Processing device and processing method

The processing device and method address the challenge of ensuring membrane contact and simplifying equipment structure by using mandrel and wedge blocks to control membrane tension, achieving reliable bending of composite laminates without vacuum systems, thus reducing costs and improving maintainability.

WO2024241602A1PCT designated stage expired Publication Date: 2024-11-28MITSUBISHI HEAVY IND LTD
View PDF 6 Cites 0 Cited by

Patent Information

Application Number
PCT/JP2023/036294
Authority / Receiving Office
WO · WO
Patent Type
Applications
Current Assignee / Owner
Priority Date
2023-05-23
Filing Date
2023-10-04
Publication Date
2024-11-28

Smart Images

  • Figure JP2023036294_28112024_PF_FP_ABST
    Figure JP2023036294_28112024_PF_FP_ABST
Patent Text Reader

Abstract

The processing device is provided with: a pair of a first mandrel block (10) and a second mandrel block (20) having side surfaces and upper surfaces and a laminate installed at the connection of the side surfaces and upper surfaces; a wedge block (30) disposed so as to protrude in the Z-axis direction between the first mandrel block (10) and the second mandrel block (20); a membrane (40) that covers the first mandrel block (10) and the second mandrel block (20) and the wedge block (30); and a drive unit that moves the first mandrel block (10) and the second mandrel block (20) apart. The membrane (40) is pulled along with the movement of the first mandrel block (10) and the second mandrel block (20). The wedge block (30) moves so that the protrusion length decreases along with the movement of the first mandrel block (10) and the second mandrel block (20).
Need to check novelty before this filing date? Find Prior Art

Description

Processing device and processing method

[0001] The present disclosure relates to a processing apparatus and a processing method.

[0002] Long components (e.g., stringers) used in aircraft and the like have a predetermined cross-sectional shape (e.g., L-shaped, C-shaped, etc.) when cut along a plane perpendicular to the longitudinal direction. One known method for manufacturing such components involves bending a flat laminate formed by stacking fiber-reinforced composite sheets. In this method, in order to evenly compress the entire surface of the laminate during bending, the laminate placed in a mold may be covered with a flexible membrane that is stretchable in the in-plane direction, and a vacuum may be drawn between the membrane and the mold. In this method, it is known that the membrane is controlled to adhere appropriately to the laminate (e.g., Patent Documents 1 and 2).

[0003] Patent Document 1 discloses a method in which a laminate is covered with a membrane and then bent and shaped by vacuuming. In this method, membranes are placed on both the top and bottom sides of the laminate, and membrane support portions are provided at positions away from the mold. Furthermore, the tension of the membrane placed below the laminate is controlled so that the membrane placed above the laminate is continuously brought into close contact with the mold from the top surface toward the bottom.

[0004] Furthermore, Patent Document 2 discloses a method in which a laminate is covered with a membrane and a plate supporting the bendable portion is mechanically lowered while a vacuum is drawn between the membrane and the mold. In this method, the position of the support plate controls the position at which the membrane comes into close contact.

[0005] U.S. Patent No. 10,016,949 U.S. Patent No. 11,313,089

[0006] However, in the method described in Patent Document 1, the membrane is controlled only by the tension of the membrane due to vacuuming, so that it is not possible to suitably control the membrane, and there are cases where the membrane cannot be tightly attached to the laminate. Also, the method described in Patent Document 2 requires the installation of equipment such as a pump and piping for vacuuming, as well as a mechanism for lowering the support plate, which may complicate the structure, increase costs, and reduce maintainability.

[0007] The present disclosure has been made in view of the above circumstances, and aims to provide a processing device and a processing method that can suitably bring a membrane into close contact with a workpiece, and also aims to provide a processing device and a processing method that can simplify the structure.

[0008] In order to solve the above problems, the processing apparatus and processing method of the present disclosure employ the following measures. a pair of mandrel blocks arranged side by side in a predetermined direction; a wedge block arranged between the pair of mandrel blocks so as to protrude from the second surface of the mandrel block in an intersecting direction intersecting the predetermined direction; and a membrane covering the workpiece, the mandrel block, and the wedge block while placed on the mandrel blocks; wherein one or both of the pair of mandrel blocks are movable in the predetermined direction so as to move the mandrel blocks apart in the predetermined direction; the membrane is pulled in the predetermined direction in response to the movement of the mandrel blocks in the predetermined direction; and the wedge block moves in the intersecting direction in response to the movement of the mandrel blocks in the predetermined direction so as to shorten the length of its protrusion from the second surface.

[0009] A processing method according to one aspect of the present disclosure is a processing method for performing a bending process on a plate-shaped workpiece, the method including a workpiece setting step of setting the workpiece at a connection between a pair of mandrel blocks arranged side by side in a predetermined direction, the pair of mandrel blocks having a first surface and a second surface extending in a bent or curved manner from an end of the first surface, the workpiece being placed at the connection between the first surface and the second surface; a wedge block setting step of setting a wedge block between the pair of mandrel blocks so as to protrude from the second surface of the mandrel block in a direction intersecting the predetermined direction; and a bending process of the workpiece placed on the mandrel blocks. The method includes an installation process of installing a membrane to cover the mandrel block and the wedge block, and a movement process of moving one or both of the pair of mandrel blocks in the predetermined direction so that the mandrel blocks are spaced apart in the predetermined direction, wherein the movement process involves the mandrel block pulling the membrane in the predetermined direction in response to the movement of the mandrel block in the predetermined direction, and the movement process involves the wedge block moving in the intersecting direction in response to the movement of the mandrel block in the predetermined direction so that the protruding length from the second surface is shortened.

[0010] According to the present disclosure, the membrane can be suitably attached to the workpiece, and the structure can be simplified.

[0011] FIG. 1 is a perspective view showing a composite material structure according to a first embodiment of the present disclosure. FIG. 2 is a perspective view showing a processing device according to a first embodiment of the present disclosure. FIG. 3 is a perspective view showing a main part of a processing device according to a first embodiment of the present disclosure. FIG. 4 is a schematic plan view showing a main part of a processing device according to a first embodiment of the present disclosure. FIG. 5 is a schematic front view showing a processing device according to a first embodiment of the present disclosure. FIG. 6 is a schematic front view showing a processing device according to a first embodiment of the present disclosure. FIG. 7 is a schematic front view showing a processing device according to a second embodiment of the present disclosure. FIG. 8 is a schematic front view showing a processing device according to a third embodiment of the present disclosure.

[0012] Hereinafter, embodiments of a processing apparatus and a processing method according to the present disclosure will be described with reference to the drawings.

[0013] First Embodiment A first embodiment of the present disclosure will be described below with reference to FIGS. 1 to 8. In the following description, the direction in which the mandrel block moves will be referred to as the X-axis direction. The direction in which the wedge block moves will be referred to as the Z-axis direction. The direction perpendicular to the X-axis direction and the Z-axis direction will be referred to as the Y-axis direction. In the following description, the Z-axis direction will be referred to as the up-down direction, and therefore the Z-axis direction may also be referred to as the up-down direction.

[0014] The shaping device according to this embodiment is used to manufacture a composite structure 2 (see FIG. 1) from a plate-like laminate (see FIG. 5, etc.) 1 formed by stacking fiber sheets 3 (see FIG. 1) impregnated with a resin such as prepreg. Specifically, it is used to bend the laminate 1 to form it into a predetermined shape. Examples of the composite structure 2 include stringers used in aircraft fuselages and main wings. Note that the material for forming the laminate 1 is not limited to the above materials. For example, the laminate may be formed from a fiber sheet (dry sheet) that contains only fiber and does not contain resin.

[0015] [Composite Material Structure] As shown in Figure 1, the composite material structure 2 according to this embodiment is a long member. The composite material structure 2 has a T-shaped longitudinal cross section (a cross section when cut along a plane perpendicular to the longitudinal direction). The composite material structure 2 extends linearly along the longitudinal direction, and the longitudinal cross section has a uniform shape. The composite material structure 2 is manufactured by joining two composite material structures 2A each having an L-shaped longitudinal cross section. In this embodiment, an apparatus and processing method for processing a plate-shaped laminate 1 into a composite material structure 2A having an L-shaped longitudinal cross section will be described.

[0016] [Processing Apparatus] As shown in FIG. 2 , the processing apparatus 5 includes a pair of mandrel blocks (first mandrel block 10 and second mandrel block 20) ​​on which the laminate 1 is placed, a wedge block 30 arranged between the first mandrel block 10 and the second mandrel block 20, a membrane 40 covering the first mandrel block 10, the second mandrel block 20, and the wedge block 30, and a drive device (drive unit) that moves the first mandrel block 10 and the second mandrel block 20.

[0017] As shown in Fig. 2, the first mandrel block 10 is arranged alongside the second mandrel block 20 in the X-axis direction (a predetermined direction). As shown in Figs. 3 and 4, the first mandrel block 10 integrally includes a base 11, which is the portion farther from the second mandrel block 20, and a plurality of first protrusions 12 protruding from an opposing surface 11a, which is the surface of the base 11 facing the second mandrel block 20. The opposing surface 11a is a plane defined by the Y-axis direction and the X-axis direction.

[0018] The laminate 1 is placed on the base 11 as shown in Fig. 5 . As shown in Figs. 3 and 5 , the base 11 has a side surface (first surface) 11b that is the surface farther from the second mandrel block 20 (i.e., the surface opposite the opposing surface 11a), and a top surface (second surface) 11c that curves and extends from the upper end of the side surface 11b toward the second mandrel block 20. The laminate 1 is placed across the side surface 11b, top surface 11c, and connection portion 11d between the side surface 11b and top surface 11c of the first mandrel block 10. The side surface 11b is a plane defined by the Y-axis direction and the X-axis direction. The top surface 11c is a plane defined by the Y-axis direction and the X-axis direction. The connection portion 11d is a curved surface.

[0019] As shown in Figures 3 and 4, the multiple first protrusions 12 are arranged at equal intervals along the Y-axis direction. The first protrusions 12 are arranged in a comb-like pattern. As shown in Figures 3 and 5, each first protrusion 12 has a mandrel inclined surface (first inclined surface) 12a that bends and extends obliquely downward from the end of the upper surface 11c of the base 11 in the X-axis direction, and a vertical surface 12b that bends and extends downward from the lower end of the mandrel inclined surface 12a. The mandrel inclined surface 12a is inclined so as to approach the second mandrel block 20 as it moves in the movement direction (downward) of the wedge block 30. The mandrel inclined surface 12a is flat. The vertical surface 12b is a plane defined by the Y-axis direction and the X-axis direction.

[0020] The second mandrel block 20 is configured to be point-symmetrical with the first mandrel block 10, with the center point of the X-axis direction and the Y-axis direction of the processing device 5 as the center. As shown in Fig. 2, the second mandrel block 20 is arranged side by side with the first mandrel block 10 in the X-axis direction (a predetermined direction). As shown in Fig. 4, the second mandrel block 20 integrally has a base 21, which is the portion farther from the first mandrel block 10, and a plurality of second protrusions 22 protruding from an opposing surface 21a, which is the surface of the base 21 facing the first mandrel block 10. The opposing surface 21a is a plane defined by the Y-axis direction and the X-axis direction.

[0021] As shown in Fig. 5, the laminate 1 is placed on the base 21. As shown in Figs. 3 and 5, the base 21 has a side (first surface) 21b that is the surface farther from the first mandrel block 10 (i.e., the surface opposite the opposing surface 21a), and an upper surface (second surface) 21c that curves and extends from the upper end of the side surface 21b toward the first mandrel block 10. The laminate 1 is placed across the side surface 21b and upper surface 21c of the second mandrel block 20, and a connection portion 21d (see Fig. 5) between the side surface 21b and the upper surface 21c. The side surface 21b is a plane defined by the Y-axis direction and the X-axis direction. The upper surface 21c is a plane defined by the Y-axis direction and the X-axis direction. The connection portion 21d is a curved surface.

[0022] As shown in Figures 3 and 4, the multiple second protrusions 22 are arranged at equal intervals along the Y-axis direction. The second protrusions 22 are arranged in a comb-like pattern. As shown in Figures 3 and 5, the second protrusions 22 have a mandrel inclined surface (first inclined surface) 22a that bends and extends obliquely downward from the end of the upper surface 21c of the base 21 in the X-axis direction, and a vertical surface 22b that bends and extends downward from the lower end of the mandrel inclined surface 22a. The mandrel inclined surface 22a is inclined so as to approach the first mandrel block 10 as it moves in the movement direction (downward) of the wedge block 30. The mandrel inclined surface 22a is flat. The vertical surface 22b is a plane defined by the Y-axis direction and the X-axis direction.

[0023] As shown in FIG. 4 , the first protrusions 12 and the second protrusions 22 are arranged so as not to overlap when viewed from the X-axis direction. That is, the first protrusions 12 and the second protrusions 22 are arranged so as to be offset in the Y-axis direction. Furthermore, the length of the first protrusions 12 in the Y-axis direction is shorter than the distance between adjacent second protrusions 22. This allows the first protrusions 12 to be inserted between adjacent second protrusions 22. Furthermore, the length of the second protrusions 22 in the Y-axis direction is shorter than the distance between adjacent first protrusions 12. This allows the second protrusions 22 to be inserted between adjacent first protrusions 12. Furthermore, the length of the first protrusions 12 in the X-axis direction and the length of the second protrusions 22 in the X-axis direction are approximately the same.

[0024] Furthermore, when the base 11 of the first mandrel block 10 and the base 21 of the second mandrel block 20 are closest to each other (the state shown in Figure 5), the distance D1 between the bases 11 and 21 is shorter than the length L1 in the X-axis direction of the lower surface 30a of the wedge block 30 described later.

[0025] As shown in Fig. 2, the wedge block 30 is an elongated member extending in the Y-axis direction. The wedge block 30 is a member having a trapezoidal cross section in the Y-axis direction. The wedge block 30 is provided between the first mandrel block 10 and the second mandrel block 20. As shown in Fig. 5, the wedge block 30 is arranged so as to protrude in the Z-axis direction (intersecting direction) from the upper surface 11c of the base 11 of the first mandrel block 10. Furthermore, the wedge block 30 is arranged so as to protrude in the Z-axis direction (intersecting direction) from the upper surface 21c of the base 21 of the second mandrel block 20.

[0026] The wedge block 30 has a lower surface 30a which is the surface facing the first mandrel block 10 and the second mandrel block 20, an upper surface 30b which is the surface opposite to the lower surface 30a, and a wedge inclined surface (second inclined surface) 30c which connects the lower surface 30a and the upper surface 30b.

[0027] The length of the lower surface 30a in the X-axis direction is shorter than the length of the upper surface 30b in the X-axis direction. The lower surface 30a is a flat surface. The lower surface 30a is a flat surface defined by the Y-axis direction and the X-axis direction. The upper surface 30b is a flat surface. The upper surface 30b is a flat surface defined by the Y-axis direction and the X-axis direction. The pair of wedge inclined surfaces 30c are inclined so that the wedge inclined surfaces 30c approach each other as they move from the upper surface 30b to the lower surface 30a. The wedge inclined surfaces 30c are flat surfaces. The inclination angle of the wedge inclined surfaces 30c with respect to the horizontal plane is the same as the inclination angle of the mandrel inclined surface 12a with respect to the horizontal plane.

[0028] The membrane 40 is made of a material (e.g., silicone rubber) that is stretchable in the X-axis direction. The membrane 40 covers the laminate 1, the first mandrel block 10, the second mandrel block 20, and the wedge block 30 from above and laterally. One end of the membrane 40 in the X-axis direction is fixed to the lower end of the side surface 11b of the first mandrel block 10. The other end of the membrane 40 in the X-axis direction is fixed to the lower end of the side surface 21b of the second mandrel block 20.

[0029] The drive device moves the first mandrel block 10 and the second mandrel block 20 in the X-axis direction.

[0030] [Processing Method] Next, a processing method for the laminate 1 using the processing apparatus 5 according to this embodiment will be described with reference to FIGS. 5 to 8. First, as shown in FIG. 5, the laminate 1 is placed on each of the first mandrel block 10 and the second mandrel block 20. When the laminate 1 is placed on the first mandrel block 10 and the second mandrel block 20, the portions to be bent are preliminarily curved. The laminate 1 is placed so that the portions to be bent (hereinafter referred to as "curved portions") abut or are close to the connecting portions 11d, 21d of the mandrel blocks. At this time, one side of the curved portions of the laminate 1 is in surface contact with the side surfaces 11b, 21b of the mandrel blocks. Furthermore, the other side of the curved portions of the laminate 1 is spaced apart from the upper surfaces 11c, 21c of the mandrel blocks.

[0031] At this time, the first mandrel block 10 and the second mandrel block 20 are in a state where the first convex portions 12 are inserted between the second convex portions 22 and the second convex portions 22 are inserted between the first convex portions 12, and the base portion 11 of the first mandrel block 10 and the base portion 21 of the second mandrel block 20 are closest to each other. In detail, the first mandrel block 10 and the second mandrel block 20 are arranged so that the separation distance D1 between the base portions 11 and 21 is shorter than the length L1 in the X-axis direction of the lower surface 30a of the wedge block 30.

[0032] Next, the wedge block 30 is positioned so as to straddle the upper surface 11c of the first mandrel block 10 and the upper surface 21c of the second mandrel block 20. The lower surface 30a of the wedge block 30 is in contact with the upper surface 11c of the first mandrel block 10 and the upper surface 21c of the second mandrel block 20. At this time, the wedge block 30 protrudes a predetermined height L2 from the upper surface 11c of the first mandrel block 10 and the upper surface 21c of the second mandrel block 20.

[0033] Next, the laminate 1, the first mandrel block 10, the second mandrel block 20, and the wedge block 30 are covered from above and from the side with a membrane 40. One end of the membrane 40 in the X-axis direction is fixed to the lower end of the side surface 11b of the first mandrel block 10, and the other end of the membrane 40 in the X-axis direction is fixed to the lower end of the side surface 21b of the second mandrel block 20. In this state, the membrane 40 is slightly loose or at its natural length. In other words, the in-plane tension is set to zero. At this time, a space is formed between the membrane 40 and the upper surface 11c of the first mandrel block 10 and the upper surface 21c of the second mandrel block 20. A portion of the laminate 1 is disposed in this space. The portion of the laminate 1 refers to a portion that moves and is pressed against each mandrel block during bending.

[0034] Next, as shown by the arrows in Figure 5, the drive device moves the first mandrel block 10 and the second mandrel block 20 apart in the X-axis direction. This pulls the membrane 40 in the X-axis direction, increasing the tension. For a while after the start of movement, the wedge block 30 remains placed on the upper surface 11c of the first mandrel block 10 and the upper surface 21c of the second mandrel block 20. As the membrane 40 is pulled in the X-axis direction, the tension continues to increase. The wedge block 30 is pressed downward by the tension of the membrane 40.

[0035] As the first mandrel block 10 and the second mandrel block 20 continue to move in the X-axis direction, the separation distance D2 between the bases 11 and 21 becomes longer than the length L1 of the lower surface 30a of the wedge block 30 in the X-axis direction, as shown in Fig. 6. When the separation distance D2 between the bases 11 and 21 becomes longer than the length L1 of the lower surface 30a of the wedge block 30 in the X-axis direction, the wedge block 30 enters the gap between the mandrel inclined surface 12a of the first mandrel block 10 and the mandrel inclined surface 22a of the second mandrel block 20, as shown in Fig. 7. When the wedge block 30 enters the gap, the mandrel inclined surface 12a of the first mandrel block 10 and the mandrel inclined surface 22a of the second mandrel block 20 come into contact with the wedge inclined surface 30c of the wedge block 30.

[0036] In this state, as the first mandrel block 10 and the second mandrel block 20 continue to move in the X-axis direction, the wedge block 30 moves downward due to its own weight and the pressing force of the membrane 40 (see the dashed arrow in Figure 7). At this time, the wedge block 30 moves so that the wedge inclined surface 30c slides on the mandrel inclined surfaces 12a and 22a. As the wedge block 30 moves downward, the protruding length L2 of the wedge block 30 also gradually decreases. In this way, the wedge block 30 moves in the Z-axis direction so that the protruding length L2 decreases in accordance with the movement of the first mandrel block 10 and the second mandrel block 20 in the X-axis direction.

[0037] When the first mandrel block 10 and the second mandrel block 20 have moved a predetermined distance, the driving device stops the movement of the first mandrel block 10 and the second mandrel block 20. At this time, the laminate 1 is in close contact with the membrane 40 and is in contact with the upper surface 11 c of the first mandrel block 10 and the upper surface 21 c of the second mandrel block 20.

[0038] In this way, two composite structures 2A each having an L-shaped cross section in the longitudinal direction are simultaneously manufactured by bending two plate-shaped laminates 1. When manufacturing a composite structure 2 having a T-shaped cross section in the longitudinal direction, two composite structures 2A each having an L-shaped cross section are joined together (see FIG. 1).

[0039] This embodiment provides the following advantageous effects. In this embodiment, the wedge block 30 is disposed so as to protrude from the upper surfaces 11 c, 21 c of the first mandrel block 10 and the second mandrel block 20 in the Z-axis direction, which intersects with the X-axis direction. As a result, the membrane 40 covering the first mandrel block 10, the second mandrel block 20, and the wedge block 30 is lifted by the wedge block 30, and some regions of the membrane 40 are separated from the upper surfaces 11 c, 21 c of the first mandrel block 10 and the second mandrel block 20. Furthermore, in this embodiment, the wedge block 30 is disposed so that the protruding length L2 shortens as the first mandrel block 10 and the second mandrel block 20 move in the X-axis direction. As a result, when the pair of first mandrel block 10 and second mandrel block 20 is moved apart by the driving device, the protruding length L2 of the wedge block 30 shortens. As the protruding length L2 of the wedge block 30 shortens, the membrane 40 held up by the wedge block 30 moves closer to the upper surfaces 11 c, 21 c of the first mandrel block 10 and the second mandrel block 20. Furthermore, because the pair of first mandrel blocks 10 and second mandrel blocks 20 move apart, the membrane 40 is pulled in the X-axis direction, increasing the tension in response to the movement of the first mandrel block 10 and the second mandrel block 20. As a result, the membrane 40 comes into close contact with the laminate 1 placed on the first mandrel block 10 and the second mandrel block 20, and presses the laminate 1 against the connecting portions 11 d, 21 d of the first mandrel block 10 and the second mandrel block 20. The laminate 1 pressed against the connecting portions 11 d, 21 d of the first mandrel block 10 and the second mandrel block 20 is shaped according to the shapes of the connecting portions 11 d, 21 d. In this manner, the laminate 1 can be subjected to bending.

[0040] Furthermore, in this embodiment, the membrane 40 is brought into close contact with the laminate 1 and the first and second mandrel blocks 10 and 20 by moving the first mandrel block 10, the second mandrel block 20, and the wedge block 30. In other words, the movement (movement and deformation mode) of the membrane 40 is controlled by the first mandrel block 10, the second mandrel block 20, and the wedge block 30. That is, the movement of the membrane 40 is controlled by a separate member. This allows the membrane 40 to be more reliably brought into close contact with the laminate 1 compared to when the movement of the membrane 40 is not controlled by a separate member (for example, when the membrane 40 is controlled only by the force generated by vacuum suction). Therefore, the laminate 1 can be bent in an optimal manner.

[0041] Furthermore, in this embodiment, the membrane 40 presses the laminate 1 against the first mandrel block 10 and the second mandrel block 20 by simply moving the first mandrel block 10 and the second mandrel block 20 in the X-axis direction and the wedge block 30 in the Z-axis direction (i.e., linear motion of the blocks), thereby bending the laminate 1. This simplifies the structure compared to, for example, a case in which a suction device or the like is provided to evacuate the space between the membrane 40 and the blocks. This reduces costs and improves maintainability. Furthermore, evacuating the space increases the risk of quality defects due to defects in the sealing structure provided on the periphery. On the other hand, in this embodiment, since a sealing structure is not required, quality defects due to defects in the sealing structure can be prevented.

[0042] In this embodiment, the wedge block 30 has a wedge inclined surface 30c that comes into surface contact with the mandrel inclined surfaces 12a, 22a. As a result, when the first mandrel block 10 and the second mandrel block 20 move in the X-axis direction and the wedge block 30 is pressed by the membrane 40, the wedge inclined surface 30c of the wedge block 30 slides on the mandrel inclined surfaces 12a, 22a. In this way, the wedge block 30 can be moved in the Z-axis direction in response to the movement of the first mandrel block 10 and the second mandrel block 20 in the X-axis direction.

[0043] Furthermore, in this embodiment, the wedge block 30 moves in the Z-axis direction in response to the movement of the first mandrel block 10 and the second mandrel block 20. In this manner, the wedge block 30 can be moved in the Z-axis direction without providing a drive mechanism for moving the wedge block 30. Therefore, compared to the case where a drive mechanism for moving the wedge block 30 is provided, the number of parts can be reduced and the structure can be simplified.

[0044] In this embodiment, the first convex portion 12 and the second convex portion 22 are arranged so as not to overlap when viewed from the X-axis direction. This allows the first mandrel block 10 and the second mandrel block 20 to be closer to each other. This allows the processing device 5 to be made smaller.

[0045] Second Embodiment Next, a second embodiment of the present disclosure will be described with reference to FIG. 9 . In this embodiment, the processing apparatus 105 of this embodiment differs from the first embodiment in that two processing apparatuses 5 of the first embodiment are combined so as to be symmetrical in the Z-axis direction with respect to a plane defined by the X-axis direction and the Y-axis direction. Therefore, the same structures are denoted by the same reference numerals, and their description will be omitted. The membrane 140 of this embodiment is not fixed to the first mandrel block 10 and the second mandrel block 20. The membrane 140 is formed endlessly.

[0046] With this configuration, the laminate 1 can be bent to produce a composite structure having a C-shaped cross section.

[0047] Third Embodiment Next, a third embodiment of the present disclosure will be described with reference to FIG. 10 . In this embodiment, a processing device 205 of this embodiment differs from the first embodiment in that two processing devices 5 according to the first embodiment are combined in a point-symmetrical manner. Therefore, the same structures are denoted by the same reference numerals, and a description thereof will be omitted. In this embodiment, two processing devices 5 are lined up in the X-axis direction, and one of the processing devices 5 is upside down. In addition, the first mandrel blocks 10 of both processing devices 5 are fixed, and only the second mandrel block 20 moves in the X-axis direction. In addition, the laminate 1 is disposed between the two processing devices 5.

[0048] With this configuration, the laminate 1 can be bent to produce a composite structure having an S-shaped cross section.

[0049] The present disclosure is not limited to the above-described embodiments and may be modified as appropriate within the scope of the present disclosure. For example, in the above-described embodiments, the mandrel inclined surfaces 12 a and 22 a are flat, but the present disclosure is not limited thereto. The mandrel inclined surfaces 12 a and 22 a may be curved.

[0050] In the above embodiment, an example in which both the first mandrel block 10 and the second mandrel block 20 move in the X-axis direction has been described, but the present disclosure is not limited to this. For example, either the first mandrel block 10 or the second mandrel block 20 may move in the X-axis direction, while the other is fixed.

[0051] Furthermore, in the first embodiment, an example in which the laminate 1 is placed on both the first mandrel block 10 and the second mandrel block 20 has been described, but the present disclosure is not limited to this. The laminate 1 may be placed on only one of the first mandrel block 10 and the second mandrel block 20. In this case, a dummy member having the same shape as the laminate after bending may be placed in the mandrel block on which the laminate 1 is not placed, in the location where the laminate 1 would normally be placed.

[0052] Furthermore, in the above embodiment, an example has been described in which the driving device moves the first mandrel block 10 and / or the second mandrel block 20 in the X-axis direction, but the present disclosure is not limited thereto. For example, the driving device may move the wedge block 30 downward. In this case, the first mandrel block 10 and / or the second mandrel block 20 are movable in the X-axis direction. That is, the first mandrel block 10 and / or the second mandrel block 20 are permitted to move in the X-axis direction. In this configuration, when the wedge block 30 moves downward, the wedge block 30 presses the first mandrel block 10 and / or the second mandrel block 20. The inclined surfaces (such as the mandrel inclined surface 12a) of the wedge block 30 and the first mandrel block 10 and / or the second mandrel block 20 are in contact with each other. Therefore, the pressing force from the wedge block 30 is converted into a pressing force in the X-axis direction when it is transmitted to the first mandrel block 10 and the second mandrel block 20. As a result, the downward movement of the wedge block 30 causes the first mandrel block 10 and / or the second mandrel block 20 to move in the X-axis direction, and the first mandrel block 10 and the second mandrel block 20 move apart.

[0053] The processing apparatus and processing method described in the above-described embodiments can be understood, for example, as follows: The processing apparatus according to a first aspect of the present disclosure is a processing apparatus (5) for bending a plate-shaped workpiece (1), the processing apparatus having a first surface (11b) and a second surface (11c) extending in a bent or curved manner from an end of the first surface, the workpiece being placed at a connection portion (11d) between the first surface and the second surface, a pair of mandrel blocks (10, 20) arranged side by side in a predetermined direction (X-axis direction), a wedge block (30) arranged between the pair of mandrel blocks so as to protrude from the second surface of the mandrel block in a cross direction (Z-axis direction) that crosses the predetermined direction, and a wedge block (30) arranged between the mandrel blocks. The workpiece is placed on a block, and a membrane (40) covers the mandrel block and the wedge block, wherein one or both of the pair of mandrel blocks are movable in the predetermined direction so that the mandrel blocks are spaced apart in the predetermined direction, the membrane is pulled in the predetermined direction in response to the movement of the mandrel block in the predetermined direction, and the wedge block moves in the intersecting direction in response to the movement of the mandrel block in the predetermined direction so that the protruding length from the second surface is shortened.

[0054] In the above configuration, the wedge block is positioned to protrude from the second surface of the mandrel block in a direction intersecting the predetermined direction. As a result, the mandrel block and the membrane covering the wedge block are lifted by the wedge block, causing a portion of the membrane to separate from the second surface of the mandrel block. In addition, in the above configuration, the wedge block is configured so that its protruding length shortens as the mandrel block moves in the predetermined direction. As a result, when the pair of mandrel blocks move apart, the protruding length of the wedge block shortens. As the protruding length of the wedge block shortens, the membrane held up by the wedge block moves closer to the second surface of the mandrel block. Furthermore, because the pair of mandrel blocks move apart, the membrane is pulled in the predetermined direction, increasing tension as the mandrel block moves. As a result, the membrane adheres closely to the workpiece placed on the mandrel block and presses the workpiece against the connection portion of the mandrel block. The workpiece pressed against the connection portion of the mandrel block is shaped according to the shape of the connection portion. In this way, the workpiece can be bent.

[0055] Furthermore, in the above configuration, the mandrel block and wedge block are moved to bring the membrane into close contact with the workpiece and mandrel block. In other words, the mandrel block and wedge block control the movement (movement and deformation) of the membrane. That is, the movement of the membrane is controlled by a separate member. This allows the membrane to be more reliably brought into close contact with the workpiece compared to when the movement of the membrane is not controlled by a separate member (for example, when the membrane is controlled only by the force generated by vacuum suction). Therefore, the workpiece can be bent in an optimal manner.

[0056] Furthermore, in the above configuration, the membrane presses the workpiece against the mandrel block by simply moving the mandrel block in a predetermined direction and the wedge block in the intersecting direction (i.e., linear motion of the blocks), thereby bending the workpiece. This simplifies the structure compared to, for example, a case where a suction device or the like is provided to evacuate the space between the membrane and the block. This also reduces costs and improves maintainability.

[0057] In addition, in the processing apparatus according to the second aspect of the present disclosure, in the first aspect described above, the pair of mandrel blocks have a first inclined surface (12a) that bends from the second surface and extends in the movement direction of the wedge block, and the wedge block has a second inclined surface (30c) that comes into surface contact with the first inclined surface, and the first inclined surface is inclined so as to approach the other mandrel block as it moves in the movement direction of the wedge block.

[0058] In the above configuration, the wedge block has a second inclined surface that is in surface contact with the first inclined surface. When the mandrel block moves in a predetermined direction and the wedge block is pressed by the membrane, the second inclined surface of the wedge block slides on the first inclined surface. In this way, the wedge block can be moved in the cross direction in response to the movement of the mandrel block in the predetermined direction.

[0059] In addition, in the above configuration, the wedge blocks move in the transverse direction in response to the movement of the mandrel blocks. In this way, the wedge blocks can be moved in the transverse direction without providing a drive mechanism for moving the wedge blocks. Therefore, compared to a case where a drive mechanism for moving the wedge blocks is provided, the number of parts can be reduced and the structure can be simplified.

[0060] Furthermore, in a processing apparatus according to a third aspect of the present disclosure, in the above-mentioned first or second aspect, the pair of mandrel blocks includes a first mandrel block (10) and a second mandrel block (20) arranged alongside the first mandrel block in the predetermined direction, the first mandrel block has a first convex portion (12) that protrudes in the predetermined direction on its surface facing the second mandrel block, and the second mandrel block has a second convex portion (22) that protrudes in the predetermined direction on its surface facing the first mandrel block, and the first convex portion and the second convex portion are arranged so as not to overlap when viewed from the predetermined direction.

[0061] In the above configuration, the first and second convex portions are arranged so as not to overlap when viewed from a predetermined direction, which allows the first and second mandrel blocks to be closer together, thereby enabling the processing device to be made smaller.

[0062] A processing method according to a first aspect of the present disclosure is a processing method for performing a bending process on a plate-shaped workpiece (1), and includes a workpiece setting step of setting the workpiece at a connection portion (11d) between a pair of mandrel blocks (10, 20) arranged side by side in a predetermined direction (X-axis direction), the pair having a first surface (11b) and a second surface (11c) extending in a bent or curved manner from an end of the first surface, the pair of mandrel blocks (10, 20), the first surface and the second surface; a wedge block setting step of setting a wedge block (30) between the pair of mandrel blocks so as to protrude from the second surface of the mandrel block in a transverse direction (Z-axis direction) that intersects the predetermined direction; The method includes an installation step of installing a membrane (40) to cover the workpiece, the mandrel block, and the wedge block while they are installed in a lock; and a moving step of moving one or both of the pair of mandrel blocks in the predetermined direction so that the mandrel blocks are spaced apart in the predetermined direction, wherein the moving step involves the mandrel block pulling the membrane in the predetermined direction in response to the movement of the mandrel block in the predetermined direction, and the moving step involves the wedge block moving in the intersecting direction in response to the movement of the mandrel block in the predetermined direction so that the protruding length from the second surface is shortened.

[0063] DESCRIPTION OF SYMBOLS 1: Laminate 2: Composite material structure 2A: Composite material structure 3: Fiber sheet 5: Processing device 10: First mandrel block 11: Base 11a: Opposing surface 11b: Side surface 11c: Upper surface 11d: Connection portion 12: First convex portion 12a: Mandrel inclined surface 12b: Vertical surface 20: Second mandrel block 21: Base 21a: Opposing surface 21b: Side surface 21c: Upper surface 21d: Connection portion 22: Second convex portion 22a: Mandrel inclined surface 22b: Vertical surface 30: Wedge block 30a: Lower surface 30b: Upper surface 30c: Wedge inclined surface 40: Membrane 105: Processing device 140: Membrane 205: Processing equipment

Claims

1. A processing device for performing bending processing on a plate-shaped workpiece, comprising: a pair of mandrel blocks arranged side by side in a predetermined direction, the pair of mandrel blocks having a first surface and a second surface extending in a bent or curved manner from an end of the first surface, the workpiece being placed at the connection between the first surface and the second surface; a wedge block arranged between the pair of mandrel blocks so as to protrude from the second surface of the mandrel block in an intersecting direction intersecting the predetermined direction; and a membrane covering the workpiece, the mandrel block, and the wedge block while placed on the mandrel blocks, wherein one or both of the pair of mandrel blocks are movable in the predetermined direction so that the mandrel blocks are separated from each other in the predetermined direction, the membrane is pulled in the predetermined direction in response to the movement of the mandrel blocks in the predetermined direction, and the wedge block moves in the intersecting direction in response to the movement of the mandrel block in the predetermined direction so that the protruding length from the second surface is shortened.

2. The processing device according to claim 1, wherein the pair of mandrel blocks have a first inclined surface that bends from the second surface and extends in the direction of movement of the wedge block, the wedge block has a second inclined surface that makes surface contact with the first inclined surface, and the first inclined surface is inclined so as to approach the other mandrel block as it progresses in the direction of movement of the wedge block.

3. The processing apparatus described in claim 1 or claim 2, wherein the pair of mandrel blocks comprises a first mandrel block and a second mandrel block arranged alongside the first mandrel block in the predetermined direction, the first mandrel block has a first convex portion protruding in the predetermined direction on its surface facing the second mandrel block, and the second mandrel block has a second convex portion protruding in the predetermined direction on its surface facing the first mandrel block, and the first convex portion and the second convex portion are arranged so as not to overlap when viewed from the predetermined direction.

4. A processing method for performing bending processing on a plate-shaped workpiece, comprising: a workpiece setting step of setting the workpiece at a connection between a first surface and a second surface extending in a bent or curved manner from an end of the first surface and a pair of mandrel blocks arranged side by side in a predetermined direction, the first surface and the second surface being connected to each other; a wedge block setting step of setting a wedge block between the pair of mandrel blocks so as to protrude from the second surface of the mandrel block in a direction intersecting the predetermined direction; a setting step of setting a membrane so as to cover the workpiece, the mandrel block and the wedge block in a state in which the workpiece is placed on the mandrel block; and a moving step of moving one or both of the pair of mandrel blocks in the predetermined direction so that the pair of mandrel blocks are separated in the predetermined direction, the moving step comprising: the mandrel block pulling the membrane in the predetermined direction in response to the movement of the mandrel block in the predetermined direction, The moving step is a processing method in which the wedge block moves in the intersecting direction in response to the movement of the mandrel block in the predetermined direction so that the protruding length from the second surface is shortened.

Citation Information

Patent Citations

  • Method of moulding a charge

    US10016949B2

  • Terminal element of a traffic barrier device, transition system, and method for providing impact protection

    US11313089B2

  • Folding molding machine of prepreg and folding molding method using it

    JP2006312260A

  • Regulator bag for vacuum forming

    JP2012218436A

  • Net-shape forming of composite stringer containing out-of-plane portion

    JP2022050330A