Abstract
Claims
DEPCT67 06 / 06 / 2567 1. A catalyst capable of / for the simultaneous reduction of both SOx and NOx in exhaust combustion gases, characterized by the inclusion of the following components: (1) an inorganic oxide support or matrix, (2) rare earth metals, (3) selectively selected Group VIII or Group VB, VIII, IB and IIB worthless metals, (4) precious metals, (5) selectively selected Group VIIB worthless metals, (6) selectively selected Group IIA metals, which, on the basis of the total weight of the catalyst, The amount of the inorganic oxide support or matrix of the component (1) as an oxide is 25-95% by weight, for example 25-93% by weight or 25-92% by weight or 40-90% by weight or 40-87% by weight or 40-85% by weight or 45-80% by weight or 50-88% by weight or 50-80% by weight; the amount of rare earth metal of the component (2) as an oxide is 2-70% by weight, for example 4-60% by weight or 4-50% by weight or 4-40% by weight or 6-70% by weight or 8-50% by weight or 8-40% by weight or 12-60% by weight.% by weight or 12-48 % by weight; the amount of precious metals selected from Group VIII or such precious metals selected from Groups VB, VIII, IB and IIB of component (3) as oxides is 1-30 % by weight, for example 1-15 % by weight or 1-12 % by weight or 2-30 % by weight or 2-12 % by weight or 2-10 % by weight or 2-8 % by weight or 3-20 % by weight or 3-15 % by weight; the amount of precious metals of component (4) as elements is 0.01-2 % by weight, for example 0.01-1.5 % by weight or 0.01-2 % by weight or 0.02-1.5 % by weight or 0.02-1.2 % by weight or 0.02-1.0 % by weight; or 0.03-1.2 % by weight; the amount of Group VIIB non-precious metals of component (5) as oxides is: 0 or 1-10 % by weight, 0 or 1-8 % by weight, 0 or 2-5 % by weight; the amount of Group IIA metals of component (6) as oxides is 0 or 1-30 % by weight, 0 or 1-20 % by weight, 0 or 2-15 % by weight; where, as metallic elements, the molar ratio of component (2) to component (3) is (0.4-18):1, for example.(0.4-12):1 or (0.5-15):1 or (0.5-12):1 or (0.5-8):1 or (0.6-18):1 or (1-10):1 or (1-6):1 or (1-4):1 or (2-12):1 or (2-5):1 or (3-6):1; preferably the sum of the amounts of Group VIIB worthless metals of component (5) as oxides and the amounts of Group IIA metals of component (6) as non-zero oxides.
2. Catalyst pursuant to claim 1 where the support or inorganic oxide matrix of component (1) is at least one of the following: alumina, silica-almina, zeolite, spinel, kaolin, diatomite, perlite and perovskite, preferably alumina; and / or the rare earth metals of component (2) are one or more in La, Ce, Pr and Nd, preferably La and / or Ce; most preferably La; and / or the chosen worthless metals from group VIII of component (3) are Co and / or Fe, preferably Co; or such worthless metals chosen from groups VB, VIII, IB and IIB of component (3) are one or more in Fe, Co, Ni, Cu, Zn and V, preferably Co and / or Fe, most preferablyCo; and / or the precious metal of component (4) is one or more of Ru, Rh, Re, Pt, Pd, Ag, Ir, and Au, preferably one or more of Pt, Pd, and Rh, preferably Pd; and / or the Group VIIB non-precious metal of component (5) is Mn; and / or the Group IIA metal of component (6) is one or more of Be, Mg, Ca, Sr, and Ba, preferably Mg.
3. A catalyst pursuant to one of the preceding claims in which the catalyst is composed of (1) a support and (2) rare earth metals, (3) non-precious metals selected from Group VIII and (4) precious metals loaded on the support; in which, on the basis of the total weight of the catalyst, the amount of the support of component (1) is 25–95% by weight; the amount of rare earth metals of component (2) as oxides is 4–60% by weight; The amount of the selected non-precious metal from group VIII of component (3) as an oxide is 2-12 % by weight; the amount of the precious metal of component (4) as an element is 0.01-2 % by weight; or the amount of the support of component (1) is 40-90 % by weight;The amount of rare earth metals of component (2) as oxides is 8-50% by weight; the amount of selected Group VIII worthless metals of component (3) as oxides is 2-12% by weight; the amount of precious metals of component (4) as elements is 0.02-1.5% by weight; or the amount of inorganic oxide supports or matrices of component (1) as oxides is 50-88% by weight; the amount of rare earth metals of component (2) as oxides is 8-40% by weight; the amount of selected Group VIII worthless metals of component (3) as oxides is 2-10% by weight; the amount of precious metals of component (4) as elements is 0.03-1.2% by weight; where, as metallic elements, The molar ratio of component (2) to component (3) is (0.5-15):1 or (1-10):1 or (2-5):
1.
4. A catalyst under one of the preceding claims in which the catalyst consists of (1) a support and (2) rare earth metals, (3) selected worthless metals from groups VB, VIII, IB and IIB, (4) precious metals and (6) Group IIA metals loaded on the support.Where, based on the total weight of the catalyst, the amount of the inorganic oxide support or matrix of component (1) as an oxide is 25-93% by weight; the amount of rare earth metals of component (2) as an oxide is 4-60% by weight; the amount of selected rare earth metals from groups VB, VIII, IB and IIB of component (3) as an oxide is 2-30% by weight; the amount of precious earth metals of component (4) as elements is 0.01-2% by weight; the amount of group IIA metals of component (6) as an oxide is 1-30% by weight; or the amount of the inorganic oxide support or matrix of component (1) as an oxide is 40-87% by weight; the amount of rare earth metals of component (2) as an oxide is 8-50% by weight; The amount of precious metals selected from groups VB, VIII, IB and IIB of component (3) as oxides is 3-20% by weight; the amount of precious metals of component (4) as elements is 0.02-1.5% by weight; the amount of metals of group IIA of component (6) as oxides is 1-20% by weight; orThe amount of the inorganic oxide support or matrix of component (1) as an oxide is 40–85% by weight; the amount of rare earth metals of component (2) as an oxide is 8–40% by weight; the amount of selected rare earth metals of groups VB, VIII, IB and IIB of component (3) as an oxide is 3–15% by weight; the amount of metals of component (4) as elements is 0.03–1.2% by weight; the amount of group IIA metals of component (6) as oxides is 2–15% by weight; where, as metallic elements, the molar ratio of component (2) to component (3) is (0.4–18):1, for example (0.4–12):1 or (0.5–8):1 or (1–4):
1.
5. A catalyst according to any of the preceding claims where the catalyst is composed of the following components: (1) The support or matrix (1) Inorganic oxides, (2) Rare metals, (3) Selected worthless metals from groups VB, VIII, IB and IIB, (4) Precious metals and (5) Worthless metals from group VIIB where, based on the total weight of the catalyst, the amount of the support or inorganic oxide matrix of component (1) asThe amount of the rare earth metals of component (1) as an oxide is 25-92% by weight; the amount of rare earth metals of component (2) as an oxide is 6-70% by weight; the amount of selected rare earth metals from groups VB, VIII, IB and IIB of component (3) as an oxide is 1-12% by weight; the amount of precious earth metals of component (4) as elements is 0.01-1.5% by weight; the amount of rare earth metals of component (5) as an oxide is: 1-10% by weight; or the amount of the inorganic oxide support or matrix of component (1) as an oxide is 40-85% by weight; the amount of rare earth metals of component (2) as an oxide is 12-60% by weight; the amount of selected rare earth metals from groups VB, VIII, IB and IIB of component (3) as an oxide is 2-10% by weight; The amount of the metal of component (4) as an element is 0.02-1.2 % by weight; the amount of the rare earth metal of component (5) as an oxide is: 1-8 % by weight; or the amount of the inorganic oxide support or matrix of component (1) as an oxide is 40-85 % by weight; the amount of the rare earth metal of component (2)As an oxide, it is 12-48% by weight; the amount of selected worthless metals from groups VB, VIII, IB and IIB of component (3) as an oxide is 2-8% by weight; the amount of precious metals of component (4) as elements is 0.02-1.0% by weight; the amount of worthless metals of group VIIB of component (5) as oxides is: 2-5% by weight; where, as elements, it is a metallic element. The molar ratio of component (2) to component (3) is (0.6-18):1, for example (2-12):1 or (3-6):
1.
6. A catalyst according to one of the preceding claims in which the catalyst is composed of the following components: (1) an inorganic oxide support or matrix, (2) rare earth metals, (3) selected no-value metals of groups VB, VIII, IB and IIB, (4) precious metals, (5) no-value metals of group VIIB and (6) metals of group IIA in which, based on the total weight of the catalyst, the amount of the inorganic oxide support or matrix of component (1) as an oxide is 25-95 % by weight; the amount of rare earth metals of component (2) as an oxide is 2-70 % by weight;The amount of selected worthless metals from groups VB, VIII, IB and IIB of component (3) as oxides is 1-15% by weight; the amount of precious metals of component (4) as elements is 0.01-1.5% by weight; the amount of group VIIB worthless metals of component (5) as oxides is 1-10% by weight; the amount of group IIA metals of component (6) as oxides is 1-30% by weight; or the amount of inorganic oxide supports or matrices of component (1) as oxides is 40-90% by weight; the amount of rare earth metals of component (2) as oxides is 4-50% by weight; the amount of selected worthless metals from groups VB, VIII, IB and IIB of component (3) as oxides is 2-12% by weight; the amount of precious metals of component (4) as elements is 0.02-1.2% by weight; The amount of Group VIIB non-essential metal of component (5) as an oxide is: 1-8 % by weight; the amount of Group IIA metal of component (6) as an oxide is 1-20 % by weight; or the amount of inorganic oxide support or matrix of component (1) as an oxide is 50-80.% by weight; the amount of rare earth metals of component (2) as oxides is 4-40 % by weight; the amount of selected rare earth metals of group VB, VIII, IB and IIB of component (3) as oxides is 2-10 % by weight; the amount of precious earth metals of component (4) as elements is 0.02-1.0 % by weight; the amount of rare earth metals of group VIIB of component (5) as oxides is: 2-5 % by weight; the amount of group IIA metals of component (6) as oxides is 2-15 % by weight; where, as metallic elements, the molar ratio of component (2) to component (3) is (0.4-18):1, for example (0.5-12):1 or (1-6):
1.
7. Catalysts according to any of the preceding claims where the catalyst is a catalyst.
8. A catalyst according to one of the preceding claims in which a rare earth metal of component (2) is incorporated with La; a selected worthless metal from Group VIII or such worthless metals selected from Groups VB, VIII, IB and IIB of component (3) is incorporated with Co; a precious metal of component (4) is incorporated with Pd;9. A catalyst under any of the preceding claims in which the rare earth metal of component (2) is La; the selected random metal of Group VIII or such random metal selected of Groups VB, VIII, IB and IIB of component (3) is Co; the precious metal of component (4) is Pd; the random earth metal of Group VIIB of component (5), if present, is Mn; the Group IIA metal of component (6), if present, is Mg.
10. A catalyst under any of the preceding claims 7-9 in which the catalyst is exposed to an atmosphere containing SO2; the catalyst has a characteristic peak.
11. Any catalyst under the preceding claims 8-9 in which the catalyst exhibits characteristic peaks of 2theta=33.0°±0.1°, 33.5°±0.1°, and 47.5°±0.1°, as well as 27.0°±0.1°, 28.0°±0.1°, and 39.5°±0.1° in the powder XRD spectrum.
12. Methods for the preparation of catalysts pursuant to any of the preceding claims, which include: (I) co-precipitation or sol-gel methods are used to produce reactive metal precursors in which the reactive metals in the reactive metal precursor consist of (2) rare earth metals, (3) selected no-value metals from Group VIII or selected no-value metals from Groups VB, VIII, IB and IIB, (5) selectively selected Group VIIB no-value metals and (6) selectively selected Group IIA metals; and (II) the reactive metal precursor and (1) an inorganic oxide support or matrix or a precursor of that substance and selectively selected a precursor of (4) precious metals are combined and a slurry is made to produce a slurry. The resulting slurry is dried and / or calcined to produce the catalyst; or the reactive metal precursor and (1) an inorganic oxide support or matrix or a precursor of that substance and selectively selected Precursors of (4) precious metals are mixed together and slurries are made to produce slurries. The resulting slurries are dried and / or calcined to produce semi-finished catalytic products;The semi-finished catalyst product is then impregnated with a solution containing a precursor of (4) precious metals as the impregnation solution to produce a solid product, and the solid product is then dried and / or calcined to produce the catalyst; where a reactive metal precursor, an inorganic oxide support or matrix, or a precursor of that substance and a precursor of precious metals are used in such quantities that the produced catalyst contains the catalyst composition according to any of the prior claims.
13. Preparation method according to any of the prior claims where in step (I) the co-precipitation method is used to produce reactive metal precursors; it is desirable that the co-precipitation method include: (I-1) Prescribing of a first solution containing a precursor of (2) rare earth metals, a precursor of (3) rare earth metals selected from Group VIII or rare earth metals selected from Groups VB, VIII, IB and IIB, a precursor of (5) rare earth metals from Group VIIB and selected. Precursor of (6) Group IIA metals; desirable.(I-2) The first solution and co-precipitate are subjected to a co-precipitation reaction; it is desirable that the co-precipitate be a carbonate salt, preferably at least one of ammonium carbonate, potassium carbonate, and sodium carbonate; it is desirable that the co-precipitation reaction be conducted at pH=8-10; (I-3) Drying and / or calcination of the solid products obtained in the co-precipitation reaction to produce reactive metal precursors; it is desirable. The conditions for calcination in steps (I-3) include: temperature of 300-800 °C, e.g., 300-700 °C; time of 0.5-8 hours, e.g., 1-8 hours, or 1-5 hours; where the support or matrix is an inorganic oxide or precursor of the substance, a rare earth metal precursor, a precursor of selected Group VIII worthless metals, or selected Group VB, VIII, IB, and IIB worthless metals, a precious metal precursor, a selective Group VIIB worthless metal precursor, and a selective Group VIIB metal precursor.IIA is used in quantities where the produced catalyst contains the catalyst composition according to any of the preceding claims.
14. The preparation method according to any of the preceding claims in which in step (II) the precursor of the precious metal component is at least one of the nitrates, chlorides and / or chlorates, for example at least one of the palladium nitrate, palladium chloride, platinum chlorate and rhodium chloride, preferably palladium nitrate and / or palladium chloride; and / or in step (II) the slurry contains 5-40% by weight of solids, for example 6-38% by weight or 7-35% by weight; and / or in step (II) the conditions for calcining the slurry include: the temperature is 300-800 °C, for example 300-700 °C; the time is 0.5-8 hours, for example 1-8 hours or 1-5 hours; and / or in step (II) the precious metal precursor is hydrolyzed in an acid solution to provide a humectant solution; preferably the acid is of a water-soluble inorganic and / or organic acid, preferably at least one of hydrochloric acid, nitric acid,Phosphoric acid and acetic acid; preferably, the acids are used in quantities where the pH of the immersion solution is less than 6.0, preferably less than 5.0, e.g., 2.0-5.0; preferably, the conditions for calcining the solid product include: temperature is 300-800 °C, e.g., 300-700 °C; time is 0.5-8 hours, e.g., 1-8 hours, or 1-5 hours.
15. A method for the simultaneous reduction of both SOx and NOx from exhaust gases, comprising the contact of the exhaust gases with a catalyst according to the preceding claim or a catalyst prepared by the method of preparation according to the preceding claim, under conditions for the removal of SOx and NOx; preferably. Conditions for SOx and NOx removal include: temperature of 300-1000°C. For example, 500-800°C, 600-750°C, 625-750°C, 650-750°C, 675-750°C, 700-750°C, 725-750°C, 600-725°C, 625-725°C, or 650-725°C.675-725 degrees Celsius or 700-725 degrees Celsius or 600-700 degrees Celsius or 625-700 degrees Celsius or 650-700 degrees Celsius or 675-700 degrees Celsius or 600-675 degrees Celsius or 625-675 degrees Celsius or 650-675 degrees Celsius or 600-650 degrees Celsius or 625-650 degrees Celsius or 600-625 degrees Celsius; Pressure is 0-4 megapascals, for example, 0.01-4 megapascals or 0.02-4 megapascals or 0-0.5 megapascals; Volumetric space velocity per hour of exhaust gas is 100-50000 per hour or 200-20000 per hour; And / or, ideally, in combustion gases, the SOx content is 0.001-0.5% by volume, the NOx content is 0.001-0.3% by volume; or the volumetric ratio of SOx and NOx in combustion gases is 1-3000 µL / L, respectively, and the molar ratio of SOx to NOx is 0.5:1-2:1; and / or, ideally, the combustion gas is a combustion gas that contains specific amounts of SOx and NOx simultaneously, for example, combustion gases generated from catalytic regeneration in catalytic cracking; desirable.Exposure to combustion gases generated by catalytic regeneration in catalytic cracking is carried out in a designated combustion gas pathway after the catalytic cracking cyclone separator and / or after the CO incinerator.