A method for producing copper target metal for thin film coating using the sputtering method in the hot extrusion process.
Patent Information
- Application Number
- TH1701005862
- Authority / Receiving Office
- TH · TH
- Patent Type
- Applications
- Current Assignee / Owner
- Filing Date
- 2017-09-29
- Publication Date
- 2026-11-02
Abstract
Claims
16 / 10 / 2569 1. Method for producing a copper target for thin-film coating using the sputtering method. (Sputtering method) From the hot extrusion process to obtain the grain size of... Copper must not exceed 100 micrometers and surface hardness must not exceed 100 HV. The assembly procedure is as follows: a. Selecting copper pipes b. Under-water hot extrusion and c. Cold Drawing 2. The method under Claim 1, whereby the selection of copper pipes is made from copper pipes of a certain diameter. 10-12 inches in diameter, with at least 99.99% copper purity by weight, and oxygen content not exceeding 5 ppm.
3. The method under claim 1 or 2 where hot-pressure rolling in water is further incorporated with the application of... Heat the copper pipe to a temperature of 750-800 degrees Celsius before hot extrusion.
4. Any of the methods under claims 1 through 3, in which water-cooled hot extrusion is incorporated. The process of rapidly cooling (quenching) a copper pipe without contact with air, after it has been compressed through a channel. The mold (Extrusion Die) moves through water at a temperature not exceeding 40 degrees Celsius.
5. Method under claim 4 where the hot extrusion speed is 5-20 mm / sec.
6. Method under Claim 1 where the percentage reduction during cold drawing (% Cold Drawing) The reduction (or deduction) must not exceed 30%.