Solar control glass with optical absorber
A multilayer coating system with optimized silicon nitride, metal nitride, and scratch-resistant layers addresses the challenges of optical absorption, mechanical durability, and thermal stability in solar control glass, achieving enhanced performance under stress conditions.
Patent Information
- Application Number
- SA1120253011
- Authority / Receiving Office
- SA · SA
- Patent Type
- Applications
- Current Assignee / Owner
- Filing Date
- 2025-05-02
- Publication Date
- 2026-10-05
AI Technical Summary
Existing solar control coatings for glass substrates face challenges in achieving optimal optical absorption, mechanical durability, and thermal stability, particularly under conditions of heat treatment and shear stress, while maintaining effective infrared reflection and scratch resistance.
A multilayer coating structure comprising a silicon nitride adhesion layer, infrared reflective layers, absorption layers made of metal nitrides, and a scratch-resistant outer layer, with specific thicknesses and compositions optimized for enhanced performance, is applied using RF reactive spraying.
The multilayer coating system provides improved optical absorption, mechanical durability, and thermal stability, ensuring effective infrared reflection and scratch resistance, even under stress conditions, thereby enhancing the performance of solar control glass.
Smart Images

Figure 033240D4-6E3B-44EB-8C34-3CEEC102F71F 
Figure 14656CF5-4967-4658-A605-3516AA9AD812 
Figure 1629E18D-4A0E-443B-93E7-09DC21BCFFEF
Abstract
Description
Figure 1 illustrates a typical stacking scheme for S-type solar control layers mounted on a glass substrate. The stacking involves a base layer I originating from the substrate surface, consisting of two base layers 1, 1' of the respective materials, as shown in the diagram. In this case, the silicon nitride or tin oxide base layer 1 forms the adhesion layer towards the substrate. The base layer I is followed by an infrared reflective coating II, consisting of an infrared reflective layer of silver 2. A spacer coating III, consisting of two spacer layers 3, 3', is provided between the infrared reflective coating II and the infrared reflective coating II', both of which have the same four-layer infrared reflective design (2' / 2' / 2'' / 2'''). Following the II' coating is the absorption coating IV, which consists of a metal nitride layer 4 sandwiched between two silicon nitride or silicon oxynitrid 4', 4' layers of the same composition.The scratch-resistant outer coating V is a two-layer coating consisting of a 5' layer of transition metal carbon oxide and a 5' layer of amorphous hydrogenated diamond-like carbon, which forms the end layer of the atmospheric-facing assemblage. The material of the layer can be one of the materials listed with the layer in question. When ":aluminum" follows the comma, aluminum can be added to any of the previously mentioned materials. "Me" in absorption layer 5 can be molybdenum (Mo), tantalum (Ta), or tungsten (W). The transition metals "TM" in layer 5 can be titanium and zirconium, respectively. Other examples of different combinations of coatings and layers involved are given in Table 1, examples 1 to 14. It should be emphasized that, with reference to examples 1, 8, 9, and 11 to 14, the substrate-adhering base layer 1 consists of an inner 4' silicon nitride layer of the adsorption coating. This means that in this case, a single substrate layer 1 is incorporated, consisting of an inner 4' silicon nitride layer that is simultaneously the substrate-adsorbing base layer 1 and is in direct contact with the substrate surface. Therefore, a separate substrate layer is not required with these types of coatings. Examples 1–8 show assemblies consisting of a single infrared-reflective layer, while examples 9–14 show assemblies consisting of two infrared-reflective layers. Absorbent coatings can be expected above (see examples 2–7 and 10), below (see example 1 and 9), or on either side of the infrared stack (see examples 8 and 11–14). Separation between two successive infrared assemblies is provided by a one- or two-layer separation coating that can be applied between any two successive infrared assemblies. Additional separation layers can be provided between the infrared coating and the scratch-resistant coating (examples 1 and 9), and between the absorbent coating and the infrared-reflective coating, as shown in example 14. Figures 2-7 illustrate specific experiments conducted using three selected absorbers (MoNx, TaNx, and WNx), which, when deposited asymmetrically, exhibited superior performance in their optical and process-related material properties (see Table 2b). Details regarding the relevant deposition parameters can be found in Table 2a. Table 4 describes the process parameters for the complete stacking of solar control glass as applied to an industrial coating with a target size of approximately 380 cm². The absorber stacking production process parameters are in the lines “Silicon Nitride or Silicon Nitride:Aluminum” and “MeNxOy”. For chemical and optical characterization, each photoabsorbing film of interest was placed in a stack between two silicon:aluminum nitride layers, where the surrounding layers have a strong influence on the properties of thin films with a thickness < 20 nm. All stacks (material and layer thicknesses, as well as process parameters) used in the chemical and optical characterization are listed in Table 2a. The "Column Number" contains four sets of samples, 1 to 4, indicating the molybdenum absorber (1), tungsten absorber (2), tantalum absorber (3), and glass substrate (4), followed by the corresponding sample number. The chemical composition was measured by X-ray photoelectron spectroscopy, the optical properties were measured by elliptic measurement and spectroscopy, and the terrace thickness was measured by surface profile measurement. The depth of leaching was measured by X-ray photoelectron spectroscopy through repeated cycles: ion leaching and subsequent X-ray photoelectron spectroscopy measurement. X-ray photoelectron spectroscopy (XPS) measurements were performed using the following parameters: monochromatic X-ray beam (Al Kα edge), spot size 100 μm, and throughput energy 26 eV (FWHM energy resolution = 0.6 eV (Ag 3d⁵ / 2), in scan mode). Leaching was performed using Zallar rotation to ensure optimal depth resolution, with Ar⁺ ions, 1 kV 2 × 2, and a leaching time of approximately 1 minute per rotation. The atomic concentrations (% atomic) of the elements were measured across the entire stack (Si₃N₄:Al / MeNxOy / Si₃N₄:Al), and the chemical composition of MeNxOy in the middle of the membrane was determined. The chemical composition of the membrane is defined as: x = N (% atomic) / Me (% atomic), y = O (% atomic) / Me (% atomic), and MeNxOy. To model the optical constants n(λ) and k(λ), elliptic measurements (Ψ(λ) and Δ(λ) for angles of 55°–75° in 5° steps were combined with optical spectroscopy (UV, visible, and near-infrared spectroscopy). The film thickness was determined by surface profile measurement for each stacked layer, which was deposited separately as a single layer on a test glass for measurement and then stabilized during subsequent modeling (CompleteEase software). B-Spline and Gen-Osc models were used to model the absorber. Figures 2a, 2b, and 2c show the wavelength dependence of the extinction coefficient k compared to MoNx, WNx, and TaNx, respectively. Each figure shows the specific MeNx curves as reactively sprayed with different amounts of nitrogen, which indicate the different MeNx ratios, respectively, as discussed below. The sample numbers (#xy) refer to Table 2a. The extinction coefficient is a good measure of the light absorption potential of a layer or layer system. A neutral photonic profile can be efficiently achieved when the photoabsorption coefficient k does not exhibit a strong change in k in the visible wavelength range λ. This was the case with low nitrogen fluxes from 5 to 75 standard cm³ / kW, and especially from 8 to 20 standard cm³ / kW. These quantities indicate quasi-stoichiometric MeNx species with x values of 0.2 to 0.7. Thus, the k curve is homogeneous, nearly linear, and the change in k is small. The highest extinction coefficient can also be achieved in the same flux range, where the best results for MoN x can be reached, in the range of 10±5 standard cubic centimeters / kW.It is important to note that the optimal reactive gas flow rate per kilowatt of power (standard cubic centimeters / kW) depends significantly on the coating size and geometry, pumping efficiency, spray target length, and the power applied to the spray target. Therefore, the definitive characterization of the absorbent layer is ultimately determined by the chemical quantification of the MeNx of the dispersed layer, as determined, for example, with X-ray photoelectron spectroscopy. Figure 3 shows the extinction coefficient at 550 nm for the MoNx, WNx, and TaNx absorbers, respectively, versus nitrogen flux per kilowatt of power. With all three target materials (molybdenum, tungsten, and tantalum), the leaching rate began to decrease significantly with increasing nitrogen flux, at most from 50 standard cm³ / kW and above. Figures 4-5 show the leaching rate and resistance for MoNx samples 1.7–1.12, WNx samples 2.6–2.10, and TaNx samples 3.3–3.7, depending on the amount of N₂ (for the corresponding nitrogen flux values in standard cm³ / kW, see Table 2a, column 4). The specific electrical resistivity is also a good indicator of absorption properties and thus allows for the design and / or control of the reactive spraying process, as illustrated in Figure 5. This means that the lower the electrical resistivity, the higher the extinction coefficient k (see Figure 3). For process efficiency, lower resistivity values are also preferred, as can be seen in the range between 10 and 75 cm³ / kW for MoN and 10–50 cm³ / kW for WN. It can be observed that the absolute values of K for tungsten, and especially for molybdenum, as illustrated in Figure 3, can be set to much higher values than those corresponding to well-known and documented materials such as TiNx (k (550 nm), which is 2.1 according to J. Pflüger and J. Fink. Determination of optical constants using high-energy electron-energy-loss spectroscopy (EELS), in Handbook of Optical Constants of Solids II, Edward D. Palik, ed. Academic Press, 1991, pp. 293-310; 2) J. Pflüger, J. Fink, W. Weber, K.P. Bohnen, G. Crecelius. Dielectric properties of TiCx, TiNx, VCx, and VNx from 1.5 to 40 eV determined by electron-energy-loss spectroscopy, Phys. Rev. B 30, 1155-1163 (1984)). Tantalum semi-stoichiometric nitrides perform similarly to TiNx. Furthermore, a surprisingly suitable N band was found for achieving the highest possible optical absorption in the visible range. Remarkably, layers with very low nitrogen content (MeNx, x ≤ 0.7, e.g., 0.04 ≤ 0.1) exhibit, in most cases, higher optical absorption than that observed with pure metal layers in the case of WNx and MoNx (see Figure 2b, No. 2.12, 2d, No. 1.8, 2e, No. 2.8). Nitride layers with low nitrogen content consistently possess higher optical absorption than those with high nitrogen content (MeNx, x > 0.7) or equivalent metal nitride layers (see Figure 2a-2e). The improved optical absorption characteristics (vs. metal) are evident due to the low nitrogen content in individual layers (Mo, tungsten) and in a stack in the case of tungsten. Note, in an extreme case, where the deposited absorption layer is metallic < 5 nm, the subsequent gas-containing process of silicon nitride deposition introduces a low amount of nitrogen to the metallic layer, resulting in a higher photoresistance coefficient k (see as an example Conformity No. 2.11 in Table 2a with dWNx = 4).(0 nm and x = 0.08, corresponding curve in Figure 2b). This can be seen by comparing it to stacking with a thicker metal film (e.g., d > 5 nm, see as stacking example No. 2.3 in Table 2a with dWNx = 8.0 nm and x = 0.003, corresponding curve in Figure 2b), or compared to a pure metal layer without the silicon nitride process (see as stacking example No. 2.6 in Table 2a, with dWNx = 55.3 nm and x = 0, as shown in Figure 2e). The most stable absorption layer with respect to chemical and mechanical properties can be achieved when the insulating layer is silicon nitride (optionally with added aluminum) and is in direct contact with the absorption layer on both sides. The minimum thickness of the stacking layers of silicon nitride to protect the absorbent layer during cooling processes is d > 8 nm, for example 8-30 nm, and especially 10-20 nm. Since the coefficient of thermal expansion of silicon-containing stack layers is expected to be approximately identical to that of molybdenum, tungsten, and tantalum layers, where it is < 7.5 μm / (m*K), with silicon: 2.6 μm / (m*K), molybdenum: 4.8 μm / (m*K), tungsten: 4.5 μm / (m*K), tantalum: 6.6 μm / (m*K), and the shear modulus is similar > 60 GPa, with molybdenum: 120 GPa, silicon: 161 GPa, and talc: 69 GPa, although the exact values depend on the chemical composition (quantification of metal nitride) and electronic structure [Ozsdolay, B., “WNx and MoNx Layers: Elastic Properties and Crystal Structure”, PhDT, 2016; Kindlund, H., Sangiovanni, D., Petrov, I., Greene, J.E., Hultman, L., (2019), “A review of the intrinsic ductility and toughness of hard transition-metal nitride alloy thin films”, Thin Solid Films, 688, 137479; W. Chen, J.Z[Jiang, “Elastic properties and electronic structures of 4d- and 5d-transition metal mononitrides”, Journal of Alloys and Compounds, Volume 499, Issue 2, 2010, Pages 243-254; C. Kral et al., “Critical review on the elastic properties of transition metal carbides, nitrides and carbonitrides”, Journal of Alloys and Compounds 265 (1998) 215-233] These fully mechanically stacked adsorption coatings are suitable for stacking solar control layers on glass substrates that have undergone heat treatment or shear stress during washing of the coated glass sheet. These adsorption coatings can preferably be applied below and / or above the infrared reflective stack, i.e., between the substrate and the lower or inner infrared reflective stack, and / or between the upper or outer infrared reflective stack and the terminal (outer) surface of the solar control layer stack towards the atmosphere.When the final surface of the layer assembly is formed by an optional scratch-resistant coating, the individual layer or the inner layer of the scratch-resistant coating can be in direct contact with the outer silicon nitride layer of the adsorption coating. Figure 6 shows the X-ray photoelectron spectroscopy (XPS) spray depth of the three-layer adsorption coating as applied to sample 1.13. The interrelational distribution of molybdenum, nitrogen, and silicon within the three layers, and oxygen, silicon, and sodium within the glass substrate, can be observed depending on the spray time. This time indicates the spray etching time of the etching device used on the sample surface prior to XPS analysis. The analysis starts at 0 minutes on the sample surface and ends 25 minutes after the Ar+ ions are sprayed onto the sample, as described above, at a depth of nanometers within the glass substrate. The molybdenum peak of the MoNx layer, i.e., the light-absorbing film with x = 0.31, is located between two silicon nitride layers, correspondingly exhibiting a higher nitrogen concentration. Figures 7a and 7b show the X-ray photoelectron spectra of MoNx sample 1.13 at the maximum Mo intensity signal (see Figure 6) and its fitting curve for measuring atomic concentrations. Figure 7a shows the Mo3d nucleus-level spectrum and fitting curve in the bonding energy region between approximately 223 and 232 eV, while Figure 7b shows the Mo3p 3 / 2 nucleus-level spectrum and fitting curve for N1s in the region between approximately 385 and 399 eV. Both figures demonstrate a very good correlation between the fitting curve (solid line), which represents the sum of the bonding contributions (different dashed lines for Mo, Mo-N, and Mo-O), and the measured curve (filled circles). Bookmarks list S stacking layers I base coat 1.1' layers of primer 1 base coat (can be combined with an absorption coating) II Infrared reflective coating 2,2,2,2 layers of infrared reflective paint 2 layers containing silver III. Separation Paint 3.3' layers of separation paint IV Absorbent Coating 4.4' layers of absorbent coating V Scratch-resistant coating 5.5 layers of scratch-resistant coating 5 layers containing a transition metal 5' Diamond-like carbon layer containing hydrogen (optional) Table 1 shows typical solar layer stacking according to the invention. Type 14 DLC scratch resistant 13 TiZrCx 12 DLC Si3N4 Extra Absorbent 11 DLC TiZrCx MoNx TiZrO2 TiZrCx Si3N4 Si3N4 9 10 Si3N4 Si3N4 MoNx ZnO Infrared Reflective TiZrO2 TiZrO2 MoNx MoNx Si3N4 NiCr Si3N4 Si3N4 Si3N4 Si3N4 ZnO Ag 6 7 8 ZnO MoNx ZnO ZnO NiCr ZnO 5 TiZrO2 TiZrO2 TiZrO2 NiCr Si3N4 NiCr NiCr Ag ZnSnO Separate 1 2 3 4 TiZrO2 Si3N4 Si3N4 Si3N4 Ag ZnO Ag Ag ZnO Si3N4 TiZrO2 TiZrO2 TiZrO2 TiZrO2 Si3N4 MoNx MoNx MoNx ZnO NiCr ZnO ZnO ZnSnO ZnO Infrared Reflective Si3N4 Si3N4 Si3N4 Si3N4 MoNx Si3N4 Si3N4 Si3N4 ZnSnO Ag ZnSnO ZnSnO Si3N4 NiCr ZnO MoNx MoNx MoNx Si3N4 ZnO ZnO ZnO ZnO ZnO ZnO ZnO ZnO Ag NiCr Si3N4 Si3N4 Si3N4 ZnO NiCr NiCr NiCr NiCr ZnSnO NiCr NiCr NiCr ZnO Ag ZnO ZnO ZnO NiCr Ag Ag Ag Ag ZnO Ag Ag Ag TiO2 Separate More ZnO NiCr NiCr NiCr Ag ZnO ZnO ZnO ZnO NiCr ZnO ZnO ZnO ZnSnO Si3N4 Ag Ag Ag ZnO TiO2 TiO2 Si3N4 Si3N4 Ag Si3N4 Si3N4 Si3N4 absorption MoNx ZnO ZnO ZnO TiO2 SnZnO SnZnO MoNx MoNx ZnO MoNx MoNx MoNx MoNx Si3N4 Si3N4 TiO2 SnO2 SnO2 SnO2 Si3N4 Si3N4 Si3N4 Si3N4 Si3N4 Si3N4 Si3N4 Pillar pillar pillar pillar pillar pillar pillar pillar pillar pillar pillar pillar pillar Scratch resistant Extra absorption Infrared reflector separate Infrared reflector More separate absorption Table 2a shows the characteristics and parameters of the absorption layer stacking production. The stacking was produced by the RF reactive spraying process, working with a metal target and Ar process gas and N2 reactive gas, where the distance of the spraying target is: 748.5 mm × 87.5 mm (approximately 660 cm2). Stacking material number* Thickness [nanometers] N2 [standard cubic centimeter / kW] [kW] Glass, [mm] MeNx x = 1.1 Si3N4 / MoNx / Si3N4 9.8 / 0.9 / 13.8 71 0.7 5.8 nm 1.2 Si3N4 / MoNx / Si3N4 9.8 / 4.6 / 13.8 71 0.7 5.8 0.53 1.3 Si3N4 / MoNx / Si3N4 9.8 / 7 / 13.8 0 1 5.8 0 1.4 Si3N4 / MoNx / Si3N4 9.8 / 7 / 13.8 10 1 5.8 nm 1.5 Si3N4 / MoNx / Si3N4 9.8 / 7 / 13.8 50 1 5.8 0.5 1.6 Si3N4 / MoNx / Si3N4 9.8 / 7 / 13.8 200 1 5.8 nm 1.7 Mo 75.5 0 1 3.8 0 1.8 MoNx 62.9 10 1 3.8 0.25 1.9 MoNx 90.0 20 1 3.8 nm 1.10 MoNx 84.9 50 1 3.8 0.47 1.11 MoNx 65.5 100 1 3.8 0.69 1.12 MoNx 44.8 200 1 3.8 0.75 1.13 Si3N4 / MoNx / Si3N4 12 / 5.5 / 13.8 29 0.7 5.8 0.31 2.1 Si3N4 / WNx / Si3N4 14 / 1.2 / 11 50 1 5.8 nm 2.2 Si3N4 / WNx / Si3N4 12 / 5.2 / 12 50 1 5.8 nm 2.3 Si3N4 / WNx / Si3N4 12 / 8.0 / 12 0 1 5.8 0.003 2.4 Si3N4 / WNx / Si3N4 12 / 8.0 / 12 50 1 5.8 0.2 2.5 Si3N4 / WNx / Si3N4 12 / 8.0 / 12 200 1 5.8 0.33 2.6 Si3N4 / W 55.3 0 1 3.8 0 2.7 WNx 65.9 10 1 3.8 nm 2.8 WNx 66.7 20 1 3.8 0.14 2.9 WNx 86.2 50 1 3.8 nm All silicon nitride layers were sprayed at 33.3 standard cm³ / kW. The silicon target was doped with aluminum (8–10% by weight). nm not measured Table 2a Continued Stacking material number* Thickness [nanometers] N2 [standard cubic centimeter / kW] [kW] Glass, [mm] MeNx x = 2.10 WNx 77.7 200 1 3.8 nm 2.11 Si3N4 / WNx / Si3N4 12 / 4.0 / 12 0 1 5.8 0.08 2.12 Si3N4 / WNx / Si3N4 12 / 8.0 / 12 10 1 5.8 0.09 3.1 Si3N4 / TaNx / Si3N4 11 / 2.4 / 11 50 1 5.8 nm 3.2 Si3N4 / TaNx / Si3N4 11 / 10.0 / 11 50 1 5.8 nm 3.3 Si3N4 / TaNx / Si3N4 6.7 / 17.6 / 8.2 20 1 5.8 0.57 3.4 Si3N4 / TaNx / Si3N4 6.7 / 16.1 / 8.2 50 1 5.8 0.76 3.5 Si3N4 / TaNx / Si3N4 6.7 / 15.1 / 8.2 100 1 5.8 nm 3.6 Si3N4 / TaNx / Si3N4 6.7 / 8.1 / 8.2 200 1 5.8 0.88 3.7 Ta 22 0 1 5.8 0 4 float glass - 5.8 nm All silicon nitride layers were sprayed at 33.3 standard cm³ / kW. The silicon target was doped with aluminum (8–10% by weight). nm not measured Table 2b shows the stacking properties of the absorption layers as used in conjunction with Table 1. Stacking number, thickness, nm BRA RA TA RGS 55° Absorption, % ΔT, % ΔET ΔEBR ε YL* a* b* YL* a* b* YL* a* b* YL* a* b* ± 0.005 1.1 Si3N4 / MoNx / Si3N4 9.8 / 0.9 / 13.8 12.3 41.7 -1.3 -5.4 15.1 45.8 -0.9 -4.6 73.9 88.9 -0.7 2.2 18.0 49.5 -1.0 -2.8 11.0 0.4 0.3 1.4 0.801 2.1 Si3N4 / WNx / Si3N4 14 / 1.2 / 11 11.3 40.1 -1.3 -5.0 15.5 46.3 -0.9 -4.7 71.0 87.5 -0.7 2.2 17.0 48.2 -0.9 -2.5 13.5 0.8 0.5 1.7 0.826 3.1 Si3N4 / TaNx / Si3N4 11 / 2.4 / 11 12.5 41.9 -1.8 -5.2 16.5 47.6 -1.0 -5.7 72.5 88.2 -0.9 3.8 17.8 49.2 -1.3 -2.3 11.0 1.2 0.6 1.0 0.825 1.2 Si3N4 / MoNx / Si3N4 9.8 / 4.6 / 13.8 11.4 40.3 -1.3 -3.6 21.4 53.4 -0.5 -0.1 43.8 72.1 -0.4 0.9 16.5 47.7 -0.9 -1.8 34.8 1.1 0.8 0.8 0.768 2.2 Si3N4 / WNx / Si3N4 12 / 5.2 / 12 12.3 41.6 -1.4 -3.5 24.5 56.6 -0.5 -1.4 39.5 69.1 -0.4 1.7 17.5 48.8 -1.1 -1.8 36.0 0.5 0.4 0.8 0.739 3.2 Si3N4 / TaNx / Si3N4 11 / 10.0 / 11 13.7 43.7 -1.3 -5.9 27.2 59.1 -0.3 -2.8 41.7 70.7 -0.9 2.5 17.9 49.4 -1.0 -3.4 31.1 -0.2 1.6 1.8 0.801 4 float glass 0.836 Table 3 Stacking of solar control layers made of scratch-resistant glass (typical stacking according to Example 7 and related variations): The coating material, layer dnanometer composition Scratch-resistant diamond-like carbon containing hydrogen 1-100, e.g., 5-20, 8-12. Diamond-like carbon containing hydrogen (without a metal), e.g., ta-C:H TiZrCx, TiZrOxCy 1-20, for example 2-6 TM:C 1:1-1:6, for example 1:3 (or 25-85% atomic weight of C) Transition metal, for example TiZrx, x = 0-1, for example 0.1-0.5 The absorption of silicon nitride or aluminum-doped silicon nitride is 1–100, for example, 3–60, 5–30. Si3N4 or Si3N4:Al,N can be semi-stoichiometric down to -15%, for example, SiNxAly, x = 1–1.4, y = 0–0.35, for example, SiN1.33Al0.18 Absorption layer: MeVNxOy (Me:Mo,Ta,W) 0.1–50, e.g. 0.4–10 O,N semi-stovalent. (5–60% atomic), e.g. MoN0.1–1, MoN0.1–0.6, WN0.1–1, WN0.1–0.6, TaN0.1–1, TaN0.1–0.6. Oxygen may be present up to 20% at a 0.5% level, and preferably <10% at a 0.5% level. Silicon nitride or aluminum-doped silicon nitride (Si3N4 or Si3N4:Al,N) can be stoichiometric or semistoichiometric down to -15% atomic weight. The aluminum content varies; for example, SiNxAlly, x = 1–1.4, y = 0–0.35, SiN1.33, Al0.18 Separating ZnO, SnO2, SnZnO or ZnO:Al, SnO2:Al, SnZnO:Al, SiNxAlly plating: <150, e.g., <100. Single layer: 0.5–100, e.g., 4–30, 4–20. O can be stoichiometric or substoichiometric (up to -15% atomic weight), Al 0–20% atomic weight, e.g., ZnAlxOy, x = 0–0.3, e.g., 0–0.1, y = 0.8–1.2, e.g., ZnO 0.8–1, Al 0.04–0.06. SnZnxOy, x = 1–4, e.g., x = 1–2.5, y = 2–4, e.g., y = 2.5–3.5, SnZn2O3 Infrared reflective alloys such as ZnO, SnO2, SnZnO, or ZnO:Al, SnO2:Al, SnZnO:Al, SiNxAlly, 0.5–100, e.g., 4–30, 4–20. O can be stoichiometric or substoichiometric (up to -15% atomic mass), Al 0–20% atomic mass e.g., ZnAlxOy, x = 0–0.3, e.g., 0–0.1, y = 0.8–1.2, e.g., ZnO 0.8–1, Al 0.04–0.06, SnZnxOy, x = 1–4, e.g., x = 1–2.5, y = 2–4, e.g., y = 2.5–3.5, SnZn2O3 NiCrx (mandatory normalization) or TiOsub (non-normalization). 0.3–20, e.g. 0.5–10, metallic or oxidized. A NiCrx-containing layer can be stoichiometric or semistoichiometric, with a metallic ratio e.g. 0.1 ≤ xCr ≤ 0.5 (see description). Ag 1-30, for example, 5-20 metal ZnO, SnZnO or ZnO:Al, SnZnO:Al 0.5 - 30, e.g. 3 - 15 O can be stoichiometric or substoichiometric (up to -15% atomic), Al 0-20% atomic, e.g. ZnAlxOy, x = 0 - 0.3, preferably 0 - 0.1, y = 0.8 - 1.2; e.g. ZnO0.8-1Al0.04-0.06 SnZnxOy, x = 1 - 4, preferably 1 - 2.5, y = 2 - 4, preferably 2.5 - 3.5, e.g. SnZn2O3. Scratch resistant absorption season Infrared reflector Table 3 Continued The base is an electrical insulator, for example: TiO2, TiZrO2, ZrO2, NbOx 1-60, for example 1-15, 3-7 TiO2, or TiZrxO2, x = 0-1, for example 0.2-0.5 SnO2, SnZnO, ZnO or SnZnO:Al, ZnO:Al 1-100, for example 5-30, 5-15 O can be stoichiometric or substoichiometric (up to -15% atomic) Silicon nitride, titanium oxide, silicon metal nitrides, oxides, oxinitides (Me: aluminum, niobium, titanium, zirconium) 1-60, for example 1-40, 5-30. Silicon nitride or Si3N4:Al,SiNxAly, x = 1-1.4, y = 0-0.35, for example SiN1.33 Al0.18,SiNxOyMez (Me: Nb, Ti, Zr), x = 0-1.4, y = 0-2, z = 0-2. 1-20mm glass substrate for any type of window glass (architectural, automotive), or composite glass panels The base Table 4) Process parameters for different coating materials in industrial coatings: Material of the working layer; process parameters for each single cathode Diamond-like carbon containing hydrogen, Plasma-Enhanced Chemical Vapor Deposition (PECVD) (Inductively coupled plasma (ICP) - Plasma+ source), Inert gas (Ar) and C2H2, rC2H2 = 10-50%, e.g. 15-45%, Pressure: 1x10-4 - 2x10-2 mbar; ICP generator 13.56 MHz, Ionic current 0.01 to 3.5 mA / cm2, Plasma density 109-1012 cm-3, Ionic energy 10 to 70 eV (For further details, see IAN 2020 / 164735 Diamond-like Carbon, pp. 9-10 and Table 4) TiZrCx, TiZrOxCy reactor, RF pulses, DC, DC, or AC-magnetic frequency (combined). Inert gas (Ar) and CH4, rCH4 = 5-50%, pressure: 1 x 10⁻⁴ - 9 x 10⁻³ mbar, 1-200 kW / cathode, 30-120 kW (for further details, see IAN 2020 / 164735, pp. 7-9) Si3N4 or Si3N4:Al reactor, RF pulses, DC, DC or AC-magnetic frequency (combined). +++ N2 and inert gas (Ar) optional, pressure: 1 × 10⁻⁴ - 9 × 10⁻³ mbar, Si3N4 + Al target, or Si3N4:Al target, 1-200 kW / cathode++, 30-120 kW; MeNxOy RF, Pulsed DC, DC, or AC-MF. Inert gas (Ar) + O2, metal (or oxidized) target Me, pressure: 1 × 10⁻⁴ - 9 × 10⁻³ mbar, 1-200 kW / cathode++, e.g. 3-100 kW, e.g. 3-60 kW; NiCr, TiOsub RF pulses or DC reactive or non-reactive or DC or AC-MF (combined). +++ Inert gas (Ar) + O2, nickelchromium or titanium metal target, pressure: 1 × 10⁻⁴ - 9 × 10⁻³ mbar, 1-200 kW / cathode++; nickelchromium 3-45 kW, e.g. 3-24 kW; Ag radio frequency, pulsed DC, DC, or AC-MF. Inert gas (Ar) only, pressure: 1 × 10⁻⁴ - 9 × 10⁻³ mbar, Ag target 1-150 kW / cathode ++ DC, e.g. 3-30 kW. ZnO, SnO2, SnZnO doped with Al: optional reactor RF pulses or DC or DC or AC-magnetic frequency (combined). +++ Oxygen and inert gas (Ar) optional, pressure: 1 × 10⁻⁴ - 9 × 10⁻³ mbar, ZnO-, SnO2 - SnZn- target 1 - 200 kW / cathode++, 20 - 120 kW, 15 - 120 kW; Me or Si oxides, oxynitrides, or nitrides reactor radio frequency pulses, DC or AC-magnetic frequency (combined). +++ Oxygen and / or nitrogen and inert gas (Ar) optional, pressure: 1 × 10⁻⁴ - 9 × 10⁻³ mbar, metal or target in order silicon nitride, 1 - 200 kW / cathode ++; Cleaning glass with an aqueous solution, rinsing with deionized water Inductively coupled plasma (ICP) sources with a single-cycle excitation electrode and coupling windows of 3360 cm² were used for all experiments in an industrial linear coating system. Physical vapor deposition (PVD) and plasma-enhanced chemical vapor deposition (PVC) treatment stations were integrated into the process sequence to treat a glass substrate with a width of up to 3.21 m and a variable length of up to 9 m. Three linearly mounted ICP sources were used across the substrate width at distances of 100–300 mm from the window to the substrate surface. The ICP energies were 1–17 kW per source, translating to 0.3–5 W / cm² per coupling window area. Planar cathode electrodes with target dimensions l × b = 375 cm × 24 cm, and / or 380 cm long rotating cathode targets were used for all experiments. The cathode electrodes were fixed across the substrate width at a distance of 100–116 mm from the target to the substrate surface, depending on the substrate thickness, and were used for each PVA coating station. +++ Spray (combined): means spraying or joint spraying.
Claims
1. Glass substrate and solar control layer stacking on at least one face of the glass substrate, where the solar control layer stacking includes: - At least one infrared-reflective coating (II) including a layer containing silver (2'); - At least one absorption coating (IV) including an optical absorption layer (4) enclosed and directly connected to two silicon nitride layers (4', 4''), and the absorption layer (4) consists of a semi-stoichiometric metal nitride MeNx, or a semi-stoichiometric metal oxide MeOy, or a mixture of both MeNxOy, where Me is at least one element from the transition metal group V and / or VI of the periodic table; - A base coating (I) consisting of at least one base layer (1) deposited directly onto the substrate, made of silicon nitride or metal oxide, thus forming an inner layer of the solar control stack. 2.The glass substrate, according to protection element 1, has a silver-containing infrared-reflective coating layer enclosed and in direct contact with both a zinc oxide (ZnO) or aluminum (Al) zinc oxide layer on the substrate side, forming an inner infrared-reflective coating layer, and a nickel chromium (NiCr) or titanium dioxide (TiO2) layer on the surface side of the silver-containing layer. There is also another zinc oxide, zinc tin oxide (SnZnO), tin oxide (SnO2), or aluminum-doped layer opposite, each in direct contact with a nickel chromium or titanium dioxide layer, forming an outer infrared-reflective coating layered towards the surface of the layer stack. 3.The glass substrate, according to one of the previous protection elements, consists of a base layer (I) that includes at least one nitride or oxide layer (1, 1') of silicon (Si), titanium (Ti), tin (Sn), zinc (Zn), tin-zinc (SnZn), niobium (Nb), or zirconium (Zr), or an stack of these different nitride or oxide layers for the metallic and / or semiconductor element(s) in successive layers.
4. The glass substrate, according to protection element 3, consists of a base layer (1) of silicon nitride, the innermost layer (4') of the absorption coating (IV). 5.The glass substrate, according to one of the previous protection elements, is at least one of the layers of silicon nitride (4', 4''), zinc oxide (2'), additional zinc oxide (2'''), zinc tin oxide (2'''), tin oxide (2'''), and / or a nitride or oxide layer of silicon, titanium, tin, zinc, tin zinc, niobium, or zirconium (1', 1') that is an aluminum-doped layer.
6. Glass substrate: In accordance with one of the aforementioned protection elements, the solar control layer also includes a scratch-resistant coating at both ends (V). The scratch-resistant coating (V) includes a composite layer (5) consisting of a transition metals (TM) compound, titanium and / or zirconium, with oxygen and / or non-metallic carbon. 7.The glass substrate, according to protection element 6, has a scratch-resistant coating (V) consisting of a titanium zirconium carbide layer (5) followed, towards the surface and in direct contact with the titanium zirconium carbide layer, by a hydrogen-containing diamond-like carbon (DLCH) layer (5').
8. The glass substrate, according to protection element 6, has a scratch-resistant coating consisting of a titanium zirconium oxide layer.
9. The glass substrate, according to one of the previous protection elements, has an infrared-reflective coating directly followed by an absorption coating.
10. Glass substrate: According to one of the protection elements 6 to 8, it includes an additional layer of silicon nitride enclosed and in direct contact with both the end layer of the infrared-reflective coating and the scratch-resistant coating. 11.
12. Glass substrate: According to one of the aforementioned protection elements, the absorption coating or additional absorption coating is immediately followed by an infrared-reflective coating or additional infrared-reflective coating.
13. Glass substrate: According to one of the aforementioned protection elements, the absorption layer is a semi-isotropic metal nitride (MeNx), and the isotropic value x is 0.1 ≤ x ≤ 1, specifically 0.1 ≤ x ≤ 0.
7.
14. Glass substrate: According to one of the aforementioned protection elements, the absorption layer is a semi-isotropic metal nitride (MeNx) or a semi-isotropic metal oxide (MeOy).
14. Glass substrate: According to one of the previously mentioned protective elements, where Me is one of the molybdenum (Mo), tantalum (Ta), tungsten (W), or a mixture thereof. 15.
16. Glass substrate: According to one of the aforementioned protection elements, the nitride, oxide, or oxynitride semi-stoichiometric material is MoNxOy.
17. Glass substrate: According to one of the aforementioned protection elements, at least one of the two silicon nitride layers and / or the additional silicon nitride layer is doped with aluminum.
18. Glass substrate: According to one of the aforementioned protection elements, at least one separating coating (III) is provided between an infrared-reflective coating (II) and a scratch-resistant coating (V) and is in direct contact with it; between two consecutive infrared-reflective coatings (II) and is in direct contact with them; and / or between an adsorption coating (IV) and an infrared-reflective coating (II) and is in direct contact with it.
19. Glass substrate according to protection element 17, where the separating layer (III) consists of, or is composed of, another layer of silicon nitride, or another layer of zinc oxide, or tin oxide, or another layer of zinc and tin oxide (3, 3'). The glass substrate according to protection element 17 or 18, where the separating coating (III) consists of a silicon nitride layer (3) followed and directly connected to a zinc and tin oxide layer (3'), where the silicon nitride layer is in direct contact with the outermost zinc oxide layer of the infrared-reflective coating and the zinc and tin oxide layer is in direct contact with the inner zinc oxide layer of the infrared-reflective coating.
20. Glass substrate: According to one of the previous protective elements, the silver-containing layer is a silver layer. 21.
22. Glass substrate: According to one of the previous protection elements, the difference Δk = k780 – k380 between the extinction coefficients of the absorption coating measured at 780 nm and at 380 nm is: │0.4 < Δk < 1.0│ 23. Glass substrate: According to one of the previous protection elements, the extinction coefficient k550 for the MeNxOy layer measured at a wavelength of 550 nm is: 1.5 < k550 < 4.2 24. Glass substrate: According to one of the previous protection elements, the specific electrical resistivity R for the MeNxOy layer is: R < 600 Ω*cm.