Thixotropic slurry with enhanced reliability for use in a wellbore

A vibratory gel slurry composed of cement and clay minerals, enhanced with epoxy resin and silica, addresses the inefficiencies of conventional sealing methods by forming a solid barrier in wellbores, reducing fluid loss and operational costs, and enhancing drilling efficiency.

SA1120253105A1Pending Publication Date: 2026-10-05HALLIBURTON ENERGY SERVICES INC
View PDF 0 Cites 0 Cited by

Patent Information

Application Number
SA1120253105
Authority / Receiving Office
SA · SA
Patent Type
Applications
Current Assignee / Owner
Filing Date
2025-05-05
Publication Date
2026-10-05

AI Technical Summary

Technical Problem

Existing methods for sealing permeable zones in wellbores to prevent fluid loss during drilling operations are inefficient, leading to increased costs and reduced wellbore productivity due to the inability of conventional lost circulation materials to effectively fill larger fractures and the need for additional pumps and line runs.

Method used

The use of a vibratory gel slurry composed of cement, clay minerals, and a suspending agent, which can be modified with additional components like epoxy resin and silica to enhance mechanical properties, is injected into the wellbore to form a solid barrier that seals permeable zones, reducing fluid loss and cement usage.

Benefits of technology

The vibratory gel slurry effectively seals permeable zones, reducing drilling fluid loss, decreasing operational costs, and allowing for faster drilling operations by minimizing the need for excess cement, thus improving wellbore productivity.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure 6D16DE25-543B-4C55-A843-B0FD3055E0FB
    Figure 6D16DE25-543B-4C55-A843-B0FD3055E0FB
  • Figure 93A40CD5-D34F-4080-BE0D-C8CF58BEE6F2
    Figure 93A40CD5-D34F-4080-BE0D-C8CF58BEE6F2
  • Figure D2B7A05A-D568-42E3-9567-0E415A2093A5
    Figure D2B7A05A-D568-42E3-9567-0E415A2093A5
Patent Text Reader

Abstract

The present invention relates to the use of a thixotropic slurry material in a wellbore during a wellbore operation. A wellbore operation may involve drilling, cementing, or any other suitable operation that may involve injecting a liquid material into the wellbore. The thixotropic slurry material may be a mixture of cement, clay mineral, and suspending agent, and may be injected into the wellbore during the wellbore operation. [Figure 2]
Need to check novelty before this filing date? Find Prior Art

Description

The current discussion relates, in certain aspects and examples, to vibratory gel liquefied plugs for wellbore operations, for example, to seal off areas of lost circulation in a wellbore or to perform cementing. Vibratory gel liquefaction can be a time-dependent shear-thinning property. For example, vibratory gel liquefied slurry can remain fluid during agitation or shaking and can readily gel under static conditions. The vibratory gel liquefaction behavior can be used in drilling operations to reduce or eliminate unwanted losses from a weak formation. Vibratory gel liquefied plugs can be injected into a wellbore to bond to the formation, seal permeable areas in the wellbore, and prevent loss of drilling fluid circulation through permeable areas within the wellbore. The gel-like liquefied sealant can be pumped down the well or otherwise placed in the borehole to treat a permeable zone within the subsurface formation to prevent or alleviate lost circulation. The sealing material can include a lost circulation material with particle sizes ranging from 2 nanometers (3.94 x 10⁻⁸ inches) to 5 millimeters (0.20 inches). This lost circulation material can be used to treat fracture sizes ranging from 1 millimeter (0.04 inches) to 2 millimeters (0.80 inches). For example, sodium silicate distributed from the drill string and calcium chloride present in the annular space near the lost circulation zone can combine to form a gel, also known as a viscous seal. Viscous sealants can be used as lost circulation materials. In some cases, the viscous sealant can be injected into a wellbore using multiple pumps and operators. Increasing the number of pumps and operators can, however, increase drilling costs. For larger fracture sizes, for example from 3 millimeters (0.12 inches) to 5 millimeters (0.20 inches) or larger, the lost circulation material may not adequately fill the larger fracture areas, which may result in fluid loss during the drilling process.For example, fracture sizes from 3 mm (0.12 in) to 5 mm (0.20 in) can be handled using bulking materials with large particles homogeneously distributed throughout the material. Larger particles may require additional pumps and line runs because their diameter is greater than the drill string diameter. The increased number of pumps and lines used to drain water to the lost circulation zones increases costs. Furthermore, continued loss of drilling fluid due to insufficient lost circulation material can lead to decreased wellbore productivity and further increased costs. In some cases, a vibrating gel slurry can be used as a missing rotation material to fill both small fractional sizes (e.g., 1 mm (0.04 in) to 2 mm (0.80 in)) and large fractional sizes (e.g., 3 mm (0.12 in) to 5 mm (0.20 in)) within a subsurface formation. For example, a vibrating gel slurry base material might include clay minerals, a suspending agent, and cement to form a dry mix. In some cases, the base vibrating gel slurry may have an initial density of 11 pounds per gallon, which can be modified by adding additional components.For example, adding at least one component of an epoxy resin composition, amorphous silica, water, a set retarder, a foaming agent, a defoaming agent, glass beads, barite, calcium carbonate, or manganese tetraoxide can generate a vibratory gel slurry with a different density than the base vibratory gel slurry. In some cases, this vibratory gel slurry can be pumped through the drill string and annulus during drilling operations. Adding one or more additional components may improve the mechanical properties of the composition. Combined, the vibratory gel slurry may improve compressive strength while also reducing the permeability of the lost circulation zone. By including one or more additional ingredients in the formula, the desired liquefied behavior of the gel consistency can be achieved with shaking.For example, a vibrating gel-melting slurry can be easily injected into desired areas of missing circulation, and the vibrating gel-melting slurry may exhibit a decrease in gel time upon injection, which is the time that may pass until the vibrating gel-melting slurry produces a gel with a desired compressive strength. These illustrative examples are intended to familiarize the reader with the general topic discussed here and are not meant to limit the scope of the concepts mentioned. The following sections describe several additional properties and examples, referencing diagrams where similar numbers indicate similar elements. Directional descriptions are used to describe illustrative aspects, but, like the illustrative aspects themselves, they should not be used to restrict the current discussion. Figure 1 is a schematic diagram of a wellbore 104 being drilled through an aquifer 102, where a plug material can be used to prevent loss of drilling fluid circulation, as demonstrated in a current discovery example. A drilling rig 106 can be used to drill wellbore 104. A drill bit 110 can be installed at the end of a drill string 112, incorporating multiple sections of drill pipe. Wellbore 104 can be drilled using a surface rotary motor to rotate the drill string 112 and apply torque and force to cause the drill bit 110 to extend through the wellbore 104. Drilling fluid can be transferred through the drill string 112 using one or more pumps 114. The drilling fluid can be circulated through the drill bit 110 and returned to the surface through the wellbore 104 loop, as indicated by arrows 108, thus removing drill cuttings (e.g., material such as rock produced during drilling) from the wellbore 104. Pump 114 can be in fluid contact with Kelly 118 via pipe 116 to transfer drilling fluid from Pump 114, through the drill string 112, and back to the wellbore 104. Although not explicitly stated, additional channels besides the drill string 112 may also be present within the wellbore 104.In some examples, the subsurface formation 102 may be a suboceanic formation into which a well hole can be drilled. The 102 formation may contain permeable zones (P120) through which drilling fluid can migrate from wellbore 104 into the 102 formation. These P120 zones may be fractures, cracks, lines, voids, openings, or similar features. The presence of such P120 zones in the 102 formation may cause fluid or material circulation during wellbore operations, which may include drilling, cementing, or other appropriate operations involving fluid injection into the wellbore. For example, during a drilling operation, a lost circulation zone may cause a loss of drilling fluid circulation in wellbore 104, preventing the fluid from flowing back to the surface. To maintain drilling fluid circulation in wellbore 104, a vibratory gel slurry can be placed in wellbore 104 and allowed to settle at the bottom of the wellbore relative to the aquifer 102 at the lost circulation zone. In some cases, vibratory gel slurry can be injected into wellbore 104 during drilling operations to seal the lost circulation zone where the fracture size is greater than 5 millimeters (0.20 inches). In other cases, vibratory gel slurry can be injected into a wellbore and sufficient time can be allowed for the slurry to set within the lost circulation zone before stabilization to prevent the use of excess cementitious stabilization material. The use of vibratory gel slurry can reduce costs and production time by preventing the injection of excess fluid into the permeable zones 120 within the wellbore. The vibratory gel slurry may increase in strength over time after placement in the wellbore. When mixed or encountered with favorable conditions downhole, a freely flowing, vibrating gel slurry can be tuned to form a solid barrier within the permeable zone. The specific slurry may prevent the flow of drilling fluid from the wellbore into the permeable zone. Favorable conditions can include, for example, pH, salinity, water content, temperature, and shear rate. The vibrating gel slurry mixture may rapidly develop compressive strength. It can also rapidly harden to form a solid, highly impermeable sealing mass (e.g., no fluid, or only a small amount, can pass through the mass). After installation, it may not be possible to wash the liquefied gel-like slurry by shaking from the permeable areas 120, and the circulation of drilling fluid through wellbore 104 may be resumed without concern that drilling fluid may leak from wellbore 104 into the subsurface formation 102. After drilling well 104 is completed, the drill string 112 and drill bit 110 can be removed from well 104, and the casing can be placed in well 104. Initial cementing can then be performed by pumping cement slurry down the casing and into the annular space between the casing and the well 104 borehole wall. The vibrating gel-like slurry seals the permeable zones 120 and prevents the cement slurry from flowing into the subsurface formation 102. As a result, the hydrostatic pressure of the cement slurry can be maintained so that the mixture returns to the surface and forms a relatively strong cement column in the annular space of well 104. The vibrating strength of a vibrating gel slurry can affect its ability to seal permeable zones within a wellbore and prevent fluid loss. The vibrating gel slurry's strength may be influenced by the overall composition of the base material used to produce it. For example, shale and suspension agents may have synergistic properties, and when combined, they may improve the desired mechanical properties for generating vibrating gel slurry. The choice of material for lost circulation may depend on the geological composition of the subsurface formation. By selecting a vibrating gel slurry with enhanced performance to effectively seal permeable zones within a wellbore, operations can be extended to geographic areas and subsurface formations that might otherwise be unworkable. The basic composition of the material for generating a gel-like slurry by basic shaking may generally include cement, clay mineral, and a suspending agent. Various types of cement can be included in the vibrating gel-like mortar described here. In some examples, the cement may be hydraulic cement and may include one or more Portland cements, pozzolanic cements, gypsum cements, high alumina cements, slag cements, high magnesium cements, shale cements, acid or base cements, fly ash cements, zeolite cement systems, kiln cement systems, metakaolin fine cements, or pumice. In some formulations, the cement may be non-hydraulic, for example, Sorel cement. Sorel cement may contain magnesium oxide, magnesium chloride, and a setting agent, for example, sodium hexametaphosphate. In some formulations, Sorel cement may also contain diotane gum, sepiolite clay, and a suitable amount of water to produce a vibrating gel cement slurry. In some formulations, the water content may range from approximately 25 percent by weight to approximately 800 percent by weight of the base material. The resulting vibrating gel cement slurry may have a density ranging from 10 lb / gal (1.198 kg / L) to 14 lb / gal (1.437 kg / L). Sorel-type liquefied cement slurry with a gel consistency can be used during well drilling operations to prevent fluid loss during well drilling operations.For example, Sorel liquefied gel-forming mortar can contain magnesium chloride in proportions ranging from about 5% by weight of the mortar to about 70% by weight of the mortar (for example, 10% by weight of the mortar, 15% by weight of the mortar, 20% by weight of the mortar, 25% by weight of the mortar, 30% by weight of the mortar, 40% by weight of the mortar, 50% by weight of the mortar, or 60% by weight of the mortar). In some examples, a shake-formed gel-like sorel mortar may contain magnesium oxide in proportions ranging from about 5% by weight of the mortar to about 70% by weight of the mortar (for example, 10% by weight of the mortar, 15% by weight of the mortar, 20% by weight of the mortar, 25% by weight of the mortar, 30% by weight of the mortar, 40% by weight of the mortar, 50% by weight of the mortar, or 60% by weight of the mortar).In some examples, a gelling agent may include a setting retarder, for example, sodium hexametaphosphate, in amounts ranging from approximately 0% wt. of the mortar to approximately 20% wt. of the mortar (e.g., 1% wt. of mortar, 2% wt. of mortar, 4% wt. of mortar, 8% wt. of mortar, 16% wt. of mortar, or 20% wt. of mortar). In some examples, sodium hexametaphosphate may be present in amounts less than 1% wt. of the mortar. The base material used in the production of a shake-to-gel slurry may include a suspending agent. Various types of suspending agents may be included in the shake-to-gel slurry described here. In some examples, the suspending agent may be a polysaccharide such as diotane gum. In some formulations, the suspending agent may be in powder form. For example, the suspending agent may be SA-1015™ or, alternatively, WG-17™, available from Halliburton Energy Services, Inc. The suspending agent may be present in amounts ranging from 0.1% by weight of the slurry to 4% by weight of the slurry (e.g., 0.2% by weight of slurry, 0.4% by weight of slurry, 0.8% by weight of slurry, 1.0% by weight of slurry, 2.0% by weight of slurry, 3.0% by weight of slurry, or 4.0% by weight of slurry). The base material used in the production of agglomerated gel-like slurry may also include a shale mineral. For example, suitable shales that may be used in the formulation include calomite, montmorillonite, bentonite, hydrated mica, attapulgite, sepiolite, and any other suitable shale mineral used by professionals in this field. In some formulations, the shale mineral may be a synthetic shale such as labonite. The shale mineral may be present in quantities ranging from approximately 1% by weight of the slurry to approximately 30% by weight. If a shale mineral is present, it may be present in the base material in sufficient quantities to provide the required compressive strength or cost, among other considerations. The selection of a vibrating gel slurry with improved mechanical or physical properties may involve adding a density modifier to a range of 9 lb / gal (1.078 kg / L) to 16 lb / gal (1.917 kg), in addition to the vibrating gel slurry itself. For example, adding at least one component of an epoxy resin formulation, amorphous silica, a setting retarder, a foaming agent, a defoaming agent, glass beads, barite, calcium carbonate, or manganese tetraoxide can change the density from the base density to a secondary density. In some formulations, a vibrating gel-forming slurry may contain an epoxy resin or a combination of multiple epoxy resins. For example, the epoxy resin may contain a functionalized diglycidyl ether molecule or any multifunctional glycidyl ether molecule. The diglycidyl ether molecule may be non-polymeric. In some examples, the epoxy resin may be butylglycidyl ether, diglycidyl cyclohexane dimethanol ether, bisphenol A diglycidyl ether, diglycidyl cyclohexane dimethanol ether, epoxy-treated bisphenol, or any combination thereof. In some formulations, the epoxy resin may contain R1 and R2, where R1 differs from R2. For example, a shake-to-gel slurry may include a combination of butylglycidyl ether (R1) and diglycylcyclohexanedimethyl ether (R2), and R1, R2, or a combination of both may be present in amounts ranging from about 5% by weight to about 50% by weight of the shake-to-gel slurry.In addition, a hardener can be incorporated into a vibrating gelling mortar in combination with the epoxy resin formulation. The hardener may include a compound consisting of aliphatic amines, tri-aliphatic amines, aromatic amines, aliphatic cyclic amines, heterocyclic amines, amidoamines, polyamides, polyethyleneamines, and carboxylic acid anhydrides. Examples of aliphatic and aromatic amines include triethylene tetraamine, ethylene diamine, N-co-alkyl trimethylene diamine, isofuron diamine, diethyltoluene diamine, and tris(dimethylaminomethylphenol). In some examples, carboxylic acid anhydrides include methyltetrahydrophthalic anhydride, hexahydrophthalic anhydride, maleic anhydride, polyazelaic polyanhydride, and phthalic anhydride. In some cases, the vibrating gel slurry may contain between approximately 1% by weight and approximately 50% by weight of the hardener. Shaking gel slurry containing resin and hardener may also include an accelerator to accelerate the curing reaction of the epoxy resin within the slurry. In some cases, the hardener itself may act as the accelerator in the shaking gel slurry. In some cases, the accelerator may be a compound consisting of tertiary amines, carboxylic acids, or alcohols (especially phenols). For example, the accelerator may be 2,4,6-tridimethylaminomethylphenol. In some cases, the accelerator may be included in a shaking gel slurry in amounts ranging from approximately 0.5% by weight to approximately 50% by weight. Factors considered when selecting a vibrating gel slurry include compressive strength, thickening time, and gel strength. The compressive strength of the material can be determined over time during processing under downhole temperature and pressure conditions using ultrasonic cement analyzers (UCA). Thickening time is a measure of how long the slurry remains fluid and pumpable. It is generally evaluated under downhole conditions as a function of consistency or pumpability. Gel strength is a measure of shear stress at a low shear rate after the material has been quietly set for a specified period. Time measurements for determining gel strength can range from ten minutes to ten seconds at 80°F (27°C) to 190°F (88°C) at atmospheric pressure. In some examples, the material described here can have a maximum compressive strength exceeding 50 psi (345 kPa). In other examples, the vibrating gelling slurry can have a 10-second gelling strength of at least 20 psi (97 kg / m²) at 80°F (27°C). In some examples, the material can have a 10-second gelling strength of at least 25 psi (122 kg / m²) at 80°F (27°C). In some examples, the material can have a 10-minute gelling strength of at least 50 psi (244 kg / m²) at 80°F (27°C). In some examples, the material can have a gel strength of at least 50 lb-f / 100 ft² (488 kg / m²) for 10 minutes at 80°F (27°C). In other examples, the material can have a gel strength of at least 100 lb-f / 100 ft² (976 kg / m²) for 10 minutes at 130°F (54°C).In some examples, the material can have a gel strength for 10 seconds of at least 15 lb-force / 100 ft² (73 kg / m²) at 130°F (54°C). The material can be placed in the wellbore to significantly seal one or more permeable or fracture zones and prevent or help prevent the loss of circulation of drilling fluids and cement slurry through these zones. In some cases, the material may be placed in the zone of lost circulation within the wellbore. Methods for using a vibrating gel slurry may involve supplying a material containing cement, a shale mineral such as sepiolite, and a suspending agent; bonding the lost circulation zone in the wellbore to the material; and allowing the material to set within the lost circulation zone. In some cases, the shale mineral may be present in amounts ranging from approximately 1% by weight of the cement to approximately 30% by weight of the cement. Amorphous silica may include silicate, silica fume, fly ash, or any other suitable silica known to a person with expertise in the field. In some formulations, silica is present in amounts ranging from 5 to 150 percent by weight of the cement. Figure 2 is a diagram 200 showing the mixing of a shake-type gel slurry for use in a borehole to treat the lost circulation zone, based on one of the current discovery examples. In some examples, the materials shown here can be prepared using a batch mixing process. In others, the material can be prepared continuously or "in real time" in the borehole. The shake-type gel slurry formulation can be mixed in a mixer 202 to generate the slurry. The shake-type gel slurry can be optionally stored for future use or injected into the borehole using an injection pump 204. The injection pump 204 can inject the shake-type gel slurry into borehole 206 to treat the lost circulation zone 208 within the subsurface formation. In some examples, the method may involve agitating the mixture using a high-shear mixer.In some examples, the vibratory gel injection method might involve supplying a slurry that may include cement, epoxy resin, epoxy resin hardener, accelerator, amorphous silica, sepiolite, and a suspending agent. The slurry can be mixed in a 202 mixer, which can continuously agitate the slurry. The vibratory gel injection slurry can then be injected into a borehole to bring the lost circulation zone into contact with the material. The vibratory gel injection slurry can be placed in the lost circulation zone and left undisturbed for a predetermined period to induce the lost circulation within the borehole. The vibrating gel slurry may include other additives such as defoamers or surfactants that can be added to the vibrating gel slurry before the material is injected by injection pump 204 into wellbore 206. Figure 3 is a diagram illustrating the changes in the base density of formulation 302 to adjust the density of the vibratory gel slurry for use within a wellbore to treat the lost circulation zone, based on one of the current detection examples. The vibratory gel slurry can have a base density of formulation 302, for example, 11 lb / gal (1.318 kg / L), which can be changed by increasing the density of formulation 306 or decreasing the density of formulation 304. The density of the vibratory gel slurry can be controlled to a predetermined density by an actuator that can be used to seal the lost circulation zone within the wellbore. In some examples, the density of the vibratory gel slurry can be less than 16 lb / gal (1.917 kg / L). In some examples, the density of a shaken gel slurry can be less than 12 lb / gal (1.437 kg / L). Shaking gel slurry with a density ranging from 10 lb / gal (1.198 kg / L) to 14 lb / gal (1.437 kg / L) is also used.437 kg / L) to seal the lost circulation zone inside the wellbore. For example, a vibrating gel slurry may have a base density that can be processed to a different density by adding water, an epoxy resin formulation, a foaming agent, a defoamer, or glass beads to the base vibrating gel slurry to reduce the density and make a different vibrating gel slurry. In some examples, the base gelling agent may be a dry mix. For example, the dry mix might include cement, clay, and a suspending agent. The base formulation may involve adding a resin formulation to reduce the density of the slurry. The resin formulation may include a primary epoxy resin, a secondary epoxy resin, an epoxy resin hardener, and an epoxy resin accelerator. In some examples, the primary epoxy resin may contain butylglycidyl ether, and the secondary epoxy resin may contain diglycyl cyclohexane dimethanol ether. An epoxy resin hardener may contain a compound of aliphatic amines, aliphatic tertiary amines, aromatic amines, aliphatic cyclic amines, heterocyclic amines, amidos, polyamides, polyethylene amines, and carboxylic acid anhydrides. An epoxy resin accelerator may contain a compound of tertiary amines, carboxylic acids, and alcohols (especially phenols).In some cases, a resin component may be added to the base mix to reduce the density to less than 11 lb / gal (1.318 kg / L). In some cases, the dry mix may include non-hydraulic cement, clay mineral, a suspending agent, and a setting retarder. The non-hydraulic cement may contain magnesium oxide and magnesium chloride. For example, a basic formulation might include adding a 314 retarder to the vibrating gel slurry to increase density. The retarder could be a compound containing organophosphoric acid, a modified styrene-maleic anhydride sulfonate polymer, lignosulfonates, polyacrylic acid, or a combination thereof. In some instances, the density of a basic vibrating gel slurry can be increased, for example, to a density greater than 11 lb / gal (1.318 kg / L) by adding a heavy-weight compound 316 to the vibrating gel slurry, which could contain barite, calcium carbonate, manganese tetraoxide, or a combination thereof. The density of the vibrating gel slurry could, for example, be less than 16 lb / gal (1.917 kg / L). In some examples, the density can be as low as 9 lb / gal (1.078 kg / L) and as low as 16 lb / gal (1.917 kg / L). In other examples, the density of the liquefied slurry with a vibrating gel consistency can be from 10 lb / gal (1.198 kg / L) to 12 lb / gal (1.437 kg / L). In some cases, a vibrating gel-forming slurry may include other solids to increase or decrease the density of the base composition. For example, the solids may take the form of beads, cubes, bars, cylinders, or mixtures thereof. These solids may include silica, barite, cellulose fibers, carbon fibers, glass fibers, mineral fibers, plastic fibers, metal shavings, Kevlar fibers, basalt fibers, wollastonite, mica, and mixtures thereof. The density of a vibrating gel slurry can be reduced, for example, by adding a lightweight material (such as resins or glass beads) to the vibrating gel slurry. In some cases, the density can be reduced by adding a foaming agent or a gas. For example, the gas that can be added could be an inert gas. Additionally, water can be added to reduce the density of the vibrating gel slurry. In some cases, the water could be fresh, brackish, or salt water. Water can be added to the vibrating gel slurry to modify the density of the slurry composition. In some cases, water can be added to reduce the density of the slurry composition. Example 1: Density variation with respect to the physical and mechanical properties of the liquefied clay with a gel-like consistency by shaking. Five batches of sealing materials were prepared. Examples 1–3, listed in Table 1, contain hydraulic cement, amorphous silica, clay mineral, suspending agent, and foaming agent. Example 4, listed in Table 2, contains a mixture of Example 1 from Table 1 and the resin formulation from Table 2, and Example 5, listed in Table 2, contains a mixture of Example 3 from Table 1 and the resin formulation from Table 3. Examples 4 and 5 were mixed using a grinding mixer at 4000 rpm to form their respective mortars. The densities of Examples 1–3 were 10.5 lb / gal (1.258 kg / L), 11.0 lb / gal (1.318 kg / L), and 11.5 lb / gal (1.318 kg / L), respectively, while the densities of Examples 4 and 5 were 10.0 lb / gal (1.198 kg / L) and 11.0 lb / gal (1.318 kg / L), respectively. The formulation in Example 4 in Table 2 comprises a mixture of 65% by weight of mortar from Example 1 in Table 1 and 35% by weight of mortar from the resin mixture in Table 3. The formulation in Example 5 in Table 2 comprises a mixture of 80% by weight of mortar from Example 3 in Table 1 and 20% by weight of mortar from the resin mixture in Table 3. Table 1 Example 1 Example 2 Example 3 Cement density: 10.5 lb / gal, 11 lb / gal, 11.5 lb / gal Resin density - - - Final density 10.5 lb / gal 11 lb / gal 11.5 lb / gal Cement of category G (g) 104.9 150.6 179.7 Silicalite™ clay mineral (g) 46.8 37.6 44.9 Sepiolite (g) 8.4 5.5 4.9 SA-1015TM Suspension Factor (g) 1.20 0.78 0.70 Water (g) 341.6 332.6 320.6 D-AIR 3000LTM Defoamer (g) 0.4 0.4 0.4 Table 2 Example 4 Example 5 Cement density 10.5 lb / gal 11.5 lb / gal Resin density 9.2 lb / gal Final density 10 lb / gal 11 lb / gal Class G cement (g) is a mixture of 65% by weight. Example 1: 35% by weight. Resin is a mixture of 80% by weight. Example 3: 20% by weight. Silicalite™ clay mineral (g) Sepiolite (g) SA-1015TM Suspension Agent (g) Water (g) D-AIR 3000LTM Defoamer (g) Table 3 Resin composition Density 9.2 lb / gal R1 (Resin 1) 200 grams R2 (resin 2) 66.6 grams H1 (Hardener 1) 77.4 grams A2 (Accelerator 2) 4.0 grams The mortars were tested for their rheological behavior and gel strength using the FANN® rheological properties meter with a FannFann Yield Stress Adapter (FYSA). All tests were performed according to the practices recommended by the American Petroleum Institute (API RP 10B-2). The test results are summarized in Table 4 below. The FYSA rheological properties were tested at 300 revolutions per minute (rpm), 200 rpm, 100 rpm, 6 rpm, and 3 rpm. Example 4 demonstrates higher rheological properties compared to Examples 1 and 2, while maintaining a lower density than both formulations. For example, the rotational speeds in Examples 1 and 2 were 300 rpm at 25 and 24 rpm, respectively, whereas Example 1's FYSA rheological properties were tested at 42 and 300 rpm. Example 5 showed an increase in streamlining properties when compared to Examples 2 and 3, with a lower density than Example 3. In addition, Example 5 showed an increase in streamlining properties when compared to Example 2, which had the same density.The results show that a vibrating gel-like mortar, which may include a mixture of cement and a mixture of resin, may have a lower density than current methods while providing increased flow strength. Table 4 FYSA Driability Properties Example 1 Example 2 Example 3 Example 4 Example 5 80 degrees Fahrenheit 80 degrees Fahrenheit 80 degrees Fahrenheit 80 degrees Fahrenheit 300 25 24 28 42 31 200 20 18 23 35 25 100 17 13 18 27 20 6 13 8 18 16 15 3 12 7 14 15 15 10-second gel strength (lb-force / 100 ft²) 23 16 32 27 35 10-minute gel strength (lb-force / 100 ft²) 120 92 132 110 94 The 10-second gel strength in Examples 4 and 5 was greater than in Examples 1–3, which have similar densities. Similarly, the 10-minute gel strength was greater than in Examples 1–3, which have similar densities. For example, Example 4 has a density of 10 lb / gal (1.198 kg / L), and Example 1 has a density of 10.5 lb / gal (1.258 kg / L). Example 4 exhibited a 10-second gel strength of 27 lb-force / 100 ft² (131 kg / m²), while Example 1 exhibited a 10-second gel strength of 23 lb-force / 100 ft² (112 kg / m²). Examples 4 and 5 demonstrate that a slurry that achieves a gel-like consistency through shaking can have a lower density than existing lost-rotation materials while still exhibiting properties that may be beneficial for lost-rotation environments. For example, examples 4 and 5 showed a 10-minute gel strength of 110 (lb-force / 100 ft²) (537 kg / m²) and 94 (lb-force / 100 ft²) (458 kg / m²), while the comparative example 2 showed a 10-minute gel strength of 92 (lb-force / 100 ft²) (449 kg / m²). The cementitious materials were also tested for properties indicative of field performance. Compressive strength (at 100°F (38°C)) was determined by ultrasonic cement analyzer according to API RP 10B-2 for Examples 1-3 and Examples 4 and 5. The compressive strength results are presented in Table 5. Table 5 UCA at 100°F (38°C) Example 1 Example 2 Example 3 Example 4 Example 5 100 pounds per square inch (689 kilopascals), (minutes:hours) 46:08 > 24 19:04 16:08 14:38 24 hours (lb / in²) 32 62 117 62 198 The vibrating gel-like slurries in Examples 4 and 5 had compressive strengths of 147 and 198, respectively, which were higher than the compressive strengths in Examples 1–3. In some examples, a lost circulation material can be selected for permeable zones to seal the permeable zones in the wellbore and prevent the loss of drilling fluid circulation through these zones within the wellbore. The desired property of a lost circulation material might include a formulation that achieves the desired compressive strength in the shortest possible time. In some examples, achieving a compressive strength of 100 psi (689 kPa) can take less than 24 hours. In some examples, a compressive strength of 100 psi (689 kPa) can be achieved in less than 20 hours. In some examples, the material must have a compressive strength of 100 psi (689 kPa) in less than 18 hours. Example 2: The synergy between silica dust, diotane and sepiolite clay on the physical and mechanical properties of a gel-like slurry by shaking. Table 6 Mortar components weight (g) G 100 grade cement A mixture of silica dust, diotane, and cypule 50 Defoamer 0.5 Water 452.2 To investigate the synergistic effect between silica fume, diotane, and cebolite, eight experiments were conducted by preparing eight different mixtures with varying weight percentages (%) of the individual components. The cement mortar was then mixed according to the formulation shown in Table 6 and tested for flowability, gel strength, and compressive strength. The target density of the formulations was 10 lb / gal (1.198 kg / L). The target mixability rating ranged from 3 to 5, with the results shown in Table 7. Table 7 Mix 1 2 3 4 5 6 7 8 Silica dust, % in the mix: 78, 90, 90, 77, 79, 89, 83, 83.1 Diotane, % in the mixture 2 2 1 3 1 3 2.1 3 Sepiolite, % in the mix 20 8 9 20 20 8 14.9 13.9 Mixability rating: 4 4 5 2 4 2 4 2 Flow properties and gel strength on FYSA at 130°F 300 RPM 23 19 10 29 11 29 19 29 200 RPM 18 15 7 25 8 25 15 26 100 revolutions per minute 14 12 4 2 4 21 12 22 6 revolutions per minute 9 9 3 16 3 15 8 17 3 revolutions per minute 9 9 3 16 3 15 8 17 Gel for 10 seconds, lb-force / 100 ft² 19 13 8 26 10 21 16 25 Gel for 10 minutes, lb-force / 100 ft² 120 65 61 122 62 58 104 86 Compressive strength at 150 degrees Fahrenheit Time for 50 psi (minutes:hours) 06:34 06:24 05:57 06:18 05:42 06:02 06:37 06:42 Time for 100 pounds per square inch (minutes:hours) 08:23 07:56 07:16 08:03 07:06 07:40 08:14 08:48 Based on the results, Mixtures 1 and 7 exhibited good mixability ratings with rapid development of gel strength and compressive strength. Specifically, Mixture 1 had a mixability rating of 4 and a 10-minute gel strength of 120 lb-force / 100 ft², while Mixture 7 had a mixability rating of 4 and a 10-minute gel strength of 104 lb-force / 100 ft². Interestingly, Mixture 4, with 3% diotane and 77% silica fume, had a higher 10-minute gel strength of 122 lb-force / 100 ft², while showing a mixability rating of less than 2, suggesting that even minor modifications to the formulation may affect the mixability rating. To further investigate the synergy between the materials used in cement mortar, a source-to-source variation experiment was conducted with silica fume and sepiolite clay, in addition to a batch-to-batch variation experiment. Table 8 below shows the variation from one source to another in silica dust. The mixture composition used to test the variation from source to source 7 was taken from Table 7 above. The composition was maintained at a density of 10 lb / gal (1.198 kg / L).In short, the composition used to test the source-to-source variation in silica dust was as follows: 83% silica fume, 2.1% diotane, 14.9% sepiolite. Table 8 Silica dust manufacturer Ferroglobe - USA; Wuhan, China; Panfam - India; Elkem Mixability rating: 4 4 5 5 Flow properties and gel strength on FYSA at 130°F 300 revolutions per minute 17 16 16 16 200 revolutions per minute 12 11 12 12 100 revolutions per minute 9 8 9 8 6 revolutions per minute 7 6 5 6 3 revolutions per minute 7 5 4 5 Gel for 10 seconds, lb-force / 100 ft² 20 15 8 9 Gel for 10 minutes, lb-force / 100 ft² 128 122 47 83 Compressive strength at 150 degrees Fahrenheit Time for 50 pounds per square inch (minutes:hours) 05:28 06:06 08:23 06:34 Time for 100 pounds per square inch (minutes:hours) 07:17 08:13 11:13 08:46 As shown in Table 8, the source of silica fume can influence the physical and mechanical properties of the agitated gel cement mortar. For example, silica fume purchased from Ferroglobe-USA recorded a gel strength of 128 lb-strength / 100 ft² for 10 minutes, while silica fume from Panvam-India recorded a gel strength of 47 lb-strength / 100 ft² for the same 10-minute period. The compressive strength of the silica fume purchased from the USA reached 50 lb-sq and 100 lb-sq at 5 hours and 28 minutes and 7 hours and 17 minutes, respectively. The compressive strength of the silica fume purchased from India reached 50 lb-sq and 100 lb-sq at 8 hours and 23 minutes and 11 hours and 13 minutes, respectively. The results show that the source of silica dust can affect both the gel strength and compressive strength of the liquefied gel mixture under shaking. After investigating the source-to-source variations in silica dust, the batch-to-batch variations were investigated. Silica dust from Wuhan was used, and the results for different batches of silica dust are shown in Table 9 below.The cement composition was consistent with the composition used in Table 8; the difference is that the source of the silica dust was from three independent batches of silica dust from Wuhan. Table 9 Silica dust batch number #1 #2 #3 Mixability rating 4 4 4 Flow properties and gel strength on FYSA at 130°F 300 revolutions per minute 16 17 19 200 revolutions per minute 11 12 15 100 revolutions per minute 8 10 13 6 revolutions per minute 6 7 9 3 revolutions per minute 5 6 8 Gel for 10 seconds, lb-force / 100 ft² 15 17 19 Gel for 10 minutes, lb-force / 100 ft² 122 127 113 Compressive strength at 150 degrees Fahrenheit Time for 50 pounds per square inch (minutes:hours) 06:06 05:48 05:22 Time for 100 pounds per square inch (minutes:hours) 08:13 07:51 07:25 Batch variation did not affect the mixability of the cement mortar, but it did affect the gel strength and compressive strength. For example, Batch 1 gelled for 10 seconds, achieving a strength of 15 lb-ft² at 15 lb-ft², and for 10 minutes, achieving a strength of 122 lb-ft². Batch 3 gelled for 10 seconds, achieving a strength of 19 lb-ft², and for 10 minutes, achieving a strength of 113 lb-ft². Batch 1 reached a compressive strength of 50 lb-ft² in 6 hours and 6 minutes, while Batch 3 took 5 hours and 22 minutes. These results demonstrate that batch variation can influence the physical and mechanical properties of cement mortar. As noted above, the source of silica fume and batch variation can affect the physical and mechanical properties of cement mortar. Given the variability in silica fume source variation, the source-to-source and batch-to-batch variations in sepiolite clay were also investigated. The source-to-source variation was performed using the same density (10 lb / gal, 1.198 kg / L) as described above, and the mix composition from Table 7 (83% silica fume, 2.1% ditan, and 14.9% sepiolite). The results for the purchased sepiolite are shown in Table 10 below. Table 10 Sepiolite manufacturers: Lewes (USA), Berwick (India), Chiangton (China), Tulsa (Spain) Mixability rating: 4 4 5 5 Flow properties and gel strength on FYSA at 130°F 300 revolutions per minute 17 21 15 15 200 revolutions per minute 12 18 10 11 100 revolutions per minute 9 14 8 8 6 revolutions per minute 7 10 8 5 3 revolutions per minute 7 9 5 4 Gel for 10 seconds, lb-force / 100 ft² 20 22 9 11 Gel for 10 minutes, lb-force / 100 ft² 128 134 74 87 Compressive strength at 150 degrees Fahrenheit Time for 50 pounds per square inch (minutes:hours) 05:28 05:47 06:02 06:17 Time for 100 pounds per square inch (minutes:hours) 07:17 08:02 07:55 08:36 The variability in the source of the sepiolite shale resulted in variations in the mixability rating of each individual source. The flow properties and gel strength of the slurry composition showed that the source influenced both the 10-second gel strength (lb-force / 100 ft²) and the 10-minute gel strength (lb-force / 100 ft²), as detailed in Table 10 above. Variability in the compressive strength of the cement slurry was also observed; for example, the sepiolite shale source from the USA exhibited a compressive strength of 50 psi at 5 hours and 28 minutes, while the silica fume source from Spain exhibited a compressive strength of 50 psi at 6 hours and 17 minutes. Variability in compressive strength can impact wellbore operations. Therefore, it may be beneficial to aim for a reduction in source and batch variability to minimize variations in wellbore operations. To further investigate batch-to-batch variation in sepiolite clay, three independent batches were purchased from Proec (India) and used to make cement mortar. The results of the batch-to-batch variation are shown in Table 11 below. Table 11 Sepiolite batch number #1 #2 #3 Mixability rating 4 4 4 Flow properties and gel strength on FYSA at 130°F 300 revolutions per minute 21 24 25 200 revolutions per minute 18 19 20 100 revolutions per minute 14 15 16 6 revolutions per minute 10 12 14 3 revolutions per minute 9 11 14 Gel for 10 seconds, lb-force / 100 ft² 22 26 32 Gel for 10 minutes, lb-force / 100 ft² 134 154 151 Compressive strength at 150 degrees Fahrenheit Time for 50 pounds per square inch (minutes:hours) 05:47 05:38 05:52 Time for 100 pounds per square inch (minutes:hours) 08:02 07:26 07:45 Among the three batches, variations in flow properties, gel strength, and compressive strength can be observed. For example, batch #1 had a 10-second gel with a strength of 22 psi, while batch #3 had a 10-second gel with a strength of 32 psi. Similarly, the 10-minute gel with a strength of 134 psi from batch #1 and the 10-minute gel with a strength of 151 psi from batch #3. The compressive strength values ​​showed variations in the time to reach 100 psi (8 hours and 2 minutes for batch #1, and 7 hours and 45 minutes for batch #3). The results from source-to-source variability and also batch-to-batch variability confirm the need for a single cement bag mix that can be used to create a liquefied, gel-like slurry by shaking for use in well-hole operations, for example, to prevent lost rotation during drilling operations. Example 3: Composition of a vibrating gel-like mortar made from Sorel cement and the resulting mechanical properties. Three batches of gel-like slurries were prepared by shaking. Examples 1–3, listed in Table 1, contain magnesium oxide, magnesium chloride, clay minerals, a suspending agent, a setting retarder, and water. Examples 6, 7, and 8 were prepared by mixing using a 4000 rpm grinding mixer to form the respective slurries. Briefly, water was first added to the grinding mixer. Sodium hexametaphosphate was slowly added to the mixer and mixed for 4 minutes. Once the magnesium chloride was completely dissolved, it was added and mixed for 5 minutes at 4000 rpm to ensure complete dissolution. The final step involved adding diotane gum, sepiolite clay, and magnesium oxide to the mixer, followed by mixing at 4000 rpm for 3 minutes. The density of examples 6–8 was 14.0 lb / gal (1.677 kg / L). Prior to performing flowability, gel strength and compressive strength tests, mortar formulations for examples 6-8 were prepared at 90 degrees Fahrenheit for 30 minutes on an atmospheric density meter.In addition to the resulting flow properties, Table 12 below shows the formulations and their properties in terms of compressive strength and gel strength, as shown in Table 13 below. Table 12 Components Example 6 Example 7 Example 8 Magnesium oxide (g) 231.9 231.9 231.9 Magnesium chloride (g) 231.9 231.9 231.9 Sodium hexametaphosphate (g) 4.6 4.6 4.6 Sepiolite (g) 24.3 -- 24.3 Diotane gum (g) 3.5 3.5 -- Water (g) 174.8 174.8 174.8 Table 13 Flow properties and gel strength Example 6 Example 7 Example 8 300 revolutions per minute 39 34 29 200 revolutions per minute 31 25 24 100 revolutions per minute 23 17 20 6 revolutions per minute 19 5 15 3 revolutions per minute 17 4 13 Gel for 10 seconds, lb-force / 100 ft² 50 5 34 Gel for 10 minutes, lb-force / 100 ft² 185 10 112 UCA compressive strength at 90°F / 3000 psi Time for 50 psi (minutes:hours) 08:13 Sedimentation 11:00 Resistance in 24 hours, pounds per square inch: 2245 2193 Example 6, which includes both diotane and sepiolite, demonstrates a rapid increase in gel strength and compressive strength, while Example 7 includes diotane without sepiolite. The compressive strength and gel strength results were lower than in Example 6. For example, Example 6 had a 10-second gel with a strength of 50 lb-force / 100 ft² and a 10-minute gel with a strength of 185 lb-force / 100 ft², while Example 2 had a 10-second gel with a strength of 5 lb-force / 100 ft² and a 10-minute gel with a strength of 10 lb-force / 100 ft². Example 8 had a 10-second gel with a strength of 50 lb-force / 100 ft² and a 10-minute gel with a strength of 112 lb-force / 100 ft², with a formulation including sepiolite but without diotane. The results show that a vibrating gel-forming cement can be designed from sorel cement and a mixture of diotane and sipolite to create a vibrating gel-forming cement with high gel and compressive strength. As used below, any reference to a series of examples should be understood as a reference to each of those examples separately (e.g., "Examples 1 to 4" should be understood as "Examples 1, 2, 3, or 4"). In some respects, methods and mixtures for vibrating gel-consistency slurries with improved reliability for use in a wellbore are provided according to one or more of the following examples: Example 1 is a method that includes: providing a base material, which includes a clay mineral, a suspending agent, and cement; creating a base thixotropic slurry material from the base material; contacting a permeable area in a wellbore with the base thixotropic slurry material; and performing a wellbore drilling operation within the wellbore. Example 2 is the method according to Example(s) 1, where the creation of the basic shaking gel slurry also involves: modifying the basic shaking gel slurry, where modifying the basic shaking gel slurry involves adding at least one of the following: epoxy resin formulation, amorphous silica, setting retarder, foaming agent, water, defoaming agent, glass beads, barite, calcium carbonate, or manganese tetraoxide, to the basic shaking gel slurry. Example 3 is the method according to Example(s) 1, where the permeable zone is a missing rotation zone, and where the well-drilling operation is a drilling operation, a cementing operation, or a combination of both. Example 4 is the method according to Example(s) 1, where the suspending agent is present in an amount ranging from 0.1 percent by weight to 4 percent by weight of the liquefied slurry to a gel consistency by basic shaking. Example 5 is the method according to Example(s) 1, where the clay mineral is present in an amount ranging from 1 percent by weight to 30 percent by weight of the liquefied slurry to a gel-like consistency by basic shaking. Example 6 is the method according to Example(s) 1, where the cement includes a non-hydraulic cement consisting of magnesium chloride, magnesium oxide, and sodium hexametaphosphate. Example 7 is the method according to Example(s) 1, where the epoxy resin formulation includes: epoxy resin; an epoxy resin hardener; and an accelerator, where the epoxy resin is present in an amount ranging from 5 to 50 percent by weight of the basic shaking gel-forming slurry, the epoxy resin hardener is present in an amount ranging from 1 to 50 percent by weight of the basic shaking gel-forming slurry, and the accelerator is present in an amount ranging from 0.5 to 50 percent by weight of the basic shaking gel-forming slurry. Example 8 is the method according to Example(s) 2, where amorphous silica is present in an amount ranging from 5 percent by weight to 150 percent by weight of the liquefied slurry to a gel-like consistency by basic shaking. Example 9 is the method according to Example(s) 2, where the basic shaking gel-forming slurry has a density of 9 to 16 pounds per gallon, a 10-minute steady gel strength of not less than 50 psi at 80°F, and a compressive strength of not less than 50 psi at 100°F. Example 10 is the method according to Example(s) 7, where the epoxy resin includes a first epoxy resin containing butylglycidyl ether and a second epoxy resin containing cyclohexane dimethanol diglycidyl ether. Example 11 is a basic mortar material that includes: cement; clay mineral; and a suspending agent. Example 12 is the basic cementing material according to Example(s) 11, which also includes at least an epoxy resin formulation, water, amorphous silica, a hardening retarder, a foaming agent, a defoamer, glass beads, barite, calcium carbonate, manganese tetraoxide, or any combination thereof. Example 13 is the basic mortar material according to Example(s) 12 where the mortar material is usable as a lost rotation material during a drilling process or a cementing process or a combination of both. Example 14 is the basic cementing material according to Example(s) 11 where the clay is present in an amount ranging from 1 percent by weight to 30 percent by weight according to the weight of the basic cementing material. Example 15 is the basic mortar material according to Example(s) 11 where the suspending agent is present in an amount ranging from 0.1 percent by weight to 4 percent by weight of the basic mortar material. Example 16 is the basic cementing material according to Example(s) 11 where the cement includes a non-hydraulic cement containing magnesium chloride, magnesium oxide and sodium hexametaphosphate. Example 17 is the basic mortar according to Example(s) 12, where the composition of the epoxy resin consists of: epoxy resin; an epoxy resin hardener; and an accelerator, where the epoxy resin is present in an amount ranging from 5 to 50 percent by weight of the basic mortar, the epoxy resin hardener is present in an amount ranging from 1 to 50 percent by weight of the basic mortar, and the accelerator is present in an amount ranging from 0.5 to 50 percent by weight of the basic mortar. Example 18 is the basic cementing material according to Example(s) 12, where amorphous silica is present in an amount ranging from 5 percent by weight to 150 percent by weight of the basic cementing material. Example 19 is the basic mortar material according to Example(s) 12, where the basic mortar material has a density of 9 to 16 pounds per gallon, has a 10-minute steady gel strength of not less than 50 psi at 80°F, and has a compressive strength of not less than 50 psi at 100°F. Example 20 is the basic cementing material according to Example(s) 17, where the epoxy resin includes a first epoxy resin containing butylglycidyl ether and a second epoxy resin containing diglycyl cyclohexane dimethanol ether. The preceding descriptions of some examples, including those illustrated, are provided for illustrative and descriptive purposes only and are not intended to be exhaustive or to limit the disclosure to the precise forms revealed. Many modifications, adaptations, and uses will become clear to specialists in this field without exceeding the scope of the disclosure.

Claims

1. A method that includes: providing a base material, which consists of a clay mineral, a suspending agent, and cement; creating a base thixotropic slurry material; contacting a permeable zone in a wellbore with the base thixotropic slurry material; and performing a wellbore operation within the wellbore. 2.The method according to protection element 1, where the creation of the base thixotropic slurry also involves: modifying the base thixotropic slurry material, where modifying the base thixotropic slurry material involves adding at least one of the following: epoxy resin composition, amorphous silica, set retarder, foaming agent, water, defoaming agent, glass beads, barite, calcium carbonate, or manganese tetraoxide to the base thixotropic slurry material.

3. The method according to protection element 1, where the permeable zone is a lost circulation zone, and the wellbore operation is a drilling operation, a cementing operation, or a combination of both. 4.The method according to protection element 1, where the suspending agent is present in an amount ranging from 0.1% by weight to 4% by weight of the base thixotropic slurry.

5. The method according to protection element 1, where the clay mineral is present in an amount ranging from 1% by weight to 30% by weight of the base thixotropic slurry.

6. The method according to protection element 1, where the cement consists of non-hydraulic cement containing magnesium chloride, magnesium oxide, and sodium hexametaphosphate. 7.The method is in accordance with protection element 2, where the composition of the epoxy resin includes: epoxy resin; epoxy resin hardener; and accelerator, where the epoxy resin is present in an amount ranging from 5 to 50 percent by weight of the base thixotropic slurry material, the epoxy resin hardener is present in an amount ranging from 1 to 50 percent by weight of the base thixotropic slurry material, and the accelerator is present in an amount ranging from 0.5 to 50 percent by weight of the base thixotropic slurry material.

8. The method according to protection element 2, where amorphous silica is present in an amount ranging from 5 to 150 percent by weight of the thixotropic slurry. 9.The method according to Protection Element 2, where the base thixotropic slurry material has a density of 9 to 16 lb / g, a 10-minute steady gel strength of at least 50 lb-f / 100 ft² at 80°F, and a compressive strength of at least 50 lb / in² at 100°F.

10. The method according to Protection Element 7, where the epoxy resin consists of a primary epoxy containing butylglycidyl ether and a secondary epoxy containing cyclohexanedimethyl ether diglycyl.

11. The base slurry material consists of: cement; clay mineral; and a suspending agent. 12.The base slurry material, according to Protection Element 11, also includes at least one of the following: an epoxy resin composition, water, amorphous silica, a set retarder, a foaming agent, a defoaming agent, glass beads, barite, calcium carbonate, manganese tetraoxide, or any combination thereof.

13. The base slurry material, according to Protection Element 12, is one that is usable as a lost circulation material during a drilling operation, a cementing operation, or a combination thereof.

14. Base slurry material according to protection element 11, where clay mineral is present in an amount ranging from 1% by weight to 30% by weight of the base slurry material.

15. Base slurry material according to protection element 11, where suspending agent is present in an amount ranging from 0.1% by weight to 4% by weight of the base slurry material.

16. Base slurry material according to protection element 11, where the cement includes non-hydraulic cement containing magnesium chloride, magnesium oxide, and sodium hexametaphosphate.

17. Base slurry material according to protection element 12, where the resin composition includes: epoxy resin; epoxy resin hardener; The accelerator, where epoxy resin is present in a quantity ranging from 5 to 50 percent by weight of the base slurry material, the epoxy resin hardener is present in a quantity ranging from 1 to 50 percent by weight of the base slurry material, and the accelerator is present in a quantity ranging from 0.5 to 50 percent by weight of the base slurry material. 18.The base slurry material, according to protection element 12, contains amorphous silica in amounts ranging from 5% by weight to 150% by weight. The slurry material, according to protection element 12, has a density of 9 to 16 pounds per gallon, a 10-minute steady gel strength of at least 50 psi at 80°F, and a compressive strength of at least 50 psi at 100°F.

20. Slurry material according to protection element 17, where epoxy resin includes a first epoxy resin containing butylglycidyl ether and a second epoxy resin containing diglycyl cyclohexane dimethanol ether.