 73. The process is carried out according to any of the embodiments 67 to 72, where contact is carried out in (2) with a pressure in the range of 5 to 100 bar, preferably 10 to 50 bar, better 14 to 32 bar, better 15 to 25 bar, where the pressure is determined by the pressure at the reactor outlet. 74. The process is according to any of the embodiments 67 to 73, where the catalyst loading in reactor in (1) is in the range of 0.05 to 5 S-1, preferably 0.1 to 4 S-1, better than 0.2 to 3.5 S-1, better than 0.7 to 3 S-1, better than 1 to 2.75 S-1, better than 1.25 to 2.5 S-1, better than 1.5 to 2.25 S-1, better than 1.75 to 2 S-1, where the catalyst loading is determined by the ratio of the mass flow rate in kg / hr of hydrogen peroxide included in the feed fluid stream divided by the amount in kg of catalyst included in reactor in (1). 75. The process according to any of the embodiments 67 to 74, where the process also includes (3) the removal of a flowing stream from the reactor, the flowing stream containing an oxidized organic compound, preferably an epoxidized organic compound, preferably an alkylene oxide, preferably an alkylene oxide selected from C2-C5 alkylene oxides, preferably from C2-C4 alkylene oxides, preferably from C2 or C3 alkylene oxides, preferably from C3 alkylene oxides, where preferably the flowing stream contains propylene oxide. 76. The catalyst may be used according to any of the embodiments 1 to 29, or the catalyst templates according to protection element 48, as a catalyst and / or catalytic component in a reaction involving the formation and / or conversion of a CC bond, preferably as a catalyst and / or catalytic component in an isomer formation reaction, in an ammonia oxidation reaction, in an amine addition reaction, in a hydrocracking reaction, in an alkylation reaction, in an acyl addition reaction, in a reaction to convert alkanes to olefins, or in a reaction to convert one or more olefin oxygenates and / or aromatic compounds, in a hydrogen peroxide synthesis reaction, in an aldol substitution reaction, in an isomer formation reaction of epoxides, in a transition esterification reaction, in a hydroxyl addition reaction, in a Baeyer-Villiger oxidation reaction, in a Dakin reaction, or in an epoxide addition reaction, preferably as a catalyst and / or catalytic component in a hydroxyl addition reaction, in a Baeyer-Villiger oxidation reaction, in a reaction Of the Dakin type, or in a reaction to add epoxide to olefin compounds, better in a reaction to add epoxide to olefin compounds, better in a reaction to add epoxide to C2-C5alkene compounds, better in a reaction to add epoxide to compoundsC2-C4alkenes, in a reaction to add epoxides to C2 or C3alkenes, better for adding epoxides to C3alkenes, and better as a catalyst or catalytic component for converting propylene to propylene oxide. The present invention is also illustrated by example, comparative examples and reference examples. Test section Reference Example 1: Methods of Selection Reference Example 1.1: Determining Water Adsorption The water adsorption characteristics of the experimental section samples were determined using a VTI SA instrument from TA Instruments based on isothermal steps. The experiment consisted of one or more operating cycles performed on the sample material placed on the microbalance vessel inside the instrument. Before the measurement began, residual moisture was removed from the sample by heating it to 120°C (with a temperature increase of 5°C / min) and holding it for 6 hours under an N2 flow. After the drying program, the temperature in the cell was reduced to 25°C, and an isothermal temperature was maintained during the measurements. The microbalance was calibrated, and the weight of the dried sample was balanced (maximum mass deviation 0.01 wt%). The water adsorption of the sample was measured as the weight increase compared to the dried sample. First, the adsorption curve was measured by increasing the relative humidity (RH) to which the samples were exposed, and then the water adsorption of the sample was measured at equilibrium.The relative humidity was increased in 10% increments from 5% to 85%. At each increment, the system controlled the relative humidity and monitored the sample weight until equilibrium conditions were reached, and the weight-based adsorption was recorded. The total amount of water absorbed by the sample after exposure to 85% relative humidity was calculated. During the adsorption measurement, the relative humidity was decreased from 85% to 5% in 10% increments, and the change in sample weight (water adsorption) was monitored and recorded. Reference Example 1.2: Determining the Spectra of KedgeXANES Titanium Ti K-edge XANES (X-ray absorption near the edge structure) spectra were recorded at the European Synchrotron Radiation Facility (Grenoble, France). The X-ray beam was dyed with liquid nitrogen-cooled silicon monochromator (111). Energy calibration was performed using titanium reference foils (Ti K-edge position at 4966 eV). K-edge XAS measurements were performed using a flux detection scheme with a silicon diode drift valve and corresponding digital electronics. All samples were measured as compressed pellets. Ti K edge XANES is highly sensitive to the local coordination field of titanium. Distinctive features can be observed in both the pre-edge and white line regions, respectively. To analyze titanium in titanium-1 silicate and determine the structure of titanium dioxide (TiO2) outside the framework, bulk titanium dioxide references, e.g., anatase and rutile, were first measured. As shown in Figure 1, anatase exhibited pre-edge properties at 4969 eV, 4971 eV, 4972 eV, and 4974 eV, respectively, and a sharp first white line at 4987 eV. Rutile exhibited pre-edge properties at 4969 eV, 4971 eV, and 4974 eV, respectively, a moderate first white line at 4987 eV, and a more pronounced white line at 4992 eV. For titanosilicates, where all titanium was incorporated into the frame and into the tetrahedral geometry, only one distinctive feature was observed at 4970 V in the pre-edge region and no distinctive feature was observed in the white line region. Regarding the X-ray absorption spectrum near the edge structure of anatase, it exhibits a signal intensity ratio at 4987 eV to the signal intensity at 4992 eV of 1.07 (1.17:1.09 = 1.07). Conversely, the X-ray absorption spectrum near the edge structure of rutile exhibits a signal intensity ratio at 4987 eV to the signal intensity at 4992 eV of 0.97 (1.12:1.16 = 0.97). Reference Example 1.3: Determination of the bridging concentration of µ2η2-peroxy species in a hydrogen peroxide-activated catalyst by 17O NMR spectroscopy All NMR measurements were acquired on a Bruker Avance III 600 MHz (14.1 T) NMR spectrometer at low temperatures (100 K) using a 3.2 mm probe. The magnetic field was externally controlled by setting the liquid water signal (at room temperature) to 0 ppm. Measurements were performed in a 3.2 mm sap-phire rotor enclosed with a zirconia cap. Previous WURST-CPMG (wideband, modulated monomorphic pulsed-response CPMG with echo sequence acquisition) experiments were performed to obtain 17O NMR spectra. The WURST pulse details were as follows: length, 50 μs; 80 steps; swiping width, 0.5 MHz; sweep from low to high frequency. A 100 kHz SPINAL64 was used for 1H separation. A titanium-1 silicate sample containing hydrogen peroxide labeled 17O was prepared by impregnating 25 mg of titanium-1 silicate zeolite with one equivalent (relative to titanium) of a 1.6 M aqueous solution of water labeled 17O. The samples were left to equilibrate for 15 minutes or 2 hours before spectroscopic measurements. As described above, the titanium-1 silicate sample was examined using 17O NMR solid-state spectroscopy at 100 K. This method allows for the observation of reaction media arising from H₂₁₇O₂ activation, while avoiding the need to average low-temperature potential values due to the dynamic properties and preventing peroxo decomposition. 17O NMR solid-state spectra of H₂₁₇O₂ and H₂₁₇O were also recorded, as these molecules are likely present in the catalyst sample. Solid-state NMR spectra of titanium-1 silicate samples at various titanium loadings that were touched with one equivalent (with respect to titanium) of a 1.6 M H217O2 solution for 2 hours showed that H217O2 reacted in all cases and that there were two new major concordance signals that showed intensity. To verify the peroxo formation rates and stability, a quantitative measurement protocol was developed. First, the WURST QCMPG spectrum was measured (as described above), and then the echo spectrum was reconstructed and decomposed into components related to water species, hydrogen peroxide, and peroxo. To avoid overfitting, the spectra obtained experimentally from water, hydrogen peroxide, and peroxo were fitted individually using DM Fit (see Figure 1). DM Fit was described by D. Massiot et al. in Magnetic Resonance in Chemistry 2002, vol. 40, pages 70–76. The initial estimate for each component was based on nuclear magnetic resonance (NMR) variables previously calculated by DFT in CP Gordon et al., Nature 2020, 586, 708–713, and the relative density of each species was optimized to approximate the best favorable fit. Based on the aforementioned DFT calculations, the observed 17O NMR signal was assigned. The corresponding concentrations were obtained by multiplying these ratios by the initial concentration (1.6 M) of the aqueous stock solution H217O2 used for wet impregnation. Relative values for H217O2, μ2η2-pyroxo bridging, and H217O2 (see "rel. H2O2", "rel. ε-pyroxo" and "rel. H2O" in Table 1 below) were obtained after 15 minutes and after 2 hours of measurements and application of the above quantitative protocol. The concentration of μ2η2 peroxo species in the H217O2-activated sample was calculated based on the relative concentration of μ2η2-peroxo bridging according to the following calculation: (Concentration of μ2η2 peroxo species) = [(Concentration of μ2η2-peroxo bridges) x (Concentration of H217O2 solution) x (Volume of labeled hydrogen peroxide 17O solution used for wet impregnation)] / [Weight of sample catalyst in mg] From the concentration mentioned, the molar concentration of μ2η2-peroxo bridging species per titanium was calculated (i.e., molar μ2η2-peroxo bridging per multititanium). Reference Example 1.4: X-ray diffraction of powder and determination of crystallinity Powder X-ray diffraction (PXRD) data were collected using a Bruker AXS GmbH D8 Advance Series II diffraction meter equipped with a LYNXEYE detector operating with a 40 kV, 40 mA copper anode X-ray tube. The engineering was by Bragg-Brentano, and air scattering was minimized using an air scatter shield. Crystallization Calculation for Titanium Silicate-1: Crystallization calculations were performed using a titration routine. Various mixtures were prepared of a perfectly crystalline sample with a dried primary crystallization suspension without seeded crystals, where the crystalline material had a mass percentage of 30%, 40%, 50%, 60%, 70%, 80%, 90%, and 100%. These samples were measured as described below. The analysis was performed by determining the net intensity values between diffraction angles of 21.3°²theta and 25°²theta. This was done using the "Space" tool within DIFFRAC.EVA provided by BrukerAXS GmbH, Karlsruhe (User Manual for DIFFRAC.EVA Version 5, April 2019, Bruker AXS GmbH, Karlsruhe). cr = Isample / Istandard Where Isample is the net intensity value of the sample and Istandard is the net intensity value of the standard sample. The crude crystallinity value was determined by calculating the net area of the sample divided by the net area of the standard sample. It was then corrected using a linear calibration function. , Where a and b are the equivalents determined using calibration data. Computing phase configuration: The phase configuration was calculated against the raw data using the DIFFRAC.TOPAS modeling software provided by Bruker AXS GmbH (User Manual for DIFFRAC.TOPAS Version 6, 2017, Bruker AXS GmbH, Karlsruhe). The crystal structures of the selected phases, the instrumental variables, and the crystal size of the individual phases were used to simulate the diffraction pattern. This was suitable for the data as well as for the background intensity modeling function. Data Collection: Samples were homogenized in a compacted mortar within a standard flat sample holder supplied by Bruker AXS GmbH for Bragg-Brentano geometry data collection. The flat surface was achieved using a glass plate to compress and level the sample powder. Data were collected from an angular range of 2 to 50°²theta with a step size of 0.02°²theta, while the variable spacing aperture was set to an angle of 0.1°. The crystalline content describes the strength of the crystal signal relative to the total dispersed intensity. Reference Example 1.5: Determining the specific surface area of Brunauer, Emmett, and Teller and the micropore size The specific surface area of Brunauer, Emmett, and Teller and the micropore size were determined via physical adsorption of nitrogen at 77 K according to the method disclosed in DIN 66131. Reference Example 1.6: Determination of propylene oxide activity (PO test) In the propylene oxide test, a preliminary experimental procedure to evaluate the suitability of molds as a catalyst for epoxide addition to propene, the molds were tested in a glass autoclave by reacting propene with aqueous hydrogen peroxide solution (30 wt%) to give propylene oxide. Specifically, 0.5 g of the molds and 45 mL of methanol were introduced into a glass autoclave, which was cooled to -25 °C. 20 mL of liquid propene was pressurized into the glass autoclave, and the autoclave was heated to 0 °C. At this temperature, 18 g of aqueous hydrogen peroxide solution (30 wt% in water) was introduced into the autoclave. After a reaction time of 5 h at 0 °C, the mixture was heated to room temperature, and the liquid phase was analyzed by gas chromatography for its propylene oxide content. The propylene oxide content of the liquid phase (by weight) was the result of the propylene oxide test, i.e., the propylene oxide activity of the molds. Reference Example 1.7: K-80 Test The K80 test was designed as a semi-quantitative assay to evaluate the rate of hydrogen peroxide decomposition by titanium-1 silicate and similar titanium-containing zeolite compounds. It allows for the quantitative determination of the effect of different catalytic treatments on hydrogen peroxide decomposition. Test procedure In a clean 100 mL flask equipped with a magnetic stir bar and a thermometer, 30 g of deionized water and 6.5 g of 40% hydrogen peroxide solution were placed at room temperature. At this point, t = zero for a 0.3 mL probe using a pipette. The flask was lightly sealed and then immersed in a pre-balanced thermostatic bath set to 80 °C. For reproducible results, it is important to always use the same amount of catalyst and control the temperature to better than ±1 °C throughout the experiment. Once the hydrogen peroxide solution was in thermal equilibrium with the thermostatic bath, 500 mg (±1 mg) of catalyst (either powder or extruded) was added. The suspension was stirred, and the supernatant was sampled at regular intervals. The probe should be taken with a 1 mL syringe using a Millipore Millex-HV SLHV 013 NL (Order No. 4875 160) or equivalent unidirectional filter. First, 0.6 mL of the solution was drawn into the syringe through the filter. Then, 0.3 mL of the solution was returned through the filter to the beaker. This is necessary to minimize catalyst loss.The remaining 0.3 ml in the syringe was then used to remove the peroxide. The interval between probes typically ranges from 30 to 60 minutes, depending on the catalyst activity. The experiment ends after 7 hours. Analytical properties The probes were analyzed for hydrogen peroxide content using standard thermal titration. It is recommended to analyze the probes as soon as possible after assembly. To ensure good calibration accuracy, the solution should be at least 5 mL. If a large amount of probe is required, it must be weighed. Data analysis The natural logarithm of hydrogen peroxide concentration over time was plotted. It is always important to use the same units when comparing data (e.g., hydrogen peroxide concentration as a percentage of weight and time in hours). This plot typically yields a straight line. The curve was obtained using least-squares methods. This curve represents the pseudo-first decomposition rate of hydrogen peroxide in the presence of the catalyst (measured in x⁻¹) and is called the k80 value. Example 1: Preparation of titanium silicate-1 catalyst according to the present invention To prepare the gel, 500 g of tetraethylorthosilicate (TEOS) and 3.75 g of tetraethylorthotitanate (TEOTi; Merck) were added to a container. A solution of 300 g of deionized water and 220 g of aqueous tetrapropylammonium hydroxide (TPAOH; 40 wt% in water) was then added under stirring (200 rpm). The resulting mixture exhibited a pH of 13.81. The mixture was then hydrolyzed at room temperature for 60 minutes, during which the temperature was raised to 60 °C. The mixture then exhibited a pH of 12.91. Ethanol was then distilled to a temperature of 95 °C. 546 g of distillate was obtained from the distillation. The synthesis gel was then cooled to 40°C under stirring, and 546 g of deionized water was added. The resulting mixture exhibited a pH of 11.91. The synthesized gel was then transferred to an autoclave. Under stirring, the gel was heated to 175 °C and stirred at this temperature for 16 hours under self-generated pressure. The pressure ranged from 8.4 to 11.9 bar (absolute). The resulting suspension was then run. To achieve this effect, the suspension was diluted with deionized water at a 1:1 weight ratio. Approximately 150 g of nitric acid (10 wt% in water) was then added, resulting in a pH of 7.53. The solids obtained were filtered and washed three times with deionized water (1000 mL of deionized water was used each time). After that, the solids were dried in an oven in air at 120 °C for 4 hours and then roasted in air at 490 °C for 5 hours, where the heating rate for roasting was 2 °C / minute. The resulting product exhibited a silicon content of 44% wt%, a titanium content of 0.52% wt%, and a total carbon loss of less than 0.1% wt%. The Brunauer, Emmett, and Teller specific surface area of the resulting product was 443 m² / g, and the water adsorption was 7.5% wt%. The crystallinity was 96%, and no anatase was detected by X-ray diffraction. The X-ray absorption spectrum was determined near the edge structure of the product, where the catalyst exhibits a signal intensity ratio of 0.95 at 4987 eV to 4992 eV (1.03:1.08 = 0.95). The results of the propylene oxide and K80 tests are shown in Tables 4 and 5, respectively. Example 2: Preparation of titanium silicate-1 catalyst according to the present invention To prepare the gel, 500 g of tetraethyl orthosilicate and 7.5 g of tetraethyl orthotitanate (Merck) were filled into a container. Then, a solution of 300 g of deionized water and 220 g of tetrapropyl ammonium hydroxide aqueous (40 wt% in water) was added under stirring (200 rpm). The resulting mixture exhibited a pH of 13.81. The mixture was then hydrated at room temperature for 60 minutes, during which time the temperature was raised to 60 °C. The mixture subsequently exhibited a pH of 12.71. Ethanol was then distilled until the infusion temperature reached 95 °C. 548 g of distillate was obtained from the distillation. The synthesis gel was then cooled to 40°C under stirring, and 548 g of deionized water was added. The resulting mixture exhibited a pH of 12.01. The synthesized gel was then transferred to an autoclave. Under stirring, the gel was heated to 175 °C and stirred at this temperature for 16 hours under self-generated pressure. The pressure ranged from 8.2 to 11.4 bar (absolute). The resulting suspension was then run. To achieve this effect, the suspension was diluted with deionized water at a 1:1 weight ratio. Approximately 155 g of nitric acid (10 wt% in water) was then added, resulting in a pH of 7.28. The solids obtained were filtered and washed three times with deionized water (1000 mL of deionized water was used each time). After that, the solids were dried in an oven in air at 120 °C for 4 hours and then roasted in air at 490 °C for 5 hours, where the heating rate for roasting was 2 °C / minute. The resulting product exhibited a silicon content of 43% wt%, a titanium content of 1.0% wt%, and a total carbon loss of less than 0.1% wt%. The Brunauer, Emmett, and Teller specific surface area of the resulting product was 450 m² / g, and the water adsorption was 8.45% wt%. Crystallization was 100%, and anatase was not detected by X-ray diffraction. The X-ray absorption spectrum was determined near the edge structure of the product, where the catalyst exhibits a signal intensity ratio of 0.96 at 4987 eV to 4992 eV (1.05:1.09 = 0.96). The results of the propylene oxide and K80 tests are shown in Tables 4 and 5, respectively. Example 3: Preparation of titanium silicate-1 catalyst according to the present invention To prepare the gel, 500 g of tetraethyl orthosilicate and 11.25 g of tetraethyl orthotitanate (Merck) were filled into a container. A solution of 300 g of deionized water and 220 g of tetrapropyl ammonium hydroxide (40 wt% in water) was then added under stirring (200 rpm). The resulting mixture exhibited a pH of 13.79. The mixture was then hydrolyzed at room temperature for 60 minutes, during which the temperature was raised to 60 °C. The mixture then exhibited a pH of 12.85. Ethanol was then distilled to a temperature of 95 °C. 546 g of distillate was obtained from the distillation. The synthesis gel was then cooled to 40°C under stirring, and 546 g of deionized water was added. The resulting mixture exhibited a pH of 11.86. The synthesized gel was then transferred to an autoclave. Under stirring, the gel was heated in the autoclave to 175 °C and stirred at this temperature for 16 hours under self-generated pressure. The pressure ranged from 8.4 to 11.9 bar (absolute). The resulting suspension was then run. To achieve this effect, the suspension was diluted with deionized water at a 1:1 weight ratio of suspension to deionized water. Approximately 150 g of nitric acid (10 wt% in water) was then added, resulting in a pH of 7.31. The solids obtained were filtered and washed three times with deionized water (1000 mL of deionized water was used each time). After that, the solids were dried in an oven in air at 120 °C for 4 hours and then roasted in air at 490 °C for 5 hours, where the heating rate for roasting was 2 °C / minute. The resulting product exhibited a silicon content of 42% wt%, a titanium content of 1.5% wt%, and a total carbon loss of less than 0.1% wt%. The Brunauer, Emmett, and Teller specific surface area of the resulting product was 449 m² / g, and the water adsorption was 9.6% wt%. The crystallinity was 96%, and no anatase was detected by X-ray diffraction. The X-ray absorption spectrum was determined near the edge structure of the product, where the catalyst exhibits a signal intensity ratio of 0.98 at 4987 eV to 4992 eV (1.06:1.08 = 0.98). The results of the propylene oxide and K80 tests are shown in Tables 4 and 5, respectively. Example 4: Preparation of titanium silicate-1 catalyst according to the present invention To prepare the gel, 500 g of tetraethyl orthosilicate and 15 g of tetraethyl orthotitanate (Merck) were placed in a container. A solution of 300 g of deionized water and 220 g of tetrapropyl ammonium hydroxide (40 wt% in water) was then added under stirring (200 rpm). The resulting mixture exhibited a pH of 13.83. The mixture was then hydrolyzed at room temperature for 60 minutes, during which time the temperature was increased to 60 °C. The mixture subsequently exhibited a pH of 12.71. Ethanol was then distilled to a temperature of 95 °C. 558 g of distillate was obtained from the distillation. The synthesis gel was then cooled to 40°C under stirring, and 558 g of deionized water was added. The resulting mixture exhibited a pH of 11.95. The synthesized gel was then transferred to an autoclave. Under stirring, the gel was heated in the autoclave to 175 °C and stirred at this temperature for 16 hours under self-generated pressure. The pressure ranged from 8.4 to 11.4 bar (absolute). The resulting suspension was then run. To achieve this effect, the suspension was diluted with deionized water at a 1:1 weight ratio of suspension to deionized water. Approximately 152 g of nitric acid (10 wt% in water) was then added, resulting in a pH of 7.21. The solids obtained were filtered and washed three times with deionized water (1000 mL of deionized water was used each time). After that, the solids were dried in an oven in air at 120 °C for 4 hours and then roasted in air at 490 °C for 5 hours, where the heating rate for roasting was 2 °C / minute. The resulting titanium-1 silicate exhibited a silicon content of 43 wt%, a titanium content of 2 wt%, and a total carbon loss of less than 0.1 wt%. The Brunauer, Emmett, and Teller specific surface area of the resulting titanium-1 silicate was 447 m² / g. The crystallinity was 92%, and approximately 0.5% of the anatase was detectable by X-ray diffraction. Next, 382.0 g of deionized water was added to any container. 150.9 g of tetrapropyl ammonium hydroxide (as an aqueous solution containing 40 wt% tetrapropyl ammonium hydroxide) was added with stirring. Then, 71.0 g of titanium-1 silicate was added. This mixture was homogenized for 30 minutes. The mixture was then transferred to an autoclave. It was hydrothermally treated at 170 °C for 6 hours. The resulting solids were separated by centrifugation, and the solid residue was washed with deionized water. The resulting solids were air-dried at 120 °C for 4 hours and then air-baked at 490 °C for 5 hours in an oven. The resulting titanium-1 silicate exhibited a silicon content of 44 wt%, a titanium content of 1.9 wt%, and a total carbon loss of less than 0.1 wt%. The Brunauer, Emmett, and Teller specific surface area of the titanium-1 silicate product was 446 m² / g, and its water adsorption was 7.25 wt%. The crystallinity was 93%, and approximately 0.7% of the anatase was detectable by X-ray diffraction. The X-ray absorption spectrum was determined near the edge structure of the product, where the catalyst exhibits a signal intensity ratio of 1.03 at 4987 eV to 4992 eV (1.13:1.10 = 1.03). The results of the propylene oxide and K80 tests are shown in Tables 4 and 5, respectively. Example 5: Preparation of titanium silicate-1 catalyst according to the present invention Titanium-1 silicate zeolite was prepared in accordance with Example 1 of International Order Document No. 064191 / 2011A1 except that 10% by weight of tetraethyl orthosilicate was used as a binding agent based on titanium-1 silicate. 1072 g of deionized water was provided in any container. Then, 424 g of tetrapropyl ammonium hydroxide (as an aqueous solution containing 40 wt% tetrapropyl ammonium hydroxide) was added under stirring. Next, 200 g of titanium-1 silicate zeolite was added. This mixture was homogenized for 30 minutes. The mixture was then transferred to an autoclave, where it was hydrothermally treated at 170 °C for 24 hours. The resulting solids were separated by centrifugation, and the solid residue was washed with deionized water. The resulting solid was then heated in air for 60 minutes to 110 °C and dried at that temperature for 4 hours. Finally, the resulting solid was heated in air for 190 minutes to 520 °C and roasted at that temperature for 16 hours. The titanium-1 silicate material obtained exhibited a silicon content of 45% wt%, a titanium content of 1.7% wt%, and a total carbon loss of less than 0.1% wt%. Its Brunauer, Emmett, and Teller specific surface area was 450 m² / g. 5000 g of aqueous nitric acid (10 wt% nitric acid (HNO3) in water) was supplied in a glass container. Under stirring, 250 g of titanium silicate-1 was added. The resulting suspension was flowed—while stirring at 250 rpm—at 100 °C for 1 hour. For processing, the resulting solids were separated by centrifugation. The resulting solids were heated in air for 60 minutes to 120 °C and dried at that temperature for 4 hours. Subsequently, the resulting solids were heated in air for 190 minutes to 500 °C and roasted at that temperature for 5 hours. The titanium-1 silicate material obtained exhibited a silicon content of 45 wt%, a titanium content of 1.8 wt%, and a total carbon loss of less than 0.1 wt%. Its Brunauer, Emmett, and Teller specific surface area was 453 m² / g, and its water adsorption was 7.0 wt%. The crystallinity was 97%, and approximately 1% of the anatase was detectable by X-ray diffraction. The results of the propylene oxide and K80 tests are detailed in Tables 4 and 5, respectively. Example 6: Preparation of a catalyst according to the present invention Using a modified synthetic procedure, titanium silicate-1 was synthesized with a silicon content of 44 wt%, a titanium content of 1.2 wt%, and a total carbon loss of less than 0.1 wt%. The Brunauer, Emmett, and Teller specific surface area of titanium silicate-1 was 429 m² / g, the micropore volume was 0.07 mL / g, the total pore volume was 0.37 mL / g, and the water adsorption was 3.4 wt%. Crystallinity was 100%, as determined by X-ray diffraction. The X-ray absorption spectrum was determined near the edge structure of the product, where the catalyst exhibits a signal intensity ratio of 0.99 at 4987 eV to 4992 eV (1.07:1.08 = 0.99). The results of the propylene oxide and K80 tests are shown in Tables 4 and 5, respectively. Example 7: Preparation of a catalyst according to the present invention Using a modified synthetic procedure, titanium-1 silicate was synthesized with a silicon content of 46 wt%, a titanium content of 1.2 wt%, and a total carbon loss of less than 0.1 wt%. The Brunauer, Emmett, and Teller specific surface area of the resulting titanium-1 silicate was 392 m² / g, the micropore volume was 0.06 mL / g, the total pore volume was 0.39 mL / g, and the water adsorption was 4.4 wt%. The crystallinity was 89%, and approximately 0.9% of anatase was detectable by X-ray diffraction. The X-ray absorption spectrum was determined near the edge structure of the product, where the catalyst exhibits a signal intensity ratio of 1.07 at 4987 eV to 4992 eV (1.16:1.08 = 1.07). The results of the propylene oxide and K80 tests are shown in Tables 4 and 5, respectively. Comparative Example 8: Preparation of a catalyst according to the previous technique To prepare the gel, 496.7 g of tetraethyl orthosilicate and 21.8 g of tetraethyl orthotitanate (Merck) were filled into a container. A solution of 298.3 g of deionized water and 218.2 g of tetrapropyl ammonium hydroxide (40 wt% in water) was then added under stirring (200 rpm). The mixture was hydrated at room temperature for 60 minutes, during which the temperature was raised to 60 °C. Ethanol was then distilled until the infusion temperature reached 85 °C. 450 g of the distillate was added. The synthesized gel was then cooled to 40°C with stirring and the addition of 450 g of deionized water. The resulting mixture exhibited a pH of 12.1. The synthesized gel was then transferred to an autoclave. Under stirring, the gel was heated in the autoclave to 175 °C and stirred at this temperature for 16 hours under self-generated pressure. The resulting suspension was then run. To achieve this effect, the suspension was diluted with deionized water at a 1:1 weight ratio of suspension to deionized water. Subsequently, 178.6 g of nitric acid (10 wt% in water) was added. The pH was adjusted to 7 with approximately 3 mL of ammonium hydroxide (NH₄OH) solution (25 wt% ammonium hydroxide in water). The resulting solids were filtered and washed three times with deionized water (1000 mL of deionized water was used each time). After that, the solids were dried in an oven in air at 120 °C for 4 hours and then roasted in air at 490 °C for 5 hours, where the heating rate for roasting was 2 °C / minute. The resulting titanium-1 silicate exhibited a silicon content of 43 wt%, a titanium content of 2.8 wt%, and a carbon content of 0.6 wt%. The Brunauer, Emmett, and Teller specific surface area of the resulting titanium-1 silicate was 434 m² / g. The crystallinity was 81%, and approximately 0.7% anatase was detectable by X-ray diffraction. The results of the propylene oxide test and the K80 test are detailed in Tables 4 and 5, respectively. Comparative Example 9: Preparation of a catalyst according to the previous technique To prepare the gel, 500 g of tetraethyl orthosilicate and 15 g of tetraethyl orthotitanate (Merck) were placed in a container. A solution of 300 g of deionized water and 220 g of tetrapropyl ammonium hydroxide (40 wt% in water) was then added under stirring (200 rpm). The resulting mixture exhibited a pH of 13.5. The mixture was then hydrolyzed at room temperature for 60 minutes, during which the temperature was raised to 60 °C. The mixture subsequently exhibited a pH of 12.6. Ethanol was then distilled to a temperature of 95 °C. 540 g of distillate was obtained from the distillation. The synthesized gel was then cooled to 40°C with stirring and 542 g of deionized water added. The resulting mixture exhibited a pH of 11.9. The synthesized gel was then transferred to an autoclave. Under stirring, the gel was heated to 175 °C and stirred at this temperature for 16 hours under self-generated pressure. The pressure ranged from 8.4 to 10.9 bar (absolute). The resulting suspension was then run. To achieve this effect, the suspension was diluted with deionized water at a 1:1 weight ratio. Approximately 164 g of nitric acid (10 wt% in water) was then added, resulting in a pH of 7.35. The solids obtained were filtered and washed four times with deionized water (1000 mL of deionized water was used each time). After that, the solids were dried in an oven in air at 120 °C for 16 hours and then roasted in air at 490 °C for 5 hours, where the heating rate for roasting was 2 °C / minute. The titanium-1 silicate material obtained exhibited a silicon content of 43 wt%, a titanium content of 2 wt%, and a total carbon loss of less than 0.1 wt%. Its Brunauer, Emmett, and Teller specific surface area was 462 m² / g, and its water adsorption was 11.5 wt%. The crystallinity was 88%, as determined by X-ray diffraction. The X-ray absorption spectrum was determined near the edge structure of the product, where the catalyst exhibits a signal intensity ratio of 0.97 at 4987 eV to 4992 eV (1.05:1.08 = 0.97). The results of the propylene oxide and K80 tests are shown in Tables 4 and 5, respectively. Reference Example 1.8: Identifying the Activating Factor of Examples and Comparative Examples To determine the activation factor of the prepared catalysts, the bridging concentration of µ2η2-peroxy species per titanium in the hydrogen peroxide-activated catalyst (“ml mol µ-peroxy species / mol titanium”) was determined for the examples and comparison examples according to the method described in Reference Example 1.3, where the concentration was determined 15 minutes and 2 hours after the corresponding samples were activated with hydrogen peroxide. Table 1 Review the relative values of H217O2, µ2η2-peroxy bridging (“µ-peroxy”), and H217O after 15 minutes and after 2 hours as determined by the measurements and using the measurement protocol described in Reference Example 1.3. # Titanium content [% by weight] H217O2 (15 min) [%] µ-Peroxy-relative (15 min) [%] H217O2 relative (15 min) [%] H217O2 relative (2 h) [%] µ-Peroxy-relative (2 h) [%] H217O2 relative (2 h) [%] Example 1 0.52 0.23 0.41 0.36 0.07 0.46 0.47 Example 2 1.0 0.24 0.53 0.23 0.07 0.58 0.35 Example 3 1.5 0.31 0.54 0.15 0.04 0.72 0.25 Comparative example 9 2.0 0.21 0.66 0.13 0.04 0.80 0.16 Example 4 1.9 0.42 0.41 0.17 0.08 0.61 0.31 Comparative example 8 2.8 0.23 0.66 0.11 0.07 0.76 0.17 Example 6 1.2 0.00 0.77 0.23 0.00 0.68 0.32 Example 7 1.2 0.00 0.67 0.33 0.00 0.59 0.41 Example 5 1.8 0.00 0.65 0.35 0.00 0.54 0.46 Table 2 Review the concentrations of H217O2, µ2η2-peroxy bridging (“µ-peroxy”), and H217O after 15 minutes calculated according to Reference Example 1.3 and based on the corresponding relative concentration value. # Titanium content [% by weight] H217O2 concentration (15 min) [micromol / mg] µ-peroxygen concentration (15 min) [micromol / mg] H217O2 concentration (15 min) [micromol / mg] Example 1 0.5 0.024 0.042 0.037 Example 2 1.0 0.050 0.112 0.049 Example 3 1.5 0.099 0.168 0.046 Comparative example 9 2.0 0.086 0.276 0.054 Example 4 1.9 0.167 0.164 0.066 Comparative example 8 2.8 0.132 0.385 0.066 Example 6 1.2 0.000 0.192 0.057 Example 7 1.2 0.000 0.166 0.083 Example 5 1.8 0.000 0.247 0.131 Table 3 Review of H217O2, µ2η2-peroxy bridging (“µ-peroxy”), and H217O concentrations after 2 hours calculated according to Reference Example 1.3 and based on the corresponding relative concentration value. # Titanium content [% by weight] H217O2 concentration (2 hours) [micromol / mg] µ-peroxygen concentration (2 hours) [micromol / mg] H217O concentration (2 hours) [micromol / mg] Example 1 0.5 0.007 0.047 0.048 Example 2 1.0 0.016 0.122 0.073 Example 3 1.5 0.011 0.226 0.077 Comparative example 9 2.0 0.015 0.333 0.068 Example 4 1.9 0.034 0.242 0.121 Comparative example 8 2.8 0.043 0.443 0.096 Example 6 1.2 0.000 0.170 0.080 Example 7 1.2 0.000 0.147 0.103 Example 5 1.8 0.000 0.203 0.174 Table 4 Activating factors after 15 minutes and results of fungal tests of the prepared catalysts. Activation factor (15 mins) [ml mol / mol] Water adsorption [g / g] 17O-NMR:ml mol µ-peroxygen / mol Titanium (15 mins) [ml mol / mol] Propylene oxide test [% wt] K-80 test Comparative example: 8 77 0.117 657 7.4 0.936 Comparative example: 9 76 0.115 660 8.7 0.56 Example 3 52 0.096 537 8.2 0.41 Example 2 45 0.0845 536 7.7 0.36 Example 5 46 0.070 655 9.3 0.23 Example 6 26 0.034 765 10.4* 0.179 Example 4 30 0.0725 412 9.4 0.16 Example 1 29 0.075 386 3.7 0.12 Example 7 29 0.044 663 12.1 0.55 (*) The propylene oxide test is carried out according to reference example 1.6 but uses only 0.25 g of catalyst instead of 0.5 g. Table 5 Activating factors after two hours and results of fungal tests of the prepared catalysts. # Activation factor (2 hours) [ml mol / mol] Water adsorption [g / g] 17O -NMR: ml mol µ-peroxygen / mol Titanium (2 hours) [ml mol / mol] Propylene oxide test [% wt] K-80 test Comparative example: 8 89 0.117 757 7 4. 0.936 Comparative Example 9 91 0.115 795 8.7 0.56 Example 3 69 0.096 719 8.2 0.41 Example 2 49 0.0845 584 7.7 0.36 Example 5 38 0.070 540 9.3 0.23 Example 6 23 0.034 677 10.4* 0.179 Example 4 44 0.0725 609 9.4 0.16 Example 1 32 0.075 431 3.7 0.12 Example 7 26 0.044 584 12.1 0.55 (*) The propylene oxide test is carried out according to reference example 1.6 but uses only 0.25 g of catalyst instead of 0.5 g. As shown in the results of Tables 4 and 5, the catalysts of the examples according to the present invention were surprisingly found to exhibit the presence of an activating agent in the range of 15 to 70 after 15 minutes and again after 2 hours. They also exhibited significantly lower hydrogen peroxide decomposition rates, as determined by the K-80 test, compared to the catalysts of the comparative examples. Specifically, the catalysts of comparative examples 8 and 9 showed hydrogen peroxide decomposition rates of 0.936 and 0.56, respectively. In contrast, the catalysts of the present invention exhibited a maximum hydrogen peroxide decomposition rate of 0.41 for the catalyst of example 3. The lowest hydrogen peroxide decomposition rate by the catalyst of example 1 was 0.12. In addition, the catalysts according to the present invention exhibit at least good, if not excellent, performance in the propylene oxide test, as shown by the results in Tables 4 and 5. Specifically, the catalysts according to examples 4-7 perform better in the propylene oxide test than the catalysts according to comparative examples 8 and 9. In particular, the catalyst according to example 6 was found to perform well, exhibiting the highest activity in the test despite using only half the amount of catalyst compared to the other samples tested.
Claims
Claims1 . A catalyst for hydrogen peroxide activation, wherein the catalyst comprises Ti, Si, and O, wherein the catalyst displays a water adsorption (W), a concentration (C) of bridging p2q2- peroxo species per Ti in the H2O2-activated catalyst as determined by quantitative17O NMR spectroscopy, and an activation factor (A) according to formula I, wherein the activation factor is in the range of from 15 to 80 mmol / mol; wherein in accordance with formula I, the activation factor is the multiplication product of the water adsorption and the concentration of bridging p2q2-peroxo species per Ti in the H2O2-activated catalyst:A = W x C (I).
2. The catalyst of claim 1 , wherein the catalyst displays a XANES spectrum having a ratio of the intensity of the signal at 4987 eV to the intensity of the signal at 4992 eV in the range of from 0.95 : 1 to 1.07 : 1.
3. The catalyst of claim 1 or 2, wherein the catalyst comprises a zeolitic material having a framework structure comprising Si, Ti, and O.
4. The catalyst of claim 3, the zeolitic material having an Si : Ti molar ratio in the range of from 1 to 250.
5. The catalyst of claim 3 or 4, wherein the zeolitic material has a framework structure type selected from the group consisting of MFI, MEL, IMF, SVY, FER, SVR, and intergrowth structures of two or more thereof.
6. A method for the preparation of a catalyst molding, comprising(a) providing a catalyst for hydrogen peroxide activation according to any of claims 1 to 5;(b) mixing the catalyst provided in step (a) with one or more binders;(c) optionally kneading of the mixture obtained in step (b);(d) molding of the mixture obtained in step (b) or (c) to obtain one or more moldings;(e) optionally drying of the one or more moldings obtained in step (d); and(f) calcining of the molding obtained in step (d) or (e).
7. The method of claim 6, wherein providing the catalyst in (a) comprises selecting the catalyst among catalysts comprising Ti, Si, and O, and displaying a water adsorption (W), and a concentration (C) of bridging p2q2-peroxo species per Ti in the H2O2-activated catalyst as determined by quantitative17O NMR spectroscopy; wherein the catalyst is selected by calculating an activation factor (A) in accordance withformula I for each of the catalysts, and selecting a catalyst displaying an activation factor in the range of from 15 to 80 mmol / mol, wherein the activation factor is the multiplication product of the water adsorption and the concentration of bridging p2q2-peroxo species per Ti in the H2O2-activated catalyst:A = W x C (I).
8. The method of claim 7, wherein providing the catalyst in (a) comprises selecting the catalyst among catalysts displaying a water adsorption in the range of from 1 to 10 wt.-%.
9. The method of claim 7 or 8, wherein providing the catalyst in (a) comprises selecting the catalyst among catalysts displaying a concentration of bridging p2q2-peroxo species per Ti in the H2O2-activated catalyst in the range of from 200 to 1 ,200 mmol / mol.
10. A catalyst molding comprising a catalyst for hydrogen peroxide activation according to any of claims 1 to 5.
11. A process for the activation of hydrogen peroxide comprising:(1 ) providing a reactor comprising a catalyst for hydrogen peroxide activation according to any of claims 1 to 5, or a catalyst molding according to claim 10;(2) contacting the catalyst or catalyst molding provided in (1 ) with hydrogen peroxide.
12. The process of claim 11 , wherein providing the catalyst in (1 ) comprises selecting the catalyst among catalysts comprising Ti, Si, and O, and displaying a water adsorption (W), and a concentration (C) of bridging p2q2-peroxo species per Ti in the H2O2-activated catalyst as determined by quantitative17O NMR spectroscopy; wherein the catalyst is selected by calculating an activation factor (A) in accordance with formula I for each of the catalysts, and selecting a catalyst displaying an activation factor in the range of from 15 to 80 mmol / mol, wherein the activation factor is the multiplication product of the water adsorption and the concentration of bridging p2q2-peroxo species per Ti in the H2O2-activated catalyst:A = W x C (I).
13. The process of claim 12, wherein providing the catalyst in (1) comprises selecting the catalyst among catalysts displaying a water adsorption in the range of from 1 to 10 wt.-%.
14. The process of claim 12 or 13, wherein providing the catalyst in (1) comprises selecting the catalyst among catalysts displaying a concentration of bridging p2q2-peroxo species per Ti in the H2O2-activated catalyst in the range of from 200 to 1 ,200 mmol / mol.
15. Use of the catalyst according to any one of claims 1 to 5, or of a catalyst molding according to claim 10, as a catalyst and / or catalyst component in a reaction involving C-C bond formation and / or conversion.