Abstract

DEPCT68 Method for the fabrication of molded objects of thermoplastic expansion beads, including crack filling and molding steps. Each expansion bead (2) to be used in the crack filling step is column-shaped and each bead has one or more defects of one or two types, the defects of which are selected from a group consisting of through holes and grooves. The molding cavity (12) of the mold (1) has a first section (121) whose length in the opening / closing direction of the mold (1) is greater than the average length LA and a second section (122) whose length is shorter than the average length LA. In the crack filling step, the difference P2max-P1min between the minimum P1min of the compression rate of the first section (121) and the maximum P2max of the compression rate of the second section (122) is 5% or more and 100% or less.
Need to check novelty before this filing date? Find Prior Art

Claims

DEPCT68 1. Method for the production of molded objects from thermoplastic expansion beads, consisting of: the crack filling step of filling the cracked cavity of the mold with each thermoplastic expansion bead layer, and then sealing the mold completely; and the molding step of supplying a heated medium into the molding cavity after the completion of the crack filling step, thus fusing the expansion beads together, where the molding cavity is in a sealed state, including the first part which is the length in the direction In the first phase, where the length in the opening / closing direction of the mold is longer than the average length LA, which is represented by formula (1) below, and in the second phase where the length in the opening / closing direction of the mold is shorter than the average length LA, the difference P2max - P1min between the minimum P1min of the compression rate in the first phase, which is represented by formula (2) below, and the maximum P2max of the compression rate in the second phase, which is represented by formula (3) below, in the crack filling phase is 5% or more and 100% or less,The average length (LA) of the molding crucible in the opening / closing direction is 10 mm or more; each expanding bead has a columnar shape; and each bead has at least one or two types of defects selected from a group consisting of through holes inserted internally into the expanding bead in its axial direction and grooves extending axially on the surrounding surface. Expansion beads, and in the surface cut obtained by cutting the expansion beads at the center in the axial direction along a plane perpendicular to the axial direction, the ratio Ca / A of the average cross-sectional area Ca per defective area to the average cross-sectional area A of the expansion beads is 0.01 or more and 0.20 or less, and the ratio Ct / A of the total cross-sectional area Ct of the defective area to the average cross-sectional area A of the expansion beads is 0.02 or more and 0.20 or less: LA = V / S ... (1) P1min = (delta / L1max) x 100 ... (2) P2max = (delta / L2min) x 100 ... (3) (in formula (1),V represents the capacity (unit: cubic millimeters) of the molding cavity in the state in which the mold is closed, and S represents the area which is protruded (unit: square millimeters) of the molding cavity when protruding in the opening / closing direction of the mold, in formulas (2) and (3), Delta represents the dimension (unit: millimeters) of the crack gap in the crack filling step, in formula (2), L1max represents the maximum value (unit: millimeters) of the length of the first segment in the opening / closing direction, which is measured in the state in which the mold is closed, and in formula (3), L2min represents the minimum value (unit: millimeters) of the length of the second segment in the opening / closing direction, which is measured in the state in which the mold is closed).

2. Method for the production of molded objects of thermoplastic resin expansion beads according to claim 1, where the ratio of the apparent density of the expansion beads to the density The total value of the expanding beads is greater than 1.6 and less than 2.0 or less.

3. Methods for the manufacture of molded objects from thermoplastic resin expanding beads according to Reservation 1 or 2.Where the maximum P2max value of the compression rate in the second section during the crack filling step is 25% or more and 150% or less.

4. Method for the manufacture of molded objects of thermoplastic resin expansion beads according to one of the claims 1 to 3, where the maximum L1max value of the length of the first section in the opening / closing direction of the mold is 55 mm or more.

5. Method for the manufacture of molded objects of thermoplastic resin expansion beads according to one of the claims 1 to 4, where in the molded object of thermoplastic resin expansion beads obtained by the manufacturing method, the melt adhesion rate of the section corresponding to the first section is 70% or more.

6. Method for the manufacture of molded objects of thermoplastic resin expansion beads according to one of the claims 1 to 5,Where the void space of the molded object of thermoplastic resin expansion beads obtained by any of the manufacturing methods is 4% or more and 12% or less.

7. Any of the manufacturing methods for molded objects of thermoplastic resin expansion beads under any of the claims 1 through 6, where each expansion bead has one or more through holes as defects.

8. Any of the manufacturing methods for molded objects of thermoplastic resin expansion beads under any of the claims 1 through 7, where each expansion bead includes a foam layer and a melt adhesion enhancing layer covering the foam layer, the base resin of the foam layer is thermoplastic resin one, and the base resin of the melt adhesion enhancing layer is thermoplastic resin two.

9. Any of the manufacturing methods for molded objects of thermoplastic resin expansion beads under any of the claims 1 through 8,10. A method for fabricating molded objects of thermoplastic resin expansion beads according to one of the claims 1 through 9, where the thermoplastic resin comprising the foam layer is a random ethylene-propylene copolymer containing 0.5% by mass or more of ethylene and 3.5% by mass or less.

11. A method for fabricating molded objects of thermoplastic resin expansion beads according to one of the claims 1 through 10, where the bulk density of the expansion beads is 10 kg / m³ or more and 50 kg / m³ or less.