Glass fiber reinforced nylon materials that are halogen-free flame retardants, methods of preparation for such materials, and their use.

TH2501003063APending Publication Date: 2026-11-16ช่างไห่ จงเล่ย นิว แมทีเรียล ไซแอนซ์ โค แอลทีดี
View PDF 0 Cites 0 Cited by

Patent Information

Application Number
TH2501003063
Authority / Receiving Office
TH · TH
Patent Type
Applications
Current Assignee / Owner
Priority Date
2022-11-10
Filing Date
2023-06-30
Publication Date
2026-11-16
Patent Text Reader

Abstract

The disclosed DEPCT68 describes a glass fiber reinforced, halogen-free flame retardant nylon material and its preparation and use. This glass fiber reinforced, halogen-free flame retardant nylon material consists of 45–85 parts by weight of nylon, 10–55 parts by weight of glass fiber, 2–10 parts by weight of phosphate flame retardant, and a terminal ester modifier of acetyleneic acid.01-2 By weight, glass fibers and phosphate-based flame retardants were bonded together by adding a terminal acetylene acid ester modifier. This improves the wick performance in glass fiber-reinforced nylon materials and enhances the compatibility of nylon, glass fibers, and flame retardants. In this way, glass fiber-reinforced nylon materials with very good flame retardant properties can be obtained with relatively small amounts of phosphate-based flame retardants without affecting the mechanical properties of the glass fiber-reinforced nylon itself. Ultimately, halogen-free glass fiber-reinforced nylon materials with good flame retardant and mechanical properties are obtained.
Need to check novelty before this filing date? Find Prior Art

Claims

DEPCT68 1. Glass fiber reinforced nylon material with halogen-free flame retardant containing the following components in units by weight: nylon 45 - 85 p / w, glass fiber 10 - 55 p / w, phosphate flame retardant 2 - 10 p / w, and terminal alkynoate modifier 0.01 - 2 p / w.

2. Glass fiber reinforced nylon material with halogen-free flame retardant as per claim 1 where the phosphate flame retardant contains one or a combination of at least two of melamine phosphate, ammonium polyphosphate, or phosphate. or organic aluminum hypophosphite.

3. Glass fiber reinforced nylon material that is a halogen-free flame retardant under any of the claims 1 or 2, where the glass fiber is alkali-free.

4. Glass fiber reinforced nylon material that is a halogen-free flame retardant under any of the claims 1-3, where the raw material for the preparation of the terminal alkinoate modifier consists of alkinic acid and fatty alcohol. 5.Glass fiber reinforced nylon materials that are halogen-free flame retardants under any of the claims 1–4, where the alkinoic acid is desirablely combined with hexinoic acid and / or 10-undechinoic acid, and the fatty alcohol is desirablely combined with ethanol and / or propanol, and the terminal alkinoate modifier is prepared by the following methods, which include: reaction of the alkinoic acid and fatty alcohol in a solvent, extraction and separation to obtain the terminal alkinoate modifier, and, desirablely, the solvent is concentrated sulfuric acid.

6. Glass fiber reinforced nylon materials that are halogen-free flame retardants under any of the claims 1–5, where the glass fiber reinforced nylon materials that are halogen-free flame retardants are desirablely combined with nano-calcium borate. The amount of nano-calcium borate in glass fiber reinforced nylon material with a halogen-free flame retardant is 1–5 parts by weight. 7.Glass fiber reinforced nylon materials that are halogen-free flame retardant as provided in any of the claims 1–6, where the glass fiber reinforced nylon materials that are halogen-free flame retardant are desirablely incorporated, or combined with at least two, of any tenderizing agent, coupling agent, antioxidant or lubricant; the tenderizing agent is desirablely incorporated, or combined with at least two, of any methyl methacrylate-butadiene-styrene copolymer, ethylene-octeene elastomer branched by maleic anhydride, ethylene-butyl acrylate-glycidyl methacrylate copolymer, ethylene-methyl acrylate-glycidyl methacrylate copolymer, or methyl methacrylate-styrene-organosilicon copolymer. The coupling agent consists of one or a combination of at least two gamma-aminopropyltrimethoxysilane, gamma-aminopropyltriethoxysilane, gamma-glycidyloxypropyltrimethoxysilane, or gamma-glycidyloxypropyltriethoxysilane.Preferably, the antioxidant contains one or a combination of at least two esters of beta-(3,5-di-tert-butyl-4-hydroxyphenyl)propionate, n-octadecyl alcohol, 2,6-tributyl-4-methylphenol, bis(3,5-tributyl-4-hydroxyphenyl)thioether, triethylene glycol, bis-beta-(3-tert-butyl-4-hydroxy-5-methylphenyl)propionate, or N,N'-bis[3-(3,5-di-tert-butyl-4-hydroxyphenyl)propionyl]hexanediamine. Preferably, the lubricant contains one or a combination of at least two For example, pentaerythol stearate, vinyl wax or silicone oil.

8. Glass fiber reinforced nylon materials that are halogen-free flame retardant under claim 7, where the amount of stiffener in the glass fiber reinforced nylon materials that are halogen-free flame retardant is desirablely 0.1 – 1 part by weight, and the amount of coupling agent in the glass fiber reinforced nylon materials that are halogen-free flame retardant is desirablely 0.5 – 5 parts by weight.The amount of antioxidant in glass fiber reinforced nylon materials with halogen-free flame retardant is 0.01 – 5 p / w. Desirably, the amount of lubricant in glass fiber reinforced nylon materials with halogen-free flame retardant is 0.01 – 5 p / w.

9. The preparation method for any one of the claims 1 – 8 for glass fiber reinforced nylon materials shall consist of the following steps: (1) mixing of glass fibers and terminal alkynoate modifiers in a solvent to obtain modified glass fibers; and (2) mixing of the modified glass fibers obtained in step (1), nylon, an alternative phosphate flame retardant, an alternative nano-calcium borate, an alternative toughener, an alternative coupling agent, an alternative antioxidant, and an alternative lubricant, and extrusion. Melted to obtain a glass fiber reinforced, flame-retardant, halogen-free nylon material.

10. Preparation method according to claim 9 in which the solvent in step (1) is composed of an alkane solvent.

11. Preparation methods under claims 9 or 10 where mixing in step (1) is carried out at a temperature of 50 – 80 °C; it is desirable that mixing in step (1) be carried out for a duration of 1 – 4 hours.

12. Preparation methods under claims 9 – 11 where mixing in step (1) is carried out in a mixer; it is desirable that the mixer speed is 300 – 700 rpm.

13. Preparation methods under claims 9 – 12 where mixing and extrusion in step (2) are carried out in a screw extruder; it is desirable that mixing and extrusion in step (2) be carried out at a temperature of 245 – 275 °C; it is desirable that mixing and extrusion are carried out in a screw extruder. The speed of the screw extruder is 400 – 600 rpm.

14. The use of glass fiber reinforced nylon material that is halogen-free and flammable, as per any of claims 1 – 8, in motor vehicles is desirable.Applications include use in peripheral components of a vehicle's engine or in components of a vehicle's electronic control system.