Aluminum Alloy With Increased Scrap Absorption Capacity and Strength

The aluminum alloy with tailored compositions addresses the limitations of existing alloys by achieving high strength, ductility, and scrap absorption, facilitating sustainable and cost-effective production with high recycled content.

US20260366104A1Pending Publication Date: 2026-11-19SPEIRA GMBH
View PDF 0 Cites 0 Cited by

Patent Information

Application Number
US19/726151
Authority / Receiving Office
US · United States
Patent Type
Applications(United States)
Current Assignee / Owner
Priority Date
2024-01-08
Filing Date
2026-06-30
Publication Date
2026-11-19

AI Technical Summary

Technical Problem

Existing aluminum alloys, such as AA5182 and AA5754, face challenges in achieving high strength and ductility while being cost-effective, and have limited capacity to absorb non-sorted aluminum scrap, which affects production efficiency and sustainability.

Method used

An aluminum alloy composition with specific ranges of Si (0.15-0.30 wt.%), Fe (0.20-0.35 wt.%), Cu (0.02-0.10 wt.%), Mn (0.35-0.45 wt.%), Mg (3.00-3.60 wt.%), Cr (0.02-0.10 wt.%), Zn (≤0.20 wt.%), and Ti (≤0.05 wt.%) is developed, allowing for high strength, ductility, and increased scrap absorption capacity.

Benefits of technology

The alloy achieves yield strengths exceeding 110 MPa, tensile strengths over 220 MPa, and high scrap absorption capacity, enabling sustainable production with high recycled content, reducing production costs and environmental footprint.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure US20260366104A1-D00000_ABST
    Figure US20260366104A1-D00000_ABST
Patent Text Reader

Abstract

The invention relates to an aluminum alloy with increased scrap absorption capacity and strength. The invention further relates to a rolled product consisting of an aluminum alloy according to the invention, a method for producing the rolled product, and a component produced from the rolled product. The object of providing an aluminum alloy which can be produced cost-effectively and additionally has a high strength is achieved in that the composition of the aluminum alloy comprises the following alloy components: Si: 0.15 wt. % to 0.30 wt. %, Fe: 0.20 wt. % to 0.35 wt. %, Cu: 0.02 wt. % to 0.10 wt. %, Mn: 0.35 wt. % to 0.45 wt. %, Mg: 3.00 wt. % to 3.60 wt. %, Cr: 0.02 wt. % to 0.10 wt. %, Zn: at most 0.20 wt. %, Ti: at most 0.05 wt. %, remainder Al and unavoidable impurities, individually at most 0.05 wt. %, in total at most 0.15 wt. %.
Need to check novelty before this filing date? Find Prior Art

Description

CROSS-REFERENCE TO RELATED PATENT APPLICATIONS

[0001] This patent application is a continuation of International Application No. PCT / EP2025 / 050295, filed on Jan. 8, 2025, which claims the benefit of priority to European Patent Application No. 24150737.5, filed Jan. 8, 2024, the entire teachings and disclosures of both applications are incorporated herein by reference thereto for all purposes.FIELD OF THE INVENTION

[0002] The invention relates to an aluminum alloy with increased scrap absorption capacity and strength. The invention further relates to a rolled product consisting of an aluminum alloy according to the invention, a method for producing the rolled product, and a component produced from the rolled product.BACKGROUND OF THE INVENTION

[0003] A rolled product refers to rolled strips or sheets. Aluminum alloys of the AA5xxx (AlMg) type are used in form of sheets or plates or strips, respectively, for the construction of welded or joined structures in ship, automotive and aircraft construction. They are characterized in particular by a high strength, which increases with increasing magnesium content. Therefore, aluminum magnesium alloys of the AA5xxx type can increasingly replace materials made of steel, for example in motor vehicle construction, and can thus contribute to further weight reduction of motor vehicles.

[0004] A standard material of the AA5xxx type for automotive interior applications is the aluminum alloy AA5182 (AlMg4.5Mn0.4), which has a yield strength Rp0.2 of more than 110 MPa in the O / H111 temper according to DIN EN 485-2. Due to the high magnesium content, alloy AA5182 achieves high strengths with good ductility. At the same time, however, it is cost-intensive in production due to high magnesium contents and, in addition, has only a limited capacity to absorb non-sorted aluminum scrap. Common materials of the AA5754 (AlMg3) type, on the other hand, do not reach the required strengths due to their lower magnesium content and are also less ductile.SUMMARY OF THE INVENTION

[0005] Proceeding from this, the object of the present invention is to provide an aluminum alloy which can be produced cost-effectively and additionally has a high strength. In addition, an advantageous rolled product and a method for producing a rolled product are to be provided, by which rolled products with a high strength can be produced cost-effectively. Finally, advantageous components of a motor vehicle, for example body parts or body add-on parts, are to be proposed.

[0006] The above-mentioned object is achieved by an aluminum alloy according to the invention having a composition with the following alloy components:

[0007] Si: 0.15 wt. % to 0.30 wt. %,

[0008] Fe: 0.20 wt. % to 0.35 wt. %,

[0009] Cu: 0.02 wt. % to 0.10 wt. %,

[0010] Mn: 0.35 wt. % to 0.45 wt. %,

[0011] Mg: 3.00 wt. % to 3.60 wt. %,

[0012] Cr: 0.02 wt. % to 0.10 wt. %,

[0013] Zn: at most 0.20 wt. %,

[0014] Ti: at most 0.05 wt. %,

[0015] remainder Al and unavoidable impurities, individually at most 0.05 wt. %, in total at most 0.15 wt. %.

[0016] It has been found that the aluminum alloy according to the invention can be used to produce aluminum alloy products, in particular rolled products, cost-effectively, which are characterized by high strength with good ductility. Due to the predetermined content limits for the individual alloying elements, on the one hand a high scrap absorption capacity is made possible, while on the other hand the closely matched contents of Mg, Cu, Mn and Cr ensure a sufficient strength level. The aluminum alloy thus allows an advantageous compromise between scrap absorption capacity, strength and formability of correspondingly produced aluminum alloy products.

[0017] In particular, it has been found that with an Mg content of 3.00 wt. % to 3.60 wt. % a good strength can already be achieved. The lower limits for Cu of 0.02 wt. %, for Mn of 0.35 wt. % and for Cr of 0.02 wt. % allow a further increase in strength. It has been found that, with the aid of the alloy composition according to the invention, an AA5754 material is obtained, which achieves an increased strength compared to known AA5754 standard materials. In particular, the increased strength level of an AA5182 material in the O / H111 temper can be achieved with the alloy composition according to the invention.

[0018] At the same time, with the aluminum alloy, an increased absorption potential for non-sorted aluminum alloy scrap can be achieved, without limiting the ductility compared to an AA5754 standard material. An increased absorption potential for non-sorted aluminum alloy scrap in particular includes higher flexibility with regard to available scrap on the scrap market. This includes, for example, non-sorted pre- and post-consumer scrap. It has been found that in particular the contents of the elements Si and Fe are relevant for the scrap absorption capacity of the aluminum alloy. It was recognized that, for contents below 0.15 wt. % Si and below 0.25 wt. % Fe, there is hardly any absorption potential for scrap, and corresponding alloy contents are therefore not practical. A higher Mg content has a positive effect not only on strength but also on formability. It was also found that an upper limit for the Zn content of 0.20 wt. % has a positive effect on the tolerance with respect to the absorption of non-sorted scrap.

[0019] The silicon (Si) content of the aluminum alloy is in the range of 0.15 wt. % to 0.30 wt. %. The lower limit of 0.15 wt. % has proven advantageous with regard to the absorption capacity of non-sorted aluminum alloy scrap of the aluminum alloy. At the same time, the limitation of the Si content to at most 0.30 wt. % leads to an improved ductility and higher strength of the rolled products produced from the aluminum alloy, since at lower Si contents less strength-increasing Mg is bound in Mg2Si phases. According to an advantageous embodiment of the aluminum alloy, the Si content is 0.20 wt. % to 0.30 wt. %. Particularly preferably, the Si content of the aluminum alloy is 0.25 wt. % to 0.30 wt. %. It has been found that a Si content in these ranges is accompanied by a higher scrap absorption capacity, since non-sorted scrap can have a relatively high Si content.

[0020] The iron (Fe) content of the aluminum alloy is in the range of 0.20 wt. % to 0.35 wt. %. It has been found that too low Fe contents of less than 0.20 wt. % limit the tolerance of the aluminum alloy for iron-containing scrap, since conventional scrap grades generally have a significant iron content. Therefore, excessive limitation of the Fe content can hinder the realization of high recycled contents. At the same time, the limitation of the Fe content to at most 0.35 wt. % leads to an improved formability of the rolled products produced from the aluminum alloy. According to an advantageous embodiment of the aluminum alloy, the Fe content is 0.25 wt. % to 0.35 wt. % Fe. An Fe content in the range of 0.25 wt. % to 0.35 wt. % has a further positive effect on the absorption capacity of non-sorted scrap. Particularly preferably, the Fe content is 0.30 wt. % to 0.35 wt. %.

[0021] The copper (Cu) content of the aluminum alloy is in the range of 0.02 wt. % to 0.10 wt. %. By permitting a Cu content of up to 0.10 wt. %, an increased tolerance of the aluminum alloy is achieved, in particular for copper-containing aluminum alloy scrap, which promotes the realization of high recycled contents in the production of rolled products. At the same time, with a minimum content of 0.02 wt. %, Cu has, alongside Mg, Mn and Cr, a positive effect on the strength of the aluminum alloy. According to an advantageous embodiment of the aluminum alloy, the Cu content is 0.05 wt. % to 0.10 wt. %, particularly preferably 0.05 wt. % to 0.08 wt. %. It has been found that Cu is hereby involved in a further increase in strength, while maintaining ductility.

[0022] The manganese (Mn) content of the aluminum alloy is in the range of 0.35 wt. % to 0.45 wt. %. The lower limit of the Mn content of 0.35 wt. % leads, as already stated above, in combination with the lower limits of Cu and Cr, to an increase in strength of the aluminum alloy compared to an AA5754 standard material. At the same time, a lower limit of 0.35 wt. %, preferably 0.40 wt. %, results in an advantageous scrap absorption capacity. Above Mn contents of at least 0.40 wt. %, significant increases in strength are also achieved.

[0023] The magnesium (Mg) content of the aluminum alloy is in the range of 3.00 wt. % to 3.60 wt. %. With a magnesium content of up to 3.60 wt. % a particularly good strength of the aluminum alloy can be achieved. According to an advantageous embodiment of the aluminum alloy, the Mg content is 3.00 wt. % to 3.30 wt. %. This allows a particularly advantageous compromise between high strength, good formability, good resistance to intergranular corrosion and cost-effective production.

[0024] The chromium (Cr) content of the aluminum alloy is in the range of 0.02 wt. % to 0.10 wt. %. According to an advantageous embodiment of the aluminum alloy, the Cr content is 0.05 wt. % to 0.10 wt. %. With a lower limit of 0.02 wt. %, preferably 0.05 wt. %, Cr contributes to the increase in strength of the aluminum alloy and at the same time allows an increased scrap absorption capacity. Limiting the Cr content to at most 0.10 wt. % additionally improves the forming properties of the aluminum alloy.

[0025] The zinc (Zn) content of the aluminum alloy is at most 0.20 wt. %. A Zn content of up to 0.20 wt. % is advantageous for an increased scrap absorption capacity of the aluminum alloy, in particular since a removal of Zn can be cost-intensive. The lower limit of Zn is, for example, at least 0.001 wt. %. According to an advantageous embodiment of the aluminum alloy, the Zn content is at most 0.10 wt. %.

[0026] The titanium (Ti) content of the aluminum alloy is at most 0.05 wt. %. Ti can optionally be contained in the aluminum alloy, e.g. for the purpose of grain refinement. Preferably, the aluminum alloy has a Ti content of at least 0.001 wt. %. The maximum content is limited to 0.05 wt. % Ti, since otherwise Ti would have a negative effect on the ductility of the aluminum alloy.

[0027] In addition to the previously mentioned alloy components, the aluminum alloy has aluminum and unavoidable impurities as the remainder. Unavoidable impurities refer to alloy components that are not intentionally added but are inevitably contained in the aluminum alloy due to the production process. According to the invention, the content of an individual unavoidable impurity is limited to 0.05 wt. %, the content of all unavoidable impurities is limited in total to 0.15 wt. %. This ensures that the unavoidable impurities have no, or no significant negative effects on the properties of the aluminum alloy, for example due to undesired phase formation.

[0028] According to a further advantageous embodiment of the aluminum alloy, the sum of Cu content and Cr content is >0.10 wt. %, and / or the Cu content and the Cr content are each ≥0.05 wt. %, when the Mg content is <3.30 wt. %. While a corresponding limitation of the Mg content can provide an improved corrosion behavior and a more cost-effective aluminum alloy, corresponding minimum contents of Cu and Cr at the same time ensure a high strength of the rolled products produced from the aluminum alloy. For example, the Mg content is <3.30 wt. %, wherein the sum of Cu content and Cr content is >0.10 wt. % and / or the Cu content and the Cr content are each ≥0.05 wt. %.

[0029] According to a further advantageous embodiment of the aluminum alloy, the sum of Cu content and Cr content is <0.10 wt. %, and / or the Cu content and the Cr content are each <0.05 wt. %, when the Mg content is >3.30 wt. %. While the strength and formability are positively influenced by more Mg, correspondingly limited upper contents of Cu and Cr ensure that the material does not become too high in strength, thereby maintaining sufficiently high ductility. For example, the Mg content is >3.30 wt. %, wherein the sum of Cu content and Cr content is <0.10 wt. %, and / or the Cu content and the Cr content are each <0.05 wt. %.

[0030] According to a further advantageous embodiment of the aluminum alloy, the aluminum alloy achieves a total score of at least 16 points in an evaluation for the scrap absorption capacity, wherein the total score is obtained from the sum of the individual scores for the contents of Si, Fe, Cu, Mn, Cr, Zn and Ti of the aluminum alloy as follows:

[0031] Si content: <0.15 wt. % gives 0 points,

[0032] 0.15 wt. % to <0.25 wt. % gives 3 points,

[0033] ≥0.25 wt. % gives 6 points,

[0034] Fe content: <0.25 wt. % gives 0 points,

[0035] 0.25 wt. % to <0.30 wt. % gives 3 points,

[0036] ≥0.30 wt. % gives 6 points,

[0037] Cu content: <0.03 wt. % gives 0 points,

[0038] 0.03 wt. % to <0.05 wt. % gives 1 point,

[0039] ≥0.05 wt. % gives 2 points,

[0040] Mn content: <0.25 wt. % gives 0 points,

[0041] 0.25 wt. % to <0.35 wt. % gives 1 point,

[0042] ≥0.35 wt. % gives 2 points,

[0043] Cr content: <0.03 wt. % gives 0 points,

[0044] 0.03 wt. % to <0.05 wt. % gives 1 point,

[0045] ≥0.05 wt. % gives 2 points,

[0046] Zn content: <0.03 wt. % gives 0 points,

[0047] 0.03 wt. % to <0.05 wt. % gives 1 point,

[0048] ≥0.05 wt. % gives 2 points,

[0049] Ti content: <0.03 wt. % gives 0 points,

[0050] 0.03 wt. % to <0.05 wt. % gives 1 point,

[0051] ≥0.05 wt. % gives 2 points.

[0052] The scrap absorption capacity of an aluminum alloy is in particular referred to as the tolerance of the alloy to an absorption of non-sorted scrap. Aluminum alloys with a high scrap absorption capacity allow, in particular, high recycled contents during the production of rolled products from the aluminum alloy. It has been found that aluminum alloys that achieve a total score of at least 16 points in the evaluation for scrap absorption capacity allow a particularly high scrap absorption capacity. Preferably, the aluminum alloy has a total score of at least 18 points in the evaluation for scrap absorption capacity.

[0053] For the individual alloying elements, respective ranges could be determined in which the respective alloying elements have a different influence on the scrap absorption capacity of an aluminum alloy. For example, it was found that contents of the respective alloying elements below a certain minimum content have a negative effect on the scrap absorption capacity of an aluminum alloy comprising these elements. The contents of the respective alloying elements that are below a defined minimum value are therefore, for example, evaluated with 0 points.

[0054] In particular, it has been found that the contents of Si and Fe have a comparatively high influence on the scrap absorption capacity of an aluminum alloy of the AA5754 type compared to the contents of the other aluminum alloying elements. This is mainly due to the fact that aluminum alloy scrap usually has high Si and Fe contents. Aluminum alloys with high Si and / or Fe contents are accordingly more tolerant of the use of scrap. In the evaluation of the scrap absorption capacity, the contents of Si and Fe are therefore each given higher weighting than the contents of the other alloying elements Cu, Mn, Cr, Zn and Ti. In particular, the contents of Si and Fe are weighted three times higher than the contents of the alloying elements Cu, Mn, Cr, Zn and Ti.

[0055] In particular, aluminum alloys with a total score of less than 10 points in the evaluation for scrap absorption capacity have a low scrap absorption capacity. Aluminum alloys with a total score of 10 points or more in the evaluation for scrap absorption capacity are more tolerant with respect to scrap absorption. Aluminum alloys with a total score of 10 to 15 points have a moderate scrap absorption capacity. Aluminum alloys with a total score of 16 points or more in the evaluation for scrap absorption capacity have a high scrap absorption capacity. Aluminum alloys with a total score of 18 points or more in the evaluation for scrap absorption capacity have a particularly high scrap absorption capacity.

[0056] The above-mentioned object is also achieved by a rolled product according to the invention comprising an aluminum alloy according to the invention. It has been found that, despite the deviations in the chemical composition of the rolled product made from an aluminum alloy with the above-mentioned contents of alloy components, a combination of mechanical properties of the rolled product can be achieved which meets the high requirements for processing of the rolled product of the aluminum alloy AA5182 and allows the rolled product to be processed on production facilities designed for this purpose. Thus, rolled products with a low CO2 footprint can be produced sustainably on existing production facilities. It has been shown in particular that the rolled product according to the invention in the O / H111 temper has the increased yield strength Rp0.2 of more than 110 MPa of a rolled product made from an AA5182 alloy according to DIN EN 485-2. Due to the combination of the lower limits of the Mg, Cu, Mn and Cr contents, higher strengths can be achieved compared to conventional AA5754 products. At the same time, the rolled product has an increased tolerance with respect to non-sorted aluminum alloy scrap and allows high recycled contents within the scope of production.

[0057] According to an advantageous embodiment of the rolled product, the rolled product in the O / H111 temper has a yield strength Rp0.2 of 110 MPa or >110 MPa, for example 110 MPa to 150 MPa, and a tensile strength Rm of ≥220 MPa, preferably >230 MPa, measured transverse to the rolling direction. Thus, the rolled product far exceeds the strength properties required for an aluminum alloy of the AA5754 type according to DIN EN 485-2.

[0058] According to a further advantageous embodiment of the rolled product, the rolled product in the O / H111 temper has a uniform elongation Ag of 18% or >18% and an elongation at break A80 mm of 20% or >20%. Thus, the rolled product also exceeds the elongation values required according to DIN EN 485-2 for an aluminum alloy of the AA5754 type.

[0059] Preferably, the rolled product has a perpendicular anisotropy r10 of ≥0.55 and / or a strain-hardening exponent n5 of ≥0.26. The perpendicular anisotropy r10 is the perpendicular anisotropy r measured in a tensile test perpendicular to the rolling direction of the rolled product according to DIN EN ISO 10113: 2021-06 at 10% strain. The strain-hardening exponent n5 is the strain-hardening exponent n determined according to DIN EN ISO 10275: 2020-12 at 5% strain.

[0060] According to a further advantageous embodiment of the rolled product, the rolled product has a thickness of 0.5 mm to 5 mm, preferably 0.7 mm to 3.5 mm, particularly preferably 0.80 mm to 3 mm. The rolled product is thus excellently suited for most applications, for example in automotive manufacturing.

[0061] According to a further advantageous embodiment of the rolled product, the rolled product comprises a recycled content of at least 60%, preferably at least 80%. Due to the high scrap absorption capacity of the aluminum alloy described above, the realization of these high recycled contents for the rolled product according to the invention is made possible without, for example, negatively affecting the process parameters for preferred production methods.

[0062] The above-mentioned object is also achieved by a method for producing a rolled product, the method comprising the following method steps:

[0063] providing a melt of an aluminum alloy having a composition comprising the following alloy components:

[0064] Si: 0.15 wt. % to 0.30 wt. %,

[0065] Fe: 0.20 wt. % to 0.35 wt. %,

[0066] Cu: 0.02 wt. % to 0.10 wt. %,

[0067] Mn: 0.35 wt. % to 0.45 wt. %,

[0068] Mg: 3.00 wt. % to 3.60 wt. %,

[0069] Cr: 0.02 wt. % to 0.10 wt. %,

[0070] Zn: at most 0.20 wt. %,

[0071] Ti: at most 0.05 wt. %,

[0072] remainder Al and unavoidable impurities, individually at most 0.05 wt. %, in total at most 0.15 wt. %,

[0073] casting the melt to form a rolling ingot,

[0074] homogenizing the rolling ingot at 480 °C to 550 °C for at least 0.5 h,

[0075] hot rolling the rolling ingot at a temperature of 280 °C to 520 °C,

[0076] cold rolling the rolled product to final thickness with a reduction rate of at least 40%,

[0077] soft annealing the finish-rolled rolled product at 300 °C to 550 °C.

[0078] The method serves in particular for producing a rolled product according to the invention. The melt is produced in particular from an aluminum alloy according to the invention. It has been found that the method can be used to produce aluminum alloy products with advantageous strength and formability properties and with an increased flexibility in the scrap absorption. In particular, it has been shown that the method according to the invention can be used to produce a rolled product with an increased yield strength of a rolled product of an AA5182 alloy in the O / H111 temper. At the same time, the method allows the use of high recycled contents during production.

[0079] The provision of the melt is preferably carried out at least partially by melting aluminum scrap, for example at least partially by melting UBC scrap or other pre- and post-consumer scrap.

[0080] Casting the melt to form a rolling ingot is preferably carried out in a semi-continuous casting process, in particular DC (direct chill) casting. The ingot can then be sawn or milled.

[0081] Homogenization of the rolling ingot is carried out at a temperature of 480 °C to 550 °C, preferably 520 °C to 550 °C, for example 540 °C, for at least 0.5 h.

[0082] Hot rolling of the rolling ingot is carried out at a temperature of 280 °C to 520 °C. The hot rolling can comprise rough rolling, in particular reverse rolling by means of a reversing roll stand, and finish rolling, in particular by means of a tandem rolling line. The rough rolling is carried out, for example, at a rough rolling temperature of 450 °C to 520 °C and / or up to an intermediate thickness of 30 mm to 40 mm. The finish rolling can be carried out, for example, up to a hot strip final thickness of 2 mm to 8 mm, preferably 2.8 mm to 7.5 mm. The hot strip final temperature is, for example, 280 °C to 350 °C, preferably 290 °C to 350 °C. It is also conceivable that the hot rolling is carried out exclusively by means of a reversing roll stand. The hot strip final thickness in the case of exclusive reversing rolling can be, for example, up to 12 mm, for example 8 mm to 12 mm.

[0083] Cold rolling of the aluminum alloy strip to final thickness is carried out with a reduction rate of at least 40%. The hot strip final thickness can be selected, for example, such that, after the hot rolling, only one cold rolling step is carried out, in which the hot strip is reduced in thickness to its final thickness with a reduction rate of at least 40%, for example 40% to 60%, preferably 50% to 60%. It is also conceivable that the cold rolling comprises two or more, for example three or four, cold rolling passes. The reduction rate during the cold rolling can be selected depending on the hot strip final thickness and the desired final thickness after the cold rolling. The reduction rate can, for example, be more than 60%, e.g. 60% to 75%. The final thickness of the cold strip is, for example, in the range of 0.5 mm to 5 mm, preferably in the range of 0.7 mm to 3.5 mm, more preferably in the range of 0.8 mm to 3.0 mm, particularly preferably 1.0 mm to 2.5 mm. In the last cold rolling pass, an EDT topography can also be impressed into at least one surface of the rolled product. A surface structure produced by “electrical discharge texturing” (EDT) allows a high number of lubricant pockets in the surface profile. As a result, the rolled product allows improved formability.

[0084] Soft annealing of the finish-rolled aluminum alloy strip is carried out at 300 to 550 °C. The soft annealing of the finish-rolled aluminum alloy strip can be carried out, for example, at 300 °C to 400 °C in a chamber furnace. The holding time during soft annealing is, for example, 0.5 to 4 h. The holding time refers to the duration during which the aluminum alloy strip is held at the final temperature. After soft annealing, the aluminum alloy strip can be cooled. The cooling is carried out either in the chamber furnace or after removal of the coil from the chamber furnace. The surface of the rolled product can then be chemically pre-treated and oiled.

[0085] According to an advantageous embodiment of the method for producing a rolled product, the soft annealing is carried out in a continuous furnace. It has been found that with the aid of a soft annealing in a continuous furnace, the ductility of the rolled product can be significantly further increased compared with a coil annealing carried out in a chamber furnace. In particular, with the aid of strip continuous annealing, an advantageous isotropy of the grain structure of the rolled product can be achieved. The soft annealing of the finish-rolled aluminum alloy strip in a continuous furnace is carried out at 380 °C to 550 °C, preferably 400 °C to 550 °C, with a holding time of, for example, 0 s to 60 s, preferably 0 s to 30 s. After the soft annealing, the aluminum alloy strip can be cooled. The cooling takes place, for example, by means of air or water or a combination of both.

[0086] According to an advantageous embodiment of the method for producing a rolled product, the melt comprises a recycled content of at least 60%. Preferably, the melt comprises a recycled content of at least 80%. Due to the high recycling tolerance of the aluminum alloy described above, the use of these high recycled contents in the method for producing rolled products is made possible. Due to the associated energy saving, the production of rolled products with the lowest possible CO2 footprint is made possible and improved sustainability is achieved. Preferably, the recycled material used has a content of at least 30%, preferably at least 50%, particularly preferably at least 70%, of post-consumer scrap. Since post-consumer scrap only arises at the end of the product life cycle, it is considered particularly sustainable and contributes more significantly to the reduction of the CO2 footprint.

[0087] Cumulatively or alternatively, the recycled material used has a content of at least 30%, preferably at least 50%, particularly preferably at least 70% or at least 75%, of pre-consumer scrap, internal and / or external process scrap. In internal process scrap, the compositions and quantities of the individual alloys are generally very well known, so that the alloy composition resulting from the melting of internal process scrap can be well determined. External process scrap is less well defined in composition than internal process scrap and may require further processing steps, but arises, for example, in large quantities in the production of stamped parts, so that the recycling is economically and, in terms of sustainability, of high relevance. By recycling external process scrap, the need for primary metal can be reduced, which reduces the overall CO2 balance. With the aluminum alloy composition, recycled contents of at least 90% can preferably be realized.

[0088] The above-mentioned object is also achieved by a component for a motor vehicle consisting at least partially of a rolled product according to the invention. As already stated above, the rolled product exhibits excellent properties in terms of strength, forming properties and scrap absorption capacities during production. A component consisting at least partially of a rolled product according to the invention is particularly advantageous when it is designed as a body or body add-on part of a motor vehicle. Typical body parts are the fender or parts of the floor assembly, roof, etc. As body add-on parts, components which are not permanently connected to the motor vehicle, for example doors and tailgates, etc. Preferably, non-visible body parts or body add-on parts are produced from the rolled product according to the invention. These are, for example, inner door parts, inner bonnet parts, inner trunk lid parts or inner parts of tailgates, etc. Body inner parts are often formed in a complex manner in order to provide the body inner parts from as few individual components as possible. This saves additional process steps in relation to the joining technique, for example joining or welding of different components. At the same time, body inner parts are also exposed to corrosive conditions, so that a good corrosion resistance is also required. The rolled product meets these requirements to a particular extent and is therefore predestined for this use. It is also conceivable that the component is designed as part of a chassis, in particular of a suspension system, for a motor vehicle.

[0089] In addition, the present invention relates to an aluminum alloy, in particular of the AA5754 type, wherein the aluminum alloy achieves a total score of at least 16 points in an evaluation for the scrap absorption capacity, wherein the total score is obtained from the sum of the individual scores for the contents of Si, Fe, Cu, Mn, Cr, Zn and Ti of the aluminum alloy as follows:

[0090] Si content: <0.15 wt. % gives 0 points,

[0091] 0.15 wt. % to <0.25 wt. % gives 3 points,

[0092] ≥0.25 wt. % gives 6 points,

[0093] Fe content: <0.25 wt. % gives 0 points,

[0094] 0.25 wt. % to <0.30 wt. % gives 3 points,

[0095] ≥0.30 wt. % gives 6 points,

[0096] Cu content: <0.03 wt. % gives 0 points,

[0097] 0.03 wt. % to <0.05 wt. % gives 1 point,

[0098] ≥0.05 wt. % gives 2 points,

[0099] Mn content: <0.25 wt. % gives 0 points,

[0100] 0.25 wt. % to <0.35 wt. % gives 1 point,

[0101] ≥0.35 wt. % gives 2 points,

[0102] Cr content: <0.03 wt. % gives 0 points,

[0103] 0.03 wt. % to <0.05 wt. % gives 1 point,

[0104] ≥0.05 wt. % gives 2 points,

[0105] Zn content: <0.03 wt. % gives 0 points,

[0106] 0.03 wt. % to <0.05 wt. % gives 1 point,

[0107] ≥0.05 wt. % gives 2 points,

[0108] Ti content: <0.03 wt. % gives 0 points,

[0109] 0.03 wt. % to <0.05 wt. % gives 1 point,

[0110] ≥0.05 wt. % gives 2 points.BRIEF DESCRIPTION OF THE DRAWINGS

[0111] In the following, the invention will be described in more detail by means of exemplary embodiments in conjunction with the drawing. The drawing shows in

[0112] FIG. 1 shows a schematic flowchart for an exemplary embodiment of a method according to the invention for producing a rolled product, and

[0113] FIG. 2 shows a schematic illustration of an exemplary embodiment of a component according to the invention for a motor vehicle.DETAILED DESCRIPTION

[0114] FIG. 1 schematically shows the method steps and the sequence of an exemplary embodiment of a method for producing a rolled product. In step A, the method comprises providing a melt of an aluminum alloy. The melt has a recycled content of at least 80%. The aluminum alloy has the following composition:

[0115] Si: 0.15 wt. % to 0.30 wt. %,

[0116] Fe: 0.20 wt. % to 0.35 wt. %,

[0117] Cu: 0.02 wt. % to 0.10 wt. %,

[0118] Mn: 0.35 wt. % to 0.45 wt. %,

[0119] Mg: 3.00 wt. % to 3.60 wt. %,

[0120] Cr: 0.02 wt. % to 0.10 wt. %,

[0121] Zn: at most 0.20 wt. %,

[0122] Ti: at most 0.05 wt. %,

[0123] remainder Al and unavoidable impurities, individually at most 0.05 wt. %, in total at most 0.15 wt. %.

[0124] Preferably, however, the aluminum alloy can also have the following composition:

[0125] Si: 0.20 wt. % to 0.30 wt. %,

[0126] Fe: 0.25 wt. % to 0.35 wt. %,

[0127] Cu: 0.05 wt. % to 0.08 wt. %,

[0128] Mn: 0.35 wt. % to 0.45 wt. %,

[0129] Mg: 3.00 wt. % to 3.30 wt. %,

[0130] Cr: 0.05 wt. % to 0.10 wt. %,

[0131] Zn: at most 0.10 wt. %,

[0132] Ti: at most 0.05 wt. %,

[0133] remainder Al and unavoidable impurities, individually at most 0.05 wt. %, in total at most 0.15 wt. %.

[0134] In step B, the method comprises casting the melt from the aluminum alloy to form a rolling ingot. This is usually done in the DC casting process.

[0135] In step C, the rolling ingot produced this way is optionally homogenized for at least 0.5 hours at a temperature of 480 °C to 550 °C, preferably at 500 °C to 550 °C. The homogenization can be integrated into a preheating process of the rolling ingot prior to the hot rolling or can be carried out separately.

[0136] In method step D, the rolling ingot is then hot rolled. The hot strip final temperature is between 280 °C and 520 °C. The final thicknesses of the hot strip are, for example, 2 to 10 mm, preferably 3 to 8 mm. The hot strip final thickness can be selected such that, after the hot rolling, only one cold rolling step E is carried out, in which the hot strip is reduced in thickness to the final thickness with a reduction rate of at least 40%, for example 40% to 60%, preferably 50% to 60%.

[0137] Subsequently, the aluminum alloy strip cold rolled to the final thickness is subjected to soft annealing. The soft annealing is preferably carried out at a temperature of 380 °C to 550 °C in the continuous furnace for a maximum of 300 s.

[0138] Exemplary embodiments of the rolled product according to the invention and rolled products made from various aluminum alloys in the O / H111 temper, have now been produced. It was assumed that the rolled products, upon achieving the specified mechanical characteristic values of the yield strength Rp0.2>110 MPa, tensile strength Rm>230 MPa, uniform elongation Ag>18% and elongation at break A80 mm>20%, achieve the advantageous yield strength level of an aluminum alloy of the AA5182 type while exhibiting typical tensile strengths and elongations of the aluminum alloy of the AA5754 type in the O / H111 temper. At the same time, the rolled products were evaluated with regard to their scrap absorption capacity.

[0139] Table 1 shows the alloy compositions of the exemplary embodiments (Inv.) and the comparative examples (Comp.). Each individual example was produced using the method parameters specified in FIG. 1.

[0140] Table 2 finally shows the mechanical properties achieved and the scrap absorption capacity of the examples. All mechanical characteristic values such as yield strength Rp0.2, tensile strength Rm, uniform elongation Ag and elongation at break A80 mm were determined according to EN ISO 6892-1: 2019. The strain-hardening exponent n5 was determined according to DIN EN ISO 10275: 2020-12 as strain-hardening exponent n at 5% strain.

[0141] For the evaluation of the scrap absorption capacity, the respective total scores were obtained for the alloys, which result from the respective sums of the respective individual scores for the contents of Si, Fe, Cu, Mn, Cr, Zn and Ti of the aluminum alloy as follows:

[0142] Si content: <0.15 wt. % gives 0 points,

[0143] 0.15 wt. % to <0.25 wt. % gives 3 points,

[0144] ≥0.25 wt. % gives 6 points,

[0145] Fe content: <0.25 wt. % gives 0 points,

[0146] 0.25 wt. % to <0.30 wt. % gives 3 points,

[0147] ≥0.30 wt. % gives 6 points,

[0148] Cu content: <0.03 wt. % gives 0 points,

[0149] 0.03 wt. % to <0.05 wt. % gives 1 point,

[0150] ≥0.05 wt. % gives 2 points,

[0151] Mn content: <0.25 wt. % gives 0 points,

[0152] 0.25 wt. % to <0.35 wt. % gives 1 point,

[0153] ≥0.35 wt. % gives 2 points,

[0154] Cr content: <0.03 wt. % gives 0 points,

[0155] 0.03 wt. % to <0.05 wt. % gives 1 point,

[0156] ≥0.05 wt. % gives 2 points,

[0157] Zn content: <0.03 wt. % gives 0 points,

[0158] 0.03 wt. % to <0.05 wt. % gives 1 point,

[0159] ≥0.05 wt. % gives 2 points,

[0160] Ti content: <0.03 wt. % gives 0 points,

[0161] 0.03 wt. % to <0.05 wt. % gives 1 point,

[0162] ≥0.05 wt. % gives 2 points.

[0163] Aluminum alloys with a total score of less than 10 points in the evaluation for scrap absorption capacity have a low scrap absorption capacity. Aluminum alloys with a total score of 10 points to 15 points have a moderate scrap absorption capacity. Aluminum alloys with a total score of more than 16 points in the evaluation for scrap absorption capacity, on the other hand, have a high scrap absorption capacity.

[0164] Examples 13, 14 and 15 are rolled products according to the teaching of the invention. These have aluminum alloys which allow high recycled contents and thus have a high scrap absorption capacity. At the same time, the exemplary embodiments achieve yield strengths Rp0.2>110 MPa, tensile strengths Rm>230 MPa, uniform elongation Ag>18% and elongation at break A80 mm>20%.

[0165] The comparative examples 2, 3, 4, 5, 6, 7, 8 and 9 exhibit only moderate scrap absorption capacities. While comparative examples 3 and 8 have comparatively low Fe contents of <0.30 wt. % and the comparative example 3 also has a low Cu content of <0.05 wt. %, Mn content of <0.35 wt. % and Cr content of 0.03 wt. %, the comparative examples 5, 6, 7, 8 and 9 in particular have low Si contents of <0.25 wt. %.

[0166] The comparative examples 1, 10, 11 and 12, on the other hand, exhibit particularly low scrap absorption capacities. This is primarily due to the low Fe contents of <0.25 wt. %. In addition, these alloy compositions exhibit low Cr contents of <0.03 wt. %, and the comparative examples 10, 11 and 12 simultaneously exhibit low Si and Cu contents of <0.15 wt. % or 0.03 wt. %, respectively.

[0167] In addition, the comparative examples 1, 2, 3 and 4 do not meet the requirements for the strength of the rolled products but have yield strengths Rp0.2<110 MPa and tensile strengths Rm<230 MPa, whereby they are below the minimum values for an aluminum alloy of the AA5182 or AA5754 type in the O / H111 temper.TABLE 1Thick-nessResult[mm]SiFeCuMnMgCrZnTi1Comp.2.50.1750.240.030.232.950.020.010.012Comp.2.50.2570.360.040.282.930.020.020.013Comp.1.20.1780.350.040.302.740.020.020.024Comp.1.20.2520.280.030.282.780.020.010.015Comp.0.850.1650.310.060.372.880.080.010.026Comp.1.20.1550.300.070.402.910.070.010.027Comp.1.20.1670.300.070.392.870.060.010.028Comp.2.50.1790.290.070.392.890.060.020.029Comp.2.50.1550.300.070.402.910.070.010.0210Comp.3.00.0880.170.020.293.490.020.010.0111Comp.3.00.1000.220.020.283.420.020.020.0212Comp.3.00.0840.180.020.263.350.010.020.0213Inv.1.20.2750.350.050.433.230.090.010.0214Inv.1.20.2840.320.070.383.040.080.010.0215Inv.2.50.2850.340.060.393.070.070.010.02*All values in wt. %, remainder being aluminum and unavoidable impurities, individually at most 0.05 wt. %, in total at most 0.15 wt. %TABLE 2Thick-Scrap nessRp0,2RmAgA80 mmabsorptionResult[mm][MPa][MPa][%][%]n5Score1Comp.2.510922319210, 3242Comp.2.510822019230, 32143Comp.1.210422320210, 34114Comp.1.210021621260, 34115Comp.0.8511923820210, 34156Comp.1.211423921240, 35157Comp.1.212624020220, 29158Comp.2.512423719230, 29129Comp.2.511924019240, 271510Comp.3.012125020250, 30111Comp.3.013025020250, 31112Comp.3.011924021260, 28113Inv.1.212425220230, 341814Inv.1.211624320250, 331815Inv.2.511824020200, 3218In Table 3, additional exemplary cold rolling pass sequences for the cold rolling E are provided. The cold rolling E can comprise two or more, for example three or four, cold rolling passes. The reduction rate for cold rolling E can be selected depending on the hot strip final thickness and the desired final thickness after the cold rolling.TABLE 3Hot strip finalCold rolling passReductionFinalthicknesssequencesratethickness[mm]thicknesses [mm][%][mm]2.82.8-1.5-0.85700.8544.0-2.7-1.9-1.2701.244.0-2.5-1.5631.56.86.8-4.5-3.4-2.3662.36.86.8-4.5-3.4-2.5632.5Finally, FIG. 2 schematically shows a component for a motor vehicle. The component consists at least partially of a rolled product which has been produced according to the method shown in FIG. 1. From the aluminum alloy strip, which was produced using the method shown in FIG. 1, sheets were cut, and an inner part of a body of a motor vehicle in the form of an inner door part was produced from these by means of deformations, for example drawing. Usually, these are made of steel. Due to the high strength and the high forming behavior, however, the rolled products according to the invention are preferably used for the production of inner body parts.

[0170] The disclosure also includes the following embodiments:

[0171] 1. Aluminum alloy having a composition comprising the following alloy components:

[0172] Si: 0.15 wt. % to 0.30 wt. %,

[0173] Fe: 0.20 wt. % to 0.35 wt. %,

[0174] Cu: 0.02 wt. % to 0.10 wt. %,

[0175] Mn: 0.35 wt. % to 0.45 wt. %,

[0176] Mg: 3.00 wt. % to 3.60 wt. %,

[0177] Cr: 0.02 wt. % to 0.10 wt. %,

[0178] Zn: at most 0.20 wt. %,

[0179] Ti: at most 0.05 wt. %,

[0180] remainder Al and unavoidable impurities, individually at most 0.05 wt. %, in total at most 0.15 wt. %.

[0181] 2. Aluminum alloy according to embodiment 1, wherein the alloy components Si, Fe, Cu, Mg, Cr and / or Zn have the following contents:

[0182] Si: 0.20 wt. % to 0.30 wt. %,

[0183] Fe: 0.25 wt. % to 0.35 wt. %,

[0184] Cu: 0.05 wt. % to 0.10 wt. %, preferably 0.05 wt. % to 0.08 wt. %,

[0185] Mg: 3.00 wt. % to 3.30 wt. %,

[0186] Cr: 0.05 wt. % to 0.10 wt. %,

[0187] Zn: at most 0.10 wt. %.

[0188] 3. Aluminum alloy according to embodiment 1 or 2, wherein the sum of Cu content and Cr content is >0.10 wt. %, when the Mg content is <3.30 wt. %.

[0189] 4. Aluminum alloy according to any one of embodiments 1 to 3, wherein the Cu content and the Cr content are each ≥0.05 wt. %, when the Mg content is <3.30 wt. %.

[0190] 5. Aluminum alloy according to any one of embodiments 1 to 4, wherein the sum of Cu content and Cr content is <0.10 wt. %, when the Mg content is >3.30 wt. %.

[0191] 6. Aluminum alloy according to any one of embodiments 1 to 5, wherein the Cu content and the Cr content are each <0.05 wt. %, when the Mg content is >3.30 wt. %.

[0192] 7. Aluminum alloy according to any one of embodiments 1 to 6, wherein the aluminum alloy achieves a total score of at least 16 points in an evaluation for the scrap absorption capacity, wherein the total score is obtained from the sum of the scores for the contents of Si, Fe, Cu, Mn, Cr, Zn and / or Ti of the aluminum alloy as follows:

[0193] Si content: <0.15 wt. % gives 0 points,

[0194] 0.15 wt. % to <0.25 wt. % gives 3 points,

[0195] ≥0.25 wt. % gives 6 points,

[0196] Fe content: <0.25 wt. % gives 0 points,

[0197] 0.25 wt. % to <0.30 wt. % gives 3 points,

[0198] ≥0.30 wt. % gives 6 points,

[0199] Cu content: <0.03 wt. % gives 0 points,

[0200] 0.03 wt. % to <0.05 wt. % gives 1 point,

[0201] ≥0.05 wt. % gives 2 points,

[0202] Mn content: <0.25 wt. % gives 0 points,

[0203] 0.25 wt. % to <0.35 wt. % gives 1 point,

[0204] ≥0.35 wt. % gives 2 points,

[0205] Cr content: <0.03 wt. % gives 0 points,

[0206] 0.03 wt. % to <0.05 wt. % gives 1 point,

[0207] ≥0.05 wt. % gives 2 points,

[0208] Zn content: <0.03 wt. % gives 0 points,

[0209] 0.03 wt. % to <0.05 wt. % gives 1 point,

[0210] ≥0.05 wt. % gives 2 points,

[0211] Ti content: <0.03 wt. % gives 0 points,

[0212] 0.03 wt. % to <0.05 wt. % gives 1 point,

[0213] ≥0.05 wt. % gives 2 points.

[0214] 8. Rolled product comprising an aluminum alloy according to any one of embodiments 1 to 7.

[0215] 9. Rolled product according to embodiment 8, wherein the rolled product in the O / H111 temper has a yield strength Rp0.2 of >110 MPa and a tensile strength Rm of >230 MPa, measured transverse to the rolling direction.

[0216] 10. Rolled product according to embodiment 8 or 9, wherein the rolled product in the O / H111 temper has a uniform elongation Ag of >18% and an elongation at break A80 mm of >20%.

[0217] 11. Rolled product according to any one of embodiments 8 to 10, wherein the rolled product has a thickness of 0.5 mm to 5 mm.

[0218] 12. Rolled product according to any one of embodiments 8 to 11, wherein the rolled product comprises a recycled content of at least 60%, preferably at least 80%.

[0219] 13. Method for producing a rolled product, in particular a rolled product according to any one of embodiments 8 to 12, the method comprising the following method steps:

[0220] providing a melt of an aluminum alloy having a composition comprising the following alloy components:

[0221] Si: 0.15 wt. % to 0.30 wt. %,

[0222] Fe: 0.20 wt. % to 0.35 wt. %,

[0223] Cu: 0.02 wt. % to 0.10 wt. %,

[0224] Mn: 0.35 wt. % to 0.45 wt. %,

[0225] Mg: 3.00 wt. % to 3.60 wt. %,

[0226] Cr: 0.02 wt. % to 0.10 wt. %,

[0227] Zn: at most 0.20 wt. %,

[0228] Ti: at most 0.05 wt. %,

[0229] remainder Al and unavoidable impurities, individually at most 0.05 wt. %, in total at most 0.15 wt. %,

[0230] casting the melt to form a rolling ingot,

[0231] homogenizing the rolling ingot at 480 °C to 550 °C for at least 0.5 h,

[0232] hot rolling the rolling ingot at a temperature of 280 °C to 520 °C,

[0233] cold rolling the rolled product to final thickness with a reduction rate of at least 40%,

[0234] soft annealing the finish-rolled rolled product at 300 °C to 550 °C.

[0235] 14. Method according to embodiment 13, wherein the soft annealing is carried out in a continuous furnace.

[0236] 15. Method according to embodiment 13 or 14, wherein the melt comprises a recycled content of at least 60%, preferably at least 80%.

[0237] 16. Component for a motor vehicle which consists at least partially of a rolled product according to any one of embodiments 8 to 12 and / or is produced by a method according to any one of embodiments 13 to 15.

[0238] All references, including publications, patent applications, and patents cited herein are hereby incorporated by reference to the same extent as if each reference were individually and specifically indicated to be incorporated by reference and were set forth in its entirety herein.

[0239] The use of the terms “a” and “an” and “the” and similar referents in the context of describing the invention (especially in the context of the following claims) is to be construed to cover both the singular and the plural, unless otherwise indicated herein or clearly contradicted by context. The terms “comprising,”“having,”“including,” and “containing” are to be construed as open-ended terms (i.e., meaning “including, but not limited to,”) unless otherwise noted. Recitation of ranges of values herein are merely intended to serve as a shorthand method of referring individually to each separate value falling within the range, unless otherwise indicated herein, and each separate value is incorporated into the specification as if it were individually recited herein. All methods described herein can be performed in any suitable order unless otherwise indicated herein or otherwise clearly contradicted by context. The use of any and all examples, or exemplary language (e.g., “such as”) provided herein, is intended merely to better illuminate the invention and does not pose a limitation on the scope of the invention unless otherwise claimed. No language in the specification should be construed as indicating any non-claimed element as essential to the practice of the invention.

[0240] Preferred embodiments of this invention are described herein, including the best mode known to the inventors for carrying out the invention. Variations of those preferred embodiments may become apparent to those of ordinary skill in the art upon reading the foregoing description. The inventors expect skilled artisans to employ such variations as appropriate, and the inventors intend for the invention to be practiced otherwise than as specifically described herein. Accordingly, this invention includes all modifications and equivalents of the subject matter recited in the claims appended hereto as permitted by applicable law. Moreover, any combination of the above-described elements in all possible variations thereof is encompassed by the invention unless otherwise indicated herein or otherwise clearly contradicted by context.

Claims

1. Aluminum alloy having a composition comprising the following alloy components:Si: 0.15 wt. % to 0.30 wt. %,Fe: 0.20 wt. % to 0.35 wt. %,Cu: 0.02 wt. % to 0.10 wt. %,Mn: 0.35 wt. % to 0.45 wt. %,Mg: 3.00 wt. % to 3.60 wt. %,Cr: 0.02 wt. % to 0.10 wt. %,Zn: at most 0.20 wt. %,Ti: at most 0.05 wt. %,remainder Al and unavoidable impurities, individually at most 0.05 wt. %, in total at most 0.15 wt. %,whereinthe aluminum alloy achieves a total score of at least 16 points in an evaluation for the scrap absorption capacity, wherein the total score is obtained from the sum of the scores for the contents of Si, Fe, Cu, Mn, Cr, Zn and / or Ti of the aluminum alloy as follows:Si content: <0.15 wt. % gives 0 points,0.15 wt. % to <0.25 wt. % gives 3 points,≥0.25 wt. % gives 6 points,Fe content: <0.25 wt. % gives 0 points,0.25 wt. % to <0.30 wt. % gives 3 points,≥0.30 wt. % gives 6 points,Cu content: <0.03 wt. % gives 0 points,0.03 wt. % to <0.05 wt. % gives 1 point,≥0.05 wt. % gives 2 points,Mn content: <0.25 wt. % gives 0 points,0.25 wt. % to <0.35 wt. % gives 1 point,≥0.35 wt. % gives 2 points,Cr content: <0.03 wt. % gives 0 points,0.03 wt. % to <0.05 wt. % gives 1 point,≥0.05 wt. % gives 2 points,Zn content: <0.03 wt. % gives 0 points,0.03 wt. % to <0.05 wt. % gives 1 point,≥0.05 wt. % gives 2 points,Ti content: <0.03 wt. % gives 0 points,0.03 wt. % to <0.05 wt. % gives 1 point,≥0.05 wt. % gives 2 points.

2. Aluminum alloy according to claim 1,whereinthe alloy components Si, Fe, Cu, Mg, Cr and / or Zn have the following contents:Si: 0.20 wt. % to 0.30 wt. %,Fe: 0.25 wt. % to 0.35 wt. %,Cu: 0.05 wt. % to 0.10 wt. %, preferably 0.05 wt. % to 0.08 wt. %,Mg: 3.00 wt. % to 3.30 wt. %,Cr: 0.05 wt. % to 0.10 wt. %,Zn: at most 0.10 wt. %.

3. Aluminum alloy according to claim 1,whereinthe sum of Cu content and Cr content is >0.10 wt. %, when the Mg content is <3.30 wt. %.

4. Aluminum alloy according to claim 1,whereinthe Cu content and the Cr content are each ≥0.05 wt. %, when the Mg content is <3.30 wt. %.

5. Aluminum alloy according to claim 1,whereinthe sum of Cu content and Cr content is <0.10 wt. %, when the Mg content is >3.30 wt. %.

6. Aluminum alloy according to claim 1,whereinthe Cu content and the Cr content are each <0.05 wt. %, when the Mg content is >3.30 wt. %.

7. Rolled product comprising an aluminum alloy according to claim 1.

8. Rolled product according to claim 7,whereinthe rolled product in the O / H111 temper has a yield strength Rp0.2 of >110 MPa and a tensile strength Rm of >230 MPa, measured transverse to the rolling direction.

9. Rolled product according to claim 7,whereinthe rolled product in the O / H111 temper has a uniform elongation Ag of >18% and an elongation at break A80 mm of >20%.

10. Rolled product according to claim 7,whereinthe rolled product has a thickness of 0.5 mm to 5 mm.

11. Rolled product according to claim 7,whereinthe rolled product comprises a recycled content of at least 60%, preferably at least 80%.

12. Method for producing a rolled product, in particular a rolled product according to claim 7, the method comprising the following method steps:providing a melt of an aluminum alloy having a composition comprising the following alloy components:Si: 0.15 wt. % to 0.30 wt. %,Fe: 0.20 wt. % to 0.35 wt. %,Cu: 0.02 wt. % to 0.10 wt. %,Mn: 0.35 wt. % to 0.45 wt. %,Mg: 3.00 wt. % to 3.60 wt. %,Cr: 0.02 wt. % to 0.10 wt. %,Zn: at most 0.20 wt. %,Ti: at most 0.05 wt. %,remainder Al and unavoidable impurities, individually at most 0.05 wt. %, in total at most 0.15 wt. %,wherein the aluminum alloy achieves a total score of at least 16 points in an evaluation for the scrap absorption capacity, wherein the total score is obtained from the sum of the scores for the contents of Si, Fe, Cu, Mn, Cr, Zn and / or Ti of the aluminum alloy as follows:Si content: <0.15 wt. % gives 0 points,0.15 wt. % to <0.25 wt. % gives 3 points,≥0.25 wt. % gives 6 points,Fe content: <0.25 wt. % gives 0 points,0.25 wt. % to <0.30 wt. % gives 3 points,≥0.30 wt. % gives 6 points,Cu content: <0.03 wt. % gives 0 points,0.03 wt. % to <0.05 wt. % gives 1 point,≥0.05 wt. % gives 2 points,Mn content: <0.25 wt. % gives 0 points,0.25 wt. % to <0.35 wt. % gives 1 point,≥0.35 wt. % gives 2 points,Cr content: <0.03 wt. % gives 0 points,0.03 wt. % to <0.05 wt. % gives 1 point,≥0.05 wt. % gives 2 points,Zn content: <0.03 wt. % gives 0 points,0.03 wt. % to <0.05 wt. % gives 1 point,≥0.05 wt. % gives 2 points,Ti content: <0.03 wt. % gives 0 points,0.03 wt. % to <0.05 wt. % gives 1 point,≥0.05 wt. % gives 2 points,casting the melt to form a rolling ingot,homogenizing the rolling ingot at 480 °C to 550 °C for at least 0.5 h,hot rolling the rolling ingot at a temperature of 280 °C to 520 °C,cold rolling the rolled product to final thickness with a reduction rate of at least 40%,soft annealing the finish-rolled rolled product at 300 °C to 550 °C.

13. Method according to claim 12,whereinthe soft annealing is carried out in a continuous furnace.

14. Method according to claim 12,whereinthe melt comprises a recycled content of at least 60%, preferably at least 80%.

15. Component for a motor vehicle which consists at least partially of a rolled product according to claim 7.

16. Component for a motor vehicle which is produced by a method according to claim 12.