Semiconductor device

The semiconductor device design with a metal oxide layer and oxide semiconductor structure addresses mobility and reliability issues, enhancing performance and integration capabilities.

WO2026234501A1PCT designated stage Publication Date: 2026-11-12SEMICON ENERGY LAB CO LTD
-1 Cites 0 Cited by

Patent Information

Application Number
PCT/IB2026/054205
Authority / Receiving Office
WO · WO
Patent Type
Applications
Current Assignee / Owner
Priority Date
2025-05-08
Filing Date
2026-04-29
Publication Date
2026-11-12

AI Technical Summary

Technical Problem

Existing semiconductor devices face challenges in achieving high field-effect mobility, high operating speed, high reliability, miniaturization, integration, low power consumption, and stable electrical characteristics, particularly in transistors using oxide semiconductors.

Method used

A semiconductor device configuration featuring a metal oxide layer, an oxide semiconductor with cubic crystal structure, and specific insulator and conductor arrangements, including a high aspect ratio insulator covered by the oxide semiconductor, reduces crystal grain boundaries and enhances channel width, thereby improving on-current and field-effect mobility.

Benefits of technology

The configuration results in a semiconductor device with enhanced field-effect mobility, high operating speed, reliable electrical characteristics, and the potential for miniaturization and integration, while reducing leakage current and power consumption.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure IB2026054205_12112026_PF_FP_ABST
    Figure IB2026054205_12112026_PF_FP_ABST
Patent Text Reader

Abstract

Provided is a semiconductor device which has a high field effect mobility. The semiconductor device comprises a metal oxide layer, an oxide semiconductor, a first insulator to a third insulator, and a first conductor to a third conductor. The metal oxide layer is in contact with an upper surface and side surfaces of the first insulator. The oxide semiconductor covers the first insulator and the metal oxide layer. The first conductor and the second conductor are disposed on the oxide semiconductor. The second insulator is disposed on the first conductor and the second conductor, and comprises an opening portion that overlaps with the region between the first conductor and the second conductor. The third insulator is disposed on the oxide semiconductor in the opening portion. The third conductor is disposed on the third insulator in the opening portion. In a cross-sectional view in a channel width direction, the height of the first insulator is greater than the width of the first insulator. The metal oxide layer overlaps with the first conductor. The metal oxide layer includes indium and comprises a crystal. The oxide semiconductor includes indium and comprises a crystal having a cubic crystal structure.
Need to check novelty before this filing date? Find Prior Art

Description

Semiconductor equipment

[0001] One aspect of the present invention relates to a semiconductor device, a memory device, and an electronic device using an oxide semiconductor layer. Another aspect of the present invention relates to a method for manufacturing the above-mentioned semiconductor device.

[0002] It should be noted that one aspect of the present invention is not limited to the above-mentioned technical field. Examples of technical fields of one aspect of the present invention include semiconductor devices, display devices, light-emitting devices, energy storage devices, memory devices, electronic devices, lighting devices, input devices (e.g., touch sensors), input / output devices (e.g., touch panels), methods for driving them, or methods for manufacturing them.

[0003] In this specification, the term "semiconductor device" refers to any device that can function by utilizing semiconductor properties. Semiconductor elements such as transistors, as well as semiconductor circuits, computing devices, and memory devices, are all forms of semiconductor devices. Display devices (such as liquid crystal displays and light-emitting displays), projection devices, lighting devices, electro-optical devices, energy storage devices, memory devices, semiconductor circuits, imaging devices, and electronic devices may also be considered to have semiconductor devices.

[0004] In recent years, the development of semiconductor devices has progressed, and LSIs (Large Scale Integration), CPUs (Central Processing Units), and memory are mainly used in semiconductor devices. A CPU is an assembly of semiconductor elements that have semiconductor integrated circuits (at least transistors and memory) formed on chips by processing semiconductor wafers, and electrodes which are connection terminals.

[0005] Semiconductor circuits (IC chips) such as LSIs, CPUs, and memory are mounted on circuit boards, such as printed circuit boards, and used as components in various electronic devices.

[0006] Furthermore, the technology of constructing transistors using semiconductor thin films formed on substrates with insulating surfaces is attracting attention. These transistors are widely applied in electronic devices such as integrated circuits (ICs) and image display devices (also simply referred to as display devices). While silicon-based semiconductor materials are widely known as semiconductor thin films applicable to transistors, oxide semiconductors are attracting attention as other materials.

[0007] Furthermore, transistors using oxide semiconductors are known to have extremely low leakage current in the non-conductive state. For example, Patent Document 1 discloses a low-power CPU that takes advantage of the low leakage current characteristic of transistors using oxide semiconductors. Also, for example, Patent Document 2 discloses a memory device that can retain its contents for a long period of time by taking advantage of the low leakage current characteristic of transistors using oxide semiconductors.

[0008] Furthermore, Patent Document 3 discloses a transistor with a microstructure in which a source electrode layer and a drain electrode layer are provided in contact with the upper surface of an oxide semiconductor.

[0009] Also, In 2 O 3 Its use in thin-film transistors has been reported (Non-Patent Document 1).

[0010] Japanese Patent Publication No. 2012-257187, Japanese Patent Publication No. 2011-151383, International Publication No. 2016-125052

[0011] Dhananjay and C. W. Chu. “Realization of In▲2▼O▲3▼ thin film transistors through reactive evaporation process.”Appl. Phys. Lett. 91, 132111 (2007).

[0012] One aspect of the present invention aims to provide a semiconductor device with high field-effect mobility. Alternatively, one aspect of the present invention aims to provide a semiconductor device with high operating speed. Alternatively, one aspect of the present invention aims to provide a semiconductor device with high reliability. Alternatively, one aspect of the present invention aims to provide a semiconductor device that can be miniaturized or highly integrated. Alternatively, one aspect of the present invention aims to provide a semiconductor device with good electrical characteristics. Alternatively, one aspect of the present invention aims to provide a semiconductor device with little variation in the electrical characteristics of transistors. Alternatively, one aspect of the present invention aims to provide a semiconductor device with high on-current. Alternatively, one aspect of the present invention aims to provide a semiconductor device with low power consumption. Alternatively, one aspect of the present invention aims to provide a novel semiconductor device. Alternatively, one aspect of the present invention aims to provide a method for manufacturing a highly productive semiconductor device. Alternatively, one aspect of the present invention aims to provide a method for manufacturing a novel semiconductor device.

[0013] Alternatively, one aspect of the present invention aims to provide a storage device that can be miniaturized or highly integrated. Alternatively, one aspect of the present invention aims to provide a storage device with a large storage capacity. Alternatively, one aspect of the present invention aims to provide a storage device with a fast operating speed. Alternatively, one aspect of the present invention aims to provide a storage device with low power consumption. Alternatively, one aspect of the present invention aims to provide a novel storage device.

[0014] Furthermore, the description of these problems does not preclude the existence of other problems. One aspect of the present invention does not necessarily have to solve all of these problems. It is possible to extract other problems from the description in the specification, drawings, and claims.

[0015] One aspect of the present invention is a semiconductor device comprising a metal oxide layer, an oxide semiconductor, first to third insulators, and first to third conductors, wherein the metal oxide layer is in contact with the upper and side surfaces of the first insulator, the oxide semiconductor covers the first insulator and the metal oxide layer, the first and second conductors are arranged on the oxide semiconductor, the second insulator is arranged on the first and second conductors and has an opening that overlaps with the region between the first and second conductors, the third insulator is arranged on the oxide semiconductor at the opening, the third conductor is arranged on the third insulator at the opening, in a cross-sectional view in the channel width direction, the height of the first insulator is greater than the width of the first insulator, the metal oxide layer overlaps with the first conductor, the metal oxide layer contains indium and has crystals, and the oxide semiconductor contains indium and has crystals with a cubic structure.

[0016] Another aspect of the present invention comprises a metal oxide layer, an oxide semiconductor, first to fourth insulators, and first to third conductors, wherein the first insulator is disposed on the fourth insulator, the metal oxide layer is in contact with the upper and side surfaces of the first insulator, the oxide semiconductor is disposed on the fourth insulator and covers the first insulator and the metal oxide layer, the first and second conductors are disposed on the oxide semiconductor, and the second insulator is disposed on the first and second conductors and the first conductor A semiconductor device having an opening that overlaps with the region between the electric body and the second conductor, a third insulator disposed on an oxide semiconductor at the opening, a third conductor disposed on the third insulator at the opening, a cross-sectional view in the channel width direction where the height of the first insulator is greater than the width of the first insulator, a metal oxide layer overlapping with the first conductor, the metal oxide layer containing indium and having crystals, and the oxide semiconductor containing indium and having crystals with a cubic structure.

[0017] In the above, it is preferable that the side surface of the fourth insulator coincides with or substantially coincides with the side surface of the metal oxide layer, the side surface of the oxide semiconductor, the side surface of the first conductor, and the side surface of the second conductor in a plan view, and that the film thickness of the first insulator is thicker than the film thickness of the third insulator.

[0018] Furthermore, in the above, it is preferable that the lower surface of the third conductor has a portion located below the lower surface of the oxide semiconductor.

[0019] Another aspect of the present invention comprises a metal oxide layer, an oxide semiconductor, first to fifth insulators, and first to third conductors, wherein the first insulator is disposed on the fourth insulator, the metal oxide layer is in contact with the upper and side surfaces of the first insulator, the oxide semiconductor is disposed on the fourth insulator and covers the first insulator and the metal oxide layer, the first and second conductors are disposed on the oxide semiconductor, the second insulator is disposed on the first and second conductors and has an opening that overlaps with the region between the first and second conductors, the third insulator is disposed on the oxide semiconductor at the opening, the third conductor is disposed on the third insulator at the opening, and the first and second conductors are each connected to the first conductive layer A semiconductor device comprising a first conductive layer and a second conductive layer on the first conductive layer, wherein the fifth insulator is positioned at an opening in the second insulator and is in contact with the upper surface of the first conductive layer of the first conductor, the side surface of the second conductive layer of the first conductor, the upper surface of the first conductive layer of the second conductor, and the side surface of the second conductive layer of the second conductor, the shortest distance between the first conductive layer of the first conductor and the first conductive layer of the second conductor is smaller than the shortest distance between the second conductive layer of the first conductor and the second conductive layer of the second conductor, in a cross-sectional view in the channel width direction, the height of the first insulator is greater than the width of the first insulator, the metal oxide layer is superimposed on the first conductor, the metal oxide layer contains indium and has crystals, and the oxide semiconductor contains indium and has crystals with a cubic structure.

[0020] In the above, it is preferable that a portion of the side surface of the second insulator coincides with or substantially coincides with the side surface of the second conductive layer of the first conductor and the side surface of the second conductive layer of the second conductor in a plan view.

[0021] Furthermore, in the above, it is preferable that the fifth insulator has silicon nitride.

[0022] Furthermore, it is preferable that the first conductive layer of the first conductor and the first conductive layer of the second conductor each contain indium and tin, respectively.

[0023] Furthermore, in the above, it is preferable that the metal oxide layer does not overlap with the second conductor and the third conductor.

[0024] Furthermore, in the above, it is preferable that the direction of the metal oxide layer is parallel to the direction of the third conductor.

[0025] Furthermore, in the above, it is preferable that the metal oxide layer has a cubic crystal structure.

[0026] Furthermore, it is preferable that the metal oxide layer contains indium, gallium, and zinc, and has a hexagonal or trigonal crystal structure.

[0027] Furthermore, in the above, it is preferable that the first insulator has gallium oxide, aluminum oxide, or silicon oxide.

[0028] According to one aspect of the present invention, a semiconductor device with high field-effect mobility can be provided. Alternatively, according to one aspect of the present invention, a semiconductor device with high operating speed can be provided. Alternatively, according to one aspect of the present invention, a semiconductor device with high reliability can be provided. Alternatively, according to one aspect of the present invention, a semiconductor device that can be miniaturized or highly integrated can be provided. Alternatively, according to one aspect of the present invention, a semiconductor device having good electrical characteristics can be provided. Alternatively, according to one aspect of the present invention, a semiconductor device with little variation in the electrical characteristics of transistors can be provided. Alternatively, according to one aspect of the present invention, a semiconductor device with high on-current can be provided. Alternatively, according to one aspect of the present invention, a semiconductor device with low power consumption can be provided. Alternatively, according to one aspect of the present invention, a novel semiconductor device can be provided. Alternatively, according to one aspect of the present invention, a method for manufacturing a highly productive semiconductor device can be provided. Alternatively, according to one aspect of the present invention, a method for manufacturing a novel semiconductor device can be provided.

[0029] Alternatively, according to one aspect of the present invention, a storage device that can be miniaturized or highly integrated can be provided. Alternatively, according to one aspect of the present invention, a storage device with a large storage capacity can be provided. Alternatively, according to one aspect of the present invention, a storage device with a fast operating speed can be provided. Alternatively, according to one aspect of the present invention, a storage device with low power consumption can be provided. Alternatively, according to one aspect of the present invention, a novel storage device can be provided.

[0030] Furthermore, the description of these effects does not preclude the existence of other effects. One aspect of the present invention does not necessarily have to possess all of these effects. Other effects can be extracted from the description, drawings, and claims.

[0031] Figure 1A is a plan view showing an example of a semiconductor device. Figures 1B, 1C, and 1D are cross-sectional views showing an example of a semiconductor device. Figures 2A and 2B are cross-sectional views showing an example of a semiconductor device. Figure 3 is a cross-sectional view showing an example of a semiconductor device. Figure 4A is a plan view showing an example of a semiconductor device. Figures 4B, 4C, and 4D are cross-sectional views showing an example of a semiconductor device. Figures 5A, 5B, 5C, and 5D are perspective views showing an example of a method for manufacturing a semiconductor device. Figures 6A and 6B are cross-sectional views showing an example of a semiconductor device. Figures 7A, 7B, and 7C are cross-sectional views showing an example of a semiconductor device. Figures 8A and 8B are cross-sectional views showing an example of a semiconductor device. Figures 9A, 9B, and 9C are cross-sectional views showing an example of a semiconductor device. Figure 10A is a plan view showing an example of a semiconductor device. Figures 10B, 10C, and 10D are cross-sectional views showing an example of a semiconductor device. Figure 11A is a plan view showing an example of a semiconductor device. Figures 11B, 11C, and 11D are cross-sectional views showing an example of a semiconductor device. Figure 12A is a plan view showing an example of a semiconductor device. Figures 12B, 12C, and 12D are cross-sectional views showing an example of a semiconductor device. Figure 13 is a cross-sectional view showing an example of a semiconductor device. Figure 14A is a plan view showing an example of a method for manufacturing a semiconductor device. Figures 14B, 14C, and 14D are cross-sectional views showing an example of a method for manufacturing a semiconductor device. Figure 15A is a plan view showing an example of a method for manufacturing a semiconductor device. Figures 15B, 15C, and 15D are cross-sectional views showing an example of a method for manufacturing a semiconductor device. Figure 16A is a plan view showing an example of a method for manufacturing a semiconductor device. Figures 16B, 16C, and 16D are cross-sectional views showing an example of a method for manufacturing a semiconductor device. Figure 17A is a plan view showing an example of a method for manufacturing a semiconductor device. Figures 17B, 17C, and 17D are cross-sectional views showing an example of a method for manufacturing a semiconductor device. Figure 18A is a plan view showing an example of a method for manufacturing a semiconductor device. Figures 18B, 18C, and 18D are cross-sectional views showing an example of a method for manufacturing a semiconductor device. Figure 19A is a plan view showing an example of a semiconductor device manufacturing method. Figures 19B, 19C, and 19D are cross-sectional views showing an example of a semiconductor device manufacturing method. Figure 20A is a plan view showing an example of a semiconductor device manufacturing method.Figures 20B, 20C, and 20D are cross-sectional views showing an example of a semiconductor device manufacturing method. Figure 21A is a plan view showing an example of a semiconductor device manufacturing method. Figures 21B, 21C, and 21D are cross-sectional views showing an example of a semiconductor device manufacturing method. Figure 22A is a plan view showing an example of a semiconductor device manufacturing method. Figures 22B, 22C, and 22D are cross-sectional views showing an example of a semiconductor device manufacturing method. Figure 23 is a block diagram illustrating an example of a semiconductor device configuration. Figures 24A, 24B, 24C, 24D, 24E, 24F, 24G, and 24H are diagrams illustrating an example of a memory cell circuit configuration. Figures 25A and 25B show an example of an electronic component. Figures 26A, 26B, and 26C show an example of a large-scale computer. Figure 26D shows an example of space equipment. Figure 26E shows an example of a storage system applicable to a data center.

[0032] Embodiments will be described in detail with reference to the drawings. However, it will be readily apparent to those skilled in the art that the present invention is not limited to the following description, and that its form and details can be modified in various ways without departing from the spirit and scope of the present invention. Accordingly, the present invention shall not be construed as being limited to the descriptions of the embodiments shown below.

[0033] In the invention described below, the same reference numerals are used in common across different drawings for identical parts or parts having similar functions, and repeated explanations are omitted. Furthermore, when referring to similar functions, the same hatching pattern may be used, and reference numerals may not be assigned.

[0034] Furthermore, for the sake of ease of understanding, the position, size, and scope of each component shown in the drawings may not represent their actual position, size, and scope. Therefore, the disclosed invention is not necessarily limited to the position, size, and scope disclosed in the drawings.

[0035] Furthermore, in particular, in plan views (also called "top views") or perspective views, the description of some components may be omitted to facilitate understanding of the invention. In addition, the description of some hidden lines may be omitted.

[0036] In this specification, the ordinal numbers "first," "second," etc., are used for convenience only and do not limit the number of components or the order of components (for example, process order or stacking order). Furthermore, the ordinal numbers used for components in one part of this specification may not be the same as those used for the same components in other parts of this specification or in the claims.

[0037] It should be noted that the terms "film" and "layer" can be interchanged depending on the context or situation. For example, the term "conductive layer" can be changed to "conductive film." Or, for example, the term "insulating film" can be changed to "insulating layer." Furthermore, the term "conductor" can be interchanged with the terms "conductive layer" or "conductive film" depending on the context or situation. Similarly, the term "insulator" can be interchanged with the terms "insulating layer" or "insulating film" depending on the context or situation.

[0038] Furthermore, in this specification, "parallel" means a state in which two lines are arranged at an angle of -10 degrees or more and 10 degrees or less. Therefore, the case of -5 degrees or more and 5 degrees or less is also included. Furthermore, "approximately parallel" means a state in which two lines are arranged at an angle of -20 degrees or more and 20 degrees or less. Furthermore, "perpendicular" means a state in which two lines are arranged at an angle of 80 degrees or more and 100 degrees or less. Therefore, the case of 85 degrees or more and 95 degrees or less is also included. Furthermore, "approximately perpendicular" means a state in which two lines are arranged at an angle of 70 degrees or more and 110 degrees or less.

[0039] An opening can include, for example, grooves and slits. Furthermore, the area in which an opening is formed may also be referred to as an opening.

[0040] Furthermore, in the drawings used in this specification, etc., the side walls of the insulator at the opening of the insulator are shown to be perpendicular or substantially perpendicular to the substrate surface or the surface to be formed, but they may also be tapered.

[0041] In this specification, a tapered shape refers to a shape in which at least a portion of the side surface of a structure is inclined with respect to the substrate surface or the surface to be formed. For example, it is preferable to have a region in which the angle between the inclined side surface and the substrate surface or the surface to be formed (hereinafter sometimes referred to as the taper angle) is less than 90°. The side surface of the structure and the substrate surface do not necessarily have to be perfectly flat, and may be substantially planar with a small curvature, or substantially planar with fine irregularities.

[0042] In this specification, "heights are equal or nearly equal" refers to a configuration in which the heights from a reference surface (for example, a flat surface such as the substrate surface) are equal in a cross-sectional view. For example, in the manufacturing process of a memory device, the surfaces of multiple layers may be exposed by a planarization process (typically a chemical mechanical polishing (CMP) method). In this case, the surfaces to be processed by the CMP process have a configuration in which the heights from the reference surface are equal. However, the heights of the multiple layers may differ depending on the processing apparatus, processing method, or material of the surface to be processed during the CMP process. In this specification, this case is also treated as "heights are equal or nearly equal." For example, if there are two layers with different heights (here referred to as a first layer and a second layer) with respect to a reference surface, the difference between the height of the top surface of the first layer and the height of the top surface of the second layer is 20 nm or less, which is also referred to as "heights are equal or nearly equal."

[0043] In this specification, "side edges coincide or nearly coincide" or "sides coincide or nearly coincide" means that, in a plan view, at least a portion of the contours of the stacked layers overlap. For example, this includes cases where the upper and lower layers are processed with the same mask pattern, or partially with the same mask pattern. However, strictly speaking, the contours may not overlap, and the contour of the upper layer may be located inside the contour of the lower layer, or the contour of the upper layer may be located outside the contour of the lower layer; in this case, it is also referred to as "side edges coincide or nearly coincide" or "sides coincide or nearly coincide."

[0044] In this specification, "planar shapes matching or nearly matching" means that at least a portion of the contours overlaps between stacked layers. For example, this includes cases where the upper and lower layers are processed with the same mask pattern, or partially with the same mask pattern. However, strictly speaking, the contours may not overlap, and the upper layer may be located inside the lower layer, or the upper layer may be located outside the lower layer; in these cases, it may also be said that the "planar shapes matching or nearly matching." Furthermore, when the planar shapes match or nearly match, it can also mean that the edges are aligned or nearly aligned, or that the side edges match or nearly match.

[0045] In this specification and elsewhere, the cubic crystal structure is sometimes referred to as cubic crystal or cubic structure. The same applies to other crystal systems (hexagonal, trigonal, tetragonal, orthorhombic, monoclinic, and triclinic).

[0046] (Embodiment 1) In this embodiment, a semiconductor device having an oxide semiconductor layer and a method for manufacturing the semiconductor device will be described with reference to Figures 1A to 22D.

[0047] <Example of Semiconductor Device Configuration> An example of a semiconductor device configuration will be explained using Figures 1A to 13. Figures 1A to 1D are plan views and cross-sectional views of a semiconductor device having a transistor 200 on a substrate (not shown).

[0048] Figure 1A is a plan view of the semiconductor device described above. Figures 1B to 1D are cross-sectional views of the same semiconductor device. Here, Figure 1B is a cross-sectional view of the area indicated by the dashed line A1-A2 in Figure 1A, and is also a cross-sectional view of the transistor 200 in the channel width direction. Figure 1C is a cross-sectional view of the area indicated by the dashed line A3-A4 in Figure 1A, and is also a cross-sectional view of the transistor 200 in the channel width direction. Figure 1D is a cross-sectional view of the area indicated by the dashed line A5-A6 in Figure 1A, and is also a cross-sectional view of the transistor 200 in the channel length direction. Here, the dashed line A5-A6 is perpendicular to the dashed lines A1-A2 and A3-A4, and the dashed lines A1-A2 and A3-A4 are parallel to each other. Note that in the plan view of Figure 1A, some elements have been omitted and some elements have been made transparent for clarity. Furthermore, Figure 2A shows an enlarged view of the vicinity of the conductor 260 in Figure 1D. Figure 2B shows an enlarged view of the vicinity of the oxide semiconductor 230 in Figure 1B. Figure 3 shows an enlarged view of the vicinity of the oxide semiconductor 230 in Figure 1C. Note that in this specification, when referring to a cross-section in the channel width direction, it does not necessarily include the channel formation region of the transistor. In some cases, the term "cross-section in the channel width direction" may include a cross-section parallel to the cross-section in the channel width direction that includes the channel formation region. For example, the cross-sectional view of the area indicated by the dashed line A3-A4 in Figure 1C is referred to as a cross-sectional view in the channel width direction.

[0049] The semiconductor device according to this embodiment includes an insulator 216 on a substrate (not shown), an insulator 221 on the insulator 216, an insulator 222 on the insulator 221, an insulator 224 on the insulator 222, an insulator 225 on the insulator 224, a metal oxide layer 235 in contact with the upper and side surfaces of the insulator 225 and the upper surface of the insulator 224, an oxide semiconductor 230 disposed on the insulator 224 and covering the metal oxide layer 235 and the insulator 225, conductors 242a (conductors 242a1 and conductors 242a2) and conductors 242b (conductors 242b1 and conductors 242b2) on the oxide semiconductor 230, an insulator 250 on the oxide semiconductor 230, and a conductor 260 on the insulator 250. The metal oxide layer 235 is preferably arranged in superimposition with the conductor 242b and not in superimposition with the conductors 242a and 260. Furthermore, in the following, the conductors 242a and 242b may be collectively referred to as the conductor 242.

[0050] An insulator 271a is provided on the conductor 242a, and an insulator 271b is provided on the conductor 242b. An insulator 275 is provided on the insulators 271a, 271b, and 222, and an insulator 280 is provided on the insulator 275. An opening 201 is provided in the insulators 280 and 275. The sides of the insulator 280 and the sides of the insulator 275 function as side walls of the opening 201. The sides of the conductors 242a1, 242a2, 242b1, and 242b2 can also be considered as side walls of the opening 201. Insulators 250 and 260 are arranged in the opening 201. Insulators 224, 225, and a portion of the oxide semiconductor 230 are also arranged in the opening 201. The opening 201 reaches the oxide semiconductor 230 and the insulator 222, and within the opening 201, the insulator 250 is in contact with the oxide semiconductor 230 and the insulator 222.

[0051] Furthermore, an insulator 255 is provided in the opening 201. The insulator 255 is positioned between the conductors 242a2, 242b2, insulator 275, and insulator 280 and insulator 250. The insulator 255 is formed in the shape of a sidewall that is in contact with the side wall of the opening 201. Since the insulator 255 is provided along the side wall of the opening 201, the insulator 255 can also be considered as part of the side wall of the opening 201.

[0052] An insulator 282 is provided on the insulator 280 and on the conductor 260. An insulator 283 is provided on the insulator 282. An insulator 285 is provided on the insulator 283. An insulator 215 is provided below the insulator 216.

[0053] An insulator 241a is provided in contact with the inner wall of an opening in the insulator 280, and a conductor 240a is provided in contact with the side surface of the insulator 241a. The lower surface of the conductor 240a is in contact with the upper surface of the conductor 242a. In addition, an insulator 241b is provided in contact with the inner wall of an opening in the insulator 280, and a conductor 240b is provided in contact with the side surface of the insulator 241b. The lower surface of the conductor 240b is in contact with the upper surface of the conductor 242b. In the following, conductors 240a and 240b may be collectively referred to as conductor 240. Also, insulators 241a and 241b may be collectively referred to as insulator 241.

[0054] The oxide semiconductor 230 has a region that functions as a channel formation region of the transistor 200. The conductor 260 also has a region that functions as a gate electrode of the transistor 200. The insulator 250 has a region that functions as a gate insulator of the transistor 200.

[0055] Conductor 242a has a region that functions as either the source electrode or the drain electrode of transistor 200. Conductor 240a functions as a plug that connects to conductor 242a. Conductor 242b has a region that functions as either the source electrode or the drain electrode of transistor 200. Conductor 240b functions as a plug that connects to conductor 242b.

[0056] Here, it is preferable that the metal oxide layer 235 is in contact with the upper and side surfaces of the insulator 225, overlaps with the conductor 242b, and does not overlap with the conductors 260 and 242a. With such a structure, the crystals elongated in the channel length direction of the oxide semiconductor 230 can be arranged in the region that overlaps with the conductor 260. Therefore, the number of crystal grain boundaries in the channel formation region can be reduced, and on-characteristics such as on-current and field-effect mobility can be improved.

[0057] Furthermore, it is preferable that the conductor 242a has a laminated structure of conductor 242a1 and conductor 242a2 on conductor 242a1, and that the conductor 242b has a laminated structure of conductor 242b1 and conductor 242b2 on conductor 242b1. It is preferable that the conductors 242a1 and conductor 242b1 that are in contact with the oxide semiconductor 230 are conductors that are not easily oxidized excessively. This prevents the conductors 242a and conductor 242b from becoming highly resistive due to oxygen contained in the oxide semiconductor 230. Thus, the contact resistance between conductor 242a1 and the oxide semiconductor 230, and the contact resistance between conductor 242b1 and the oxide semiconductor 230 can be reduced. Furthermore, it is preferable that conductors 242a2 and conductor 242b2 are conductors such as metal layers that have higher conductivity than conductors 242a1 and conductor 242b1. This allows the conductors 242a and 242b to function as highly conductive wiring or electrodes. In this way, a semiconductor device can be provided in which the conductors 242a and 242b, which function as wiring or electrodes, are provided in contact with the upper surface of the oxide semiconductor 230, which functions as an active layer.

[0058] As shown in Figure 2A, in a cross-sectional view of the transistor 200 in the channel length direction, the distance D1 between conductor 242a1 and conductor 242b1 is smaller than the distance D2 between conductor 242a2 and conductor 242b2. Here, distance D2 refers to the shortest distance between the opposing sides of conductor 242a2 and conductor 242b2. The difference between D1 and D2 may coincide with or approximately coincide with twice the film thickness of the insulator 255. Here, the film thickness of the insulator 255 refers to the film thickness in the A5-A6 direction in at least a portion of the insulator 255. With this configuration, the distance between the source and drain can be shortened, and the channel length can be shortened accordingly. Therefore, the frequency characteristics of the transistor 200 can be improved. In this way, by shortening the channel length, a semiconductor device with a high operating speed can be provided.

[0059] The opening 201 overlaps with the region between conductor 242a2 and conductor 242b2. It can also be considered that parts of conductor 242a1 and conductor 242b1 are formed to protrude into the opening 201. Therefore, the insulator 255 is in contact with the upper surface of conductor 242a1, the upper surface of conductor 242b1, the side surface of conductor 242a2, and the side surface of conductor 242b2 within the opening 201. In addition, the insulator 250 is in contact with the upper surface of insulator 222 and the upper surface of oxide semiconductor 230 in the region between conductor 242a1 and conductor 242b1.

[0060] The insulator 255 is preferably an insulator that is resistant to oxidation, such as a nitride. The insulator 255 is formed in contact with the side surfaces of the conductor 242a2 and the conductor 242b2, and has the function of protecting the conductor 242a2 and the conductor 242b2. After separating the conductor 242a1 and the conductor 242b1, it is preferable to perform heat treatment in an oxygen-containing atmosphere before forming the insulator 250. At this time, because the insulator 255 is formed in contact with the side surfaces of the conductor 242a2 and the conductor 242b2, it is possible to prevent the conductor 242a2 and the conductor 242b2 from being excessively oxidized.

[0061] The oxide semiconductor 230 is formed by covering the metal oxide layer 235 and the insulator 225. As shown in Figures 2B and 3, the insulator 225 has a shape with a high aspect ratio in a cross-sectional view in the channel width direction. For this reason, the insulator 225 can also be said to have a fin-like shape. Here, the aspect ratio of the insulator 225 in a cross-sectional view in the channel width direction refers to the ratio of the length L of the insulator 225 in the A1-A2 direction (which can also be called the width L of the insulator 225) to the length H of the insulator 225 in the direction perpendicular to the surface to which it is formed (for example, the insulator 224) (which can also be called the height H of the insulator 225). The aspect ratio of the insulator 225 is preferably as large as possible without the insulator 225 tipping over during the manufacturing process of the transistor 200. In the insulator 225, it is preferable that the height H is greater than the width L.

[0062] A high aspect ratio insulator 225 is covered by an oxide semiconductor 230 and a conductor 242. Near the channel formation region of the transistor 200, as shown in Figure 2B, the oxide semiconductor 230 is provided in a folded state with the insulator 225 in between. As a result, in a cross-sectional view in the channel width direction, the oxide semiconductor 230 and the conductor 260 are provided facing each other with the insulator 250 in between at the top of the insulator 225, the side on the A1 side, the side on the A2 side, and near the insulator 224. In other words, the top of the oxide semiconductor 230, the side on the A1 side, the side on the A2 side, and near the insulator 224 each function as a channel formation region. Therefore, compared to the case where the insulator 225 is not provided, the channel width of the transistor 200 is increased by the amount of the side on the A1 side and the side on the A2 side of the oxide semiconductor 230.

[0063] As described above, increasing the channel width improves the on-current, transconductance, and frequency characteristics of the transistor 200. This makes it possible to provide a semiconductor device with a high operating speed. It also makes it possible to increase the operating speed of a memory device using this semiconductor device. Furthermore, in the above structure, by covering the insulator 225 with the oxide semiconductor 230, the channel width can be increased without excessively expanding the area occupied by the transistor 200. This makes it possible to miniaturize or highly integrate the semiconductor device. It also makes it possible to increase the storage capacity of a memory device using this semiconductor device. In addition, with the above structure, the area where the sides of the conductor 260 and the oxide semiconductor 230 face each other becomes larger, so the threshold can be controlled to normally turn off the transistor 200.

[0064] Furthermore, as shown in Figure 2B, it is preferable that the film thickness t1 of the insulator 224 within the opening 201 is thicker than the film thickness t2 of the insulator 250. With this configuration, the lower surface (or lower end) of the conductor 260 located in a region within the opening 201 that does not overlap with the oxide semiconductor 230 is located below the lower surface (or lower end) of the oxide semiconductor 230. Therefore, a sufficient electric field can be applied from the conductor 260 to the upper and lower ends of the oxide semiconductor 230. This reduces the leakage current between the source electrode and the drain electrode via the lower end of the oxide semiconductor 230. In addition, it is possible to suppress characteristic defects such as normally-on behavior of the transistor caused by this leakage current. In other words, the electrical characteristics of the transistor 200 can be improved.

[0065] The above describes a configuration in which one transistor 200 is provided on one island-shaped oxide semiconductor 230, but the present invention is not limited to this. For example, as shown in Figures 4A to 4D, two transistors (transistor 200_1 and transistor 200_2) can be provided on one island-shaped oxide semiconductor 230. Here, Figures 4A to 4D correspond to Figures 1A to 1D, and corresponding components are denoted by the same reference numerals. Therefore, for details of the configurations shown in Figures 4A to 4D, refer to the description in Figures 1A to 1D. Note that for the components of transistor 200_2, the reference numerals are omitted for components that are the same as those of transistor 200_1.

[0066] The transistors 200_1 and 200_2 shown in Figures 4A to 4D have a structure in which two transistors 200, shown in Figures 1A to 1D, are provided with the dashed line A3-A4 as the axis of symmetry. Here, transistors 200_1 and 200_2 are provided on insulators 224 and 225, and oxide semiconductor 230. Furthermore, the metal oxide layer 235, conductor 242b, insulator 271b, conductor 240b, and insulator 241b formed between transistors 200_1 and 200_2 function as components of both transistors 200_1 and 200_2. In other words, transistors 200_1 and 200_2 are arranged symmetrically with respect to the metal oxide layer 235, conductor 242b, insulator 271b, conductor 240b, and insulator 241b. On the other hand, insulator 250, conductor 260, insulator 255, conductor 242a, insulator 271a, conductor 240a, and insulator 241a are individually provided for transistor 200_1 and transistor 200_2, respectively.

[0067] Here, for convenience, the insulators 250, conductors 260, insulator 255, conductor 242a, insulator 271a, conductor 240a, and insulator 241a, which are individually provided, are denoted as _1 and _2, and the configurations of transistors 200_1 and 200_2 can be shown as follows. Transistor 200_1 has insulators 224, insulator 225, oxide semiconductor 230, metal oxide layer 235, conductor 242b, insulator 271b, conductor 240b, insulator 241b, insulator 250_1, conductor 260_1, insulator 255_1, conductor 242a_1, insulator 271a_1, conductor 240a_1, and insulator 241a_1. The transistor 200_2 has an insulator 224, an insulator 225, an oxide semiconductor 230, a metal oxide layer 235, a conductor 242b, an insulator 271b, a conductor 240b, an insulator 241b, an insulator 250_2, a conductor 260_2, an insulator 255_2, a conductor 242a_2, an insulator 271a_2, a conductor 240a_2, and an insulator 241a_2.

[0068] In addition, transistors 200_1 and 200_2 are provided between insulators 215, 216, 221, and 222, which function as interlayer films, and insulators 275, 280, 282, 283, and 285, similar to transistor 200.

[0069] As described above, by sharing some components and providing two transistors, the area occupied by the transistors can be reduced, thereby enabling higher integration of the semiconductor device. For example, when this semiconductor device is used as a memory device, the number of elements per unit area can be increased, thereby increasing the memory capacity.

[0070] Figures 4A to 4D show a configuration in which transistors 200_1 and 200_2 are formed around the dashed line A3-A4, but the present invention is not limited to this. Transistors 200_1 and 200_2 do not have to be arranged symmetrically. At least, it is preferable that a metal oxide layer 235 is provided between the conductor 260 of transistor 200_1 and the conductor 260 of transistor 200_2.

[0071] Furthermore, the following description will mainly focus on transistor 200, similar to Figure 1, but the description of transistor 200 can be reflected in the configurations of transistors 200_1 and 200_2.

[0072] The oxide semiconductor 230 shown in Figure 1, etc., preferably has good crystallinity. This reduces carrier scattering in the oxide semiconductor 230, enabling the realization of a transistor with high field-effect mobility. It also enables the realization of a highly reliable transistor. Furthermore, the metal oxide layer 235 preferably has good crystallinity. The metal oxide layer 235 functions as a seed or nucleus when processing to improve the crystallinity of the oxide semiconductor 230, thus improving the crystallinity of the oxide semiconductor 230.

[0073] The oxide semiconductor 230 has a channel-forming region. The oxide semiconductor 230 further has a source region and a drain region. The source region and drain region are n-type regions (low-resistance regions) with a higher carrier concentration compared to the channel-forming region. The oxide semiconductor 230 may have a single-layer structure or a stacked structure of two or more layers.

[0074] The transistor 200 has a metal oxide that functions as a semiconductor in the oxide semiconductor 230, which includes a channel formation region. In the following, a transistor in which a channel is formed in an oxide semiconductor, such as transistor 200, may be referred to as an OS transistor. In this specification, since the oxide semiconductor 230 has a metal oxide, the oxide semiconductor 230 can be replaced with a metal oxide layer. In addition, a transistor having silicon in the channel formation region may be referred to as a Si transistor.

[0075] OS transistors have oxygen vacancies (V) in the channel formation region of an oxide semiconductor. OThe presence of oxygen vacancies and impurities can easily lead to fluctuations in electrical properties and reduced reliability. Therefore, it is preferable that oxygen vacancies and impurities be reduced as much as possible in the channel formation region of an oxide semiconductor. In other words, it is preferable that the channel formation region in an oxide semiconductor has a reduced carrier concentration and is i-type (intrinsic) or substantially i-type.

[0076] Furthermore, when an excess amount of oxygen is supplied to the oxide semiconductor 230, electron traps caused by the excess oxygen are formed in the insulator 250. As a result, the OS transistor becomes more susceptible to positive drift degradation in +GBT (Gate Bias-Temperature) stress tests. In other words, the amount of positive drift degradation in +GBT stress tests increases.

[0077] Therefore, in a semiconductor device according to one aspect of the present invention, it is preferable that the impurity concentration in the oxide semiconductor 230 is low. It is also preferable that an appropriate amount of oxygen is supplied to the oxide semiconductor 230. Furthermore, it is preferable to reduce the excess amount of oxygen in the oxide semiconductor 230.

[0078] It is preferable to use indium oxide for the oxide semiconductor 230. In this case, the oxide semiconductor 230 contains indium and oxygen. For example, it is preferable that the oxide semiconductor 230 has an indium oxide film. The higher the ratio of the number of indium atoms to the sum of the number of atoms of all metal elements contained in the metal oxide, the higher the field-effect mobility of the transistor can be. Therefore, by using indium oxide for the oxide semiconductor 230, the transistor can obtain a large on-current and high frequency characteristics.

[0079] Furthermore, it is preferable that the indium oxide film is crystalline. For example, it is preferable that the indium oxide film has crystal grains. Examples of films having crystal grains include single-crystal films, polycrystalline films, or amorphous films containing crystal grains. A polycrystalline film is composed of two or more crystal grains, while a single-crystal film can be considered to be composed of one crystal grain. In polycrystalline films, crystal grain boundaries (also called grain boundaries) can be observed, whereas in single-crystal films, crystal grain boundaries cannot be observed.

[0080] Furthermore, unlike polycrystalline films, single-crystal films do not exhibit grain boundaries in the channel formation region. Impurities that inhibit carrier flow (typically insulating impurities, insulating oxides, etc.) tend to segregate at grain boundaries. Therefore, when grain boundaries are present in the channel formation region, variations in transistor characteristics become large. On the other hand, in a single-crystal film according to one aspect of the present invention, since no grain boundaries are observed in the channel formation region, it exhibits the excellent effect of suppressing variations in transistor characteristics caused by such grain boundaries.

[0081] Furthermore, in this specification, a semiconductor layer in which no grain boundaries are observed in the channel-forming region, a semiconductor layer in which the channel-forming region is contained within a single crystal grain, or a semiconductor layer in which the crystal axis directions are the same in at least two regions within the channel-forming region can be called a single-crystal film. Alternatively, a semiconductor layer in which at least one crystal orientation is oriented in one direction in the channel-forming region can be called a single-crystal film.

[0082] The channel-forming region refers to a region within a semiconductor layer that overlaps with (or faces) the gate electrode via the gate insulating layer, and is located between the region in contact with the source electrode and the region in contact with the drain electrode. Furthermore, a semiconductor layer in which no grain boundaries are observed in the region between the source electrode and the drain electrode, a semiconductor layer in which the region between the source electrode and the drain electrode is contained within a single crystal grain, or a semiconductor layer in which at least two regions located between the source electrode and the drain electrode have the same crystal axis direction can also be called a single-crystal film. Alternatively, a semiconductor layer in which at least one crystal orientation is oriented in one direction in the region between the source electrode and the drain electrode can also be called a single-crystal film.

[0083] Furthermore, in the channel formation region, the current path is the shortest distance between the source electrode and the drain electrode. Therefore, the crystal grains, grain boundaries, crystal axes, and crystal orientations in the channel formation region, or the region located between the region in contact with the source electrode and the region in contact with the drain electrode, can be confirmed by cross-sectional observation including the semiconductor layer, source electrode, and drain electrode.

[0084] The crystallinity of the oxide semiconductor 230 can be analyzed, for example, by X-ray diffraction (XRD), transmission electron microscopy (TEM), or electron diffraction (ED). Alternatively, a combination of these methods may be used for the analysis.

[0085] Crystal grains can be identified, for example, using high-resolution transmission electron microscope (TEM) images. Furthermore, crystal grain boundaries can sometimes be identified, for example, using high-resolution TEM images. In other words, crystal grains and crystal grain boundaries can sometimes be observed in high-resolution TEM images of crystalline films. The overall magnification when acquiring TEM images is preferably 2 million times or more, and more preferably 4 million times or more.

[0086] The indium oxide film is more preferably a single-crystal film. Since a single-crystal film does not have grain boundaries, carrier scattering at grain boundaries can be suppressed, enabling the realization of transistors with high field-effect mobility. Furthermore, highly reliable transistors can be realized.

[0087] The indium oxide film may be a polycrystalline film or an amorphous film containing crystal grains. In this case, it is preferable that no crystal grain boundaries are observed or that there are few grain boundary components in the channel formation region. For example, by having one crystal grain located in the channel formation region, it is possible to create a configuration in which no crystal grain boundaries are observed in the channel formation region. Even with such a configuration, the same effects as the configuration in which the indium oxide film is a single crystal film can be achieved.

[0088] Furthermore, two or more crystal grains can be located in the channel-forming region. For example, when a first crystal grain and a second crystal grain are located in the channel-forming region, it is preferable that the crystal orientation of the first crystal grain and the crystal orientation of the second crystal grain coincide or approximately coincide. When the crystal orientations of the first and second crystal grains coincide or approximately coincide, a grain boundary may not be observed at the boundary between the first and second crystal grains. By having the crystal orientations of the first and second crystal grains coincide or approximately coincide, the formation of a grain boundary between the first and second crystal grains can be suppressed. Therefore, even in such a configuration, the same effects as in a configuration where the indium oxide film is a single crystal film can be achieved. Note that the coincidence or approximately coincidence of the crystal orientations of the first and second crystal grains can sometimes be confirmed, for example, by a high-resolution TEM image. Specifically, in a high-resolution TEM image, if the lattice fringes of the first crystal grain and the lattice fringes of the second crystal grain are continuously connected at the boundary between the first and second crystal grains, then it can be said that the crystal orientation of the first crystal grain and the crystal orientation of the second crystal grain coincide or nearly coincide.

[0089] In this specification, a grain boundary refers to, for example, a grain boundary formed at the boundary between adjacent grains with different crystal orientations. Therefore, in this specification, a grain boundary formed at the boundary between adjacent grains with the same crystal orientation is not included in the definition of a grain boundary. For example, even if a boundary is observed between two crystal grains in a high-resolution TEM image, if the crystal orientations of the two crystal grains are the same or nearly the same, the boundary may not be referred to as a grain boundary.

[0090] The degree of polycrystalline nature of an indium oxide film can be evaluated by the grain size. The grain size can be calculated, for example, by determining the area of ​​the grain and then determining the diameter of a circle corresponding to that area. This diameter is sometimes referred to as the area-circle equivalent diameter.

[0091] Furthermore, the degree of polycrystalline nature of an indium oxide film can also be evaluated by the length of the grain boundaries. The length of the grain boundaries can be calculated, for example, by extracting a field of view of a specific area from a TEM image of the film acquired at a total magnification where the grain boundaries can be observed, and summing the lengths of the grain boundaries observed in that field of view. An indium oxide film with a grain boundary length of 0 nm can be considered a single-crystal film. Also, a longer grain boundary length indicates a higher proportion of grain boundary components.

[0092] The extended grain boundary length in the indium oxide film is preferably 0 nm to 1500 nm, more preferably 0 nm to 1000 nm, and even more preferably 0 nm to 800 nm. By having an indium oxide film with an extended grain boundary length within the above range in the oxide semiconductor 230, a configuration can be achieved in which no crystal grain boundaries are observed or where there are few grain boundary components in the channel formation region. Unless otherwise specified in this specification, the field of view used to calculate the extended grain boundary length is 90 nm square.

[0093] The film thickness of the oxide semiconductor 230 is more preferably 2 nm to 50 nm, more preferably 2.5 nm to 30 nm, more preferably 2.5 nm to 20 nm, more preferably 5 nm to 20 nm, and even more preferably 5 nm to 10 nm. It is sufficient that the oxide semiconductor 230 has regions with the above-mentioned film thickness in at least a portion of it. For example, it is sufficient that the channel-forming region of the oxide semiconductor 230 has regions with the above-mentioned film thickness. By setting the film thickness of the oxide semiconductor 230 within the above range, the crystallinity of the oxide semiconductor 230 can be increased. By increasing the crystallinity of the oxide semiconductor 230, the oxide semiconductor 230 can have crystal grains.

[0094] Note that when the metal oxide contains indium and zinc, the metal oxide may have a CAAC (c-axis aligned crystal) structure. The CAAC structure has fewer crystal grain boundaries in the a-b plane than a polycrystalline structure. Examples of the metal oxide containing indium and zinc include indium zinc oxide (also referred to as In-Zn oxide, IZO (registered trademark)), indium gallium zinc oxide (also referred to as In-Ga-Zn oxide, IGZO), and the like.

[0095] In the crystalline oxide semiconductor layer, the indium oxide film is a film in which one or both of hydrogen and oxygen are more likely to move, for example, as compared with an IGZO film. Therefore, it can be said that the indium oxide film is a film to which one or both of hydrogen and oxygen are more likely to be supplied, and from which one or both of hydrogen and oxygen are more likely to be discharged, for example, as compared with an IGZO film. Note that the indium oxide film can be said to be a film having higher permeability to one or both of hydrogen and oxygen, for example, as compared with an IGZO film. In other words, the indium oxide film can be said to be a film having lower barrier properties against one or both of hydrogen and oxygen, for example, as compared with an IGZO film.

[0096] The indium oxide film is subjected to a heat treatment at a heating temperature of 400° C. for a treatment time of 8 hours, for example, oxygen is 1×10 20 atoms / cm 3 or more and 2×10 21 atoms / cm 3 or less, preferably 2×10 20 atoms / cm 3 or more and 1×10 21 atoms / cm 3 or less. It is preferable to have a property of transmitting oxygen. In addition, the indium oxide film is subjected to a heat treatment at a heating temperature of 400° C. for a treatment time of 8 hours, so that, for example, 1×10 20 atoms / cm 3 or more and 2×10 21 atoms / cm 3 or less, preferably 2×10 20 atoms / cm 3 or more and 1×10 21 atoms / cm 3The following oxygen molecules preferably have the property of diffusing within the crystal grains.

[0097] Oxygen in the indium oxide film diffuses through the crystal grains and grain boundaries, causing V to be present in the crystal grains or grain boundaries. O This can reduce the noise. Therefore, the electrical characteristics and reliability of the transistor can be improved.

[0098] The band gap of indium oxide is between 2.5 eV and 3.7 eV. By using indium oxide, which has a large band gap, in the oxide semiconductor 230, the off-current of the transistor can be reduced, and the power consumption of the semiconductor device can be significantly reduced.

[0099] An OS transistor is a storage-type transistor that uses electrons as its majority carriers. In other words, the carriers in an OS transistor are electrons. Assuming that the carrier relaxation time is constant, the smaller the effective mass of electrons (carriers), the higher the electron mobility (carrier mobility). Therefore, by using a metal oxide with a small effective mass of electrons in the semiconductor layer of the transistor, the on-current, frequency characteristics (also called f-characteristics), or field-effect mobility of the transistor can be improved.

[0100] Furthermore, indium oxide has a large effective hole mass. Therefore, by using indium oxide, which has a large effective hole mass, in the oxide semiconductor 230, a transistor with an extremely low off-current can be realized. In addition, the effective hole mass of indium oxide is larger than, for example, the effective hole mass of silicon. Therefore, from the viewpoint of the effective hole mass, the off-current of a transistor using indium oxide in the channel formation region is significantly smaller than the off-current of a Si transistor.

[0101] In a transistor using indium oxide as the oxide semiconductor 230, the off-current value at room temperature per 1 μm channel width is 1 × 10⁻¹⁶ −17 A / μm or less, preferably 1 × 10 −18 A / μm or less, more preferably 1 × 10 −19 It is possible to reduce the A / μm or less. Also, the off-current value at 85°C per 1 μm of channel width is 1 × 10⁻¹⁶ −16A / μm or less, preferably 1 × 10 −17 A / μm or less, more preferably 1 × 10 −18 It is possible to reduce the A / μm level to less than or equal to 1 / μm.

[0102] Furthermore, miniaturizing the OS transistor can improve the frequency characteristics of the transistor. For example, the cutoff frequency of the transistor can be improved. Specifically, the cutoff frequency of the transistor can be set to 50 GHz or higher, preferably 100 GHz or higher, and more preferably 150 GHz or higher, under room temperature conditions.

[0103] The indium oxide film may contain other elements, as long as the crystal structure of the crystal grains maintains a cubic crystal system. For example, in addition to indium, a first element may be included. The first element may be one or more selected from tin, zinc, antimony, copper, cobalt, and gallium. The content of the first element in the crystal grains is preferably 0.1% or more and less than 30%, more preferably 0.1% or more and less than 20%, more preferably 0.1% or more and less than 10%, and even more preferably 0.1% or more and less than 5%. When elements Mx1 and Mx2 are selected as the first element, the content of the first element in the crystal grains can be calculated as the sum of the content of element Mx1 and the content of element Mx2 in the crystal grains. For example, by adding atoms that can become cations with a valence of 4 or higher (tin, antimony, and cobalt) to indium oxide, these atoms can substitute for indium atoms, resulting in one or more electrons remaining, and the carrier concentration of the oxide semiconductor layer can be increased. Furthermore, by adding atoms that can become divalent or less cations (zinc and copper) to indium oxide, for example, these atoms can substitute for indium atoms, resulting in a deficiency of one or more electrons and thus reducing the carrier concentration in the oxide semiconductor layer.

[0104] In this specification, the content of a metal element in a metal oxide refers to the ratio of the number of atoms of that element to the total number of atoms of that metal element contained in the metal oxide. For example, if a metal oxide contains metal elements X, Y, and Z, then the number of atoms of each of metal elements X, Y, and Z contained in the metal oxide is A. X A Y AZ In this case, the content of metal element X is A X / (A X +A Y +A Z ) can be shown as follows. Also, the ratio of the number of atoms of metal elements X, Y, and Z in a metal oxide (atomic ratio) is B X : B Y : B Z When shown as follows, the content of metal element X is B X / (B X +B Y +B Z This can be shown by:

[0105] Figures 1A to 1D show an example where the oxide semiconductor 230 has a single-layer structure, but it is not limited to this, and the oxide semiconductor 230 can have a stacked structure of two or more layers. For example, in the configuration example shown in Figure 8A, the oxide semiconductor 230 has an oxide semiconductor 230a, an oxide semiconductor 230b on the oxide semiconductor 230a, and an oxide semiconductor 230c on the oxide semiconductor 230b. Note that the boundaries between oxide semiconductor 230a and oxide semiconductor 230b, and between oxide semiconductor 230b and oxide semiconductor 230c may be unclear, so these boundaries are shown with dotted lines in Figure 8A, etc.

[0106] The oxide semiconductors 230a to 230c preferably contain indium oxide. Furthermore, oxide semiconductors 230a and 230c may contain indium oxide containing a second element. For example, one or more of the following can be used as the second element: gallium, aluminum, yttrium, scandium, titanium, tungsten, molybdenum, tin, zirconium, hafnium, and tantalum. The second element is preferably one or more selected from gallium, aluminum, scandium, and yttrium, more preferably gallium or aluminum, and even more preferably gallium.

[0107] For example, the oxide semiconductors 230a to 230c can be indium gallium oxide (In-Ga oxide), indium gallium aluminum oxide (In-Ga-Al oxide), indium gallium tin oxide (In-Ga-Sn oxide), aluminum zinc oxide (Al-Zn oxide, also written as AZO), indium aluminum zinc oxide (In-Al-Zn oxide, also written as IAZO), indium gallium zinc oxide (In-Ga-Zn oxide, also written as IGZO), indium gallium tin zinc oxide (In-Ga-Sn-Zn oxide, also written as IGZTO), indium gallium aluminum zinc oxide (In-Ga-Al-Zn oxide, also written as IGAZO or IAGZO), etc.

[0108] Furthermore, the oxide semiconductor can be configured such that one or two of the oxide semiconductors 230a to 230c contain a second element but do not contain indium. For example, gallium oxide, zinc gallium oxide (also written as Ga-Zn oxide or GZO), etc., can be used.

[0109] Oxides containing the second element have a larger band gap than indium oxide. Therefore, the band gap of indium oxide containing the second element may be larger than that of indium oxide. Also, the electron affinity of indium oxide containing the second element may be smaller than that of indium oxide. By making the electron affinity of oxide semiconductors 230a and 230c smaller than that of oxide semiconductor 230b, the carrier flow path can be moved away from the interface between the insulator 250 and the oxide semiconductor 230, which may reduce the effects of surface scattering. As a result, it may be possible to increase the on-current or improve reliability. With such a configuration, the transistor can be made into an embedded channel structure.

[0110] For example, the oxide semiconductor 230a and oxide semiconductor 230c can be made using In-Ga oxide, and the oxide semiconductor 230b can be made using indium oxide. Alternatively, the oxide semiconductor 230a and oxide semiconductor 230c can be made using gallium oxide, and the oxide semiconductor 230b can be made using indium oxide. Alternatively, the oxide semiconductor 230a and oxide semiconductor 230c can be made using gallium oxide, and the oxide semiconductor 230b can be made using In-Ga oxide. Alternatively, the oxide semiconductor 230a can be made using gallium oxide, the oxide semiconductor 230b can be made using indium oxide, and the oxide semiconductor 230c can be made using In-Ga oxide. In the above In-Ga oxide, it is also possible to add a small amount of gallium to the indium oxide. In this case, for example, it is preferable to make the gallium concentration 5 atomic% or less. Here, the gallium concentration in the In-Ga oxide refers to the ratio of the number of gallium atoms to the sum of the number of indium and gallium atoms.

[0111] The crystallinity of the metal oxides in oxide semiconductors 230a and 230c is not particularly limited. For example, oxide semiconductors 230a and 230c may include one or more amorphous semiconductors (semiconductors having an amorphous structure), single-crystal semiconductors (semiconductors having a single-crystal structure), or semiconductors having crystalline properties other than single crystals (microcrystalline semiconductors, polycrystalline semiconductors, or semiconductors having crystalline regions in part).

[0112] Next, the crystal structure of the oxide semiconductor 230 will be described using Figures 5A to 5D. In one embodiment of the present invention, the oxide semiconductor 230 and the insulator 224 are formed in island shapes, as shown in Figure 4A, etc. Before the oxide semiconductor 230 and the insulator 224 are formed in island shapes, a film that will become the oxide semiconductor 230 (hereinafter referred to as the oxide semiconductor film 230f) and a film that will become the insulator 224 (hereinafter referred to as the insulating film 224f) are deposited, as shown in Figure 5D. Figures 5A to 5C show the process of manufacturing the oxide semiconductor film 230f shown in Figure 5D.

[0113] Figures 5A to 5D are perspective views corresponding to the structures shown in Figures 4A to 4D. However, Figures 5A to 5D illustrate a configuration in which multiple insulators 225 are provided in accordance with the arrangement of multiple transistors. Figures 5A to 5D are also labeled with the X, Y, and Z axes.

[0114] In Figure 5D, a metal oxide layer 235 and an insulator 225 are provided in contact with the upper surface of the insulating film 224f, and an oxide semiconductor film 230f is provided so as to cover the metal oxide layer 235 and the insulator 225. As shown in Figure 5D, the insulator 225 is provided extending in the X-axis direction, and the metal oxide layer 235 is provided extending in the Y-axis direction. Furthermore, multiple insulators 225 can be provided arranged in the Y-axis direction. Here, it is preferable that the metal oxide layer 235 is provided in contact with the upper and side surfaces of each insulator 225. That is, in a plan view, the metal oxide layer 235 is provided intersecting with multiple insulators 225. For example, in a plan view, the metal oxide layer 235 can be provided orthogonally to multiple insulators 225.

[0115] Here, a portion of Figure 5D corresponds to Figure 4A, and region 220_1 shown in Figure 5D is the region where transistor 200_1 is formed, and region 220_2 is the region where transistor 200_2 is formed. In other words, transistors 200_1 and 200_2 can be formed on each insulator 225 with a metal oxide layer 235 in between. Furthermore, as shown in Figure 5D, by arranging multiple insulators 225 in the Y-axis direction, a configuration can be made in which multiple transistors are arranged in the Y-axis direction.

[0116] The metal oxide layer 235 has crystals. The metal oxide layer 235 functions as a seed or nucleus when performing a treatment to enhance the crystallinity of the oxide semiconductor film 230f. In other words, the metal oxide layer 235 functions as a seed or nucleus when the oxide semiconductor film 230f undergoes crystal growth. In this specification, the metal oxide layer 235, or the crystals contained in the metal oxide layer 235, can be referred to as a seed crystal or a crystal nucleus. Furthermore, since the metal oxide layer 235 has crystals, the metal oxide layer 235 can be referred to as a crystalline portion.

[0117] Indium oxide crystals have a cubic crystal structure (Bixbite type). When using indium oxide in the oxide semiconductor film 230f, it is preferable to use an oxide with a cubic crystal structure as the metal oxide layer 235. By having the metal oxide layer 235 crystals have the same crystal structure as the oxide semiconductor film 230f crystals, the oxide semiconductor film 230f can be epitaxially grown with the metal oxide layer 235 as a nucleus, thereby increasing the crystallinity of the oxide semiconductor film 230f. As the metal oxide layer 235, oxides containing indium (typically indium oxide), oxides containing one or both of yttrium and zirconium, erbium oxide, etc., can be used. Examples of oxides containing one or both of yttrium and zirconium include yttrium oxide, zirconium oxide, and oxides containing both yttrium and zirconium. Furthermore, as the metal oxide layer 235, a metal oxide containing indium and the first element mentioned above can be used. Examples of such metal oxides include indium tin oxide (In-Sn oxide, also known as ITO). These oxides have a cubic crystal structure.

[0118] When indium oxide is used for the metal oxide layer 235, the oxide semiconductor film 230f can be homoepitaxially grown using the metal oxide layer 235 as a nucleus, thereby increasing the crystallinity of the oxide semiconductor film 230f. In this case, the crystal orientation of the crystals in the metal oxide layer 235 and the crystal orientation of the crystals in the oxide semiconductor film 230f are identical or nearly identical. For example, using the method described later, indium oxide having a crystal orientation of <111> with respect to the surface to be formed, similar to the oxide semiconductor film 230f, can be formed, and the metal oxide layer 235 can be formed by processing the indium oxide. This makes it possible to homoepitaxially grow an oxide semiconductor film 230f with a crystal orientation of <111> using the metal oxide layer 235 with a crystal orientation of <111> as a nucleus.

[0119] As shown in Figure 5D, it is preferable that the crystal orientation of the crystal grains of the oxide semiconductor film 230f matches or substantially matches the surface to be formed at all locations. For example, as shown in Figure 5D, it is preferable that the crystal orientation <111> of the crystal grains of the oxide semiconductor film 230f is perpendicular to the surface to be formed in the region in contact with the upper surface of the insulator 225, the region in contact with the side surface of the insulator 225, and the region in contact with the upper surface of the insulating film 224f. In other words, it is preferable that the crystal orientation <111> of the crystal grains of the oxide semiconductor film 230f in the region in contact with the upper surface of the insulator 225 and the region in contact with the upper surface of the insulating film 224f intersects or is perpendicular to each other with the crystal orientation <111> of the crystal grains of the oxide semiconductor film 230f in the region in contact with the side surface of the insulator 225.

[0120] This is also true for the oxide semiconductor 230 of the transistor 200 shown in Figure 2B, and it is preferable that the crystal orientation of the crystal grains of the oxide semiconductor 230 relative to the surface being formed in the region in contact with the side surface of the insulator 225 and the crystal orientation of the crystal grains relative to the surface being formed in the region in contact with the top surface of the insulator 225 coincide or substantially coincide. Here, the crystal orientation <111> of the crystal grains of the oxide semiconductor 230 is perpendicular or substantially perpendicular to the surface being formed (the top surface of the insulator 225, the side surface of the insulator 225, the top surface of the insulator 224, etc.) at all locations. Therefore, it can also be said that the crystal orientation <111> of the crystal grains of the oxide semiconductor 230 is perpendicular or substantially perpendicular to the top surface and side surface of the insulator 225, and the top surface of the insulator 224.

[0121] Crystal orientation can be evaluated by the diffraction pattern (also called the nano-beam electron diffraction pattern) observed by nano-beam electron diffraction (NBED). Alternatively, it can be evaluated by the pattern (also called the FFT pattern) obtained by performing a Fast Fourier Transform (FFT) on the TEM image. The FFT pattern reflects reciprocal lattice space information similar to that of the diffraction pattern described above.

[0122] As described above, the oxide semiconductor 230 functions as a channel-forming region both near the top surface and near the side surface of the insulator 225. Therefore, the uniform crystal structure of the oxide semiconductor 230 in the region near the top surface and near the side surface of the insulator 225 helps to stabilize the electrical characteristics of the transistor 200. This improves the on-current, field-effect mobility, and frequency characteristics of the transistor 200.

[0123] In this specification, space groups are expressed using international notation (or Hermann-Mauguin notation) in short notation. Crystal planes and crystal orientations are expressed using Miller indices. In crystallography, space groups, crystal planes, and crystal orientations are expressed by superscripting numbers, but in this specification, due to formatting constraints, a minus sign (-) may be placed before the number instead of a superscript. Individual orientations within a crystal are represented by [ ], collective orientations representing all equivalent orientations are represented by < >, individual crystal planes are represented by ( ), and collective planes with equivalent symmetry are represented by {}.

[0124] In this specification, the crystal orientation of an oxide semiconductor crystal refers to the orientation of the oxide semiconductor with respect to the surface on which it is formed. For example, a crystal with a crystal orientation of <100> can be said to be a crystal in which the (100) plane is parallel to the surface on which it is formed. Here, if the surface on which it is formed has multiple regions with different angles, as shown on the top and side surfaces of the insulator 225 in Figure 5D, the crystal orientation of the oxide semiconductor crystal refers to the orientation of the regions on which the oxide semiconductor is in contact with the surface on which it is formed.

[0125] Furthermore, it is preferable that the difference (also called lattice mismatch) between the lattice constant or unit cell vector of the crystal nucleus and the lattice constant or unit cell vector of the crystal of the oxide semiconductor film 230f is small. By using an oxide that reduces lattice mismatch for the metal oxide layer 235, the crystallinity of the oxide semiconductor film 230f can be improved.

[0126] One method for evaluating the degree of lattice mismatch is the lattice mismatch index. The lattice mismatch index Δa [%] of the crystals of the forming film relative to the crystals of the film being formed is calculated using the following formula (1). Hereafter, the lattice mismatch index Δa of the crystals of the forming film relative to the crystals of the film being formed may simply be referred to as the lattice mismatch index Δa of the forming film relative to the film being formed.

[0127]

[0128] In formula (1), L 1 L is the lattice constant or unit cell vector of the crystal of the formed film. 2 This is the lattice constant or unit cell vector of the crystal of the film to be formed.

[0129] The lattice mismatch Δa of the crystal grains of the oxide semiconductor film 230f with respect to the crystal nucleus is preferably -10% or more and 10% or less, more preferably -5% or more and 5%, and even more preferably -3% or more and 3% or less. By using a material for the metal oxide layer 235 that has a smaller absolute value of lattice mismatch with respect to the oxide semiconductor film 230f, the crystallinity of the oxide semiconductor film 230f can be improved.

[0130] For example, the lattice constant of indium oxide crystals (Bixbite type) is said to be 1.01194 nm. Also, the lattice constant of yttrium oxide crystals (Bixbite type) is said to be 1.05976 nm. Therefore, the degree of lattice mismatch between the crystals of indium oxide and those of yttrium oxide is -4.5%. Thus, when using indium oxide for the oxide semiconductor film 230f, yttrium oxide can be used as the metal oxide layer 235.

[0131] For example, the lattice constant of an erbium oxide crystal (Bixbyte type) is said to be 1.0582 nm. Therefore, the degree of lattice mismatch between the crystal of indium oxide and that of erbium oxide is -4.4%. Thus, when using indium oxide for the oxide semiconductor film 230f, erbium oxide can be used as the metal oxide layer 235.

[0132] For example, Zr is an example of yttrium zirconium oxide. 0.9 Y 0.1 O 1.95 The lattice constant of the crystal (fluorite type) is 0.51481 nm (see ICSD col.code.248790). Therefore, Zr 0.9 Y 0.1 O 1.95 The lattice mismatch of indium oxide with respect to the crystal is -1.7%. Therefore, when indium oxide is used for the oxide semiconductor film 230f, yttrium zirconium oxide can be suitably used as the metal oxide layer 235. Yttrium zirconium oxide contains yttrium, zirconium, and oxygen.

[0133] The crystal structure of zirconium oxide can be stabilized by adding yttrium or yttrium oxide to zirconium oxide, that is, by increasing the yttrium content in yttrium zirconium oxide to more than 0 atomic percent. However, if the content is too high, the crystal structure of yttrium zirconium oxide may change from a cubic crystal system to another crystal system, so it is preferable that the content not be too high. For example, the yttrium content in yttrium zirconium oxide is preferably 2 atomic percent or more and 15 atomic percent or less, and more preferably 5 atomic percent or more and 10 atomic percent or less.

[0134] Furthermore, the metal oxide layer 235 can also have a hexagonal or trigonal crystal structure. In this case, by having crystals in the metal oxide layer 235 whose crystal orientation with respect to the surface or the surface to be formed on the metal oxide layer 235 is <001>, an oxide semiconductor film 230f having crystals with a crystal orientation of <111> can be formed. When the crystal orientation of the crystals in the metal oxide layer 235 with respect to the surface or the surface to be formed on the metal oxide layer 235 is <001>, the c-axis of the crystal is perpendicular or approximately perpendicular to the surface or the surface to be formed on the metal oxide layer 235. Note that hexagonal or trigonal crystals can sometimes be rephrased as layered crystals, so the above structure can be understood as a structure in which an oxide semiconductor film 230f having cubic crystals is formed on a metal oxide layer 235 having layered crystals. That is, it can also be considered as a layered structure fabricated using heteroepitaxial growth technology or a technology like heteroepitaxial growth.

[0135] Specifically, the metal oxide layer 235 can be zinc oxide, In-Ga oxide, gallium zinc oxide (also written as Ga-Zn oxide, GZO), aluminum zinc oxide (also written as Al-Zn oxide, AZO), In-Al-Zn oxide, In-Ga-Zn oxide, or In-Sn-Zn oxide. It is preferable to use In-Ga-Zn oxide as the metal oxide layer 235. In this case, the metal oxide layer 235 contains indium, gallium, zinc, and oxygen. More specifically, it is preferable to have a composition of In:Ga:Zn = 1:1:1 [atomic ratio] or close to that, In:Ga:Zn = 1:3:2 [atomic ratio] or close to that, or In:Ga:Zn = 1:3:4 [atomic ratio] or close to that. Metal oxides with these compositions are suitable as the metal oxide layer 235 because they easily form a layered structure. In this specification, the term "nearby composition" includes a range of ±30% of the desired atomic ratio.

[0136] In-Ga-Zn oxides and In-Sn-Zn oxides, etc., tend to have a CAAC structure. When an oxide having a CAAC structure is used in the metal oxide layer 235, the c-axis of the crystal nucleus is perpendicular or approximately perpendicular to the surface or the surface on which it is formed in the metal oxide layer 235. In other words, by using an oxide that tends to have a CAAC structure in the metal oxide layer 235, the controllability of the crystal orientation of the crystal nucleus can be improved.

[0137] When an oxide that readily has a CAAC structure is used for the metal oxide layer 235, an oxide semiconductor film 230f having crystals with a crystal orientation of <111> can be formed.

[0138] The metal oxide layer 235 may be made of an insulating material or a semiconductor material. When a semiconductor material is used as the metal oxide layer 235, the metal oxide layer 235 may be considered as part of the oxide semiconductor film 230f.

[0139] In Figure 5D, etc., the metal oxide layer 235 is shown as a strip-shaped structure extending in the Y-axis direction, but the present invention is not limited to this. The metal oxide layer 235 can also be formed in an island-like shape in a plan view. When the metal oxide layer 235 is formed in an island shape, for example, in a plan view, it can be a roughly circular or elliptical shape, a triangle, a quadrilateral (including rectangles, rhombuses, and squares), a pentagon, a star polygon, or a polygon with rounded corners.

[0140] Furthermore, the metal oxide layer 235 may have a tapered shape in cross-section. For example, the angle between the upper surface of the insulating film 224f and the side surface of the metal oxide layer 235 may be less than 90°, preferably 30° or more and less than 90°. By making the metal oxide layer 235 tapered, the coverage of the oxide semiconductor film 230f is improved, and defects such as porosity can be reduced. In addition, crystal growth of the oxide semiconductor film 230f can be promoted.

[0141] It is preferable that the metal oxide layer 235 has a thin film thickness. For example, it is preferable that the film thickness of the metal oxide layer 235 is thinner than the film thickness of the oxide semiconductor film 230f. Specifically, it is preferable that the metal oxide layer 235 has a region with a film thickness of 0.1 nm or more and less than 2 nm, and more preferably has a region with a film thickness of 0.5 nm or more and less than 2 nm. By making the film thickness of the metal oxide layer 235 thin, the coverage of the oxide semiconductor film 230f is improved and defects such as porosity can be reduced. In addition, crystal growth of the oxide semiconductor film 230f can be promoted. The metal oxide layer 235 may be in the form of layers or granules.

[0142] It is preferable that the insulator 225 and the insulating film 224f have an amorphous structure. If the insulator 225 and the insulating film 224f have a polycrystalline or single-crystal structure, when forming the oxide semiconductor film 230f, the oxide semiconductor film 230f may crystallize, reflecting the crystal structure of the insulator 225 and the insulating film 224f, and there is a risk that a polycrystalline structure with small crystal grains will be formed. Therefore, by having an amorphous structure for the insulator 225 and the insulating film 224f, it is possible to suppress unintended crystallization of the oxide semiconductor film 230f and obtain an oxide semiconductor film 230f with large crystal grains.

[0143] It is preferable that the side surfaces of the insulator 225 and the upper surface of the insulating film 224f, which are the surfaces on which the oxide semiconductor film 230f is formed, are flat. This configuration suppresses nucleation caused by irregularities on the side surfaces of the insulator 225 and the upper surface of the insulating film 224f, thereby promoting crystal growth of the oxide semiconductor film 230f.

[0144] The insulator 225 and the insulating film 224f preferably have an oxygen supply function. This allows oxygen to be supplied to the oxide semiconductor film 230f, thereby reducing oxygen deficiency. An insulator having an oxygen supply function is, for example, an insulator that has a region containing oxygen that is desorbed by heating (hereinafter sometimes referred to as excess oxygen). In the semiconductor device manufacturing process, oxygen can be supplied from the insulator when heating is performed. Examples of insulators having an oxygen supply function include silicon oxide or silicon oxynitride.

[0145] Furthermore, it is preferable that the insulator 225 and the insulating film 224f have barrier properties against oxygen. This suppresses the detachment of oxygen from the oxide semiconductor film 230f and the formation of oxygen vacancies. Examples of insulators with barrier properties against oxygen include gallium oxide or aluminum oxide.

[0146] It is particularly preferable to use gallium oxide as the insulator 225 and the insulating film 224f. Compared to aluminum, the ionic radius of gallium is close to that of indium. Therefore, when indium oxide is used as the oxide semiconductor film 230f, using gallium oxide as the insulator 225 and the insulating film 224f makes it possible to bring the surface density of metal atoms in the oxide semiconductor film 230f closer to that of the insulator 225 and the insulating film 224f. As a result, the frequency of bonding between the indium atoms in the oxide semiconductor film 230f and the gallium atoms in the insulator 225 and the insulating film 224f via oxygen atoms increases, and the generation of oxygen vacancies or oxygen with dangling bonds at the interface between the oxide semiconductor film 230f and the insulator 225 and the insulating film 224f can be suppressed.

[0147] Furthermore, gallium oxide or aluminum oxide, to which the metal elements contained in the oxide semiconductor film 230f have been added, can also be used as the insulator 225 and the insulating film 224f. For example, if the oxide semiconductor film 230f contains indium, gallium oxide containing indium or aluminum oxide containing indium can also be used as the insulator 225 and the insulating film 224f. In this case, the insulator 225 and the insulating film 224f contain gallium or aluminum, indium, and oxygen. Even in this case, it is possible to suppress the generation of oxygen vacancies or oxygen with dangling bonds at the interface between the oxide semiconductor film 230f and the insulator 225 and insulating film 224f. In addition, gallium atoms and aluminum atoms in oxides tend to exist in tetrahedral coordination positions, while indium atoms in oxides tend to exist in octahedral coordination positions. In other words, it is presumed that in gallium oxide containing indium and aluminum oxide containing indium, tetrahedral and octahedral coordination are mixed, resulting in low crystallinity. Therefore, by using gallium oxide containing indium or aluminum oxide containing indium for the insulator 225 and the insulating film 224f, the crystallinity of the insulator 225 and the insulating film 224f can be reduced. Furthermore, the insulator 225 and the insulating film 224f can have an amorphous structure.

[0148] In gallium oxide containing indium, the indium content is preferably 0.5% to 5%, and more preferably 0.5% to 2%. This allows the insulating properties of the insulator 225 and the insulating film 224f to be maintained. Similarly, in aluminum oxide containing indium, the indium content is preferably 0.5% to 5%, and more preferably 0.5% to 2%.

[0149] Furthermore, it is preferable that the insulating film 224f functions as an etching stopper when the insulator 225 is processed by etching or other methods. In other words, it is preferable to use a material for the insulating film 224f that has a suitable etching selectivity ratio with respect to the insulator 225. For example, if gallium oxide is used for the insulator 225, silicon oxide can be used for the insulating film 224f.

[0150] Furthermore, while Figure 5D and others show a configuration in which the insulating film 224f and the insulator 225 are formed from different insulating films, the present invention is not limited to this. The insulating film 224f and the insulator 225 may also be integrally molded from an insulating film.

[0151] Furthermore, the insulator 225 and the insulating film 224f are not limited to those described above, and any insulating material listed in the section "<<Insulator>>" described later may be used.

[0152] Figure 5D shows an example where the insulating film 224f has a single-layer structure. However, the insulating film 224f can also have a multilayer structure of two or more layers. When the insulating film 224f has a multilayer structure of two or more layers, it is preferable to use an insulating material (typically silicon oxide) applicable to the insulating film 224f as the layer in contact with the oxide semiconductor film 230f among the two or more layers included in the insulating film 224f. This configuration improves the crystallinity of the oxide semiconductor film 230f.

[0153] Next, an example of a method for fabricating the oxide semiconductor film 230f will be described using Figures 5A to 5D.

[0154] The layers constituting the semiconductor device (insulating film 224f, metal oxide layer 235, oxide semiconductor film 230f, etc.) can be formed using sputtering, chemical vapor deposition (CVD), vacuum deposition, pulsed laser deposition (PLD), or ALD.

[0155] Unlike film deposition methods in which particles emitted from a target or other source are deposited, the ALD method is a film deposition method in which a film is formed by a reaction on the surface of the workpiece. Therefore, it is less affected by the shape of the workpiece and is a film deposition method that has good stepped coverage. In particular, the ALD method has excellent stepped coverage and excellent thickness uniformity, making it suitable for coating the surface of openings or grooves with a high aspect ratio.

[0156] Furthermore, precursors used in the ALD method may contain elements such as carbon or chlorine. Therefore, films formed by the ALD method may contain higher levels of carbon or chlorine compared to films formed by other deposition methods. These elements can be quantified using XPS or SIMS. Additionally, when using the ALD method, applying either or both of the following conditions—using a high substrate temperature during deposition and / or impurity removal—may result in lower levels of carbon and chlorine in the film compared to using the ALD method without these conditions.

[0157] Examples of ALD methods include thermal ALD, which carries out the reaction of the precursor and reactant using only thermal energy, and plasma-enhanced ALD (PEALD), which uses a plasma-excited reactant.

[0158] A film deposition apparatus using the ALD method alternately introduces a first raw material gas (sometimes called a precursor, metal precursor) and a second raw material gas (sometimes called a reactant, reactant, oxidizer, or nonmetal precursor) into the chamber, and performs film deposition by repeatedly introducing these raw material gases. The switching of the raw material gases can be done, for example, by switching the respective switching valves (sometimes called high-speed valves). Also, when introducing the raw material gases, nitrogen (N) 2 An inert gas such as argon (Ar) or helium (He) may be introduced into the chamber together with the raw material gas as a carrier gas. By using a carrier gas, even if the raw material gas has low volatility or low vapor pressure, it is possible to suppress the adsorption of the raw material gas inside the piping and valves and introduce the raw material gas into the chamber. Furthermore, the uniformity of the formed film is also improved, which is preferable.

[0159] Furthermore, the ALD method allows for the deposition of films with any desired composition by using multiple different types of precursors. Alternatively, when using multiple different types of precursors, films with any desired composition can be deposited by controlling the number of cycles for each precursor.

[0160] First, a substrate (not shown) is prepared, and an insulating film 224f is formed on the substrate. The insulating film 224f has an amorphous structure, and it is preferable that the upper surface of the insulating film 224f is flat.

[0161] The insulating film 224f can be formed, for example, using a sputtering method in an oxygen-containing atmosphere. By using a sputtering method that does not require the use of hydrogen-containing molecules in the deposition gas, the hydrogen concentration in the insulating film 224f can be reduced. Furthermore, by forming the insulating film 224f using a sputtering method in an oxygen-containing atmosphere, oxygen can be added to the insulating film 224f. Heat applied after the formation of the oxide semiconductor film 230f can supply oxygen from the insulating film 224f to the oxide semiconductor film 230f, thereby reducing oxygen deficiency.

[0162] It is preferable to perform a heat treatment before forming the insulator 225 and the metal oxide layer 235. The heat treatment is performed, for example, at a temperature of 250°C to 650°C, preferably 300°C to 500°C, and more preferably 320°C to 450°C.

[0163] The heat treatment is carried out in an atmosphere of nitrogen gas or an inert gas, or in an atmosphere containing 10 ppm (0.001%) or more, 1% or more, or 10% or more of an oxidizing gas. For example, when heat treatment is carried out in a mixed atmosphere of nitrogen gas and oxygen gas, it is preferable to have about 20% oxygen gas. The heat treatment may also be carried out under reduced pressure. Alternatively, after heat treatment in an atmosphere of nitrogen gas or an inert gas, heat treatment may be carried out in an atmosphere containing 10 ppm or more, 1% or more, or 10% or more of an oxidizing gas to replenish the desorbed oxygen. By performing the above heat treatment, impurities such as hydrogen or water contained in the insulating film 224f, insulator 225, etc., can be reduced before the deposition of the oxide semiconductor film 230f.

[0164] Furthermore, it is preferable that the gas used in the above heat treatment is highly purified. For example, the amount of water contained in the gas used in the above heat treatment should be 1 ppb (1 × 10⁻¹⁶). −3 Preferably less than ppm, and 0.1 ppb (1 × 10⁻¹⁰ −4 It is more preferable to have a ppm of 0.05 ppb (5 × 10) or less, and 0.05 ppb (5 × 10) −5A concentration of ppm or less is even more preferable. By performing the heat treatment using a highly purified gas, it is possible to prevent moisture and other substances from being incorporated into the insulating film 224f as much as possible.

[0165] There are no special limitations on the heating device used for heat treatment; it may be a device that heats the workpiece by heat conduction or thermal radiation from a heating element such as a resistance heating element. For example, an electric furnace or an RTA (Rapid Thermal Anneal) device such as an LRTA (Lamp Rapid Thermal Anneal) device or a GRTA (Gas Rapid Thermal Anneal) device can be used. An LRTA device heats the workpiece by radiation of light (electromagnetic waves) emitted from a lamp such as a halogen lamp, metal halide lamp, xenon arc lamp, carbon arc lamp, high-pressure sodium lamp, or high-pressure mercury lamp. A GRTA device is a device that performs heat treatment using high-temperature gas.

[0166] Furthermore, it is preferable to perform an oxygen supply treatment before forming the metal oxide layer 235. This supplies oxygen to the insulating film 224f, and the heat applied after the formation of the oxide semiconductor film 230f can supply oxygen from the insulating film 224f to the oxide semiconductor film 230f.

[0167] Examples of oxygen supply processes include heating in an oxygen-containing atmosphere or plasma treatment in an oxygen-containing atmosphere. Note that the plasma treatment described herein includes microwave plasma treatment, which will be discussed later. Alternatively, oxygen may be supplied to the insulating film 224f by depositing an oxide film (preferably a metal oxide film) in an oxygen-containing atmosphere using, for example, a sputtering method. The deposited oxide film may be removed immediately or left as is. If the deposited oxide film is left as is, it can be used as part of the oxide semiconductor film 230f. Note that the oxygen-containing atmosphere may include oxygen gas (O2). 2 ) as well as ozone (O 3 ) or nitrous oxide (N 2The atmosphere includes a gas containing oxygen-containing compounds such as O). Furthermore, the substrate temperature during plasma treatment shall be between room temperature (25°C) and 450°C.

[0168] Furthermore, the insulating film 224f may be subjected to a hydrogen addition treatment. For example, the hydrogen addition treatment may be performed after the insulating film 224f has been formed. The hydrogen addition treatment can be carried out using an ion implanter, an ion doping device, or a plasma treatment device. Alternatively, as a hydrogen addition treatment, microwave plasma treatment can be performed in a hydrogen-containing atmosphere. This adds hydrogen to the surface of the insulating film 224f, thereby suppressing nucleation near the insulating film 224f.

[0169] Next, an insulator 225 and a metal oxide layer 235 are formed on the insulating film 224f (see Figure 5A). The metal oxide layer 235 serves as a nucleus for crystal growth of the oxide semiconductor film 230f.

[0170] First, an insulating film that will become the insulator 225 is deposited on the insulating film 224f. Any insulating material suitable for the insulator 225 described above can be used as the insulating film for the insulator 225. The insulating film for the insulator 225 can be deposited using, for example, sputtering, CVD, MBE, PLD, or ALD. For example, gallium oxide can be deposited as the insulating film for the insulator 225 using the sputtering method.

[0171] Next, the insulating film that will become the insulator 225 is processed to form a plurality of insulators 225 arranged in the Y-axis direction. As shown in Figure 5A, it is preferable to process the insulators 225 into island-like structures extending in the X-axis direction. The insulating film that will become the insulator 225 can be processed using lithography. For this processing, dry etching or wet etching can be used. Dry etching is suitable for microfabrication.

[0172] Next, a metal oxide film is formed to cover the multiple insulators 225 and become the metal oxide layer 235. Any metal oxide material suitable for the metal oxide layer 235 described above can be used as the metal oxide film for the metal oxide layer 235. The metal oxide film for the metal oxide layer 235 can be formed using, for example, sputtering, CVD, MBE, PLD, or ALD. For the method of forming the metal oxide film for the metal oxide layer 235, refer to the method for forming the oxide semiconductor film 230f described later.

[0173] Here, it is preferable to perform a treatment to enhance the crystallinity of the metal oxide film that will become the metal oxide layer 235. Oxides with a cubic crystal structure (typically indium oxide) are presumed to grow crystals while maximizing the surface area of ​​the {111} plane. In other words, they are presumed to preferentially orient themselves to the {111} plane. Therefore, by performing a treatment to enhance crystallinity, crystal grains with a crystal orientation <111> oriented in the direction normal to the surface to be formed (also called <111> oriented crystal grains) can be formed in the metal oxide film that will become the metal oxide layer 235.

[0174] Examples of treatments to enhance the crystallinity of the metal oxide film that forms the metal oxide layer 235 include heat treatment, plasma treatment, microwave treatment (including microwave plasma treatment), and light (e.g., ultraviolet light) irradiation treatment. Multiple of these treatments can be performed simultaneously or sequentially.

[0175] As a treatment to improve the crystallinity of the metal oxide film that forms the metal oxide layer 235, microwave plasma treatment is preferred, and microwave plasma treatment in an oxygen-containing atmosphere is particularly preferred.

[0176] In this specification, microwaves refer to electromagnetic waves having a frequency of 300 MHz or more and 300 GHz or less. Microwave plasma processing refers to processing using a device that has a power supply that generates high-density plasma using microwaves, for example. Microwave plasma processing can also be called microwave-excited high-density plasma processing.

[0177] Microwave plasma treatment is preferably carried out under reduced pressure, with a pressure of 10 Pa to 1000 Pa being preferred, more preferably 50 Pa to 700 Pa, and even more preferably 100 Pa to 400 Pa. The treatment temperature is preferably room temperature (25°C) to 750°C, more preferably 300°C to 500°C, and can be 400°C to 450°C.

[0178] When performing microwave plasma processing, the substrate may be heated. It is preferable that the heating temperature of the substrate be above room temperature (e.g., 25°C), 100°C or higher, 200°C or higher, 300°C or higher, or 400°C or higher, and 500°C or lower, or 450°C or lower. For example, it is preferable that the heating temperature of the substrate be above room temperature and 500°C or lower, more preferably 100°C or higher and 450°C or lower, more preferably 200°C or higher and 450°C or lower, more preferably 300°C or higher and 450°C or lower, and even more preferably 400°C or higher and 450°C or lower.

[0179] Microwave plasma treatment can be performed using, for example, oxygen gas and argon gas. For example, the oxygen flow rate ratio (O) in microwave plasma treatment. 2 / ( O 2 The value of +Ar) is preferably greater than 0% and 10% or less, preferably between 0.5% and 5%, more preferably between 0.5% and 3%, and typically 1%.

[0180] The shorter the processing time for microwave plasma treatment, the higher the productivity. For example, the processing time for microwave plasma treatment is preferably 1 minute or more and 60 minutes or less, more preferably 1 minute or more and 30 minutes or less, and even more preferably 1 minute or more and 10 minutes or less.

[0181] Next, the metal oxide film that will become the metal oxide layer 235 is processed to form a metal oxide layer 235 that is in contact with the upper and side surfaces of the insulator 225 and the upper surface of the insulating film 224f. It is preferable that the metal oxide layer 235 extends in the Y-axis direction. The metal oxide film that will become the metal oxide layer 235 can be processed using lithography. For this processing, dry etching or wet etching can be used. Dry etching is suitable for microfabrication.

[0182] The above-described microwave plasma treatment may be performed after forming the insulator 225 and the metal oxide layer 235 on the insulating film 224f.

[0183] Next, the oxide semiconductor film 230f is formed by covering the metal oxide layer 235 and the insulator 225 (see Figure 5B). Since the oxide semiconductor film 230f is formed along the metal oxide layer 235 and the insulator 225, it is preferable that it has good coverage. Therefore, it is preferable to form the oxide semiconductor film 230f using an ALD method or the like, which has good coverage. Also, since the oxide semiconductor 230 preferably has a high aspect ratio, it is preferable that the oxide semiconductor film 230f has a thin film thickness. Therefore, it is preferable to form the oxide semiconductor film 230f using an ALD method that allows for film thickness adjustment at a thin film thickness. By forming the oxide semiconductor film 230f in this way, the oxide semiconductor film 230f is formed in contact with the upper and side surfaces of the insulator 225. Note that the formation of the oxide semiconductor film 230f is not limited to this, and the above film formation method may be used as appropriate.

[0184] For the deposition of the oxide semiconductor film 230f by the ALD method, a source gas and an oxidizing agent can be used. When the source gas contains a precursor containing indium, a film containing indium and oxygen is formed as the oxide semiconductor film 230f. When the precursor contains indium, the thermal ALD method can be used as the ALD method.

[0185] Indium-containing precursors that can be used include trimethylindium, triethylindium, ethyldimethylindium, tris(1-methylethyl)indium, tris(2,2,6,6-tetramethyl-3,5-heptanedionic acid)indium, cyclopentadienylindium, indium(III) acetylacetonate, (3-(dimethylamino)propyl)dimethylindium, (diethylphosphino)dimethylindium, chlorodimethylindium, bromodimethylindium, and dimethyl(2-propanolat)indium.

[0186] Furthermore, inorganic precursors that do not contain hydrocarbons may be used as indium precursors. As inorganic precursors containing indium, halogenated indium compounds such as trifluoroindium (indium(III) fluoride), indium trichloride (indium(III) chloride), indium tribromide (indium(III) bromide), and indium triiodide (indium(III) iodide) can be used.

[0187] In the method for forming the oxide semiconductor film 230f, it is preferable to use a high-purity raw material gas with a low impurity concentration. For example, by using a precursor with a purity of 3N (99.9%) or higher, more preferably 4N (99.99%) or higher, even more preferably 5N (99.999%) or higher, and 6N (99.9999%) or higher, the impurities in the oxide semiconductor film 230f can be reduced.

[0188] The gallium and aluminum content of the indium-containing precursor is preferably 1000 ppm or less, more preferably 500 ppm or less, even more preferably 100 ppm or less, even more preferably 50 ppm or less, even more preferably 10 ppm or less, and even more preferably 1 ppm or less. By using a precursor with a low gallium content, the gallium concentration in the oxide semiconductor film 230f can be reduced, thereby improving the reliability of the transistor. Furthermore, by using a precursor with a low aluminum content, the aluminum concentration in the oxide semiconductor film 230f can be reduced, thereby improving the crystallinity of the oxide semiconductor film 230f.

[0189] Furthermore, it is preferable that the raw material gas is purified by two or more distillations (also called rectification or precision distillation). Using such a raw material gas makes it easier to form metal oxide films with fewer impurities, which is preferable. Performing distillation multiple times is preferable because it further suppresses the retention of impurities in the raw material gas that originate from the starting materials used in the production of the raw material gas. However, the present invention is not limited to the above, and a raw material gas purified by a single distillation, i.e., simple distillation, may also be used. Using simple distillation is preferable because it can reduce manufacturing costs. By performing distillation one or more times, the aluminum content in the raw material gas can be set to 100 ppm or less, 1 ppm or less, or 1 ppb (0.001 ppm) or less.

[0190] As an oxidizing agent, ozone (O 3 ), oxygen (O 2 ), water (H 2 O), hydrogen peroxide (H 2 O 2) and the like can be used. Preferably, the oxidizing agent contains at least one of ozone and oxygen. By using ozone, oxygen, etc., which do not contain hydrogen, as the oxidizing agent, the amount of hydrogen mixed into the oxide semiconductor film 230f can be reduced. Furthermore, by using water, hydrogen peroxide, etc., which contain hydrogen, as the oxidizing agent, an oxide semiconductor film 230f with low crystallinity can be formed. In addition, nucleation can be suppressed or crystal nuclei other than the crystalline portion 31 can be promoted during the formation of the oxide semiconductor film 230f.

[0191] Unless otherwise specified in this specification, when ozone, oxygen, water, or hydrogen peroxide are used as oxidizing agents, these shall include not only gaseous or molecular states, but also plasma states, radical states, or ionic states.

[0192] When introducing the raw material gas into the reaction chamber, the substrate heating temperature is preferably set to a temperature corresponding to the decomposition temperature of the precursor. For example, in the case of a thermal ALD method using triethylindium as the precursor containing indium, the substrate heating temperature can be 100°C to 350°C, preferably 150°C to 300°C. When a metal oxide layer 235 is provided, the substrate heating temperature can be room temperature (25°C) to 300°C, preferably room temperature to 200°C, more preferably room temperature to 150°C. Lowering the substrate heating temperature can reduce the crystallinity of the oxide semiconductor film 230f during film formation.

[0193] Furthermore, the oxide semiconductor film 230f can also be formed using the sputtering method. Hydrogen (H) can be used as the sputtering gas. 2 It is preferable to use a gas containing ). By introducing hydrogen when forming the oxide semiconductor film 230f using the sputtering method, it is possible to form an oxide semiconductor film 230f with low crystallinity, for example, an oxide semiconductor film 230f with an amorphous structure. Furthermore, nucleation can be suppressed or crystal nuclei other than the crystalline portion 31 can be promoted during the formation of the oxide semiconductor film 230f. As the sputtering gas, hydrogen, noble gas (typically argon), and oxygen (O) are preferred. 2 A mixed gas of the following can be used.

[0194] Furthermore, a sputtering gas that does not contain hydrogen may be used. As the sputtering gas, for example, a noble gas or oxygen as a single gas, or a mixture of a noble gas and oxygen, may be used.

[0195] Furthermore, when forming an oxide semiconductor film 230f using the sputtering method, the substrate temperature during film formation of the oxide semiconductor film 230f is preferably between room temperature (25°C) and 250°C, more preferably between room temperature and 200°C, and even more preferably between room temperature and 140°C. For example, setting the substrate temperature to between room temperature and 140°C is preferable because it increases productivity. It is also preferable because it suppresses nucleation. Alternatively, the oxide semiconductor film 230f can be formed at room temperature or without heating the substrate.

[0196] When the oxide semiconductor film 230f has a multilayer structure, the oxide semiconductor film 230f can also be formed using, for example, sputtering and ALD methods. For example, when the oxide semiconductor film 230f has a two-layer structure consisting of a first semiconductor layer and a second semiconductor layer on the first semiconductor layer, the first semiconductor layer can be formed by the ALD method and the second semiconductor layer by the sputtering method. Since the ALD method is a film formation method with superior coverage compared to the sputtering method, the coverage of the oxide semiconductor film 230f can be improved by forming the first semiconductor layer by the ALD method. In addition, damage to the substrate (in this case, the insulating film 224f) can be reduced, the formation of a mixed layer at the interface between the substrate and the oxide semiconductor film 230f can be suppressed, and the crystallinity can be increased. Furthermore, productivity can be increased by forming the second semiconductor layer by the sputtering method.

[0197] Alternatively, the first semiconductor layer may be deposited by sputtering and the second semiconductor layer by ALD. Even if pinholes or stepped defects are formed in the first semiconductor layer deposited by sputtering, the overlapping portions can be covered with the second semiconductor layer deposited by the ALD method, which has good coverage.

[0198] Furthermore, as shown in Figure 8A, when the oxide semiconductor 230 is made into a stacked structure of oxide semiconductors 230a to 230c, the above methods can be appropriately used to form each film. For example, the film that will become oxide semiconductor 230a and the film that will become oxide semiconductor 230c can be formed using the ALD method, and the film that will become oxide semiconductor 230b can be formed using the sputtering method. Alternatively, for example, the film that will become oxide semiconductor 230a and the film that will become oxide semiconductor 230c can be formed using the sputtering method, and the film that will become oxide semiconductor 230b can be formed using the ALD method. Alternatively, for example, the film that will become oxide semiconductor 230a can be formed using the sputtering method, and the film that will become oxide semiconductor 230b and the film that will become oxide semiconductor 230c can be formed using the ALD method.

[0199] Next, it is preferable to perform a heat treatment. This heat treatment can be performed, for example, at a temperature of 250°C to 650°C, preferably 300°C to 500°C, and more preferably 320°C to 450°C. By performing this heat treatment, crystal growth can be promoted from the metal oxide layer 235, and crystal grains can be formed in the oxide semiconductor film 230f. Furthermore, the crystal grains in the oxide semiconductor film 230f can be enlarged. Therefore, a crystalline oxide semiconductor film 230f can be formed. In addition, by performing the heat treatment, excess hydrogen in the oxide semiconductor film 230f can be reduced.

[0200] By performing heat treatment, epitaxial growth and lateral growth of crystal grains of the oxide semiconductor film 230f proceed with the metal oxide layer 235 as a nucleus, thereby increasing the crystallinity of the oxide semiconductor film 230f (see Figure 5C). As a result, crystal grains grow along the insulator 225, the metal oxide layer 235, and the insulating film 224f. This growth of crystal grains can be called lateral growth. Here, as shown in Figure 5C, crystals grow laterally in the X-axis direction with the metal oxide layer 235 as a nucleus, and region 231c expands. Region 231c is a region with higher crystallinity than region 231a. As the processing time progresses, region 231c expands further along the surface of the substrate.

[0201] The crystal growth described above occurs similarly both near the upper surface of the insulator 225 parallel to the substrate surface and near the side surface of the insulator 225 perpendicular to the substrate surface. In other words, regardless of the surface of the oxide semiconductor film 230f being formed, crystal grains grow laterally in the X-axis direction, centered on the strip-shaped metal oxide layer 235. As a result, regions 231c with similarly high crystallinity are formed in the region of the oxide semiconductor film 230f in contact with the side surface of the insulator 225, the region in contact with the upper surface of the insulator 225, and the region in contact with the upper surface of the insulating film 224f. When regions 231c spread throughout the entire oxide semiconductor film 230f, as shown in Figure 5D, the crystal orientations of the crystal grains in the region of the oxide semiconductor film 230f in contact with the side surface of the insulator 225, the region in contact with the upper surface of the insulator 225, and the region in contact with the upper surface of the insulating film 224f, with respect to the surface of formation, coincide or nearly coincide. Furthermore, the crystal orientation of each crystal grain with respect to the surface of formation becomes <111>.

[0202] Furthermore, as shown in Figure 5C, since crystal grains grow in the X-axis direction centered on the metal oxide layer 235, the crystal grains of the oxide semiconductor film 230f become elongated in the X-axis direction. Therefore, the crystal grain boundaries in the oxide semiconductor film 230f are also formed by elongation in the X-axis direction. Here, the X-axis direction in Figure 5C corresponds to the channel length direction in the transistor shown in Figure 4A. In other words, in the oxide semiconductor 230 of transistors 200_1 and 200_2, crystal grain boundaries are formed along the direction of carrier flow. This reduces the number of crystal grain boundaries that are formed to obstruct carriers. In particular, when the width of the conductor 260 of transistors 200_1 and 200_2 is sufficiently small, the channel length becomes shorter, which further reduces the number of crystal grain boundaries that are formed to obstruct carriers. Also, as described above, since crystal grains grow similarly near the top surface and near the side surface of the insulator 225, the number of crystal grain boundaries can be similarly reduced near the top surface and near the side surface of the insulator 225. By forming the oxide semiconductor 230 as described above, on-current and field-effect mobility characteristics can be improved.

[0203] The heat treatment is preferably carried out under reduced pressure. Furthermore, the gas used in the heat treatment is preferably highly purified. By performing the heat treatment using a highly purified gas, it is possible to prevent moisture and other substances from being incorporated into the oxide semiconductor film 230f as much as possible. The conditions for the heat treatment can be the same as those described above.

[0204] There are no special limitations on the heating device used for the heat treatment; it may be a device that heats the object to be treated by heat conduction or thermal radiation from a heat source such as a resistance heating element. For example, an electric furnace or an RTA device such as an LRTA device or a GRTA device can be used. An LRTA device is a device that heats the object to be treated by radiation of light (electromagnetic waves) emitted from a lamp such as a halogen lamp, metal halide lamp, xenon arc lamp, carbon arc lamp, high-pressure sodium lamp, or high-pressure mercury lamp. A GRTA device is a device that performs heat treatment using high-temperature gas.

[0205] By using an RTA (Real-Time Attenuation) device, the heat treatment time can be shortened. The treatment time is preferably 1 minute or more and 10 minutes or less, more preferably 3 minutes or more and 10 minutes or less, and even more preferably 5 minutes or more and 10 minutes or less. When using an RTA device to shorten the heat treatment time, the heating temperature can be set to be above the strain point of the substrate. This further shortens the heat treatment time. The heating temperature is preferably 400°C or more and 750°C or less, and more preferably 450°C or more and 700°C or less.

[0206] Furthermore, the above heat treatment can be performed multiple times under different conditions. For example, the first treatment and the second treatment can be performed in this order as the heat treatment. Specifically, the first treatment can be performed under reduced pressure, and the second treatment can be performed in an oxygen atmosphere using an RTA apparatus. It is also preferable that the temperature of the first treatment is lower than the temperature of the second treatment. By performing the first treatment at a relatively low temperature, crystal growth from the metal oxide layer 235 can be promoted while suppressing nucleation. In addition, the growth rate of crystal grains can be slowed down, and the formation of crystal grain boundaries can be suppressed. Furthermore, the oxygen that has been removed can be replenished by performing the second treatment. The first treatment can be performed, for example, at a temperature of 100°C to 300°C, preferably 120°C to 250°C, and more preferably 150°C to 200°C. Note that only the first treatment may be performed as the heat treatment.

[0207] Alternatively, microwave plasma treatment may be performed instead of the above heat treatment. In this case as well, it may be possible to improve the crystallinity of the oxide semiconductor film 230f. For details of microwave plasma treatment, please refer to the explanation above.

[0208] As a result, the oxide semiconductor film 230f shown in Figure 5D can be fabricated. This allows a well-crystallinity oxide semiconductor 230 to be provided on the transistor 200.

[0209] In transistors using oxide semiconductors, the electrical properties tend to fluctuate and reliability may be poor if impurities such as hydrogen and oxygen vacancies are present in the region where the channel is formed in the oxide semiconductor. Furthermore, hydrogen near oxygen vacancies can cause V O H can be formed, generating electrons that act as carriers. Therefore, if oxygen vacancies and hydrogen are present in the channel formation region of an oxide semiconductor, the transistor is likely to exhibit normally-on characteristics (a characteristic in which a channel exists and current flows through the transistor even without applying voltage to the gate electrode). Consequently, in the channel formation region of an oxide semiconductor, impurities, oxygen vacancies, and V are present. OIt is preferable that H is reduced as much as possible. In other words, it is preferable that the channel-forming region in the oxide semiconductor has a reduced carrier concentration and is i-type (intrinsic) or substantially i-type.

[0210] In contrast, by placing an insulator containing excess oxygen near the oxide semiconductor and performing heat treatment, oxygen is supplied from the insulator to the oxide semiconductor, eliminating oxygen deficiencies and V O H can be reduced. Furthermore, an insulator having a barrier property against hydrogen is formed near the transistor 200, and V in the channel formation region of the oxide semiconductor 230 and its vicinity is reduced. O It is preferable to reduce H.

[0211] Preferably, at least one of insulators 215, 221, 222, 275, 282, and 283 functions as a barrier insulator against hydrogen. Furthermore, preferably at least one of insulators 215, 221, 222, 275, 282, and 283 functions as a barrier insulator against impurities. Also, preferably at least one of insulators 215, 221, 222, 275, 282, and 283 functions as a barrier insulator against oxygen. Note that it is not necessarily required to provide all of insulators 215, 221, 222, 275, 282, and 283. If sufficient barrier properties are provided against hydrogen, impurities, oxygen, etc., the insulator can be appropriately selected from insulators 215, 221, 222, 275, 282, and 283 to form the insulator.

[0212] In this specification, a barrier insulator refers to an insulator that possesses barrier properties. Furthermore, in this specification, "having barrier properties" means having the property of making it difficult for the corresponding substance to diffuse (also referred to as the property of making it difficult for the corresponding substance to permeate, the property of having low permeability to the corresponding substance, or the function of suppressing the diffusion of the corresponding substance). Alternatively, it refers to having the function of capturing or fixing the corresponding substance within the insulator (also called gettering). When hydrogen is described as a corresponding substance, it refers to, for example, hydrogen atoms, hydrogen molecules, and water molecules and OH groups. − This refers to at least one substance that is bonded with hydrogen, such as [substance name]. Furthermore, when an impurity is listed as a corresponding substance, unless otherwise specified, it refers to an impurity in the channel-forming region or semiconductor layer, such as a hydrogen atom, hydrogen molecule, water molecule, nitrogen atom, nitrogen molecule, nitrogen oxide molecule (N 2 O, NO, NO 2 It refers to at least one substance, such as a copper atom. Furthermore, when oxygen is listed as a corresponding substance, it refers to at least one substance, such as an oxygen atom or an oxygen molecule.

[0213] As an insulator that has the function of suppressing hydrogen diffusion, it is preferable to use, for example, silicon nitride or silicon nitride oxide. In addition, for example, aluminum oxide, magnesium oxide, hafnium oxide, zirconium oxide, oxides containing aluminum and hafnium (hafnium aluminate), oxides containing hafnium and zirconium (hafnium zirconium oxide), gallium oxide, indium gallium zinc oxide, etc. may also be used.

[0214] In this specification, "oxide nitride" refers to a material in which the oxygen content is greater than the nitrogen content, and "nitride oxide" refers to a material in which the nitrogen content is greater than the oxygen content. For example, when "silicon oxynitride" is written, it refers to a material in which the oxygen content is greater than the nitrogen content, and when "silicon nitride oxide" is written, it refers to a material in which the nitrogen content is greater than the oxygen content.

[0215] It is preferable to use insulators 221, 275, and 283 that have a function of suppressing hydrogen diffusion. For example, silicon nitride with higher hydrogen barrier properties may be used for insulators 221, 275, and 283.

[0216] As an insulator having the function of capturing or fixing hydrogen, it is preferable to use metal oxides such as hafnium oxide, aluminum oxide, aluminum and hafnium oxide (hafnium aluminate), or magnesium oxide. The insulator having the function of capturing or fixing hydrogen preferably has an amorphous structure. In metal oxides having such an amorphous structure, oxygen atoms have dangling bonds, and these dangling bonds may have the property of capturing or fixing hydrogen. In other words, metal oxides having an amorphous structure can be said to have a high ability to capture or fix hydrogen. By adding silicon to the above metal oxide, polycrystallization can be suppressed and it can be made more amorphous. Therefore, it is preferable to use metal oxides to which silicon has been added (for example, hafnium silicate, aluminum silicate, etc.).

[0217] It is preferable to use insulators 222 and 282 that have the function of capturing or fixing hydrogen. For example, aluminum oxide may be used for insulator 282. Also, for example, it is preferable to use hafnium oxide for insulator 222.

[0218] Furthermore, the inorganic insulators listed as having the function of suppressing hydrogen diffusion, and those having the function of capturing or fixing hydrogen, also possess barrier properties against oxygen.

[0219] Furthermore, as shown in Figure 1D, it is preferable to provide an insulator 221 having the function of suppressing hydrogen diffusion and an insulator 222 having the function of capturing or fixing hydrogen below the transistor 200. By providing the insulator 221 below the transistor 200, the diffusion of hydrogen from the lower layer of the transistor 200 can be suppressed. Also, by providing the insulator 222 on top of the insulator 221, hydrogen contained in the insulator 224 and the like can be captured or fixed to the insulator 222. This makes it possible to reduce the hydrogen concentration in the oxide semiconductor 230 and its vicinity.

[0220] Furthermore, as shown in Figure 1D, it is preferable to provide an insulator 275 to cover the oxide semiconductor 230, conductor 242a, conductor 242b, etc. By providing the insulator 275 in this way, it is possible to suppress the diffusion of hydrogen from the insulator 280 to the oxide semiconductor 230, conductor 242a, conductor 242b, etc.

[0221] Furthermore, as shown in Figure 1D, it is preferable to provide an insulator 282 having the function of capturing or fixing hydrogen, and an insulator 283 having the function of suppressing hydrogen diffusion, on top of the transistor 200. By providing the insulator 283 on top of the transistor 200, the diffusion of hydrogen from the upper layer of the transistor 200 can be suppressed. Also, by providing the insulator 282 below the insulator 283, hydrogen contained in the insulator 280 and the like can be captured or fixed to the insulator 282. This makes it possible to reduce the hydrogen concentration in the oxide semiconductor 230 and its vicinity.

[0222] Furthermore, the insulator 215 provided below the transistor 200 may have the same configuration as either one or both of the insulators 282 and 283. In this case, the insulator 215 may have a laminated structure of insulators 282 and 283, and may be configured with insulator 282 at the bottom and insulator 283 at the top, or with insulator 282 at the top and insulator 283 at the bottom.

[0223] In this way, by surrounding the top and bottom of the transistor 200 with a barrier insulator against hydrogen, the diffusion of hydrogen into the oxide semiconductor is reduced, and the V in the channel formation region is reduced. O This allows for a reduction in H. This, in turn, improves the electrical characteristics and reliability of transistor 200.

[0224] Furthermore, it is preferable to include oxygen that is desorbed by heating in the insulator 280. By supplying this oxygen to the oxide semiconductor 230 via the insulator 250 through the heat treatment, oxygen vacancies in the channel formation region can be reduced. Similarly, it is preferable to include oxygen that is desorbed by heating in the insulator 224. This allows oxygen to be supplied from the insulator 224 to the oxide semiconductor 230, further reducing oxygen vacancies in the channel formation region.

[0225] In this embodiment, oxygen can be added to the insulator 280 by forming the insulator 282 using a sputtering method in an atmosphere containing oxygen gas.

[0226] As described above, by heat-treating the insulator 280, which contains oxygen that is desorbed by heating, oxygen can be supplied to the oxide semiconductor 230 via the insulator 250. In this heat-treating process, since insulators 282 and 283, which have barrier properties against oxygen, are formed on the insulator 280, it is possible to prevent excessive diffusion of oxygen contained in the insulator 280 from the insulator 280.

[0227] If an excessive amount of oxygen is supplied to the source or drain region, it may cause a decrease in the on-current or field-effect mobility of the transistor 200. Furthermore, variations in the amount of oxygen supplied to the source or drain region within the substrate surface can lead to variations in the characteristics of the semiconductor device containing the transistor. In addition, if the amount of oxygen supplied from the insulator to the oxide semiconductor becomes excessively large, it may adversely affect the electrical characteristics and reliability of the transistor. Moreover, oxygen may diffuse into conductors such as the gate electrode, source electrode, and drain electrode, causing oxidation of these conductors and impairing their conductivity.

[0228] In contrast, since an insulator 275 having barrier properties against oxygen is formed between the insulator 280 and the oxide semiconductor 230, conductor 242a, and conductor 242b, it is possible to prevent oxygen contained in the insulator 280 from excessively diffusing into the oxide semiconductor 230, conductor 242a, and conductor 242b.

[0229] Here, it is preferable that the insulator 250 is configured to diffuse oxygen from the insulator 280 to the oxide semiconductor 230 and to suppress oxidation of the conductors 242a, 242b, and 260.

[0230] As shown in Figures 1B and 1D, the insulator 250 is placed within the opening 201 formed in the insulators 280 and 275. Within the opening 201, the insulator 250 is formed in contact with the upper surface of the insulator 222, the side surface of the insulator 224, the side surface and upper surface of the oxide semiconductor 230, the side surface of the conductor 242a1, the side surface of the conductor 242b1, and the side surface of the insulator 255.

[0231] Here, as shown in Figure 2A, it is preferable that the insulator 250 has a laminated structure consisting of an insulator 250a in contact with the oxide semiconductor 230, an insulator 250b on the insulator 250a, an insulator 250c on the insulator 250b, and an insulator 250d on the insulator 250c.

[0232] It is preferable to use silicon oxide or silicon oxynitride, which have a high dielectric strength, for the insulator 250b. Furthermore, in order to improve the dielectric strength, the film thickness of insulator 250b may be greater than that of insulators 250a and 250d. By using such an oxide insulator, oxygen can be diffused in insulator 250b by performing a high-temperature heat treatment. Therefore, by performing the heat treatment, oxygen contained in insulator 280 can be supplied to the oxide semiconductor 230 via insulator 250b.

[0233] To suppress excessive oxidation of conductors 242a1, 242b1, and 260, it is preferable to provide oxygen barrier insulators near each of them. For example, it is preferable that insulators 250a and 250d are made of insulating materials that have oxygen barrier properties.

[0234] The insulator 250a preferably has barrier properties against oxygen. Preferably, the insulator 250a is less permeable to oxygen than at least the insulator 250b. The insulator 250a has regions that are in contact with the side surfaces of the conductor 242a1 and the conductor 242b1. The oxygen barrier properties of the insulator 250a suppress the excessive oxidation of the side surfaces of the conductor 242a1 and the conductor 242b1, and the formation of an oxide film on those side surfaces. This suppresses a decrease in the on-current of the transistor 200 or a decrease in the field-effect mobility. Furthermore, with this configuration, the amount of oxygen in the insulator 250b absorbed by the conductor 242a1 and the conductor 242b1 can be reduced. Therefore, an appropriate amount of oxygen can be supplied from the insulator 250b to the oxide semiconductor 230, and oxygen deficiencies in the channel formation region of the oxide semiconductor 230 can be reduced.

[0235] Furthermore, by providing an insulator 250a between the insulator 280 and the insulator 250b, and between the insulator 250b and the oxide semiconductor 230, it is possible to suppress the excessive supply of oxygen from the insulator 280 to the oxide semiconductor 230 and supply an appropriate amount of oxygen to the oxide semiconductor 230. Therefore, the amount of oxygen in the channel formation region of the oxide semiconductor 230 and its vicinity can be controlled to an appropriate amount, thereby preventing excessive positive shift of the transistor 200 and improving reliability. In addition, it is possible to suppress excessive oxidation of the source region and drain region, which can cause a decrease in the on-current of the transistor 200 or a decrease in the field-effect mobility.

[0236] Therefore, it is preferable that the insulator 250a has a film thickness that does not excessively hinder the diffusion of oxygen from the insulator 280 to the insulator 250b, and from the insulator 250b to the oxide semiconductor 230. For example, the film thickness of the insulator 250a is preferably 0.1 nm or more and 5.0 nm or less, more preferably 0.5 nm or more and 5.0 nm or less, more preferably 0.5 nm or more and less than 3.0 nm, and even more preferably 0.5 nm or more and 2.0 nm or less.

[0237] As described above, it is preferable to allow for a moderate amount of oxygen diffusion from the insulator 280 to the insulator 250b and from the insulator 250b to the oxide semiconductor 230, while suppressing the diffusion of oxygen from the insulator 250b to the conductors 242a1 and 242b1 as much as possible. In this embodiment of the semiconductor device, the contact area between the insulator 250a and the conductor 242a1, and the contact area between the insulator 250a and the conductor 242b1 are much smaller than the contact area between the insulator 250a and the oxide semiconductor 230. In other words, it is presumed that the amount of oxygen that diffuses from the insulator 250b to the conductors 242a1 and 242b1 via the insulator 250a is less than the amount of oxygen that diffuses from the insulator 250b to the oxide semiconductor 230 via the insulator 250a. Therefore, by controlling the amount of oxygen contained in the insulator 280 and ensuring that a suitable amount of oxygen is supplied from the insulator 280 to the insulator 250b and the oxide semiconductor 230, excessive oxidation of the conductor 242a1 and conductor 242b1 can be reduced.

[0238] The insulator 250a in contact with the channel formation region in the oxide semiconductor 230 preferably has the function of capturing or fixing hydrogen. This makes it possible to reduce the hydrogen concentration in the channel formation region of the oxide semiconductor 230. O By reducing H, the channel-forming region can be made i-type or substantially i-type.

[0239] Furthermore, it is preferable to use a high-dielectric constant (high-k) material for the insulator 250a. An example of a high-k material is an oxide containing either or both aluminum and hafnium. By using a high-k material as the insulator 250a, it becomes possible to reduce the gate potential applied during transistor operation while maintaining the physical thickness of the gate insulator. It also becomes possible to thin the equivalent oxide thickness (EOT) of the insulator that functions as a gate insulator. In this embodiment, a hafnium oxide film is used as the insulator 250a. Hafnium oxide has the function of capturing or fixing hydrogen and has barrier properties against oxygen, making it suitable for use as the insulator 250a.

[0240] It is preferable that the insulator 250d also has barrier properties against oxygen. The insulator 250d is provided between the channel-forming region of the oxide semiconductor 230 and the conductor 260, and between the insulator 280 and the conductor 260. With this configuration, it is possible to suppress the diffusion of oxygen contained in the channel-forming region of the oxide semiconductor 230 into the conductor 260, thereby preventing the formation of oxygen vacancies in the channel-forming region of the oxide semiconductor 230. Furthermore, it is possible to suppress the diffusion of oxygen contained in the oxide semiconductor 230 and the oxygen contained in the insulator 280 into the conductor 260, thereby preventing the oxidation of the conductor 260. It is preferable that the insulator 250d is at least less permeable to oxygen than the insulator 250b. It is also preferable that the insulator 250d has a function to suppress the diffusion of hydrogen. This prevents impurities such as hydrogen contained in the conductor 260 from diffusing into the oxide semiconductor 230. For example, it is preferable to use a silicon nitride film as the insulator 250d.

[0241] Furthermore, as shown in Figure 2A, it is preferable to have a structure in which an insulator 250c is provided on top of the insulator 250b. In this case, the insulator 250c can be an insulator that can be used for insulator 250a. For example, hafnium oxide can be used as the insulator 250c. By providing the insulator 250c between the insulator 250d and the insulator 250b, hydrogen contained in the insulator 250b and the like can be captured or fixed more effectively.

[0242] By adopting the above configuration, the channel formation region can be made i-type or substantially i-type, and the source and drain regions can be made n-type, thereby providing a semiconductor device with good electrical characteristics. Furthermore, with the above configuration, good electrical characteristics can be maintained even when the semiconductor device is miniaturized or highly integrated. In addition, the frequency characteristics can be improved by miniaturizing the transistor 200. Specifically, the cutoff frequency can be improved.

[0243] Insulators 250a to 250d function as part of the gate insulator. Insulators 250a to 250d are provided together with the conductor 260 in the opening formed in the insulator 280. In order to miniaturize the transistor 200, it is preferable that the film thickness of insulators 250a, 250c, and 250d be thin. The film thickness of insulators 250a, 250c, and 250d is preferably 0.1 nm to 20 nm, more preferably 0.1 nm to 10 nm, more preferably 0.5 nm to 5.0 nm, more preferably 1.0 nm to less than 5.0 nm, and even more preferably 1.0 nm to 3.0 nm. Note that insulators 250a, 250c, and 250d each only need to have a region with the above-mentioned film thickness in at least a part of it.

[0244] To make the film thickness of insulators 250a to 250d as described above, it is preferable to deposit the film using the ALD method. Furthermore, to form insulators 250a to 250d with good coverage within openings such as insulator 280, it is preferable to deposit the film using the ALD method.

[0245] In the above description, the insulator 250 has been described as having a four-layer structure of insulators 250a to 250d, but the present invention is not limited to this. The insulator 250 can have a configuration having at least one of the insulators 250a to 250d. By configuring the insulator 250 with one, two, or three layers of the insulators 250a to 250d, the manufacturing process of the semiconductor device can be simplified and productivity can be improved.

[0246] The insulator 225 is formed in contact with the upper surface of the insulator 224. As shown in Figures 2B and 3, the insulator 225 has a shape with a high aspect ratio in a cross-sectional view in the channel width direction. In the insulator 225, it is preferable that the height H of the insulator 225 is greater than the width L of the insulator 225. The height H of the insulator 225 can be 1 to 20 times the width L of the insulator 225, preferably 1.3 to 15 times, and more preferably 1.5 to 10 times. For example, the width L can be 5 nm to 100 nm, preferably 5 nm to 50 nm, and more preferably 8 nm to 30 nm. Also, for example, the height H can be 30 nm to 300 nm, preferably 50 nm to 150 nm.

[0247] Furthermore, as shown in Figure 2B, in a cross-sectional view in the channel width direction, the angle θ between the side surface of the insulator 225 and the upper surface of the insulator 224 is preferably perpendicular or nearly perpendicular. For example, the angle θ is preferably 80° or more and 100° or less, and more preferably 85° or more and 95° or less.

[0248] The metal oxide layer 235 is preferably provided in contact with the upper and side surfaces of the insulator 225, and the upper surface of the insulator 224. Furthermore, it is preferable that the metal oxide layer 235 overlaps with the conductor 242b, but does not overlap with the conductors 260 and 242a. With this structure, the laterally grown crystals of the oxide semiconductor 230 can be arranged in the region that overlaps with the conductor 260. Therefore, the number of crystal grain boundaries in the channel formation region can be reduced, thereby improving on-characteristics such as on-current and field-effect mobility. Alternatively, the metal oxide layer 235 may overlap with the conductor 240b. Also, as shown in Figure 1C, it is preferable that the side surfaces on the A3 side and the A4 side of the metal oxide layer 235 are flush with the side surfaces on the A3 side and the A4 side of the insulator 224, the oxide semiconductor 230, and the conductor 242b, respectively.

[0249] Furthermore, as shown in Figure 3, the upper part of the metal oxide layer 235 may have a curved shape. Having such a curved shape prevents the formation of defects such as pores in the oxide semiconductor 230 and the conductor 242 near the upper part of the metal oxide layer 235.

[0250] An oxide semiconductor 230 and a conductor 242 are provided covering the insulator 225 with a high aspect ratio. Near the channel formation region of the transistor 200, as shown in Figure 2B, the oxide semiconductor 230 is provided in a folded state with the insulator 225 in between, and an insulator 250 and a conductor 260 are provided covering the oxide semiconductor 230. As a result, the channel width of the transistor 200 is increased by the amount of the A1 side and the A2 side of the insulator 225.

[0251] As described above, increasing the channel width improves the on-current, field-effect mobility, and frequency characteristics of the transistor 200. This makes it possible to provide a semiconductor device with a high operating speed. Furthermore, it is possible to increase the operating speed of a memory device using this semiconductor device. In addition, in the above structure, by providing the insulator 225, the channel width can be increased without increasing the area occupied by the transistor 200. This makes it possible to miniaturize or highly integrate the semiconductor device. Furthermore, it is possible to increase the storage capacity of a memory device using this semiconductor device.

[0252] The insulator 224 has its lower surface in contact with the insulator 222, and its upper surface in contact with the insulator 225 and the oxide semiconductor 230. The planar shape of the insulator 224 is the same as that of the oxide semiconductor 230, and in plan view, the insulator 224 overlaps with the oxide semiconductor 230. In other words, in plan view, the side surface of the insulator 224 coincides with, or substantially coincides with, the side surface of the oxide semiconductor 230. Furthermore, at least a portion of the insulator 224 overlaps with the conductors 242a (conductors 242a1 and 242a2) and conductors 242b (conductors 242b1 and 242b2) in plan view. In other words, at least a portion of the side surface of the insulator 224 coincides with, or substantially coincides with, the side surface of the conductor 242a (conductor 242a1 and conductor 242a2) and the side surface of the conductor 242b (conductor 242b1 and conductor 242b2) in a plan view.

[0253] As shown in Figure 2B, it is preferable that the film thickness t1 of the insulator 224 within the opening 201 is thicker than the film thickness t2 of the insulator 250. With this configuration, the lower surface of the conductor 260 (conductor 260a) located within the opening 201 can be positioned below the lower surface of the oxide semiconductor 230 by the difference in film thickness t1 and film thickness t2 (t1-t2).

[0254] By positioning the lower surface of the conductor 260 below the lower surface of the oxide semiconductor 230, a sufficient gate electric field can be applied from the upper end to the lower end of the oxide semiconductor 230. In other words, within the opening of the insulator 280, the entire oxide semiconductor 230 can be electrically surrounded by the electric field of the conductor 260, allowing it to function as a channel-forming region. This configuration prevents the lower end of the oxide semiconductor 230 from functioning as a parasitic channel, thereby reducing the leakage current between the source electrode and the drain electrode. Furthermore, it is possible to suppress characteristic defects such as normally-on behavior of the transistor caused by the parasitic channel. In short, the electrical characteristics of the transistor 200 can be improved.

[0255] Furthermore, as described above, by making the entire region from the top to the bottom of the oxide semiconductor 230 function as a channel-forming region, the channel width can be increased. This improves the on-current, transconductance, and frequency characteristics of the transistor 200.

[0256] In this specification, the transistor structure in which the channel formation region is electrically surrounded by the electric field of the gate electrode, as described above, is called a surrounded channel (S-channel) structure. In an S-channel structure, the gate electrode is arranged to surround at least two sides of the channel (specifically, two, three, or four sides, etc.). By adopting an S-channel structure, it is possible to increase resistance to short-channel effects, or in other words, to create a transistor in which short-channel effects are less likely to occur.

[0257] Furthermore, since the S-channel structure electrically surrounds the channel formation region, it can be said that it is essentially equivalent to the GAA (Gate All Around) structure or the LGAA (Lateral Gate All Around) structure. By making the transistor 200 an S-channel structure, a GAA structure, or an LGAA structure, it is possible to improve the current density flowing through the transistor, and thus an improvement in the transistor's on-current or an increase in the transistor's field-effect mobility can be expected.

[0258] Furthermore, even if the film thickness of the oxide semiconductor 230 is reduced as described above, by creating a structure in which the oxide semiconductor 230 is provided by covering it with an insulator 225 that has a high aspect ratio, the oxide semiconductor 230 can be supported by the insulator 225. This allows the oxide semiconductor 230 to be formed extending upward relative to the substrate without tilting. Therefore, the channel width can be increased without increasing the occupied area.

[0259] Furthermore, although the above describes an example in which an insulator 224 is provided below the insulator 225, the present invention is not limited to this. As shown in Figure 6A, a configuration without an insulator 224 is also possible. In this case, the insulator 225 and the oxide semiconductor 230 are formed in contact with the upper surface of the insulator 222. Also, when processing the oxide semiconductor 230 into an island shape, or when forming the opening 201, a part of the upper surface of the insulator 222 may be removed. As a result, as shown in Figure 6A, the upper surface of the region of the insulator 222 that overlaps with the oxide semiconductor 230 may be higher than the upper surface of the region of the insulator 222 that does not overlap with the oxide semiconductor 230.

[0260] Furthermore, although the above describes an example where the side surface of the insulator 225 is located inward from the side surface of the insulator 224, the present invention is not limited to this. As shown in Figure 6B, the side surface of the insulator 225 and the side surface of the insulator 224 can also be formed to be flush. Here, the lower end of the side surface of the insulator 225 and the upper end of the side surface of the insulator 224 can coincide or substantially coincide.

[0261] Conductive materials described in the section "Conductive Materials" can be used for conductors 242a and 242b. It is preferable to use conductive materials that are not easily oxidized excessively as conductors 242a and 242b. Examples of such conductive materials include conductive oxides and conductive nitrides. By using these, it is possible to suppress excessive oxidation of conductors 242a and 242b, which would reduce the conductivity of conductors 242a and 242b.

[0262] Conductors 242a and 242b are arranged spaced apart from each other via an opening 201 and are provided in contact with the oxide semiconductor 230. Conductor 242 is provided so as to cover the insulator 225, which has a high aspect ratio, as shown in Figure 3 and other figures.

[0263] Here, near the source or drain of the transistor 200, as shown in Figure 3, the oxide semiconductor 230 and the conductor 242b are arranged so as to be folded in half with the insulator 225 in between. As a result, in a cross-sectional view in the channel width direction, the conductor 242b is in contact with the oxide semiconductor 230 at the top of the insulator 225, the side on side A3, the side on side A4, and near the insulator 224. Therefore, compared to the case where the insulator 225 is not provided, the contact area between the conductor 242b and the oxide semiconductor 230 is increased by the amount of the side on side A3 and the side A4 of the insulator 225. Note that although Figures 3 and 1C show the vicinity of the conductor 242b, the same applies to the conductor 242a. In other words, the contact area between the conductor 242a and the oxide semiconductor 230 is increased, similar to the contact area between the conductor 242b and the oxide semiconductor 230 described above.

[0264] As described above, increasing the contact area between the conductor 242 and the oxide semiconductor 230 reduces the contact resistance between the conductor 242 and the oxide semiconductor 230 without significantly increasing the area occupied by the transistor 200. Therefore, the on-current and frequency characteristics of the transistor 200 can be improved. This makes it possible to provide a semiconductor device with a high operating speed. Furthermore, the operating speed of a memory device using this semiconductor device can be increased. In addition, this makes it possible to miniaturize or highly integrate the semiconductor device. Furthermore, the storage capacity of a memory device using this semiconductor device can be increased.

[0265] As shown in Figures 1D and 2A, it is preferable to have a two-layer structure for the conductor 242a and conductor 242b. Conductor 242a is a laminated film of conductor 242a1 and conductor 242a2 on conductor 242a1, and conductor 242b is a laminated film of conductor 242b1 and conductor 242b2 on conductor 242b1. Conductors 242a1 and conductor 242b1 are provided in contact with the upper surface of the oxide semiconductor 230. Conductor 242a2 is provided in contact with a part of conductor 242a1, and conductor 242a2 is provided in contact with a part of conductor 242b1. In addition, an insulator 255 is provided in contact with another part of conductor 242a1 and another part of conductor 242b1.

[0266] It is preferable to use conductive materials that are not easily oxidized excessively as the layers (conductors 242a1 and 242b1) in contact with the oxide semiconductor 230. This suppresses excessive oxidation of conductors 242a and 242b, which reduces their conductivity. It also suppresses the extraction of oxygen from the oxide semiconductor 230, which can lead to the formation of excessive oxygen vacancies.

[0267] As conductors 242a1 and 242b1, indium tin oxide (In-Sn oxide, also known as ITO), silicon-containing ITO (In-Sn-Si oxide, also known as ITSO), indium zinc oxide (In-Zn oxide, also known as IZO®), indium titanium oxide (In-Ti oxide), ruthenium, ruthenium oxide, ruthenium nitride, oxides containing strontium and ruthenium, oxides containing lanthanum and nickel, etc., can be used. These materials are preferred because they are conductive materials that are resistant to oxidation or materials that maintain conductivity even when absorbing oxygen. Furthermore, since these materials are conductive metal oxides, the contact resistance between conductor 242a and oxide semiconductor 230, and the contact resistance between conductor 242b and oxide semiconductor 230 can be reduced. By using such a structure, the on-current of transistor 200 can be increased.

[0268] Furthermore, it is preferable to use metal nitrides as conductors 242a1 and 242b1, for example, nitrides containing tantalum, nitrides containing titanium, nitrides containing molybdenum, nitrides containing tungsten, nitrides containing titanium and aluminum, etc. For example, tantalum nitride can be used as conductors 242a1 and 242b1.

[0269] Furthermore, it is preferable that conductors 242a2 and 242b2 have higher conductivity than conductors 242a1 and 242b1. For example, it is preferable to make the film thickness of conductors 242a2 and 242b2 greater than the film thickness of conductors 242a1 and 242b1. As conductors 242a2 and 242b2, for example, conductive materials mainly composed of tungsten, copper, or aluminum can be used. By adopting the above structure, the resistance of conductors 242a2 and 242b2 can be reduced. This makes it possible to increase the on-current of transistor 200 and improve the operating speed of the semiconductor device according to this embodiment.

[0270] For example, ITO can be used as conductors 242a1 and 242b1, and tungsten can be used as conductors 242a2 and 242b2.

[0271] With the above structure, the upper surface of the oxide semiconductor 230 is exposed in the region between the conductor 242a1 and the conductor 242b1, and the insulator 250 is in contact with this region. Here, as shown in Figure 7A, the upper surface of the oxide semiconductor 230 in this region may be lower than that of other regions. In other words, in the oxide semiconductor 230, the upper surface of the region between the conductor 242a1 and the conductor 242b1 may be lower than the upper surface of the region that overlaps with the conductor 242a1 or the conductor 242b1. It is also possible that the film thickness of the oxide semiconductor 230 in the region overlapping with the insulator 250 is thinner than the film thickness of the oxide semiconductor 230 in the region overlapping with the conductor 242a1 or the conductor 242b1.

[0272] Furthermore, as described above, when the oxide semiconductor 230 is made into a stacked structure of oxide semiconductors 230a to 230c, the oxide semiconductor 230c may be divided in the region overlapping with the insulator 250, as shown in Figure 8B. In this case, a part of the upper surface of the oxide semiconductor 230b comes into contact with the insulator 250. By using such a structure, it is possible to make the structure formed only on the oxide semiconductor 230b of the transistor 200.

[0273] As shown in Figures 1B and 1D, the insulator 255 is positioned within an opening 201 formed in the insulator 280, etc., and is in contact with the side surface of the insulator 280, the side surface of the insulator 275, the side surface of the conductor 242a2, the side surface of the conductor 242b2, the top and side surfaces of the conductor 242a1, the top and side surfaces of the conductor 242b1, and the top surface of the insulator 222. In other words, it is formed in a sidewall shape within the opening 201. Furthermore, in the region within the opening 201 where the insulator 255 is not formed, the insulator 250 is in contact with the oxide semiconductor 230, the insulator 224, and the insulator 222. Although not shown in Figures 1B, etc., depending on the shape of the oxide semiconductor 230, the insulator 255 may also be formed in contact with the side surface of the oxide semiconductor 230.

[0274] The insulator 255 is formed in contact with the side surfaces of the conductor 242a2 and the conductor 242b2, and is an inorganic insulator that protects the conductor 242a2 and the conductor 242b2. Since the insulator 255 is exposed to an oxidizing atmosphere, an inorganic insulator that is resistant to oxidation is preferred. Furthermore, since the insulator 255 is in contact with the conductor 242a2 and the conductor 242b2, it is preferable that the inorganic insulator 255 is resistant to oxidation of the conductor 242a2 and the conductor 242b2. Therefore, it is preferable that the insulator 255 be an insulating material that can be used for the insulator 250d which has barrier properties against oxygen. For example, silicon nitride deposited using the PEALD method can be used as the insulator 255. However, it is not limited to this, and insulating materials described in the section "<<Insulator>>" described later can be used for the insulator 255.

[0275] By using such an insulator 255, even if heat treatment is performed in an oxygen-containing atmosphere after separating the conductor 242a1 and conductor 242b1 and before forming the insulator 250, the conductors 242a2 and 242b2 will not be excessively oxidized. For example, the thickness of the oxide film on the sides of the conductors 242a2 and 242b2 near the conductor 260 can be set to 0.5 nm or more and 5 nm or less, preferably 0.5 nm or more and 3 nm or less, and more preferably 0.5 nm or more and 2 nm or less.

[0276] Furthermore, it is preferable that the insulator 255 has a film thickness greater than any one of the insulators 250a to 250d. The film thickness of the insulator 255 is preferably 1 nm to 20 nm, more preferably 1 nm to 15 nm, and more preferably 3 nm to 10 nm. For example, the film thickness can be about 5 nm. By making the insulator 255 such a film thickness, the distance between the conductor 260 and the conductor 242a or conductor 242b can be increased, thereby reducing parasitic capacitance. It is sufficient that the insulator 255 has a region with the above-mentioned film thickness in at least a part of it. Also, since the insulator 255 is provided in an opening formed in the insulator 280, it is preferable to deposit it using a method with good coverage, such as the ALD method.

[0277] Furthermore, the insulator 255 may be a laminated structure of two or more layers using inorganic insulators. When the insulator 255 is a laminated structure of two or more layers, at least one layer should be an inorganic insulator that is resistant to oxidation as described above. For example, as shown in Figure 9A, the insulator 255 can be configured to have an insulator 255a and an insulator 255b on the insulator 255a. In this case, silicon oxide can be used as the insulator 255a and silicon nitride can be used as the insulator 255b.

[0278] Furthermore, the insulator 255 functions as part of the mask when separating the conductor 242a1 and the conductor 242b1. Therefore, as shown in Figure 2A, it is preferable that, in a cross-sectional view of the transistor 200, the inner side surface of the insulator 255 coincides with or substantially coincides with the side edge of the conductor 242a1 and the side edge of the conductor 242b1.

[0279] Here, in the conductor 242a1, the portion on which the insulator 255 is formed on the upper surface (hereinafter sometimes referred to as the protruding portion of the conductor 242a1) protrudes toward the conductor 260 side from the conductor 242a2. Similarly, in the conductor 242b1, the portion on which the insulator 255 is formed on the upper surface (hereinafter sometimes referred to as the protruding portion of the conductor 242b1) protrudes toward the conductor 260 side from the conductor 242b2. As shown in Figure 2A, in a cross-sectional view of the transistor 200 in the channel length direction, the distance D1 between the conductor 242a1 and the conductor 242b1 is smaller than the distance D2 between the conductor 242a2 and the conductor 242b2.

[0280] The distance D1 between the conductor 242a1 and the conductor 242b1 is reflected in the channel length of the transistor 200, and therefore it is preferable that it be small. For example, it is preferable that the distance D1 is 60 nm or less, 50 nm or less, 40 nm or less, 30 nm or less, 20 nm or less, or 10 nm or less, and 1 nm or more, or 5 nm or more. For example, it is more preferable that the distance D1 is between 2 nm and 20 nm. With such a configuration, it is possible to shorten the distance between the source and the drain and shorten the channel length accordingly. Therefore, the frequency characteristics of the transistor 200 can be improved. In this way, by shortening the channel length of the semiconductor device, it is possible to provide a semiconductor device with improved operating speed.

[0281] Furthermore, in the transistor 200 shown in Figure 2A, the opposing sides of conductor 242a1 and conductor 242b1, and the opposing sides of conductor 242a2 and conductor 242b2 are perpendicular or approximately perpendicular to the upper surface of the oxide semiconductor 230, but the present invention is not limited thereto. For example, as shown in Figure 9B, the opposing sides of conductor 242a1 and conductor 242b1, and the opposing sides of conductor 242a2 and conductor 242b2 may be tapered. In this case, the sides of insulator 271a, insulator 271b, insulator 275, and insulator 280 may be tapered. Note that in Figure 9B, the taper angles of insulator 280, insulator 275, insulator 271a, insulator 271b, conductor 242a2, and conductor 242b2 are equal, but the present invention is not limited thereto, and their respective taper angles may be different. For example, the taper angles of the conductors 242a1 and 242b1 may be acuter than the taper angles of the conductors 242a2 and 242b2.

[0282] Furthermore, as shown in Figure 9C, the upper part of the side surface of the insulator 255 may have a curved shape. Also, as shown in Figure 9C, the upper part of the insulator 280 may also have a curved shape that is continuous with or substantially continuous with the curved shape of the side surface of the insulator 255. Here, the insulator 250 may be in contact with the curved parts of the upper part of the insulator 255 and the upper part of the insulator 280.

[0283] In the above, an example was shown in which the conductor 242a and conductor 242b are arranged in a two-layer laminated structure. However, the present invention is not limited to this, and the conductor 242a and conductor 242b can also be arranged in a single layer or a laminated structure of three or more layers. For example, as shown in Figure 7B, the conductor 242a and conductor 242b can be arranged in a single layer structure. In this case, the conductor 242a and conductor 242b can be made of conductive materials that can be used for conductor 242a1 and conductor 242b1. In this case, as shown in Figure 7B, the insulator 255 can be omitted, and the insulator 280 and insulator 275 can be in contact with the insulator 250. Furthermore, as shown in Figure 7C, the conductor 242a and conductor 242b can be arranged in a two-layer laminated structure, similar to the structure shown in Figure 2A, without the insulator 255. In this case, it is preferable that oxidation of the sides of the conductor 242a2 and conductor 242b2 is suppressed.

[0284] Insulators 271a and 271b are inorganic insulators that function as etching stoppers during processing of conductors 242a2 and 242b2, protecting them. Furthermore, since insulator 271a is in contact with conductor 242a2 and insulator 271b is in contact with conductor 242b2, it is preferable that insulators 271a and 271b are inorganic insulators that do not easily oxidize conductors 242a2 and 242b2. Therefore, as shown in Figure 2A, it is preferable that insulator 271a has a laminated structure of insulator 271a1 and insulator 271a2 on insulator 271a1, and insulator 271b has a laminated structure of insulator 271b1 and insulator 271b2 on insulator 271b1. Here, it is preferable to use nitride insulators that can be used for insulator 250d for insulators 271a1 and 271b1 so as to prevent oxidation of conductors 242a2 and 242b2. Furthermore, it is preferable to use oxide insulators that can be used for insulator 250b for insulators 271a2 and 271b2 so as to function as etching stoppers.

[0285] Here, insulator 271a1 is in contact with the upper surface of conductor 242a2 and a part of insulator 275, and insulator 271b1 is in contact with the upper surface of conductor 242b2 and a part of insulator 275. In addition, insulator 271a2 is in contact with the upper surface of insulator 271a1 and the lower surface of insulator 275, and insulator 271b2 is in contact with the upper surface of insulator 271b1 and the lower surface of insulator 275. For example, silicon nitride can be used as insulator 271a1 and insulator 271b1, and silicon oxide can be used as insulator 271a2 and insulator 271b2.

[0286] The conductor 260 can be any conductive material as described in the section on "Conductors," similar to conductors 242a and 242b. It is preferable to use a conductive material that is not easily oxidized excessively, or a conductive material that has a function to suppress oxygen diffusion, as the conductor 260. Examples of such conductive materials include conductive materials containing nitrogen and conductive materials containing oxygen. This helps to suppress a decrease in the conductivity of the conductor 260.

[0287] As shown in Figures 1B and 1D, the conductor 260 is positioned within the opening 201 formed in the insulators 280 and 275. Within the opening 201, the conductor 260 is positioned to cover the upper surface of the insulator 222, the side surface of the oxide semiconductor 230, and the upper surface of the oxide semiconductor 230, via the insulator 250. Furthermore, the upper surface of the conductor 260 is positioned so that its height is the same as or approximately the same as the top of the insulator 255, the top of the insulator 250, and the upper surface of the insulator 280.

[0288] In addition, in the opening 201 where the conductor 260 and the insulator 250 are arranged, the side walls of the opening 201 may be perpendicular or substantially perpendicular to the upper surface of the insulator 222, or they may be tapered. By making the side walls tapered, the covering of the insulator 250 and the like provided in the opening of the insulator 280 is improved, and defects such as porosity can be reduced.

[0289] The conductor 260 functions as the gate electrode of the transistor 200. Here, it is preferable that the conductor 260 extends in the channel width direction, as shown in Figures 1A and 1B. With this configuration, when multiple transistors are provided, the conductor 260 functions as wiring.

[0290] A portion of the conductor 260 is provided in a folded state with the insulator 225 in between. As a result, as shown in Figure 2B, in a cross-sectional view in the channel width direction, the oxide semiconductor 230 and the conductor 260 are provided facing each other with the insulator 250 in between at the top of the oxide semiconductor 230, the side on the A1 side, the side on the A2 side, and near the insulator 224. In other words, the top of the oxide semiconductor 230, the side on the A1 side, the side on the A2 side, and near the insulator 224 each function as a channel-forming region. Therefore, compared to the case where the insulator 225 is not provided, the channel width of the transistor 200 is increased by the amount of the side on the A1 side and the side on the A2 side of the oxide semiconductor 230.

[0291] In Figure 2A and other figures, the conductor 260 is shown as a two-layer structure. Here, it is preferable that the conductor 260 has a conductor 260a and a conductor 260b disposed on top of the conductor 260a. For example, it is preferable that the conductor 260a is arranged to enclose the lower surface and side surfaces of the conductor 260b. In this case, it is preferable to use a conductive material that is resistant to oxidation or a conductive material that has the function of suppressing oxygen diffusion as the conductor 260a.

[0292] It is preferable to use a conductive material for the conductor 260a that has the function of suppressing the diffusion of impurities such as hydrogen atoms, hydrogen molecules, water molecules, nitrogen atoms, nitrogen molecules, nitrogen oxide molecules, and copper atoms. Alternatively, it is preferable to use a conductive material that has the function of suppressing the diffusion of oxygen (for example, at least one such as oxygen atoms and oxygen molecules).

[0293] Furthermore, because the conductor 260a has the function of suppressing oxygen diffusion, it is possible to suppress the oxidation of the conductor 260b by oxygen contained in the insulator 280 and the like, which would reduce its conductivity. As a conductive material that has the function of suppressing oxygen diffusion, it is preferable to use, for example, titanium, titanium nitride, tantalum, tantalum nitride, ruthenium, ruthenium oxide, etc.

[0294] Furthermore, it is preferable to use a highly conductive material for the conductor 260b. For example, the conductor 260b can be a conductive material mainly composed of tungsten, copper, or aluminum. The conductor 260b may also be in a laminated structure, for example, a laminated structure of titanium or titanium nitride and the above conductive material.

[0295] Furthermore, in transistor 200, the conductor 260 is formed in a self-aligning manner so as to fill the opening 201 formed in the insulator 280 or the like. Here, the side surface of the insulator 280 at the opening 201 coincides with, or nearly coincides with, the side surface of the conductor 242a2 and the side surface of the conductor 242b2. Therefore, the conductor 260 can be placed superimposed in the region between the conductor 242a2 and the conductor 242b2 without the need for alignment.

[0296] It is preferable that insulators 216, 280, and 285 each have a lower dielectric constant than insulator 222. By using a material with a low dielectric constant as the interlayer film, parasitic capacitance occurring between wiring can be reduced.

[0297] For example, it is preferable that insulators 216, 280, and 285 each contain one or more of the following: silicon oxide, silicon oxynitride, silicon oxide with added fluorine, silicon oxide with added carbon, silicon oxide with added carbon and nitrogen, and silicon oxide with voids.

[0298] In particular, silicon oxide and silicon oxide-nitride are preferred because they are thermally stable. Materials such as silicon oxide, silicon oxide-nitride, and silicon oxide with vacancies are especially preferred because they can easily form regions containing oxygen that is desorbed by heating.

[0299] Furthermore, the upper surfaces of insulator 216, insulator 280, and insulator 285 may each be flattened.

[0300] It is preferable that the concentration of impurities such as water and hydrogen in the insulator 280 is reduced. For example, it is preferable that the insulator 280 has a silicon-containing oxide such as silicon oxide or silicon oxynitride.

[0301] Conductors 240a and 240b are formed within openings in insulators 275, 280, 282, 283, and 285, respectively. These openings are also formed in insulators 271a and 271b. The lower surface of conductor 240a is in contact with the upper surface of conductor 242a, and the lower surface of conductor 240b is in contact with the upper surface of conductor 242b. Here, the height of the upper surface of conductor 240 and the height of the upper surface of insulator 283 are approximately the same.

[0302] The conductor 240 is preferably made of a conductive material mainly composed of tungsten, copper, or aluminum. Alternatively, the conductor 240 may have a laminated structure in which the first conductor is provided in contact with the side surface of the insulator 241, and the second conductor is provided further inside. In this case, the above-mentioned conductive material can be used as the second conductor. Here, the first conductor corresponds to the conductor 240b1 shown in Figure 3, and the second conductor corresponds to the conductor 240b2 shown in Figure 3.

[0303] Furthermore, when the conductor 240 has a laminated structure, it is preferable to use a conductive material that has the function of suppressing the permeation of impurities such as water and hydrogen for the first conductor arranged near the insulators 285, 283, 282, 280, and 275. For example, it is preferable to use tantalum, tantalum nitride, titanium, titanium nitride, ruthenium, ruthenium oxide, etc. The conductive material that has the function of suppressing the permeation of impurities such as water and hydrogen may be used in a single layer or a laminate. With such a configuration, it is possible to suppress the mixing of impurities such as water and hydrogen contained in the layer above the insulator 285 into the oxide semiconductor 230 through the conductors 240a and 240b.

[0304] Insulators 241a and 241b are formed in contact with the inner walls of the openings of insulators 275, 280, 282, 283, and 285, respectively. Also, as shown in Figure 3, insulator 241b is formed in contact with the inner walls of the openings of insulators 271b1 and 271b2. Similarly, insulator 241a is formed in contact with the inner walls of the openings of insulators 271a1 and 271a2. The inner side surface of insulator 241a is in contact with conductor 240a, and the inner side surface of insulator 241b is in contact with conductor 240b.

[0305] As the insulator 241, a barrier insulating film that can be used for the insulator 275 and the like may be used. For example, as the insulator 241, an insulator such as silicon nitride, aluminum oxide, or silicon oxide nitride may be used. By providing the insulator 241, it is possible to suppress the mixing of impurities such as water and hydrogen contained in the insulator 280, etc., into the oxide semiconductor 230 through the conductors 240a and 240b. Silicon nitride is particularly suitable because it has high barrier properties against hydrogen. In addition, it is possible to prevent oxygen contained in the insulator 280 from being absorbed by the conductors 240a and 240b.

[0306] When the insulator 241 is made into a laminated structure, it is preferable to use a combination of an oxygen barrier insulating film and a hydrogen barrier insulating film for the first insulator in contact with the inner wall of the opening such as the insulator 280 and the second insulator inside it. For example, aluminum oxide deposited by the thermal ALD method may be used as the first insulator, and silicon nitride deposited by the PEALD method may be used as the second insulator. By using such a configuration, oxidation of the conductor 240 can be suppressed, and furthermore, the contamination of the conductor 240 with hydrogen can be reduced.

[0307] Although the above describes a configuration in which the insulator 241 has a two-layer laminated structure, the present invention is not limited thereto. For example, the insulator 241 may be provided as a single layer or as a laminated structure of three or more layers. Similarly, although the above describes a configuration in which the conductor 240 has a two-layer laminated structure, the present invention is not limited thereto. For example, the conductor 240 may be provided as a single layer or as a laminated structure of three or more layers.

[0308] Although Figure 3 and other figures show a configuration in which the conductor 240b is mainly in contact with the upper surface of the conductor 242b2, the present invention is not limited to this. The conductor 240b may also be configured to cover the sides of the conductor 242b2, the conductor 242b1, the oxide semiconductor 230, and the insulator 224. By using such a configuration, the contact area between the conductor 240b and the conductor 242b can be increased. In addition, although the above description has focused on the conductor 240b, the same applies to the conductor 240a.

[0309] As described above, increasing the contact area between conductor 240 and conductor 242 reduces the contact resistance between conductor 240 and conductor 242. This allows for improved on-current and frequency characteristics of transistor 200 without significantly increasing the area occupied by transistor 200. This enables the provision of a semiconductor device with a high operating speed. Furthermore, it enables the operation speed of a memory device using this semiconductor device. Additionally, it allows for miniaturization or high integration of the semiconductor device. Furthermore, it enables the storage capacity of a memory device using this semiconductor device.

[0310] In the above, as shown in Figure 1A, the shape of the opening for providing the conductor 240 and the insulator 241 is a rectangle in plan view, but it is not limited to this. For example, the opening may be circular, an ellipse or other approximate circular shape, a rectangle or other polygon, or a rectangle or other polygon with rounded corners in plan view. Also, the opening is formed to overlap with the oxide semiconductor 230 and the insulator 225, but it is not limited to this, and it is sufficient that it is formed to overlap with at least the conductor 242a or the conductor 242b.

[0311] In Figures 1A to 1D, the insulator 224 is provided only in the region overlapping with the oxide semiconductor 230, but the present invention is not limited to this. For example, as shown in Figures 10A to 10D, the insulator 224 may be provided not only in the region overlapping with the oxide semiconductor 230 but also outside the opening 201. Here, Figures 10A to 10D correspond to Figures 1A to 1D, respectively, so for detailed configurations, please refer to the above description.

[0312] In one embodiment of the present invention, the shape of the insulator 224 in a plan view and the shape of the oxide semiconductor 230 in a plan view should be made to match or substantially match within the opening 201. In other words, it is preferable that the opening 201 reaches the oxide semiconductor 230, and in the vicinity of the oxide semiconductor 230, it reaches the insulator 222. In this case, as shown in Figures 10B to 10D, the insulator 224 is provided between the insulator 222 and the insulator 275.

[0313] Furthermore, although Figures 1A to 1D show that one insulator 225 is provided on the transistor 200, the present invention is not limited to this, and a configuration in which multiple insulators 225 are provided on a single transistor 200 is also possible. For example, as shown in Figures 11A to 11D, an insulator 225a and an insulator 225b are arranged in the A1-A2 direction, and an oxide semiconductor 230 is provided covering the insulators 225a and 225b. As shown in Figures 11A and 11C, the metal oxide layer 235 extends in the A1-A2 direction and is therefore in contact with the upper and side surfaces of the insulator 225a and the upper and side surfaces of the insulator 225b. Note that Figures 11A to 11D correspond to Figures 1A to 1D, respectively, so for detailed configurations, please refer to the above description.

[0314] As shown in Figure 11B, by providing insulators 225a and 225b, the area in which the oxide semiconductor 230 and the conductor 260 face each other across the insulator 250 can be increased compared to the case where only one insulator 225 is provided. This makes it possible to increase the channel width per unit area. Also, as shown in Figure 11C, by providing insulators 225a and 225b, the contact area between the oxide semiconductor 230 and the conductor 242b2 (conductor 242a2) can be increased compared to the case where only one insulator 225 is provided. This makes it possible to reduce the contact resistance between the oxide semiconductor 230 and the conductor 242b2 (conductor 242a2).

[0315] In the above description, the insulators 225a and 225b are given a rectangular shape extending in the A5-A6 direction, but the present invention is not limited to this. For example, the planar shape of the insulator 225 can be a circumferential shape (which can also be described as frame-shaped, annular, donut-shaped, or closed curve-shaped) with both ends coinciding or substantially coinciding. For example, the insulators 225a and 225b shown in Figure 11A can be given a shape in which both ends are connected.

[0316] Furthermore, in Figures 4A to 4D, a metal oxide layer 235 is provided between transistor 200_1 and transistor 200_2, but the present invention is not limited to this, and a configuration without the metal oxide layer 235 is also possible. For example, as shown in Figures 12A to 12D, a configuration can be made in which the metal oxide layer 235 is not provided and transistor 200_1 and transistor 200_2 are provided separately. Here, in the structure shown in Figures 4A to 4B, the insulator 224, insulator 225, oxide semiconductor 230, conductor 242b, insulator 271b, conductor 240b, and insulator 241b were shared by transistor 200_1 and transistor 200_2, but in the structure shown in Figures 12A to 12D, they are provided individually for transistor 200_1 and transistor 200_2, respectively. Note that Figures 12A to 12D correspond to Figures 4A to 4D, respectively, so for detailed configurations, please refer to the above description.

[0317] The semiconductor device shown in Figures 12A to 12D can be formed by removing the metal oxide layer 235 when processing the oxide semiconductor film 230f, etc., into island shapes after the process shown in Figure 5D. When removing the metal oxide layer 235, the oxide semiconductor film 230f, insulator 225, etc., are divided into region 220_1 and region 220_2, so that transistors 200_1 and 200_2 can be formed separately, as shown in Figures 12A to 12D. In this case, since the metal oxide layer 235 is removed, as shown in Figure 12C, etc., the metal oxide layer 235 is not formed between the oxide semiconductor 230 and the insulators 225 and 224 in the region overlapping with the conductor 242b. Therefore, in the region overlapping with the conductor 242b, the insulators 225 and 224 are in contact with the lower surface of the oxide semiconductor 230.

[0318] Furthermore, as shown in Figure 12D, it is preferable that the A5-side surfaces of the insulator 271a, conductor 242a, oxide semiconductor 230, insulator 225, and insulator 224 are flush. In this case, it is preferable that the A5-side surfaces of the insulator 271a, conductor 242a, oxide semiconductor 230, insulator 225, and insulator 224 are in contact with the insulator 275. Similarly, as shown in Figure 12D, it is preferable that the A6-side surfaces of the insulator 271b, conductor 242b, oxide semiconductor 230, insulator 225, and insulator 224 are flush. In this case, it is preferable that the A6-side surfaces of the insulator 271b, conductor 242b, oxide semiconductor 230, insulator 225, and insulator 224 are in contact with the insulator 275.

[0319] The semiconductor device shown in Figures 12A to 12D is an example in which the region of the insulator 225 that overlaps with the metal oxide layer 235 is removed after the process shown in Figure 5D, but the present invention is not limited to this. For example, when the metal oxide layer 235 is removed after the process shown in Figure 5D, the insulator 225 can be left in place. In this case, in the semiconductor device shown in Figures 12A to 12D, transistors 200_1 and 200_2 are formed on island-shaped insulators 224 and 225.

[0320] Furthermore, as shown in Figure 13, the transistors 200_1, 200_2, 205_1, 205_2, and 310 can be used to create a memory device having two 1T (transistor) 1C (capacitance) type memory cells. As shown in Figure 13, the configuration can include a layer containing transistor 310, a layer above it containing transistors 200_1 and 200_2, and a layer above that containing 205_1 and 205_2.

[0321] The transistor 310 is provided on a substrate 311 and has a conductor 316 that functions as a gate, an insulator 315 that functions as a gate insulator, a semiconductor region 313 that includes a part of the substrate 311, and low-resistance regions 314a and 314b that function as a source region or drain region. The transistor 310 may be either a p-channel transistor or an n-channel transistor. For example, a single-crystal silicon substrate can be used as the substrate 311.

[0322] Furthermore, the transistor 310 has a convex shape in the semiconductor region 313 (part of the substrate 311) where the channel is formed. In addition, the sides and top surface of the semiconductor region 313 are covered by a conductor 316 via an insulator 315. The conductor 316 may be made of a material that adjusts the work function. Such a transistor 310 is also called a fin-type transistor because it utilizes the convex portion of the semiconductor substrate. It may also have an insulator that is in contact with the upper part of the convex portion and functions as a mask for forming the convex portion. In addition, although the case of forming the convex portion by processing a part of the semiconductor substrate is shown here, a semiconductor film having a convex shape may also be formed by processing an SOI (Silicone on Insulator) substrate.

[0323] Note that the transistor 310 shown in Figure 13 is just one example, and its structure is not limited to this example; an appropriate transistor can be used depending on the circuit configuration or driving method.

[0324] A wiring layer containing an interlayer film, wiring, and plugs may be provided between each structure. Furthermore, multiple wiring layers may be provided depending on the design. Also, in this specification, the wiring and the plugs electrically connected to the wiring may be integrated into a single unit. That is, a portion of the conductor may function as wiring, and a portion of the conductor may function as a plug.

[0325] For example, on the transistor 310, insulators 320, 322, 324, and 326 are stacked in order as interlayer films. Conductors such as 328 are embedded in insulators 320 and 322. Conductors such as 330 are embedded in insulators 324 and 326. Conductors 328 and 330 function as contact plugs or wiring.

[0326] Furthermore, the insulator functioning as an interlayer film may also function as a planarizing film that covers the uneven shape beneath it. For example, the upper surface of the insulator 322 may be planarized by a planarizing treatment using the CMP method or the like to improve its flatness.

[0327] Transistors 200_1 and 200_2 are provided on the insulator 326. Here, transistors 200_1 and 200_2 are the transistors 200_1 and 200_2 shown in Figure 4D. The structure of transistors 200_1, 200_2 and the layer containing them is the same as the structure described above, and is indicated by the same hatching pattern and reference numerals. For detailed structure, refer to the description above. An insulator 286 and a conductor 290 are provided on the insulator 285. The insulator 286 functions as an interlayer film, and conductors 240a, conductor 290, etc. can be provided in the openings formed in the insulator 286. Conductor 290 functions as wiring and is connected to conductor 240b.

[0328] Capacitive elements 205_1 and 205_2 are provided on the insulator 286. Note that for components of capacitive element 205_2, the same components as those of capacitive element 205_1 are omitted from the reference numerals. The configuration of capacitive element 205_2 can be referenced from capacitive element 205_1.

[0329] A conductor 292, a capacitive element 205_1, a capacitive element 205_2, and an insulator 288 are provided on the insulator 286. The insulator 287 and the insulator 288 on the insulator 287 function as interlayer films. The insulator 287 is provided covering the conductor 292, and the insulator 288 is provided covering the capacitive elements 205_1 and 205_2. The conductor 292 functions as an electrode and is connected to the conductor 240a.

[0330] The capacitive element 205_1 has a conductor 294 on the conductor 292, an insulator 296 on the conductor 294, and a conductor 298 on the insulator 296.

[0331] The conductor 294 has a region that functions as one electrode (lower electrode) of the capacitive element 205_1. The insulator 296 has a region that functions as the dielectric of the capacitive element 205_1. The conductor 298 has a region that functions as the other electrode (upper electrode) of the capacitive element 205_1. The capacitive element 205_1 constitutes a MIM (Metal-Insulator-Metal) capacitance.

[0332] The conductor 294 is provided extending in the direction normal to the substrate 311, with a portion of it provided in an opening formed in the insulator 287. The insulator 296 is provided covering the insulator 287 and the conductor 294. The conductor 298 is provided covering the portion of the conductor 294 that protrudes from the insulator 287 via the insulator 296. The insulator 288 is provided covering the conductor 298 and the insulator 296.

[0333] In the portion of the conductor 294 that protrudes from the insulator 287, the upper and side surfaces of the conductor 294 face the conductor 298 via the insulator 296, and function as a capacitive element. Therefore, the higher the portion of the conductor 294 that protrudes from the insulator 287, the larger the capacitance of the capacitive element 205_1 can be. By increasing the capacitance per unit area of ​​the capacitive element 205_1, miniaturization or high integration of the memory device can be achieved.

[0334] It is preferable to use a material with a high dielectric constant (high-k) for the insulator 296 of the capacitive element 205_1. Examples of insulators with a high dielectric constant include gallium oxide, hafnium oxide, zirconium oxide, oxides having aluminum and hafnium, oxiditrides having aluminum and hafnium, oxides having silicon and hafnium, oxiditrides having silicon and hafnium, and nitrides having silicon and hafnium. By using such a high-k material, the insulator 296 can be made thick enough to suppress leakage current, while ensuring sufficient capacitance of the capacitive element 205_1. Furthermore, it is preferable to deposit the insulator 296 using a film deposition method with good coverage, such as the ALD method or the CVD method.

[0335] Furthermore, it is preferable to use insulators made of the above materials in a laminated form, and it is preferable to use a laminated structure of a material with a high dielectric constant (high-k) and a material with a greater dielectric strength than the material with a high dielectric constant (high-k). For example, as the insulator 296, an insulator laminated in the order of zirconium oxide, aluminum oxide, and zirconium oxide can be used. Alternatively, for example, an insulator laminated in the order of zirconium oxide, aluminum oxide, zirconium oxide, and aluminum oxide can be used. Alternatively, for example, an insulator laminated in the order of hafnium zirconium oxide, aluminum oxide, hafnium zirconium oxide, and aluminum oxide can be used. By using laminated insulators with relatively high dielectric strength, such as aluminum oxide, the dielectric strength is improved, and electrostatic discharge breakdown of the capacitive element 205_1 can be suppressed.

[0336] Furthermore, a material capable of ferroelectricity may be used as the insulator 296. Examples of materials capable of ferroelectricity include hafnium oxide, zirconium oxide, and hafnium-zirconium oxide (HfZrO). X Examples include metal oxides such as (where X is a real number greater than 0).

[0337] Furthermore, in the example shown in Figure 13, a pillar-type capacitive element is used in which the conductor 294, which functions as the lower electrode, extends in the direction normal to the substrate. However, the present invention is not limited to this. For example, a cylindrical capacitive element formed in the opening of the interlayer film may be used.

[0338] Furthermore, it is preferable to superimpose the capacitive element 205_1 and the transistor 200_1. Similarly, it is preferable to superimpose the capacitive element 205_2 and the transistor 200_2. It is also preferable to provide a conductor 240b or the like between transistor 200_1 and transistor 200_2. By adopting the above configuration, the occupied area of ​​the memory cell can be reduced, and the miniaturization or high integration of the memory device can be achieved.

[0339] Furthermore, it is preferable to use the transistor 310 to form a drive circuit for the memory cell array including the memory cell. With this configuration, the drive circuit can be superimposed on the memory cell array, thereby reducing the occupied area of ​​the storage device.

[0340] Furthermore, although Figure 13 shows a configuration in which a transistor 310 formed on a silicon substrate is provided, the present invention is not limited to this. For example, an OS transistor having a structure similar to the transistor 200 described above may also be provided.

[0341] Furthermore, while the above describes a configuration for forming a memory cell, it is not limited to this. For example, a CMOS circuit can be constructed by using an n-channel transistor for the OS transistor, which is located in the same layer as transistor 200_1, and a p-channel transistor for transistor 310.

[0342] <Materials for semiconductor devices> The following describes materials that can be used in semiconductor devices. Note that each layer constituting a semiconductor device may be a single-layer structure or a multilayer structure.

[0343] <<Substrate>> As the substrate for forming a transistor, for example, an insulator substrate, a semiconductor substrate, or a conductor substrate can be used. Examples of the insulator substrate include a glass substrate, a quartz substrate, a sapphire substrate, a stabilized zirconia substrate (such as an yttria-stabilized zirconia substrate), and a resin substrate. Examples of the semiconductor substrate include a semiconductor substrate made of silicon or germanium, and a compound semiconductor substrate made of silicon carbide, silicon germanium, gallium arsenide, indium phosphide, zinc oxide, or gallium oxide. Further, a semiconductor substrate having an insulator region inside the aforementioned semiconductor substrate, for example, an SOI substrate and the like can be mentioned. Examples of the conductor substrate include a graphite substrate, a metal substrate, an alloy substrate, and a conductive resin substrate. Examples of the substrate also include a substrate containing a metal nitride, a substrate containing a metal oxide, a substrate in which a conductor or a semiconductor is provided on an insulator substrate, a substrate in which a conductor or an insulator is provided on a semiconductor substrate, and a substrate in which a semiconductor or an insulator is provided on a conductor substrate. Alternatively, a substrate in which one or more types of elements are provided on these substrates may be used. Examples of the elements provided on the substrate include a capacitive element, a resistive element, a switch element, a light-emitting element, and a memory element.

[0344] <<Insulator>> Examples of the insulator that can be used for at least one of insulator 215, insulator 216, insulator 221, insulator 222, insulator 224, insulator 225, insulator 241, insulator 250, insulator 255, insulator 271a, insulator 271b, insulator 275, insulator 280, insulator 282, insulator 283, insulator 285, insulator 285, insulator 286, insulator 287, insulator 288, insulator 315, insulator 320, insulator 322, insulator 324, and insulator 326 include an insulating oxide, nitride, oxynitride, nitride oxide, metal oxide, metal oxynitride, and metal nitride oxide.

[0345] For example, as transistors are miniaturized and highly integrated, thinning of the gate insulator may cause problems such as leakage current. By using a high-k material for the insulator functioning as a gate insulator, the operating voltage of the transistor can be lowered while maintaining the physical film thickness. On the other hand, by using a material with a low relative permittivity for the insulator functioning as an interlayer film, parasitic capacitance generated between wirings can be reduced. Therefore, a material is preferably selected in accordance with the function of the insulator.

[0346] Examples of the insulator with a high relative permittivity include gallium oxide, hafnium oxide, zirconium oxide, an oxide containing aluminum and hafnium, an oxynitride containing aluminum and hafnium, an oxide containing silicon and hafnium, an oxynitride containing silicon and hafnium, and a nitride containing silicon and hafnium.

[0347] Examples of the insulator with a low relative permittivity include silicon oxide, silicon oxynitride, silicon nitride oxide, silicon nitride, silicon oxide to which fluorine is added, silicon oxide to which carbon is added, silicon oxide to which carbon and nitrogen are added, silicon oxide having a void, and a resin.

[0348] In addition, a transistor using a metal oxide can have stable electrical characteristics by being surrounded by an insulator having a function of suppressing permeation of oxygen and impurities such as hydrogen. Examples of the insulator having a function of suppressing permeation of oxygen and impurities such as hydrogen include an insulator containing one or more of boron, carbon, nitrogen, oxygen, fluorine, magnesium, aluminum, silicon, phosphorus, chlorine, argon, gallium, germanium, yttrium, zirconium, lanthanum, neodymium, hafnium, and tantalum, which can be used as a single layer or a stacked layer. Specifically, examples of the insulator having a function of suppressing permeation of oxygen and impurities such as hydrogen include oxides such as aluminum oxide, magnesium oxide, gallium oxide, germanium oxide, yttrium oxide, zirconium oxide, lanthanum oxide, neodymium oxide, hafnium oxide, and tantalum oxide, and nitrides such as aluminum nitride, silicon nitride oxide, and silicon nitride.

[0349] Furthermore, the insulator that functions as a gate insulator is preferably an insulator having a region containing oxygen that is desorbed by heating. For example, by having silicon oxide or silicon oxynitride having a region containing oxygen that is desorbed by heating in contact with the oxide semiconductor 230, the oxygen vacancies in the oxide semiconductor 230 can be compensated for.

[0350] <<Conductors>> It is preferable to use a conductor that can be used in at least one of conductors 240, 242, 260, 290, 292, 294, 298, 316, 328, and 330 that is a metallic element selected from aluminum, chromium, copper, silver, gold, platinum, tantalum, nickel, cobalt, titanium, molybdenum, tungsten, hafnium, vanadium, niobium, manganese, magnesium, zirconium, beryllium, indium, ruthenium, iridium, strontium, lanthanum, etc., or an alloy containing the above-mentioned metallic elements, or an alloy combining the above-mentioned metallic elements. Examples of conductors include tantalum nitride, titanium nitride, nitrides containing titanium and aluminum, nitrides containing tantalum and aluminum, ruthenium oxide, ruthenium nitride, oxides containing strontium and ruthenium, and oxides containing lanthanum and nickel. Furthermore, tantalum nitride, titanium nitride, nitrides containing titanium and aluminum, nitrides containing tantalum and aluminum, ruthenium oxide, ruthenium nitride, oxides containing strontium and ruthenium, and oxides containing lanthanum and nickel are preferred because they are conductive materials that are resistant to oxidation or maintain conductivity even when absorbing oxygen. Alternatively, highly conductive semiconductors such as polycrystalline silicon containing impurity elements like phosphorus, or silicides such as nickel silicide may be used.

[0351] When using a laminated conductor, for example, a laminated structure combining a material containing the aforementioned metal element and a conductive material containing oxygen, a laminated structure combining a material containing the aforementioned metal element and a conductive material containing nitrogen, or a laminated structure combining a material containing the aforementioned metal element, a conductive material containing oxygen, and a conductive material containing nitrogen may be applied.

[0352] Furthermore, when using an oxide in the channel formation region of a transistor, it is preferable to use a laminated structure for the conductor functioning as the gate electrode, which combines a material containing the aforementioned metal element with a conductive material containing oxygen. In this case, it is preferable to provide the conductive material containing oxygen on the channel formation region side. By providing the conductive material containing oxygen on the channel formation region side, oxygen detached from the conductive material is more easily supplied to the channel formation region.

[0353] In particular, it is preferable to use a conductive material containing metal elements and oxygen contained in the metal oxide in which the channel is formed as the conductor that functions as the gate electrode. Alternatively, conductive materials containing the aforementioned metal elements and nitrogen may be used. For example, conductive materials containing nitrogen such as titanium nitride and tantalum nitride may be used. Alternatively, one or more of the following may be used: indium tin oxide, indium oxide containing tungsten oxide (which can also be called indium oxide), indium zinc oxide containing tungsten oxide, indium oxide containing titanium oxide, indium tin oxide containing titanium oxide, indium zinc oxide, and silicon-doped indium tin oxide. In addition, indium gallium zinc oxide containing nitrogen may be used. By using such materials, it may be possible to capture hydrogen contained in the metal oxide in which the channel is formed. Alternatively, it may be possible to capture hydrogen that is mixed in from an external insulator or the like.

[0354] <Example of Semiconductor Device Fabrication Method> An example of a semiconductor device fabrication method according to one embodiment of the present invention will be described using Figures 14A to 22D. Here, the case of fabricating the semiconductor device shown in Figures 4A to 4D will be used as an example. Figures 14A to 22D correspond to Figures 4A to 4D, and corresponding components are denoted by the same reference numerals. Therefore, similar to Figures 4A to 4D, the reference numerals are omitted for components of transistor 200_2 that are the same as those of transistor 200_1. In the following, mainly transistor 200_1 will be described, but the description relating to transistor 200_1 can be reflected in the configuration of transistor 200_2.

[0355] (A) in each figure is a plan view. (B) in each figure is a cross-sectional view corresponding to the area indicated by the dashed line A1-A2 in (A), and is also a cross-sectional view of transistor 200_1 in the channel width direction. (C) in each figure is a cross-sectional view corresponding to the area indicated by the dashed line A3-A4 in (A), and is also a cross-sectional view of transistors 200_1 and 200_2 in the channel width direction. (D) in each figure is a cross-sectional view of the area indicated by the dashed line A5-A6 in (A), and is also a cross-sectional view of transistors 200_1 and 200_2 in the channel length direction. Note that in the plan view (A) of each figure, some elements have been omitted for clarity.

[0356] In the following, insulating materials for forming an insulator, conductive materials for forming a conductor, or semiconductor materials for forming a semiconductor can be deposited using sputtering, CVD, MBE, PLD, ALD, or other appropriate methods.

[0357] Sputtering methods include RF sputtering, which uses a high-frequency power supply; DC sputtering, which uses a DC power supply; and pulsed DC sputtering, which changes the voltage applied to the electrodes in pulses. For film deposition using insulating targets, RF sputtering is preferable. DC sputtering is mainly used when depositing films using conductive targets. In addition to forming conductive films, DC sputtering can also be used to form insulating films by reactive sputtering using pulsed DC sputtering. Specifically, pulsed DC sputtering can be used when depositing compounds such as oxides, nitrides, and carbides using reactive sputtering.

[0358] Furthermore, CVD methods can be classified into plasma CVD (PECVD), which utilizes plasma; thermal CVD (TCD), which utilizes heat; and photo CVD (Photo CVD), which utilizes light. They can also be further divided into metal CVD (MCCVD) and MOCVD depending on the source gas used.

[0359] Plasma CVD allows for the production of high-quality films at relatively low temperatures. Thermal CVD, on the other hand, does not use plasma, thus minimizing plasma damage to the workpiece. For example, wiring, electrodes, and components (transistors, capacitive elements, etc.) in semiconductor devices can be charged up by receiving charge from the plasma. This accumulated charge can damage these components. In contrast, thermal CVD, which does not use plasma, avoids such plasma damage, resulting in higher yields for semiconductor devices. Furthermore, thermal CVD produces films with fewer defects because it avoids plasma damage during deposition.

[0360] Furthermore, ALD methods such as thermal ALD, which carries out the reaction of the precursor and reactant using only thermal energy, and PEALD, which uses plasma-excited reactants, can be used.

[0361] CVD and ALD methods differ from sputtering, where particles emitted from a target or other source are deposited. Therefore, they are less affected by the shape of the workpiece and are film deposition methods that provide good step-level coverage. In particular, the ALD method has excellent step-level coverage and excellent thickness uniformity, making it suitable for coating the surface of openings with high aspect ratios. However, since the ALD method has a relatively slow deposition rate, it is sometimes preferable to use it in combination with other film deposition methods such as the CVD method, which has a faster deposition rate.

[0362] Furthermore, the CVD method allows for the deposition of films with arbitrary compositions by changing the flow rate ratio of the source gases. For example, in the CVD method, by changing the flow rate ratio of the source gases while deposition is occurring, films with continuously changing compositions can be deposited. When deposition is performed while changing the flow rate ratio of the source gases, the deposition time can be shortened compared to deposition using multiple deposition chambers, because time required for transport or pressure adjustment is eliminated. Therefore, it may be possible to increase the productivity of semiconductor devices.

[0363] First, a substrate (not shown) is prepared, and an insulator 215 is deposited on the substrate (see Figures 14A to 14D). As described above, the insulator 215 can be an insulator similar to one or more of the laminated films of insulators 282 and 283. For example, the insulator 215 can be deposited by sputtering, CVD, MBE, PLD, or ALD. It is preferable to use a sputtering method, which does not require the use of hydrogen-containing molecules in the deposition gas, because this can reduce the hydrogen concentration in the insulator 215.

[0364] Next, an insulator 216 is deposited on the insulator 215. The deposition of the insulator 216 is preferably carried out using a sputtering method. By using a sputtering method that does not require the use of hydrogen-containing molecules in the deposition gas, the hydrogen concentration in the insulator 216 can be reduced. However, the deposition of the insulator 216 is not limited to the sputtering method; CVD, MBE, PLD, ALD, etc., may be used as appropriate. In this embodiment, silicon oxide is deposited as the insulator 216 using the sputtering method.

[0365] It is preferable to continuously deposit the insulators 215 and 216 without exposure to the atmosphere. For example, a multi-chamber type deposition apparatus can be used. This allows for the deposition of the insulators 215 and 216 with reduced hydrogen content in the film, and further reduces the incorporation of hydrogen into the film between each deposition process.

[0366] Next, an insulating film 221 is formed on the insulating film 216 (see Figures 14A to 14D).

[0367] The insulator 221 may be any insulator having barrier properties against oxygen, hydrogen, and water as described above. The insulator 221 can be formed using, for example, sputtering, CVD, MBE, PLD, or ALD. In this embodiment, silicon nitride is formed as the insulator 221 using the PEALD method.

[0368] Next, an insulating film 222 is formed on the insulating film 221 (see Figures 14A to 14D).

[0369] As the insulator 222, it is preferable to form a film of an insulator containing an oxide of either or both aluminum and hafnium. For example, it is preferable to use aluminum oxide, hafnium oxide, or an oxide containing both aluminum and hafnium (hafnium aluminate) as the insulator containing an oxide of either or both aluminum and hafnium. Alternatively, it is preferable to use hafnium zirconium oxide. The insulator containing an oxide of either or both aluminum and hafnium has barrier properties against oxygen, hydrogen, and water. Because the insulator 222 has barrier properties against hydrogen and water, the diffusion of hydrogen and water contained in the structure provided around the transistor through the insulator 222 into the inside of the transistor is suppressed, thereby suppressing the generation of oxygen vacancies in the oxide semiconductor 230.

[0370] The insulator 222 can be formed using, for example, sputtering, CVD, MBE, PLD, or ALD. In this embodiment, hafnium oxide is formed as the insulator 222 using the thermal ALD method.

[0371] In this embodiment, silicon nitride is deposited as the insulator 221 using the PEALD method, and hafnium oxide is deposited as the insulator 222 using the thermal ALD method. By using silicon nitride, which has the function of suppressing hydrogen diffusion, for the insulator 221, it is possible to suppress the diffusion of hydrogen from the lower layer of transistors 200_1 and 200_2. Furthermore, by using hafnium oxide, which has the function of capturing or fixing hydrogen, for the insulator 222, hydrogen contained in the oxide semiconductor 230 can be captured or fixed to the insulator 222. This makes it possible to reduce the hydrogen concentration in and near the oxide semiconductor 230.

[0372] Next, an insulating film 224f is deposited on the insulator 222 (see Figures 14A to 14D). The insulating film 224f is the insulating film that will become the insulator 224 in a later step. Therefore, any insulating material that can be used for the insulator 224 described above should be used. The insulating film 224f can be deposited using, for example, sputtering, CVD, MBE, PLD, or ALD. For example, silicon oxide can be deposited as the insulating film 224f using the sputtering method.

[0373] Next, an insulator 225 and a metal oxide layer 235 are formed on the insulating film 224f (see Figures 14A to 14D). Details of the formation of the insulator 225 and the metal oxide layer 235 can be found in the description in Figure 5A above. As the insulating film that will become the insulator 225, any insulating material that can be used for the insulator 225 as described above may be used. Similarly, as the metal oxide film that will become the metal oxide layer 235, any metal oxide material that can be used for the metal oxide layer 235 as described above may be used. The insulating film that will become the insulator 225 and the metal oxide film that will become the metal oxide layer 235 can be formed using sputtering, CVD, MBE, PLD, or ALD. For example, gallium oxide can be formed as the insulating film that will become the insulator 225 using sputtering. Alternatively, for example, as the metal oxide film that will become the metal oxide layer 235, a film of indium oxide formed using the ALD method and then crystallized by microwave plasma treatment can be used.

[0374] The insulator 225 and the metal oxide layer 235 can each be processed using lithography. Dry etching or wet etching can be used for this processing. Dry etching is suitable for microfabrication.

[0375] In lithography, the resist is first exposed through a mask. Next, the exposed area is removed or left intact using a developer to form a resist mask. Then, by etching through this resist mask, conductors, semiconductors, or insulators can be processed into the desired shape. For example, a resist mask can be formed by exposing the resist using KrF excimer laser light, ArF excimer laser light, or EUV (Extreme Ultraviolet) light. Alternatively, immersion technology may be used, in which a liquid (e.g., water) is filled between the substrate and the projection lens for exposure. In addition, an electron beam or ion beam may be used instead of the aforementioned light. When using an electron beam or ion beam, a photomask may not be necessary.

[0376] Furthermore, the resist mask that is no longer needed after processing can be removed by dry etching, such as ashing using oxygen plasma (hereinafter sometimes referred to as oxygen plasma treatment), wet etching, wet etching after dry etching, or dry etching after wet etching.

[0377] Further, a hard mask made of an insulator or a conductor may be used under the resist mask. For example, in the above description, the aluminum oxide film on the silicon nitride film functions as a hard mask. When a hard mask is used, an insulating film or a conductive film to be a hard mask material is formed, a resist mask is formed thereon, and the hard mask material is etched, whereby the hard mask having a desired shape can be formed. The etching of the silicon nitride film may be performed after removing the resist mask, or may be performed while leaving the resist mask. In the latter case, the resist mask may disappear during etching. After the etching of the silicon nitride film, the hard mask may be removed by etching. On the other hand, when the material of the hard mask does not affect subsequent processes or can be used in subsequent processes, it is not always necessary to remove the hard mask.

[0378] Further, a configuration in which an SOC (Spin On Carbon) film and an SOG (Spin On Glass) film are formed between the object to be processed and the resist mask may be adopted. By using the SOC film and the SOG film as masks, the durability of the mask pattern can be improved. For example, the SOC film, the SOG film, and the resist mask can be formed in this order over the object to be processed to perform a lithography method.

[0379] As an etching gas for dry etching treatment, an etching gas containing halogen can be used, and specifically, an etching gas containing one or more of fluorine, chlorine, and bromine can be used. For example, as the etching gas, C 4 F 6 gas, C 5 F 6 gas, C 4 F 8 gas, CF 4 gas, SF 6 gas, CHF 3 gas, CH 2 F 2 gas, Cl 2 gas, BCl 3 gas, SiCl 4 gas, or BBr 3A gas or the like may be used alone, or two or more gases may be used as a mixture. In addition, oxygen gas, carbon dioxide gas, nitrogen gas, helium gas, argon gas, hydrogen gas, hydrocarbon gas or the like may be appropriately added to the above etching gas. Further, depending on the workpiece subjected to the dry etching treatment, a gas containing no halogen gas and containing a hydrocarbon gas or hydrogen gas may be used as the etching gas. Examples of the hydrocarbon used for the etching gas include methane (CH 4 ), ethane (C 2 H 6 ), propane (C 3 H 8 ), butane (C 4 H 10 ), ethylene (C 2 H 4 ), propylene (C 3 H 6 ), acetylene (C 2 H 2 ), and propyne (C 3 H 4 ), one or more thereof may be used. The etching conditions can be appropriately set according to the object to be etched.

[0380] As a dry etching apparatus, a capacitively coupled plasma (CCP) etching apparatus having parallel plate electrodes can be used. A capacitively coupled plasma etching apparatus having parallel plate electrodes may be configured to apply a high-frequency voltage to one of the parallel plate electrodes, or to apply a high-frequency voltage of the same frequency to each of the parallel plate electrodes, or to apply multiple different high-frequency voltages to the parallel plate electrodes. Such a CCP etching apparatus is called a dual-frequency excited capacitively coupled plasma (DF-CCP) etching apparatus. In a DF-CCP etching apparatus, a configuration can be used in which high-frequency voltages of different frequencies are applied to each of the parallel plate electrodes, or to apply multiple different high-frequency voltages to one of the parallel plate electrodes. Alternatively, a dry etching apparatus having a high-density plasma source can be used. For example, an inductively coupled plasma (ICP) etching apparatus can be used as a dry etching apparatus having a high-density plasma source. The etching apparatus can be appropriately configured according to the object to be etched. In addition, reactive ion etching can be performed by applying a high-frequency voltage to the electrode on the substrate side of the dry etching apparatus to generate a self-bias potential. In reactive ion etching, etching is performed by accelerating ion species in the plasma and causing them to collide with the workpiece, thus enabling highly anisotropic etching.

[0381] Furthermore, when indium oxide is used for the metal oxide layer 235 and gallium oxide is used for the insulator 225, silicon oxide is used for the insulating film 224f, which allows the insulating film 224f to function as an etching stopper during the etching process of the insulator 225.

[0382] Furthermore, while Figures 14A to 14D show a configuration in which one insulator 225 is provided on transistors 200_1 and 200_2, the present invention is not limited to this. It is also possible to provide two or more insulators 225 spaced apart. For example, by providing insulators 225a and 225b, it is possible to form a transistor in which two or more insulators 225 are arranged in the A1-A2 direction, similar to the transistor 200 in the configuration shown in Figures 11A to 11D.

[0383] Next, an oxide semiconductor film 230f, which will become the oxide semiconductor 230, is formed by covering the insulator 225 and the metal oxide layer 235 (see Figures 15A to 15D). Furthermore, it is preferable to crystallize the oxide semiconductor film 230f by heat treatment. The oxide semiconductor film 230f is a metal oxide film that will become the oxide semiconductor 230 in a later step, and the above-described oxide semiconductor film can be used. The oxide semiconductor film 230f can be formed using sputtering, CVD, MBE, PLD, or ALD.

[0384] The deposition and crystallization of the oxide semiconductor film 230f can be described by referring to the description in Figures 5B to 5D above. This makes it possible to make the oxide semiconductor film 230f an indium oxide having a single crystal structure or a highly crystalline indium oxide. Furthermore, the number of grain boundaries in the channel formation regions of transistors 200_1 and 200_2 can be reduced. With this configuration, a semiconductor device with high field-effect mobility can be provided. Furthermore, a semiconductor device with good electrical characteristics, frequency characteristics, and reliability can be provided.

[0385] Furthermore, microwave plasma treatment may be performed after the deposition of the oxide semiconductor film 230f. This may further enhance the crystallinity of the oxide semiconductor film 230f.

[0386] Next, a conductive film 242Af is deposited on the oxide semiconductor film 230f, and a conductive film 242Bf is deposited on the conductive film 242Af (see Figures 15A to 15D). The conductive film 242Af is a conductive film that becomes conductor 242a1 and conductor 242b1, and the conductive film 242Bf is a conductive film that becomes conductor 242a2 and conductor 242b2. For the conductive film 242Af, a conductive material that can be used for conductor 242a1 and conductor 242b1 may be used, and for the conductive film 242Bf, a conductive material that can be used for conductor 242a2 and conductor 242b2 may be used. Hereinafter, the conductive film 242Af and the conductive film 242Bf may be collectively referred to as the conductive film 242f.

[0387] The conductive films 242Af and 242Bf can be deposited using, for example, sputtering, CVD, MBE, PLD, or ALD. For example, ITO can be deposited as the conductive film 242Af using sputtering. Also, for example, tungsten can be deposited as the conductive film 242Bf using sputtering. By depositing the conductive film 242f over the oxide semiconductor film 230f, the contact area between the oxide semiconductor film 230f and the conductors 242a and 242b can be increased without increasing the occupied area. This makes it possible to improve the on-current and frequency characteristics of transistors 200_1 and 200_2.

[0388] Next, an insulating film 271f is deposited on the conductive film 242Bf (see Figures 15A to 15D). The insulating film 271f can be deposited using sputtering, CVD, MBE, PLD, or ALD. It is preferable to use an insulating film 271f that has the function of suppressing oxygen permeation. For example, as the insulating film 271f, a laminated film of a silicon nitride film and a silicon oxide film on the silicon nitride film can be deposited by sputtering. With such a configuration, the insulator 271a (insulator 271b) can be made into a laminated structure of a silicon nitride insulator 271a1 (insulator 271b1) and a silicon oxide insulator 271a2 (insulator 271b2).

[0389] Here, when forming a laminated film of the insulating film 271f, it is preferable to deposit the film continuously without exposing it to the atmosphere. By depositing the film without exposing it to the atmosphere, the interface or vicinity of the interface of the laminated film of insulating film 271f can be kept clean. Furthermore, it is even more preferable to deposit the film continuously from the conductive film 242Af to the insulating film 271f without exposing it to the atmosphere.

[0390] Furthermore, a heat treatment may be performed before the deposition of the insulating film 271f. This heat treatment may be carried out under reduced pressure, and the insulating film 271f may be deposited continuously without exposure to the atmosphere. By performing such a treatment, moisture and hydrogen adsorbed on the surface of the conductive film 242Bf can be removed, and the moisture and hydrogen concentrations in the conductive film 242Af and conductive film 242Bf can be further reduced. The temperature of the heat treatment is preferably between 100°C and 400°C.

[0391] Next, using lithography, the insulating film 224f, oxide semiconductor film 230f, conductive film 242Af, conductive film 242Bf, and insulating film 271f are processed into island-like structures to form insulator 224, oxide semiconductor 230, conductor 242A, conductor 242B, and insulator 271A (see Figures 16A to 16D). At this time, the region of the metal oxide layer 235 that does not overlap with insulator 271A is removed. As a result, insulator 222 is exposed in the region that does not overlap with insulator 271A.

[0392] The above processing can be performed using either a dry etching method or a wet etching method. Dry etching is suitable for microfabrication. For details on the conditions and equipment for the dry etching method, please refer to the description above. Furthermore, the processing of the insulating film 224f, oxide semiconductor film 230f, conductive film 242Af, conductive film 242Bf, and insulating film 271f may be performed under different conditions. In addition, a hard mask may be provided on the insulating film 271f when performing the above processing.

[0393] Here, it is preferable to process the insulator 224, oxide semiconductor 230, conductor 242A, conductor 242B, and insulator 271A together in an island shape. In this case, it is preferable that the side edge of insulator 271A coincides with or substantially coincides with the side edge of conductor 242A and the side edge of conductor 242B. It is preferable that the side edge of conductor 242A and the side edge of conductor 242B coincides with or substantially coincides with the side edge of oxide semiconductor 230. Furthermore, it is preferable that the side edge of insulator 224 coincides with or substantially coincides with the side edge of oxide semiconductor 230. Also, as shown in Figure 16C, it is preferable that the side edges on the A3 side and the A4 side of the metal oxide layer 235 coincide with or substantially coincides with the side edges on the A3 side and the A4 side of insulator 224 and oxide semiconductor 230, respectively. By adopting such a configuration, the number of processes for the semiconductor device according to one aspect of the present invention can be reduced. Therefore, a method for manufacturing a semiconductor device with good productivity can be provided.

[0394] As described above, by processing the insulator 224 into an island shape, the lower surface of the conductor 260 in transistors 200_1 and 200_2 can be positioned below the lower surface of the oxide semiconductor 230. This allows a sufficient electric field to be applied from the conductor 260 to the entire oxide semiconductor 230. Therefore, the electrical characteristics of transistors 200_1 and 200_2 can be improved.

[0395] The sides of the insulator 224, oxide semiconductor 230, conductor 242A, conductor 242B, and insulator 271A may be configured to be perpendicular or approximately perpendicular to the upper surface of the insulator 222. Such a configuration makes it possible to reduce the area and increase the density when providing multiple transistors.

[0396] However, the above is not limited to the above, and the sides of the insulator 224, oxide semiconductor 230, conductor 242A, conductor 242B, and insulator 271A may be tapered. The taper angle of the sides of the insulator 224, oxide semiconductor 230, conductor 242A, conductor 242B, and insulator 271A may be, for example, 60° or more and less than 90°. By making the sides tapered in this way, the coverage of the insulator 275 and the like can be improved in subsequent processes, and defects such as porosity can be reduced.

[0397] Furthermore, as shown in Figure 6A, a configuration without the insulator 224 is also possible. In this case, when the oxide semiconductor 230 is processed into an island shape, a portion of the upper surface of the insulator 222 may be removed. As a result, as shown in Figure 6A, the upper surface of the region of the insulator 222 that overlaps with the oxide semiconductor 230 may be higher than the upper surface of the region of the insulator 222 that does not overlap with the oxide semiconductor 230.

[0398] Furthermore, the dry etching process of the insulator 271A, conductor 242B, conductor 242A, oxide semiconductor 230, and insulator 224 can be carried out continuously without exposure to the outside air.

[0399] Furthermore, in the process shown in Figures 16A to 16D, the metal oxide layer 235 can be removed, and the insulating film 224f, insulator 225, oxide semiconductor film 230f, conductive film 242Af, conductive film 242Bf, and insulating film 271f can be processed to be separated by the dashed line A3-A4. By processing in this way, transistors 200_1 and 200_2 can be manufactured individually, as shown in Figures 12A to 12D.

[0400] Next, an insulator 275 is formed by covering the insulator 224, oxide semiconductor 230, conductor 242A, conductor 242B, and insulator 271A, and then an insulator 280 is formed on top of the insulator 275 (see Figures 17A to 17D). The insulators 275 and 280 can be the insulators described above.

[0401] In this case, it is preferable that the insulator 275 is in contact with the upper surface of the insulator 222.

[0402] Preferably, the insulator 280 is formed by creating an insulating film that will serve as the insulator 280, and then performing a CMP treatment on the insulating film to form an insulator with a flat top surface. Alternatively, silicon nitride may be deposited on the insulator 280, for example, by sputtering, and then the silicon nitride may be subjected to a CMP treatment until it reaches the insulator 280.

[0403] The insulators 275 and 280 can be deposited using, for example, sputtering, CVD, MBE, PLD, or ALD.

[0404] It is preferable to use an insulator 275 that has the function of suppressing oxygen permeation. For example, it is preferable to deposit silicon nitride as the insulator 275 using the PEALD method. Alternatively, it is preferable to deposit aluminum oxide as the insulator 275 using the sputtering method, and then deposit silicon nitride on top of it using the PEALD method. By making the insulator 275 such a structure, it is possible to improve the function of suppressing the diffusion of impurities such as water and hydrogen, and oxygen.

[0405] In this way, the oxide semiconductor 230, conductor 242A, and conductor 242B can be covered with an insulator 275 that has the function of suppressing oxygen diffusion. This makes it possible to suppress the direct diffusion of oxygen from the insulator 280, etc., into the oxide semiconductor 230, conductor 242A, and conductor 242B in a later process.

[0406] Furthermore, it is preferable to deposit silicon oxide as the insulator 280 using a sputtering method. By depositing the insulating film that will become the insulator 280 using a sputtering method in an oxygen-containing atmosphere, an insulator 280 containing excess oxygen can be formed. In addition, by using a sputtering method that does not require the use of hydrogen-containing molecules in the deposition gas, the hydrogen concentration in the insulator 280 can be reduced. Before depositing the insulating film, a heat treatment may be performed. The heat treatment may be performed under reduced pressure, and the insulating film may be deposited continuously without exposure to the atmosphere. By performing such a treatment, moisture and hydrogen adsorbed on the surface of the insulator 275 can be removed, and the moisture concentration and hydrogen concentration in the oxide semiconductor 230 can be further reduced. The heat treatment conditions described above can be used for this heat treatment.

[0407] Next, the conductor 242B, insulator 271A, insulator 275, and insulator 280 are processed using lithography to form openings 201 that reach the conductor 242A and insulator 222 (see Figures 18A to 18D). As shown in Figures 18A and 18D, the openings 201 are formed on the A5 side (transistor 200_1 side) and the A6 side (transistor 200_2 side), respectively.

[0408] The conductor 242B is divided to form conductors 242a2 and 242b2. Similarly, the insulator 271A is divided to form insulators 271a and 271b. The opening 201 is formed so that at least a portion of it overlaps with the oxide semiconductor 230. Here, the conductor 242b2 and insulator 271b are formed overlapping the metal oxide layer 235. As shown in Figures 18A and 18D, the conductor 242a2 and insulator 271a are formed on the A5 side (transistor 200_1 side) and the A6 side (transistor 200_2 side), respectively.

[0409] In a cross-sectional view of transistors 200_1 and 200_2 in the channel length direction, the width of the opening 201 is D2, which corresponds to the distance D2 between the conductors 242a2 and 242b2 described above. In other words, the width D2 of the opening 201 is greater than the distance D1 between the conductors 242a1 and 242b1 described above.

[0410] The lithography method can be appropriately adapted to the above method. To finely process the aperture of the insulator 280, it is preferable to use a lithography method that uses short-wavelength light such as i-line (wavelength 365 nm), g-line (wavelength 436 nm), h-line (wavelength 405 nm), ultraviolet light, KrF laser light, ArF laser light, EUV light, or an electron beam.

[0411] The above processing is preferably carried out using a dry etching method. Since the dry etching method allows for anisotropic etching, it is suitable for forming an opening 201 with a high aspect ratio. For details regarding the conditions and apparatus for the dry etching method, please refer to the above description.

[0412] Furthermore, although the above describes the process of forming island-shaped insulators 224 in the process shown in Figures 16A to 16D, it is also possible to form the insulator 224 by processing the insulating film 224f in the process shown in Figures 18A to 18D. In this case, the insulating film 224f can be further etched after etching the insulator 275. This removes the region of the insulator 224 that does not overlap with the oxide semiconductor 230 within the opening 201, and forms an opening that reaches the insulator 222. With this configuration, it is possible to form a transistor with a structure similar to the transistor 200 shown in Figures 10A to 10D.

[0413] Next, an insulating film 255A is formed by covering the insulator 280, the conductor 242A, and the insulator 222 (see Figures 19A to 19D). The insulating film 255A is an insulating film that will become the insulator 255 in a later step, and the above-mentioned insulators can be used. The insulating film 255A can be formed using, for example, a sputtering method, a CVD method, a MBE method, a PLD method, or an ALD method.

[0414] Since the insulating film 255A is formed along the opening 201, it is preferable that it has good coverage. Therefore, it is preferable to form the insulating film 255A using a method such as ALD that has good coverage. For example, it is preferable to form silicon nitride as the insulating film 255A using the PEALD method.

[0415] Next, a portion of the insulating film 255A is removed by anisotropic etching to form an insulator 255 in contact with the side wall of the opening 201. Furthermore, the conductor 242A is etched using the insulator 255 as a mask to form conductors 242a1 and 242b1 (see Figures 20A to 20D). As a result, the opening 201 becomes an opening that reaches the oxide semiconductor 230 and the insulator 222. Here, the conductor 242b1 is formed overlapping the metal oxide layer 235. As shown in Figures 20A and 20D, the insulator 255 and conductor 242a1 are formed on the A5 side (transistor 200_1 side) and the A6 side (transistor 200_2 side), respectively.

[0416] Here, in a cross-sectional view of transistors 200_1 and 200_2 in the channel length direction, if the distance between the insulator 255 on side A1 and the insulator 255 on side A2 is denoted as D1, this corresponds to the distance D1 between the conductors 242a1 and 242b1 described above. Since the insulator 255 is formed inside the opening 201, the distance D1 between the conductors 242a1 and 242b1 is shorter than the distance D2 between the conductors 242a2 and 242b2. The difference between D1 and D2 may coincide with or approximately coincide with twice the film thickness of the insulator 255.

[0417] The above processing is preferably carried out using a dry etching method. Since the dry etching method allows for anisotropic etching, it is suitable for performing microfabrication, such as the opening of the insulator 255 within the opening 201. The conditions for the dry etching method and the dry etching apparatus can be found in the description above.

[0418] Furthermore, during etching of the insulating film 255A, generated ions may collide with the corners of the edges of the openings in the insulators 280 and 255. As a result, these corners may be polished and become curved, as shown in Figure 9C and other figures. For example, by including an easily ionizable gas such as argon in the etching gas, or by applying a bias voltage to the electrodes on the substrate side, these corners can be more easily removed.

[0419] As described above, by using anisotropic etching to form an insulator 255 on the conductor 242A, and then using the insulator 255 as a mask to divide the conductor 242A, the insulator 255 that functions as a mask can be formed in a self-aligned manner. This makes it possible to reduce the number of masks and the number of processes in the semiconductor device manufacturing process shown in this embodiment. Therefore, a highly productive method for manufacturing semiconductor devices can be provided.

[0420] Furthermore, by using the above method, the island-shaped oxide semiconductor 230 can be exposed to dry etching only during the processing of the conductor 242A. In other words, the upper surface of the island-shaped oxide semiconductor 230 can be prevented from being exposed to dry etching during the formation of the insulator 255. This reduces the damage (for example, damage due to ion collisions) that the oxide semiconductor 230, which functions as the channel formation region of transistors 200_1 and 200_2, suffers from dry etching. During the dry etching process of the conductor 242A, the damage to the oxide semiconductor 230 can be further reduced by lowering the bias power midway through the process.

[0421] Furthermore, recesses may be formed in the portions of the oxide semiconductor 230 that are exposed from the conductors 242a1 and 242b1. For example, if indium oxide is used for the oxide semiconductor 230 and ITO is used for the conductor 242A, both the oxide semiconductor 230 and the conductor 242A contain indium oxide, making it difficult to selectively etch the conductor 242A relative to the oxide semiconductor 230. In this case, as shown in Figure 7A, the film thickness of the oxide semiconductor 230 in the region overlapping with the insulator 250 becomes thinner than the film thickness of the oxide semiconductor 230 in the region overlapping with the conductor 242a1 or conductor 242b1.

[0422] Furthermore, Figure 20B shows an example in which an insulator 255 is formed in a sidewall-like manner on the side surface of the insulator 280 and the side surface of the insulator 275 that form the side wall of the opening 201, but it is not limited to this. For example, an insulator 255 may remain on the side surface of the oxide semiconductor 230 inside the opening 201.

[0423] As described above, conductors 242a2 and 242b2 with a distance D2 from each other, and conductors 242a1 and 242b1 with a distance D1 from each other can be formed. By using this configuration, the distance between the source and drain of transistors 200_1 and 200_2 can be shortened, thereby improving the frequency characteristics of transistor 200 and the operating speed of the semiconductor device. Furthermore, by using the above configuration, the channel length of transistors 200_1 and 200_2 can be shortened, and the number of crystal grain boundaries included in the channel formation region can be reduced. This improves on-characteristics such as field-effect mobility.

[0424] Furthermore, after processing the conductor 242A and after processing the conductor 242B, an ashing treatment using oxygen plasma may be performed. By performing such oxygen plasma treatment, impurities generated during the etching process and diffused into the oxide semiconductor 230 can be removed. These impurities may be caused by components contained in the workpiece subjected to the etching process and components contained in the gas used for etching. Examples include chlorine, fluorine, tantalum, silicon, and hafnium. By removing these impurities attached to the oxide semiconductor 230, the electrical characteristics and reliability of the transistor can be improved.

[0425] Furthermore, the above-mentioned oxygen plasma treatment may cause at least a portion of the insulator 255 to be oxidized. In other words, oxygen may be present in the insulator 255. As the oxidation of the insulator 255 progresses, at least a portion of the insulator 255 may become silicon oxidized nitride or silicon nitride oxide after the formation of transistors 200_1 and 200_2.

[0426] Furthermore, the processing of the insulating film 255A and the conductor 242A, as well as the oxygen plasma treatment, can be carried out continuously without exposure to the atmosphere. For example, the processing can be performed without exposure to the atmosphere using a multi-chamber etching apparatus.

[0427] Furthermore, a cleaning process may be performed to remove impurities and other substances that have adhered to the surface of the oxide semiconductor 230 during the etching process described above. Cleaning methods include wet cleaning using a cleaning solution (which can also be called wet etching), plasma treatment using plasma, and cleaning by heat treatment, and these cleaning methods may be combined as appropriate. Note that the grooves may become deeper as a result of this cleaning process.

[0428] For wet cleaning, an aqueous solution may be used in which one or more of oxalic acid, phosphoric acid, and hydrofluoric acid are diluted with carbonated water or distilled water. Alternatively, wet cleaning may be used in which ammonia water is diluted with carbonated water or distilled water. Alternatively, wet cleaning may be used with distilled water or carbonated water. Or, ultrasonic cleaning may be performed using these aqueous solutions, distilled water, or carbonated water. Alternatively, these cleaning methods may be combined as appropriate. Furthermore, the above cleaning process may be performed multiple times, and the cleaning solution may be changed each time the cleaning process is performed.

[0429] It is preferable to perform a heat treatment after etching or cleaning as described above. The temperature of the heat treatment should be between 100°C and 650°C, preferably between 250°C and 600°C, more preferably between 300°C and 550°C, and even more preferably between 350°C and 400°C. The heat treatment should be performed in an atmosphere of nitrogen gas or an inert gas, or in an atmosphere containing 10 ppm or more, 1% or more, or 10% or more of an oxidizing gas. It is preferable to perform the heat treatment in an atmosphere containing oxygen, for example, by setting the flow rate ratio of nitrogen gas to oxygen gas to 4:1 and performing the treatment at a temperature of 350°C for 1 hour. This allows oxygen to be supplied to the oxide semiconductor 230, thereby reducing oxygen deficiency. Furthermore, by performing such a heat treatment, the crystallinity of the oxide semiconductor 230 can be improved. In addition, the supplied oxygen reacts with the hydrogen remaining in the oxide semiconductor 230, thereby converting the hydrogen into H 2 It can be removed as O (dehydrated). As a result, the hydrogen remaining in the oxide semiconductor 230 recombines with the oxygen vacancy and V OThe formation of H can be suppressed. Therefore, the electrical characteristics of the transistor provided with the oxide semiconductor 230 can be improved, and its reliability can be enhanced. In addition, variations in the electrical characteristics of multiple transistors formed on the same substrate can be suppressed. The above heat treatment may be performed under reduced pressure. Alternatively, the heat treatment may be performed in an oxygen atmosphere, and then continuously in a nitrogen atmosphere without exposure to the atmosphere. Furthermore, the above heat treatment can also serve as a heat treatment for the oxide semiconductor film 230f. Therefore, the crystalline region of the oxide semiconductor 230 may grow as a result of the above heat treatment.

[0430] Here, as described above, an insulator 255 having an inorganic insulator that is resistant to oxidation is provided in contact with the side surfaces of the conductor 242a2 and the conductor 242b2. This prevents the conductors 242a2 and 242b2 from being excessively oxidized by the heat treatment, even if relatively easily oxidized tungsten films or the like are used for the conductors 242a2 and 242b2. Furthermore, it prevents the interfaces between the conductor 242a2 and conductor 242a1, and between the conductor 242b2 and conductor 242b1 from being excessively oxidized.

[0431] Furthermore, when heat treatment is performed on the oxide semiconductor 230 while the conductors 242a and 242b are in contact, the sheet resistance may decrease in the regions of the oxide semiconductor 230 that overlap with conductor 242a and the regions that overlap with conductor 242b, respectively. Also, the carrier concentration may increase. Therefore, the resistance of the regions of the oxide semiconductor 230 that overlap with conductor 242a and the regions that overlap with conductor 242b can be reduced.

[0432] Furthermore, processing of the conductor 242A as described above, or subsequent cleaning treatments, may remove a portion of the upper surface of the oxide semiconductor 230 in the region between conductor 242a1 and conductor 242b1. As a result, as shown in Figure 7A, the upper surface of the region between conductor 242a1 and conductor 242b1 in the oxide semiconductor 230 may be lower than the upper surface of the region overlapping with conductor 242a1 or conductor 242b1.

[0433] Next, an insulating film 250A, which will become an insulator 250, is formed along the side and bottom surfaces of the opening 201 formed in the insulator 280 or the like (see Figures 21A to 21D). Here, the insulating film 250A is in contact with the insulator 255, the conductor 242a1, the conductor 242b1, the insulator 222, the insulator 224, and the oxide semiconductor 230.

[0434] The insulating film 250A can be deposited using sputtering, CVD, MBE, PLD, or ALD. For example, it is preferable to deposit the insulating film 250A using the ALD method. Similar to the insulator 250 described above, it is preferable to form the insulating film 250A with a thin film thickness, and it is necessary to minimize variations in film thickness. In contrast, the ALD method is a film deposition method that alternately introduces a precursor and a reactant (e.g., an oxidizing agent), and the film thickness can be adjusted by the number of times this cycle is repeated, thus enabling precise film thickness adjustment. Furthermore, the insulating film 250A needs to be deposited with good coverage on the bottom and sides of the opening. By using the ALD method, layers of atoms can be deposited one by one on the bottom and sides of the opening, so the insulating film 250A can be formed with good coverage on the opening.

[0435] Furthermore, when the insulating film 250A is deposited by the ALD method, ozone (O) is used as the oxidizing agent. 3 ), oxygen (O 2 ), water (H 2 O) can be used. Hydrogen-free ozone (O) 3 ), oxygen (O 2 By using oxidizing agents such as ), the amount of hydrogen diffusing into the oxide semiconductor 230 can be reduced.

[0436] The insulator 250 can be made into a laminated structure, as shown in Figure 2A. For example, as shown in Figure 2A, the insulator 250 can be made into a laminated structure of insulators 250a to 250d. In this case, aluminum oxide can be deposited as insulator 250a by thermal ALD, silicon oxide can be deposited as insulator 250b by PEALD, hafnium oxide can be deposited as insulator 250c by thermal ALD, and silicon nitride can be deposited as insulator 250d by PEALD. Furthermore, the insulator 250 is not limited to a four-layer laminated structure. For example, it can also be made into a three-layer laminated structure of insulator 250a, insulator 250b on insulator 250a, and insulator 250d on insulator 250b.

[0437] Furthermore, it is preferable to perform microwave plasma treatment in an oxygen-containing atmosphere after the deposition of the insulating film 250A, or after the deposition of any of the insulators constituting the insulating film 250A.

[0438] By performing microwave plasma treatment in an oxygen-containing atmosphere, the oxygen gas is converted into plasma using microwaves or high-frequency waves such as RF, and this oxygen plasma can be applied to the region of the oxide semiconductor 230 between the conductor 242a and the conductor 242b. Due to the action of the plasma, microwaves, etc., the V in that region O H can be separated into oxygen vacancies and hydrogen, and the hydrogen can be removed from the region. Here, when using the structure shown in Figure 2A, it is preferable to use an insulating film (for example, aluminum oxide) that has the function of capturing or fixing hydrogen as the insulator 250a. With such a configuration, the hydrogen generated by microwave plasma treatment can be captured or fixed to the insulating film 250A. In this way, the V included in the channel formation region O H can be reduced. As a result, oxygen deficiency in the channel formation region and V O This reduces H and lowers the carrier concentration. Furthermore, by supplying oxygen radicals generated by the oxygen plasma to the oxygen vacancies formed in the channel formation region, the oxygen vacancies in the channel formation region can be further reduced, and the carrier concentration can be lowered.

[0439] The oxygen injected into the channel-forming region can take various forms, including oxygen atoms, oxygen molecules, oxygen ions, and oxygen radicals (also called O radicals, which are atoms, molecules, or ions with unpaired electrons). The oxygen injected into the channel-forming region may be one or more of the above forms, with oxygen radicals being particularly preferred. Furthermore, the film quality of the insulator 250 can be improved, thereby increasing the reliability of the transistor. Additionally, the above microwave plasma treatment can supply oxygen to the insulators 250a and 250b. Excess oxygen from the insulators 250a and 250b can be supplied to the channel-forming region of the oxide semiconductor 230 by subsequent heat treatment.

[0440] Furthermore, by performing microwave plasma treatment, impurities such as carbon in the oxide semiconductor 230 can also be removed. By removing carbon, which is an impurity in the oxide semiconductor 230, the crystallinity of the oxide semiconductor 230 can be improved. In particular, when the oxide semiconductor 230 is deposited by the ALD method, carbon contained in the precursor may be incorporated into the oxide semiconductor 230, so it is preferable to remove the carbon by microwave plasma treatment.

[0441] On the other hand, the oxide semiconductor 230 has a region that overlaps with either the conductor 242a or the conductor 242b. This region can function as a source region or a drain region. Here, it is preferable that the conductors 242a and 242b function as shielding films against the effects of microwaves, high frequencies such as RF, and oxygen plasma when performing microwave plasma processing in an oxygen-containing atmosphere.

[0442] Conductors 242a and 242b shield against the effects of microwaves, RF or other high-frequency waves, oxygen plasma, etc., so these effects do not extend to the region of the oxide semiconductor 230 that overlaps with either conductor 242a or conductor 242b. As a result, the microwave plasma treatment does not affect the source region and drain region. O Because H is reduced and excessive oxygen supply does not occur, a decrease in carrier concentration can be prevented.

[0443] Here, an insulator 255 is provided in contact with the sides of the conductors 242a2 and 242b2, and has barrier properties against oxygen. This makes it possible to suppress the formation of an oxide film on the sides of the conductors 242a2 and 242b2 by microwave plasma treatment.

[0444] As described above, oxygen vacancies and V are selectively formed in the channel formation region of the oxide semiconductor. O By removing H, the channel formation region can be made i-type or substantially i-type. Furthermore, it is possible to suppress the supply of excess oxygen to the region that functions as the source or drain region, and maintain the conductivity (low resistance state) before microwave plasma treatment. This suppresses variations in the electrical properties of the transistor and prevents variations in the electrical properties of the transistor within the substrate surface.

[0445] Furthermore, by performing microwave plasma treatment to modify the film quality of the insulator 250, the diffusion of hydrogen, water, impurities, etc., can be suppressed. Therefore, in subsequent processes such as deposition of a conductive film to become the conductor 260, or post-treatment such as heat treatment, the diffusion of hydrogen, water, impurities, etc., into the oxide semiconductor 230, etc., via the insulator 250 can be suppressed. In this way, by improving the film quality of the insulator 250, the reliability of the transistor can be improved.

[0446] When the insulator 250 is formed into a laminated structure of insulators 250a to 250d, it is preferable to perform microwave plasma treatment after the deposition of insulator 250b. Furthermore, microwave plasma treatment may be performed again after the deposition of insulator 250c. Thus, microwave plasma treatment in an oxygen-containing atmosphere may be performed multiple times (at least twice). In addition, the above microwave plasma treatment may also serve as a heat treatment for the oxide semiconductor film 230f. Therefore, the above microwave plasma treatment may cause the crystalline region of the oxide semiconductor 230 to grow.

[0447] Alternatively, a heat treatment may be performed while maintaining a reduced pressure state after microwave plasma treatment. By performing such treatment, hydrogen in the insulating film and oxide semiconductor 230 can be efficiently removed. Alternatively, the step of performing a heat treatment while maintaining a reduced pressure state after microwave plasma treatment may be repeated multiple times. By repeating the heat treatment, hydrogen in the insulating film and oxide semiconductor 230 can be removed even more efficiently. The heat treatment temperature is preferably 300°C to 500°C. Furthermore, the above heat treatment can also serve as a heat treatment for the oxide semiconductor film 230f. Therefore, the crystalline region of the oxide semiconductor 230 may grow as a result of the above heat treatment.

[0448] Next, a conductive film 260A, which will become the conductor 260, is deposited (see Figures 21A to 21D). The conductive film 260A is deposited so as to fill the openings 201 formed in the insulator 280 or the like. The conductive film 260A can be deposited using, for example, sputtering, CVD, MBE, PLD, plating, or ALD. For example, as shown in Figure 2A, when a laminated structure of conductor 260a and conductor 260b is formed, titanium nitride can be deposited as the conductive film that will become conductor 260a using the ALD method. Furthermore, tungsten can be deposited as the conductive film that will become conductor 260b using the CVD method. Note that the deposition of the conductive film 260A may be carried out while heating the substrate. Heating the substrate can also serve as a heat treatment for the oxide semiconductor film 230f mentioned above. Therefore, the crystalline region of the oxide semiconductor 230 may grow due to the above substrate heating.

[0449] The conductive film that will become the conductor 260a can be formed by thermal ALD using an inorganic precursor, without using a hydrogen-containing gas. For example, TiCl 4 In this case, NH can be used as the nitride agent. 3 A gas can be used. By forming the film using the method described above, the conductor 260a can be made into a conductive film with a low hydrogen concentration as described above. Therefore, these conductive films can act as a hydrogen source, preventing hydrogen from diffusing into the oxide semiconductor.

[0450] Here, the conductor 260a overlaps with the oxide semiconductor 230 via a thin insulator 250, and is close to the channel formation region of the oxide semiconductor 230. Therefore, if a hydrogen-containing treatment is performed during the film formation process of the conductor 260a, hydrogen will easily diffuse into the channel formation region of the oxide semiconductor 230. For this reason, it is preferable to make the conductor 260a a conductive film with a low hydrogen concentration, as described above.

[0451] Next, the insulating film 250A and the conductive film 260A are polished by CMP processing until the insulator 280 is exposed. In other words, the portions of the insulating film 250A and the conductive film 260A that are exposed from the opening 201 are removed. As a result, the insulator 250 and the conductor 260 (conductor 260a and conductor 260b) are formed inside the opening 201 (see Figures 22A to 22D). As shown in Figures 22A and 22D, the insulator 250 and the conductor 260 are formed on the A5 side (transistor 200_1 side) and the A6 side (transistor 200_2 side), respectively.

[0452] As a result, the insulator 250 is provided in contact with the insulator 255, conductor 242a1, conductor 242b1, oxide semiconductor 230, insulator 224, and insulator 222 within the opening 201. The conductor 260 is provided so as to fill the opening 201 via the insulator 250. In this way, transistors 200_1 and 200_2 are formed.

[0453] Next, an insulator 282 is formed on the insulator 255, the insulator 250, the conductor 260, and the insulator 280 (see Figures 1A to 1D). The insulator 282 can be deposited using, for example, sputtering, CVD, MBE, PLD, or ALD. It is preferable to deposit the insulator 282 using the sputtering method. By using a sputtering method that does not require the use of hydrogen-containing molecules in the deposition gas, the hydrogen concentration in the insulator 282 can be reduced.

[0454] Here, by using the sputtering method to deposit the insulator 282 in an oxygen-containing atmosphere, oxygen can be added to the insulator 280 while the film is being deposited. This allows the insulator 280 to contain excess oxygen. At this time, it is preferable to deposit the insulator 282 while heating the substrate.

[0455] Furthermore, the insulator 282 can also be made into a laminated structure. In this case, it is preferable to make the lower layer a thin aluminum oxide film deposited by the ALD method and the upper layer a thick aluminum oxide film deposited by the sputtering method. By depositing an aluminum oxide film on top of the thin aluminum oxide film using the sputtering method in this way, the amount of oxygen injected into the insulator 280 can be controlled. This makes it possible to supply a sufficient amount of oxygen to the oxide semiconductor 230 while preventing an excessive amount of oxygen from being supplied to the oxide semiconductor 230.

[0456] Next, an insulator 283 is formed on the insulator 282. The insulator 283 can be deposited using sputtering, CVD, MBE, PLD, or ALD. It is preferable to deposit the insulator 283 using sputtering. By using a sputtering method that does not require the use of hydrogen-containing molecules in the deposition gas, the hydrogen concentration in the insulator 283 can be reduced. In this embodiment, silicon nitride is deposited as the insulator 283 using sputtering.

[0457] In this embodiment, silicon nitride is deposited as the insulator 283, and aluminum oxide is deposited as the insulator 282. By using silicon nitride, which has the function of suppressing hydrogen diffusion, as the insulator 283, it is possible to suppress the diffusion of hydrogen from the upper layer of transistors 200_1 and 200_2 to the oxide semiconductor 230. Furthermore, by using aluminum oxide, which has the function of capturing or fixing hydrogen, as the insulator 282, hydrogen contained in the insulator 280 and the like can be captured or fixed to the insulator 282. As a result, the hydrogen concentration in and near the oxide semiconductor 230 can be reduced.

[0458] Next, an insulator 285 is formed on the insulator 283 (see Figures 20A to 20D). The insulator 285 can be deposited using sputtering, CVD, MBE, PLD, or ALD. It is preferable to deposit the insulator 285 using sputtering. By using a sputtering method that does not require the use of hydrogen-containing molecules in the deposition gas, the hydrogen concentration in the insulator 285 can be reduced. In this embodiment, silicon oxide is deposited as the insulator 285 using sputtering.

[0459] Here, it is preferable to deposit the insulators 282, 283, and 285 continuously by sputtering without exposing them to the atmospheric environment. By depositing the films without exposure to the atmosphere, it is possible to prevent impurities or moisture from the atmospheric environment from adhering to the insulators 282, 283, and 285, and to keep the interface or vicinity of the interface between insulator 282 and insulator 283, and the interface or vicinity of the interface between insulator 283 and insulator 285 clean.

[0460] Next, openings reaching the conductor 242a and openings reaching the conductor 242b are formed in insulators 275, 280, 282, 283, and 285 (see Figures 1A to 1D). These openings may be formed using lithography. It is preferable to process the workpiece using a dry etching method when forming these openings. Dry etching is suitable for forming openings with a high aspect ratio because it allows for anisotropic etching. When performing anisotropic etching, it is preferable to perform reactive ion etching, for example. The conditions for the dry etching method and the dry etching apparatus can be found in the description above. In Figure 1A, the shape of the opening is shown as a rectangle in plan view, but it is not limited to this. For example, the opening may be circular, an ellipse or other approximate circular shape, a rectangle or other polygon, or a rectangle or other polygon with rounded corners in plan view.

[0461] Next, after the formation of the openings, a heat treatment may be performed. The temperature of the heat treatment can be 100°C to 600°C, preferably 250°C to 550°C, and more preferably 350°C to 450°C. The heat treatment is preferably performed in an atmosphere of nitrogen gas or an inert gas. Furthermore, since the heat treatment is performed with the conductors 242a and 242b exposed, it is preferable to perform it in an atmosphere that does not contain oxidizing gases or oxygen gas. For example, it is preferable to perform a heat treatment in a nitrogen gas atmosphere at a temperature of 400°C for 1 hour. The heat treatment may also be performed under reduced pressure. The heat treatment allows oxygen contained in the insulator 280 to be supplied to the oxide semiconductor 230 via the insulator 250. This reduces oxygen vacancies in the channel formation region of the oxide semiconductor 230. In addition, the heat treatment can also serve as a heat treatment for the oxide semiconductor film 230f. Therefore, the crystalline region of the oxide semiconductor 230 may grow as a result of the heat treatment.

[0462] Here, since the side surface of the insulator 280 is exposed at the opening, the amount of oxygen contained in the insulator 280 can be controlled by the heat treatment by diffusing the oxygen contained in the insulator 280 outward. On the other hand, since insulators 282 and 283, which have barrier properties against oxygen, are provided on top of the insulator 280, oxygen does not diffuse outward from the upper surface of the insulator 280. This prevents excessive oxygen from diffusing outward from the insulator 280 and prevents the formation of oxygen vacancies in the insulator 280. In addition, the oxide semiconductor 230, conductor 242a and conductor 242b are covered by the insulator 275. This prevents an excessive amount of oxygen from directly diffusing from the insulator 280 to the oxide semiconductor 230, conductor 242a and conductor 242b during the heat treatment.

[0463] In this way, the amount of oxygen in the insulator 280 can be more favorably adjusted, and a suitable amount of oxygen can be supplied to the oxide semiconductor 230. This reduces oxygen deficiency in the oxide semiconductor 230 and prevents an excessive amount of oxygen from being supplied to the oxide semiconductor 230. Therefore, the electrical characteristics and reliability of transistors 200_1 and 200_2 can be improved. Furthermore, since the step of exposing the side surface of the insulator 280 can be combined with the step of forming the openings for embedding the conductors 240a and 240b, the manufacturing process of the semiconductor device can be simplified.

[0464] Next, an insulating film to become the insulator 241 is formed, and the insulating film is anisotropically etched to form an insulator 241a at the openings reaching the conductor 242a, and an insulator 241b at the openings reaching the conductor 242b (see Figures 1A to 1D). The insulating film to become the insulator 241 can be formed using sputtering, CVD, MBE, PLD, or ALD methods. It is preferable to use an insulating film that has the function of suppressing oxygen permeation as the insulating film to become the insulator 241. For example, it is preferable to form silicon nitride using the PEALD method. Silicon nitride is preferred because it has high barrier properties against hydrogen.

[0465] Furthermore, for the anisotropic etching of the insulating film that will become the insulator 241, a dry etching method, for example, can be used. By providing the insulator 241 on the side walls of the opening, the permeation of oxygen from the outside can be suppressed, and oxidation of the conductors 240a and 240b that will be formed next can be prevented. In addition, impurities such as water and hydrogen contained in the insulator 280 can be prevented from diffusing into the conductors 240a and 240b. Note that, as a result of this anisotropic etching, recesses may be formed on a part of the upper surface of the conductors 242a and 242b.

[0466] Next, conductive films that will become conductors 240a and 240b are formed. It is desirable that the conductive films that will become conductors 240a and 240b have a laminated structure containing a conductor that has the function of suppressing the permeation of impurities such as water and hydrogen. For example, a laminate of tantalum nitride, titanium nitride, etc., and tungsten, molybdenum, copper, etc. can be formed. The conductive films that will become conductors 240a and 240b can be formed using sputtering, CVD, MBE, PLD, or ALD methods.

[0467] Next, by performing CMP processing, a portion of the conductive film that will become conductors 240a and 240b is removed, exposing the upper surface of the insulator 283. As a result, the conductive film remains only in the openings, making it possible to form conductors 240a and 240b with flat upper surfaces (see Figures 4A to 4D). Here, it is preferable that the conductor 240b is formed overlapping the metal oxide layer 235. As shown in Figures 4A and 4D, the conductor 240a is formed on the A5 side (transistor 200_1 side) and the A6 side (transistor 200_2 side), respectively. In addition, a portion of the upper surface of the insulator 283 may be removed by this CMP processing.

[0468] As described above, by providing a conductor 240a in contact with conductor 242a, the conductor 240a, which functions as one of the source and drain of transistors 200_1 and 200_2, can be electrically connected to the wiring. Furthermore, by providing a conductor 240b in contact with conductor 242b, the conductor 240b, which functions as the other of the source and drain of transistors 200_1 and 200_2, can be electrically connected to the wiring.

[0469] Furthermore, conductive films that function as wiring or conductive films that function as plugs can be formed on the conductors 240a and 240b.

[0470] Based on the above, the semiconductor devices shown in Figures 4A to 4D can be fabricated. Furthermore, the semiconductor devices shown in Figures 1A to 1D can be fabricated using the same method.

[0471] The semiconductor device according to this embodiment has an OS transistor. In this embodiment, by using a single-crystal indium oxide or a highly crystalline indium oxide as the oxide semiconductor layer of the OS transistor, a semiconductor device with high field-effect mobility can be provided. Furthermore, the electrical characteristics, on-current, S-value (Subthreshold swing value), and frequency characteristics of the transistor can be improved. In addition, a highly reliable semiconductor device can be provided.

[0472] This embodiment can be combined with other embodiments as appropriate. Furthermore, if multiple configuration examples are shown within a single embodiment in this specification, these configuration examples can be combined as appropriate.

[0473] (Embodiment 2) This embodiment describes an indium oxide film that can be used in the semiconductor layer of a transistor in a semiconductor device according to one aspect of the present invention.

[0474] In this specification, indium oxide having at least a crystalline portion or crystalline region in the film is referred to as crystalline indium oxide (crystal IO) or crystalline indium oxide (crystalline IO). Examples of crystal IO or crystalline IO include single-crystal indium oxide, polycrystalline indium oxide, and microcrystalline indium oxide.

[0475] Indium oxide is a semiconductor material with completely different physical properties from oxide semiconductors such as In-Ga-Zn oxide (hereinafter also referred to as IGZO) and zinc oxide.

[0476] This paper describes the carrier concentration dependence of the hole mobility of indium oxide, silicon, and IGZO.

[0477] IGZO tends to exhibit higher hole mobility as the carrier concentration increases. On the other hand, single-crystal indium oxide tends to exhibit higher hole mobility as the carrier concentration decreases. This trend is similar to that of silicon, where lower dopant (impurity) concentrations in the material reduce impurity scattering and increase hole mobility. In other words, the higher the purity and intrinsic nature of single-crystal indium oxide, the higher its hole mobility. From these results, it can be said that single-crystal indium oxide, unlike IGZO, is a material with physical properties similar to silicon. Note that when indium oxide is not single-crystal (e.g., polycrystalline), the trend may differ from that of single-crystal indium oxide.

[0478] The range of carrier concentrations suitable for the channel formation region of a transistor is 1 × 10⁻⁶. 15 cm −3 This range includes, for example, 1 × 10 14 cm −3 The above is 1 x 10 18 cm −3 The range is as follows: By sufficiently reducing the carrier concentration, the hole mobility value can be increased to 270 cm⁻¹. 2 It can be expected to be raised to the level of / (V・s).

[0479] Indium oxide can contain elements that lower the carrier concentration. Examples of elements that lower the carrier concentration include magnesium, calcium, zinc, cadmium, and copper. These elements can lower the carrier concentration by substituting for indium. Other examples include nitrogen, phosphorus, arsenic, and antimony. These elements can lower the carrier concentration by substituting for oxygen.

[0480] Elements that reduce carrier concentration can also be called elements that confer p-type properties. Adding elements that reduce carrier concentration to an indium oxide film can make the indium oxide film i-type or substantially i-type. In this case, the concentration of the above-mentioned carrier-reducing element in the indium oxide film is 1 × 10⁻⁶. 16 atoms / cm 3 The above 8 x 10 20 atoms / cm 3 The following is preferable: 1 × 10 16atoms / cm 3 The above 4 x 10 20 atoms / cm 3 The following is more preferable: 1 × 10 16 atoms / cm 3 The above 8 x 10 19 atoms / cm 3 The following is more preferable: 1 × 10 16 atoms / cm 3 The above 5 x 10 19 atoms / cm 3 The following is even more preferable. By using such concentrations, the carrier concentration can be reduced while maintaining the crystal structure of indium oxide.

[0481] On the other hand, electrical resistance can be reduced by increasing the carrier concentration. For example, the suitable carrier concentration range for the source and drain regions of a transistor, or for a resistor or transparent conductive film, is when the carrier concentration value is 1 × 10⁻⁶ 20 cm −3 This range includes, for example, 1 × 10 19 cm −3 The above is 1 x 10 22 cm −3 The range is as follows: By making the carrier concentration sufficiently high, the resistivity can be increased to 1 × 10⁻⁶. −4 It is expected that the level can be reduced to below Ω·cm.

[0482] Indium oxide may contain elements that increase the carrier concentration. For example, it is preferable to include elements common to the source and drain electrodes of the transistor. Examples of elements that increase the carrier concentration include titanium, zirconium, hafnium, tantalum, tungsten, molybdenum, tin, silicon, and boron. In particular, it is more preferable to use elements in which the oxide is conductive or semiconducting.

[0483] Elements that increase carrier concentration can also be called elements that confer n-type properties. The concentration of the above-mentioned carrier-increasing elements in an indium oxide film is 1 × 10⁻⁶ 16 atoms / cm 3 The above 8 x 10 20 atoms / cm 3 The following is preferable: 1 × 10 16atoms / cm 3 The above 4 x 10 20 atoms / cm 3 The following is more preferable: 1 × 10 16 atoms / cm 3 The above 8 x 10 19 atoms / cm 3 The following is more preferable: 1 × 10 16 atoms / cm 3 The above 5 x 10 19 atoms / cm 3 The following is even more preferable. By using such concentrations, the carrier concentration can be increased while maintaining the crystal structure of indium oxide. Antimony can also function as an element that increases the carrier concentration.

[0484] Because indium oxide is an oxide whose valence electrons can be controlled, the threshold voltage of a transistor using a semiconductor layer containing indium oxide can be controlled. Furthermore, regions with low carrier concentration can be used for the transistor's channel formation region, while regions with high carrier concentration can be used for the transistor's source and drain regions. This makes it possible to create a so-called n-i-n junction (a junction between an n-type region, an i-type region, and an n-type region). Valence electron control in transistors using silicon is generally known. On the other hand, valence electron control in transistors using indium oxide is a novel technological concept that would not normally be conceived. By using this technological concept, it is possible to realize a transistor with high mobility, low off-current, normally-off capability, and high reliability.

[0485] The indium oxide film is preferably crystalline. In particular, the indium oxide film is preferably polycrystalline, and more preferably single-crystal. A single-crystal film does not have grain boundaries. By using a single-crystal film, carrier scattering at grain boundaries can be suppressed, enabling the realization of transistors that exhibit high field-effect mobility. Furthermore, it has the excellent effect of suppressing variations in transistor characteristics caused by these grain boundaries.

[0486] Furthermore, polycrystalline films are preferable because they can reduce carrier scattering and exhibit high field-effect mobility compared to microcrystalline or amorphous films. When using polycrystalline films, it is preferable to use films with the largest possible grain size and few grain boundaries. In a transistor to which a polycrystalline film is applied, if there are no grain boundaries in the channel formation region, or if no grain boundaries are observed, the channel formation region is located within the single-crystal region contained in the polycrystalline film, and therefore it can be considered a transistor to which a single-crystal film is applied.

[0487] The crystallinity of indium oxide can be analyzed, for example, by X-ray diffraction (XRD), transmission electron microscopy (TEM), or electron diffraction (ED). Alternatively, a combination of these methods may be used for analysis.

[0488] Furthermore, in this specification, a semiconductor layer in which no grain boundaries are observed in the channel formation region, a semiconductor layer in which the channel formation region is contained within a single crystal grain, or a semiconductor layer in which the crystal axis directions are the same in at least two regions within the channel formation region can be considered as a single crystal film.

[0489] Impurities in the indium oxide film can act as a source of carrier scattering, thus potentially causing a decrease in field-effect mobility and inhibiting crystal growth. Examples of impurities in the indium oxide film include boron and silicon. In the channel-forming region of the indium oxide film, lower concentrations of these impurities are preferable. For example, the concentration of each of the above impurity elements should be 0.1% or less, more preferably 0.01% (100 ppm) or less. Note that elements such as carbon and hydrogen may be present in the deposition gas or precursor during film formation, and may remain in the indium oxide film in higher concentrations than the above impurities.

[0490] Furthermore, the indium oxide film may contain elements that can become trivalent cations like indium, as long as their crystals maintain a cubic crystal structure (Bixbite type). Examples include Group 13 elements of the periodic table such as gallium and aluminum, and Group 3 elements of the periodic table. Since the bonding force of these elements is stronger than that of indium and oxygen, adding these elements to the indium oxide film can reduce oxygen vacancies (V) in the indium oxide film. O This can suppress the formation of ions. Furthermore, since these elements mainly exist as trivalent cations in the oxide, the carrier concentration of the indium oxide film can be kept low. Therefore, it becomes possible to shift the threshold voltage of the transistor to the positive side. Also, normally-off operation becomes possible. Thus, a transistor with good electrical characteristics can be provided.

[0491] The concentration of the above elements in the indium oxide film is 1 × 10⁻⁶ 16 atoms / cm 3 The above 8 x 10 20 atoms / cm 3 The following is preferable: 1 × 10 16 atoms / cm 3 The above 4 x 10 20 atoms / cm 3 The following is more preferable: 1 × 10 16 atoms / cm 3 The above 8 x 10 19 atoms / cm 3 The following is more preferable: 1 × 10 16 atoms / cm 3 The above 5 x 10 19 atoms / cm 3 The following are even more preferable.

[0492] Furthermore, the elements that impart n-type, p-type, and trivalent cations mentioned above can be added to the indium oxide film by methods such as ion doping, ion implantation, and thermal diffusion. Alternatively, the elements that impart n-type, p-type, and trivalent cations mentioned above can be added to the sputtering target, deposition gas, ALD deposition precursor, etc., when depositing the indium oxide film. Alternatively, the elements that impart n-type, p-type, and trivalent cations mentioned above can be auto-doped from the chamber used when depositing the indium oxide film. Auto-doping refers to the automatic addition of elements contained in the chamber components, etc., into the indium oxide film during deposition.

[0493] By using such an indium oxide film in a transistor, the field-effect mobility of the transistor can be increased to 50 cm². 2 / (V·s) or more, preferably 100 cm 2 / (V·s) or more, more preferably 150 cm 2 / (V·s) or more, more preferably 200 cm 2 / (V·s) or more, more preferably 250 cm 2 It can be set to (V・s) or more.

[0494] One of the characteristics of indium oxide films is their higher oxygen permeability (diffusivity) compared to IGZO films. For example, oxygen diffusing into an indium oxide film permeates the film and is released as oxygen molecules. In some cases, it may also be released as water molecules by reacting with hydrogen contained in the film. Furthermore, if there is an oxygen deficiency in the film, diffusing oxygen atoms will fill the deficiency. Because oxygen diffuses easily through indium oxide films, it can be said that oxygen deficiencies are more easily filled in compared to IGZO films.

[0495] Thus, because indium oxide films are more likely to reduce oxygen vacancies in the film compared to IGZO films, applying such indium oxide films to transistors makes it possible to realize transistors with extremely high reliability.

[0496] Furthermore, the indium oxide film diffuses hydrogen. Hydrogen diffusing into the indium oxide film from the outside permeates the film and is released as hydrogen molecules. Alternatively, it reacts with oxygen contained in the film and is released as water molecules.

[0497] Indium oxide is characterized by a small effective electron mass and a large effective hole mass. Furthermore, the effective electron mass of indium oxide is largely independent of the crystal orientation. Therefore, using crystalline indium oxide in transistors allows for the realization of transistors with high field-effect mobility and high frequency characteristics (also known as f-response). Moreover, due to the large effective hole mass, transistors with extremely low off-currents can be realized. For example, by applying an indium oxide film to a vertical transistor, the off-current per 1 μm of channel width is 1 fA (1 × 10⁻¹⁶) at 125°C. −15 A) Less than or equal to, or 1aA (1 × 10 −18 A) is less than or equal to 1aA (1 × 10) under room temperature (25°C) conditions. −18 A) Less than or equal to, or 1zA (1 × 10⁻¹⁰ −21 A) The following is possible. Furthermore, because indium oxide has a smaller effective electron mass and a larger effective hole mass than silicon, it may be possible to realize transistors with higher field-effect mobility and lower off-current than Si transistors.

[0498] It is preferable to provide a seed layer so as to be in contact with at least a portion of the crystalline indium oxide film. It is preferable to use a material containing crystals with a small difference in lattice constant (also called lattice mismatch) with the indium oxide for the seed layer. This improves the crystallinity of the indium oxide film. A substrate (e.g., a single-crystal substrate) may be used as one of the layers in contact with at least a portion of the crystalline indium oxide film.

[0499] One method for evaluating the degree of lattice mismatch is to use the following lattice mismatch value. The lattice mismatch Δa [%] of the crystals in the formed film (in this case, the indium oxide film) relative to the crystals in the seed layer is given by Δa = ((L1 -L 2 ) / L 2 It is calculated as ) × 100. Here L 1 L is the length of the unit cell vector of the crystals in the formed film, or the lattice constant. 2 This is the length of the unit cell vector of the crystal in the seed layer, or the lattice constant.

[0500] The lattice mismatch Δa between the seed layer and the indium oxide film is preferably small in absolute value, and most preferably zero. For example, Δa can be -5% or more and 5% or less, preferably -4% or more and 4% or less, more preferably -3% or more and 3% or less, and even more preferably -2% or more and 2% or less.

[0501] Here, the indium oxide crystal has a cubic structure (bixbite type). For example, yttria-stabilized zirconia (YSZ) crystals can have a cubic structure (fluorite type). The lattice mismatch of the indium oxide crystal with respect to the cubic YSZ crystal is in the range of -2% to 2%, and a single crystal film of indium oxide can be epitaxially grown on a YSZ substrate.

[0502] Furthermore, the crystal structure of the seed layer and the crystal structure of the indium oxide film do not necessarily have to be the same in terms of crystal system or crystal orientation. For example, a film with a hexagonal or trigonal crystal structure can be used beneath an indium oxide film with a cubic crystal structure. For example, by setting the crystal orientation of the surface of the seed layer to

[001] and the crystal orientation of the underside of the indium oxide film to

[111] , the requirements related to crystal orientation necessary for epitaxial growth can be met. Examples of hexagonal or trigonal crystals include wurtzite-type structures and YbFe. 2 O 4 Type structure, Yb 2 Fe 3 O 7 These include type structures and their modified type structures. YbFe 2 O 4 Type structure or Yb 2 Fe 3 O 7 An example of a crystal having a type structure is IGZO.

[0503] This embodiment can be implemented in appropriate combination with other embodiments described herein, at least in part.

[0504] (Embodiment 3) In this embodiment, a semiconductor device 900 according to one aspect of the present invention will be described. The semiconductor device 900 can function as a memory device.

[0505] Figure 23 shows a block diagram illustrating an example configuration of a semiconductor device 900. The semiconductor device 900 shown in Figure 23 includes a drive circuit 910 and a memory array 920. The memory array 920 has one or more memory cells 950. Figure 23 shows an example in which the memory array 920 has multiple memory cells 950 arranged in a matrix.

[0506] The transistor exemplified in Embodiment 1 can be applied to the memory cell 950. By using the above transistor, the operating speed of the memory device can be improved. Furthermore, miniaturization and high integration of the memory device can be achieved. In addition, the capacity per unit area of ​​the memory device can be increased.

[0507] The drive circuit 910 includes a PSW 931 (power switch), a PSW 932, and a peripheral circuit 915. The peripheral circuit 915 includes a peripheral circuit 911, a control circuit 912 (Control Circuit), and a voltage generation circuit 928.

[0508] In the semiconductor device 900, each circuit, each signal, and each voltage can be appropriately selected or omitted as needed. Alternatively, other circuits or other signals may be added. Signals BW, CE, GW, CLK, WAKE, ADDR, WDA, PON1, and PON2 are external input signals, and signal RDA is an external output signal. Signal CLK is a clock signal.

[0509] Furthermore, signals BW, CE, and GW are control signals. Signal CE is the chip enable signal, signal GW is the global write enable signal, and signal BW is the byte write enable signal. Signal ADDR is the address signal. Signal WDA is the write data signal, and signal RDA is the read data signal. Signals PON1 and PON2 are power gating control signals. Signals PON1 and PON2 may be generated by the control circuit 912.

[0510] The control circuit 912 is a logic circuit that has the function of controlling the overall operation of the semiconductor device 900. For example, the control circuit 912 performs logical operations on signals CE, GW, and BW to determine the operating mode of the semiconductor device 900 (e.g., write operation, read operation). Alternatively, the control circuit 912 generates control signals for the peripheral circuit 911 so that this operating mode is executed.

[0511] The voltage generation circuit 928 has the function of generating voltage. The signal WAKE has the function of controlling the input of the signal CLK to the voltage generation circuit 928. For example, when a high-level signal is given as the signal WAKE, the signal CLK is input to the voltage generation circuit 928, and the voltage generation circuit 928 generates voltage.

[0512] The peripheral circuit 911 is a circuit for writing and reading data to and from the memory cell 950. The peripheral circuit 911 includes a row decoder 941, a column decoder 942, a row driver 923, a column driver 924, an input circuit 925, an output circuit 926, and a sense amplifier 927.

[0513] The row decoder 941 and column decoder 942 have the function of decoding the ADDR signal. The row decoder 941 is a circuit for specifying the row to access, and the column decoder 942 is a circuit for specifying the column to access. The row driver 923 has the function of selecting the row specified by the row decoder 941. The column driver 924 has the function of writing data to the memory cell 950, reading data from the memory cell 950, and holding the read data.

[0514] The input circuit 925 has the function of holding the signal WDA. The data held by the input circuit 925 is output to the column driver 924. The output data of the input circuit 925 is the data (Din) to be written to the memory cell 950. The data (Dout) read by the column driver 924 from the memory cell 950 is output to the output circuit 926. The output circuit 926 has the function of holding Dout. The output circuit 926 also has the function of outputting Dout to the outside of the semiconductor device 900. The data output from the output circuit 926 is the signal RDA.

[0515] PSW931 provides V to peripheral circuit 915 DD It has the function of controlling the supply. PSW932 has the function of V to line driver 923 HM It has a function to control the supply. Here, the high power supply potential of the semiconductor device 900 is V DD Therefore, the low power supply potential is GND (ground potential). Also, V HM This is a high power supply potential used to raise the word line to a high level, V DD It is higher than that. The on / off state of PSW931 is controlled by signal PON1, and the on / off state of PSW932 is controlled by signal PON2. In Figure 23, in peripheral circuit 915, V DD The number of power domains supplied is set to one, but it can be multiple. In this case, a power switch should be provided for each power domain.

[0516] Using Figures 24A to 24H, other examples of memory cell configurations applicable to the memory cell 950 will be described.

[0517] [DOSRAM] Figure 24A shows an example of the circuit configuration of a DRAM memory cell. In this specification, a DRAM using an OS transistor is called a DOSRAM (Dynamic Oxide Semiconductor Random Access Memory). The DOSRAM shown in Figure 24A has a memory cell 951a and a memory cell 951b. The memory cell 951a has a transistor M1a and a capacitive element CAa, and the memory cell 951b has a transistor M1b and a capacitive element CAb.

[0518] Transistors M1a and M1b may have a front gate (sometimes simply called a gate) and a back gate. In this case, the back gate may be connected to a wire to which a constant potential or signal is supplied. Alternatively, the front gate and the back gate may be connected.

[0519] The first terminal of transistor M1a is connected to the first terminal of capacitive element CAa, the second terminal of transistor M1a is connected to wiring BIL, and the gate of transistor M1a is connected to wiring WOLa. The second terminal of capacitive element CAa is connected to wiring CAL.

[0520] The first terminal of transistor M1b is connected to the first terminal of capacitive element CAb, the second terminal of transistor M1b is connected to wiring BIL, and the gate of transistor M1b is connected to wiring WOLb. The second terminal of capacitive element CAb is connected to wiring CAL.

[0521] Wiring BIL functions as a bit line, and wiring WOLa and WOLb function as word lines. Wiring CAL functions as wiring for applying a predetermined potential to the second terminals of capacitive elements CAa and CAb. When writing and...

Claims

It comprises a metal oxide layer, an oxide semiconductor, a first to third insulator, and a first to third conductor. The metal oxide layer is in contact with the upper and side surfaces of the first insulator. The oxide semiconductor covers the first insulator and the metal oxide layer. The first conductor and the second conductor are arranged on the oxide semiconductor. The second insulator is disposed on the first conductor and the second conductor and has an opening that overlaps with the region between the first conductor and the second conductor. The third insulator is disposed on the oxide semiconductor at the opening. The third conductor is placed on the third insulator in the opening. In a cross-sectional view in the channel width direction, the height of the first insulator is greater than the width of the first insulator. The metal oxide layer is superimposed on the first conductor, The metal oxide layer contains indium and has crystals. The oxide semiconductor contains indium and has a cubic crystal structure. Semiconductor equipment.   It comprises a metal oxide layer, an oxide semiconductor, first to fourth insulators, and first to third conductors. The first insulator is placed on the fourth insulator. The metal oxide layer is in contact with the upper and side surfaces of the first insulator. The oxide semiconductor is disposed on the fourth insulator and covers the first insulator and the metal oxide layer. The first conductor and the second conductor are arranged on the oxide semiconductor. The second insulator is disposed on the first conductor and the second conductor and has an opening that overlaps with the region between the first conductor and the second conductor. The third insulator is disposed on the oxide semiconductor at the opening. The third conductor is placed on the third insulator in the opening. In a cross-sectional view in the channel width direction, the height of the first insulator is greater than the width of the first insulator. The metal oxide layer is superimposed on the first conductor, The metal oxide layer contains indium and has crystals. The oxide semiconductor contains indium and has a cubic crystal structure. Semiconductor equipment.   In claim 2, The side surface of the fourth insulator coincides with or substantially coincides with the side surface of the metal oxide layer, the side surface of the oxide semiconductor, the side surface of the first conductor, and the side surface of the second conductor in a plan view. The thickness of the first insulator is greater than the thickness of the third insulator. Semiconductor equipment.   In claim 3, The lower surface of the third conductor has a portion located below the lower surface of the oxide semiconductor. Semiconductor equipment.   It comprises a metal oxide layer, an oxide semiconductor, first to fifth insulators, and first to third conductors. The first insulator is placed on the fourth insulator. The metal oxide layer is in contact with the upper and side surfaces of the first insulator. The oxide semiconductor is disposed on the fourth insulator and covers the first insulator and the metal oxide layer. The first conductor and the second conductor are arranged on the oxide semiconductor. The second insulator is disposed on the first conductor and the second conductor and has an opening that overlaps with the region between the first conductor and the second conductor. The third insulator is disposed on the oxide semiconductor at the opening. The third conductor is placed on the third insulator in the opening. The first conductor and the second conductor each have a first conductive layer and a second conductive layer on the first conductive layer. The fifth insulator is positioned in the opening of the second insulator and is in contact with the upper surface of the first conductive layer of the first conductor, the side surface of the second conductive layer of the first conductor, the upper surface of the first conductive layer of the second conductor, and the side surface of the second conductive layer of the second conductor. The shortest distance between the first conductive layer of the first conductor and the first conductive layer of the second conductor is smaller than the shortest distance between the second conductive layer of the first conductor and the second conductive layer of the second conductor. In a cross-sectional view in the channel width direction, the height of the first insulator is greater than the width of the first insulator. The metal oxide layer is superimposed on the first conductor, The metal oxide layer contains indium and has crystals. The oxide semiconductor contains indium and has a cubic crystal structure. Semiconductor equipment.   In claim 5, A portion of the side surface of the second insulator coincides with or substantially coincides with the side surface of the second conductive layer of the first conductor and the side surface of the second conductive layer of the second conductor in a plan view. Semiconductor equipment.   In claim 5, The fifth insulator has silicon nitride, Semiconductor equipment.   In claim 5, The first conductive layer of the first conductor and the first conductive layer of the second conductor each contain indium and tin, respectively. Semiconductor equipment.   In any one of claims 1 to 8, The metal oxide layer does not overlap with the second conductor and the third conductor. Semiconductor equipment.   In any one of claims 1 to 8, The direction in which the metal oxide layer extends is parallel to the direction in which the third conductor extends. Semiconductor equipment.   In claim 9, The metal oxide layer has a cubic crystal structure. Semiconductor equipment.   In claim 9, The metal oxide layer comprises indium, gallium, and zinc, and has a hexagonal or trigonal crystal structure. Semiconductor equipment.   In claim 9, The first insulator has gallium oxide, aluminum oxide, or silicon oxide. Semiconductor equipment.