Method of rebuilding a PEM electrolyzer
By forming unified assemblies and storing them in protective enclosures, the method addresses the challenge of cell damage during disassembly and enables the reuse of cells in PEM electrolyzers, enhancing rebuilding efficiency and reducing costs.
Patent Information
- Application Number
- US19/211436
- Authority / Receiving Office
- US · United States
- Patent Type
- Applications(United States)
- Current Assignee / Owner
- Filing Date
- 2025-05-19
- Publication Date
- 2026-11-19
AI Technical Summary
Disassembling a PEM electrolyzer stack is difficult without causing damage to other cell components, and once removed, traditional cell assemblies cannot be reused effectively.
The method involves forming unified assemblies of electrolyzer components, storing them in protective enclosures, and reusing them in different stacks or the original stack, using a unified cell configuration to prevent damage and facilitate rebuilding.
This approach allows for the reuse of removed cells without degrading other cells, reducing service costs and increasing flexibility and reliability by preventing wrinkling and other adverse impacts during rebuilding.
Smart Images

Figure US20260366175A1-D00000_ABST
Abstract
Description
BACKGROUND
[0001] This disclosure relates to electrochemical devices including unified layer arrangements and methods of fabrication.
[0002] Electrolyzers are known electrochemical devices that may be configured to convert electricity and water into hydrogen and oxygen. Electrolyzers comprising proton exchange membrane (PEM) electrolyzer cell assemblies provide a variety of challenges. A PEM electrolyzer stack is traditionally comprised of a series of PEM cell assemblies that are positioned between bi-polar plates in an alternating fashion. Under certain conditions, one or more of the cell assemblies may cease to function properly. When dis-assembling the PEM electrolyzer stack, it is typically difficult to prevent damage to other cells in the electolyzer stack.SUMMARY
[0003] A method of building an electrochemical device according to an implementation may include: forming at least one unified assembly including one or more electrolyzer components; forming an electrolyzer by stacking a plurality of electrolyzer cell assemblies on each other to provide a first electrolyzer stack, wherein at least one electrolyzer cell assembly of the plurality of electrolyzer cell assemblies includes the at least one unified assembly; at least partially unstacking the first electrolyzer stack by removing at least some electrolyzer cell assemblies from the first electrolyzer stack, including removing the electrolyzer cell assembly that includes the at least one unified assembly; and rebuilding the first electrolyzer stack with a removed electrolyzer cell assembly that includes the at least one unified assembly or building a second electrolyzer stack with the removed electrolyzer cell assembly that includes the at least one unified assembly.
[0004] In any implementations, the method may include storing the removed electrolyzer cell assembly in a protective enclosure.
[0005] In any implementations, the method may include the protective enclosure comprising a sealed enclosure made from a water-impermeable material.
[0006] In any implementations, the method may include the protective enclosure comprising a mylar bag.
[0007] In any implementations, the method may include removing the removed electrolyzer cell assembly from the protective enclosure and re-installing the removed electrolyzer cell assembly in the first electrolyzer stack or installing the removed electrolyzer cell assembly in the second electrolyzer stack.
[0008] In any implementations, the method may include rebuilding the first electrolyzer stack with the removed electrolyzer cell assembly.
[0009] In any implementations, the method may include rebuilding the second electrolyzer stack with the removed electrolyzer cell assembly.
[0010] In any implementations, the method may include operating the first electrolyzer stack over time, subsequently identifying one or more damaged electrolyzer cell assemblies from the plurality of electrolyzer cell assemblies, removing the one or more damaged electrolyzer cell assemblies, removing the electrolyzer cell assembly that includes the at least one unified assembly, installing an operational electrolyzer cell assembly to replace each damaged electrolyzer cell assembly, and re-installing the removed electrolyzer cell assembly.
[0011] In any implementations, the method may include each electrolyzer cell assembly of the plurality of electrolyzer cell assemblies having the at least one unified assembly.
[0012] In any implementations, the method may include stacking each electrolyzer cell assembly of the plurality of electrolyzer cell assemblies between an adjacent set of bi-polar separator plates.
[0013] In any implementations, the method may include the one or more electrolyzer components comprising one or more PEM electrolyzer components, and wherein the electrolyzer comprises a PEM electrolyzer, and wherein the at least one unified assembly comprises at least one of an anode unified assembly, a cathode unified assembly, and a unified cell assembly including an anode portion and a cathode portion.
[0014] In any implementations, the method may include the one or more electrolyzer components comprising one or more PEM electrolyzer components, and wherein the electrolyzer comprises a PEM electrolyzer, and wherein the at least one unified assembly includes a catalyst coated membrane comprising an anode catalyst layer, a proton exchange membrane, and a cathode catalyst layer, and wherein an outer peripheral edge of the catalyst coated membrane is completely encapsulated in a thermoplastic material.
[0015] In any implementations, the method may include the at least one unified assembly having a gas diffusion layer and / or a porous transport layer that is integrally formed with the catalyst coated membrane.
[0016] An electrolyzer stack according to an implementation may include the removed electrolyzer cell as described anywhere herein, and a plurality of additional electrolyzer cell assemblies stacked to form a rebuilt electrolyzer stack.
[0017] In any implementations, the electrolyzer stack may include each electrolyzer cell assembly of the plurality of electrolyzer cell assemblies having the at least one unified assembly.
[0018] In any implementations, the electrolyzer stack may include each electrolyzer cell assembly of the plurality of electrolyzer cell assemblies being stacked between an adjacent set of bi-polar separator plates.
[0019] In any implementations, the electrolyzer stack may include the one or more electrolyzer components comprising one or more PEM electrolyzer components, and wherein the rebuilt electrolyzer stack comprises a rebuilt PEM electrolyzer stack, wherein the at least one unified assembly comprises at least one of an anode unified assembly, a cathode unified assembly, and a unified cell assembly including an anode portion and a cathode portion.
[0020] In any implementations, the electrolyzer stack may include the at least one unified assembly having a catalyst coated membrane comprising an anode catalyst layer, a proton exchange membrane, and a cathode catalyst layer, and wherein an outer peripheral edge of the catalyst coated membrane is completely encapsulated in a thermoplastic material.
[0021] In any implementations, the electrolyzer stack may include the at least one unified assembly having a gas diffusion layer or a porous transport layer that is integrally formed with the catalyst coated membrane.
[0022] In any implementations, the electrolyzer stack may include the at least one unified assembly having a gas diffusion layer and a porous transport layer that are integrally formed with the catalyst coated membrane.
[0023] The present disclosure may include any one or more of the individual features disclosed above and / or below alone or in any combination thereof.
[0024] Various features and advantages of at least one disclosed example embodiment will become apparent to those skilled in the art from the following detailed description. The drawing that accompanies the detailed description can be briefly described as follows.BRIEF DESCRIPTION OF THE DRAWINGS
[0025] FIG. 1 schematically illustrates a selected portion of an electrochemical device.
[0026] FIG. 2 is a schematic representation of a PEM electrolyzer according to an implementation.
[0027] FIG. 3 is a schematic representation of a stacked PEM electrolyzer according to an implementation.
[0028] FIG. 4 is a schematic representation of a bonding process / lay-up for a unified cell assembly according to an implementation.
[0029] FIG. 5 shows the unified cell assembly of FIG. 3 with a bipolar separation plate.
[0030] FIG. 6 is a schematic representation of removing, storing, and re-using a cell assembly.
[0031] FIG. 7 shows a method of building an electrochemical device such as a PEM electrolyzer.
[0032] Like reference numbers and designations in the various drawings indicate like elements.DETAILED DESCRIPTION
[0033] The subject disclosure relates to a method of rebuilding an electrochemical device such as a PEM electrolyzer stack using previously used and unstacked cell assemblies, which may include a unified assembly of one or more PEM electrolyzer components.
[0034] FIG. 1 schematically discloses an electrochemical device (e.g., assembly) 20 according to an implementation. The electrochemical device 20 may be an electrolyzer assembly such as a proton exchange membrane water electrolysis (PEMWE). The operation of an electrolyzer assembly is known and it should be understood that the PEMWE is just one example of an electrolyzer, other types could also be used. The teachings disclosed herein may be utilized with other electrochemical devices, such as a fuel cell. The electrochemical device 20 may incorporate any of the features disclosed herein. In the implementation of FIG. 1, a PEM 22 is situated between an anode catalyst layer 24 and a cathode catalyst layer 26. An anode portion 28 includes an anode flowfield component 30 and an anode transport layer 32. A cathode portion 34 includes a cathode flowfield component 36 and a cathode transport layer 38. FIG. 1 shows O2 being generated on and removed from the anode 28 and H2 generated on and removed from a cathode 34. A power source 40 may be operable to supply current to facilitate an electrolysis reaction for producing hydrogen and oxygen, for example.
[0035] FIG. 2 shows an example of a PEMWE 50 according to one implementation. In this example, the PEMWE 50 includes an anode side bipolar plate (BPP) 52, an anode side porous transfer layer (PTL) 54, an anode catalyst layer 56, a proton exchange membrane (PEM) 58, a cathode catalyst layer 60, a cathode side PTL 62, and a cathode side BPP 64.
[0036] In some implementations, frames F may be associated with the anode side PTL 54 and / or the cathode side PTL 62. The frames F may have various geometries. In implementations, the frame F may be dimensioned to follow a perimeter of the PTL 54, 62.
[0037] In some implementations, one or more of the individual cell components may be integrated with the frame to form a unified assembly. In some implementations, the frames F are removed and one or more of the individual cell components may be integrated together to form a unified assembly. This will be discussed in greater detail below.
[0038] The anode side BPP 52 of FIG. 2 comprises an anode flow field plate that distributes water evenly across the anode side, conducts electrons out of the cell, and provides channels for oxygen (O2) gas removal.
[0039] The anode side PTL 54 may comprise a combination of a PTL and a gas diffusion layer (GDL) 55 for the anode side. The anode side PTL 54 ensures uniform water delivery to the catalyst layer, allows oxygen (O2) gas to escape, and provides electrical conductivity. The GDL 55 may enhance gas diffusion and conductivity. The anode side PTL 54 may include materials such as titanium felt, sintered porous titanium, or other similar corrosion-resistant materials, for example.
[0040] The anode catalyst layer 56 provides for an oxygen evolution reaction (OER) and may be made of iridium or iridium oxide (IrO2) due to its stability in acidic environments. The anode catalyst layer 56 promotes the reaction:H2O→O2+4H++4e−
[0041] The PEM 58 may comprise Nafion® or other perfluorosulfonic acid membranes, for example. The PEM 58 conducts H+ (protons) from the anode to the cathode and is electrically insulating but ionically conductive.
[0042] The cathode catalyst layer 60 provides for a hydrogen evolution reaction (HER) and is typically platinum (Pt) based.
[0043] The cathode catalyst layer 60 promotes the reaction:4H++4e−→2H2
[0044] The cathode side PTL 62 may comprise a combination of a PTL and GDL 63 for the cathode side. The cathode side PTL 62 transports hydrogen gas (H2) away from the catalyst layer and ensures electrical conductivity. The GDL 63 may enhance gas diffusion and conductivity. The cathode side PTL 62 may include materials such as carbon paper (for fuel cells) or sintered stainless steel (for PEMWE to avoid corrosion), for example.
[0045] The cathode side BPP 64 comprises a cathode flow field / plate that distributes hydrogen gas evenly, conducts electrons into the cell, and channels for hydrogen (H2) gas removal.
[0046] In some implementations, combinations of stacked layers may be referred to as active cell components. For example, active cell components may include the anode side PTL 54, the cathode side PTL 62, and / or a catalyst coated membrane (CCM). The CCM may be comprised of the anode catalyst layer 56, the PEM 58, and / or the cathode catalyst layer 60. The active cell components exclude the frames F.
[0047] It should be understood that the configuration shown in FIG. 2 is just an example configuration and other configurations of stacked active cell components may also be contemplated.
[0048] As discussed above, one or more of the active components may be integrated together to form one or more unified partial cell assemblies or a complete unified cell assembly. For example, there may be a unified anode assembly 70, a unified cathode assembly 72, or a unified cell assembly 74 that includes both an anode portion and a cathode portion. The anode and cathode portions may comprise the unified anode assembly 70 and the unified cathode assembly 72, respectively, or in some implementations, the layers may be individually stacked and then integrated together to form the unified cell assembly 74. In some implementations, the unified cell assembly 74 may include only one of the unified anode assembly 70 and the unified cathode assembly 72 with the other comprising stacked layers in any combination thereof. The assembly 70 / 72 / 74 may be unified to establish a unitary construction such that separation of adjacent layers may cause damage to the layers.
[0049] FIG. 3 discloses a stacked PEM electrolyzer 76 according to an implementation. The stacked PEM electroylzer 76 may have a unified cathode assembly 72 positioned on one side of a bipolar separator plate 78 with a unified anode assembly 70 positioned on an opposite side of the bipolar separator plate 78. A membrane electrode assembly (MEA) or CCM 80 (combination of the anode catalyst layer 56, the PEM 58, and / or the cathode catalyst layer 60) may be positioned on an opposite side of the unified cathode assembly 72 from the bipolar separator plate 54. Another CCM 80′ may be positioned on an opposite side of the unified anode assembly 70 from the bipolar separator plate 54. Another unified cathode assembly 72′ may be positioned on an opposite side of the CCM 80′, with another bipolar separator plate 78′ being stacked thereon. Another unified anode assembly 70′ may be stacked on an opposite side of the CCM 80 from the unified cathode assembly 72, with another bipolar separator plate 78″ being stacked thereon.
[0050] In this example, between each set of adjacent bipolar separator plates 78, a cell assembly 82 is provided where the cell assembly 82 may include one unified cathode assembly 72, one CCM 80, and one unified anode assembly 70. In other words, there is one cell assembly 82 provided between bipolar separator plate 78 and bipolar separator plate 78′, and another cell assembly 82 provided between bipolar separator plate 78 and bipolar separator plate 78″. This stacking process may be continued as needed to provide a required number of cell assemblies 82 for the stacked PEM electroylzer 76.
[0051] In an implementation of FIG. 4, a gas diffusion layer (GDL) 84, the CCM 80, and a porous transport layer (PTL) 86 may be combined into one laminated structure to establish a unified assembly. A thermoplastic bond film 88 may be used to secure layers together and establish an edge seal, which may avoid the need for a separate cell frame and active area. In implementations, the porous substrate may be impregnated or coated with an uncured material that may be cured in place. In implementations, a CCM edge 90 can be encapsulated by the established edge seal as shown in FIG. 5.
[0052] In implementations, on a cathode side of the cell assembly, the thermoplastic material may impregnate the GDL 84 to establish the unified cathode assembly 72. In implementations, the GDL 84 may be a porous conductive substrate that establishes a flow field. In implementations, the thermoplastic film 88 may impregnate a reinforcement layer, such as mesh for example, along a periphery of the GDL 84. In other implementations, the thermoplastic film 88 may be hot pressed onto a substrate.
[0053] Similarly, on an anode side of the cell assembly, thermoplastic material may impregnate the PTL 86 to establish the unified anode assembly 70. In implementations, the thermoplastic film 88 may impregnate a reinforcement layer along a periphery of a porous conductive substrate of the PTL 86.
[0054] FIG. 5 shows an implementation of a bonding process / lay-up method where the GDL 84, the CCM 80, and the PTL 86 are combined into one laminated structure 94. The CCM 80 comprises a PEM 58 with a cathode catalyst 60 on one side and an anode catalyst 56 on an opposite side (FIG. 4). The GDL 84 is positioned on one side of the CCM 80 and the PTL 86 is positioned on an opposite side of the CCM 80. The thermoplastic film 88 is impregnated within outer peripheral edges of the GDL 84 and the PTL 86 to form the laminated structure 94 to have a sealed outer edge 92 as shown in FIG. 5. In implementations, the sealed outer edge 92 extends about an entirety of a periphery of the assembly.
[0055] Various materials may be utilized to establish the film layer. In implementations, the film layer comprises materials that are cure-in-place, such as certain plastics (DuPont PVF “Tedlar” for example, or cross-linked polymers), UV / heat / reaction cured resins, etc. The porous substrates are impregnated or coated the with the uncured material that is then cured in place.
[0056] In some implementations, the laminated structure 94 includes at least one reinforcement 96 impregnated by the thermoplastic film 88. In the example shown in FIGS. 4-5, the reinforcement 96 is part of the PTL 86. The reinforcement 96 may be situated on the anode side. In implementations, the reinforcement may be provided about an entirety of the outer peripheral edge of the PTL 86. In implementations, the reinforcement 96 may comprise a woven fiber material, e.g., glass or carbon fiber fabric, or other similar types of reinforcing materials. In other implementations, the reinforcement 96 may comprise fibrous material such as spun fiber, loose fiber, etc.
[0057] In some implementations, a first layer 98 of bond film 88 may be positioned between the GDL 84 and the CCM 80 and a second layer 100 of bond 88 may be positioned between the PTL 86 and the CCM 80. In implementations, in order to form the laminated structure 94, the various layers are positioned between a first, e.g. upper, platen 102 and a second, e.g. lower, platen 104. These platens 102, 104 are pressed together to form the sealed outer edge 92 of the laminated structure 94. When the platens 102, 104 are pressed together, steps of heating and curing can occur in a known manner to form the sealed outer edge 92. In some implementations, release film layers 106 are positioned between each platen 102, 104 and the respective GDL 84 and PTL 86 to facilitate the release of the laminated structure 94 from the platens 102, 104.
[0058] As shown in FIG. 5, the outer edges of the GDL 84, PTL 96, and reinforcement 96 are all impregnated with the thermoplastic material to form laminated structure 94. The outer edge 90 of the CCM 80 may be completely encapsulated as shown.
[0059] The laminated structure 94 may then be placed on one side of the bipolar separation plate 78. Another laminated structure 94 may be placed on an opposite side of the bipolar separation plate 78. Another, bipolar separation plate 78 may then be stacked on that laminated structure 94, and the stacking of plates 78 and laminated structures 94 can be continued until a desired number of structures 94 are provided.
[0060] In some implementations, porting 108 may be formed to extend through the plate 78 and the laminated structure 94, which can be used to direct fluid flow through the assembly. In some implementations, additional porting 110 may be provided in the bipolar separation plate 78. Seals 112 may then be installed in the bipolar separation plate 78 to prevent or otherwise reduce a likelihood of leakage from the porting 108, 110.
[0061] The implementation of FIGS. 4-5 is only one example of forming a unified cell structure (e.g., assembly). Other implementations of forming unified structures are also contemplated, such as those disclosed in application Ser. No. 18 / 789,953, filed on Jul. 31, 2024, which is assigned to the assignee of the subject application, and which is incorporated herein in its entirety.
[0062] As discussed above, one or more active cell components may be integrated together to form one or more unified partial cell assemblies or a complete unified cell assembly. The unified anode assembly 70, the unified cathode assembly 72, and the unified cell assembly 74 are just examples of integrated formations. The unified assembly may be comprised of one or more of the PEM electrolyzer components stacked in any combination of layers. Further, partial integrated cell assemblies may also be integrated together to form a complete integrated cell assembly.
[0063] In some implementations, once a complete cell assembly 82 is formed, the cell assemblies 82 are then stacked on top of each other to form a stacked PEM electroylzer 76 (FIG. 3). The cell assemblies that are stacked may include one or more cell assemblies that include unified structures. The cell assemblies that are stacked may also include cell assemblies that do not include unified structures. Non-unified cells and unified cells may be stacked in any combination thereof. The stack may also include only unified cells.
[0064] Under certain conditions, after operating over time, one or more of the cell assemblies may cease to function properly. When dis-assembling the stacked PEM electrolyzer 76, it may be difficult to prevent damage to components within a cell and / or other cells in the electrolyzer stack. Further, once traditionally formed cells, e.g. non-unified cells, are removed they are not able to be re-used.
[0065] However, in some implementations, it has been determined that using a unified cell configuration prevents wrinkling and other adverse impacts that may permanently damage cell performance and durability during a rebuild process. By using a unified cell integration approach, a cell that was completely removed from a stack may be re-used at a later time. For example, the cell may used in another build for a different cell stack, or the cell may be re-used in the existing cell stack from which it was originally removed. The cell and / or (e.g., unified) components may be reinstalled in the same position or in another position within the cell stack.
[0066] In some implementations, one or more cells 82′ may be removed from a first stack and then may be immediately re-used in another, second stack, or may be reused in the same stack once damaged cells are replaced.
[0067] In some implementations, one or more cells 82′ may be removed from a first stack 76 and stored in a protective enclosure 114 (e.g., container), such as a bag for example, as shown in FIG. 6. The protective enclosure may be suitable for maintaining hydration of component(s) of the cell 82′.
[0068] In some implementations, the one or more cells 82′ are hydrated and stored in protective enclosures that comprise plastic bags, e.g. mylar bags. A mylar bag is a type of packaging made from mylar, which is a material comprising a polyester film referred to as biaxially-oriented polyethylene terephthalate (BoPET). This type of material is durable, lightweight, and has strong barrier properties. For example, these types of bags are able to provide an oxygen barrier, a moisture barrier, and a light barrier; as well as being heat sealable to create an airtight enclosure.
[0069] In some implementations, the removed cells 82′ may then be removed from the protective enclosure 114 and installed in a second stack 76′ as shown in FIG. 6. As such, the use of a unified cell configuration facilities rebuilding a stack without impacting or degrading other existing cells in the stack. Also, it provides the ability to completely remove axial loads on other cells in stack. Further, cells may be handled without special equipment and there is the ability to modify the order of cells within the stack. This results in lower service cost, increased reliability, and increased flexibility.
[0070] A method of building an electrochemical device such as PEM electrolyzer is disclosed in FIG. 7. Although the method primarily refers to a PEM electrolyzer, the method may be utilized with any of the electrochemical devices disclosed herein. Fewer or additional steps than are recited below could be performed within the scope of this disclosure, and the recited order of steps is not intended to limit this disclosure.
[0071] At step 200, at least one unified assembly is formed to include one or more PEM electrolyzer components. At step 300, a PEM electrolyzer is formed by stacking a plurality of PEM cell assemblies and / or components on top of each other to provide a first PEM electrolyzer stack, wherein at least one PEM cell assembly of the plurality of PEM cell assemblies includes the unified assembly. At step 400, the first PEM electrolyzer stack is at least partially unstacked by removing at least some of the PEM cell assemblies from the first PEM electrolyzer stack, including removing the PEM cell assembly that includes the unified assembly. At step 500, the first PEM electrolyzer stack is rebuilt with a removed PEM cell assembly that includes the unified assembly or a second PEM electrolyzer stack is built with the removed PEM cell assembly that includes the unified assembly.
[0072] Additional method steps may be used either alone or in any combination thereof. The method may include storing the removed PEM cell assembly in a protective enclosure.
[0073] The method may include the protective enclosure comprising a sealed enclosure made from a water-impermeable material.
[0074] The method may include the protective enclosure comprising a mylar bag.
[0075] The method may include removing the removed PEM cell assembly from the protective enclosure and re-installing the removed PEM cell assembly in the first PEM electrolyzer stack, or installing the removed PEM cell assembly in the second PEM electrolyzer stack.
[0076] The method may include rebuilding the first PEM electrolyzer stack with the removed PEM cell assembly.
[0077] The method may include building the second PEM electrolyzer stack that includes the removed PEM cell assembly.
[0078] The method may include operating the first PEM electrolyzer stack over time, subsequently identifying one or more damaged PEM cell assemblies from the plurality of PEM cell assemblies, removing the one or more damaged PEM cell assemblies, removing the PEM cell assembly that includes the unified assembly, installing an operational PEM cell assembly to replace each damaged PEM cell assembly, and re-installing the removed PEM cell assembly.
[0079] The method may include each PEM cell assembly of the plurality of PEM cell assemblies including the unified assembly.
[0080] The method may include stacking each PEM cell assembly of the plurality of PEM cell assemblies between an adjacent set of bi-polar separator plates.
[0081] The method may include the unified assembly comprising at least one of an anode unified assembly, a cathode unified assembly including cathode portion, and / or a unified cell assembly including an anode portion.
[0082] The method may include the unified assembly including a catalyst coated membrane comprising an anode catalyst layer, a proton exchange membrane, and a cathode catalyst layer, wherein an outer peripheral edge of the catalyst coated membrane is completely encapsulated in a thermoplastic material.
[0083] The method may include the unified assembly including a gas diffusion layer and / or a porous transport layer that is integrally formed with the catalyst coated membrane.
[0084] The preceding description is illustrative rather than limiting in nature. Variations and modifications to the disclosed examples may become apparent to those skilled in the art that do not necessarily depart from the essence of this invention.
Claims
1. A method of building an electrochemical device comprising:forming at least one unified assembly including one or more electrolyzer components;forming an electrolyzer by stacking a plurality of electrolyzer cell assemblies on each other to provide a first electrolyzer stack, wherein at least one electrolyzer cell assembly of the plurality of electrolyzer cell assemblies includes the at least one unified assembly;at least partially unstacking the first electrolyzer stack by removing at least some electrolyzer cell assemblies from the first electrolyzer stack, including removing the electrolyzer cell assembly that includes the at least one unified assembly; andrebuilding the first electrolyzer stack with a removed electrolyzer cell assembly that includes the at least one unified assembly or building a second electrolyzer stack with the removed electrolyzer cell assembly that includes the at least one unified assembly.
2. The method as recited in claim 1, including storing the removed electrolyzer cell assembly in a protective enclosure.
3. The method as recited in claim 2, wherein the protective enclosure comprises a sealed enclosure made from a water-impermeable material.
4. The method as recited in claim 2, wherein the protective enclosure comprises a mylar bag.
5. The method as recited in claim 2, including removing the removed electrolyzer cell assembly from the protective enclosure and re-installing the removed electrolyzer cell assembly in the first electrolyzer stack or installing the removed electrolyzer cell assembly in the second electrolyzer stack.
6. The method as recited in claim 1, including rebuilding the first electrolyzer stack with the removed electrolyzer cell assembly.
7. The method as recited in claim 1, including rebuilding the second electrolyzer stack with the removed electrolyzer cell assembly.
8. The method as recited in claim 1, including operating the first electrolyzer stack over time, subsequently identifying one or more damaged electrolyzer cell assemblies from the plurality of electrolyzer cell assemblies, removing the one or more damaged electrolyzer cell assemblies, removing the electrolyzer cell assembly that includes the at least one unified assembly, installing an operational electrolyzer cell assembly to replace each damaged electrolyzer cell assembly, and re-installing the removed electrolyzer cell assembly.
9. The method as recited in claim 1, wherein each electrolyzer cell assembly of the plurality of electrolyzer cell assemblies includes the at least one unified assembly.
10. The method as recited in claim 1, including stacking each electrolyzer cell assembly of the plurality of electrolyzer cell assemblies between an adjacent set of bi-polar separator plates.
11. The method as recited in claim 1, wherein the one or more electrolyzer components comprise one or more PEM electrolyzer components, and wherein the electrolyzer comprises a PEM electrolyzer, and wherein the at least one unified assembly comprises at least one of an anode unified assembly, a cathode unified assembly, and a unified cell assembly including an anode portion and a cathode portion.
12. The method as recited in claim 1, wherein the one or more electrolyzer components comprise one or more PEM electrolyzer components, and wherein the electrolyzer comprises a PEM electrolyzer, and wherein the at least one unified assembly includes a catalyst coated membrane comprising an anode catalyst layer, a proton exchange membrane, and a cathode catalyst layer, and wherein an outer peripheral edge of the catalyst coated membrane is completely encapsulated in a thermoplastic material.
13. The method as recited in claim 12, wherein the at least one unified assembly includes a gas diffusion layer and / or a porous transport layer that is integrally formed with the catalyst coated membrane.
14. An electrolyzer stack including:the removed electrolyzer cell assembly according to claim 1; anda plurality of additional electrolyzer cell assemblies stacked to form a rebuilt electrolyzer stack.
15. The electrolyzer stack as recited in claim 14, wherein each electrolyzer cell assembly of the plurality of electrolyzer cell assemblies includes the at least one unified assembly.
16. The electrolyzer stack as recited in claim 14, wherein each electrolyzer cell assembly of the plurality of electrolyzer cell assemblies is stacked between an adjacent set of bi-polar separator plates.
17. The electrolyzer stack as recited in claim 14, wherein the one or more electrolyzer components comprise one or more PEM electrolyzer components, and wherein the rebuilt electrolyzer stack comprises a rebuilt PEM electrolyzer stack, wherein the at least one unified assembly comprises at least one of an anode unified assembly, a cathode unified assembly, and a unified cell assembly including an anode portion and a cathode portion.
18. The electrolyzer stack as recited in claim 14, wherein the at least one unified assembly includes a catalyst coated membrane comprising an anode catalyst layer, a proton exchange membrane, and a cathode catalyst layer, and wherein an outer peripheral edge of the catalyst coated membrane is completely encapsulated in a thermoplastic material.
19. The electrolyzer stack as recited in claim 18, wherein the at least one unified assembly includes a gas diffusion layer or a porous transport layer that is integrally formed with the catalyst coated membrane.
20. The electrolyzer stack as recited in claim 18, wherein the at least one unified assembly includes a gas diffusion layer and a porous transport layer that are integrally formed with the catalyst coated membrane.