A biaxially aligned, metallic polypropylene film with high sealing strength and strong barrier forces for airtight packaging.

TH2501003904APending Publication Date: 2026-11-09พีที อินโดโพลี สวาคาร์ซา อินดัสตรี ทีบีเค
0 Cites 0 Cited by

Patent Information

Application Number
TH2501003904
Authority / Receiving Office
TH · TH
Patent Type
Applications
Current Assignee / Owner
Priority Date
2025-01-15
Filing Date
2025-06-13
Publication Date
2026-11-09
Patent Text Reader

Abstract

This invention relates to a high-bonding, biaxially aligned, metallized polypropylene (mBOPP) film exhibiting enhanced vapor barrier and oxygen barrier properties. The film product comprises six layers: a core layer C, layer T1 on the first side of layer C, layer B on top of layer T1, layer M on top of layer B, layer T2 on the second side of layer C, and layer A on the bottom of layer T2. Layer C consists of polypropylene homopolymer and polypropylene elastic material; layer T1 consists of polypropylene transplanted with maleic anhydrate; layer B consists of ethylene vinyl alcohol; and layer M consists of aluminum produced by vacuum metallization. Layer T2 consists of polypropylene copolymer, and layer A consists of polypropylene copolymer and antiblocking additives to achieve a COF of less than 0.8 and a SIT of less than 120°C. The mBOPP film will have a bond strength of greater than 1200 g / 25 mm and a modulus of elasticity of less than 1300 N / mm².WVTR less than 0.3 g / m² / day and O2TR less than 0.3 cc / m² / day, total film thickness of 15 to 50 micrometers, and density of 0.55 to 0.95 g / cm³.
Need to check novelty before this filing date? Find Prior Art

Claims

1. Biaxially aligned metallized polypropylene film (mBOPP) comprising: a. Core layer C, composed of polypropylene homopolymer with a melt flow index (MFI) of 2 to 4 g / 10 min and an isotacetic index greater than 90%, accounting for 50 to 100% by weight, and elastic polypropylene with a melt flow index (MFI) of 4 to 10 g / 10 min; modulus of bending less than 500 Mpa, accounting for 0 to 50% by weight; b. Intermediate layer T1, located on the first side of core layer C, comprising polypropylene transplanted with maleic anhydrate with a melt flow index (MFI) of 2 to 8 g / 10 min; vecatalysis softening point between 100 and 160°C, accounting for 100% by weight; C. Layer B, which is on the top surface layer T1 and consists of ethylene vinyl alcohol (EVOH) with an ethylene content of 35 to 50%, which is 100% by weight; the thickness of this layer is between 0.2 and 1.5 micrometers; d.e. Layer M, located on the top surface of layer T1, consists of aluminum with a purity of over 99.5% obtained through vacuum metallurgy of aluminum, with a thickness of 100 to 400 angstroms (0.01 to 0.04 µm); e. The intermediate layer T2, located on the second side of the core layer C, consists of polypropylene copolymer with a molten flow index (MFI) of 4 to 10 g / 10 min; melting point between 70 and 110 °C, representing 100% by weight, with a thickness of 2 to 8 µm; f. Layer A, located on the bottom of layer T2, consists of polypropylene copolymer with a molten flow index (MFI) of 4 to 10 g / 10 min; melting point between 70 and 110 °C, representing 98.0 to 99.8% by weight; and antiblocking additives amounting to 0.2 to 2.0% by weight; the thickness of this layer will be between 2 and 4 micrometers; it has a coefficient of friction (COF) less than 0.8; where the film has a bonding strength greater than 1200 g / 25 mm, and an elastic modulus less than 1300 N / mm² (N / mm²).

1. mBOPP film as specified in Claim 1, where the C core layer consists of calcium carbonate (CaCO3) particles of 1 to 5 micrometers in size, representing 2 to 20% by weight.

3. mBOPP film as specified in Claim 1, where the C core layer consists of titanium dioxide (TiO2) particles of 1 to 5 micrometers in size, representing 2 to 20% by weight.

4. mBOPP film as specified in Claim 1, where the C core layer consists of calcium carbonate (CaCO3) particles of 1 to 5 micrometers in size, representing 2 to 20% by weight, and titanium dioxide (TiO2) particles of 1 to 5 micrometers in size. Up to 5 micrometers, which accounts for 2 to 20% by weight.mBOPP film as specified in Claim 1, whereby the T1 intermediate layer is comprised of polypropylene transplanted with maleic anhydrate having a melt flow index (MFI) of 2 to 8 g / 10 min; VC softening point between 100 and 160 °C, accounting for 40 to 80% by weight, and polypropylene homopolymer having a melt flow index of 2 to 4 g / 10 min; isotactic index greater than 90%, accounting for 20 to 60% by weight, where the thickness of this layer is between 0.5 and 2.0 µm.

6. mBOPP film as specified in Claim 1, whereby the B layer is comprised of an aromatic ring copolyamide selected from amorphous or crystalline copolyamides or a combination of these, with an transition temperature of 100 to 160 °C, accounting for 40 to 80% by weight. The glassy state occurs between 80 and 130 degrees Celsius, representing 100% by weight, with the thickness of this layer between 0.2 and 1.5 micrometers.The mBOPP film as described in Claim 1, where the intermediate layer T2, shall consist of polypropylene terpolymer with a melt flow index (MFI) of 4 to 8 g / 10 min, accounting for 50% to 90% by weight, and polypropylene elastic material with a melt flow index (MFI) of 4 to 10 g / 10 min; modulus of bending less than 500 Mpa, accounting for 10% to 50% by weight, with the thickness of this layer being between 2 and 8 µm.

8. The mBOPP film as described in Claim 1, where layer A, shall consist of polypropylene terpolymer with a melt flow index (MFI) of 4 to 8 g / 10 min, accounting for 50.0 to 90.0% by weight; polypropylene elastic material with a melt flow index (MFI) of 4 to 10 g / 10 min; The modulus of bending is less than 500 MPa, representing 10 to 49.8% by weight, and anti-blocking additives are present at 0.2 to 2.0% by weight; the layer thickness is between 2 and 4 micrometers; the sealing strength is greater than 1200 g / 25 mm; and the coefficient of friction (COF) is less than 0.8.mBOPP film as specified in Reputation 7 or 8, where the polypropylene terpolymer is a carbon chain monomer with 3 to 20% total comomomers, and the polypropylene elastic material is a carbon chain monomer with 3 to 20% total comomomers; 10. mBOPP film as specified in Reputation 1 or 8, where the sealing strength is measured at 130 °C; the set time is between 0.05 and 2 seconds; the pressure is greater than 10 N / cm²; 11. mBOPP film as specified in Reputation 1 or 8, where the initial sealing temperature (SIT) is lower than 120 °C; 12. mBOPP film as specified in Reputation 1 through 11, where the density is 0.55 to 0.95 g / cm³; The total film thickness is 15 to 50 micrometers.