Laminated packaging materials; methods for manufacturing laminated packaging materials and packaging containers incorporating laminated packaging materials.
Patent Information
- Application Number
- TH2501003304
- Authority / Receiving Office
- TH · TH
- Patent Type
- Applications
- Current Assignee / Owner
- Filing Date
- 2023-07-20
- Publication Date
- 2026-11-16
Abstract
Claims
DEPCT68 13 / 08 / 2568 1. Laminated packaging material for the packaging of liquid food, consisting of an aggregate layer (11; 21) of paper, cardboard or other cellulose-based material; a first outermost heat-sealed liquid-tight layer (12; 22) composed of a thermoplastic polymer; a barrier layer or barrier multilayer (15; 24) composed of at least one gas barrier material arranged on the inner side opposite the aggregate layer (11; 21); and a second innermost heat-sealed liquid-tight layer (15) on the inner side of the barrier layer or barrier multilayer; and a second innermost heat-sealed liquid-tight layer (14; 26) directed toward the inside of the container to be formed from the packaging material, where the first outermost heat-sealed liquid-tight layer The second innermost liquid barrier (14; 26) is a pre-fabricated polyethylene film (14; 26) which isPre-fabricated polyethylene films are manufactured using linear low-density polyethylene (LLDPE) of 60 to 100 percent, with 80 to 100 percent LLDPE being desirable, and even more desirable with 90 to 100 percent LLDPE. The pre-fabricated polyethylene films should also possess the following characteristics: - A total thickness of 15 to 25 micrometers - An elastic modulus of at least 400 MPa in MD and at least 500 MPa in CD as measured by ASTM D 882-02 (2018) with an initial strain rate of 0.1 mm / (mm*min) - A tensile strength greater than 40 MPa, preferably greater than 50 MPa in MD and greater than 100 MPa in CD as measured by ASTM D638M-14 (2017) with a crosshead rate of 200 mm / min - Elongation at break less than 350 MPa. Percentage in MD and less than 100 percent in CD as measured by ASTM D638M-14 (2017) at a crosshead rate of 200 mm / min - Initial sealing temperature, SIT, from 80 to 100 °C as defined by ASTM F1921 (2018) at 2 N -Maximum hot bond strength is greater than 7 Nm as measured by ASTM F1921 (2018) and - penetration resistance of 10 Nm or higher. As measured by ASTM F1306-16 (2016) at a crosshead speed of 500 mm / min.
2. Laminated packaging material as claimed in Reputation 1 where the pre-fabricated polyethylene film (14; 26) has a melt flow ratio / melt flow index (MFR / MFI) of 2 to 5 g / 10 min at 2.16 kg 190 °C as measured by ASTM D1238 or ISO 1133.
3. Laminated packaging material as claimed in Reputation 1 or Reputation 2 where the pre-fabricated polyethylene film (14; 26) contains 60 to 100 percent m-LLDPE, preferably 80 to 100 percent m-LLDPE, more preferably 90 to 100 percent m-LLDPE.
4. Laminated packaging materials as claimed under any of the preceding claims, in which a prefabricated polyethylene film (14; 26) has a core layer composed of m-LLDPE.More than 60 percent by weight, a first “skin” layer on one side of the core layer, which is also incorporated with LLDPE, preferably m-LLDPE, and which is also adapted for heat sealing of the film, more than the polyethylene of the core layer, and alternatively, a pre-fabricated polyethylene film with a second skin layer on the other side of the core layer.
5. Laminated packaging material as claimed in one of the preceding claims, where the pre-fabricated polyethylene film (14; 26) has a total thickness of 16 to 23 micrometers, e.g., from 16 to 20 micrometers.
6. Laminated packaging material as claimed in claim 4, where the core layer of the film Pre-fabricated polyethylene (14; 26) with a thickness of 10 to 16 micrometers, e.g., from 10 to 14 micrometers.
7. Laminated packaging materials as claimed under any of the claims 4-6 where the thickness of the first and alternative second layers is from 1 to 3, e.g., from 2 to 3 micrometers. 8.Laminated packaging materials as claimed under any of the pre-existing claims where the pre-fabricated polyethylene film (14; 26) has a sealing initial temperature (SIT) of 80 to 95 °C, i.e. 80 to 90 °C as defined by ASTM F1921 (2018) at 2 N.
9. Laminated packaging materials as claimed under any of the pre-existing claims where the pre-fabricated polyethylene film (14; 26) has a maximum hot bond strength greater than 8 N as measured by ASTM F1921 (2018).
10. Laminated packaging materials as claimed under any of the pre-existing claims where the pre-fabricated polyethylene film (14; 26) has a puncture resistance of 10 N or greater. As measured by ASTM F1306-16 (2016) at a crosshead speed of 500 mm / min and having an elongation at the hole (i.e. at maximum load) of less than 10 mm.
11. Laminated packaging material as claimed in any of the preceding claims, where12. Laminated packaging material as claimed in claim 11, where the coatings (15b-15d) consist of a gas-blocking polymer and / or a vapor deposition coating of a gas-blocking material of choice from metal oxides.
13. Laminated packaging materials as claimed in any of the preceding claims, in which a barrier layer or barrier multilayer (14; 26) is laminated to an aggregate layer (11; 21) by means of one (16; 25) bonding layer of one or more polymers.
14. Laminated packaging materials as claimed in any of the preceding claims, in which a prefabricated polyethylene film (14; 26) is laminated to a barrier layer or barrier multilayer (15; 24).
15. Laminated packaging material as claimed in any of the preceding claims, in which a pre-fabricated polyethylene film (14; 26) has a stretch ratio of 5 to 7 in the machine direction (MD) and from 7 to 10 in the transverse direction, CD.
16. Laminated packaging material as claimed in any of the preceding claims, consisting of an aggregate layer of cardboard (11) of standard weight from 100 to 520 g / m², e.g. from 200 to 300 g / m², and a multi-layer barrier (15) in which the multi-layer barrier (15) is composed of a paper substrate (15a) on which at least one coating (15b-15d) of a gas barrier material is applied. The desirable thickness range is from 2 to 5000 nanometers (5 micrometers) in order to provide more environmentally sustainable and recyclable packaging materials.17.Laminated packaging materials as claimed in any of the preceding claims, consisting of an aggregate layer (21) of standard weight from 50 to 140 g / m², e.g. from 70 to 120 g / m², e.g. from 70 to 110 g / m², and a barrier layer (24) of aluminum foil, for the purpose of manufacturing pouch packaging.
18. Methods for manufacturing laminated packaging materials (10; 20) as defined in any of the preceding claims, consisting of steps in any order of a) lamination (30b, 35b) of continuous fibers of aggregate layers (11; 21; 34b) of paper, cardboard or other material with cellulose as the main component to the outer side of continuous fibers of the barrier layer or multi-layered barrier layer (15; 24; 31b) consisting of b) Lamination (35c, 37c) of a continuous strand of pre-fabricated inner polyethylene film (14; 26; 38c)This is a heat-sealed, liquid-tightening second innermost layer on the opposite side of the barrier layer fibers or multi-layered barrier (15; 24; 31b), for example, by melt extrusion lamination with a second bonding layer in between (17a, 17b; 27,28; 36c) of bonding polymers, and c) extruded coating (320, 34c), a heat-sealed, liquid-tightening first outermost layer (12; 22; 33c) on the outer side of the aggregate layer (11; 21; 31c; 34b), where a pre-fabricated polyethylene film (14; 26; 38c) is cast and oriented. A biaxial composite material consisting of 60 to 100 percent linear low-density polyethylene (LLDPE), preferably 80 to 100 percent LLDPE, and even more desirable, 90 to 100 percent LLDPE, should be used. The pre-fabricated polyethylene film should also possess – a total thickness of 15 to 25 micrometers – an elastic modulus of at least 400 megapascals in MD and at least 500 megapascals in CD, as measured by ASTM D 882-02 (2018).At a crosshead rate of 10 mm / min - tensile strength greater than 40 MPa, preferably greater than 50 MPa in MD and greater than 100 in CD, as measured by ASTM D638M-14 (2017) at a crosshead rate of 200 mm / min - elongation at break less than 350 percent in MD and less than 100 percent in CD, as measured by ASTM D638M-14 (2017) at a crosshead rate of 200 mm / min - initial sealing temperature, SIT, from 80 to 100 °C, as defined by ASTM F1921 (2018) at 2 N - maximum hot bond strength greater than 7 N, as measured by ASTM F1921 (2018) and - puncture resistance of 10 N or greater. As measured by ASTM F1306-16 (2016) at a crosshead speed of 500 mm / min.
19. The method as claimed in claim 18, where procedure a) is carried out by wet application of an aqueous dispersion of the adhesive composition, which includes a polymer bonding agent, to the fibers of the aggregate layer (11; 21) or to the fibers of the barrier layer or multilayer barriers (15; 24).At a quantity of 1 to 5 g / m² of dry weight and the pressing of the two fibers together as they are passed through the laminating rollers without the need for forced drying.
20. Packaging containers (50a; 50b; 50c; 50d) for the packaging of oxygen-sensitive food products, such as semi-liquid, viscous, watery food products, which are incorporated with laminated packaging materials (10; 20) as defined in any of the claims 1-17.