Methods for evaluating the characteristics of slow-occurring crevices, methods for predicting slow-occurring crevices, programs and methods for manufacturing pressed products.

TH2501007323APending Publication Date: 2026-11-09JFE STEEL CORP
View PDF 0 Cites 0 Cited by

Patent Information

Application Number
TH2501007323
Authority / Receiving Office
TH · TH
Patent Type
Applications
Current Assignee / Owner
Priority Date
2023-04-26
Filing Date
2023-12-05
Publication Date
2026-11-09

Smart Images

  • Figure 2501007323_DRAWING_01
    Figure 2501007323_DRAWING_01
  • Figure 2501007323_DRAWING_02
    Figure 2501007323_DRAWING_02
  • Figure 2501007323_DRAWING_03
    Figure 2501007323_DRAWING_03
Patent Text Reader

Abstract

DEPCT69 09 / 01 / 2569 Provided is a technology for evaluating the influence of post-trimming stress on the slow-occurring crevice characteristics of the shear end surfaces of sheet metal (3) made of high tensile steel. The slow-occurring crevice characterization method for evaluating the slow-occurring crevice characteristics of the shear end surfaces of sheet metal (3) made of high tensile steel includes the fabrication of test specimens (1) with shear end surfaces of sheet metal (3) in which at least a portion of the plastic stress is fed by the shearing operation on the sheet metal at the location including the portion in which the plastic stress is fed, the release of test specimen (1) under a hydrogen-filled environment with stress from a load applied to the shear end surface of test specimen (1), and the evaluation of the slow-occurring crevice characteristics of the shear end surfaces.
Need to check novelty before this filing date? Find Prior Art

Claims

DEPCT69 09 / 01 / 2569 1. Slow Cree Characterization Method for evaluating the slow cree characterization of the sheared end surfaces of high-tensile steel sheets, where the slow cree characterization method comprises the fabrication of test specimens with sheared end surfaces of the sheet, application of plastic stress to at least a portion of the sheet, and shearing operations on the sheet at locations including the portion where the plastic stress is applied. After fabrication, the test specimens are left under a hydrogen-filled environment with applied load stresses to the sheared end surfaces, and the slow cree characterization of the sheared end surfaces is evaluated relative to the plastic stress.

2. Slow Cree Characterization Method according to Claim 1, where the test specimens include more than one specimen in which different plastic stresses are applied prior to shearing, and the slow cree characterization of the sheet is evaluated for each different plastic stress.

3. A method for characterizing slow-occurring crevices based on claim 1 or claim 2, which includes determining the pre-load stress limit under a hydrogen-filled environment, where the pre-load stress limit does not cause slow-occurring crevices on the shear end surface after shear for the pre-shear plastic strain. The slow-occurring crevice characterization of the shear end surface is evaluated based on the determined pre-load stress limit.

4. A method for characterizing slow-occurring crevices based on claim 3, which includes determining the correlation between the pre-shear plastic strain and the pre-load stress limit, and evaluating the allowable pre-load stress relative to the plastic strain applied to the shear end surface before shear, based on the correlation coefficient.

5. A method for predicting slow-occurring crevices to forecast their occurrence.Or, in pressed products manufactured by shearing, the pressed component has at least one section where plastic stress is applied, where the slow crevice prediction method incorporates the determination of the correlation between the amount of plastic stress before shearing and the preload stress limit in terms of sheet metal, based on the slow crevice characterization method according to claim 3 or claim 4, and the prediction of whether slow crevice occurs in the pressed product, based on the correlation coefficient.

6. The program performs: a data storage unit for the correlation coefficients of the correlation between the amount of plastic stress before shearing and the preload stress limit, which are determined based on the slow crevice characterization method according to claim 3 or claim 4, and a computer to perform the process of determining the usable preload stress limit.Following shearing, the load stress limit corresponds to the input plastic strain before shearing, referencing the stored correlation information.

7. A program for predicting whether slow crevice occurs in a pressed product manufactured by shearing a pressed component containing at least one section where plastic strain is applied, where the program performs: A storage unit stores correlation information regarding the correlation between the pre-shearing plastic strain and the load stress limit, the correlation of which is determined based on the slow crevice characterization method according to claim 3 or claim 4; and the computer performs the first step to determine the load stress limit corresponding to the input plastic strain before shearing, referencing the stored correlation information; and the second step to determine whether slow crevice occurs.Based on the forming stress as the load stress applied to the sheared end surface formed by shearing performed on the compressed component after shearing, and the load stress limit value determined in the first operating step.

8. Compression Production Method for the production of compressed products with sheared end surfaces created by shearing at a location including the area where plastic stress is applied, where the compression production method is incorporated, the determination of the load stress conditions that are evaluated so as not to cause slow crevice in the compressed product by the slow crevice characteristic evaluation method according to Claim 3 or Claim 4, and the production of the compressed product under forming conditions that satisfy the determined load stress conditions.