Equipment for abscess drainage training and manufacturing process.
Patent Information
- Application Number
- TH2503001149
- Authority / Receiving Office
- TH · TH
- Patent Type
- Utility models
- Current Assignee / Owner
- Filing Date
- 2025-03-26
- Publication Date
- 2026-11-09
- Estimated Expiration
- 2045-03-25
Smart Images

Figure 00000001_0000 
Figure 00000014_0000
Claims
OCR10KL(25 / 03 / 2026)1. An abscess training device consisting of an abscess training device (1) with a base (2) on one side of which is raised to form a curved surface. The curved surface is arranged to form a channel for the assembly of a sheath (3) which encloses a simulated abscess (4) inside. Its specific characteristics are that the sheath (3) can be freely removed and connected to the base (2), and the shape of the sheath (3) fits perfectly into the channel on the base (2), on which the surface of the sheath (3) is arranged to have one side convex, and inside the sheath (3) is filled with a simulated abscess (4), which is a liquid-filled part containing liquid.
2. The manufacturing process of the abscess training device according to claim 1, which has the following steps: Preparation of the base (2) is as follows: a. Stir the latex mixture until it is homogeneous and then leave it at a temperature of 25-40 degrees Celsius for 100-200 minutes. Then separate the latex into 2 parts for preparing the base (2) and the sheath (3). b. Take the latex obtained from step a.100-200 grams of latex for preparing the base (2) is beaten with a foaming machine at a medium speed until the latex expands 2-3 times, then stirred further at a reduced speed of 20-30 revolutions per minute to obtain finer foam, and the stirring time at this slower speed is 5-10 minutes. c. Add 1-15 grams of catalyst to the latex obtained from step b and stir for 1-5 minutes. Add 0.5-10 grams of liquid foaming agent to the latex obtained from step c and stir for 1-5 minutes, then pour into a mold for shaping the base. (2) Then wait for it to harden for 5-10 minutes and then steam it at a temperature of 80-120 degrees Celsius for 20-40 minutes. The hardened rubber obtained from step 1, remove it from the mold for the base (2), then wash it with water and then bake it in a hot air oven at a temperature of 70-110 degrees Celsius for 5-8 hours to get the base (2) of the abscess training device (1). The preparation of the abscess simulation (4) consists of the following steps:
1. Take the viscosity adjusting mixture, which is sodium polyacrylate with a concentration of 18 percent, in the amount of 1-4 milliliters, and mix it with water in the amount of 0.5-3.5 ml. Then divide it into 2 parts, the first part, 3-5 ml., mixed with yellow color and the second part, 0.1-2 ml., mixed with red color. Ch. Take the liquid obtained from step f. and fill the packing part while it is not yet filled with air. Add the liquid mixed with yellow color, 3-5 ml., and tie the end of the packing part closed to retain the viscosity adjuster inside as a simulated abscess (4). The preparation of the packing part (3) containing the simulated abscess (4) consists of the following steps: Z. Take the latex for preparing the packing part (3) obtained from step a., 100-200 g., and beat it with a foaming machine. Stir at a medium speed until the latex expands 4-5 times, then continue stirring at a reduced speed of 20-30 revolutions per minute to obtain fine, uniform foam for 5-10 minutes. Take the latex obtained from step 3 in the section reserved for preparing the wrapping material (3), add 5-15 grams of catalyst and stir for 1-5 minutes. Take the latex obtained from step 4, add 1-10 grams of foaming agent to solidify the liquid and stir for 1-5 minutes, then pour into the mold for wrapping material (3) to obtain a rubber layer with a thickness of 0.5-2 centimeters. Take the latex obtained from step 5 in the section reserved for preparing the wrapping material (3).
1. Cover the molded abscess (4) obtained from the abscess preparation step (4) with latex and leave it to solidify and hold the abscess (4) in place at a temperature of 25-40 degrees Celsius for 10-30 minutes.
2. Bake the latex in the mold for the covering part (3) obtained from step 2 in a steam oven at a temperature of 80-120 degrees Celsius for 20-40 minutes, then remove it from the mold.
3. Wash the parts obtained from step 3 with water and dry them at a temperature of 60-80 degrees Celsius for 20-30 hours.
4. Leave the parts obtained from step 3 to solidify at a temperature of 25-40 degrees Celsius for 5-10 days, then inject the parts. A liquid mixed with red color obtained from the preparation step of the abscess model (4) in the amount of 0.1-2 ml will be the encapsulation (3) that contains the abscess model (4) in conjunction with the base (2) to obtain the abscess incision training device.
3. The manufacturing process of the abscess incision training device according to claim 2 in which the medium speed of the foaming machine is 30-60 rpm.
4. The manufacturing process of the abscess incision training device according to claim 2 in which step c. The appropriate catalyst is zinc oxide at a concentration of 50 percent.
5. The manufacturing process of the abscess incision training device according to claim 2 in which step d.The appropriate liquid-to-solid foaming agent is 20% sodium silicofluoride.
6. The manufacturing process of the abscess training device under claim 2, in which step d. appropriate molding is provided for the molding of the base (2) which is 10-15% larger than the size of the base (2).
7. The manufacturing process of the abscess training device under claim 2, in which the preparation of the abscess model (4) in step d. the filling part is 3-7 ml.
8. The manufacturing process of the abscess training device under claim 7, in which the appropriate filling part is a balloon.
9. The latex formulation for the manufacture of the abscess training device under claim 2 shall consist of: - 75-95% by weight of latex - 1-10% by weight of stabilizer - 1-10% by weight of stabilizer - 0.5-5% by weight of first-grade stabilizer - 0.1-5% by weight of second-grade stabilizer - 0.5-5% by weight of antioxidant. 10.The latex formulation for the production of abscess surgery training devices under claim 9, whereby: - The appropriate latex is provided as low-ammonia latex at a concentration of 60 percent; - The appropriate stabilizer is provided as potassium oleate soap at a concentration of 20 percent; - The appropriate stabilizer is provided as sulfur at a concentration of 50 percent; - The appropriate primary stabilizing catalyst is provided as zinc dithiocarbamate catalyst at a concentration of 50 percent; - The appropriate secondary stabilizing catalyst is provided as 1,3-diphenylguanidine at a concentration of 50 percent.