Method for preparing polymers containing aldehyde functional groups.
Patent Information
- Application Number
- TH2401002529
- Authority / Receiving Office
- TH · TH
- Patent Type
- Applications
- Current Assignee / Owner
- Priority Date
- 2021-10-22
- Filing Date
- 2022-10-22
- Publication Date
- 2026-11-16
Abstract
Claims
DEPCT67 18 / 07 / 2567 1. A method for obtaining GPAM which includes: (a) the inclusion of at least polyacrylamide and glyoxal to obtain a reaction solution, and (b) termination of the reaction by adjusting the pH of the reaction solution to a range from approximately 2 to approximately 6 to obtain such GPAM, where the progress of the reaction is monitored by measuring the viscosity of the reaction solution using an online viscometer.
2. A method according to claim 1 where such GPAM has a weight-average molecular weight from approximately 10,000 g / mol to 10,000,000 g / mol.
3. A method according to any of the preceding claims where such GPAM has a glyoxal to acrylamide (G / A ratio) of approximately 0.05:1 to approximately 20:
1.
4. A method according to any of the preceding claims where the progress of such reaction is monitored. Monitoring is performed by continuously measuring the viscosity of the solution of the reaction, with the selection of feedback control.
5. Methods in accordance with any prior claim to which the online viscometer is included: (a)The transducer assembly which comprises: (i) at least one flow tube inserted into the delivery tube, such flow tube has a cavity that guides the reaction solution and such flow tube is clamped at the inlet and outlet ends so that it can vibrate; (ii) an electromechanical excitation arrangement; and (iii) a sensor arrangement; and (b) the electronic system of the meter.
6. The method according to any of the preceding claims in which the reaction is terminated when the viscosity of the reaction solution, compared to its initial viscosity, has increased by more than 100%.
7. The method of claim 1 in which the pH of the reaction in step (a) is maintained in the range from approximately 8 to approximately 9 by the addition of a corrosive solution, which is selectively further diluted with water.
8. The method of claim 1 in which in step (b) the termination of the reaction is comprised of:
9. Addition of organic acid to the solution of reaction 10. Any method under the preceding claim where such GPAM has a glyoxal to acrylamide (G / A ratio) in the range of approximately 0.4:1 to approximately 20:1.
11. Method of Reputation 10 where the polyacrylamide is an acrylamide / DADMAC copolymer.
12. Method of Reputation 10 where the copolymer is approximately 1-30% by mole of DADMAC and approximately 70-99% by mole of acrylamide.
13. Method according to any preceding Reputation where the viscometer is an open-flow tube viscometer.
14. Method according to any preceding Reputation 1 where the viscometer comprises a measurement system with at least one measuring tube which, in the measurement operation, is filled with the reaction solution or through which the reaction solution flows, and which has at least one activating section of the tube. To perform oscillations, a triggering system is used to excite at least two desired oscillation modes at different frequencies, at which at least one section of the tube is excited to perform oscillations, specifically resonant oscillations; a sensing system is shaped in such a way that it determines the frequency and damping, specifically the frequency, amplitude, and damping of the resulting oscillations of at least one section of the tube.The part that is triggered to perform the oscillation of one of the desired oscillation modes for the desired oscillation mode that is triggered in the measurement operation in each case, and the evaluation system, which is characterized in such a way that such evaluation system determines the shear rate and the measured viscosity value based on the calibration data stored in memory for each desired oscillation mode that is triggered in the measurement operation in each case, based on the frequency and damping determined by the trigger, specifically the frequency, amplitude and damping of the resulting oscillation where the measured viscosity value corresponds to the dynamic viscosity of the GPAM at a constant shear rate corresponding to the shear rate value 14. The method of fabricating the aldehyde functional polymer, which includes: (a) combining at least one polymer containing at least one amide or amino group and an aldehyde to obtain a reaction solution, and (b) terminating the reaction by adjusting the pH of the reaction solution to a value in the range from approximately 2 to approximately 6.To obtain the aldehyde-functionalized polymer, the progress of the reaction is monitored by measuring the viscosity of the reaction solution using an online viscometer.
15. The method of claim 14, in which the aldehyde is selected from formaldehyde, paraformaldehyde, and glutaraldehyde.
16. The method of claim 15, in which the method is further incorporated by contacting the aldehyde-functionalized polymer with a fibrous slurry or with a sheet of paper.
17. A GPAM composition consisting of any GPAM prepared according to the preceding claims, in which the GPAM has a weight-average molecular weight from approximately 10,000 g / mol to 10,000,000 g / mol and in which the GPAM has a glyoxal to acrylamide (G / A ratio) in the range of approximately 0.05:1 to approximately 20:1.