Hot-rolled thin steel sheets

TH2501005029APending Publication Date: 2026-11-16NIPPON STEEL CORPORATION
View PDF 0 Cites 0 Cited by

Patent Information

Application Number
TH2501005029
Authority / Receiving Office
TH · TH
Patent Type
Applications
Current Assignee / Owner
Priority Date
2023-01-31
Filing Date
2024-01-31
Publication Date
2026-11-16
Patent Text Reader

Abstract

DEPCT69 22 / 10 / 2568 Disclosure: Excellent hot-rolled thin steel sheets in terms of balance of strength, ductility, and hole expansion, and excellent impact properties. The hot-rolled thin steel sheets as currently disclosed have a predetermined chemical composition, a preceding austenite grain size of 25 μm or less, a GAM ratio greater than 0.6 degrees and less than 2.0 degrees of 50 percent or more and less than 100 percent, a GAM ratio of 0.6 degrees or less of 0 percent or more and less than 50 percent, a GAM ratio of 2.0 degrees or more of greater than 0 percent and 50 percent or less, and conform to a relationship of 1.7 less than or equal to LGr / LGt, and 1.20 Less than or equal to (LGr / LGt) / (LMr / LMt), where LGr is the average area of ​​the overhang length in the rolling direction of the preceding austenite grain, LGt is the average area of ​​the overhang length in the sheet thickness direction of the preceding austenite grain, LMr is the average area of ​​the overhang length in the rolling direction of the area with a GAM of 2.0 degrees or more, and LMt is the average area of ​​the overhang length in the sheet thickness direction of the area with a GAM of 2.0 degrees or more.
Need to check novelty before this filing date? Find Prior Art

Claims

DEPCT69 22 / 10 / 2568 1. Hot-rolled thin steel sheets composed of, in percentage by mass, the following: C: 0.045 percent or more and 0.120 percent or less, Si: 0 percent or more and 3.00 percent or less, Mn: 1.20 percent or more and 2.60 percent or less, Ti: 0.020 percent or more and 0.180 percent or less, Al: 0.010 percent or more and 0.400 percent or less, P: 0 percent or more and 0.080 percent or less, S: 0 percent or more and 0.0100 percent or less, N: 0 percent or more and 0.0050 percent or less, O: 0 percent or more and 0.010 percent or less, Nb: 0 percent or more and 0.100 percent or less, V: 0 percent or more and 1.000 percent or less. Percent or less, Cu: 0 percent or more and 1.000 percent or less, Cr: 0 percent or more and 2.0.000 percent or less, Mo: 0 percent or more and 3.000 percent or less, Ni: 0 percent or more and 0.500 percent or less, B: 0 percent or more and 0.0100 percent or less, Ca: 0 percent or more and 0.0500 percent or less, Mg: 0 percent or more and 0.050 percent or less, REM: 0 percent or more and 0.100 percent or less, Bi: 0 percent or more and 0.100 percent or less, Ta: 0 percent or more and 0.100 percent or less, Zr: 0 percent or more and 0.500 percent or less, Co: 0 percent or more and 3.000 percent or less, Zn: 0 percent or more and 0.200 percent or less, W: 0 percent or more and 0.200 percent or less, Sb: 0 percent or more and 0.500 percent or less. Percentage or less, As: 0 percent or more and 0.0.50 percent or less, Sn: 0 percent or more and 0.050 percent or less, and the remainder: Fe and impurities, where the preceding austenite grain size is 25 μm or less, the area ratio of regions with GAM greater than 0.6 degrees and less than 2.0 degrees is 50 percent or more and less than 100 percent, the area ratio of regions with GAM 0.6 degrees or less is 0 percent or more and less than 50 percent, the area ratio of regions with GAM 0.2 degrees or more is greater than 0 percent and 50 percent or less, and corresponds to the following relationships (1) and (2): 1.7 less than or equal to LGr / LGt ... (1) 1.20 less than or equal to (LGr / LGt) / (LMr / LMt) ... (2) where LGr: the mean of the area of ​​the lengths protruding in the rolling direction of the previous austenite grain; LGt: the mean of the area of ​​the lengths protruding in the sheet thickness direction of the previous austenite grain; LMr: the mean of the area of ​​the lengths protruding in the rolling direction of the area with GAM 2.0 degrees or more LMt: Average of the area of ​​the lengths overlapping in the sheet thickness direction of the area with a GAM of 2.0 degrees or more.

2. Hot-rolled thin steel sheet according to claim 1 where the ratio of the area of ​​the area with a GAM of 0.6 degrees or less is 0 percent or more and 45 percent or less.

3. Hot-rolled thin steel sheet according to claim 1 or 2 where the ratio of the area of ​​the area with a GAM of 2.0 degrees or more is greater than 0 percent and 20 percent or less.

4. Hot-rolled thin steel sheet according to any one of claims 1 through 3 where it conforms to the following (1-1) relationship: 1.7 less than or equal to LGr / LGt less than or equal to 10.0 ... (1-1).

5. Hot-rolled thin steel sheet according to any one of claims 1 through 4 where it conforms to the following (2-1) relationship: 1.20 less than or equal to (LGr / LGt) / (LMr / LMt) less than or equal to 5.00 ... (2-1).