Steel plates, components, and methods for manufacturing them.

TH2501004900APending Publication Date: 2026-11-09JFE STEEL CORP
View PDF 0 Cites 0 Cited by

Patent Information

Application Number
TH2501004900
Authority / Receiving Office
TH · TH
Patent Type
Applications
Current Assignee / Owner
Priority Date
2023-01-30
Filing Date
2024-01-25
Publication Date
2026-11-09
Patent Text Reader

Abstract

DEPCT69 21 / 10 / 2568 provided steel plates and components with high strength, excellent bending and formability, and excellent slow-crack properties, and methods for manufacturing such components. The steel plates have a chemical composition with the following elements in % by mass: C: not less than 0.15% and not more than 0.45%, Si: not more than 0.3% and not more than 2.0%, Mn: not less than 1.7% and not more than 4.0%, P: not more than 0.10%, S: not more than 0.01%, soluble Al: not more than 0.50%, N: not more than 0.010%, and B: not less than 0.0008% and not more than 0.00%.0100% with the remainder being Fe and unintended impurities, where the steel plate has a microstructure of steel in which the ratio of area of ​​martensite to the total microstructure is not less than 85% and not less than 95%, and the ratio of area of ​​residual austenite to the total microstructure is not less than 5% and not more than 15%, and where the density of number A of the precipitate with an equivalent circle diameter of 500 nm or more follows the formula A (number / sq mm) less than or equal to 8.5 x 10⁵ x [B].
Need to check novelty before this filing date? Find Prior Art

Claims

DEPCT69 21 / 10 / 2568 1. Steel plate with a chemical composition containing the following elements in % by mass: C: not less than 0.15% and not more than 0.45%; Si: not less than 0.3% and not more than 2.0%; Mn: not less than 1.7% and not more than 4.0%; P: not more than 0.10%; S: not more than 0.01%; Soluble Al: not more than 0.50%; N: not more than 0.010%; and B: not less than 0.0008% and not more than 0.0100%, with the remainder being Fe and unintended impurities, where the steel plate has a steel microstructure in which the area ratio of Martensite to total microstructure is not less than 85% and not less than 95% and the ratio of residual austenite area to total microstructure is not less than 5% and not more than 15% and where the density of number A of sediment with equivalent circle diameter of 500 nm or more follows the following formula (1), A (number / sq mm) is less than or equal to 8.5 x 10⁵ x [B] formula (1), where [B] represents the quantity (% by mass) of B.

2. Steel plate according to claim 1.Whereas the chemical composition is further included as a percentage by mass with one or more elements selected from the following: Cu: not more than 1.00%, Cr: not more than 1.00%, Nb: not more than 0.10%, Ti: not more than 0.10%, V: not more than 0.50%, Mo: not more than 0.50%, Ni: not more than 1.00%, Sb: not more than 0.10%, Sn: not more than 0.10%, As: not more than 0.10%, Ta: not more than 0.10%, Ca: not more than 0.020%, Mg: not more than 0.020%, Zn: not more than 0.020%, Co: not more than 0.020%, Zr: not more than 0.020%, W: not more than 0.020%, and REM: not more than 0.020%.

3. Steel plates according to claim 1 or 2 with a coating on the surface of the steel plate.

4. Components using steel plates as per one of the claims in Treaties 1 through 3.

5. Method of manufacturing steel plates which includes the holding of flat steel billets with the chemical composition as per Treaty 1 or 2 at a heating and holding temperature of 1100°C or higher for 30 minutes or more, followed by hot rolling of the billets under specified time conditions.Holding for no less than 20 seconds and no more than 150 seconds at 900 to 1000 degrees Celsius, and surface finishing rolling temperature of 850 degrees Celsius or higher. Cooling of the rolled steel at an average cooling rate of 40 degrees Celsius / second or more in the range from surface finishing rolling temperature to 650 degrees Celsius. Then, coiling the rolled steel at a coiling temperature of 650 degrees Celsius or lower to obtain hot-rolled steel sheets. The hot-rolled steel sheets are then subjected to cold rolling with a rolling reduction of 40% or more to obtain cold-rolled steel sheets. The cold-rolled steel sheets are then subjected to continuous annealing by heating the cold-rolled steel sheets from 400 degrees Celsius to annealing temperatures of 830 to 950 degrees Celsius at an average heating rate of 1.0 degree Celsius / second or more. The steel sheets are held at the annealing temperature for no more than 600 seconds, and then cooled from the annealing temperature to the stopping temperature. Cooling to a temperature of 150 to 250 degrees Celsius at an average cooling rate of...10 degrees Celsius / second or more. Heating the steel plate from the cool-down temperature to the reheating and holding temperature of 250 to 450 degrees Celsius, and then holding the steel plate at the reheating and holding temperature for 20 to 1500 seconds.

6. A method for manufacturing steel plates according to claim 5, where the continuously annealed steel plate is subjected to a surface coating.

7. A method for manufacturing assemblies which includes at least one forming and welding process for the steel plate according to claims 1 to 3.