Ultra-quick cooling sand-casting device and method

The sand-casting device and method use a cooling gas to rapidly cool sand molds through a multi-stage process, addressing slow cooling rates and defects, improving productivity and mechanical properties.

US20260364673A1Pending Publication Date: 2026-11-19HYUNDAI MOTOR CO LTD +1
View PDF 0 Cites 0 Cited by

Patent Information

Application Number
US19/413827
Authority / Receiving Office
US · United States
Patent Type
Applications(United States)
Current Assignee / Owner
Priority Date
2025-05-16
Filing Date
2025-12-09
Publication Date
2026-11-19

AI Technical Summary

Technical Problem

Existing casting techniques using air or water for cooling sand molds have slow cooling rates, leading to reduced productivity and increased defects due to uneven cooling, and techniques using moisture-absorbent cores require additional time, further reducing productivity.

Method used

A sand-casting device and method utilizing a cooling gas, controlled by a controller, to rapidly cool the sand mold through a multi-stage process, ensuring uniform cooling and reducing internal stress.

Benefits of technology

The method improves productivity and mechanical properties by achieving rapid cooling, reducing defects, and enhancing cooling efficiency while minimizing nitrogen consumption.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure US20260364673A1-D00000_ABST
    Figure US20260364673A1-D00000_ABST
Patent Text Reader

Abstract

An ultra-quick cooling sand-casting device and method. The ultra-quick cooling sand-casting device includes: a sand mold having a molding space to be filled with molten metal; a cooling bath having an internal space configured to accommodate the sand mold and including cooling gas spray nozzles that are disposed toward the internal space to spray a cooling gas; a cooling gas supply system connected to the cooling gas spray nozzles to supply the cooling gas; and a controller configured to control the operation of the cooling gas supply system.
Need to check novelty before this filing date? Find Prior Art

Description

CROSS-REFERENCE TO RELATED APPLICATION(S)

[0001] This application is based on and claims priority under 35 U.S.C. 119 to Korean Patent Application No. 10-2025-0064010, filed on May 16, 2025, in the Korean Intellectual Property Office, the disclosure of which is herein incorporated by reference in its entirety.TECHNICAL FIELD

[0002] The present disclosure generally relates to a sand-casting device and method.BACKGROUND

[0003] Casting techniques are used in manufacturing various products for automobile parts. Numerous advantages can be achieved in manufacturing products through mold-based casting, such as improved ability to satisfy requirements of automobile parts that demand particular dimensions, and achieving microstructural refinement through mold cooling, resulting in increased strength and elongation.SUMMARY

[0004] In one aspect, of the present disclosure, an ultra-quick cooling sand-casting device includes: a sand mold having a molding space to be filled with molten metal; a cooling bath having an internal space configured to accommodate the sand mold and including one or more cooling gas spray nozzles disposed toward the internal space to spray a cooling gas; a cooling gas supply system connected to the cooling gas spray nozzles to supply the cooling gas; and a controller configured to control the operation of the cooling gas supply system.

[0005] In another aspect, an ultra-quick cooling sand-casting method according to implementations of the present disclosure may include: injecting molten metal into a sand mold having a molding space defined therein; placing the sand mold filled with the molten metal into an internal space of a cooling bath and sealing the cooling bath; spraying a cooling gas into the internal space of the cooling bath to cool the sand mold; stabilizing the cooled sand mold at room temperature; and removing sand from the stabilized sand mold and extracting a cast part.BRIEF DESCRIPTION OF THE DRAWINGS

[0006] The above and other aspects, features, and advantages of the present disclosure will be more apparent from the following detailed description taken in conjunction with the accompanying drawings, in which:

[0007] FIG. 1 is a view illustrating an example of an ultra-quick cooling sand-casting process according to an implementation of the present disclosure;

[0008] FIGS. 2 and 3 are views illustrating examples of the configurations of a cooling gas supply system and an air supply system of an ultra-quick cooling sand-casting device according to an implementation of the present disclosure;

[0009] FIGS. 4 and 5 are views illustrating examples of a support member on which a sand mold is seated according to an implementation of the present disclosure;

[0010] FIG. 6 is a photograph illustrating an example of the microstructure of Comparative Example 1;

[0011] FIG. 7 is a photograph illustrating an example of the microstructure of Example 1; and

[0012] FIG. 8 is a flowchart illustrating an example of an ultra-quick cooling sand-casting method according to an implementation of the present disclosure.DETAILED DESCRIPTION

[0013] In a sand-casting process, a step of cooling the sand mold can be a critical factor that determines the microstructure and mechanical properties of the products. Typically, when cooling the sand mold, molten metal can be poured into the mold and then cooled using air or water.

[0014] However, techniques using air or water spraying generally have a slow cooling rate, which not only reduces the productivity of products but also increases the likelihood of defects due to shrinkage deformation caused by uneven cooling.

[0015] To address these issues, techniques have been introduced in which a sand mold that filled with molten metal is immersed in water to cool the product. However, such techniques often require the use of a moisture-absorbent core that enables the sand mold to absorb water, and time is required for the moisture-absorbent core to absorb water. Thus, there is a problem of reduced productivity, making improvement necessary.

[0016] Implementations of the present disclosure can provide a rapid-cooling sand-casting device and method capable of improving productivity, cooling efficiency, and mechanical properties by rapidly cooling a sand mold using a cooling gas.

[0017] In some implementations, by precisely controlling the cooling temperature and cooling rate through a multi-stage cooling method, internal stress may be reduced and cracking may be prevented.

[0018] Furthermore, in some implementations, by circulating the cooling gas filled in the internal space of the cooling bath in a balanced manner, nitrogen consumption during cooling may be reduced and cooling efficiency may be improved.

[0019] Advantageous effects obtainable from implementations of the present disclosure are not limited to the above-mentioned effects, and other effects which are not mentioned herein may be clearly understood from the following description by those skilled in the art to which the present disclosure pertains.

[0020] Hereinafter, various implementations of the present disclosure will be described with reference to the accompanying drawings. However, it should be appreciated that they are not intended to limit the technology set forth herein to particular implementations and include various modifications, equivalents, and / or alternatives to the implementations of the present disclosure. With regard to the description of the drawings, the same or like reference signs may be used to designate the same or like elements.

[0021] As used herein, the expression “have”, “may have”, “include”, or “may include” refers to the existence of a corresponding feature (e.g., numeral, function, operation, or constituent element such as component) and does not exclude the existence of additional features.

[0022] As used herein, the expression “A or B”, “at least one of A and / or B”, or “one or more of A and / or B” may include all possible combinations of items enumerated together. For example, “A or B”, “” at least one of A and B”, or “at least one of A or B” may refer to all of (1) including at least one A, (2) including at least one B, or (3) including all of at least one A and at least one B.

[0023] The terms used herein are used merely to describe specific implementations, and may not be intended to limit the scope of other implementations. A singular expression may include a plural expression unless they are definitely different in a context. The terms used herein, including technical and scientific terms, may have the same meaning as those commonly understood by a person skilled in the art to which the disclosure pertains. Among the terms user herein, such terms as those defined in a generally used dictionary may be interpreted to have the meanings equal to the contextual meanings in the relevant field of art, and are not to be interpreted to have ideal or excessively formal meanings unless clearly defined herein. In some cases, even the term defined herein should not be interpreted to exclude implementations of the present disclosure.

[0024] It will be apparent to those ordinarily skilled in the art to which the present disclosure pertains that various modifications may be made without departing from the scope of the present disclosure as defined in the claims, and such modifications should not be interpreted as being understood separately from the technical spirit or perspective of the present disclosure.

[0025] Referring to FIGS. 1 to 5, an ultra-quick cooling sand-casting device according to an implementation of the present disclosure may include: a sand mold 10 having a molding space to be filled with molten metal; a cooling bath 20 having an internal space configured to accommodate the sand mold 10 and including one or more cooling gas spray nozzles 21 disposed toward the internal space to spray a cooling gas; a cooling gas supply system 30 connected to the cooling gas spray nozzles 21 to supply the cooling gas; and a controller 50 configured to control the operation of the cooling gas supply system 30.

[0026] In an implementation, the cooling gas may include one or more of argon gas, oxygen gas, and nitrogen gas. For example, the cooling gas may include nitrogen gas.

[0027] The ultra-quick cooling sand-casting device (hereinafter referred to as “the device”) according to implementations of the present disclosure is designed to rapidly cool the sand mold 10 during the casting process, thereby improving the quality of a cast product and reducing process time.

[0028] Referring to the examples of FIGS. 1 and 2, the sand mold 10 may be a mold made of sand used for performing a casting process, and may serve to refine the microstructure through rapid cooling after casting, thereby improving product quality.

[0029] In an implementation, the cooling bath 20 may provide a space in which the sand mold 10, after being placed therein, can be rapidly cooled using a cooling gas.

[0030] In an implementation, the internal space of the cooling bath 20 may include one or more cooling gas spray nozzles 21 configured to spray a cooling gas. For example, a plurality of cooling gas spray nozzles 21 may be provided so as to in uniformly spray the cooling gas in various directions, such as from the top, bottom, and lateral sides of the sand mold 10. For example, the positions of the cooling gas spray nozzles 21 may be variably adjusted depending on the shape and size of the sand mold 10.

[0031] In an implementation, the cooling gas supply system 30 may store liquid nitrogen, vaporize and convert the liquid nitrogen into a cooling gas, and supply the cooling gas into the cooling bath 20. A detailed configuration of the cooling gas supply system 30 will be described further below.

[0032] In an implementation, the controller 50 may control components of the cooling gas supply system 30, which will be described below, and may be implemented through a controller including at least one processor and at least one memory storing instructions for performing the control techniques.

[0033] Referring to the examples of FIGS. 2 and 3, the cooling gas supply system 30 may include: a cooling gas storage tank 31 configured to store the cooling gas to be sprayed through the cooling gas spray nozzles 21; and a cooling gas supply pipe 32 connected to the cooling gas storage tank 31 to deliver the cooling gas to the cooling gas spray nozzles 21. In some implementations, the controller 50 may be configured to gradually lower the temperature of the cooling gas sprayed into the internal space of the cooling bath 20 through the cooling gas spray nozzles 21, e.g., lowered at specific time intervals such as periodic intervals, so as to perform multi-stage cooling of the sand mold 10.

[0034] In an implementation, the cooling gas storage tank 31 may store a cooling gas in a liquefied state at a cryogenic temperature. For example, the cooling gas storage tank 31 may store liquid nitrogen in a cryogenic state.

[0035] In an implementation, the liquefied and stored cooling gas may be vaporized, gasified, and supplied to the cooling gas supply pipe 32. For example, the liquid nitrogen stored in the cooling gas storage tank 31 may be vaporized, gasified, and then supplied to the cooling gas supply pipe 32. For example, a gasification device configured to gasify the liquid nitrogen and a temperature control device configured to adjust the temperature may additionally be provided.

[0036] In an implementation, the cooling gas supply pipe 32 may be a pipe that connects the cooling gas storage tank 31 to the cooling gas spray nozzles 21 to deliver the cooling gas, and in some scenarios may include a valve to control internal pressure and flow rate.

[0037] In an implementation, the controller 50 may increase the supply amount or spray pressure of the cooling gas sprayed, e.g., based on the decreasing temperature according to the multi-stage cooling of the sand mold 10.

[0038] In an implementation, by gradually cooling the sand mold using the cooling gas as described above, cooling uniformity may be ensured, and problems of rapidly transferring thermal shock to the sand mold 10 may be prevented. The sand mold 10 may be progressively cooled through the multi-stage cooling process.

[0039] An example of a detailed method for multi-stage cooling of the sand mold 10 using the cooling gas will be described further below.

[0040] In an implementation, the ultra-quick cooling sand-casting device may include an air supply system 60 configured to spray air into the internal space of the cooling bath 20. The air supply system 60 may include: one or more air spray nozzles 61 disposed to spray air toward the internal space of the cooling bath 20; a blower 62 configured to supply air to be sprayed through the air spray nozzles 61; and an air supply pipe 63 connected to the blower 62 to deliver air to the air spray nozzles 61. The controller 50 may selectively control the operation of one or more of the cooling gas supply system 30 and the air supply system 60.

[0041] In an implementation, by spraying air into the internal space of the cooling bath 20, the air supply system 60 can assist the flow of the cooling gas and activate the circulation of the cooling gas inside the cooling bath 20, thereby promoting more uniform cooling.

[0042] In an implementation, the air spray nozzles 61 may be a nozzle configured to spray air toward the internal space of the cooling bath 20 and may function to evenly distribute air around the sand mold 10.

[0043] In an implementation, the blower 62 may be a device configured to supply air to the air spray nozzles 61 and may push air at a preset pressure. For example, the speed and output of the air being blown in may be adjusted through the controller 50.

[0044] In an implementation, the air supply pipe 63 may be a pipe that connects the blower 62 to the air spray nozzles 61 to deliver air, and in some scenarios may include an air flow control valve to adjust the air flow as needed.

[0045] In an implementation, the cooling gas spray nozzles 21 and the air spray nozzles 61 may be configured to allow adjustment of the spray angle to improve the spray efficiency of the cooling gas and air, and rotary nozzles may be applied to more effectively perform multi-directional spraying.

[0046] In an implementation, although the sand mold 10 may be effectively cooled through the above configuration, in a case where more rapid cooling is required, a fine spray system capable of spraying fine moisture particles together with air may be applied to induce an evaporative cooling effect.

[0047] Referring to the examples of FIGS. 4 and 5, the internal space of the cooling bath 20 may include a support member 40 configured to allow the lower surface of the sand mold 10 to be seated at a predetermined height above the bottom surface of the cooling bath 20. In some implementations, the upper surface of the support member 40 may be configured in a lattice or hollow structure so as to allow the cooling gas and air sprayed into the cooling bath 20 to come into contact with the lower surface of the sand mold 10.

[0048] In an implementation, the support member 40 may be provided inside the cooling bath 20 so as to allow the sand mold 10 to be stably placed therein. The support member 40 may be arranged such that the lower surface of the sand mold 10 remains spaced apart from the bottom surface of the cooling bath 20 at a predetermined distance, thereby allowing the cooling gas and air to smoothly come into contact with the lower portion of the sand mold 10.

[0049] In an implementation, the upper surface of the support member 40 on which the sand mold 10 is seated may be formed in a lattice or hollow structure so as to maximize the cooling performance for the lower surface of the sand mold 10.

[0050] For example, the lattice structure may be formed in a lattice shape made of metal or ceramic material including a plurality of openings, and the cooling gas and air passing through the openings may effectively cool the lower surface of the sand mold 10.

[0051] For example, the hollow structure may include support frames that support the lower edge portion of the sand mold in a hollow state, and the cooling gas and air may cool the lower surface of the sand mold 10 through the empty space therein.

[0052] The support member 40 may be made of a material such as a heat-resistant alloy or ceramic that exhibits excellent heat and cold resistance, and does not deform or crack even under a rapid temperature change.

[0053] In addition, fine protrusions may be formed on the upper surface of the support member 40, and flow paths may be formed between the fine protrusions that come into contact with the lower surface of the sand mold 10, thereby enhancing the cooling efficiency.

[0054] With such a configuration, it is possible to implement an implementation of an ultra-quick cooling sand-casting device of the present disclosure capable of forming a uniform microstructure and improving cooling efficiency, as confirmed in experimental examples described below.

[0055] Hereinafter, an example of a sand-casting method using the casting device according to implementations the present disclosure will be described with reference to FIG. 8.

[0056] In an implementation, molten metal may be poured into the sand mold 10 in which a molding space is formed (S100).

[0057] For example, the step of pouring the molten metal into the molding space of the sand mold 10 may be performed in the same manner as in a general casting process.

[0058] For example, the molten metal may be a metallic material such as aluminum, iron, or copper, and may be melted to an appropriate temperature depending on the characteristics of the material before being poured.

[0059] For example, the molten metal may be heated to 680 °C to 700 °C and poured into the sand mold 10. In consideration of castability, the molten metal may be poured within 5 seconds using a holding furnace so that the temperature does not fall below 650 °C.

[0060] In an implementation, the sand mold 10 may be placed inside the internal space of the cooling bath 20 and sealed (S200).

[0061] For example, after placing the sand mold 10 filled with molten metal into the internal space of the cooling bath 20, the cooling space may be sealed using a sealing cover.

[0062] For example, the sealing cover may be made of a cold-resistant material (e.g., SUS304 or alumina-coated steel plate) to prevent the inflow of outside air and maximize the cooling efficiency of the cooling gas.

[0063] In an implementation, the sand mold 10 may be cooled using a cooling gas (S300).

[0064] As described above, the cooling gas may include one or more of argon gas, oxygen gas, and nitrogen gas. For example, the cooling gas may include nitrogen gas.

[0065] For example, the temperature of the cooling gas sprayed into the internal space of the cooling bath 20 may be gradually changed, e.g., at specific time intervals, to perform multi-stage cooling of the sand mold.

[0066] For example, a cooling gas spraying process including multiple stages may be performed to rapidly cool the sand mold 10.

[0067] As a specific example, the process may include: a first stage of spraying a cooling gas at −40 °C to −60 °C into the internal space of the cooling bath for 1 to 2 minutes; a second stage of spraying a cooling gas at −90 °C to −110 °C into the internal space of the cooling bath for 1 to 2 minutes; and a third stage of spraying a cooling gas at −140 °C to −160 °C into the internal space of the cooling bath for 1 to 2 minutes.

[0068] For example, in the first stage of cooling gas spraying, the relatively higher temperatures may help ensure that internal stress caused by a rapid temperature difference between the molten metal and the sand mold 10 can be minimized.

[0069] For example, in the second stage of cooling gas spraying, the interior of the sand mold 10 may be effectively cooled by spraying a cooling gas at a lower temperature, e.g., −90 °C to −110 °C for 1 to 2 minutes, to increase the cooling rate.

[0070] For example, in the third stage of cooling gas spraying, rapid cooling may be achieved at the central portion of the sand mold 10 by spraying a cryogenic cooling gas at an even lower temperature, e.g., −140 °C to −160 °C for 1 to 2 minutes.

[0071] Different numbers of stages with different temperatures for different time durations can be used. In general, the sand mold 10 may be rapidly cooled by performing a cooling gas spraying process including multiple steps.

[0072] In some implementations, to achieve more efficient cooling, air may be sprayed into the internal space of the cooling bath to enable circulation of the cooling gas.

[0073] For example, the air may also be sprayed in multiple stages by gradually changing the spray speed of the air at specific (e.g., periodic) time intervals, which may guide the flow of the cooling gas to improve cooling uniformity and disturb the gas layer around the sand mold 10, thereby accelerating the cooling rate.

[0074] As a specific example, the process may include: a first stage of air spraying to spray air at 5 to 10 m / s, a second stage of air spraying to spray air at 15 to 20 m / s, and third stage of air spraying to spray air at 30 m / s or higher.

[0075] For example, the first stage of air spraying may be performed during the first stage of cooling gas spraying, the second stage of air spraying may be performed during the second stage of cooling gas spraying, and the third stage of air spraying may be performed during the third stage of cooling gas spraying. However, implementations are not limited thereto, and the air spraying stages may be coordinated with the gas spraying stages in other ways, to help ensure cooling uniformity and accelerated cooling rate.

[0076] In an implementation, the cooled sand mold 10 may be stabilized at room temperature (S400).

[0077] For example, after the cooling gas spraying is completed, the sand mold 10 may be taken out from the cooling bath 20 and stabilized at room temperature for a period of time (e.g., 30 seconds to 5 minutes).

[0078] In an implementation, the stabilized sand mold may undergo sand removal to extract the cast part (S500).

[0079] For example, the sand removal process may employ various methods depending on user preference, such as vibration-based sand removal, high-pressure air blow, or water-jet sand removal.

[0080] Hereinafter, experimental examples are provided to describe the effects of the present disclosure. However, these are merely illustrative examples of an implementation of the present disclosure, and the effects of the present disclosure are not limited to those described in the following implementations and experimental examples.EXAMPLES AND COMPARATIVE EXAMPLESExample 1

[0081] A cast product cooled using a cooling gas was prepared by employing the ultra-quick cooling sand-casting device and the ultra-quick cooling sand-casting method of the present disclosure.Comparative Example 1

[0082] A cast product cooled using water was prepared.Comparative Example 2

[0083] A cast product cooled at room temperature was prepared.Test Example1) Physical Property Comparison

[0084] To demonstrate the superior effects of the present disclosure, the physical properties of Example 1 and Comparative Example 1 were compared and summarized in Table 1 below.

[0085] More specifically, the average grain size, yield strength, tensile strength, and elongation of Example 1 were compared with those of Comparative Examples 1 and 2. FIG. 6 is a photograph showing the structure of Comparative Example 1, and FIG. 7 is a photograph showing the structure of Example 1.TABLE 1AverageYieldTensilegrain sizeStrengthStrengthElongation(μm)(MPa)(MPa)(%)Example 12020030015Comparative401802308Example 1Comparative601502006Example 2

[0086] As shown in Table 1, it was confirmed that Example 1 has a smaller average grain size and superior yield strength, tensile strength, and elongation compared to Comparative Examples 1 and 2, thereby exhibiting excellent physical properties.

[0087] Through this, it was confirmed that the present disclosure has an excellent effect in resolving the limitations in securing physical properties due to grain coarsening in sand casting, and in improving the cooling rate regardless of shape complexity.

[0088] The foregoing has somewhat broadly described the feature and advantages of the present disclosure so as to allow the claims as described below to be more readily understood. Those skilled in the art will appreciate that other specific modifications and changes may be easily made to the forms of the present disclosure without changing the technical idea or essential features of the present disclosure. Therefore, the implementations set forth above should be understood not from limitative viewpoints but from illustrative viewpoints in all aspects. The scope of the present disclosure is defined by the appended claims, rather than the above detailed description, and the scope of the present disclosure should be construed to include all changes or modifications derived from the meaning and scope of the claims and equivalents thereof.

Claims

1. A sand-casting device comprising:a sand mold having a molding space to be filled with molten metal;a cooling bath having an internal space configured to accommodate the sand mold, the cooling bath comprising one or more cooling gas spray nozzles disposed toward the internal space to spray a cooling gas;a cooling gas supply system connected to the one or more cooling gas spray nozzles and configured to supply the cooling gas; anda controller configured to control an operation of the cooling gas supply system.

2. The device of claim 1, wherein the cooling gas supply system is configured to supply the cooling gas comprising nitrogen gas.

3. The device of claim 1, wherein the cooling gas supply system comprises:a cooling gas storage tank configured to store the cooling gas to be sprayed through the one or more cooling gas spray nozzles; anda cooling gas supply pipe connected to the cooling gas storage tank and configured to deliver the cooling gas to the one or more cooling gas spray nozzles, andwherein the controller is configured to perform a multi-stage cooling of the sand mold by incrementally reducing a temperature of the cooling gas sprayed into the internal space of the cooling bath through the one or more cooling gas spray nozzles at a plurality of time intervals.

4. The device of claim 3, wherein the controller is configured to increase a supply amount or a spray pressure of the cooling gas sprayed into the internal space of the cooling bath, based on a decreasing temperature according to the multi-stage cooling of the sand mold.

5. The device of claim 1, further comprising:an air supply system configured to spray air into the internal space of the cooling bath,wherein the air supply system comprises:one or more air spray nozzles disposed to spray air toward the internal space of the cooling bath;a blower configured to supply air to be sprayed through the one or more air spray nozzles; andan air supply pipe connected to the blower to deliver air to the one or more air spray nozzles, andwherein the controller is further configured to selectively control operation of at least one of the cooling gas supply system or the air supply system.

6. The device of claim 5, wherein the internal space of the cooling bath comprises a support member configured to support a lower surface of the sand mold to be seated at a height above a bottom surface of the cooling bath, andwherein an upper surface of the support member is configured in a lattice or hollow structure and allows the cooling gas and air sprayed into the cooling bath to come into contact with the lower surface of the sand mold.

7. A method of performing cooling in a sand-casting device, the method comprising:injecting molten metal into a sand mold having a molding space;placing the sand mold filled with the molten metal into an internal space of a cooling bath and sealing the cooling bath;controlling a cooling gas supply system to adjustably spray a cooling gas through one or more cooling gas spray nozzles, into the internal space of the cooling bath to cool the sand mold; andstabilizing the cooled sand mold at room temperature; and removing sand from the stabilized sand mold and extracting a cast part.

8. The method of claim 7, wherein the cooling gas comprises nitrogen gas.

9. The method of claim 7, wherein the controlling of the cooling gas supply system to adjustably spray the cooling gas into the internal space of the cooling bath to cool the sand mold comprises:incrementally changing a temperature of the cooling gas sprayed into the internal space of the cooling bath at a plurality of time intervals to perform multi-stage cooling of the sand mold.

10. The method of claim 7, wherein the controlling of the cooling gas supply system to adjustably spray the cooling gas into the internal space of the cooling bath to cool the sand mold comprises:a first stage of spraying the cooling gas at −40 °C to −60 °C into the internal space of the cooling bath for 1 to 2 minutes;a second stage of spraying the cooling gas at −90 °C to −110 °C into the internal space of the cooling bath for 1 to 2 minutes; anda third stage of spraying the cooling gas at −140 °C to −160 °C into the internal space of the cooling bath for 1 to 2 minutes.

11. The method of claim 7, wherein the cooling of the sand mold comprises:controlling an air supply system to adjustably spray air into the internal space of the cooling bath to enable circulation of the cooling gas.

12. The method of claim 11, wherein the controlling of the air supply system to adjustably spray the air comprises:performing multi-stage spraying of the air by incrementally changing a spray speed of the air at a plurality of time intervals.

13. The method of claim 11, wherein the controlling of the air supply system to adjustably spray the air comprises:a first stage of spraying air at 5 to 10 m / s;a second stage of spraying air at 15 to 20 m / s; anda third stage of spraying air at 30 m / s or higher.

14. A manufacturing system for manufacturing a multi-component product, the manufacturing system comprising:a sand mold having a molding space configured to be filled with molten metal to be shaped into a component for the multi-component product;a cooling bath having an internal space configured to accommodate the sand mold;cooling gas spray nozzles configured to spray a cooling gas into the internal space of the cooling bath;a cooling gas supply system connected to the cooling gas spray nozzles and configured to supply the cooling gas into the internal space of the cooling bath; anda controller configured to control an operation of the cooling gas supply system to supply different temperatures of the cooling gas at different time intervals.