Abstract

The supplied DEPCT69 is a hot-dip coated Al-Zn alloy steel plate exhibiting excellent machinability and corrosion resistance, stabilized at the processed site. In this disclosure, the coating has a chemical composition of Al: 45% by mass to 65% by mass and Si: 1.0% by mass to 3.0% by mass, with a balance of Zn and unavoidable impurities, and the Mg content in unavoidable impurities is less than 0.5% by mass of the total coating mass.
Need to check novelty before this filing date? Find Prior Art

Claims

DEPCT69 1. Hot-dip coated steel plates with Al-Zn alloy coating comprising a coating material whose chemical composition is Al: 45% by mass to 65% by mass and Si: 1.0% by mass to 3.0% by mass, with an unavoidable balance of Zn and impurities, and the Mg content in the unavoidable impurities is less than 0.5% by mass relative to the total mass of the coating.

2. Hot-dip coated steel plates with Al-Zn alloy coating comprising claim 1, where the coating material is a Mg-Zn based compound, and the principal axis length of the Mg-Zn based compound is less than 10 µm.

3. Hot-dip coated steel plates with Al-Zn alloy coating comprising claim 1, where the coating material does not contain a Mg-Zn based compound.

4. Hot-dip coated steel plates with Al-Zn alloy coating comprising any of the above. Claims 1 through 3, whereby the coating continues, in total, 0.01% by mass to 3.0% by mass of at least one element selected from the group consisting of B, Ca, Ti, V, Cr, Mn, Sr, Mo, In, Sn, Sb, Ce, and Bi.

5. A steel plate coated with a hot-dip Al-Zn alloy according to one of the claims 1 through 4, where the diffraction intensity of MgZn2 in the coating, measured by X-ray diffraction, corresponds to the subsequent relational expression (1): MgZn2(100)=0 ...(1), where MgZn2(100) is the plane diffraction intensity (100) of MgZn2 with an interplane gap d = 0.4510 nm.

6. The method of fabricating a steel plate coated with a hot-dip Al-Zn alloy assembled with the coating, where the assembly method involves forming the coating on a base steel plate using a molten bath. The chemical composition contains Al: 45% to 65% by mass and Si: 1.0% to 3.0% by mass, with a balance of Zn and unavoidable impurities, and the amount of Mg in the unavoidable impurities in the molten bath is controlled to be less than 0.5% by mass, relative to the total mass of the molten bath.

7. Method of producing hot-dip coated Al-Zn alloy steel plates according to claim 6, whereby the molten bath further contains, in total, 0.01% by mass to 3.0% by mass of at least one element selected from the group consisting of B, Ca, Ti, V, Cr, Mn, Sr, Mo, In, Sn, Sb, Ce, and Bi.