A process for producing heat-modified supported aluminoxane in an aliphatic solvent using solid aluminoxane.
Patent Information
- Application Number
- TH2401006036
- Authority / Receiving Office
- TH · TH
- Patent Type
- Applications
- Current Assignee / Owner
- Priority Date
- 2022-03-17
- Filing Date
- 2022-12-15
- Publication Date
- 2026-11-16
Abstract
Claims
DEPCT68 14 / 11 / 2567 1. The process for producing supported single-site catalysts consists of: (a) the formation of a slurry consisting of an inorganic oxide support, an organic solvent, and a solid aluminoxane activator; (b) the holding of the slurry at approximately 100°C to approximately 200°C for a period of approximately 0.5 to approximately 10 hours to obtain a supported aluminoxane slurry; and (c) the contact of the supported aluminoxane slurry with the single-site catalyst components to obtain the supported single-site catalyst; in which the organic solvent consists of one or more branched-chain aliphatic compounds with a boiling point of approximately 100°C to 2 ...
1. 100 degrees Celsius or higher and present in an amount equal to approximately 50 wt.% or more in relative proportion to the total amount of organic solvent.
2.
2.
3. The process under claim 1, in which the slurry in step (a) does not contain any aromatic compounds. 3.Any process under Reputation 1-2, where the organic solvent, consisting of one or more branched-chain aliphatic compounds, is incorporated with isoparaffins.
4. Any process under Reputation 1-3, where the organic solvent, consisting of one or more branched-chain aliphatic compounds, is incorporated with one or more C7-C12 isoparaffins.
5. Any process under Reputation 4, where one or more C7-C12 isoparaffins are selected from one or more C7-C10 isoparaffins and C9-C12 isoparaffins.
6. Any process under Reputation 1-5, where the organic solvent is incorporated with mineral oil.
7. Any process under Reputation 1-6, where an aluminoxane activator is incorporated.
8. Solid compounded with methyl aluminoxane.
9. Process according to claim 7, in which a solid aluminoxane activator is obtained by solvent removal precipitation, heating and solvent removal distillation and trimethylaluminum, or chemical conditioning.
10. One of the processes under claims 7-8, where the solid aluminoxane activator has a total aluminum content ranging from approximately 35 to approximately 50 wt%, based on the total weight of the solid aluminoxane activator.
11. One of the processes under claims 1-9, which includes the cooling of the supported aluminoxane slurry to approximately 50 °C or lower before contact of the supported aluminoxane slurry with the singlesite catalyst component.
12. One of the processes under claims 1-10, which includes the cooling of the supported aluminoxane slurry to approximately 25 °C. Prior to contact of the aluminoxane slurry supported by the singlesite catalytic component 12. The process according to one of the claims 1-11, where the slurry temperature at step (b) is maintained from approximately 115°C to approximately 155°C 13.
14. Any process under Reputation 1-13, where the organic solvent is contained in an amount of approximately 50 wt.% or more of one non-aromatic organic compound with a boiling point higher than the maximum temperature reached by the slurry; 15. Any process under Reputation 1-14, where the organic solvent is contained in an amount of approximately 60 wt.% or more, approximately 70 wt.% or more, approximately 75 wt.% or more, approximately 80 wt.% or more, approximately 90 wt.% or more, or approximately 95 wt.% or more; 16. Any process under Reputation 1-15, where the process is contained in an amount of approximately 50 wt.% or more of one non-aromatic organic compound with a boiling point higher than the maximum temperature reached by the slurry; By separating the supported aluminoxane from the organic solvent prior to the contact of the supported aluminoxane with the singlesite catalytic component.
17. One of the processes of claims 1-16, where the inorganic oxide support is composed of silica. 18.
19. Any process under Claims 17-18, where the inorganic oxide support contains approximately 50 wt.% or more of silica, approximately 60 wt.% or more, approximately 80 wt.% or more, approximately 90 wt.% or more, or approximately 99 wt.% or more of silica.
20. Any process under Claims 1-19, where the catalyst component...
21. Singlesite formulations of metallocene compounds.
22. Processes under claim 20, in which metallocene compounds are combined with scandium, titanium, zirconium, hafnium, vanadium, niobium, tantalum, manganese, rhenium, iron, ruthenium, osmium, cobalt, rhodium, iridium, or nickel.
23. Processes under claim 21, in which metallocene compounds are combined with titanium, zirconium, or hafnium.
24. The process for producing supported singlesite catalysts consists of: (a) contact of the inorganic oxide support, organic solvent, and solid aluminoxane activator at temperatures from approximately 0°C to approximately 50°C to obtain a slurry; (b) heating the slurry to temperatures from approximately 100°C to approximately 200°C over a period of approximately 0°C.(5 to approximately 10 hours to obtain a supported aluminoxane slurry; (c) cooling the slurry to a temperature from approximately 0 °C to approximately 50 °C; and (d) adding the singlesite catalyst component to the supported aluminoxane slurry to obtain a supported singlesite catalyst; where the organic solvent consists of one or more branched-chain aliphatic compounds with a boiling point of approximately 100 °C or higher and is present in an amount of approximately 50 wt.% or more of the total amount of organic solvent.
25. The process according to claim 24, where the inorganic oxide support is heat-conditioned.
26. The process according to either claim 24-25, where the supported singlesite catalyst has a total residual solvent amount of less than approximately 50 wt.% and / or where the supported singlesite catalyst has a residual aromatic solvent amount. All of them are less than approximately 0.5 wt.% 27.
28. The process under one of the claims 24–26, in addition to the contact of a supported singlesite catalyst with an olefin monomer, yields polyolefins.
29. Polyolefins produced by the process under claim 27.
30. A supported singlesite catalyst produced by the process under one of the claims 1–27.
31. A slurry consisting of: an inorganic oxide support; an organic solvent consisting of one or more branched-chain aliphatic compounds with a boiling point of approximately 100 °C or higher, present in an amount of approximately 50 wt.% or more of the total amount of organic solvent; and a solid aluminoxane activator.
32. The process under claim 30, where the slurry contains less than approximately 50 wt.% of the total residual solvent and / or where the supported singlesite catalyst contains... The total amount of residual aromatic solvent is less than approximately 0.5 wt.%.