Galvanized steel plate

TH2501004997APending Publication Date: 2026-11-02NIPPON STEEL CORPORATION
View PDF 0 Cites 0 Cited by

Patent Information

Application Number
TH2501004997
Authority / Receiving Office
TH · TH
Patent Type
Applications
Current Assignee / Owner
Priority Date
2023-02-09
Filing Date
2024-02-09
Publication Date
2026-11-02

Smart Images

  • Figure 2501004997_DRAWING_01
    Figure 2501004997_DRAWING_01
  • Figure 2501004997_DRAWING_02
    Figure 2501004997_DRAWING_02
  • Figure 2501004997_DRAWING_03
    Figure 2501004997_DRAWING_03
Patent Text Reader

Abstract

DEPCT69 21 / 10 / 2568 To improve further hydrogen dehydration while maintaining corrosion resistance after painting, the plated steel plates according to this invention include, on the surface of the steel plate, a plated layer which has a chemical composition with the following chemical elements in % by mass, Al: 0.50 to 5.00%, Mg: 0.50 to 3.00%, Fe: 0.01 to 15.00% and selected to also contain one or two or more elements chosen from groups consisting of elements A, B, C, D, E, F and G, with the remainder consisting of Zn and impurities, where in the surface structure in the plan view of the plated layer. The average area ratio of the eta phase with precipitated alpha, a metallic structure in which the alpha phase is precipitated within the main eta phase, ranges from 5 to 95%. When a 130 µm x 100 µm region of the plated layer surface is observed under an electron microscope, the total sum of crack lengths present in this region is 50 µm or more.
Need to check novelty before this filing date? Find Prior Art

Claims

DEPCT69 21 / 10 / 2568 1. Quenched steel plate composed of: On the surface of the steel plate, the quenching layer has a chemical composition of the following elements in % by mass: Al: 0.50 to 5.00%, Mg: 0.50 to 3.00%, Fe: 0.01 to 15.00%, and one or more elements selected from the following groups: A, B, C, D, E, F, and G, with the remainder consisting of Zn and impurities. In the surface structure in the plan view of the quenching layer surface, the average area ratio of the eta phase with precipitated alpha, which is the metallic structure in which the alpha phase is precipitated in the main eta phase, is 5 to 95%, and when the 130 µm x 100 µm region of the quenching layer surface is observed under an electron microscope. The total sum of the fracture lengths present in the region is 50 micrometers or more. [Group A]: One or two elements selected from the group containing Si: greater than 0% and 2.00% or less, and Ca: greater than 0% and 2.00%.0.5000% or less [Group B elements]: One or two or more elements selected from the group containing Sb: greater than 0% and 0.5000% or less, Pb: greater than 0% and 0.5000% or less, and Sr: greater than 0% and 0.5000% or less. [Group C elements]: One or two or more elements selected from the group containing Cu: greater than 0% and 1.0000% or less, Ti: greater than 0% and 1.0000% or less, Cr: greater than 0% and 1.0000% or less, Nb: greater than 0% and 1.0000% or less, Ni: greater than 0% and 1.0000% or less, Mn: greater than 0% and 1.0000% or less, Mo: greater than 0% and 1.0000% or less. Co: Greater than 0% and 1.0000% or less, and V: Greater than 0% and 1.0000% or less. [Group D elements]: One or two or more elements selected from the group consisting of Sn: Greater than 0% and 1.0000% or less, In: Greater than 0% and 1.0000% or less, and Bi: Greater than 0% and 1.0000%.0.0000% or less [Group E elements]: One or two or more elements selected from the group containing Zr: greater than 0% and 1.0000% or less, Ag: greater than 0% and 1.0000% or less, and Li: greater than 0% and 1.0000% or less. [Group F elements]: One or two or more elements selected from the group containing La: greater than 0% and 0.5000% or less, Ce: greater than 0% and 0.5000% or less, and Y: greater than 0% and 0.5000% or less. [Group G elements]: B: greater than 0% and 0.5000% or less.

2. Quenched steel plate according to claim 1 containing a chemical composition with group A elements.

3. Quenched steel plate according to claim 1 containing a chemical composition with group B elements.

4. Quenched steel plate according to claim 1.

5. Quenched steel plate according to claim 1, containing a chemical composition of group C elements.

6. Quenched steel plate according to claim 1, containing a chemical composition of group D elements.

7. Quenched steel plate according to claim 1, containing a chemical composition of group E elements.

8. Quenched steel plate according to claim 1, containing a chemical composition of group F elements.

9. Quenched steel plate according to claim 1, containing a chemical composition of group G elements.

10. Quenched steel plate according to any of claims 1 through 8, where the quenching layer contains 1.00 to 5.00% Al by mass and 1.00 to 3.00% Mg by mass.

11. Quenched steel plate according to claim 1, where the tensile strength of the steel plate is 980 MPa or higher.

12. Quenched steel plate according to claim 1, where the tensile strength of the steel plate is 1180 MPa or higher.

13. Quenched steel plate according to claim 1, where the average area ratio of the eta phase with alpha precipitation is 5 to 70%.

14. Quenched steel plate according to claim 1, where the average area ratio of the eta phase with alpha precipitation is 5. Up to 40%.