Methods for preparing c2 to c4 hydrocarbons

A hybrid catalyst combining zirconia with gallium oxide and microporous molecular sieves addresses inefficiencies in forming 2- to 4-carbon hydrocarbons, achieving high yields and stability through optimized porosity and integration.

SA1120247323B1Active Publication Date: 2026-10-06DOW SILICONES CORP +1
View PDF 0 Cites 0 Cited by

Patent Information

Application Number
SA1120247323
Authority / Receiving Office
SA · SA
Patent Type
Patents
Current Assignee / Owner
Filing Date
2024-12-21
Publication Date
2026-10-06
Estimated Expiration
2043-07-21

AI Technical Summary

Technical Problem

Existing hybrid catalysts are inefficient in forming 2- to 4-carbon hydrocarbons from hydrogen and carbon-containing gas feed streams due to low carbon conversion rates and rapid loss of activity.

Method used

A hybrid catalyst composed of a metal oxide catalyst component, such as zirconia with gallium oxide, and a microporous catalyst component, such as molecular sieves with 8-atom ring pores, integrated with a binder to form a shaped catalyst, which is extruded, dried, and calcined, optimizing macroporosity and activity.

Benefits of technology

The hybrid catalyst achieves high and stable yields of 2- to 4-carbon hydrocarbons with improved carbon conversion and selectivity, maintaining efficiency over prolonged use.

✦ Generated by Eureka AI based on patent content.
Patent Text Reader

Abstract

According to the applied models, the preparation of a formed hybrid catalyst involves mixing a metal oxide catalyst component with a microporous catalyst component, adding a binder to the mixture of the metal oxide catalyst component and the microporous catalyst component to form a paste, where the binder is a colloidal solution, suspension, or gel of binder precursors consisting of aluminum oxides or aluminum hydroxides, zirconium oxides or zirconium hydroxides, or mixtures thereof, and extruding the paste to produce the formed hybrid catalyst. The metal oxide catalyst component may include gallium oxide and zirconia, where the zirconia has a macroporosity ratio of less than 0.3. The microporous catalyst component includes a molecular sieve with pore openings containing an 8-membered ring (8-MR).The hybrid catalyst formed can be used in a process to convert a feed current into an output current containing hydrocarbons with 2 to 4 carbon atoms.
Need to check novelty before this filing date? Find Prior Art

Description

The applied models for preparing the formed hybrid catalyst and the processes for forming 2- to 4-carbon hydrocarbons from a feed stream containing hydrogen gas and carbon-containing gas will now be described in detail. As used here, "carbon-containing gas" refers to a gas selected from carbon monoxide, carbon dioxide, and mixtures thereof. As used here, the term "synthesis gas" or "synthesis gas" refers to a gas containing hydrogen gas and carbon-containing gas. According to one applied model, the methods for preparing the formed hybrid catalyst may involve mixing a metal oxide catalyst component and a microporous catalyst component to form a mixture, adding a binder to this mixture to form a paste, extruding the paste to produce the formed hybrid catalyst, followed by drying and calcination.The metal oxide catalyst component may include gallium oxide and zirconia, with the zirconia having a macroporosity of less than 0.30. The microporous catalyst component consists of a molecular sieve with pore openings containing an 8-atom ring. The binder may be a colloidal solution, suspension, or gel of a binder precursor composed of aluminum oxides or aluminum hydroxides, zirconium oxides or zirconium hydroxides, or mixtures thereof. In one application model, the preparation of 2- to 4-carbon hydrocarbons involves introducing a feed stream of hydrogen gas and a carbon-containing gas (chosen from a range of carbon monoxide, carbon dioxide, and mixtures thereof) into a reactor reaction zone. This feed stream is then converted into a product stream of 2- to 4-carbon hydrocarbons in the reaction zone in the presence of a shaped hybrid catalyst. The shaped hybrid catalyst can be prepared using methods specifically designed for shaped hybrid catalysts, as described here. Hybrid-formed catalysts are commonly used in the hydrocarbon products industry, such as diesel or aromatics. However, many known hybrid-formed catalysts are inefficient in forming 2- to 4-carbon hydrocarbons, such as 2- to 4-carbon paraffins or 2- to 4-carbon olefins, from hydrogen gas and carbon-containing gas feed streams, due to their low carbon conversion rate in the feed stream and / or rapid loss of activity and efficiency.In contrast, the hybrid shaped catalysts described here exhibit high and stable yields of 2- to 4-carbon hydrocarbons, even with prolonged use, compared to hybrid catalysts incorporating a metal oxide catalyst on zirconia with a relatively high macropore content (indicating a high percentage of large pores). The preparation method and composition of these hybrid shaped catalysts used in the applied models are described below. According to one application model, the term "metal oxide catalyst component" may refer to a metal oxide support material coated with one or more dopants. For example, such a metal oxide catalyst component might include a zirconia support material coated with one or more dopants, including gallium oxide and a rare-earth oxide. In another application model, the term "microporous catalyst component" may refer to a molecular sieve zeolitic component containing crystalline aluminosilicates with a three-dimensional interconnecting network of silicate tetrahedra (SiO4) and aluminate ions (AlO4-).According to one application model, the term "microporous catalyst component" may refer to a molecular sieve zeotype component comprising crystalline silico-aluminophosphates with a three-dimensional network connected to a network of tetrahedra of [PO4]phosphate and [AlO4]- phosphate ions, where aluminum and / or phosphorus are partially replaced by silicon. Another application model suggests that the term "bonding material" may refer to a substance capable of linking the metal oxide catalyst component with the microporous catalyst component to integrate them into a single catalyst body. According to one application model, the metal oxide catalyst component may include zirconia, which acts as a metal oxide support material. The term "metal oxide support material" may refer to a supporting material that supports other components of the metal oxide catalyst component, such as gallium oxide or rare-earth oxide. In some application models, the zirconia in the metal oxide catalyst component may contain micropores. The term "micropores" may refer to pores in a material where one or more pores have a diameter of less than 2 nanometers. In some application models, the zirconia in the metal oxide catalyst component may contain mesopores. The term "mesopores" may refer to pores in a material where one or more pores have a diameter between 2 and 50 nanometers. In some application models, the zirconia in the metal oxide catalyst component may contain macropores. The term "macropores" may refer to pores in a material where the diameter of one or more pores is greater than or equal to 80 nanometers.It has been shown here that large quantities of macropores in zirconia increase the inhibition of hybrid catalyst activity. Therefore, zirconia should ideally possess a low macropore count. The term "macroporosity ratio" may refer to the size of large pores in the zirconia support material compared to the total pore size of zirconia support material smaller than 500 nm. To test the macroporosity ratio, mercury porosimetry can be used. This test measures the porosity of the zirconia by immersing the material in mercury and applying controlled pressure to the system so that the mercury can penetrate the pores of the material. Based on the pressure required to introduce the mercury into specific pores in the zirconia support material, the pore diameter and volume can be calculated. The pore diameter and its associated pressure can be related using the formula below, where D represents the pore diameter of the zirconia support material, P represents the pressure required for mercury to enter the pore of that zirconia support material, γ represents the surface tension of the mercury, and θ represents the contact angle between the zirconia and the mercury. (Form I) For example, when the NorPro SZ31164 zirconia support was tested using mercury porosimetry, the total immersion volume of mercury in the macropores of the zirconia support (i.e., pores with diameters ranging from 80-500 nm) was found to be 0.0406 ml / g, while the total immersion volume of mercury in all pores with diameters ranging from 3-500 nm was 0.294 ml / g, resulting in a macroporosity ratio of 0.138. Without adhering to a specific theory, it is believed that the low macroporosity of the zirconia support material leads to the hybrid catalyst achieving a higher conversion rate of compounds in the feed gas stream containing hydrogen and carbon-containing gas, with a lower catalyst deactivation rate. In applied models, the mixed metal oxide catalyst component includes gallium oxide. As used here, "gallium oxide" refers to gallium in various oxidation states. In applied models, gallium oxide can be deposited on the surface of zirconia or be in a solid solution with zirconia. In other applied models, gallium oxides may include, but are not limited to, gallium oxide (Ga2O3), gallium oxyhydroxide (GaO(OH)), and gallium oxyhydroxide (Ga5O7(OH)). Gallium oxides may also include various forms, such as monoclinic (β-Ga2O3), rhombohedral (α-Ga2O3), defective spinel (γ-Ga2O3), cubic (δ-Ga2O3), or orthorhombic (ε-Ga2O3).In other applied models, gallium oxide can contain gallium in one or more oxidation states. For example, individual gallium may be in different oxidation states. Gallium oxide is not limited to gallium in homogenous oxidation states. In short, hybrid catalysts closely link independent reactions on both independent catalysts. In the first step, a feed stream consisting of hydrogen gas (H₂) and a carbon-containing gas (chosen from a group of carbon monoxide, carbon dioxide, or a mixture of carbon monoxide and carbon dioxide, such as, for example, syngas) is converted into an intermediate compound(s), such as oxygenated hydrocarbons. In the next step, these intermediate compounds are converted into a product stream consisting of hydrocarbons (mostly short-chain hydrocarbons, such as, for example, hydrocarbons with 2 to 4 carbon atoms).The continuous formation and consumption of intermediate oxygenates formed in the first step by the reactions of the second step is ensured with the emphasis that there is no thermodynamic limit to the conversions. In one or more application models, the formulated hybrid catalyst is characterized by a particle size ranging from 0.5 mm to 6.0 mm. For example, the formulated hybrid catalyst may have a particle size of at least 0.5 mm, or at least 1.0 mm, or at least 1.5 mm, or at least 2.0 mm, or at least 2.5 mm, or at least 3.0 mm, or at least 3.5 mm, or at least 4.0 mm, or at least 4.5 mm, or at least 5.0 mm, or at least 5.5 mm, or even 6.0 mm. In some applied models, the shaped hybrid catalyst may have particle sizes less than 3.0 mm, for example, less than 2.5 mm, less than 2.0 mm, less than 1.5 mm, less than 1.0 mm, or less than 0.5 mm. In other applied models, the shaped hybrid catalyst may have particle sizes ranging from 0.5 mm to 5.5 mm, from 0.5 mm to 5.0 mm, from 0.5 mm to 4.5 mm, from 0.5 mm to 4.0 mm, from 0.5 mm to 3.5 mm, from 0.5 mm to 3.0 mm, from 0.5 mm to 2.5 mm, from 0.5 mm to 2.0 mm, or from 0.5 mm to 1.5 mm.In some applied models, the shaped hybrid catalyst may have particle sizes ranging from 1.0 mm to 6.0 mm, 1.5 mm to 6.0 mm, 2.0 mm to 6.0 mm, 2.5 mm to 6.0 mm, 3.0 mm to 6.0 mm, 3.5 mm to 6.0 mm, 4.0 mm to 6.0 mm, 4.5 mm to 6.0 mm, 5.0 mm to 6.0 mm, or 5.5 mm to 6.0 mm. The particle size may primarily represent the shorter dimension of the catalyst particle. For example, when the hybrid catalyst particle is shaped like a hollow cylinder or a ring, the particle size is the thickness of the hollow cylinder wall. When the shaped hybrid catalyst particle is spherical, the particle size is the diameter of the spherical particle. The particle size of the formed hybrid catalyst can be controlled by selecting the diameter of the extrusion die and measuring it using dynamic image analysis methods. In one or more application models, zirconia in the metal oxide catalyst component may have a macroporosity of less than 0.30, for example, less than 0.25, less than 0.20, less than 0.15, or even less than 0.10. In one or more application models, the macroporosity may range between 0.05 and 0.25, between 0.10 and 0.25, or between 0.10 and 0.20. In some application models, the macroporosity may range between 0.05 and 0.25, between 0.05 and 0.20, between 0.05 and 0.15, or between 0.0 and 0.10. In some applied models, the macroporosity ratio may range between 0.10 and 0.30, or between 0.15 and 0.30, or between 0.20 and 0.30, or between 0.25 and 0.30. The metal oxide catalyst component includes gallium oxide and / or zirconia oxide (ZrO2). As used in this document, the zirconia used in the applied models described here in the hybrid metal oxide catalyst component is "phase-pure zirconia," which is defined here as zirconia to which no other materials have been intentionally added during its formation. Therefore, the term "phase-pure zirconia" includes zirconia with small amounts of components other than zirconium (including other oxides besides zirconia) that are unintentionally present in the zirconia as a natural part of the zirconia formation process, such as, for example, hafnium (Hf). Accordingly, as used here, "zirconia" and "phase pure zirconia" are used interchangeably unless specifically specified otherwise.In other application models, zirconia can be non-phase pure zirconia, such as zirconia doped with calcium, yttria, lanthanum, cerium, or any of the rare earth elements. In the applied models presented here, the composition of the metal oxide catalyst component is determined by the weight ratio of gallium to pure zirconia (by stoichiometry of zirconia oxide and gallium oxide). In one or more of the applied models, the composition of the metal oxide catalyst component is determined by the weight ratio of gallium. For example, a metal oxide catalyst component may contain gallium in a weight percentage ranging from 0.1% to 10%, or from 0.1% to 9%, 0.1% to 8%, 0.1% to 7%, 0.1% to 6%, 0.1% to 5%, 0.1% to 4%, 0.1% to 3%, 0.1% to 2%, 0.5% to 10%, 1% to 10%, 2% to 10%, 3% to 10%, 4% to 10%, 5% to 10%, 6% to 10%, 7% to 10%, 8% to 10%, 9% to 10%, or 1% to 10%. 5%, or between 3% and 10%, or between 3% and 7%. In some applied models, the metal oxide catalyst component includes lanthanide oxide. In other applied models, additional elements from a range of rare earth elements, and / or lanthanides, and / or transition metals, such as nickel (Ni), palladium (Pd), or platinum (Pt), can be precipitated with gallium precursors, or they can be introduced only when preparing the mixed composition that includes gallium oxide and zirconia first. In the applied models presented here, the composition of the metal oxide catalyst component is determined by the weight percentage of lanthanide oxide metal to pure zirconia (by zirconia oxide valence assay). In one or more applied models, the composition of the metal oxide catalyst component is determined by the weight percentage of lanthanide on an oxidic basis. According to one or more application models, the metal oxide catalyst component can include lanthanide in a weight percentage ranging from 0.1% to 7%, for example, containing lanthanide in a weight percentage ranging from 0.5% to 7%, or from 1% to 7%, or from 2% to 7%, or from 3% to 7%, or from 4% to 7%, or from 5% to 7%, or from 6% to 7%, or from 0.1% to 6%, or from 0.1% to 5%, or from 0.1% to 4%, or from 0.1% to 3%, or from 0.1% to 2%, or from 0.1% to 1%, or from 0.5% to 5%, or from 0.5% to 3%, or from 3% to 7%, or from 5% to 7%. In applied models, one of the methods used to prepare the metal oxide catalyst component for the hybrid catalyst is by incipient wetness impregnation. In this method, an aqueous mixture of a gallium precursor, such as gallium(III) nitrate hydrate (Ga(NO3)3∙xH2O), and / or an aqueous mixture of a rare earth metal precursor, such as lanthanum(III) nitrate hexahydrate (La(NO3)3∙6H2O), is added to zirconia powder. In application models, the aqueous mixture containing the gallium precursor and / or rare earth metal precursor can be sprayed, added by distillation, or by any other similar method to ensure a uniform or near-uniform distribution of the mixture over the zirconia. This can be achieved by mixing the zirconia powder with the aqueous mixture.In other application models, gallium oxide can be deposited or distributed onto zirconia oxide using chemical vapor deposition (CVD). However, the method for fabricating the gallium oxide and metal oxide component of the resulting hybrid catalyst is not specifically limited, and any method involving the application of a thin layer of gallium oxide and rare earth oxide onto the surface of zirconium oxide can be used according to the application models. It is worth noting that the total amount of gallium precursors and rare earth metal precursors mixed with zirconia will be determined based on the target amount of gallium and rare earth metals required in the metal oxide catalyst component. According to some applied models, zirconia particles are crystalline in structure. In other applied models, zirconia particles are monoclinic in structure. In one or more applied models, zirconia particles are primarily composed of, or include, crystalline zirconia particles, while in some applied models, zirconia particles are primarily composed of, or include, monoclinic zirconia particles. In applied models, the surface area of ​​zirconia particles may be greater than or equal to 5 square meters per gram (m² / g). For example, the surface area of ​​zirconia particles may be at least 5 m² / g, at least 10 m² / g, at least 20 m² / g, at least 50 m² / g, at least 75 m² / g, at least 100 m² / g, at least 125 m² / g, or at least 150 m² / g. In some applied models, the surface area of ​​zirconia particles ranges from 5 m² / g to 200 m² / g, or from 10 m² / g to 200 m² / g, or from 20 m² / g to 200 m² / g, such as from 30 m² / g to 200 m² / g, or from 40 m² / g to 200 m² / g, or from 50 m² / g to 200 m² / g, or from 60 m² / g to 200 m² / g, or from 70 m² / g to 200 m² / g, or from 80 m² / g to 200 m² / g, or from 90 m² / g to 200 m² / g, or from 100 m² / g to 200 m² / g, or from 110 m² / g to 200 m² / g m2 / g, or from 120 m2 / g to 200 m2 / g, or from 130 m2 / g to 200 m2 / g, or from 140 m2 / g to 200 m2 / g.In some applied models, the surface area of ​​zirconia particles ranges from 5 m² / g to 180 m² / g, such as 5 m² / g to 160 m² / g, 5 m² / g to 140 m² / g, 5 m² / g to 120 m² / g, 5 m² / g to 100 m² / g, 5 m² / g to 90 m² / g, 5 m² / g to 80 m² / g, 5 m² / g to 70 m² / g, 5 m² / g to 60 m² / g, 5 m² / g to 50 m² / g, 5 m² / g to 40 m² / g, 5 m² / g to 30 m² / g, or 5 m² / g to 20 m² / g. From 5 m2 / g to 10 m2 / g. In some applied models, the surface area of ​​zirconia particles ranges from 10 m2 / g to 160 m2 / g, or from 20 m2 / g to 130 m2 / g, or from 30 m2 / g to 120 m2 / g, or from 40 m2 / g to 110 m2 / g, or from 50 m2 / g to 100 m2 / g, or from 60 m2 / g to 90 m2 / g, or from 70 m2 / g to 80 m2 / g. Once the gallium precursor and zirconia particles are sufficiently mixed, the metal oxide catalyst component can be dried at temperatures below 200°C, below 175°C, below 150°C, below 100°C, or approximately 85°C. In applied models, the metal oxide catalyst component can be dried at temperatures between 40 and 200°C. In applied models, the metal oxide catalyst component can be dried at temperatures between 40 and 160°C, between 40 and 120°C, or between 40 and 80°C. In applied models, the metal oxide catalyst component can be dried at temperatures between 80 and 200°C, between 120 and 200°C, or between 160 and 200°C.After drying, the metal oxide catalyst component can be calcined at temperatures ranging from 400 to 800 °C, 425 to 775 °C, 450 to 750 °C, 475 to 725 °C, 500 to 700 °C, 525 to 675 °C, 550 to 650 °C, 575 to 625 °C, approximately 550 °C, or approximately 600 °C. Following calcination, the composition of the metal oxide catalyst component is measured and reported as a percentage by weight of gallium, referring to the oxidic composition of the material. It is important to understand that, according to certain application models, the metal oxide catalyst component can be formed by other methods that ultimately lead to close contact between zirconia and gallium precursors. Some unrestricted cases include vapor phase deposition of gallium-containing precursors (whether organic or inorganic in nature), followed by controlled decomposition. Similarly, liquid gallium metal dispersion processes can be modified by experts in the field to result in close contact between gallium precursors and zirconia. In one or more application models, after the metal oxide catalyst component has been formed—for example, by the methods described above—the metal oxide catalyst component can be mixed with a microporous catalyst component and a binder in order to form a single catalyst. In applied models, the microporous catalyst component can be selected from molecular sieves containing pore openings with an 8-membered ring and a framework type chosen from the following range: chabazite (CHA), aluminophosphate-18 (AEI), silico-aluminophosphate-56 (AFX), erionite (ERI), levynite (LEV), linde type A (LTA), ultrastable faujasite-type (UFI), rho-type zeolite (RTH), edingtonite (EDI), gismondine (GIS), merlinoite (MER), rho-type zeolite (RHO), and combinations thereof. Compliant with the nomenclature system adopted by the International Zeolite Association.It is evident that in certain application models, frameworks of both aluminosilicate and silicoaluminophosphate can be used. Some application models may include tetrahedral aluminosilicates, aluminophosphates ALPOs (e.g., tetrahedral aluminophosphates), silicoaluminophosphates SAPOs (e.g., tetrahedral silicoaluminophosphates), and tectosilicates based solely on silica. In certain application models, the microporous catalyst component of silicoaluminophosphate may have a chabazite-type framework.Examples include, but are not limited to, the following: applied models of chabazite, such as silicoaluminophosphates-34 (SAPO-34) or small-pore silicoaluminophosphate zeolite-13 (SSZ-13); and applied models of aluminophosphate-18 (AEI), such as silicoaluminophosphate-18 (SAPO-18) or small-pore silicoaluminophosphate zeolite-39 (SSZ-39). Combinations of microporous catalyst components incorporating any of the aforementioned framework types can also be used. It is evident that the microporous catalyst component can incorporate a ring-shaped pore opening of varying atomic weights, depending on the desired product. For example, a microporous catalyst component containing pore openings with an 8-membered ring (8-MR) can be used to convert to a 12-membered ring (12-MR) based on the desired product.However, to produce hydrocarbons with 2 to 4 carbon atoms, a microporous catalyst component with holes containing a ring of 8 atoms is used in certain application models. The metal oxide catalyst component and the microporous catalyst component of the molded hybrid catalyst can be mixed together in any suitable manner to achieve homogeneous mixing of all components prior to extrusion. Initially, the metal oxide catalyst component and the microporous catalyst component can be mixed as powders to achieve homogeneity in a suitable dry mixer, such as a plow mixer or ribbon plow. The binder precursor can be added to a mixture containing the metal oxide catalyst component and the microporous catalyst component and mixed in a suitable heavy-duty industrial mixer capable of handling thick paste formulations. Alternatively, the pre-mixed metal oxide catalyst component and the microporous catalyst component can be fed directly into the feeding screws of a screw extruder along with the peptized binder precursor formulation and mixed directly in the screw extruder. The molded hybrid catalyst can then be extruded into the desired shape by any suitable extrusion method. Examples of shapes include spherical, semi-spherical, and cylindrical shapes, etc.In applied models, the metal oxide catalyst component can include a hybrid catalyst formed with a weight percentage ranging from 1.0% to 85.0%, for example, between 5.0% and 85.0%, or between 10.0% and 85.0%, or between 15.0% and 85.0%, or between 20.0% and 85.0%, or between 25.0% and 85.0%, or between 30.0% and 85.0%, or between 35.0% and 85.0%, or between 40.0% and 85.0%, or between 45.0% and 85.0%, or between 50.0% and 85.0%, or between 55.0% and 85.0%, or between 60.0% and 85.0%, or between 65.0% and 85.0%, or between 70.0% 85.0%, or between 75.0% and 85.0%. In applied models, the weight percentage of the hybrid catalyst formed in the metal oxide catalyst component ranges between 1.0% and 85.0%, or between 1.0% and 75.0%, or between 1.0% and 70.0%, or between 1.0% and 65.0%, or between 1.0% and 60.0%, or between 1.0% and 55.0%, or between 1.0% and 50.0%, or between 1.0% and 45.0%, or between 1.0% and 40.0%, or between 1.0% and 35.0%, or between 1.0% and 30.0%, or between 1.0% and 25.0%, or between 1.0% and 20.0%, or between 1.0% and 15.0%, or between 1.0% and 10.0%, or between 1.0% and 5.0%. In applied models, the metal oxide catalyst component includes the hybrid catalyst formed with a weight percentage ranging between 5.0% and 85%.0%, for example, with a weight percentage ranging between 10.0% and 80.0%, or between 15.0% and 80.0%, or between 20.0% and 80.0%, or between 25.0% and 75.0%, or between 30.0% and 70.0%, or between 35.0% and 65.0%, or between 40.0% and 60.0%, or between 45.0% and 55.0%. In applied models, the metal oxide catalyst component includes the hybrid catalyst formed with a weight percentage between 40.0% and 80.0%, for example, with a weight percentage between 50.0% and 75.0%, or between 50.0% and 70.0%, or between 60.0% and 80.0%, or between 60.0% and 75.0%, or between 60.0% and 70.0%. The metal oxide catalyst component can be mixed with the microporous catalyst component in any mass ratio from 1:10 to 10:1. For example, the mass ratio of the oxide catalyst component to the microporous catalyst component may be 1:1, 1:2, 1:3, 1:4, 1:5, 1:6, 1:7, 1:8, 1:9, and 1:10. The mass ratio of the microporous catalyst component to the metal oxide component may be 1:1, 1:2, 1:3, 1:4, 1:5, 1:6, 1:7, 1:8, 1:9, and 1:10. After preparing the metal oxide catalyst component and combining it with the microporous catalyst component, a binder is added to form a paste. The binder may be able to hold the metal oxide catalyst and microporous catalyst components together. The paste can then be extruded to produce a shaped hybrid catalyst. The shaped hybrid catalyst can be formed by any suitable extrusion process. Various binders are suitable. For example, the binder may contain alumina, zirconia, or both. In application models, the binder may contain pure alumina. In other application models, the binder may contain pure zirconia. When the binder contains alumina, it may be hydrous alumina. Hydrous alumina can be prepared from boehemitic precursors with water and a peptizing agent. The binder can be mixed with a metal oxide catalyst and a microporous catalyst. After mixing the binder with the metal oxide catalyst and the microporous catalyst, the mixture can be extruded, dried, and calcined. Following calcination, the bonding material can form aluminum oxide and bind the metal oxide catalyst component and the microporous catalyst component together to provide mechanical strength for extruding the formed hybrid catalyst.Without adhering to any specific theory, other commonly used binders, such as silicon dioxide (SiO2) and titanium dioxide (TiO2), may lead to catalyst poisoning or a significant loss of olefin selectivity. Combining the two catalyst components in a single catalyst body is not straightforward. While the physical mixture of a metal oxide catalyst component and a microporous catalyst component (i.e., not formed in a single catalyst body) may reduce the pressure drop in reactors, catalytic performance, such as hydrocarbon or olefin selectivity and carbon conversion, may be significantly reduced. A binder, including alumina, zirconia, or both, can integrate the metal oxide catalyst component and the microporous catalyst component into a single catalyst body to improve the yield of 2- to 4-carbon olefins and carbon conversion.It should be noted that forming both the metal oxide catalyst and the microporous catalyst and combining them as a physical mixture cannot achieve the conversion rate of carbon compounds containing 2 to 4 carbon atoms that can be achieved using a hybrid catalyst formed as described and illustrated here. In some applied models, the bonding agent is a colloidal solution, suspension, or gel of the bonding precursor. The bonding precursor may include aluminum oxides or hydroxides, zirconium oxides or hydroxides, or mixtures thereof. In one applied model, the bonding precursor may include pure alumina, boehmite, gibbsite (pseudo-bohemite), or mixtures thereof. In other applied models, the bonding precursor may include pure zirconia, hydrous zirconia, or mixtures thereof. In applied models where the bonding agent includes hydrous alumina, for example, pseudo-bohemite or gibbsite, an acid is usually added as a peptization agent. The peptide ratio is defined as the number of moles of acid added during the peptide process divided by the number of moles of aluminum, the ratio of hydrogen ion concentration to aluminum concentration, denoted as [H+] / [Al].In one or more of the applied models, the peptide ratio for the hydrogen ion concentration / aluminum concentration may range from 0.005 to 0.1, or from 0.01 to 0.1, or about 0.05. In applied models, the bonding material may have a surface area ranging from 25 m2 / g to 400 m2 / g, or from 50 m2 / g to 400 m2 / g, or from 75 m2 / g to 400 m2 / g, or from 100 m2 / g to 400 m2 / g, or from 125 m2 / g to 400 m2 / g, or from 150 m2 / g to 400 m2 / g, or from 100 m2 / g to 200 m2 / g, or from 125 m2 / g to 200 m2 / g, or from 150 m2 / g to 200 m2 / g, or from 25 m2 / g to 175 m2 / g, or from 25 m2 / g to 150 m2 / g, or from 25 m2 / g to 125 m2 / g. Or from 25 m2 / g to 100 m2 / g, or from 125 m2 / g to 175 m2 / g, or from 150 m2 / g to 175 m2 / g, or from 100 m2 / g to 150 m2 / g, or from 125 m2 / g to 150 m2 / g, or from 100 m2 / g to 125 m2 / g. Without adhering to any particular theory, it has been shown that the use of typical molecular sieves (e.g., non-calcined) for the formulation has a positive effect on the catalyst's performance and structural properties, especially under highly acidic conditions, such as saturation ratios exceeding 0.05, or more than 0.025, which are used during the preparation of shaped hybrid catalysts. In some applied models, the mixed metal oxide catalyst component and / or binder is largely silica-free. The term "largely silica-free" may refer to the presence of a particular component in the formulation at a weight percentage of less than 0.5 percent (wt%). For example, a metal oxide catalyst component and binder that are essentially silicon- or phosphorus-free may contain less than 0.5 percent (wt%) of silicon or phosphorus based on the combined weight of the metal oxide catalyst component and binder. The hybrid catalyst formed can be used in carbon-containing feed stream conversion methods to hydrocarbons containing 2 to 4 carbon atoms. These processes will be described in more detail below. In certain application models, the reaction zone is fed with a feed stream consisting of hydrogen gas and a carbon-containing gas, selected from carbon monoxide, carbon dioxide, and a mixture thereof. In some application models, the hydrogen gas is present in the feed stream at a volumetric percentage ranging from 10% to 90%, depending on the total amount of hydrogen gas. The selected gas is carbon monoxide, carbon dioxide, and a mixture thereof. The feed stream is then in contact with the hybrid catalyst, as described here, within the reaction zone. The hybrid catalyst comprises a metal oxide catalyst component consisting of zirconia and gallium oxide, a microporous catalyst component, and a binder. It should be understood that the efficiency of the hybrid catalyst will be highest for feed streams containing carbon monoxide (CO), such as carbon-containing gas, and that its efficiency decreases as the proportion of carbon-containing gas in the feed stream increases (which is carbon dioxide). However, this does not preclude the use of the hybrid catalyst described here in methods where the feed stream consists entirely of carbon dioxide or a significant proportion of carbon-containing gas. The feed stream is brought into contact with the hybrid catalyst formed in the reaction zone under sufficient reaction conditions to form a product stream containing hydrocarbons with 2 to 4 carbon atoms. The reaction conditions include a temperature within the reaction zone ranging, according to one or more application models, from 350°C to 480°C, or from 375°C to 450°C, or from 400°C to 450°C, or from 350°C to 425°C, or from 375°C to 425°C, or from 400°C to 425°C, or from 350°C to 400°C, or from 375°C to 400°C. In certain applied models, the pressure within the reaction zone is at least 100 kPa (1 bar), such as at least 500 kPa (5 bar), or at least 1,000 kPa (10 bar), or at least 1,500 kPa (15 bar), or at least 2,000 kPa (20 bar), or at least 2,500 kPa (25 bar), or at least 3,000 kPa (30 bar), or at least 3,500 kPa (35 bar), or at least 4,000 kPa (40 bar), or at least 4,500 kPa (45 bar), or at least 5,000 kPa (50 bar), or at least 5,500 kPa (55 bar), or at least 6,000 kPa (60 bar), or 6,500 kPa At least 65 bar Pascals, or at least 7,000 kPa (70 bar), or at least 7,500 kPa (75 bar), or at least 8,000 kPa (80 bar), or at least 8,500 kPa (85 bar), or at least 9,000 kPa (90 bar), or at least 9,500 kPa (95 bar), or at least 10,000 kPa (100 bar).In other applied models, the reaction conditions include a pressure within the reaction zone ranging from 500 kPa (5 bar) to 10,000 kPa (100 bar), such as from 1,000 kPa (10 bar) to 9,500 kPa (95 bar), or from 1,500 kPa (15 bar) to 9,000 kPa (90 bar), or from 2,000 kPa (20 bar) to 8,500 kPa (85 bar), or from 2,500 kPa (25 bar) to 8,000 kPa (80 bar), or from 3,000 kPa (30 bar) to 7,500 kPa (75 bar), or from 3,500 kPa (35 bar) to 7,000 kPa (70 bar), or from 4,000 kPa (40 bar). To 6,500 kPa (65 bar), or from 4,500 kPa (45 bar) to 6,000 kPa (60 bar), or from 5,000 kPa (50 bar) to 5,500 kPa (55 bar). In some applied models, the pressure within the reaction zone ranges from 2,000 kPa (20 bar) to 6,000 kPa (60 bar). According to certain application models, the gas-hourly space velocity (GHSV) in the reaction zone ranges from 500 to 12,000 hours per hour (hpm), such as 500 to 10,000, 1,200 to 12,000, 1,500 to 10,000, 2,000 to 9,500, 2,500 to 9,000, 3,000 to 8,500, 3,500 to 8,000, 4,000 to 7,500, 4,500 to 7,000, or 5,000 to 8,500. 6,500 / hour, or from 5,500 / hour to 6,000 / hour. In some applied models, the value of the vacuum velocity of the gas per hour in the reaction zone ranges from 1800 / hour to 3600 / hour, for example from 2000 / hour to 3600 / hour, or from 2200 / hour to 3600 / hour, or from 2400 / hour to 3600 / hour, or from 2600 / hour to 3600 / hour, or from 2800 / hour to 3600 / hour, or from 3000 / hour to 3600 / hour, or from 3200 / hour to 3600 / hour, or from 3400 / hour to 3600 / hour.In some applied models, the vacuum velocity of the gas per hour in the reaction zone ranges from 1800 / hr to 3400 / hr, for example, from 1800 / hr to 3200 / hr, or from 1800 / hr to 3000 / hr, or from 1800 / hr to 2800 / hr, or from 1800 / hr to 2600 / hr, or from 1800 / hr to 2400 / hr, or from 1800 / hr to 2200 / hr, or from 1800 / hr to 2000 / hr. In some applied models, the vacuum velocity of the gas per hour in the reaction zone is from 2000 / hr to 3400 / hr, for example from 2200 / hr to 3200 / hr, or from 2400 / hr to 3000 / hr, or from 2600 / hr to 2800 / hr. In other applied models, using the hybrid catalysts described here, along with the process conditions described here, the carbon conversion rate can be improved. Within the process ranges described, the conversion of carbon oxide and hydrogen-containing feedstocks can be carried out in a series of reactors with a water-repellent by-product, for example, by phase separation, membrane separation, or some type of selective water absorption or adsorption process. Furthermore, without being bound by any particular theory, channeling the partially converted, water-free output to the next reactor in the series and repeating these technological processes will generally enhance hydrocarbon production. In some applied models, when using the hybrid catalysts formed here with the process conditions described here, the selectivity ratio of olefins (2 to 4 carbon atoms) to paraffins may be greater than or equal to 2, such as the selectivity ratio of olefins (2 to 4 carbon atoms) to paraffins being greater than or equal to 2, greater than or equal to 3, greater than or equal to 4, greater than or equal to 5, greater than or equal to 10, greater than or equal to 15, or even the selectivity ratio of olefins (2 to 4 carbon atoms) to paraffins being equal to 20. Examples The following examples illustrate the advantages of the present invention but are not intended to limit its scope. For both the following examples and the comparative examples, the microporous catalyst component was prepared as follows: silicoaluminophosphates-34 were synthesized. When using calcined silicoaluminophosphates-34, the material was calcined in air using the following scheme: the temperature was raised from 25°C to 600°C at a heating rate of 5°C / min, then the temperature was held at 600°C for 4 hours, followed by cooling to 25°C for 4 hours. The material was then sieved into particles smaller than 75 micrometers (200 mesh). Measuring the porosity of different zirconia oxide carrier materials using mercury Mercury porosimetry analysis was performed on a Micromeritics Autopore IV 9520 instrument, where the gas was mechanically removed from the samples under very low pressure prior to mercury analysis to remove any physiosorbed species (such as moisture) from the sample surface. The test conditions included a mercury filling pressure of 3.45 kPa (0.50 psi), a mercury contact angle of 130°, a mercury surface tension of 0.485 N / m (485 dyn / cm³), a mercury density of 13.53 g / mL, a 30-minute evacuation time, a small-hole penetrator (solid type: 0.392 cm³ stem size) with a 5 cm³ bulb, a 30-second equilibration time, a 92-point pressure table (75 penetration points and 17 contraction points), and mechanical evacuation of less than 50 µmHg. The transition point between low and high pressure was collected at approximately 317.16 kPa (46 psi). A pressure table was developed to allow for a uniformly increasing pressure distribution on a logarithmic scale ranging from 3.45 kPa to 413.69 MPa (0.5 psi to 60,000 psi), and it is used to detect pore diameters ranging from 0.003 to 400 µm. Mercury is introduced into increasingly smaller pores as the pressure in the vacuum is gradually increased to a maximum of approximately 413.69 MPa (60,000 psi).Table 1 below shows the resulting macroporosity ratio for each zirconia support material, which is calculated by dividing the total pore penetration volume ranging from 80-500 nanometers by the total pore penetration volume ranging from 3-500 nanometers. Table 1 Carrier type: ZrO2; Total penetration volume: 3-500 nm (ml / g); Total penetration volume: 80-500 nm (ml / g) *ɸmacro RC-100 0.703 0.462 0.657 MEL XZO1501 / 25 (ZrO2) 0.570 0.141 0.247 DKKK Z3186 0.217 0.019 0.086 DKKK Z3101 0.354 0.162 0.458 NorPro SZ31164 0.294 0.0406 0.138 The symbol ɸmacro indicates the macroporosity fraction. The RC-100 zirconia oxide bearing described in this invention is available from Daiichi Kigenso Kagaku-Kogyo Co., Ltd. under the trade name RC-100. The MEL XZO1501 / 25 zirconia oxide bearing described in this invention is available from MEL Chemicals Inc. under the trade name or series name XZO1501 / 25. The DKKK Z3186 zirconia bearing described in this invention is available from Daiichi Kigenso Kagaku-Kogyo Co., Ltd. under the trade name Z3186. The DKKK Z3101 zirconia oxide bearing described in this invention is available from Daiichi Kigenso Kagaku-Kogyo Co., Ltd. under the trade name Z3101. The zirconia oxide material of type NorPro SZ31164 described in this invention is a zirconia oxide material bearing the product code SZ31164 and manufactured by Saint-Gobain NorPro. Example 1 A gallium metal oxide catalyst component was prepared on a zirconia support using the incipient wetness impregnation method. An impregnation solution of Ga(NO3)3.xH2O and La(NO3)3.6H2O was prepared at concentrations of 1 mol / L and 0.3 mol / L, respectively, in deionized water. Ten grams of zirconia oxide carrier material with a particle size of less than 75 μm (200 mesh) (NORPRO SZ31164, more than 95% of the material in the monoclinic phase according to X-ray diffraction (XRD), pore size = 0.4 mL / g measured in deionized water) were weighed and placed in a glass vial. Then, 4 ml of gallium and lanthanum infusion solution were added by distillation to the carrier material with continuous shaking.After impregnation, the catalyst was dried overnight in an oven at 85°C and then heated in increments of 3°C / minute until it reached 550°C. This temperature was held for 4 hours. After calcination, the catalyst was re-sifted to a particle size of less than 75 µm (200 mesh) to remove larger agglomerated particles. The hybrid catalyst was prepared by mixing 8 g of the metal oxide catalyst component described above with 1.808 g of uncalcined silicoaluminophosphates-34 (smaller than 75 μm (200 mesh)) for 10 minutes using a mortar and pestle. Separately, pseudoboehmite (aluminum oxyhydroxide, AlOOH) (manufactured by Sasol Limited, trade name Catapal D) was converted to a colloidal state in water using nitric acid (HNO3) (65% by weight in water) at a nitric acid / aluminum concentration ratio (HNO3 / Al) of 0.05, resulting in a total solids content of 35% by weight. Peptized pseudoboehmite was added to the mixed dry powders, targeting a pseudoboehmite concentration of 24.6% by weight of the total solids. The mixture was then stirred for at least 10 minutes using a mortar and pestle until an extrusive paste was obtained.The paste was transferred to a ceramic dish and dried overnight at 85°C. The dried precursor was then heated in a stationary oven at increments of 2°C / minute until it reached 600°C, and this temperature was maintained for 4 hours. After calcination, the hybrid catalyst was crushed and sieved to a size of 400 µm to 177 µm (40–80 mesh) for testing. Example 2 A gallium-based metal oxide catalyst was prepared on a zirconia support using the pre-hydration impregnation method. An impregnation solution of materials with the chemical formulas Ga(NO3)3.xH2O and La(NO3)3.6H2O was prepared at concentrations of 0.72 mol / L and 0.22 mol / L, respectively, in deionized water. Ten grams of zirconia support material (DKKK Z3186, with over 94% of the material in the monoclinic phase according to X-ray diffraction analysis, and a pore volume of 0.55 mL / g measured in deionized water) were weighed and placed in a glass vial. Subsequently, 5.5 mL of a gallium-lanthanum impregnation solution was added to the support material by distillation while continuously shaking. After impregnation, the catalyst was dried overnight in an oven at 85°C and then heated in increments of 3°C / minute until it reached 550°C. This temperature was maintained for 4 hours. After calcination, the catalyst was sieved to less than 75 µm (200 mesh) to remove larger agglomerated particles.The hybrid catalyst was prepared by mixing 8 g of the metal oxide catalyst component described above with 1.808 g of uncalcined silicoaluminophosphates-34 (smaller than 75 μm (200 mesh)) for 10 minutes using a mortar and pestle. Separately, pseudoboehmite (manufactured by Sasol Limited, trade name Catapal D) was colloidalized in water using nitric acid (65% wt. in water) at a nitric acid / aluminum ratio of 0.05, resulting in a total solids content of 35 wt. The peptide-treated pseudoboehmite mixture was then added to the dry powder mixture, targeting a pseudoboehmite content of 24.6 wt. The dough was then mixed for at least 10 minutes using a mortar and pestle until it was extruded. The dough was transferred to a ceramic dish and dried overnight at 85°C.The dry precursors were heated in a stationary oven at increments of 2°C / min until the temperature reached 600°C, and this temperature was then maintained for 4 hours. After calcination, the hybrid catalyst was crushed and sieved to a size of 400 µm to 177 µm (40–80 mesh) for testing. Example 3: A gallium metal oxide catalyst component was prepared on a zirconia support using the pre-hydration impregnation method. An impregnation solution of materials with the chemical formulas Ga(NO3)3.xH2O and La(NO3)3.6H2O was prepared at concentrations of 0.8 mol / L and 0.24 mol / L, respectively, in deionized water. Ten grams of zirconia support material (XZO1501 / 25 MEL Chemicals, 73% monoclinic according to X-ray diffraction analysis, pore volume = 0.5 mL / g measured in deionized water) were weighed and placed in a glass flask. Five mL of the gallium-lanthanum impregnation solution was then added distillateically to the support material while continuously shaking. After impregnation, the catalyst was dried overnight in an oven at 85°C and then heated in increments of 3°C / minute until it reached 550°C. This temperature was maintained for 4 hours. After calcination, the catalyst was sieved to less than 75 µm (200 mesh) to remove larger agglomerated particles.The hybrid catalyst was prepared by mixing 8 g of the metal oxide catalyst component described above with 1.808 g of uncalcined silicoaluminophosphates-34 (smaller than 75 μm (200 mesh)) for 10 minutes using a mortar and pestle. Separately, pseudoboehmite (manufactured by Sasol Limited, trade name Catapal D) was converted to a colloidal state in water using nitric acid (65% wt in water) at a nitric acid / aluminum ratio of 0.05, resulting in a total solids content of 35% wt. The peptide-treated pseudoboehmite mixture was added to the dry powder mixture, targeting a pseudoboehmite content of 24.6% wt based on the total solids. The dough was then mixed for at least 10 minutes using a mortar and pestle until it was extruded. The dough was transferred to a ceramic dish and dried overnight at 85°C.The dry precursors were heated in a stationary oven at increasing intervals of 2°C / minute until the temperature reached 600°C, and this temperature was then maintained for 4 hours. After calcination, the hybrid catalyst was crushed and sieved to a size of 400 µm to 177 µm (40–80 mesh) for testing. Example 4: The metal oxide catalyst component was prepared according to Example 2. A hybrid catalyst was prepared by mixing 4 g of the metal oxide catalyst component described above with 1 g of uncalcined silicoaluminophosphates-34 (less than 75 μm (200 mesh)) for 2 minutes using a mortar and pestle. 15 mL of 20 wt% zirconium acetate solution (from Daiichi Kigenso Kagaku-Kogyo Co., Ltd., under the trade name Zircosol ZA-20) was prepared separately and then partially neutralized by the slow addition of 20 wt% ammonium zirconium carbonate AZC solution (from Daiichi Kigenso Kagaku-Kogyo Co., Ltd., under the trade name Zircosol AC-20) at approximately 50 °C with stirring until a pH of 5-6 was reached (1.8 mL of ammonium zirconium carbonate solution was added in total). A solution of zirconium-containing binder (zirconium Zr) was added to the mixed dry powders, targeting a final concentration of zirconia oxide binder at 20% by weight based on the total weight of the solids.The mixture was then stirred for at least 15 minutes using a mortar and pestle until an extrusive paste was obtained. The paste was transferred to a ceramic dish and dried overnight at 85°C. The dried precursor was heated in a stationary oven at 2°C / minute increments until it reached 600°C, and this temperature was then maintained for 4 hours. After calcination, the hybrid catalyst was crushed and sieved to a size of 400 µm to 177 µm (40–80 mesh) for testing. Comparative Example 1 A gallium-based metal oxide catalyst was prepared on a zirconia support using the pre-hydration impregnation method. An impregnation solution of materials with the chemical formulas Ga(NO3)3.xH2O and La(NO3)3.6H2O was prepared at concentrations of 0.57 mol / L and 0.17 mol / L, respectively, in deionized water. Ten grams of the zirconia oxide carrier (trade name RC-100, more than 94% of the material in the monoclinic phase according to X-ray diffraction analysis, pore size = 0.7 mL / g measured in deionized water) were weighed and placed in a glass vial. Subsequently, 7 mL of the gallium-lanthanum impregnation solution was added by distillation to the carrier material with continuous shaking. After impregnation, the catalyst was dried overnight in an oven at 85°C and then heated in increments of 3°C / minute until it reached 550°C. This temperature was maintained for 4 hours. After calcination, the catalyst was sieved to less than 75 µm (200 mesh) to remove larger agglomerated particles. The hybrid catalyst was prepared by mixing 8 g of the metal oxide catalyst component described above with 1.808 g of uncalcined silicoaluminophosphates-34 (smaller than 75 μm (200 mesh)) for 10 minutes using a mortar and pestle. Separately, pseudoboehmite (manufactured by Sasol Limited, trade name Catapal D) was colloidalized in water using nitric oxide (65% wt in water) at a nitric acid / aluminum ratio of 0.05, resulting in a total solids content of 35% wt. The peptized pseudoboehmite mixture was then added to the dry powder mixture, targeting a pseudoboehmite concentration of 24.6 wt% based on the total solids. The dough was then mixed for at least 10 minutes using a mortar and pestle until an extrusive dough was obtained. The dough was transferred to a ceramic dish and dried overnight at 85°C.The dry precursors were heated in a stationary oven at increasing intervals of 2°C / minute until the temperature reached 600°C, and this temperature was then maintained for 4 hours. After calcination, the hybrid catalyst was crushed and sieved to a size of 400 µm to 177 µm (40–80 mesh) for testing. Comparative Example 2 A gallium-based metal oxide catalyst was prepared on a zirconia support using the pre-hydration impregnation method. An impregnation solution of materials with the chemical formulas Ga(NO3)3.xH2O and La(NO3)3.6H2O was prepared at concentrations of 0.59 mol / L and 0.18 mol / L, respectively, in deionized water. Ten grams of zirconia support material (DKKK Z3101, with a surface area of ​​80 m² / g according to the Brunauer-Emmett-Teller (BET) method and a pore volume of 0.68 mL / g measured in deionized water) were weighed and placed in a glass vial. Subsequently, 6.8 mL of the gallium-lanthanum impregnation solution was added by distillation to the support material while continuously shaking. After impregnation, the catalyst was dried overnight in an oven at 85°C and then heated in increments of 3°C / minute until it reached 550°C. This temperature was maintained for 4 hours. After calcination, the catalyst was sieved to less than 75 µm (200 mesh) to remove larger agglomerated particles. The hybrid catalyst was prepared by mixing 8 g of the metal oxide catalyst component described above with 1.808 g of uncalcined silicoaluminophosphates-34 (smaller than 75 μm (200 mesh size)) for 10 minutes using a mortar and pestle. Separately, pseudoboehmite (manufactured by Sasol Limited, trade name Catapal D) was converted to a colloidal state in water using nitric acid (65% wt in water) at a nitric acid / aluminum ratio of 0.05, with a total solids content of 35% wt. The peptide-treated pseudoboehmite mixture was added to the dry powder mixture, targeting a pseudoboehmite concentration of 24.6 wt% based on the total solids weight. The dough was then mixed for at least 10 minutes using a mortar and pestle until it was extruded. The dough was transferred to a ceramic dish and dried overnight at 85°C.The dry precursors were heated in a stationary oven at increasing intervals of 2°C / minute until the temperature reached 600°C, and this temperature was then maintained for 4 hours. After calcination, the hybrid catalyst was crushed and sieved to a size of 400 µm to 177 µm (40–80 mesh) for testing. Comparative Example 3 The metal oxide catalyst component was prepared according to comparative example 1. A hybrid catalyst was prepared by mixing 4 g of the metal oxide catalyst component described above with 1 g of uncalcined silicoaluminophosphates-34 (less than 75 μm (200 mesh)) for 2 minutes using a mortar and pestle. 15 mL of 20 wt% zirconium acetate solution (from Daiichi Kigenso Kagaku-Kogyo Co., Ltd., under the trade name Zircosol ZA-20) was prepared separately and then partially neutralized by the slow addition of 20 wt% ammonium zirconium carbonate solution (from Daiichi Kigenso Kagaku-Kogyo Co., Ltd., under the trade name Zircosol AC-20) at approximately 50 °C with stirring until a pH of 5-6 was reached (1.8 mL of ammonium zirconium carbonate solution was added in total). A zirconium-containing binder solution was added to the mixed dry powders, targeting a final zirconia oxide binder concentration of 20% by weight based on the total weight of the solids.The mixture was then stirred for at least 15 minutes using a mortar and pestle until an extrusive paste was obtained. The paste was transferred to a ceramic dish and dried overnight at 85°C. The dried precursor was heated in a stationary oven at 2°C / minute increments until it reached 600°C, and this temperature was then maintained for 4 hours. After calcination, the hybrid catalyst was crushed and sieved to a size of 400 µm to 177 µm (40–80 mesh) for testing. Catalyst performance data The hybrid catalysts were tested in a fixed bed reactor system made of stainless-steel (with an internal diameter of 7.7 mm) under the following conditions: 420 °C, where the hydrogen-to-carbon monoxide ratio is denoted as H2 / CO = 3, the pressure is 4000 kPa (40 bar), and the vacuum velocity of mass per hour is 1.54 h-1. Prior to contact with the synthesis gas, the catalyst was heated in a nitrogen-containing environment to the reaction temperature and pressure. The reactor flux composition was obtained by gas chromatography, and the conversion and carbon-based selectivities were calculated using the following equations: XCO (%) = [(ηCO, in – ηCO, out) / ηCO, in] · 100(1) Sj (%) = [αj · ηj, out / (ηCO, in – ηCO, out)] · 100(2) The symbol ΧCO is defined as the percentage conversion of carbon dioxide, while the symbol ηCO,in is defined as the molar inlet flux of carbon dioxide (µmol / s), and the symbol ηCO,out is the molar outlet flux of carbon dioxide (µmol / s). The symbol Sj is defined as the carbon-based selectivity of product j (%), and the symbol αj is the number of carbon atoms of product j, while the symbol ηj,out is the molar outlet flux of product j (µmol / s). Table 2 below shows the results of the stimulation test. The conversion values ​​shown represent average conversion levels over time periods ranging from 50 to 150 hours of time-on-stream TOS. The normal deactivation rate, denoted by the symbol a, is calculated by fitting the logarithmic decay curve to the data spanning 24 to 150 hours according to the following equation: X / X0 = a + k*ln(TOS(h)). Table 2 ɸmacro binding material X(CO) (%) K (% / ln(h)-1) Example 1 0.138 Al2O3 61.0 -0.025 Example 2 0.086 Al2O3 63.2 -0.026 Example 3 0.247 Al2O3 56.6 -0.030 Example 4 0.086 ZrO2 61.0 -0.026 Comparative example 1 0.657 Al2O3 48.9 -0.061 Comparative example 2 0.458 Al2O3 45.2 -0.055 Comparative example 3 0.657 ZrO2 60.4 -0.050 Table 2 follows... Paraffin selectivity C2-C5 (%) Olefin selectivity C2-C4 (%) Olefin to paraffin ratio Example 1 9 51.4 5.7 Example 2 8.9 51.8 5.8 Example 3 8.4 51.7 6.1 Example 4 10 51.2 5.1 Comparative example 1 10,5 47,0 4,5 Comparative example 2 10,9 46 4,2 Comparative example 3 10,1 51,3 5,1 As can be seen in Table 2, bifunctional catalyst formulations based on metal oxide catalysts with a macroporosity fraction (θmacro) less than 0.3 (Examples 1–4) exhibit higher shift and a lower deactivation rate (k) compared to formulations containing metal oxide catalysts with a macroporosity fraction greater than 0.3 (Comparative Examples 1–3). This behavior is generally observed regardless of the zirconia polymorphism (Example 4) or the nature of the bonding material (Comparative Examples 1 and 3). The subject matter of the present invention is described in detail, with reference to specific application models. It should be noted that a detailed description of a component or feature in any application model does not necessarily imply that the component or feature is essential to that particular application model or any other. Furthermore, it should be clear to experts in the field that various modifications and changes can be made to the application models described in this document without deviating from the substance and scope of the application. It is noted that one or more of the safeguards use the term "where" as a transitional phrase. For the purposes of defining the current technique, it is noted that this term is introduced in the safeguards as a general transitional phrase used to state a set of structural properties and should be understood in the same way as the general preamble term "which includes". It should be understood that when the first component is described as "containing" a second component, it is conceivable that, in some applied models, the first component "consists of" or "is essentially composed of" that second component. It should also be understood that when the first component is described as "containing" a second component, it is conceivable that, in some applied models, the first component contains at least 10%, or at least 20%, or at least 30%, or at least 40%, or at least 50%, or at least 60%, or at least 70%, or at least 80%, or at least 90%, or at least 95%, or even at least 99% of that second component (where % can be % by weight or % molar). For the purposes of describing and defining the technology of the present invention, it is important to note that referring to any variable as a "function" of another parameter or variable does not necessarily mean that the variable is an exclusive function of that parameter or variable. Rather, referring to a variable as a "function" of a listed parameter means that it is open-ended, meaning that the variable may be a function of one parameter or several. It is also worth noting that references here to indefinite forms such as "at least one element" and the like do not necessarily mean that the meaning is limited to the existence of only one element or one component. For the purposes of describing and defining the present invention, it should be noted that the terms "largely" and "approximately" are used here to represent an inherent degree of uncertainty that can be attributed to any comparison, value, measurement, or other quantitative representation. The terms "largely" and "approximately" are also used here to represent the degree to which the quantitative representation may differ from a given reference without resulting in a change to the fundamental function of the subject matter.

Claims

1. A process for preparing hydrocarbons containing 2 to 4 carbon atoms that includes: introducing a feed stream containing hydrogen gas and carbon-containing gas selected from the group consisting of carbon monoxide, carbon dioxide, and mixtures thereof into the reaction zone of a reactor; The feed current is converted into a product current containing hydrocarbons with 2 to 4 carbon atoms in the reactor's reaction zone in the presence of a formed hybrid catalyst. The reaction zone has a temperature of 350°C to 480°C and a pressure of 100 kPa to 10,000 kPa. The formed hybrid catalyst is prepared from a metal oxide catalyst component consisting of gallium oxide and zirconia, where the zirconia has a macroporosity fraction of 0.05 to 0.

3. A microporous catalyst component consisting of a molecular sieve with pore openings containing an 8-membered ring (8-MR); and a binder in the form of a colloidal solution, suspension, or gel of binder precursor materials including alumina, zirconia, or mixtures thereof.

2. A process for preparing a formed hybrid catalyst, which includes the following steps: mixing a metal oxide catalyst component and a microporous catalyst component, where: the metal oxide catalyst component includes gallium oxide and zirconia, and zirconia has a macroporosity of 0.05 to 0.

3. The microporous catalyst component includes a molecular sieve with pore openings containing an 8-membered ring (8-MR). A binder is added to the metal oxide catalyst component and the microporous catalyst component to form a paste. The binder is a colloidal solution, suspension, or gel of a binder precursor containing aluminum oxides or aluminum hydroxides, zirconium oxides or zirconium hydroxides, or mixtures thereof. The paste is extruded to produce the resulting hybrid catalyst, and the paste is calcined after extrusion.

3. The process is carried out according to Protection Element 1 or Protection Element 2, where the metal oxide catalyst component also includes nickel, palladium, or platinum.

4. The process is carried out according to protection element 1 or protection element 2, where the particle size of the formed hybrid catalyst is 0.5 mm to 6 mm.

5. The process is carried out according to protection element 1 or protection element 2, where the particle size of the formed hybrid catalyst is 0.5 mm to 3 mm.

6. The process is carried out according to protection element 1 or protection element 2, where the metal oxide catalyst component contains gallium at a weight percentage of 0.1% to 10% by weight.

7. The process is performed according to Protection Element 1 or Protection Element 2, where the microporous catalyst component contains silicoaluminophosphates-34 (SAPO-34).

8. The process is performed according to Protection Element 1 or Protection Element 2, where the microporous catalyst component contains unsintered silicoaluminophosphates-34 (SAPO-34).

9. The process is performed according to Protection Element 1 or Protection Element 2, where the binder contains alumina.

10. The process is performed according to Protection Element 1 or Protection Element 2, where the binder contains zirconia.

11. The process is conducted according to protection element 1 or protection element 2, where the metal oxide catalyst component includes a formed hybrid catalyst with a weight percentage of 40.0% to 85.0%.

12. The process is conducted according to protection element 1, where hydrocarbons containing 2 to 4 carbon atoms consist mainly of olefins containing 2 to 4 carbon atoms.