Display apparatus

The display device integrates color conversion layers and light-emitting devices with specific organic compounds and a microcavity structure to achieve full-color display, enhancing efficiency and reliability while reducing costs.

WO2026234520A1PCT designated stage Publication Date: 2026-11-12SEMICON ENERGY LAB CO LTD
View PDF 0 Cites 0 Cited by

Patent Information

Application Number
PCT/IB2026/054265
Authority / Receiving Office
WO · WO
Patent Type
Applications
Current Assignee / Owner
Priority Date
2025-05-09
Filing Date
2026-04-30
Publication Date
2026-11-12

AI Technical Summary

Technical Problem

Existing display devices using organic electroluminescent elements face challenges in achieving full-color display, high luminous efficiency, reliability, long operating life, and cost-effectiveness, with a need for materials with better properties and easier synthesis methods.

Method used

A display device design incorporating a first and second color conversion layer, a first and second light-emitting device, with specific organic compounds and electrode configurations, utilizing a microcavity structure and quantum dots to enhance color conversion and light extraction efficiency.

Benefits of technology

Enables full-color display with high luminous efficiency, improved reliability, extended operating life, and reduced manufacturing costs, while minimizing power consumption.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure IB2026054265_12112026_PF_FP_ABST
    Figure IB2026054265_12112026_PF_FP_ABST
Patent Text Reader

Abstract

Provided is a display apparatus which has good characteristics. The display apparatus has a first color conversion layer, a second color conversion layer, a first light-emitting device, and a second light-emitting device. The display apparatus has the first color conversion layer on the first light-emitting device, the second color conversion layer on the second light-emitting device, and has a partition wall between the first light-emitting device and the second light-emitting device. The first light-emitting device and the second light-emitting device each have an organic compound layer between a pair of electrodes. The organic compound layer has a first light-emitting layer and a second light-emitting layer, wherein the first light-emitting layer has a fluorescent light-emitting substance and a first organic compound, and the second light-emitting layer has a phosphorescent light-emitting substance and a second organic compound. The difference between the maximum peak wavelength in the PL spectrum of the fluorescent light-emitting substance and the maximum peak wavelength in the PL spectrum of the phosphorescent light-emitting substance is 30 nm or less. The GSP_slope of a film that is formed of the first organic compound is 20 mV / nm to 100 mV / nm inclusive, and the GSP_slope of a film that is formed of the second organic compound is 20 mV / nm to 100 mV / nm inclusive.
Need to check novelty before this filing date? Find Prior Art

Description

display device

[0001] One aspect of the present invention relates to organic compounds, organic semiconductor elements, light-emitting devices, light-receiving devices, photodiode sensors, display modules, lighting modules, display devices, electronic equipment, lighting devices, and electronic devices. However, one aspect of the present invention is not limited to the above-mentioned technical fields. The technical fields of one aspect of the invention disclosed herein relate to products, methods, or methods of manufacturing. Alternatively, one aspect of the present invention relates to processes, machines, manufacturers, or compositions of matter. Therefore, more specifically, examples of the technical fields of one aspect of the present invention disclosed herein include semiconductor devices, display devices, liquid crystal display devices, lighting devices, energy storage devices, memory devices, imaging devices, methods for driving them, or methods for manufacturing them.

[0002] The practical application of organic electroluminescent devices (organic EL elements), such as light-emitting devices, light-receiving devices, and light-receiving / receiving devices, which utilize electroluminescence using organic compounds, is progressing.

[0003] The basic configuration of a light-emitting device consists of an organic compound layer (EL layer) containing a light-emitting material sandwiched between a pair of electrodes. By applying a voltage to this device, carriers are injected, and by utilizing the recombination energy of these carriers, light emission can be obtained from the light-emitting material.

[0004] For example, a functional panel is known in which pixels provided in the display area are equipped with light-emitting elements (light-emitting devices) and photoelectric conversion elements (light-receiving devices) (Patent Document 1).

[0005] While displays and lighting devices using light-emitting devices are suitable for various electronic devices, there is still room for improvement in their performance and cost competitiveness. Therefore, there is a growing demand for materials with better properties and easier handling, as well as easy synthesis methods for such materials (see, for example, Non-Patent Document 1).

[0006] Furthermore, displays using quantum dots (QDs) as a color conversion layer are beginning to become widespread. Quantum dots are semiconductor nanoparticles with a diameter of only a few nanometers. Due to the quantum size effect, the band gap can be adjusted by changing the size of the nanoparticle, allowing incident light to be converted into light of different wavelengths depending on the size of the nanoparticle. Specifically, as the size of the nanoparticle decreases, it becomes possible to convert it into light of shorter wavelengths, and as the size of the nanoparticle increases, it becomes possible to convert it into light of longer wavelengths. Displays using quantum dots as a color conversion layer utilize this property to change the size of the nanoparticles for each sub-pixel, thereby converting a light source of the same wavelength into light of different colors for each sub-pixel, enabling full-color display (see, for example, Patent Document 2).

[0007] WO2020 / 152556 Patent No. 6159302 Japanese Patent Publication No. 2020-096171

[0008] Yutaka Noguchi, et al., "Orientation Polarization Phenomena of Polar Molecules and Interface Properties of Organic Thin Film Devices," Journal of the Vacuum Society of Japan, 2015, Vol. 58, No. 3. Yutaka Noguchi, et al., "Spontaneous orientation polarization in organic light-emitting diodes," Japanese Journal of Applied Physics 58, 2019, SF0801.

[0009] One aspect of the present invention aims to provide a novel display device. Another aspect of the present invention aims to provide a display device capable of full-color display. Another aspect of the present invention aims to provide a display device with high luminous efficiency and good reliability.

[0010] One aspect of the present invention aims to provide an organic EL device with a long operating life. Another aspect of the present invention aims to provide a novel organic EL device. Another aspect of the present invention aims to reduce the manufacturing cost of an organic EL device. Another aspect of the present invention aims to provide a light-emitting device, electronic device, or lighting device with low power consumption.

[0011] Furthermore, the description of these problems does not preclude the existence of other problems. Also, one aspect of the present invention does not need to solve all of these problems. Other problems will naturally become clear from the description in the specification, drawings, claims, etc., and it is possible to extract other problems from the description in the specification, drawings, claims, etc.

[0012] One aspect of the present invention is a display device having a first color conversion layer, a second color conversion layer, a first light-emitting device, and a second light-emitting device, wherein the first color conversion layer is located on the first light-emitting device, the second color conversion layer is located on the second light-emitting device, there is a partition between the first light-emitting device and the second light-emitting device, the first light-emitting device and the second light-emitting device have an organic compound layer between a pair of electrodes, the organic compound layer has a first light-emitting layer and a second light-emitting layer, and the first light-emitting layer is firefly The material comprises a photoluminescent material and a first organic compound, the second light-emitting layer comprises a phosphorescent material and a second organic compound, the difference between the maximum peak wavelength in the PL spectrum of the fluorescent material and the maximum peak wavelength in the PL spectrum of the phosphorescent material is 30 nm or less, the GSP_slope of the film made of the first organic compound is 20 mV / nm or more and 100 mV / nm or less, and the GSP_slope of the film made of the second organic compound is 20 mV / nm or more and 100 mV / nm or less.

[0013] In the above invention, the difference between the GSP_slope of the film made of the first organic compound and the GSP_slope of the film made of the second organic compound is 10 mV / nm or less.

[0014] One aspect of the present invention is a display device having a first color conversion layer, a second color conversion layer, a first light-emitting device, and a second light-emitting device, wherein the first color conversion layer is located on the first light-emitting device, the second color conversion layer is located on the second light-emitting device, there is a partition between the first light-emitting device and the second light-emitting device, the first light-emitting device and the second light-emitting device have an organic compound layer between a pair of electrodes, the organic compound layer has a first light-emitting layer and a second light-emitting layer, the first light-emitting layer has a fluorescent material and a first organic compound, the second light-emitting layer has a phosphorescent material and a second organic compound, the difference between the maximum peak wavelength in the PL spectrum of the fluorescent material and the maximum peak wavelength in the PL spectrum of the phosphorescent material is 30 nm or less, and the difference between the GSP_slope of the film made of the first organic compound and the GSP_slope of the film made of the second organic compound is 10 mV / nm or less.

[0015] In the above invention, the lowest triplet excitation energy level of the fluorescent material is higher than the lowest triplet excitation energy level of the first organic compound, and the lowest triplet excitation energy level of the phosphorescent material is lower than the lowest triplet excitation energy level of the second organic compound.

[0016] In the above invention, the first organic compound is an organic compound having a polycyclic aromatic hydrocarbon, and the second organic compound is an organic compound having a heteroaromatic ring.

[0017] In the above invention, the second light-emitting layer has a third organic compound, the GSP_slope of the film made of the third organic compound is 20 mV / nm or more and 100 mV / nm or less, the second organic compound is an organic compound having a π-electron-deficient heteroaromatic ring, and the third organic compound is an organic compound having a π-electron-rich heteroaromatic ring.

[0018] In the above invention, the second organic compound and the third organic compound are a combination that forms an excited complex.

[0019] In the above invention, the pair of electrodes comprises a first electrode and a second electrode formed on a substrate, and the first light-emitting layer is located between the first electrode and the second light-emitting layer.

[0020] In the above invention, the pair of electrodes comprises a first electrode and a second electrode formed on a substrate, the end of the first electrode is covered with an insulator, the first electrode is electrically connected to a transistor, and the first light-emitting layer is located between the first electrode and the second light-emitting layer.

[0021] In the above invention, the first light-emitting layer and the second light-emitting layer are in contact.

[0022] In the above invention, the fluorescent material has the maximum peak of its PL spectrum in the wavelength range of 440 nm to 520 nm, and the phosphorescent material has the maximum peak of its PL spectrum in the wavelength range of 440 nm to 520 nm.

[0023] According to one aspect of the present invention, a novel display device can be provided. Furthermore, according to one aspect of the present invention, a display device capable of full-color display can be provided. Furthermore, according to one aspect of the present invention, a display device with high luminous efficiency and good reliability can be provided.

[0024] Furthermore, according to one aspect of the present invention, a novel organic EL device can be provided. Furthermore, according to one aspect of the present invention, an organic EL device with a long operating life can be provided. Furthermore, according to one aspect of the present invention, the manufacturing cost of the organic EL device can be reduced. Furthermore, according to one aspect of the present invention, a light-emitting device, electronic device, or lighting device with low power consumption can be provided.

[0025] Furthermore, the description of these effects does not preclude the existence of other effects. Moreover, one aspect of the present invention does not necessarily have to possess all of these effects. Other effects will naturally become apparent from the description in the specification, drawings, and claims, and it is possible to extract other effects from the description in the specification, drawings, and claims.

[0026] Figure 1A is a top view illustrating the configuration of the display device, and Figure 1B is a cross-sectional view illustrating the configuration of the display device. Figures 2A, 2B, and 2C are schematic diagrams of the light-emitting device. Figure 3 is a diagram showing the capacitance-voltage characteristics of the measuring device 1. Figure 4 is a diagram showing the current density-voltage characteristics of the measuring device 1. Figures 5A, 5B, 5C, 5D, and 5E are diagrams illustrating the configuration of the light-emitting device. Figures 6A, 6B, 6C, and 6D are examples of the configuration of the display device. Figure 7 is an example of a partial configuration of the display device. Figures 8A and 8B are examples of a partial configuration of the display device. Figures 9A and 9B are examples of a partial configuration of the display device. Figures 10A, 10B, 10C, 10D, 10E, 10F, 10G, 10H, and 10I are examples of the configuration of the display device. Figures 11A, 11B, 11C, 11D, 11E, and 11F illustrate examples of methods for manufacturing a display device. Figure 12 shows an example of the configuration of a display device. Figure 13 shows an example of the configuration of a display device. Figures 14A and 14B show examples of the configuration of a display device. Figures 15A, 15B, 15C, and 15D show examples of electronic equipment. Figures 16A, 16B, 16C, 16D, 16E, and 16F show examples of electronic equipment. Figures 17A, 17B, 17C, 17D, 17E, 17F, and 17G show examples of electronic equipment. Figure 18 illustrates the configuration of a light-emitting device. Figure 19 illustrates the luminance-current density characteristics of a light-emitting device. Figure 20 illustrates the luminance-voltage characteristics of a light-emitting device. Figure 21 illustrates the current efficiency-luminance characteristics of a light-emitting device. Figure 22 illustrates the current density-voltage characteristics of a light-emitting device. Figure 23 illustrates the electroluminescence spectrum of a light-emitting device. Figure 24 shows the blue index-current density characteristics of the sample. Figures 25A and 25B show the phosphorescence spectra of 3,10PCA2Nbf(IV)-02. Figures 26A and 26B show the phosphorescence spectra of Bnf(II)PhA. Figure 27 illustrates the PL spectra (room temperature) of SiTrzCz2, PSiCzCz, and mixed films of SiTrzCz2 and PSiCzCz. Figure 28 illustrates the PL spectrum (10K) of SiTrzCz2.Figure 29 illustrates the PL spectrum (10K) of a single film of PSiCzCz. Figure 30 illustrates the absorption and emission spectra of PtON-TBBI. Figure 31 illustrates the absorption and emission spectra of 3,10PCA2Nbf(IV)-02. Figure 32 illustrates the change in brightness with respect to the operating time of the light-emitting device. Figure 33 illustrates the brightness-current density characteristics of the light-emitting device. Figure 34 illustrates the brightness-voltage characteristics of the light-emitting device. Figure 35 illustrates the current efficiency-brightness characteristics of the light-emitting device. Figure 36 illustrates the current density-voltage characteristics of the light-emitting device. Figure 37 illustrates the electroluminescence spectrum of the light-emitting device. Figure 38 shows the blue index-current density characteristics of the sample. Figure 39 illustrates the change in brightness with respect to the operating time of the light-emitting device.

[0027] The embodiments of the present invention will be described in detail below with reference to the drawings. However, the present invention is not limited to the following description, and its form and details can be modified in various ways without departing from the spirit and scope of the present invention. Accordingly, the present invention should not be interpreted as being limited to the contents of the embodiments shown below.

[0028] In this specification, "deuterated organic compound" refers to an organic compound in which, when focusing on hydrogen atoms (including deuterium) at specific positions within the organic compound, the proportion of deuterium (including deuterium) is greater than the natural abundance of deuterium. This proportion is preferably sufficiently greater than the natural abundance. "Sufficiently" means, for example, that 7.5% or more is deuterated. The deuteration of an organic compound can be confirmed by methods such as NMR and mass spectrometry.

[0029] Please note that the positions, sizes, and ranges of each component shown in the drawings may not represent their actual positions, sizes, and ranges for the sake of ease of understanding. Therefore, the disclosed invention is not necessarily limited to the positions, sizes, and ranges disclosed in the drawings.

[0030] Furthermore, in this specification and other documents, when describing the structure of the invention using drawings, reference numerals that refer to the same thing will be used consistently across different drawings.

[0031] Furthermore, in this specification, terms representing "layers" or "films," such as "hole transport layer," "light-emitting layer," "insulating layer," "semiconductor layer," or "semiconductor film," may be simply referred to as "layer" or "film." Ordinal numbers may also be used. In addition, the words "film" and "layer" can be interchanged depending on the circumstances or situation. For example, "hole transport layer" can be referred to as "layer," "film," or "first layer." Similarly, anodes or cathodes may be simply referred to as "electrodes," or they may be referred to using ordinal numbers, such as "first electrode."

[0032] Furthermore, in this specification, ordinal numbers such as "first," "second," etc., are added to avoid confusion of constituent elements and do not limit the number of constituent elements or the order of constituent elements (e.g., layering order or process order). Also, even if an ordinal number is not used for a term in this specification, an ordinal number may be used in the claims to avoid confusion of constituent elements. Even if an ordinal number is used for a term in this specification, a different ordinal number may be used in the claims. Even if an ordinal number is used for a term in this specification, the ordinal number may be omitted in the claims.

[0033] (Embodiment 1) This embodiment describes a display device that is one aspect of the present invention.

[0034] A display device according to one aspect of the present invention comprises a plurality of light-emitting devices having the same light-emitting material, and a color conversion layer overlapping at least some of the light-emitting devices. By changing the presence or absence of the color conversion layer and the type of color conversion layer used depending on the sub-pixel, the display device can perform full-color display.

[0035] Figure 1A shows a top view of the display device 100. The display device 100 has a display unit on which a plurality of pixels 15 are arranged, and a connection unit 140 on the outside of the display unit. Multiple subpixels are arranged in a matrix on the display unit. In Figure 1A, subpixels in 2 rows and 6 columns are shown, and these constitute a 2 row and 2 column pixel 15. The connection unit 140 can also be called a cathode contact unit.

[0036] The top surface shape of the subpixel shown in Figure 1A corresponds to the top surface shape of the light-emitting region. In this specification, the term "top surface shape" refers to the shape in a plan view, that is, the shape viewed from above.

[0037] Note that the top surface shape of a subpixel is not limited to the shape shown in Figure 1A. Examples of top surface shapes of subpixels include polygons such as triangles, quadrilaterals (including rectangles, rhombuses, and squares), pentagons, polygons with rounded corners, ellipses, or circles.

[0038] Furthermore, the circuit layout constituting the subpixel is not limited to the subpixel range shown in Figure 1A, and the circuit components may be arranged outside of it. In other words, some or all of the transistors in the subpixel 11R shown in Figure 1A may be located outside the range of the subpixel 11R. The transistors in the subpixel 11R may be located within the range of the subpixel 11R shown in Figure 1A, within the range of the subpixel 11G, within the range of the subpixel 11B, or may be arranged across multiple of these ranges.

[0039] In Figure 1A, the aperture ratios (sizes, also known as the size of the light-emitting area) of sub-pixels 11R, 11G, and 11B are shown to be equal or approximately equal, but one aspect of the present invention is not limited thereto. The aperture ratios of sub-pixels 11R, 11G, and 11B can each be determined as appropriate. The aperture ratios of sub-pixels 11R, 11G, and 11B may be different, or two or more may be equal or approximately equal.

[0040] A stripe array is applied to the pixel 15 shown in Figure 1A. The pixel 15 shown in Figure 1A is composed of three subpixels: subpixel 11R, subpixel 11G, and subpixel 11B. Subpixels 11R, 11G, and 11B each emit light of a different color. Examples of subpixels 11R, 11G, and 11B include subpixels of three colors: red (R), green (G), and blue (B); and subpixels of three colors: yellow (Y), cyan (C), and magenta (M). Furthermore, the number of subpixel types is not limited to three; there may be four or more. Examples of four subpixels include subpixels of four colors: R, G, B, and white (W); subpixels of four colors: R, G, B, and yellow (Y); and subpixels of four colors: R, G, B, and infrared (IR).

[0041] In this specification, the row direction is sometimes referred to as the X direction, the column direction as the Y direction, and the depth direction as the Z direction. Figure 1A shows an example where subpixels of different colors are arranged in the X direction, and subpixels of the same color are arranged in the Y direction.

[0042] Figure 1B shows a cross-sectional view between the dashed lines X1 and X2 in Figure 1A. In the cross-sectional view shown in Figure 1B, the top surface of the display device 100 is shown at the bottom.

[0043] The sub-pixel 11R includes a light-emitting device 10 and a color conversion layer 12R that overlaps the light-emitting device 10. The color conversion layer 12R can convert the light emitted by the light-emitting device 10 into red light. As a result, in the sub-pixel 11R, the light emitted by the light-emitting device 10 is extracted as red light to the outside of the display device 100 via the color conversion layer 12R.

[0044] The sub-pixel 11G includes a light-emitting device 10 and a color conversion layer 12G that overlaps the light-emitting device 10. The color conversion layer 12G can convert the light emitted by the light-emitting device 10 into green light. As a result, in the sub-pixel 11G, the light emitted by the light-emitting device 10 is extracted as green light to the outside of the display device 100 via the color conversion layer 12G.

[0045] The sub-pixel 11B includes a light-emitting device 10 and a layer 12B that overlaps the light-emitting device 10. The layer 12B can transmit, scatter, or convert the light emitted by the light-emitting device 10 into blue light. As a result, in the sub-pixel 11B, the light emitted by the light-emitting device 10 is extracted as blue light to the outside of the display device 100 via the layer 12B.

[0046] The light-emitting device 10 can be configured to emit, for example, blue light.

[0047] In the case where the light-emitting device 10 emits blue light, it is preferable that the color conversion layer 12R converts the blue light into red light and transmits the red light. By providing such a color conversion layer 12R on top of the light-emitting device 10, the blue light emitted by the light-emitting device 10 can be converted into red light and extracted to the outside of the display device.

[0048] Similarly, if the light-emitting device 10 is configured to emit blue light, it is preferable that the color conversion layer 12G converts the blue light into green light and transmits the green light. By providing such a color conversion layer 12G on top of the light-emitting device 10, the blue light emitted by the light-emitting device 10 can be converted into green light and extracted to the outside of the display device.

[0049] In other words, even if all of the light-emitting devices 10 are configured to emit blue light, a full-color display device can be realized.

[0050] Furthermore, in the case where the light-emitting device 10 emits blue light, a microcavity structure may be applied to enhance the blue light emitted by the light-emitting device. Alternatively, a microcavity structure may not be applied.

[0051] Here, blue light can be defined as light whose maximum peak wavelength in the emission spectrum is between 400 nm and 480 nm. Green light can be defined as light whose maximum peak wavelength in the emission spectrum is between 480 nm and 580 nm. Red light can be defined as light whose maximum peak wavelength in the emission spectrum is between 580 nm and 700 nm.

[0052] Furthermore, the light-emitting device 10 can be configured to emit multiple colors of light, such as a configuration that emits white light or a configuration that emits blue and green light.

[0053] In a configuration where the light-emitting device 10 emits light of multiple colors, it is preferable that the color conversion layer 12R converts blue and green light into red light and transmits red light. By providing such a color conversion layer 12R in superimposed on the light-emitting device 10, the blue and green light components of the multiple colors of light can be converted into red light components and extracted to the outside of the display device. Therefore, compared to a configuration without the color conversion layer 12R, the efficiency of extracting red light can be increased. Furthermore, it is preferable that the color conversion layer 12R converts light with a shorter wavelength than red (for example, light from blue to orange) into red light and transmits red light. Alternatively, a colored layer that transmits red light may be provided. This can increase the color purity of red.

[0054] Similarly, if the light-emitting device 10 is configured to emit light of multiple colors, it is preferable that the color conversion layer 12G converts blue light into green light and transmits green light. By providing such a color conversion layer 12G in superimposed on the light-emitting device 10, the blue light component of the multiple colors of light can be converted into the green light component and extracted to the outside of the display device. Therefore, the efficiency of extracting green light can be increased compared to a configuration without the color conversion layer 12G. Alternatively, a colored layer that transmits green light may be provided. This can increase the purity of the green color.

[0055] Furthermore, if the light-emitting device 10 is configured to emit light of multiple colors, it is preferable to provide a blue light-transmitting layer 12B on top of the light-emitting device 10. This allows the blue light component of the multiple colors of light to be extracted to the outside of the display device. Alternatively, a colored layer that transmits blue light may be provided. This can enhance the purity of the blue color.

[0056] Furthermore, by applying a microcavity structure, light-emitting devices configured to emit multiple colors of light may also emit light with a specific wavelength, such as red, green, or blue, being amplified.

[0057] For example, by applying a configuration to the light-emitting device 10 that emits multiple colors of light, and by applying a microcavity structure, red light can be obtained from the light-emitting device 10 in the sub-pixel 11R, green light from the light-emitting device 10 in the sub-pixel 11G, and blue light from the light-emitting device 10 in the sub-pixel 11B.

[0058] Here, by applying a microcavity structure, it is possible to intensify and extract light of a desired wavelength in the forward direction, but the light extracted from an oblique direction will contain components of multiple colors.

[0059] Therefore, even in a display device to which a microcavity structure is applied, providing color conversion layers 12R and 12G is preferable because it can improve the efficiency of extracting light of the desired color.

[0060] Furthermore, the light-emitting device 10 may be configured to emit light with a shorter wavelength than blue light; for example, it may be configured to emit purple light or ultraviolet light.

[0061] Here, examples of light with wavelengths shorter than blue include light whose emission spectrum peak wavelength is between 100 nm and 400 nm.

[0062] If the light-emitting device 10 is configured to emit light with a wavelength shorter than blue, it is preferable to provide a layer 12B that converts the light emitted by the light-emitting device 10 into blue light and transmits blue light, superimposed on the light-emitting device 10. It is also preferable to provide a colored layer at a position that overlaps with the light-emitting device 10 via layer 12B.

[0063] Thus, for the sub-pixel 11B that emits blue light, a configuration using a color conversion layer, or a configuration using a combination of a color conversion layer and a coloring layer, can also be applied.

[0064] Furthermore, if the light-emitting devices 10 in the sub-pixels 11R and 11G are configured to emit light with a shorter wavelength than blue, it is preferable that the color conversion layers 12R and 12G can also convert light with a shorter wavelength than blue into red or green light.

[0065] It is preferable to use either a phosphor or quantum dots, or both, as the color conversion layer. In particular, quantum dots have a narrow spectral width in their emission spectrum, allowing for emission with good color purity. This can improve the display quality of the display device.

[0066] There are no particular limitations on the materials that constitute quantum dots. Examples include Group 14 elements, Group 15 elements, Group 16 elements, compounds consisting of multiple Group 14 elements, compounds of elements belonging to Groups 4 through 14 and Group 16 elements, compounds of Group 2 elements and Group 16 elements, compounds of Group 13 elements and Group 15 elements, compounds of Group 13 elements and Group 17 elements, compounds of Group 14 elements and Group 15 elements, compounds of Group 11 elements and Group 17 elements, iron oxides, titanium oxides, chalcogenide spinels, and various semiconductor clusters.

[0067] Specifically, cadmium selenide, cadmium sulfide, cadmium telluride, zinc selenide, zinc oxide, zinc sulfide, zinc telluride, mercury sulfide, mercury selenide, mercury telluride, indium arsenide, indium phosphide, gallium arsenide, gallium phosphide, indium nitride, gallium nitride, indium antimonide, gallium antimonide, aluminum phosphide, aluminum arsenide, aluminum antimonide, lead selenide, lead telluride, lead sulfide, indium selenide, telluride Indium sulfide, indium sulfide, gallium selenide, arsenic sulfide, arsenic selenide, arsenic telluride, antimony sulfide, antimony selenide, antimony telluride, bismuth sulfide, bismuth selenide, bismuth telluride, silicon, silicon carbide, germanium, tin, selenium, tellurium, boron, carbon, phosphorus, boron nitride, boron phosphide, boron arsenide, aluminum nitride, aluminum sulfide, barium sulfide, barium selenide, barium telluride, calcium sulfide, gallium selenide Calcium, calcium telluride, beryllium sulfide, beryllium selenide, beryllium telluride, magnesium sulfide, magnesium selenide, germanium sulfide, germanium selenide, germanium telluride, tin sulfide, tin selenide, tin telluride, lead oxide, copper fluoride, copper chloride, copper bromide, copper iodide, copper oxide, copper selenide, nickel oxide, cobalt oxide, cobalt sulfide, iron oxide, iron sulfide, manganese oxide, molybdenum sulfide, vanadium oxide, tungsten oxide, tantalum oxide Examples include titanium dioxide, zirconium oxide, silicon nitride, germanium nitride, aluminum oxide, barium titanate, compounds of selenium, zinc, and cadmium, compounds of indium, arsenic, and phosphorus, compounds of cadmium, selenium, and sulfur, compounds of cadmium, selenium, and tellurium, compounds of indium, gallium, and arsenic, compounds of indium, gallium, and selenium, compounds of indium, selenium, and sulfur, compounds of copper, indium, and sulfur, and combinations thereof. In addition, so-called alloy-type quantum dots, whose composition is expressed in any ratio, may also be used.

[0068] Quantum dot structures include core type, core-shell type, and core-multishell type. Furthermore, because quantum dots have a high proportion of surface atoms, they are highly reactive and prone to aggregation. Therefore, to prevent aggregation and improve dispersibility in the dispersion medium, it is preferable that a protective agent is attached to the surface of the quantum dots, or that protective groups are provided. This can also reduce reactivity and improve electrical stability.

[0069] As the size of a quantum dot decreases, its band gap increases, so its size is adjusted appropriately to obtain light of a desired wavelength. As the size decreases, the emission of quantum dots shifts towards the blue side, that is, towards higher energy, so by changing the size of the quantum dots, the emission wavelength can be adjusted across the ultraviolet, visible, and infrared spectral wavelength ranges. The size (diameter) of a quantum dot is, for example, 0.5 nm to 20 nm, preferably 1 nm to 10 nm. Furthermore, the narrower the size distribution of quantum dots, the narrower the emission spectrum becomes, and the better the color purity of the emission can be obtained. The shape of the quantum dots is not particularly limited and may be spherical, rod-shaped, disc-shaped, or other shapes. A quantum rod, which is a rod-shaped quantum dot, has the function of exhibiting directional light.

[0070] The color conversion layer can be formed using methods such as droplet ejection (e.g., inkjet), coating, imprint, and various printing methods (screen printing, offset printing). Alternatively, a color conversion film such as a quantum dot film may be used.

[0071] When processing the film that will become the color conversion layer, it is preferable to use photolithography. Photolithography methods include a method in which a resist mask is formed on the thin film to be processed, the thin film is processed by etching or the like, and the resist mask is removed, and a method in which a photosensitive thin film is formed, and then exposed and developed to process the thin film into the desired shape. For example, an island-shaped color conversion layer can be formed by forming a thin film using a material in which quantum dots are mixed with photoresist, and then processing the thin film using photolithography.

[0072] Furthermore, in a display device according to one aspect of the present invention, it is preferable to provide an insulating layer having an opening on a substrate and to provide a color conversion layer within the opening. The insulating layer can be formed using an organic resin film such as acrylic resin, polyamide resin, or epoxy resin, an inorganic insulating film, or an organic polysiloxane. It is particularly preferable to use a photosensitive material and to form the insulating layer so that the side walls of the opening are inclined surfaces with a continuous curvature. By providing the insulating layer, the color conversion layers of each color can be separated, thereby preventing color mixing. Thus, a display device with high display quality can be provided. The insulating layer is also called a partition or embankment because it has the function of separating the color conversion layers of each color.

[0073] However, quantum dots have the drawback of being susceptible to degradation due to the intrusion of impurities such as oxygen. When quantum dots degrade, the light emission intensity of the pixels decreases, and the display quality of the display device deteriorates. Therefore, in display devices that use quantum dots as a color conversion layer, it is necessary to prevent the intrusion of impurities such as oxygen from around the color conversion layer and to prevent the degradation of the quantum dots.

[0074] Therefore, in one embodiment of the present invention, an inorganic film is provided to cover the color conversion layer. This prevents impurities such as oxygen from entering the color conversion layer, thereby providing a display device with high display quality.

[0075] As shown in Figure 1B, the display device 100 has a structure in which a unit 30 including a substrate 40, a partition wall 20, a color conversion layer 12R, a color conversion layer 12G, a layer 12B, and an inorganic film 22, and a unit 31 including a layer 251 including a transistor and a light-emitting device 10 are bonded together by a resin layer 32. In Figure 1B, the dashed arrows indicate the direction of light emission.

[0076] In unit 30, the partition wall 20 is an insulating layer located on the substrate 40 and having an opening. The color conversion layer 12R, color conversion layer 12G, and layer 12B each have portions located within the opening of the partition wall 20. In the description of unit 30, "upper" refers to the vertical relationship when the substrate 40 side is considered lower and the color conversion layer 12R, color conversion layer 12G, and layer 12B side are considered upper.

[0077] The inorganic film 22 has portions located on the color conversion layer 12R, the color conversion layer 12G, and layer 12B.

[0078] In other words, the color conversion layer 12R, the color conversion layer 12G, and the layer 12B are each covered with an inorganic film 22. By providing the inorganic film 22 that covers the color conversion layers in this way, it is possible to prevent impurities such as oxygen from entering the color conversion layer 12R, the color conversion layer 12G, and the layer 12B, thereby preventing the color conversion layer 12R, the color conversion layer 12G, and the layer 12B from degrading due to impurities such as oxygen. Therefore, a highly reliable display device can be made.

[0079] An inorganic insulating film is preferred as the inorganic film 22. Examples of inorganic insulating films that can be used include silicon nitride film, silicon oxide nitride film, silicon oxide film, silicon nitride oxide film, aluminum oxide film, and aluminum nitride film. Alternatively, hafnium oxide film, yttrium oxide film, zirconium oxide film, gallium oxide film, tantalum oxide film, magnesium oxide film, lanthanum oxide film, cerium oxide film, and neodymium oxide film may also be used. Furthermore, two or more of the above insulating films may be laminated together. In particular, using a metal nitride film such as silicon nitride or aluminum nitride film is effective in preventing oxygen from entering the color conversion layer because the material itself does not contain oxygen.

[0080] From the viewpoint of suppressing the permeation of oxygen and the like, the thickness of the inorganic film 22 is preferably 10 nm or more, and more preferably 50 nm or more. On the other hand, from the viewpoint of suppressing a decrease in the transmittance of light emitted by the light-emitting device, the thickness of the inorganic film 22 is preferably 1000 nm or less, and more preferably 500 nm or less.

[0081] The substrate 40 can be made of glass, quartz, ceramics, sapphire, resin, metal, alloy, semiconductor, etc. The substrate on the side that extracts light from the light-emitting device should be made of a material that transmits the light. Using a flexible material for the substrate 40 can increase the flexibility of the display device. Alternatively, a polarizing plate or the like may be used as the substrate 40. Thus, a variety of materials can be used as the substrate.

[0082] As the substrate 40, polyester resins such as polyethylene terephthalate (PET) and polyethylene naphthalate (PEN), polyacrylonitrile resin, acrylic resin, polyimide resin, polymethyl methacrylate resin, polycarbonate (PC) resin, polyethersulfone (PES) resin, polyamide resin (nylon, aramid, etc.), polysiloxane resin, cycloolefin resin, polystyrene resin, polyamide-imide resin, polyurethane resin, polyvinyl chloride resin, polyvinylidene chloride resin, polypropylene resin, polytetrafluoroethylene (PTFE) resin, ABS resin, cellulose nanofiber, etc. may be used. Glass with a thickness sufficient to provide flexibility may also be used for the substrate 40.

[0083] Furthermore, when a circular polarizing plate is superimposed on a display device, it is preferable to use a substrate 40 with high optical isotropy. A substrate with high optical isotropy has low birefringence (or a small amount of birefringence).

[0084] For substrates with high optical isotropy, the absolute value of the retardation (phase difference) is preferably 30 nm or less, more preferably 20 nm or less, and even more preferably 10 nm or less.

[0085] Examples of films with high optical isotropy include triacetylcellulose (TAC, also known as cellulose triacetate) film, cycloolefin polymer (COP) film, cycloolefin copolymer (COC) film, and acrylic film.

[0086] Furthermore, when a film is used as the substrate 40, the film may absorb water, which could cause changes in shape, such as wrinkles, in the display device. For this reason, it is preferable to use a film with a low water absorption rate for the substrate. For example, it is preferable to use a film with a water absorption rate of 1% or less, more preferable to use a film with a water absorption rate of 0.1% or less, and even more preferable to use a film with a water absorption rate of 0.01% or less.

[0087] As the resin layer 32, various types of curing adhesives can be used, such as UV-curing adhesives, reaction-curing adhesives, thermosetting adhesives, and anaerobic adhesives. Examples of these adhesives include epoxy resins, acrylic resins, silicone resins, phenolic resins, polyimide resins, imide resins, PVC (polyvinyl chloride) resins, PVB (polyvinyl butyral) resins, and EVA (ethylene vinyl acetate) resins. Materials with low moisture permeability, such as epoxy resins, are particularly preferred. Two-component mixed resins may also be used. Adhesive sheets may also be used.

[0088] In unit 31, light-emitting devices 10 are provided on a layer 251 containing transistors, and a protective layer 135 is provided to cover these light-emitting devices. In addition, an insulating layer 133 and a partition wall 120 on the insulating layer 133 are provided in the region between adjacent light-emitting devices. In the description of unit 31, "upper" refers to the upper and lower relationship when the layer 251 containing transistors is considered lower and the light-emitting devices 10 are considered upper.

[0089] <Example of Light-Emitting Device Configuration> Figure 2A is a schematic cross-sectional view of a light-emitting device 10 that can be used in a display device according to one embodiment of the present invention. The light-emitting device 10 has a pair of electrodes (a first electrode 101 and a second electrode 102) and an organic compound layer 103 provided between the pair of electrodes. The organic compound layer 103 has at least a light-emitting layer 113.

[0090] Furthermore, the organic compound layer 103 shown in Figure 2A has functional layers such as a hole injection layer 111, a hole transport layer 112, an electron transport layer 114, and an electron injection layer 115, in addition to the light-emitting layer 113. Each layer may be a single layer or a configuration in which multiple layers are stacked.

[0091] In this embodiment, the first electrode 101 is described as the anode and the second electrode 102 as the cathode, but the configuration of the light-emitting device 10 is not limited to this. In other words, the first electrode 101 may be the cathode and the second electrode 102 as the anode, and the stacking order of the layers between the electrodes may be reversed. That is, the stacking order from the anode side may be the hole injection layer 111, the hole transport layer 112, the light-emitting layer 113, the electron transport layer 114, and the electron injection layer 115.

[0092] The configuration of the organic compound layer 103 is not limited to the configuration shown in Figure 2A, and may include at least one selected from the hole injection layer 111, hole transport layer 112, electron transport layer 114, and electron injection layer 115. Alternatively, the organic compound layer 103 may have a functional layer that has functions such as reducing the hole or electron injection barrier, improving hole or electron transport, inhibiting hole or electron transport, or suppressing quenching by electrodes. Each functional layer may be a single layer or a configuration in which multiple layers are stacked.

[0093] Figure 2B is a schematic cross-sectional view showing an example of the light-emitting layer 113 shown in Figure 2A. In one embodiment of the present invention, the light-emitting layer 113 has at least two layers. Specifically, Figure 2B shows light-emitting layer 113_1 and light-emitting layer 113_2. Light-emitting layer 113_1 has a host material 118_1 and a guest material 119_1 (light-emitting substance). Light-emitting layer 113_2 has a host material 118_2 and a guest material 119_2 (light-emitting substance).

[0094] The light-emitting layer 113_1 may have two types of host materials 118_1 (organic compound 118_1a and organic compound 118_1b) and a guest material 119_1 (luminescent substance). The light-emitting layer 113_2 may have two types of host materials 118_2 (organic compound 118_2a and organic compound 118_2b) and a guest material 119_2 (luminescent substance). In this embodiment, the case in which the host material 118_1 has two types, organic compound 118_1a and organic compound 118_2b, is described, but the host material 118_1 only needs to have at least one organic compound. Similarly, the host material 118_2 only needs to have at least one organic compound.

[0095] Furthermore, in the light-emitting layer 113_1, the host material 118_1 is present in the largest amount by weight, and the guest material 119_1 is dispersed within the host material 118_1. Similarly, in the light-emitting layer 113_2, the host material 118_2 is present in the largest amount by weight, and the guest material 119_2 is dispersed within the host material 118_2.

[0096] Furthermore, it is preferable to use a fluorescent substance (hereinafter also referred to as a fluorescent substance) as one of the guest materials 119_1 and 119_2, and a phosphorescent substance (hereinafter also referred to as a phosphorescent substance) as the other. In this specification, a fluorescent material is a compound that emits light in the visible light region when relaxing from a singlet excited state to the ground state. A phosphorescent material is a compound that emits light in the visible light region at room temperature when relaxing from a triplet excited state to the ground state. In other words, a phosphorescent material is one of the compounds that can convert triplet excitation energy into visible light.

[0097] Because phosphorescent materials can convert singlet excited states to triplet excited states through intersystem crossing, their internal quantum efficiency can theoretically reach 100% when used in a light-emitting layer. On the other hand, fluorescent materials have a generation probability ratio of 1:3 between singlet and triplet excited states, and can only utilize singlet excited states for light emission. Therefore, when used in a light-emitting layer, the theoretical limit of their internal quantum efficiency is 25%. Consequently, light-emitting devices having a light-emitting layer containing phosphorescent materials (also called light-emitting devices with phosphorescent materials) tend to have higher luminescence efficiency than light-emitting devices having a light-emitting layer containing fluorescent materials (also called light-emitting devices with fluorescent materials).

[0098] Furthermore, triplet excited states have a longer excitation lifetime than singlet excited states, making them more susceptible to degradation-related chemical reactions. Additionally, the triplet excitation energy of phosphorescent materials is higher than that of fluorescent materials. Therefore, light-emitting devices using phosphorescent materials tend to have shorter operating lifetimes.

[0099] Therefore, in one embodiment of the present invention, guest material 119_1 and guest material 119_2 are made of light-emitting materials with different transition processes. For example, if a fluorescent light-emitting material is used for guest material 119_1, a phosphorescent light-emitting material may be used for guest material 119_2. Alternatively, a phosphorescent light-emitting material may be used for guest material 119_1 and a fluorescent light-emitting material may be used for guest material 119_2. By using a phosphorescent light-emitting material with high luminescence efficiency and a fluorescent light-emitting material with high stability in the light-emitting device, it is possible to create a light-emitting device with high luminescence efficiency and a long operating life. Furthermore, it is preferable that the difference between the maximum peak wavelength in the emission (PL) spectrum of guest material 119_1 and the maximum peak wavelength in the emission spectrum of guest material 119_2 be 30 nm or less. By doing so, it is possible to create a light-emitting device with high color purity.

[0100] However, when a light-emitting layer containing a fluorescent material and a light-emitting layer containing a phosphorescent material are stacked, the recombination region between holes and electrons in the light-emitting layer 113 may be unevenly distributed, resulting in only one of the light-emitting layers, either the one containing the fluorescent material or the one containing the phosphorescent material, emitting light.

[0101] Therefore, in one aspect of the present invention, the giant surface potential (GSP) and the slope of the GSP (GSP_slope) as a physical property of the layer are adjusted in the light-emitting layer 113_1 and the light-emitting layer 113_2 to design the region where holes and electrons recombine to be the light-emitting layer 113_1 and the light-emitting layer 113_2. In another aspect of the present invention, in each light-emitting layer, the host material 118_1 and the host material 118_2, which are the most abundant by weight, are host materials with an appropriate GSP_slope of the film, thereby adjusting the light-emitting layer containing a fluorescent material and the light-emitting layer containing a phosphorescent material so that carriers (electrons and holes) recombine.

[0102] Furthermore, in vapor-deposited films of organic compounds such as light-emitting layers, spontaneous orientation polarization (SOP) may occur in the vapor-deposited film perpendicular to the substrate surface due to a bias in the orientation of the permanent electric dipole moments of the molecules in the film thickness direction.

[0103] Furthermore, a giant surface potential (GSP) may be generated in the film due to the internal electric field caused by the magnitude (Pz) of the SOP perpendicular to the substrate surface. In this specification, the magnitude (Pz) of the spontaneous orientation polarization perpendicular to the substrate surface is sometimes referred to as the magnitude (Pz) of the spontaneous orientation polarization (SOP). The GSP per unit film thickness is called GSP-slope. The GSP_slope of a film is the value obtained by dividing the film's Pz by the film's dielectric constant. The measurement methods for Pz and GSP_slope in a deposited film will be described later.

[0104] When layers having different Pz or GSP_slope are stacked, a positive or negative charge can be assumed to be generated at the interface due to the difference in Pz between the two layers, and this virtual interfacial charge affects the device characteristics. Therefore, in a light-emitting device, the interfacial charge can be controlled by selecting the material used for each layer, taking into account the Pz or GSP_slope of the light-emitting layer 113_1 and the light-emitting layer 113_2. In this specification, the virtual charge that can be considered as an interfacial charge is sometimes referred to as interfacial charge.

[0105] Specifically, Pz of the light-emitting layer 113_1 and the light-emitting layer 113_2 is 0.5 mC / m 2 or more and 3.0 mC / m 2 or less, which is preferable. Further, for the host material 118_1 and the host material 118_2, the Pz of the film is 0.5 mC / m 2 or more and 3.0 mC / m 2 or less, which is desirable. With this configuration, carriers can be adjusted to recombine in the light-emitting layer 113_1 and the light-emitting layer 113_2 to emit light.

[0106] Note that when the light-emitting layer 113_1 or the light-emitting layer 113_2 includes two or more types of host materials, at least one of the host materials has a film Pz of 0.5 mC / m 2 or more and 3.0 mC / m 2 or less, which is desirable. Note that preferably, in all host materials used for the light-emitting layer 113_1 or the light-emitting layer 113_2, the Pz of the film is 0.5 mC / m 2 or more and 3.0 mC / m 2 or less, which is desirable.

[0107] Further, the difference between the Pz of the light-emitting layer 113_1 and the Pz of the light-emitting layer 113_2 is 0.25 mC / m 2 or less, which is preferable. Further, the difference between the Pz of the film composed of the host material 118_1 and the Pz of the film composed of the host material 118_2 is 0.25 mC / m 2 or less, which is preferable. By using the host material 118_1 and the host material 118_2 whose film Pz difference is 0.25 mC / m 2 or less, carriers can be adjusted to recombine in the light-emitting layer 113_1 and the light-emitting layer 113_2, so that light is emitted in the light-emitting layer 113_1 and the light-emitting layer 113_2.

[0108] Note that when the light-emitting layer 113_1 or the light-emitting layer 113_2 includes two or more types of host materials, in each light-emitting layer, the difference in film Pz of at least one host material is 0.25 mC / m 2The following is preferable. For example, if the light-emitting layer 113_1 has organic compound 118_1a and organic compound 118_1b, and the light-emitting layer 113_2 has organic compound 118_2a and organic compound 118_2b, then for example, the difference in Pz between the film made of organic compound 118_1a and the film made of organic compound 118_2a is 0.25 mC / m 2 The following would be preferable.

[0109] Similarly, it is preferable that the GSP_slope of the light-emitting layer 113_1 and light-emitting layer 113_2 is between 20 mV / nm and 100 mV / nm. Furthermore, it is preferable that the GSP_slope of the film of the host material 118_1 and host material 118_2 is between 20 mV / nm and 100 mV / nm. With this configuration, it is possible to adjust the carriers to recombine in the light-emitting layer 113_1 and light-emitting layer 113_2.

[0110] Furthermore, if the light-emitting layer 113_1 or light-emitting layer 113_2 has two or more host materials, it is preferable that at least one of the host materials has a GSP_slope of 20 mV / nm or more and 100 mV / nm or less. Preferably, all host materials used in the light-emitting layer 113_1 or light-emitting layer 113_2 have a GSP_slope of 20 mV / nm or more and 100 mV / nm or less.

[0111] Furthermore, it is preferable that the difference between the GSP_slope of the light-emitting layer 113_1 and the GSP_slope of the light-emitting layer 113_2 is 10 mV / nm or less. Also, it is preferable that the difference between the GSP_slope of the host material 118_1 and the GSP_slope of the host material 118_2 is 10 mV / nm or less. By using host materials 118_1 and 118_2 in which the difference in GSP_slope of the films is 10 mV / nm or less, carriers can be recombined in the light-emitting layers 113_1 and 113_2, causing light to be emitted in the light-emitting layers 113_1 and 113_2.

[0112] Furthermore, if the light-emitting layer 113_1 or light-emitting layer 113_2 has two or more host materials, it is preferable that the difference in GSP_slope of the film in at least one host material in each light-emitting layer be 10 mV / nm or less. For example, if the light-emitting layer 113_1 has organic compound 118_1a and organic compound 118_1b, and the light-emitting layer 113_2 has organic compound 118_2a and organic compound 118_2b, it is preferable that the difference in GSP_slope between the film made of organic compound 118_1a and the film made of organic compound 118_2a be 10 mV / nm or less.

[0113] Therefore, by having a light-emitting device with both a phosphorescent material and a fluorescent material, and adjusting the carrier recombination between the two, it is possible to design a light-emitting device with high luminous efficiency and a good operating life. Although Figure 2B shows a configuration in which the light-emitting layer 113 has a two-layer structure, the light-emitting layer 113 may have a laminated structure of three or more layers. The number of layers of the phosphorescent material and the number of layers of the fluorescent material can be adjusted to suit the desired characteristics of the light-emitting device.

[0114] Furthermore, in one aspect of the present invention, as shown in Figure 2C, a separation layer 116 may be provided between the light-emitting layer 113_1 and the light-emitting layer 113_2. The separation layer 116 may be made of a hole-transporting material, an electron-transporting material, a mixture of a hole-transporting material and an electron-transporting material, or a bipolar material (an electron-transporting and hole-transporting material). In particular, a mixture of a hole-transporting material and an electron-transporting material or a bipolar material is preferred because it can transport holes and electrons to the light-emitting layer 113_1 and the light-emitting layer 113_2, respectively.

[0115] Specifically, the separation layer 116 can be a layer made of the same organic compound as the host material 118_1 or host material 118_2. Alternatively, the separation layer 116 can be made of the same material used for the charge generation layer.

[0116] <Host material when using fluorescent material> For example, when using a fluorescent material as the guest material 119_1 of the light-emitting layer 113_1, the lowest triplet excitation energy level (T) of the host material 118_11 The level is the T of the guest material 119_1 of the light-emitting layer 113_1. 1 Lower than the level, the lowest singlet excitation energy level of the host material 118_1 (S 1 The level is S of guest material 119_1 of luminescent layer 113_1. 1 A level higher than the current level is preferable because it increases the proportion of singlet excitons generated by TTA (Triple-Triple Annihilation), thereby improving luminescence efficiency.

[0117] Specifically, when a fluorescent material is used as the guest material 119_1 of the light-emitting layer 113_1, the host material 118_1 preferably contains an organic compound having an aromatic hydrocarbon, and more preferably contains an organic compound having a polycyclic aromatic hydrocarbon. It is also preferable to contain an organic compound having both a polycyclic aromatic hydrocarbon and a heteroaromatic ring. By using organic compounds having different heteroaromatic rings for organic compound 118_1a and organic compound 118_1b, a light-emitting device with a low driving voltage and low power consumption can be provided. Furthermore, this configuration makes it easier to maintain carrier balance, thus enabling the provision of a highly efficient light-emitting device.

[0118] Furthermore, it is preferable that the host material 118_1 includes an aromatic compound made of aromatic hydrocarbons. By using different aromatic compounds made of aromatic hydrocarbons for organic compound 118_1a and organic compound 118_1b, a highly reliable light-emitting device can be provided.

[0119] Furthermore, for example, organic compound 118_1a may be an organic compound having a polycyclic aromatic hydrocarbon and a heteroaromatic ring, and organic compound 118_1b may be an aromatic compound consisting of an aromatic hydrocarbon. By having an organic compound having a polycyclic aromatic hydrocarbon and a heteroaromatic ring, it is possible to maintain a carrier balance, thereby achieving high efficiency and low power consumption, and by having an aromatic compound consisting of an aromatic hydrocarbon, a light-emitting device with good reliability can be provided.

[0120] Furthermore, when an organic compound having an anthracene skeleton and a heteroaromatic ring is used for organic compound 118_1a, and an aromatic compound consisting of an aromatic hydrocarbon having an anthracene skeleton is used for organic compound 118_1b, the carrier balance of the light-emitting layer is improved, making it possible to provide a device with high luminescence efficiency, which is preferable. In particular, when the skeleton on which the orbitals of the lowest unoccupied molecular orbital (LUMO) level responsible for electron transport are distributed is an anthracene skeleton, it is preferable because high electron injection into the light-emitting layer and high electron transport of the light-emitting layer can be achieved.

[0121] Furthermore, when an aromatic compound consisting of aromatic hydrocarbons is used as the host material 118_1, the electron injection properties into the light-emitting layer and the electron transport properties of the light-emitting layer are improved. However, if excessive electron injection into the light-emitting layer occurs, the carrier balance of the light-emitting layer may be disrupted, and the recombination region may be extremely biased towards the anode side of the light-emitting layer. Using both an organic compound having a heteroaromatic ring and an aromatic compound consisting of aromatic hydrocarbons in the light-emitting layer is preferable because it improves the hole injection properties into the light-emitting layer and improves the balance of holes and electrons in the light-emitting layer. When the highest occupied molecular orbital (HOMO) level of the organic compound having a heteroaromatic ring is lower than the HOMO level of the aromatic compound consisting of aromatic hydrocarbons, the electron mobility of the organic compound having a heteroaromatic ring is suppressed, electron injection into the light-emitting layer is suppressed, and the carrier balance of the light-emitting layer is improved. On the other hand, if the HOMO level of an organic compound having a heteroaromatic ring is higher than that of an aromatic compound consisting of aromatic hydrocarbons, the hole mobility of the organic compound having a heteroaromatic ring increases, leading to increased hole implantation into the light-emitting layer and improving the carrier balance of the light-emitting layer.

[0122] Furthermore, the polycyclic aromatic hydrocarbons and organic compounds having heteroaromatic rings used in the host material 118, as well as aromatic compounds consisting of aromatic hydrocarbons, are preferable if they contain deuterium, as this improves their reliability. For example, when using a polycyclic aromatic hydrocarbon and an organic compound having heteroaromatic rings for organic compound 118_1a, and an aromatic compound consisting of aromatic hydrocarbons for organic compound 118_1b, the organic compound 118_1a, which is an organic compound having heteroaromatic rings, is preferable to an aromatic compound consisting of aromatic hydrocarbons, as the presence of deuterium improves its reliability.

[0123] On the other hand, when organic compound 118_1a, which is an aromatic compound composed of aromatic hydrocarbons, contains deuterium, the carbon-deuterium bond in the excited state is more stable than the carbon-practicum bond in the excited state, and the reaction that produces degraded products from the excited state is suppressed, thus improving reliability.

[0124] Furthermore, when both organic compound 118_1a, which is an organic compound having polycyclic aromatic hydrocarbons and heteroaromatic rings, and organic compound 118_1b, which is an aromatic compound consisting of aromatic hydrocarbons, are used, the carrier balance of the light-emitting layer is improved, the exciton density increases, and degradation tends to be accelerated. However, when both organic compound 118_1a, which is an organic compound having heteroaromatic rings, and organic compound 118_1b, which is an aromatic compound consisting of aromatic hydrocarbons, contain deuterium, degradation can be sufficiently suppressed even when the exciton density is high, resulting in a synergistic effect and a dramatic improvement in reliability, which is preferable.

[0125] The polycyclic aromatic hydrocarbon in organic compound 118_1a is preferably an aromatic hydrocarbon having 6 to 22 carbon atoms, in order to efficiently inject carriers into the light-emitting layer. It is also preferable that it is possible to provide a light-emitting element with high luminescence efficiency and a long operating life. Furthermore, the polycyclic aromatic hydrocarbon in organic compound 118_1a preferably has an anthracene skeleton, in order for the fluorescent material to emit light efficiently. When the polycyclic aromatic hydrocarbon in organic compound 118_1a has an anthracene skeleton, it is preferable that the anthracene skeleton has substituents at positions 9 and 10 in order to provide a light-emitting element with high reliability. In addition, it is preferable that organic compound 118_1a further contains a heteroaromatic ring. This heteroaromatic ring may be a polycyclic heteroaromatic ring.

[0126] Furthermore, it is preferable that the organic compound 118_1b has a polycyclic aromatic hydrocarbon, and it is preferable that the polycyclic aromatic hydrocarbon is an aromatic hydrocarbon having 6 to 30 carbon atoms in order to efficiently inject carriers into the light-emitting layer. It is also preferable that it is possible to provide a light-emitting element with high luminescence efficiency and a long operating life. It is preferable that the polycyclic aromatic hydrocarbon of the organic compound 118_1b has an anthracene skeleton in order to efficiently emit light from the fluorescent material. When the polycyclic aromatic hydrocarbon of the organic compound 118_1b has an anthracene skeleton, it is preferable that the anthracene skeleton has substituents at positions 9 and 10. Furthermore, it is preferable that the organic compound 118_1b further contains an aromatic ring. The aromatic ring may be either an aromatic hydrocarbon or a heteroaromatic ring.

[0127] Furthermore, it is preferable that the polycyclic aromatic hydrocarbon in organic compound 118_1a and the polycyclic aromatic hydrocarbon in organic compound 118_1b are the same, as this improves the carrier balance of the light-emitting layer and allows for the production of a light-emitting element with high luminous efficiency. This improves the carrier balance of the light-emitting layer and increases the heat resistance of the light-emitting layer, thereby improving the overall heat resistance of the light-emitting element. Furthermore, it is preferable that organic compound 118_1a and organic compound 118_1b are different organic compounds, and that they have different carrier transport properties, as this allows for a good carrier balance. The ratio of organic compound 118_1a to organic compound 118_1b is preferably 1:19 to 19:1 by weight or volume, preferably 1:9 to 9:1, and preferably 3:7 to 7:3.

[0128] Examples of aromatic rings possessed by organic compound 118_1a and organic compound 118_1b include condensed rings such as naphthalene rings, fluorene rings, benzofluorene rings, triphenylene rings, benzonaphthofuran rings, xanthene rings, benzoxanthene rings, spirofluorenexanthene rings, spirobenzofluorenexanthene rings, carbazole rings, benzocarbazole rings, dibenzofuran rings, dibenzothiophene rings, and benzonaphthothiophene rings.

[0129] Furthermore, since these condensed rings can adjust carrier transport properties or heat resistance depending on the bonding position, condensed rings with different bonding positions can be applied to one organic compound and another organic compound.

[0130] Furthermore, it is not limited to the same aromatic ring; aromatic rings with structural isomerisms may also be used. By using aromatic rings with structural isomerisms, it may be possible to manufacture the material using the same raw materials, thus reducing raw material costs or shortening the synthesis steps. For example, three condensed structures of the benzonaphthofuran ring can be identified by the difference in the fused position of the benzene ring: benzo[b]naphtho[2,1-d]furan ring, benzo[b]naphtho[2,3-d]furan ring, and benzo[b]naphtho[1,2-d]furan ring. In addition, materials using aromatic rings with structural isomerisms have different properties (carrier transport properties, HOMO, LUMO, etc.), so by using an aromatic ring suitable for the desired properties, improvements in properties can also be achieved.

[0131] Specific examples of organic compounds that can be used in host material 118_1 include 7-[4-(10-phenyl-9-antryl)phenyl]-7H-dibenzo[c,g]carbazole (abbreviation: cgDBCzPA) shown in structural formula (400), 2-(10-phenyl-9-antryl)benzo[b]naphtho[2,3-d]furan (abbreviation: Bnf(II)PhA) shown in structural formula (401), 9-[4-(10-phenyl-9-antryl)phenyl]-9H-carbazole (abbreviation: CzPA) shown in structural formula (402), and 1-[10-(phenyl-2,3,4,5,6-d 5 Examples of organic compounds include )-9-anthryl]benzo[b]naphtho[2,3-d]furan (abbreviation: Bnf(II)PhA-02-d5).

[0132]

[0133] Furthermore, the Pz and GSP_slope of the organic compounds shown by structural formulas (400) to (403) are shown below. In all cases, the Pz is 0.5 mC / m. 2 As described above, the GSP_slope is 20 mV / nm or higher. Therefore, it can be suitably used in a light-emitting device according to one embodiment of the present invention.

[0134]

[0135] By using the above-mentioned organic compound as the host material for a light-emitting layer having a fluorescent substance, a light-emitting device with high luminescence efficiency can be provided.

[0136] <Host material when using phosphorescent material> For example, when a phosphorescent material is used as the guest material 119_2 of the light-emitting layer 113_2, it is preferable that the host material 118_2 has an organic compound having a heteroaromatic ring. It is also preferable that it has at least one of an organic compound having a π-electron-rich heteroaromatic ring and an organic compound having a π-electron-deficient heteroaromatic ring. Furthermore, it is preferable that it has at least one of an organic compound having a heteroaromatic ring, an organic compound having a carbazole skeleton, or an organic compound having an aromatic amine skeleton.

[0137] Organic compounds having heteroaromatic rings function as electron-transporting hosts, while organic compounds having a carbazole skeleton or an aromatic amine skeleton function as hole-transporting hosts. It is preferable to use an electron-transporting host and a hole-transporting host in combination because it facilitates the formation of excited complexes (also called exciplexes).

[0138] Furthermore, by incorporating a phosphorescent material and an excitation complex into the light-emitting layer, the energy transfer from the excitation complex to the light-emitting material, known as ExTET (Exciplex-Triplet Energy Transfer), can be performed efficiently, thereby increasing the luminescence efficiency. This configuration also enables high efficiency, low voltage operation, and a long lifespan for the light-emitting device.

[0139] For efficient excitation complex formation, it is preferable that the HOMO level of the hole-transporting material is higher than or equal to the HOMO level of the electron-transporting material. It is also preferable that the LUMO level of the hole-transporting material is higher than or equal to the LUMO level of the electron-transporting material. Furthermore, it is preferable that the energy difference between the HOMO level of the hole-transporting material and the HOMO level of the electron-transporting material is 0.2 eV or higher. Such a configuration is preferable because it facilitates the injection of holes into the hole-transporting material and electrons into the electron-transporting material. The LUMO and HOMO levels of the materials can be derived from the electrochemical properties (reduction potential and oxidation potential) of the materials measured by cyclic voltammetry (CV), and can also be derived by photoelectron spectroscopy, optical absorption spectroscopy, inverse photoelectron spectroscopy, etc. When comparing values ​​between different compounds, it is preferable to use values ​​estimated from the same measurement.

[0140] Furthermore, it is preferable that the HOMO level of the phosphorescent material is lower than the HOMO level of the hole-transporting material, and the LUMO level of the phosphorescent material is higher than the LUMO level of the electron-transporting material. In other words, it is preferable that the energy difference between the LUMO level and the HOMO level of the phosphorescent material is greater than the energy difference between the LUMO level of the electron-transporting material and the HOMO level of the hole-transporting material. By doing so, it is possible to suppress the reaction that forms an excited complex between the phosphorescent material and the hole-transporting material or the electron-transporting material, thereby providing a light-emitting device that emits light efficiently.

[0141] Furthermore, phosphorescent materials have the ability to convert triplet excitation energy into light emission. Also, the triplet excited state is more energy stable than the singlet excited state. Therefore, phosphorescent materials can exhibit light emission with an energy lower than the energy difference between the LUMO level and the HOMO level. Even when the energy difference between the LUMO level and the HOMO level of a phosphorescent material is greater than the energy difference between the LUMO level of an electron-transporting material and the HOMO level of a hole-transporting material, if the emission energy exhibited by the phosphorescent material or the transition energy calculated from the absorption spectrum is equal to or smaller than the energy difference between the LUMO level of the electron-transporting material and the HOMO level of the hole-transporting material, or equal to or smaller than the emission energy of the excited complex formed by the electron-transporting material and the hole-transporting material, then excitation energy can be transferred from the excited complex formed by the electron-transporting material and the hole-transporting material to the phosphorescent material, and emission can be efficiently obtained from the phosphorescent material.

[0142] Furthermore, for phosphorescent materials to exhibit emission with high emission energy (short wavelength), the lowest triplet excitation energy level (T) of the phosphorescent material is required. 1 The energy level is preferably high. To achieve this, the ligand that coordinates to the heavy metal atoms in the phosphorescent material should also be T 1A high energy level is preferable, and low electron-accepting ability and a high LUMO level are preferable. Phosphorescent materials having such a structure tend to have a high LUMO level and a high HOMO level, making them molecular structures that readily accept holes. When a phosphorescent material has a molecular structure that readily accepts holes, the HOMO level of the phosphorescent material may be higher than the HOMO level of a material with hole-transporting properties. However, even if the energy difference between the LUMO level and the HOMO level of the phosphorescent material is greater than the energy difference between the LUMO level of the electron-transporting material and the HOMO level of the hole-transporting material, and the HOMO level of the phosphorescent material is higher than the HOMO level of the hole-transporting material, if the transition energy calculated from the emission energy or absorption spectrum exhibited by the phosphorescent material is equal to or smaller than the energy difference between the LUMO level of the electron-transporting material and the HOMO level of the hole-transporting material, then excitation energy can be transferred from the excited complex formed by the electron-transporting material and the hole-transporting material to the phosphorescent material, and emission can be efficiently obtained from the phosphorescent material. Alternatively, even if the luminescence energy of the excited complex formed by the electron-transporting material and the hole-transporting material is equal to or lower than that of the excited complex formed by the electron-transporting material and the hole-transporting material, the excitation energy can be transferred from the excited complex formed by the electron-transporting material and the hole-transporting material to the phosphorescent material, and luminescence can be efficiently obtained from the phosphorescent material.

[0143] The formation of excited complexes can be confirmed, for example, by comparing the PL spectra of a hole-transporting material, an electron-transporting material, and a mixed film made by mixing these materials, and observing that the PL spectrum of the mixed film shifts to a longer wavelength than the PL spectra of each individual material (or has a new peak on the longer wavelength side). Alternatively, it can be confirmed by comparing the transient photoluminescence (PL) of a hole-transporting material, the transient PL of an electron-transporting material, and the transient PL of a mixed film made by mixing these materials, and observing differences in the transient response, such as the transient PL lifetime of the mixed film having a longer lifetime component or a larger proportion of the delayed component than the transient PL lifetime of each individual material. Furthermore, the transient PL mentioned above may be read as transient electroluminescence (EL). That is, the formation of excited complexes can also be confirmed by comparing the transient EL of a hole-transporting material, the transient EL of an electron-transporting material, and the transient EL of a mixed film made by mixing these materials, and observing the differences in the transient response.

[0144] For example, when organic compound 118_2a and organic compound 118_2b form an excited complex, it is preferable that the short-wavelength emission edge of the photoluminescence (PL) spectrum of the excited complex is located at a shorter wavelength than the long-wavelength absorption edge of the absorption spectrum of the luminescent central material. This positional relationship between the PL spectrum of the excited complex and the absorption edge of the luminescent central material allows for efficient energy transfer.

[0145] Alternatively, it is preferable that the peak wavelength of the PL spectrum of the excited complex formed by organic compound 118_2a and organic compound 118_2b is shorter than the peak wavelength of the PL spectrum of the luminescent central material. Furthermore, it is more preferable that the difference between the peak wavelength of the PL spectrum of the excited complex and the peak wavelength of the PL spectrum of the luminescent central material is within 30 nm. This relationship between the peak wavelengths of the PL spectra of the excited complex and the luminescent central material allows for efficient energy transfer.

[0146] Alternatively, it is preferable that the difference between the peak wavelength of the PL spectrum of the excited complex formed by organic compound 118_2a and organic compound 118_2b and the wavelength of the long-wavelength absorption edge in the absorption spectrum of the luminescent central material is within 30 nm. This relationship between the peak wavelength of the PL spectrum of the excited complex and the wavelength of the long-wavelength absorption edge in the absorption spectrum of the luminescent central material allows for efficient energy transfer.

[0147] Alternatively, it is preferable that the short-wavelength emission edge of the PL spectrum of the excited complex formed by organic compound 118_2a and organic compound 118_2b is located at a shorter wavelength than the short-wavelength emission edge of the PL spectrum of the luminescent central material. Furthermore, it is more preferable that the energy difference between the short-wavelength emission edge of the PL spectrum of the excited complex and the short-wavelength emission edge of the PL spectrum of the luminescent central material is within 0.3 eV. This relationship between the short-wavelength emission edges of the PL spectrum of the excited complex and the short-wavelength emission edges of the PL spectrum of the luminescent central material allows for efficient energy transfer.

[0148] Furthermore, the emission edge on the short-wavelength side of the PL spectrum can be calculated by drawing a tangent line at the point where the absolute value of the slope on the short-wavelength side of the shortest wavelength peak (or shoulder peak) observed in the PL spectrum is maximum, and then calculating the point of intersection of this tangent line with the horizontal axis or baseline. Similarly, the absorption edge on the long-wavelength side of the absorption spectrum can be calculated by drawing a tangent line at the point where the absolute value of the slope on the long-wavelength side of the longest wavelength peak (or shoulder peak) observed in the absorption spectrum is maximum, and then calculating the point of intersection of this tangent line with the horizontal axis or baseline.

[0149] The PL spectrum of the excited complex is preferably measured using a co-evaporated film of organic compound 118_2a and organic compound 118_2b. The mixing ratio of organic compound 118_2a and organic compound 118_2b can be expressed by weight ratio, volume ratio, or molar ratio, and should be organic compound 118_2a:organic compound 118_2b = 1:19 to 19:1, preferably 1:9 to 9:1, and more preferably 3:7 to 7:3. Alternatively, the PL spectrum of the mixed film of organic compound 118_2a and organic compound 118_2b may be measured using the spectrum of a mixed film mixed at a ratio of organic compound 118_2a:organic compound 118_2b = 1:1. On the other hand, the sample form when measuring the PL spectrum or absorption spectrum of the luminescence center material may be a thin film or a solution, but a solution is preferred from the viewpoint of verifying the state of isolated molecules. As the solvent for the solution, a relatively low polar solvent such as toluene or chloroform is preferred.

[0150] Furthermore, when a phosphorescent material is used in the light-emitting layer, the T of organic compound 118_2a and organic compound 118_2b 1 The energy level is the T of the phosphorescent material. 1 It is preferable that the level is higher than the T level. The singlet excitation energy and triplet excitation energy of organic compound 118_2a and organic compound 118_2b are the S1 level and T level of organic compound 118_2a and organic compound 118_2b. 1 T from the energy level of phosphorescent material 1 Energy can be transferred to the next energy level. As a result, the phosphorescent material enters a triplet excited state and emits phosphorescence.

[0151] Note, - 1 As an indicator of the energy level, the phosphorescence component (phosphor spectrum) of the PL spectrum observed at low temperatures (for example, any temperature in the range of 4K to 80K) can be used. Specifically, for example, a thin film prepared by depositing a sample to a thickness of 50 nm on a quartz substrate is used, the PL spectrum (phosphor spectrum) is measured at a measurement temperature of 10 K, and the energy at the short-wavelength emission edge is defined as T. 1It can be considered as an energy level. The emission edge can be calculated by drawing a tangent line at the point where the absolute value of the slope on the short-wavelength side of the shortest wavelength peak (or shoulder peak) observed in the PL spectrum (phosphorescence spectrum) is maximum, and then finding the intersection of that tangent line with the horizontal axis (wavelength) or baseline.

[0152] Also, the T of phosphorescent materials 1 The energy level is determined by measuring the PL spectrum observed at low temperatures (e.g., any temperature in the range of 4K to 80K) or room temperature (e.g., any temperature in the range of 275K to 305K) and determining the energy at the short-wavelength emission edge. 1 It can be considered a level.

[0153] Compounds having heteroaromatic rings that can be used as host materials preferably have an azine skeleton. Examples of azine skeletons include pyridine rings, pyrimidine rings, and triazine rings. These can improve electron transport properties. Furthermore, it is preferable to use compounds in which a carbazole skeleton is directly or via an arylene group bonded to the azine skeleton, and it is preferable to have multiple carbazole skeletons. It is also preferable that the multiple carbazole skeletons are not bonded to each other. In this way, electron transport properties can be adjusted by having a carbazole skeleton. In addition, compounds having heteroaromatic rings may contain one or more elements such as silicon, boron, oxygen, and sulfur.

[0154] Furthermore, it is preferable that the compound having a carbazole skeleton has multiple carbazole skeletons. It is preferable that it has at least one of the following structures: a structure in which the 3 position of one carbazole skeleton is bonded to the 9 position of another carbazole skeleton; a structure in which the 2 position of one carbazole skeleton is bonded to the 9 position of another carbazole skeleton; a structure in which the 4 position of one carbazole skeleton is bonded to the 9 position of another carbazole skeleton; a structure in which the 1 position of one carbazole skeleton is bonded to the 9 position of another carbazole skeleton; or a structure in which the 3 position of one carbazole skeleton is bonded to the 3 position of another carbazole skeleton. It is even more preferable that it has multiple of these structures. In addition, the compound having a carbazole skeleton may have one or more elements such as silicon, boron, oxygen, and sulfur.

[0155] Furthermore, when using two compounds in combination as a host material, it is preferable that both the compound having a heteroaromatic ring and the compound having a carbazole skeleton have multiple carbazole skeletons. In this case, the number of carbazole skeletons in the compound having a carbazole skeleton should be the same as, or greater than, the number of carbazole skeletons in the compound having a heteroaromatic ring. By adjusting the number of carbazole skeletons in this way, the electron transport and hole transport properties of the host material can be controlled.

[0156] Furthermore, it is preferable that the two compounds, one having a heteroaromatic ring and the other having a carbazole skeleton, both contain elements such as silicon, boron, oxygen, and sulfur, because the presence of the same elements in both compounds can improve the properties of light-emitting devices using phosphorescent materials.

[0157] Specific examples of organic compounds that can be used in host material 118_2 include 9,9'-{6-[3-(triphenylsilyl)phenyl]-1,3,5-triazine-2,4-diyl}bis(9H-carbazole) (abbreviation: SiTrzCz2), shown in structural formula (450), and 2-phenyl-4,6-bis[3-(triphenylsilyl)phenyl]-1,3,5-triazine (abbreviation: mS), shown in structural formula (451). iTrz), 9-{4-phenyl-6-[3-(triphenylsilyl)phenyl]-1,3,5-triazine-2-yl}-9H-carbazole (abbreviation: SiCzTrz), shown in structural formula (452), 9-{4,6-bis[3-(triphenylsilyl)phenyl]-1,3,5-triazine-2-yl}-9H-carbazole (abbreviation: DSiCzTrz), shown in structural formula (453), and shown in structural formula (454). 9-(biphenyl-4-yl)-3-(4-{[4'-(4,6-diphenyl-1,3,5-triazine-2-yl)biphenyl-4-yl]diphenylsilyl}phenyl)-9H-carbazole (abbreviation: CzSiTZn), shown in structural formula (455), 3-{6-[3-(4,6-diphenyl-1,3,5-triazine-2-yl)phenyl]dibenzothiophen-4-yl}-9-phenyl-9H-carbazole Examples include rubazole (abbreviation: mPCDBtPTzn), 9-[3-(triphenylsilyl)phenyl]-3,9'-bi-9H-carbazole (abbreviation: PSiCzCz) shown in structural formula (456), and [4-(2,12-di-tert-butyl-5,9-dioxa-13b-boranaphtho[3,2,1-de]anthracene-7-yl)phenyl]triphenylsilane shown in structural formula (457). In addition, organic compounds shown in structural formulas (458), (459), and (460) can be used.

[0158]

[0159]

[0160] By using the above-mentioned organic compound as the phosphorescent material, a light-emitting device with high luminescence efficiency can be provided.

[0161] <Method for determining Pz and GSP_slope> The following describes a method for determining the Pz and GSP_slope of a film formed by vacuum deposition of an organic compound.

[0162] The surface potential generated in a deposited film is called GSP (Giant Surface Potential). Generally, the slope when the surface potential of a deposited film measured by a Kelvin probe is plotted in the direction of film thickness is discussed as GSP_slope (mV / nm). Pz (mC / m 2 Alternatively, an element can be fabricated in which a charge accumulates at the interface when a layer containing a known material with a GSP_slope (mV / nm) and a layer with an unknown Pz (the layer to be measured) are stacked, and the unknown Pz can be estimated by performing a C-V (capacitance-voltage) measurement. The GSP_slope (mV / nm) can be determined from Pz and dielectric constant (which can also be the square of the refractive index at a wavelength of 633 nm).

[0163] When organic thin films with different Pz values ​​(having thin film 1 and thin film 2, where thin film 1 is located on the substrate side) are stacked and a voltage is applied, and charge accumulates at the interface, the following equation holds true.

[0164]

[0165]

[0166]

[0167]

[0168]

[0169]

[0170] In equation (1), σ acc σ is the amount of charge that is accumulated. int V is the interfacial charge density. inj V is the carrier injection voltage (V), V th d is the threshold voltage, acc The film thickness of the charge storage layer is ε acc V is the dielectric constant of the charge storage layer. inj , V th This can be estimated from the capacitance-voltage characteristics of the device. Furthermore, the dielectric constant is the refractive index n. oAssuming the square of (the value at a wavelength of 633 nm) is the relative permittivity, the vacuum permittivity ε 0 It can be found by multiplying by ε. r1 ε of thin film 1 r2 ε is the relative permittivity of thin film 2. r1 and ε r2 Of these, the dielectric constant of the layer where charge does not penetrate after Vinj and charge accumulates at the interface is ε acc Thus, V is estimated from the capacitance-voltage characteristics. inj , V th And the dielectric constant ε of the charge storage layer, calculated from the refractive index and the permittivity of vacuum. acc , and the film thickness d of the charge storage layer acc Therefore, using equation (1), the interfacial charge density σ int This can be calculated. In equation (1), q is the sign of the interfacial charge. When the interfacial charge is negative and holes are injected, use q = -1; when the interfacial charge is positive and electrons are injected, use q = +1. Non-patent document 1 describes the case where q = -1 and holes are injected.

[0171] For configurations in which holes are injected, you can refer to the description of hole injection layers later, which will be used as materials for the hole injection layer. Similarly, for configurations in which electrons are injected, you can refer to the description of electron injection layers later, which will be used as materials for the electron injection layer.

[0172] Next, in equation (2)-(4), P 1 and P 2 Pz, ε of thin film 1 and thin film 2 1 ε of thin film 1 2 d is the dielectric constant of thin film 2. 1 d of thin film 1 2 is the thickness of thin film 2. Also, GSP_slope is obtained by dividing Pz by the dielectric constant. Here, from the above equation (1), the interfacial charge density σ int Since this can be determined, by using a material with a known GSP_slope as thin film 1 or thin film 2, the Pz and GSP_slope of the desired thin film can be estimated.

[0173] Therefore, as thin film 2, tris(8-quinolinolato)aluminum (abbreviated as Alq) has a known GSP_slope of 48 mV / nm. 3 The following is an example of how a measurement device 1 was fabricated using (Non-Patent Document 2, Figure 2) and the GSP_slope of 4,4'-bis[N-(1-naphthyl)-N-phenylamino]biphenyl (abbreviated as NPB) was determined.

[0174] The device structure of measurement device 1 is shown in Table 1. For the anode, indium tin oxide (ITSO) containing silicon or silicon oxide was used. Layers 1_1 and 3_1 of measurement device 1 were formed from the anode side by vacuum deposition at room temperature. The deposition rate for forming layers 2_1 and 3_1 was set to 0.2 nm / s to 0.6 nm / s. Deposition was carried out without stopping the deposition process between layers. In measurement device 1, layer 2_1 corresponds to thin film 1, and layer 3_1 corresponds to thin film 2. OCHD-003 is an organic compound with electron acceptor properties.

[0175] When fabricating the measurement device, the deposition rate of each layer is preferably 3 nm / min to 600 nm / min. Furthermore, the film thickness of each layer in the measurement device is preferably 3 nm to 500 nm, and more preferably 50 nm to 300 nm.

[0176] Furthermore, the capacitance-voltage characteristics of the measurement device 1 are shown in Figure 3. The capacitance-voltage characteristics were measured using a potentiometer / galvanostat SP-300 manufactured by Biologic, France, at a frequency of 10 Hz.

[0177]

[0178] Table 3 shows the Hole injection voltage V of the measuring device 1, which was determined using Figure 3 and equations (1) and (2). i , threshold voltage V bi , interfacial charge density σ if_h , Pz and GSP_slope, and the refractive index n of the NPB used in the calculation o and Alq 3 refractive index n oThe results are shown. The refractive index was measured using a spectroscopic ellipsometer (M-2000U, manufactured by J.A. Woolam Japan Co., Ltd.).

[0179]

[0180] Furthermore, it has almost the same configuration as measurement device 1, Alq 3 A measurement device 2 with a film thickness of only 80 nm was fabricated, and it was confirmed that the hole injection voltage in each device was shifted to a lower voltage than that of measurement device 1. In other words, in such a device, the holes are injected first, and Alq 3 This suggests that charge is accumulating at the interface. Furthermore, using measurement device 2, Pz and GSP_slope were estimated in the same way as with measurement device 1, and it was confirmed that the same results were obtained. In addition, if multiple measurements are taken, the average value of the measured values ​​may be used as Pz and GSP_slope.

[0181] Furthermore, the threshold voltage V can be obtained from the capacitance-voltage characteristics. bi If it is difficult to determine, the threshold voltage of the current density-voltage characteristic may be used.

[0182] Figure 4 shows the current density-voltage characteristics of the measuring device 1.

[0183] V calculated from current density-voltage characteristics bi The voltage was 2.0V, which was the same value as the one calculated from the capacitance-voltage characteristics.

[0184] Thus, Alq, whose membrane GSP_slope is known 3 By fabricating a device having a multilayer film with an organic compound and measuring its capacitance-voltage characteristics, the Pz and GSP_slope of the organic compound film can be estimated.

[0185] It is preferable to select the organic compound to be used in each layer of the light-emitting device by considering the Pz of the vapor-deposited film of the organic compound, or the GSP_slope, which has been measured in advance using the measurement method described above.

[0186] In some cases, light-emitting devices use layers co-deposited with multiple types of organic compounds. Since the Pz or GSP_slope of a co-deposited layer changes depending on the combination and mixing ratio of the organic compounds, it is ideal to measure the Pz or GSP_slope of a film co-deposited with the same combination and mixing ratio of organic compounds in advance, and then select the organic compounds considering the Pz or GSP_slope. However, this method requires fabricating different co-deposited films for each combination or mixing ratio of organic compounds and measuring the Pz or GSP_slope, making the experiments for selecting organic compounds complicated.

[0187] Therefore, in a light-emitting device, if one layer contains multiple types of organic compounds, it is preferable to select the organic compounds by considering the average value of the Pz or GSP_slope of the deposited film of each organic compound, which has been measured in advance, as the Pz or GSP_slope of that layer. This makes it relatively easy to select organic compounds that take Pz or GSP_slope into consideration.

[0188] However, even if a single layer contains multiple types of organic compounds, if their content differs significantly, the Pz or GSP_slope of the vapor-deposited film of the organic compound with the highest content among the multiple types of organic compounds can be considered as the Pz or GSP_slope of that layer, and the selection of the organic compound can be performed accordingly. For example, if a single layer contains two types of organic compounds, and the content of one organic compound is less than 20% by weight of the total, then that organic compound can be judged as a minor component of that layer, and the other organic compound with the higher content can be judged as the main component of that layer, and the Pz or GSP_slope of the vapor-deposited film of that main component can be considered as the Pz or GSP_slope of that layer. Furthermore, if a single layer contains three or four types of organic compounds, and the content of one type of organic compound is less than 20% by weight of the total, that organic compound can be determined to be a minor component of that layer, and the remaining organic compounds can be determined to be the main components of that layer. In this case, the average value of the Pz or GSP_slope of the vapor-deposited film of each main component can be considered to be the Pz or GSP_slope of that layer.

[0189] <Basic Structure of Light-Emitting Devices> Below, the basic structure of light-emitting devices will be explained in more detail using Figures 5A to 5E. Figure 5A shows a light-emitting device with a structure (single structure) having an organic compound layer (also called an EL layer) containing a light-emitting layer between a pair of electrodes. Specifically, it has a structure in which an organic compound layer 103 is sandwiched between a first electrode 101 and a second electrode 102.

[0190] Furthermore, Figure 5B shows a light-emitting device with a laminated structure (tandem structure) having multiple (two layers in Figure 5B) organic compound layers (103a, 103b) between a pair of electrodes, and a charge generation layer 106 between the organic compound layers. The tandem structure light-emitting device can realize a highly efficient light-emitting device with the same amount of current as a single structure light-emitting device.

[0191] The charge generation layer 106 has the function of injecting electrons into one organic compound layer (103a or 103b) and holes into the other organic compound layer (103b or 103a) when a potential difference is created between the first electrode 101 and the second electrode 102. Therefore, in Figure 5B, when a voltage is applied to the first electrode 101 such that its potential is higher than that of the second electrode 102, electrons are injected from the charge generation layer 106 into the organic compound layer 103a and holes are injected into the organic compound layer 103b.

[0192] Furthermore, from the viewpoint of light extraction efficiency, it is preferable that the charge generation layer 106 is transparent to visible light (specifically, the transmittance of visible light to the charge generation layer 106 is 40% or more). In addition, the charge generation layer 106 can function even if its conductivity is lower than that of the first electrode 101 and the second electrode 102.

[0193] Figure 5C also shows the laminated structure of the organic compound layer 103 of a light-emitting device that can be used in a display device according to one embodiment of the present invention. In this case, the first electrode 101 functions as an anode and the second electrode 102 functions as a cathode. The organic compound layer 103 has a structure in which a hole injection layer 111, a hole transport layer 112, a light-emitting layer 113, an electron transport layer 114, and an electron injection layer 115 are sequentially laminated on the first electrode 101. The light-emitting layer 113 may be configured by laminating multiple light-emitting layers with different light-emitting colors. For example, a light-emitting layer containing a red light-emitting substance, a light-emitting layer containing a green light-emitting substance, and a light-emitting layer containing a blue light-emitting substance may be laminated, or laminated via a layer having a carrier transport material. Alternatively, a combination of a light-emitting layer containing a yellow light-emitting substance and a light-emitting layer containing a blue light-emitting substance may be used. However, the laminated structure of the light-emitting layer 113 is not limited to the above. For example, the light-emitting layer 113 may be configured by stacking multiple light-emitting layers of the same emission color. For example, it may be a structure in which a first light-emitting layer containing a blue light-emitting substance and a second light-emitting layer containing a blue light-emitting substance are stacked, or stacked via a layer having a carrier transport material. In the case of a configuration in which multiple light-emitting layers of the same emission color are stacked, reliability can be increased compared to a single-layer configuration. Also, even when there are multiple light-emitting layers as in the tandem structure shown in Figure 5B, each light-emitting layer is stacked sequentially from the anode side as described above. Furthermore, when the first electrode 101 is the cathode and the second electrode 102 is the anode, the stacking order of the organic compound layer 103 is reversed. Specifically, on the first electrode 101 which is the cathode, 111 is an electron injection layer, 112 is an electron transport layer, 113 is a light-emitting layer, 114 is a hole transport layer, and 115 is a hole injection layer.

[0194] The light-emitting layers 113 contained in the organic compound layers (103, 103a, 103b) each contain a light-emitting substance and a combination of multiple substances as appropriate, and can be configured to produce fluorescence emission or phosphorescence emission exhibiting a desired emission color. Alternatively, the light-emitting layers 113 may be arranged in a laminated structure with different emission colors. In this case, the light-emitting substance and other substances used in each laminated light-emitting layer may be made of different materials. Furthermore, a configuration may be used in which different emission colors can be obtained from multiple organic compound layers (103a, 103b) as shown in Figure 5B. In this case as well, the light-emitting substance and other substances used in each light-emitting layer may be made of different materials.

[0195] Furthermore, in a light-emitting device that can be used in a display device according to one aspect of the present invention, for example, by making the first electrode 101 shown in Figure 5C a reflective electrode and the second electrode 102 a semi-transparent / semi-reflective electrode, and by using a microcavity structure, the light emitted from the light-emitting layer 113 contained in the organic compound layer 103 resonates between the two electrodes, thereby strengthening the light emitted from the second electrode 102. Therefore, it is easy to achieve high resolution. In addition, since it is possible to strengthen the light emission intensity in the front direction at a specific wavelength, power consumption can be reduced.

[0196] Furthermore, if the first electrode 101 of the light-emitting device is a reflective electrode consisting of a laminated structure of a reflective conductive material and a translucent conductive material (transparent conductive film), optical adjustment can be performed by controlling the film thickness of the transparent conductive film. Specifically, it is preferable to adjust the optical distance (product of film thickness and refractive index) between the first electrode 101 and the second electrode 102 to be mλ / 2 (where m is an integer of 1 or more) or close to it, with respect to the wavelength λ of light obtained from the light-emitting layer 113.

[0197] Furthermore, in order to amplify the light obtained from the light-emitting layer 113 at a desired wavelength (wavelength: λ), it is preferable to adjust the optical distance from the first electrode 101 to the region where light emission is obtained in the light-emitting layer 113 (light-emitting region), and the optical distance from the second electrode 102 to the region where light emission is obtained in the light-emitting layer 113 (light-emitting region), so that they are (2m'+1)λ / 4 (where m' is an integer of 1 or more) or near that value. The light-emitting region referred to here is the region in the light-emitting layer 113 where holes and electrons recombine.

[0198] By performing such optical adjustments, the spectrum of specific monochromatic light obtained from the light-emitting layer 113 can be narrowed, resulting in light emission with good color purity.

[0199] However, in the above case, the optical distance between the first electrode 101 and the second electrode 102 can be precisely defined as the total thickness from the reflective region of the first electrode 101 to the reflective region of the second electrode 102. However, since it is difficult to precisely determine the reflective regions of the first electrode 101 and the second electrode 102, the above effects can be sufficiently obtained by assuming that any position on the first electrode 101 and the second electrode 102 is a reflective region. Furthermore, the optical distance between the first electrode 101 and the light-emitting layer can be precisely defined as the optical distance between the reflective region of the first electrode 101 and the light-emitting region of the light-emitting layer. However, since it is difficult to precisely determine the reflective region of the first electrode 101 and the light-emitting region of the light-emitting layer, the above effects can be sufficiently obtained by assuming that any position on the first electrode 101 is a reflective region and any position on the light-emitting layer is a light-emitting region.

[0200] The light-emitting device shown in Figure 5D is a light-emitting device having a tandem structure. The tandem structure allows for a light-emitting device capable of high-brightness illumination. Furthermore, compared to a single structure, the tandem structure reduces the current required to achieve the same brightness, thereby improving reliability. It also reduces power consumption.

[0201] The light-emitting device shown in Figure 5E is an example of a tandem-structured light-emitting device shown in Figure 5B. As shown in the figure, it has a structure in which three organic compound layers (103a, 103b, 103c) are stacked with charge generation layers (106a, 106b) in between. Each of the three organic compound layers (103a, 103b, 103c) has a light-emitting layer (113a, 113b, 113c), and the light-emitting colors of each light-emitting layer can be freely combined. For example, light-emitting layer 113a can be blue, light-emitting layer 113b can be red, green, or yellow, and light-emitting layer 113c can be blue. Alternatively, light-emitting layer 113a can be red, light-emitting layer 113b can be blue, green, or yellow, and light-emitting layer 113c can be red.

[0202] In the light-emitting device that can be used in a display device according to one aspect of the present invention described above, at least one of the first electrode 101 and the second electrode 102 is a light-transmitting electrode (transparent electrode, semi-transparent / semi-reflective electrode, etc.). When the light-transmitting electrode is a transparent electrode, the transmittance of visible light of the transparent electrode is 40% or more. When it is a semi-transparent / semi-reflective electrode, the reflectance of visible light of the semi-transparent / semi-reflective electrode is 20% or more and 80% or less, preferably 40% or more and 70% or less. Furthermore, the resistivity of these electrodes is 1 × 10⁻¹⁶. −2 It is preferable to keep it below Ωcm.

[0203] Furthermore, in a light-emitting device that can be used in a display device according to one aspect of the present invention described above, if one of the first electrode 101 and the second electrode 102 is a reflective electrode (reflective electrode), the visible light reflectance of the reflective electrode is 40% or more and 100% or less, preferably 70% or more and 100% or less. Also, the resistivity of this electrode is 1 × 10⁻¹⁶. −2 It is preferable to keep it below Ωcm.

[0204] <Specific Structure of the Light-Emitting Device> Next, a specific structure of a light-emitting device that can be used in a display device according to one aspect of the present invention will be described. Here, a tandem structure, as shown in Figure 5D, will be used for the explanation. The same applies to the configuration of the organic compound layer for the single-structure light-emitting devices shown in Figures 5A and 5C. Furthermore, if the light-emitting device shown in Figure 5D has a microcavity structure, the first electrode 101 is formed as a reflective electrode, and the second electrode 102 is formed as a semi-transparent / semi-reflective electrode. Thus, one or more desired electrode materials can be used and formed in a single layer or in a stacked manner. The second electrode 102 is formed by selecting an appropriate material after the organic compound layer 103b has been formed.

[0205] <Materials for Light-Emitting Devices> <Light-Emitting Layers> The light-emitting layers (113, 113a, 113b, 113c) are layers containing a light-emitting material. The light-emitting material that can be used in the light-emitting layers (113, 113a, 113b, 113c) can be any material that exhibits a light-emitting color such as blue, purple, blue-violet, green, yellow-green, yellow, orange, or red. Furthermore, if there are multiple light-emitting layers, a configuration exhibiting different light-emitting colors can be achieved by using different light-emitting materials in each layer (for example, white light emission obtained by combining complementary light-emitting colors). Additionally, a laminated structure in which one light-emitting layer contains a different light-emitting material is also possible.

[0206] Furthermore, the light-emitting layers (113, 113a, 113b, 113c) contain one or more organic compounds (host materials, etc.) in addition to the light-emitting substance (guest material).

[0207] For example, the structure described with reference to Figure 2B can be used as the light-emitting layer 113.

[0208] Next, a preferred configuration of the light-emitting layer 113_2 using a phosphorescent compound as the guest material 119_2 will be described.

[0209] In the light-emitting layer 113_2 using a phosphorescent compound as the guest material 119_2, the T of the host material 118_2 (organic compound 118_2a and organic compound 118_2b) 1 The energy level is the T of the guest material (guest material 119_2) of the light-emitting layer 113. 1It is preferable that the level be higher than the current level.

[0210] Furthermore, the lowest triplet excitation energy level (T 1 The lowest triplet excitation energy level (T) can be calculated from the emission edge of the phosphorescence spectrum. Furthermore, compounds whose phosphorescence spectrum is not detectable at room temperature may be detectable by lowering the temperature (for example, any temperature in the range of 4K to 80K). The sample form when measuring the emission spectrum of the emission center material may be a thin film or a solution, but a solution is preferred from the viewpoint of verifying the state of isolated molecules. A solvent with relatively low polarity, such as toluene or chloroform, is preferred for the solution. Also, in the case of phosphorescent compounds used as emission center materials, the phosphorescence spectrum can be observed even at room temperature. Therefore, the lowest triplet excitation energy level (T) can be calculated. 1 The temperature at which the energy level is measured can be low (for example, any temperature in the range of 4K to 80K) or room temperature (for example, 298K). The emission edge can be calculated by drawing a tangent line at the point where the slope on the short-wavelength side of the peak (or shoulder peak) observed at the shortest wavelength of the emission spectrum (phosphorescence spectrum) is maximum, and then taking the point where this tangent line intersects with the horizontal axis (wavelength) or baseline.

[0211] Furthermore, if no phosphorescent component is detected in the PL spectrum observed even at low temperatures in a thin film containing only the material to be measured, or in a solution to which only the material to be measured has been added, a phosphorescent sensitizer may be added. The phosphorescent sensitizer has a higher T than the material to be measured. 1 Phosphorescent materials having energy levels can be used. Specifically, Ir(ppy) 3 The following can be used.

[0212] Examples of materials that can be used as compounds exhibiting phosphorescence in the light-emitting layer 113 include the following. Other phosphorescent materials can also be used.

[0213] Tris{2-[5-(2-methylphenyl)-4-(2,6-dimethylphenyl)-4H-1,2,4-triazole-3-yl-κN2]phenyl-κC}Iridium(III) (Abbreviation: [Ir(mpptz-dmp)3 ]), Tris(5-methyl-3,4-diphenyl-4H-1,2,4-triazolato) iridium (III) (abbreviation: [Ir(Mptz) 3 ]) an organometallic iridium complex having a 4H-triazole skeleton, such as tris[3-methyl-1-(2-methylphenyl)-5-phenyl-1H-1,2,4-triazolato]iridium(III) (abbreviation: [Ir(Mptz1-mp) 3 ]), Tris(1-methyl-5-phenyl-3-propyl-1H-1,2,4-triazolato) Iridium(III) (abbreviation: [Ir(Prptz1-Me) 3 ]) an organometallic iridium complex having a 1H-triazole skeleton, such as fac-tris[1-(2,6-diisopropylphenyl)-2-phenyl-1H-imidazole]iridium(III) (abbreviation: [Ir(iPrpim) 3 ]), Tris[3-(2,6-dimethylphenyl)-7-methylimidazo[1,2-f]phenanthridine]iridium(III) (abbreviation: [Ir(dmpimpt-Me) 3 ]), organometallic iridium complexes having an imidazole skeleton such as tris(2-{1-[2,6-bis(1-methylethyl)phenyl]-1H-imidazole-2-yl-κN3}-4-cyanophenyl-κC) iridium(III) (abbreviation: CNImIr), tris[(6-tert-butyl-3-phenyl-2H-imidazol[4,5-b]pyrazine-1-yl-κC2)phenyl-κC] iridium(III) (abbreviation: [Ir(cb) 3 Organometallic iridium complexes having a benzimidazolidene skeleton such as ]), bis[2-(4',6'-difluorophenyl)pyridinato-N,C 2’ Iridium(III) tetrakis(1-pyrazolyl) borate (abbreviation: FIr6), bis[2-(4',6'-difluorophenyl)pyridinate-N,C 2’ Iridium(III) picolinate (abbreviation: FIrpic), bis{2-[3',5'-bis(trifluoromethyl)phenyl]pyridinate-N,C 2’ Iridium (III) picolinate (abbreviation: [Ir(CF) 3 ppy)2 (pic)]), bis[2-(4',6'-difluorophenyl)pyridinato-N,C 2’ iridium(III) acetylacetonate (abbreviation: FIracac), and other organometallic iridium complexes having a phenylpyridine derivative with an electron-withdrawing group as a ligand. Other examples include platinum complexes such as (2-{3-[3-(3,5-di-tert-butylphenyl)benzimidazol-1-yl-2-ylidene-κC2]phenoxy-κC2}-9-(4-tert-butyl-2-pyridinyl-κN)carbazole-2,1-diyl-κC1)platinum(II) (abbreviation: PtON-TBBI). These are compounds that exhibit blue phosphorescence, and are compounds having an emission peak in the wavelength range from 440 nm to 520 nm. In addition, compounds in which some of the hydrogen atoms in these compounds are replaced with deuterium can also be used.

[0214] Further, tris(4-methyl-6-phenylpyrimidinato)iridium(III) (abbreviation: [Ir(mppm) 3 ), tris(4-t-butyl-6-phenylpyrimidinato)iridium(III) (abbreviation: [Ir(tBuppm) 3 ), (acetylacetonato)bis(6-methyl-4-phenylpyrimidinato)iridium(III) (abbreviation: [Ir(mppm) 2 (acac)]), (acetylacetonato)bis(6-tert-butyl-4-phenylpyrimidinato)iridium(III) (abbreviation: [Ir(tBuppm) 2 (acac)]), (acetylacetonato)bis[6-(2-norbornyl)-4-phenylpyrimidinato]iridium(III) (abbreviation: [Ir(nbppm) 2 (acac)]), (acetylacetonato)bis[5-methyl-6-(2-methylphenyl)-4-phenylpyrimidinato]iridium(III) (abbreviation: [Ir(mpmppm) 2 (acac)]), (acetylacetonato)bis(4,6-diphenylpyrimidinato)iridium(III) (abbreviation: [Ir(dppm) 2Organometallic iridium complexes having a pyrimidine skeleton such as (acac) (acetylacetonato)bis(3,5-dimethyl-2-phenylpyradinato)iridium(III) (abbreviation: [Ir(mppr-Me) 2 (acac)), (acetylacetonato)bis(5-isopropyl-3-methyl-2-phenylpyradinato)iridium(III) (abbreviation: [Ir(mppr-iPr) 2 Organometallic iridium complexes having a pyrazine skeleton such as (acac), Tris(2-phenylpyridinato-N,C) 2’ Iridium (III) (abbreviation: [Ir(ppy) 3 ]), bis(2-phenylpyridinate-N,C 2’ Iridium (III) acetylacetonate (abbreviation: [Ir(ppy) 2 (acac)), bis(benzo[h]quinolinate)iridium(III)acetylacetonate (abbreviation: [Ir(bzq) 2 (acac)), Tris(benzo[h]quinolinate) Iridium(III) (abbreviation: [Ir(bzq) 3 ]), Tris(2-phenylquinolinato-N,C) 2’ Iridium (III) (abbreviation: [Ir(pq) 3 ]), bis(2-phenylquinolinato-N,C 2’ Iridium(III) acetylacetonate (abbreviation: [Ir(pq) 2 (acac)]), [2-d3-methyl-8-(2-pyridinyl-κN)benzofl[2,3-b]pyridine-κC]bis[2-(5-d 3 [-methyl-2-pyridinyl-κN2)phenyl-κC]iridium(III) (abbreviation: Ir(5mppy-d3) 2 (mbfpypy-d3)), {2-(methyl-d3)-8-[4-(1-methylethyl-1-d)-2-pyridinyl-κN]benzofl[2,3-b]pyridine-7-yl-κC}bis{5-(methyl-d 3 )-2-[5-(methyl-d 3 )-2-pyridinyl-κN]phenyl-κC}iridium(III) (abbreviation: Ir(5mtpy-d6) 2(mbfpypy-iPr-d4)), [2-(methyl-d3)-8-(2-pyridinyl-κN)benzofl[2,3-b]pyridine-κC]bis[2-(2-pyridinyl-κN)phenyl-κC]iridium(III) (abbreviation: Ir(ppy) 2 (mbfpypy-d3)), [2-(4-d 3 [methyl-5-phenyl-2-pyridinyl-κN2)phenyl-κC]bis[2-(5-d 3 [Methyl-2-pyridinyl-κN2)phenyl-κC]iridium(III) (abbreviation: [Ir(5mppy-d3) 2 (mdppy-d3)]), [2-methyl-8-(2-pyridinyl-κN)benzofl[2,3-b]pyridine-κC]bis[2-(2-pyridinyl-κN)phenyl-κC]iridium(III) (abbreviation: [Ir(ppy) 2 (mbfpypy))]), [2-(4-methyl-5-phenyl-2-pyridinyl-κN)phenyl-κC]bis[2-(2-pyridinyl-κN)phenyl-κC]iridium(III) (abbreviation: Ir(ppy) 2 (mdppy)), Tris{2-[5-(methyl-d3)-4-phenyl-2-pyridinyl-κN]phenyl-κC}Iridium(III) (abbreviation: Ir(5m4dppy-d 3 ) 3 In addition to organometallic iridium complexes with a pyridine skeleton such as tris(acetylacetonato)(monophenanthroline)terbium(III) (abbreviation: [Tb(acac) 3Rare earth metal complexes such as (Phen) (2-{1-(5-tert-butylbiphenyl-2-yl)-4-[3-tert-butyl-5-(4-phenyl-2-pyridinyl-κN)phenyl-κC6]-2-benzimidazolyl-κN3}-4,6-di-tert-butylphenolate-κO)platinum(II) (abbreviation: Pt(tBudpppymmtBubiz-tBubp) Examples of organometallic platinum complexes include [2-(4-(3,5-di-tert-butylphenyl)-6-{3-[4-(5'-tert-butyl[1,1':3',1''-terphenyl]-2'-yl)-2-pyridinyl-κN]phenyl-κC2}-2-pyridinyl-κN)phenolate-κO]platinum(II) (abbreviation: Pt(4tButpppypyp-mmtBup)). These are mainly compounds that exhibit green phosphorescence and have emission peaks in the wavelength range of 500 nm to 600 nm. Organometallic iridium complexes having a pyrimidine skeleton are particularly preferred due to their outstanding reliability and luminescence efficiency. Compounds in which some of the hydrogen atoms in these compounds are replaced with deuterium can also be used.

[0215] Also, (diisobutyrylmethanato)bis[4,6-bis(3-methylphenyl)pyrimidinato]iridium(III) (abbreviation: [Ir(5mdppm) 2 (dibm)]), bis[4,6-bis(3-methylphenyl)pyrimidinato](dipivaloylmethanato)iridium(III) (abbreviation: [Ir(5mdppm) 2 (dpm)]), bis[4,6-di(naphthalene-1-yl)pyrimidinato](dipivaloylmethanato)iridium(III) (abbreviation: [Ir(d1npm) 2 Organometallic iridium complexes having a pyrimidine skeleton such as (dpm)]), (acetylacetonato)bis(2,3,5-triphenylpyradinato)iridium(III) (abbreviation: [Ir(tppr) 2 (acac)), bis(2,3,5-triphenylpyrazinate)(dipivaloylmethanato) iridium(III) (abbreviation: [Ir(tppr) 2(dpm)]), (acetylacetonato)bis[2,3-bis(4-fluorophenyl)quinoxalinato]iridium(III) (abbreviation: [Ir(Fdpq) 2 Organometallic iridium complexes having a pyrazine skeleton such as (acac), tris(1-phenylisoquinolinato-N,C) 2’ Iridium (III) (abbreviation: [Ir(piq) 3 ]), bis(1-phenylisoquinolinato-N,C 2’ Iridium (III) acetylacetonate (abbreviation: [Ir(piq) 2 (acac)), (3,7-diethyl-4,6-nonanedionato-κO4,κO6)bis[2,4-dimethyl-6-[7-(1-methylethyl)-1-isoquinolinyl-κN]phenyl-κC]iridium(III), (3,7-diethyl-4,6-nonanedionato-κO4,κO6)bis[2,4-dimethyl-6-[5-(1-methylethyl)-2-quinolinyl-κN]phenyl In addition to organometallic iridium complexes with a pyridine skeleton such as [-κC]iridium(III), there are platinum complexes such as 2,3,7,8,12,13,17,18-octaethyl-21H,23H-porphyrin platinum(II) (abbreviation: PtOEP), and tris(1,3-diphenyl-1,3-propanedionato)(monophenanthroline)europium(III) (abbreviation: [Eu(DBM)] 3 (Phen)]), Tris[1-(2-tenoyl)-3,3,3-trifluoroacetonate](monophenanthroline) europium(III) (abbreviation: [Eu(TTA) 3 Examples include rare earth metal complexes such as (Phen)). These exhibit emission peaks in the wavelength range of 600 nm to 700 nm. Furthermore, organometallic iridium complexes with a pyrazine skeleton yield red emission with good chromaticity. Other known substances that exhibit red phosphorescence can also be used. Compounds in which some of the hydrogen atoms in these compounds are replaced with deuterium can also be used.

[0216] Next, a preferred configuration for the light-emitting layer 113_1 will be described when a fluorescent compound is used as the guest material 119_1. It is preferable to use a configuration in the light-emitting layer 113_1 that generates a TTA mechanism.

[0217] In the case of a light-emitting device that uses a fluorescent material in the light-emitting layer and utilizes the TTA mechanism to increase light-emitting efficiency, the lowest singlet excitation energy level (S) of the host material is important. 1 The level is the S of the fluorescent material. 1 Higher than the level, and the lowest triplet excitation energy level of the host material (T 1 The T level of a fluorescent material is 1 It is preferable that the luminescence level is lower than the host level. Furthermore, it is more preferable that the energy difference between the HOMO level of the host material and the HOMO level of the fluorescent material is 0.25 eV or more. In addition, it is preferable that the concentration of the fluorescent material in the luminescence layer is 0.5 wt% to 25 wt% relative to the host material. With this configuration, holes are more easily trapped in the luminescence layer, and carriers recombine locally in the region on the hole transport layer side of the luminescence layer, increasing the exciton density and thus improving the efficiency of TTA. Another configuration that enhances luminescence efficiency using TTA is that it is more preferable that the LUMO level of the fluorescent material is lower than the LUMO level of the host material. With this configuration, electrons are more easily trapped in the luminescence layer, and carriers recombine locally in the region on the hole transport layer side of the luminescence layer, increasing the exciton density and thus improving the efficiency of TTA.

[0218] The energies of the HOMO and LUMO levels used in this specification can be determined by electrochemical measurements. Typical examples of electrochemical measurements include square wave voltammetry (SWV), cyclic voltammetry (CV), and differential pulse voltammetry (DPV).

[0219] Specifically, in square wave voltammetry (SWV) measurements, the energies (E) of the HOMO and LUMO levels are obtained by changing the potential of the working electrode relative to the reference electrode. Oxidation peak potential (Ep ox ) and reduction peak potential (Ep red The default current obtained in square wave voltammetry (SWV) measurement is used. In the measurement, the HOMO level is determined from the positive potential scan and the LUMO level is determined from the negative potential scan.

[0220] For example, the parameters for measurement can be set as follows: potential increase Incr E (V) = 0.004, amplitude Amplitude (V) = 0.025, and frequency Frequency (Hz) = 15. The scan speed in the measurement can be calculated by multiplying the potential increase (Incr E (V)) by 2πf (where f is the frequency). Specifically, under these parameter settings, 0.004 (V) × 2 × π × 15 (1 / s) = 0.3768 (V / s), and the scan speed is 0.38 (V / s).

[0221] Furthermore, the specific procedures for calculating the HOMO and LUMO levels will be explained. The oxidation peak potential (Ep) obtained from the rectangular wave voltammogram of the material is... ox ), or reduction peak potential (Ep red ) is determined, and the potential energy (E) of the reference electrode with respect to the vacuum level is calculated. x By subtracting from ), the HOMO level ((E) = Ex - Ep ox ), and the energy of the LUMO level ((E) = Ex - Ep red ) can be calculated for each of these.

[0222] Furthermore, in cyclic voltammetry (CV) measurements, the energy (E) of the HOMO and LUMO levels is obtained by changing the oxidation peak potential (E) relative to the reference electrode. pa ), and reduction peak potential (E pc It can be calculated based on the following. In the measurement, the HOMO level is determined from the positive potential scan and the LUMO level is determined from the negative potential scan. The scan speed in the measurement is set to 0.1 V / s.

[0223] This section describes the specific procedure for calculating the HOMO and LUMO levels using CV measurements. The oxidation peak potential (E) obtained from the cyclic voltammogram of the material is then described. pa ), and reduction peak potential (E pc ) From the standard oxidation-reduction potential (E o ) (=(E pa +E pc ) / 2) is calculated, and the potential energy (E) of the reference electrode with respect to the vacuum level is calculated.x By subtracting from ), the energy (E) (= Ex - Eo) of the HOMO level and the LUMO level can be determined, respectively.

[0224] Note that the above shows the case where a reversible redox wave is obtained, but when an irreversible redox wave is obtained, the oxidation peak potential (E) is used to calculate the HOMO level. pa The reduced peak potential (E) is obtained by subtracting a certain value (0.1 eV) from the value obtained by subtracting a certain value (0.1 eV) from the value obtained by subtracting a certain value (0.1 eV) from the value obtained by subtracting a certain value (E pc ) Assuming the standard oxidation-reduction potential (E o ) is calculated to one decimal place. Also, the reduction peak potential (E) is used to calculate the LUMO level. pc The oxidation peak potential (E) is calculated by adding a constant value (0.1 eV) to the value obtained). pa ) Assuming the standard oxidation-reduction potential (E o Calculate the result to one decimal place.

[0225] Note S 1 Levels and T 1 The energy levels can be determined by using values ​​calculated from the emission edge of the phosphorescence or fluorescence spectrum and the absorption edge of the absorption spectrum, as described above.

[0226] Examples of materials that can be used as fluorescent light-emitting substances in the light-emitting layer 113 include the following. Other fluorescent light-emitting substances can also be used.

[0227] 5,6-bis[4-(10-phenyl-9-antryl)phenyl]-2,2'-bipyridine (abbreviation: PAPP2BPy), 5,6-bis[4'-(10-phenyl-9-antryl)biphenyl-4-yl]-2,2'-bipyridine (abbreviation: PAPP2BPy), N,N'-diphenyl-N,N'-bis[4-(9-phenyl-9H-fluoren-9-yl)phenyl]pyren-1,6-diamine (abbreviation: 1,6FLPAPrn), N,N'-bis(3-methylphenyl)-N,N'-bis[3-(9-phenyl-9H-fluoren-9-yl] )phenyl]pyrene-1,6-diamine (abbreviation: 1,6mMemFLPAPrn), N,N'-bis[4-(9H-carbazole-9-yl)phenyl]-N,N'-diphenylstilbene-4,4'-diamine (abbreviation: YGA2S), 4-(9H-carbazole-9-yl)-4'-(10-phenyl-9-anthryl)triphenylamine (abbreviation: YGAPA), 4-(9H-carbazole-9-yl)-4'-(9,10-diphenyl-2-anthryl)triphenylamine (abbreviation: 2YGAAPPA), N,9-diphenyl-N-[4-( 10-phenyl-9-anthryl)phenyl]-9H-carbazole-3-amine (abbreviation: PCAPA), perylene, 2,5,8,11-tetra-tert-butylperylene (abbreviation: TBP), 4-(10-phenyl-9-anthryl)-4'-(9-phenyl-9H-carbazole-3-yl)triphenylamine (abbreviation: PCBAPA), N,N''-(2-tert-butylanthracene-9,10-diyldi-4,1-phenylene)bis(N,N',N'-triphenyl-1,4-phenylenediamine) (abbreviation: DPABPA), N,9 -Diphenyl-N-[4-(9,10-diphenyl-2-anthryl)phenyl]-9H-carbazole-3-amine (abbreviation: 2PCAPPA), N-[4-(9,10-diphenyl-2-anthryl)phenyl]-N,N',N'-triphenyl-1,4-phenylenediamine (abbreviation: 2DPAPPA), N,N,N',N',N'',N'',N''',N'''-octaphenyldibenzo[g,p]chrysene-2,7,10,15-tetraamine (abbreviation: DBC1), coumarin 30, N-(9,10-diphenyl-2-anthryl)-N,9-diphenyl-9H-carbazole-3-amine (abbreviation: 2PCAPA), N-[9,10-bis(biphenyl-2-yl)-2-anthryl]-N,9-diphenyl-9H-carbazole-3-amine (abbreviation: 2PCABPhA), N-(9,10-diphenyl-2-anthryl)-N,N',N'-triphenyl-1,4-phenylenediamine (abbreviation: 2DPAPA), N-[9,10-bis(biphenyl-2-yl)-2-anthryl]-N,N',N'-triphenyl-1,4-phenylenediamine (abbreviation: 2DPABPhA) 9,10-bis(biphenyl-2-yl)-N-[4-(9H-carbazole-9-yl)phenyl]-N-phenylanthracene-2-amine (abbreviation: 2YGABPhA), N,N,9-triphenylanthracene-9-amine (abbreviation: DPhAPhA), coumarin 545T, N,N'-diphenylquinacridone (abbreviation: DPQd), rubren, 5,12-bis(biphenyl-4-yl)-6,11-diphenyltetracene (abbreviation: BPT), 2-(2-{2-[4-(dimethylamino)phenyl]ethenyl}-6-methyl-4H-pyra N-4-ylidene)propanedinitrile (abbreviation: DCM1), 2-{2-methyl-6-[2-(2,3,6,7-tetrahydro-1H,5H-benzo[ij]quinoridine-9-yl)ethenyl]-4H-pyran-4-ylidene}propanedinitrile (abbreviation: DCM2), N,N,N',N'-tetrakis(4-methylphenyl)tetracene-5,11-diamine (abbreviation: p-mPhTD), 7,14-diphenyl-N,N,N',N'-tetrakis(4-methylphenyl)acenaphtho[1,2-a]fluorantene-3,10-diamine (abbreviation) Name: p-mPhAFD), 2-{2-isopropyl-6-[2-(1,1,7,7-tetramethyl-2,3,6,7-tetrahydro-1H,5H-benzo[ij]quinoridine-9-yl)ethenyl]-4H-pyran-4-ylidene}propanedinitrile (abbreviation: DCJTI), 2-{2-tert-butyl-6-[2-(1,1,7,7-tetramethyl-2,3,6,7-tetrahydro-1H,5H-benzo[ij]quinoridine-9-yl)ethenyl]-4H-pyran-4-ylidene}propanedinitrile (abbreviation: DCJTB), 2-(2,6-bis{2-[4-(dimethylamino)phenyl]ethenyl}-4H-pyran-4-ylidene)propanedinitrile (abbreviation: BisDCM), 2-{2,6-bis[2-(8-methoxy-1,1,7,7-tetramethyl-2,3,6,7-tetrahydro-1H,5H-benzo[ij]quinoridine-9-yl)ethenyl]-4H-pyran-4-ylidene}propanedinitrile (abbreviation: BisDCJTM), N,N'-diphenyl-N,N'-(1,6-pyrene-diyl)bis[(6-phenylbenzo[b]naph Examples include to[1,2-d]furan)-8-amine] (abbreviation: 1,6BnfAPrn-03), N,N'-diphenyl-N,N'-bis(9-phenyl-9H-carbazole-2-yl)naphtho[2,3-b;6,7-b']bisbenzofuran-3,10-diamine (abbreviation: 3,10PCA2Nbf(IV)-02), and 3,10-bis[N-(dibenzofuran-3-yl)-N-phenylamino]naphtho[2,3-b;6,7-b']bisbenzofuran (abbreviation: 3,10FrA2Nbf(IV)-02). In particular, condensed aromatic diamine compounds, such as pyrenediamine compounds like 1,6FLPAPrn, 1,6mMemFLPAPrn, and 1,6BnfAPPrn-03, are preferred because they exhibit high hole-trapping properties and excellent luminescence efficiency or reliability.

[0228] Also, 5,9-diphenyl-5,9-diaza-13b-boranaphtho[3,2,1-de]anthracene (abbreviation: DABNA-1), 9-(biphenyl-3-yl)-N,N,5,11-tetraphenyl-5H,9H-[1,4]benzazavolino[2,3,4-kl]phenazavolin-3-amine (abbreviation: DABNA-2), 2,12-di(tert-butyl)-5,9-di(4-tert-butylphenyl)-N,N-diphenyl Lu-5H,9H-[1,4]benzazabolino[2,3,4-kl]phenazabolin-7-amine (abbreviation: DPhA-tBu4DABNA), 2,12-di(tert-butyl)-N,N,5,9-tetra(4-tert-butylphenyl)-5H,9H-[1,4]benzazabolino[2,3,4-kl]phenazabolin-7-amine (abbreviation: tBuDPhA-tBu4DABNA), 2,12-di(tert-butyl)-5, 9-di(4-tert-butylphenyl)-7-methyl-5H,9H-[1,4]benzazabolino[2,3,4-kl]phenazabolin (abbreviation: Me-tBu4DABNA), N7,N7,N13,N13,5,9,11,15-octaphenyl-5H,9H,11H,15H-[1,4]benzazabolino[2,3,4-kl][1,4]benzazabolino[4',3',2':4,5][1,4]benzazabolino[3,2 Condensed heteroaromatic compounds containing nitrogen and boron, such as -b]phenazavolin-7,13-diamine (abbreviated as ν-DABNA) and 2-(4-tert-butylphenyl)benz[5,6]indro[3,2,1-jk]benzo[b]carbazole (abbreviated as tBuPBibc), particularly compounds having a diaza-boranaphtho-anthracene skeleton, can be suitably used because they produce blue emission with a narrow emission spectrum and good color purity.

[0229] In addition to these, 9,10,11-tris[3,6-bis(1,1-dimethylethyl)-9H-carbazolyl-9-yl]-2,5,15,18-tetrakis(1,1-dimethylethyl)indoro[3,2,1-de]indoro[3',2',1':8,1][1,4]benzazaborino[2,3,4-kl]phenazavolin (abbreviation: BBCz-G), 9,11-bis[ Compounds having an indole skeleton, such as 3,6-bis(1,1-dimethylethyl)-9H-carbazolyl-9-yl]-2,5,15,18-tetrakis(1,1-dimethylethyl)indro[3,2,1-de]indro[3',2',1':8,1][1,4]benzazavolino[2,3,4-kl]phenazavolin (abbreviation: BBCz-Y), can be suitably used.

[0230] As an electron transport material used in the host material 118 (host material 118_1 and host material 118_2) of the light-emitting layer 113 (light-emitting layer 113_1 and light-emitting layer 113_2), for example, bis(10-hydroxybenzo[h]quinolinato)beryllium(II) (abbreviation: BeBq) 2Metal complexes such as bis(2-methyl-8-quinolinolato)(4-phenylphenololato)aluminum(III) (abbreviated as BAlq), bis(8-quinolinolato)zinc(II) (abbreviated as Znq), bis[2-(2-benzoxazollyl)phenololato]zinc(II) (abbreviated as ZnPBO), and bis[2-(2-benzothiazolyl)phenololato]zinc(II) (abbreviated as ZnBTZ), as well as organic compounds having a π-electron-deficient heteroaromatic ring, can be used. Examples of organic compounds having a π-electron-deficient heteroaromatic ring include 2-(4-biphenyl)-5-(4-tert-butylphenyl)-1,3,4-oxadiazole (abbreviated as PBD), 3-(4-biphenylyl)-4-phenyl-5-(4-tert-butylphenyl)-1,2,4-triazole (abbreviated as TAZ), and 1,3-bis[5-(4-tert-butylphenyl)-1,3,4-oxadiazole-2-yl]benzene (abbreviated as Azole skeletons such as OXD-7), 9-[4-(5-phenyl-1,3,4-oxadiazole-2-yl)phenyl]-9H-carbazole (abbreviation: CO11), 2,2',2''-(1,3,5-benzenetriyl)tris(1-phenyl-1H-benzimidazole) (abbreviation: TPBI), and 2-[3-(dibenzothiophen-4-yl)phenyl]-1-phenyl-1H-benzimidazole (abbreviation: mDBTBIm-II) Organic compounds containing heteroaromatic rings, such as 2-[3-(dibenzothiophen-4-yl)phenyl]dibenzo[f,h]quinoxaline (abbreviation: 2mDBTBPDBq-II), 2-[3'-(dibenzothiophen-4-yl)biphenyl-3-yl]dibenzo[f,h]quinoxaline (abbreviation: 2mDBTBPBQ-II), and 2-[3'-(9H-carbazole-9-yl)biphenyl-3-yl]dibenzo[f,h]quinoxaline (abbreviation: 2m CzBPDBq), 4,6-bis[3-(phenanthren-9-yl)phenyl]pyrimidine (abbreviation: 4,6mPnP2Pm), 4,6-bis[3-(dibenzothiophen-4-yl)phenyl]pyrimidine (abbreviation: 4,6mDBTP2Pm-II), 2,4-bis[4-(1-naphthyl)phenyl]-6-[4-(3-pyridyl)phenyl]pyrimidine (abbreviation: 2,4NP-6PyPPm), 6-(biphenyl-3-yl)-4-[3,Organic compounds containing heteroaromatic rings with a diazine skeleton, such as 5-bis(9H-carbazole-9-yl)phenyl]-2-phenylpyrimidine (abbreviation: 6mBP-4Cz2PPm), 4-[3,5-bis(9H-carbazole-9-yl)phenyl]-2-phenyl-6-(biphenyl-4-yl)pyrimidine (abbreviation: 6BP-4Cz2PPm), and 7-[4-(9-phenyl-9H-carbazole-2-yl)quinazoline-2-yl]-7H-dibenzo[c,g]carbazole (abbreviation: PC-cgDBCzQz), and 3,5-bis[3-(9 Organic compounds containing heteroaromatic rings with a pyridine skeleton, such as H-carbazole-9-yl)phenyl]pyridine (abbreviation: 35DCzPPy), 1,3,5-tri[(3-pyridyl)phenyl-3-yl]benzene (abbreviation: TmPyPB), 2-[3'-(9,9-dimethyl-9H-fluoren-2-yl)biphenyl-3-yl]-4,6-diphenyl-1,3,5-triazine (abbreviation: mFBPTZn), 2-(biphenyl-4-yl)-4-phenyl-6-(9,9'-spirobio[9H-fluoren]-2-yl)-1,3,5-triazine Zin (abbreviation: BP-SFTZn), 2-{3-[3-(benzo[b]naphtho[1,2-d]furan-8-yl)phenyl]phenyl}-4,6-diphenyl-1,3,5-triazine (abbreviation: mBnfBPTZn), 2-{3-[3-(benzo[b]naphtho[1,2-d]furan-6-yl)phenyl]phenyl}-4,6-diphenyl-1,3,5-triazine (abbreviation: mBnfBPTZn-02), 5-[3-(4,6-diphenyl-1,3,5-triazine-2-yl)phenyl]-7,7-dimethyl-5H,7H-indeno[2, 1-b]carbazole (abbreviation: mINc(II)PTZn), 2-[3'-(triphenylene-2-yl)biphenyl-3-yl]-4,6-diphenyl-1,3,5-triazine (abbreviation: mTpBPTZn), 3-[9-(4,6-diphenyl-1,3,5-triazine-2-yl)-2-dibenzofuranyl]-9-phenyl-9H-carbazole (abbreviation: PCDBfTZn), 2-(biphenyl-3-yl)-4-phenyl-6-[8-([1,1':4',1''-terphenyl]-4-yl)-1-dibenzofuranyl]-1,3,Examples include organic compounds containing heteroaromatic rings having a triazine skeleton, such as 5-triazine (abbreviated as mBP-TPDBfTZn). Among those mentioned above, organic compounds containing heteroaromatic rings having a diazine skeleton, organic compounds containing heteroaromatic rings having a pyridine skeleton, and organic compounds containing heteroaromatic rings having a triazine skeleton are preferred due to their good reliability. In particular, organic compounds containing heteroaromatic rings having a diazine (pyrimidine and pyrazine) skeleton and organic compounds containing heteroaromatic rings having a triazine skeleton exhibit high electron transport properties and contribute to reducing the driving voltage.

[0231] As the hole transport material used in the host material 118 (host material 118_1 and host material 118_2) of the light-emitting layer 113 (light-emitting layer 113_1 and light-emitting layer 113_2), an organic compound having an amine skeleton or a π-electron-rich heteroaromatic ring can also be used. Examples of such organic compounds having an amine skeleton or a π-electron-rich heteroaromatic ring include 4,4'-bis[N-(1-naphthyl)-N-phenylamino]biphenyl (abbreviated as NPB), N,N'-diphenyl-N,N'-bis(3-methylphenyl)-4,4'-diaminobiphenyl (abbreviated as TPD), N,N'-bis(9,9'-spirobi[9H-fluoren]-2-yl)-N,N'-diphenyl-4,4'-diaminobiphenyl (abbreviated as BSPB), and 4-phenyl-4'-(9-phenyl Phenylfluoren-9-yl)triphenylamine (abbreviation: BPAFLP), 4-phenyl-3'-(9-phenylfluoren-9-yl)triphenylamine (abbreviation: mBPAFLP), 4-phenyl-4'-(9-phenyl-9H-carbazole-3-yl)triphenylamine (abbreviation: PCBA1BP), 4,4'-diphenyl-4''-(9-phenyl-9H-carbazole-3-yl)triphenylamine (abbreviation: PCBi1BP), 4-(1-naphthyl)-4'-(9- Phenyl-9H-carbazole-3-yl)triphenylamine (abbreviation: PCBANB), 4,4'-di(1-naphthyl)-4''-(9-phenyl-9H-carbazole-3-yl)triphenylamine (abbreviation: PCBNBB), 9,9-dimethyl-N-phenyl-N-[4-(9-phenyl-9H-carbazole-3-yl)phenyl]fluoren-2-amine (abbreviation: PCBAF), N-phenyl-N-[4-(9-phenyl-9H-carbazole-3-yl)phenyl]-9, Compounds having an aromatic amine skeleton such as 9'-spirobi[9H-fluorene]-2-amine (abbreviated as PCBASF), compounds having a carbazole skeleton such as 1,3-bis(N-carbazolyl)benzene (abbreviated as mCP), 4,4'-di(N-carbazolyl)biphenyl (abbreviated as CBP), 3,6-bis(3,5-diphenylphenyl)-9-phenylcarbazole (abbreviated as CzTP), 9,9'-diphenyl-9H,9'H-3,3'-bicarbazole (abbreviated as PCCP), 4,4',Examples include compounds having a thiophene skeleton such as 4''-(benzene-1,3,5-triyl)tri(dibenzothiophene) (abbreviation: DBT3P-II), 2,8-diphenyl-4-[4-(9-phenyl-9H-fluoren-9-yl)phenyl]dibenzothiophene (abbreviation: DBTFLP-III), and 4-[4-(9-phenyl-9H-fluoren-9-yl)phenyl]-6-phenyldibenzothiophene (abbreviation: DBTFLP-IV), and compounds having a furan skeleton such as 4,4',4''-(benzene-1,3,5-triyl)tri(dibenzofuran) (abbreviation: DBF3P-II) and 4-{3-[3-(9-phenyl-9H-fluoren-9-yl)phenyl]phenyl}dibenzofuran (abbreviation: mmDBFFLBi-II). Among those mentioned above, compounds having an aromatic amine skeleton or a carbazole skeleton are preferred because they offer good reliability, high hole transport properties, and contribute to reducing the driving voltage. Furthermore, the organic compounds listed as examples of hole-transporting materials in the hole transport layer 112 can also be used as hole transport materials for the host.

[0232] Furthermore, by mixing electron transport material and hole transport material, the transport properties of the light-emitting layer 113 can be easily adjusted, and the recombination region can be easily controlled.

[0233] Furthermore, TADF materials can also be used as electron transport materials or hole transport materials. The TADF materials listed above can be used as host materials 118 (host material 118_1 and host material 118_2). When a TADF material is used as a host material, the triplet excitation energy generated by the TADF material is converted to singlet excitation energy through reverse intersystem crossing, and this energy is then transferred to the light-emitting material, thereby increasing the luminescence efficiency of the light-emitting device. In this case, the TADF material functions as an energy donor, and the light-emitting material functions as an energy acceptor.

[0234] This is very effective when the above-mentioned luminescent material is a fluorescent luminescent material. Also, in order to obtain high luminescence efficiency in this case, the S of the TADF material 1The energy level is S of the fluorescent material. 1 It is preferable that the level be higher than the level. Also, the T of the TADF material 1 The energy level is S of the fluorescent material. 1 It is preferable that the level be higher than the level of the TADF material. 1 The energy level is the T of the fluorescent material. 1 A level higher than the current level is preferable.

[0235] Furthermore, it is preferable to use a TADF material that exhibits emission that overlaps with the wavelength of the lowest-energy absorption band of the fluorescent material. This is preferable because it allows for a smooth transfer of excitation energy from the TADF material to the fluorescent material, resulting in efficient emission.

[0236] Furthermore, for singlet excitation energy to be efficiently generated from triplet excitation energy by reverse intersystem crossing, it is preferable that carrier recombination occurs in the TADF material. It is also preferable that the triplet excitation energy generated in the TADF material does not transfer to the triplet excitation energy of the fluorescent material. To achieve this, it is preferable that the fluorescent material has protecting groups around the luminescent phosphoform (the skeleton that causes luminescence). Preferred protecting groups are substituents without π bonds, and saturated hydrocarbons are preferred. Specifically, examples include alkyl groups having 3 to 10 carbon atoms, substituted or unsubstituted cycloalkyl groups having 3 to 10 carbon atoms, and trialkylsilyl groups having 3 to 10 carbon atoms. It is even more preferable to have multiple protecting groups. Substituents without π bonds have poor carrier transport function, and therefore can increase the distance between the TADF material and the luminescent phosphoform of the fluorescent material with little effect on carrier transport and carrier recombination. Here, the luminescent phosphoform refers to the atomic group (skeleton) that causes luminescence in the fluorescent material. The luminescent phosphophore preferably has a skeleton containing π bonds, preferably contains an aromatic ring, and preferably has a condensed aromatic ring or a condensed heteroaromatic ring. Examples of such luminescent phosphophores include phenanthrene skeletons, stilbene skeletons, acridone skeletons, phenoxazine skeletons, phenothiazine skeletons, naphthalene skeletons, anthracene skeletons, fluorene skeletons, chrysene skeletons, triphenylene skeletons, tetracene skeletons, pyrene skeletons, perylene skeletons, coumarin skeletons, quinacridone skeletons, and naphthobisbenzofuran skeletons. Fluorescent materials having naphthalene, anthracene, fluorene, chrysene, triphenylene, tetracene, pyrene, perylene, coumarin, quinacridone, and naphthobisbenzofuran skeletons are particularly preferred due to their high fluorescence quantum yield.

[0237] Furthermore, when a fluorescent material is used as the luminescent material in the guest material 119_1 of the luminescent layer 113_1, it is more preferable to use polycyclic aromatic hydrocarbons such as anthracene derivatives, tetracene derivatives, phenanthrene derivatives, pyrene derivatives, chrysene derivatives, and dibenzo[g,p]chrysene derivatives as the host material 118_1, which are organic compounds with a high energy level in the singlet excited state and a low energy level in the triplet excited state. Materials having an anthracene skeleton are particularly preferred. When a substance having an anthracene skeleton is used as the host material for the fluorescent material, it is possible to realize a luminescent layer with good luminescence efficiency and durability. As a substance having an anthracene skeleton to be used as the host material, a diphenylanthracene skeleton, and especially a substance having a 9,10-diphenylanthracene skeleton, is preferred because it is chemically stable. Examples of such substances include organic compounds having heteroaromatic rings and aromatic compounds consisting of aromatic hydrocarbons. Examples of organic compounds having heteroaromatic rings include 9-phenyl-3-[4-(10-phenyl-9-antryl)phenyl]-9H-carbazole (abbreviated as PCzPA), 3-[4-(1-naphthyl)phenyl]-9-phenyl-9H-carbazole (abbreviated as PCPN), 9-[4-(10-phenyl-9-antryl)phenyl]-9H-carbazole (abbreviated as CzPA), and 7-[4-(10-phenyl-9-antryl)phenyl]-7H-dibenzo[c,g]carbazole (abbreviated as c gDBCzPA), 6-[3-(9,10-diphenyl-2-anthryl)phenyl]benzo[b]naphtho[1,2-d]furan (abbreviation: 2mBnfPPA), 2-(10-phenyl-9-anthryl)benzo[b]naphtho[2,3-d]furan (abbreviation: Bnf(II)PhA), 1-{4-[10-(biphenyl-4-yl)-9-anthryl]phenyl}-2-ethyl-1H-benzimidazole (abbreviation: EtBImPBPhA), 1-[10-(phenyl-2,3,4,5,6-d 5 )-9-anthryl]benzo[b]naphtho[2,3-d]furan (abbreviation: Bnf(II)PhA-02-d5), and 7-(phenyl-2,3,4,5,6-d 5 )-1-[10-(phenyl-2,3,4,5,6-d 5)-9-anthryl]dibenzofuran (abbreviation: PDBfPhA-d 10 Examples of aromatic compounds consisting of aromatic hydrocarbons include 9-phenyl-10-[4'-(9-phenyl-9H-fluoren-9-yl)biphenyl-4-yl]anthracene (abbreviation: FLPPA), 9-(1-naphthyl)-10-(2-naphthyl)anthracene (abbreviation: α,βADN), 2-(10-phenylanthracene-9-yl)dibenzofuran, 9-(2-naphthyl)-10-[3-(2-naphthyl)phenyl]anthracene (abbreviation: βN-mβNPAnth), 9-(1-naphthyl)-10-[4-(2-naphthyl)phenyl]anthracene (abbreviation: αN-βNPAnth), and 2,9-di(1-naphthyl)-10-phenylanthracene (abbreviation: 2αN-αNPhA). The light hydrogen atoms in these organic compounds having heteroaromatic rings and aromatic compounds consisting of aromatic hydrocarbons may each be independently deuterium.

[0238] Furthermore, an excitation complex may be formed between the mixed materials described above. It is preferable to select a combination of materials that forms an excitation complex that exhibits emission overlapping with the wavelength of the lowest-energy absorption band of the luminescent material, as this facilitates smooth energy transfer and efficiently obtains light emission. This configuration is also preferable because it reduces the driving voltage.

[0239] Furthermore, at least one of the materials forming the excitation complex may be a phosphorescent material. This allows for the efficient conversion of the triplet excitation energy to the singlet excitation energy through reverse intersystem crossing.

[0240] For efficient excitation complex formation, it is preferable that the HOMO level of the hole-transporting material is at or above the HOMO level of the electron-transporting material. Furthermore, it is preferable that the LUMO level of the hole-transporting material is at or above the LUMO level of the electron-transporting material.

[0241] The formation of excited complexes can be confirmed, for example, by comparing the emission spectra of a hole-transporting material, an electron-transporting material, and a mixed film made by mixing these materials, and observing that the emission spectrum of the mixed film shifts to a longer wavelength than the emission spectra of each individual material (or has a new peak on the longer wavelength side). Alternatively, it can be confirmed by comparing the transient photoluminescence (PL) of a hole-transporting material, the transient PL of an electron-transporting material, and the transient PL of a mixed film made by mixing these materials, and observing differences in the transient response, such as the transient PL lifetime of the mixed film having a longer lifetime component or a larger proportion of the delayed component than the transient PL lifetime of each individual material. Furthermore, the transient PL mentioned above may be read as transient electroluminescence (EL). That is, the formation of excited complexes can also be confirmed by comparing the transient EL of a hole-transporting material, the transient EL of an electron-transporting material, and the transient EL of a mixed film made by mixing these materials, and observing the differences in the transient response.

[0242] Next, we will describe a preferred configuration for the light-emitting layer 113_2 in which a fluorescent compound is used as the guest material 119_1, and in which the TADF mechanism is likely to occur.

[0243] TADF is S 1 Level and T 1 In systems with a very small energy difference between levels, a small amount of thermal energy can cause a reverse intersystem crossing from triplet excitation energy to singlet excitation energy, and fluorescence emission is generated from the converted singlet excitation energy. Therefore, it is possible to upconvert (reverse intersystem crossing) triplet excitation energy to singlet excitation energy, and singlet excited states can be efficiently generated. Furthermore, triplet excitation energy can be converted into luminescence. Materials exhibiting the TADF mechanism are sometimes called TADF materials.

[0244] The TADF mechanism may manifest with only one substance or with two substances. Note that the excited complex (also called an exciplex) formed by two substances is S 1 Level and T 1It has an extremely small energy difference with the energy level and functions as a TADF material capable of converting triplet excitation energy into singlet excitation energy.

[0245] Note, - 1 The level indicator can be calculated using the emission edge of the phosphorescence spectrum observed at low temperatures (for example, any temperature in the range of 4K to 80K). 1 As an indicator of the energy level, the emission edge of the PL spectrum measured at low temperature (e.g., any temperature in the range of 4K to 80K) or at room temperature can be used. Furthermore, the S of the fluorescent material... 1 As an indicator of the energy level, an absorption spectrum measured at room temperature can also be used. For example, if an absorption spectrum is measured at room temperature, the energy at the absorption edge on the longer wavelength side can be defined as S. 1 It can also be considered as an energy level. The absorption edge on the long-wavelength side of the absorption spectrum can be calculated by drawing a tangent line at the point where the slope on the long-wavelength side of the peak (or shoulder peak) observed at the longest wavelength of the absorption spectrum is minimum (maximum absolute value), and then taking the intersection of that tangent line with the horizontal axis (wavelength) or baseline. 1 Level and T 1 For comparing energy levels, it is particularly preferable to compare the emission edge of the fluorescence spectrum with the emission edge of the phosphorescence spectrum. 1 Level and T 1 The energy difference between the levels is preferably 0.3 eV or less, and more preferably 0.2 eV or less.

[0246] Furthermore, when using TADF material as a light-emitting material, the S of the host material 1 The level is S of the TADF material. 1 A higher level is preferable. Also, the T of the host material 1 The level is T of the TADF material. 1 A level higher than the current level is preferable.

[0247] As TADF materials, fullerenes and their derivatives, acridines and their derivatives, eosin derivatives, etc., can be used. Also, metal-containing porphyrins containing magnesium (Mg), zinc (Zn), cadmium (Cd), tin (Sn), platinum (Pt), indium (In), or palladium (Pd) can be used. As a metal-containing porphyrin, for example, the protoporphyrin-tin fluoride complex (SnF) shown in the following structural formula is used. 2 (Proto IX)), Mesoporphyrin-Tin Fluoride Complex (SnF 2 (Meso IX), hematoporphyrin-tin fluoride complex (SnF 2 (Hemato IX), coproporphyrin tetramethyl ester-tin fluoride complex (SnF 2 (Copro III-4Me)), Octaethylporphyrin-Tin Fluoride Complex (SnF 2 (OEP)), Ethioporphyrin-Tin Fluoride Complex (SnF 2 (Etio I)), Octaethylporphyrin-Platinum Chloride Complex (PtCl 2 OEP (Open Economic Programme) is another example.

[0248]

[0249] Furthermore, the following structural formulas represent 2-(biphenyl-4-yl)-4,6-bis(12-phenylindoro[2,3-a]carbazol-11-yl)-1,3,5-triazine (abbreviation: PIC-TRZ), 9-(4,6-diphenyl-1,3,5-triazin-2-yl)-9'-phenyl-9H,9'H-3,3'-bicarbazole (abbreviation: PCCzTZn), 9-[4-(4,6-diphenyl-1,3,5-triazin-2-yl)phenyl]-9'-phenyl-3,3'-bi-9H-carbazole (abbreviation: PCCzPTZn), and 2-[4-(10H-phenoxazine-10-yl)phenyl]-4,6-diphenyl-1,3,5-triazine (abbreviation: PXZ). Heterocyclic compounds having one or both of a π-electron-rich heteroaromatic ring and a π-electron-deficient heteroaromatic ring can also be used, such as -TRZ), 3-[4-(5-phenyl-5,10-dihydrophenadin-10-yl)phenyl]-4,5-diphenyl-1,2,4-triazole (abbreviated as PPZ-3TPT), 3-(9,9-dimethyl-9H-acridine-10-yl)-9H-xanthene-9-one (abbreviated as ACRXTN), bis[4-(9,9-dimethyl-9,10-dihydroacridine)phenyl]sulfone (abbreviated as DMAC-DPS), and 10-phenyl-10H,10'H-spiro[acridine-9,9'-anthracene]-10'-one (abbreviated as ACRSA). The heterocyclic compound is preferred because it has both a π-electron-excess heteroaromatic ring and a π-electron-deficient heteroaromatic ring, resulting in high electron transport and hole transport properties. Among the skeletons having a π-electron-deficient heteroaromatic ring, the pyridine skeleton, diazine skeleton (pyrimidine skeleton, pyrazine skeleton, pyridazine skeleton), and triazine skeleton are preferred because they are stable and reliable. In particular, the benzoflopyrimidine skeleton, benzothienopyrimidine skeleton, benzoflopyrazine skeleton, and benzothienopyrazine skeleton are preferred because they have high acceptability and are reliable. Furthermore, among the skeletons having a π-electron-excess heteroaromatic ring, the acridine skeleton, phenoxazine skeleton, phenothiazine skeleton, furan skeleton, thiophene skeleton, and pyrrole skeleton are preferred because they are stable and reliable, and therefore it is preferable to have at least one of these skeletons.Furthermore, a dibenzofuran skeleton is preferred as the furan skeleton, and a dibenzothiophene skeleton is preferred as the thiophene skeleton. In addition, an indole skeleton, carbazole skeleton, indrocarbazole skeleton, bicarbazole skeleton, and 3-(9-phenyl-9H-carbazole-3-yl)-9H-carbazole skeleton are particularly preferred as the pyrrole skeleton. Furthermore, in a substance in which a π-electron-rich heteroaromatic ring and a π-electron-deficient heteroaromatic ring are directly bonded, both the electron-donating ability of the π-electron-rich heteroaromatic ring and the electron-accepting ability of the π-electron-deficient heteroaromatic ring are strengthened. 1 Level and T 1 This is particularly preferable because the energy difference between the energy levels becomes small, allowing for efficient acquisition of thermally activated delayed fluorescence. Alternatively, an aromatic ring to which an electron-withdrawing group such as a cyano group is attached may be used instead of the π-electron-deficient heteroaromatic ring. Furthermore, aromatic amine skeletons, phenazine skeletons, etc., can be used as the π-electron-rich skeleton. Additionally, boron-containing skeletons such as xanthene skeletons, thioxanthene dioxide skeletons, oxadiazole skeletons, triazole skeletons, imidazole skeletons, anthraquinone skeletons, boron-containing skeletons such as phenylborane or volanthrene, aromatic rings or heteroaromatic rings having a nitrile group or a cyano group such as benzonitrile or cyanobenzene, carbonyl skeletons such as benzophenone, phosphine oxide skeletons, sulfone skeletons, etc. Thus, a π-electron-deficient skeleton and a π-electron-rich skeleton can be used instead of at least one of the π-electron-deficient heteroaromatic ring and the π-electron-rich heteroaromatic ring.

[0250]

[0251] Furthermore, a TADF material may be used that enables extremely fast and reversible intersystem crossing, and in which the singlet and triplet excited states emit light according to a thermal equilibrium model. Such a TADF material has an extremely short emission lifetime (excitation lifetime) as a TADF material, and can suppress the decrease in efficiency in the high-brightness region of the light-emitting element. Specifically, materials with the molecular structure shown below can be used.

[0252]

[0253] The light-emitting layer 113 can be formed by methods other than the light-emitting mechanism, such as vapor deposition (including vacuum deposition), inkjet printing, coating, and gravure printing. In addition to the materials mentioned above, it may also contain inorganic compounds such as quantum dots or polymer compounds (oligomers, dendrimers, polymers, etc.).

[0254] ≪Hole Injection Layer≫ The hole injection layer (111, 111a, 111b) is a layer that injects holes from the first electrode 101, which is the anode, and the charge generation layer (106, 106a, 106b) into the organic compound layer (103, 103a, 103b), and is a layer that contains an organic acceptor material and a material with high hole injection potential.

[0255] The hole injection layers (111, 111a, 111b) can be compounds having electron-withdrawing groups (halogen groups or cyano groups), such as 7,7,8,8-tetracyano-2,3,5,6-tetrafluoroquinodimethane (abbreviation: F 4Examples include HAT-CN (H6-TCNNQ), chloranil, 2,3,6,7,10,11-hexacyano-1,4,5,8,9,12-hexaazatriphenylene (abbreviated as HAT-CN), 1,3,4,5,7,8-hexafluorotetracyano-naphthoquinodimethane (abbreviated as F6-TCNNQ), and 2-(7-dicyanomethylene-1,3,4,5,6,8,9,10-octafluoro-7H-pyrene-2-ylidene)malononitrile. In particular, compounds in which an electron-withdrawing group is bonded to a condensed aromatic ring having multiple heteroatoms, such as HAT-CN, are thermally stable and therefore preferred. Furthermore, [3]radialene derivatives having electron-withdrawing groups (especially halogen groups such as fluoro groups or cyano groups) are preferred because they have very high electron-accepting properties. Specifically, examples include α,α',α''-1,2,3-cyclopropanetriylidenates (4-cyano-2,3,5,6-tetrafluorobenzeneacetonitrile) (abbreviated as Rad), α,α',α''-1,2,3-cyclopropanetriylidenates [2,6-dichloro-3,5-difluoro-4-(trifluoromethyl)benzeneacetonitrile], and α,α',α''-1,2,3-cyclopropanetriylidenates [2,3,4,5,6-pentafluorobenzeneacetonitrile]. In addition to the organic compounds mentioned above, molybdenum oxide, vanadium oxide, ruthenium oxide, tungsten oxide, manganese oxide, etc. can be used as substances with acceptor properties. Other examples include phthalocyanine (abbreviated as H 2 Hole injection layers (111, 111a, 111b) can also be formed by phthalocyanine compounds such as Pc, phthalocyanine complex compounds such as copper phthalocyanine (CuPc), aromatic amine compounds such as 4,4'-bis[N-(4-diphenylaminophenyl)-N-phenylamino]biphenyl (abbreviated as DPAB), N,N'-bis[4-bis(3-methylphenyl)aminophenyl]-N,N'-diphenyl-4,4'-diaminobiphenyl (abbreviated as DNTPD), or polymers such as poly(3,4-ethylenedioxythiophene) / polystyrene sulfonic acid (abbreviated as PEDOT / PSS). Accepting substances can extract electrons from adjacent hole transport layers (or hole transport materials) by applying an electric field.

[0256] Furthermore, among substances with acceptor properties, organic compounds with acceptor properties are easy to use because they are readily deposited and easy to form films.

[0257] Furthermore, a composite material containing the above-mentioned acceptor substance in a hole-transporting material can also be used as the hole injection layer (111, 111a, 111b). By using a composite material containing the acceptor substance in a hole-transporting material, it is possible to select the material for forming the electrode regardless of the work function. In other words, not only materials with a large work function but also materials with a small work function can be used as the anode (first electrode 101).

[0258] Various organic compounds can be used as hole-transporting materials in composite materials, including aromatic amine compounds, carbazole derivatives, aromatic hydrocarbons, and polymer compounds (oligomers, dendrimers, polymers, etc.). −6 cm 2 It is preferable that the material has a hole mobility of 1 / Vs or higher. Below, we specifically list organic compounds that can be used as hole transporting materials in composite materials.

[0259] Aromatic amine compounds that can be used in composite materials include N,N'-di(p-tolyl)-N,N'-diphenyl-p-phenylenediamine (abbreviated as DTDPPA), 4,4'-bis[N-(4-diphenylaminophenyl)-N-phenylamino]biphenyl (abbreviated as DPAB), N,N'-bis[4-bis(3-methylphenyl)aminophenyl]-N,N'-diphenyl-4,4'-diaminobiphenyl (abbreviated as DNTPD), and 1,3,5-tris[N-(4-diphenylaminophenyl)-N-phenylamino]benzene (abbreviated as DPA3B). Specifically, carbazole derivatives include 3-[N-(9-phenylcarbazole-3-yl)-N-phenylamino]-9-phenylcarbazole (abbreviated as PCzPCA1), 3,6-bis[N-(9-phenylcarbazole-3-yl)-N-phenylamino]-9-phenylcarbazole (abbreviated as PCzPCA2), and 3-[N-(1-naphthyl)-N-(9-phenylcarbazole-3-yl)amino]-9-phenyl Carbazole (abbreviated as PCzPCN1), 4,4'-di(N-carbazolyl)biphenyl (abbreviated as CBP), 1,3,5-tris[4-(N-carbazolyl)phenyl]benzene (abbreviated as TCPB), 9-[4-(10-phenyl-9-antryl)phenyl]-9H-carbazole (abbreviated as CzPA), 1,4-bis[4-(N-carbazolyl)phenyl]-2,3,5,6-tetraphenylbenzene, etc. can be used.Examples of aromatic hydrocarbons include 2-tert-butyl-9,10-di(2-naphthyl)anthracene (abbreviation: t-BuDNA), 2-tert-butyl-9,10-di(1-naphthyl)anthracene, 9,10-bis(3,5-diphenylphenyl)anthracene (abbreviation: DPPA), 2-tert-butyl-9,10-bis(4-phenylphenyl)anthracene (abbreviation: t-BuDBA), 9,10-di(2-naphthyl)anthracene (abbreviation: DNA), 9,10-diphenylanthracene (abbreviation: DPAth), 2-tert-butylanthracene (abbreviation: t-BuAnth), 9,10-bis(4-methyl-1-naphthyl)anthracene (abbreviation: DMNA), 2-tert- Examples include butyl-9,10-bis[2-(1-naphthyl)phenyl]anthracene, 9,10-bis[2-(1-naphthyl)phenyl]anthracene, 2,3,6,7-tetramethyl-9,10-di(1-naphthyl)anthracene, 2,3,6,7-tetramethyl-9,10-di(2-naphthyl)anthracene, 9,9'-biantryl, 10,10'-diphenyl-9,9'-biantryl, 10,10'-bis(2-phenylphenyl)-9,9'-biantryl, 10,10'-bis[(2,3,4,5,6-pentaphenyl)phenyl]-9,9'-biantryl, anthracene, tetracene, rubrene, perylene, and 2,5,8,11-tetra(tert-butyl)perylene. In addition, pentacene, coronene, and the like can also be used. Furthermore, it may have a vinyl skeleton. Examples of aromatic hydrocarbons having a vinyl group include 4,4'-bis(2,2-diphenylvinyl)biphenyl (abbreviated as DPVBi) and 9,10-bis[4-(2,2-diphenylvinyl)phenyl]anthracene (abbreviated as DPVPA). Organic compounds according to one embodiment of the present invention can also be used.

[0260] In addition, polymer compounds such as poly(N-vinylcarbazole) (abbreviated as PVK), poly(4-vinyltriphenylamine) (abbreviated as PVTPA), poly[N-(4-{N'-[4-(4-diphenylamino)phenyl]phenyl-N'-phenylamino}phenyl)methacrylamide] (abbreviated as PTPDMA), and poly[N,N'-bis(4-butylphenyl)-N,N'-bis(phenyl)benzidine] (abbreviated as Poly-TPD) can also be used.

[0261] The hole-transporting material used in the composite material more preferably has at least one of the following skeletons: carbazole, dibenzofuran, dibenzothiophene, and anthracene. In particular, it may be an aromatic amine having substituents including a dibenzofuran ring or a dibenzothiophene ring, an aromatic monoamine having a naphthalene ring, or an aromatic monoamine in which a 9-fluorenyl group is bonded to the nitrogen of the amine via an arylene group. It is preferable that these organic compounds are substances having an N,N-bis(4-biphenyl)amino group, as this allows for the creation of light-emitting devices with a good lifetime. Specifically, the organic compounds described above include N-(4-biphenyl)-6,N-diphenylbenzo[b]naphtho[1,2-d]furan-8-amine (abbreviated as BnfABP), N,N-bis(4-biphenyl)-6-phenylbenzo[b]naphtho[1,2-d]furan-8-amine (abbreviated as BBABnf), and 4,4'-bis(6-phenylbenzo[b]naphtho[1,2-d]furan-8-yl). )-4''-phenyltriphenylamine (abbreviation: BnfBB1BP), N,N-bis(4-biphenyl)benzo[b]naphtho[1,2-d]furan-6-amine (abbreviation: BBABnf(6)), N,N-bis(4-biphenyl)benzo[b]naphtho[1,2-d]furan-8-amine (abbreviation: BBABnf(8)), N,N-bis(4-biphenyl)benzo[b]naphtho[2,3-d]furan -4-amine (abbreviation: BBABnf(II)(4)), N,N-bis[4-(dibenzofuran-4-yl)phenyl]-4-amino-p-terphenyl (abbreviation: DBfBB1TP), N-[4-(dibenzothiophen-4-yl)phenyl]-N-phenyl-4-biphenylamine (abbreviation: ThBA1BP), 4-(2-naphthyl)-4',4''-diphenyltriphenylamine (abbreviation: BB AβNB), 4-[4-(2-naphthyl)phenyl]-4',4''-diphenyltriphenylamine (abbreviation: BBAβNBi), 4,4'-diphenyl-4''-([2,1'-binaphthyl]-6-yl)triphenylamine (abbreviation: BBAαNβNB), 4,4'-diphenyl-4''-([2,1'-binaphthyl]-7-yl)triphenylamine (abbreviation: BBAαNβNB-03), 4,4'-diphenyl-4''-(7-phenyl)naphthyl-2-yltriphenylamine (abbreviation: BBAPβNB-03), 4,4'-diphenyl-4''-([2,2'-binaphthyl]-6-yl)triphenylamine (abbreviation: BBA(βN2)B), 4,4'-diphenyl-4''-([2,2'-binaphthyl]-7-yl)triphenylamine (abbreviation: BBA(βN2)B-03), 4,4'-diphenyl-4''-([1,2'-binaphthyl]-4-yl)triphenylamine (abbreviation: BBAβNαNB), 4,4'-diphenyl-4''-( [1,2'-binaphthyl]-5-yl)triphenylamine (abbreviation: BBAβNαNB-02), 4-(4-biphenylyl)-4'-(2-naphthyl)-4''-phenyltriphenylamine (abbreviation: TPBiAβNB), 4-(3-biphenylyl)-4'-[4-(2-naphthyl)phenyl]-4''-phenyltriphenylamine (abbreviation: mTPBiAβNBi), 4-(4-biphenylyl)-4'-[4-(2-naphthyl)phenyl]-4''-phenyltriphenylamine (abbreviation: TPBiAβNBi), 4-phenyl-4'-(1-naphthyl Triphenylamine (abbreviation: αNBA1BP), 4,4'-bis(1-naphthyl)triphenylamine (abbreviation: αNBB1BP), 4,4'-diphenyl-4''-[4'-(carbazole-9-yl)biphenyl-4-yl]triphenylamine (abbreviation: YGTBi1BP), 4'-[4-(3-phenyl-9H-carbazole-9-yl)phenyl]tris(biphenyl-4-yl)amine (abbreviation: YGTBi1BP-02), 4-[4'-(carbazole-9-yl)biphenyl-4-yl]-4'-(2-naphthyl)-4''-phenyl Triphenylamine (abbreviation: YGTBiβNB), N-[4-(9-phenyl-9H-carbazole-3-yl)phenyl]-N-[4-(1-naphthyl)phenyl]-9,9'-spirobio[9H-fluorene]-2-amine (abbreviation: PCBNBSF), N,N-bis(biphenyl-4-yl)-9,9'-spirobio[9H-fluorene]-2-amine (abbreviation: BBASF), N,N-bis(biphenyl-4-yl)-9,9'-spirobio[9H-fluorene]-4-amine (abbreviation: BBASF(4)), N-(biphenyl-2-yl)-N-(9,9-dimethyl-9H-fluoren-2-yl)-9,9'-spirobi[9H-fluoren]-4-amine (abbreviation: oFBiSF), N-(biphenyl-4-yl)-N-(9,9-dimethyl-9H-fluoren-2-yl)dibenzofuran-4-amine (abbreviation: FrBiF), N-[4-(1-naphthyl)phenyl]-N-[3-(6-phenyldibenzofuran-4-yl)phenyl]-1-naphthylamine (abbreviation: mPDBfBNBN), 4-phenyl-4'-(9-phenylfluoren-9-yl)triphenylamine (abbreviation: BPAFLP), 4-phenyl-3'-(9-phenylfluoren-9-yl)triphenylamine (abbreviation: mBPAFLP), 4-phenyl-4'-[4-(9-phenylfluoren-9-yl)phenyl]triphenylamine (abbreviation: BPAFLBi), 4-phenyl-4'-(9-phenyl-9H-carbazole-3-yl)triphenylamine (abbreviation: PCBA1BP), 4,4'-diphenyl-4''-(9-phenyl-9H-carbazole-3-yl)triphenylamine (abbreviation: PCBi1BP), 4-(1-naphthyl)-4'-(9-phenyl-9 H-carbazole-3-yl)triphenylamine (abbreviation: PCBANB), 4,4'-di(1-naphthyl)-4''-(9-phenyl-9H-carbazole-3-yl)triphenylamine (abbreviation: PCBNBB), N-phenyl-N-[4-(9-phenyl-9H-carbazole-3-yl)phenyl]-9,9'-spirobi[9H-fluorene]-2-amine (abbreviation: PCBASF), N-(biphenyl-4-yl)-N-[4-(9-phenyl-9H-carbazole-3-yl)phenyl]-9,9-dimethyl-9H-fluorene-2-amine Examples include PCBiF (abbreviation: PCBiF), N,N-bis(9,9-dimethyl-9H-fluoren-2-yl)-9,9'-spirobio-9H-fluoren-4-amine, N,N-bis(9,9-dimethyl-9H-fluoren-2-yl)-9,9'-spirobio-9H-fluoren-3-amine, N,N-bis(9,9-dimethyl-9H-fluoren-2-yl)-9,9'-spirobio-9H-fluoren-2-amine, and N,N-bis(9,9-dimethyl-9H-fluoren-2-yl)-9,9'-spirobio-9H-fluoren-1-amine.

[0262] Furthermore, it is even more preferable that the hole-transporting material used in the composite material has a relatively low HOMO level between -5.7 eV and -5.4 eV. Having a relatively low HOMO level in the hole-transporting material used in the composite material facilitates the injection of holes into the hole transport layer 112 and makes it easier to obtain a light-emitting device with a good lifetime. In addition, having a relatively low HOMO level in the hole-transporting material used in the composite material moderately suppresses hole induction, resulting in a light-emitting device with an even better lifetime.

[0263] Furthermore, by mixing alkali metal or alkaline earth metal fluoride into the above composite material (preferably with an atomic ratio of fluorine atoms of 20% or more in the layer), the refractive index of the layer can be reduced. This also makes it possible to form a layer with a low refractive index inside the EL layer 103, thereby improving the external quantum efficiency of the light-emitting device.

[0264] By forming hole injection layers (111, 111a, 111b), hole injection performance is improved, and a light-emitting device with a low driving voltage can be obtained.

[0265] ≪Hole Transport Layer≫ The hole transport layer (112, 112a, 112b) is a layer containing a hole transport material, and the hole transport material exemplified as the material for the hole injection layer (111, 111a, 111b) can be used. Since the hole transport layer (112, 112a, 112b) has the function of transporting holes injected into the hole injection layer (111, 111a, 111b) to the light-emitting layer (113, 113a, 113b), it is preferable that it has the same or close HOMO level as the HOMO level of the hole injection layer (111, 111a, 111b).

[0266] Also, 1 x 10 −6 cm 2 It is preferable that the material has a hole mobility of 1 / Vs or higher. However, other materials may be used as long as they have higher hole transport capabilities than electron transport capabilities. The layer containing the material with high hole transport capabilities may be a single layer, or two or more layers made of the above material may be stacked.

[0267] Materials that can be used for the hole transport layers (112, 112a, 112b) include 4,4'-bis[N-(1-naphthyl)-N-phenylamino]biphenyl (abbreviated as NPB), N,N'-diphenyl-N,N'-bis(3-methylphenyl)-4,4'-diaminobiphenyl (abbreviated as TPD), N,N'-bis(9,9'-spirobi[9H-fluoren]-2-yl)-N,N'-diphenyl-4,4'-diaminobiphenyl (abbreviated as BSPB), and 4-phenyl-4'-(9-phenylfluoren-9-yl)triphenylamine (abbreviated as BPA). FLP), 4-phenyl-3'-(9-phenylfluoren-9-yl)triphenylamine (abbreviation: mBPAFLP), 4-phenyl-4'-(9-phenyl-9H-carbazole-3-yl)triphenylamine (abbreviation: PCBA1BP), 4,4'-diphenyl-4''-(9-phenyl-9H-carbazole-3-yl)triphenylamine (abbreviation: PCBi1BP), 4-(1-naphthyl)-4'-(9-phenyl-9H-carbazole-3-yl)triphenylamine (abbreviation: PCBANB), 4,4'-di(1-naphthyl)-4'' Compounds having an aromatic amine skeleton such as -(9-phenyl-9H-carbazole-3-yl)triphenylamine (abbreviation: PCBNBB), 9,9-dimethyl-N-phenyl-N-[4-(9-phenyl-9H-carbazole-3-yl)phenyl]fluoren-2-amine (abbreviation: PCBAF), N-phenyl-N-[4-(9-phenyl-9H-carbazole-3-yl)phenyl]-9,9'-spirobi[9H-fluoren]-2-amine (abbreviation: PCBASF), 1,3-bis(N-carbazolyl)benzene (abbreviation: mCP), 4,4'-di (N-carbazolyl)biphenyl (abbreviation: CBP), 3,6-bis(3,5-diphenylphenyl)-9-phenylcarbazole (abbreviation: CzTP), 9,9'-diphenyl-9H,9'H-3,3'-bicarbazole (abbreviation: PCCP), 9,9'-bis(biphenyl-4-yl)-3,3'-bi-9H-carbazole (abbreviation: BisBPCz), 9,9'-bis(biphenyl-3-yl)-3,3'-bi-9H-carbazole (abbreviation: BismBPCz), 9-(biphenyl-3-yl)-9'-(biphenyl-4-yl)-9H,9'H-3,Compounds having a carbazole skeleton such as 3'-bicarbazole (abbreviation: mBPCCP), 4,4',4''-(benzene-1,3,5-triyl)tri(dibenzothiophene) (abbreviation: DBT3P-II), 2,8-diphenyl-4-[4-(9-phenyl-9H-fluoren-9-yl)phenyl]dibenzothiophene (abbreviation: DBTFLP-III), 4-[4-(9-phenyl-9H-fluoren-9-yl) Examples include compounds having a thiophene skeleton such as phenyl]-6-phenyldibenzothiophene (abbreviated as DBTFLP-IV), and compounds having a furan skeleton such as 4,4',4''-(benzene-1,3,5-triyl)tri(dibenzofuran) (abbreviated as DBF3P-II) and 4-{3-[3-(9-phenyl-9H-fluoren-9-yl)phenyl]phenyl}dibenzofuran (abbreviated as mmDBFFLBi-II). Among the above, compounds having an aromatic amine skeleton or a carbazole skeleton are preferred because they have good reliability, high hole transportability, and contribute to reducing the driving voltage. Furthermore, the materials listed as having hole transportability used in the composite material of the hole injection layer 111 can also be suitably used as materials constituting the hole transport layer 112.

[0268] ≪Electron Transport Layer≫ The electron transport layers (114, 114a, 114b) have the function of transporting electrons injected from the other electrode of the pair (first electrode 101 or second electrode 102) to the light-emitting layer 113 via the electron injection layers (115, 115a, 115b).

[0269] Furthermore, as an electron-transporting material, it is an organic compound having electron-transporting properties, and the electron mobility at which the square root of the electric field strength [V / cm] is 600 is 1 × 10⁻⁶. −6 cm 2 A substance having an electron mobility of 1 / Vs or higher is preferred. The electron mobility can be measured in the same manner as described in Japanese Patent Application Publication No. 2020-096171 (Patent Document 3). Furthermore, the configuration of the electron-only element used for measurement can be appropriately selected to facilitate electron injection into the compound whose electron mobility is to be measured.

[0270] In addition, any other material that has higher electron transport capabilities than holes can be used. The organic compound described above is preferably an organic compound having a π-electron-deficient heteroaromatic ring. The organic compound having a π-electron-deficient heteroaromatic ring is preferably one or more of the following: an organic compound containing a heteroaromatic ring having an azole skeleton, an organic compound containing a heteroaromatic ring having a pyridine skeleton, an organic compound containing a heteroaromatic ring having a diazine skeleton, and an organic compound containing a heteroaromatic ring having a triazine skeleton.

[0271] Organic compounds having a π-electron-deficient heteroaromatic ring that can be used in the above electron transport layer include, specifically, 2-(4-biphenyl)-5-(4-tert-butylphenyl)-1,3,4-oxadiazole (abbreviated as PBD), 3-(4-biphenylyl)-4-phenyl-5-(4-tert-butylphenyl)-1,2,4-triazole (abbreviated as TAZ), 1,3-bis[5-(4-tert-butylphenyl)-1,3,4-oxadiazole-2-yl]benzene (abbreviated as OXD-7), and 9-[4-(5-phenyl-1,3,4-oxadiazole-2-yl]benzene. Organic compounds having an azole skeleton, such as sadiazole-2-yl)phenyl]-9H-carbazole (abbreviation: CO11), 2,2',2''-(1,3,5-benzenetriyl)tris(1-phenyl-1H-benzimidazole) (abbreviation: TPBI), 2-[3-(dibenzothiophen-4-yl)phenyl]-1-phenyl-1H-benzimidazole (abbreviation: mDBTBIm-II), 4,4'-bis(5-methylbenzoxazole-2-yl)stilbene (abbreviation: BzOs), and 3,5-bis[3-(9H-carbazole-9-yl)phenyl Organic compounds containing heteroaromatic rings with a pyridine skeleton, such as [nyl]pyridine (abbreviation: 35DCzPPy), 1,3,5-tri[(3-pyridyl)phenyl-3-yl]benzene (abbreviation: TmPyPB), vasophenanthroline (abbreviation: Bphen), vasocuproin (abbreviation: BCP), 2,9-di(naphthalene-2-yl)-4,7-diphenyl-1,10-phenanthroline (abbreviation: NBphen), 2-[3-(dibenzothiophen-4-yl)phenyl]dibenzo[f,h]quinoxaline (abbreviation: 2mDBTPDBq-II), 2-[3 '-(dibenzothiophen-4-yl)biphenyl-3-yl]dibenzo[f,h]quinoxaline (abbreviation: 2mDBTBPDBq-II), 2-[3'-(9H-carbazole-9-yl)biphenyl-3-yl]dibenzo[f,h]quinoxaline (abbreviation: 2mCzBPDBq), 2-[4'-(9-phenyl-9H-carbazole-3-yl)-3,1'-biphenyl-1-yl]dibenzo[f,h]quinoxaline (abbreviation: 2mpPCBPDBq), 2-[4-(3,6-diphenyl-9H-carbazole-9-yl)phenyl]dibenzo[f,[h]Quinoxaline (abbreviation: 2CzPDBq-III), 7-[3-(dibenzothiophen-4-yl)phenyl]dibenzo[f,h]Quinoxaline (abbreviation: 7mDBTPDBq-II), 6-[3-(dibenzothiophen-4-yl)phenyl]dibenzo[f,h]Quinoxaline (abbreviation: 6mDBTPDBq-II), 9-[3'-(dibenzothiophen-4-yl)biphenyl-3-yl]naphtho[1',2':4,5]flo[2,3-b]pyrazine (abbreviation: 9mDBtBPNfpr), 9-[3'-(dibenzothiophen-4-yl)biphenyl -4-yl]naphtho[1',2':4,5]flo[2,3-b]pyrazine (abbreviation: 9pmDBtBPNfpr), 4,6-bis[3-(phenanthren-9-yl)phenyl]pyrimidine (abbreviation: 4,6mPnP2Pm), 4,6-bis[3-(dibenzothiophen-4-yl)phenyl]pyrimidine (abbreviation: 4,6mDBTP2Pm-II), 4,6-bis[3-(9H-carbazole-9-yl)phenyl]pyrimidine (abbreviation: 4,6mCzP2Pm), 9,9'-[pyrimidine-4,6-diylbis(biphenyl-3,3'-diyl)]bis(9 H-carbazole) (abbreviation: 4,6mCzBP2Pm), 8-(biphenyl-4-yl)-4-[3-(dibenzothiophen-4-yl)phenyl]-[1]benzoflo[3,2-d]pyrimidine (abbreviation: 8BP-4mDBtPBfpm), 3,8-bis[3-(dibenzothiophen-4-yl)phenyl]benzoflo[2,3-b]pyrazine (abbreviation: 3,8mDBtP2Bfpr), 8-[3'-(dibenzothiophen-4-yl)biphenyl-3-yl]naphtho[1',2':4,5]flo[3,2-d]pyrimidine (abbreviation: 8mDBtBPNfp m), 8-[(2,2'-binaphthalene)-6-yl]-4-[3-(dibenzothiophen-4-yl)phenyl]-[1]benzoflozyrimidine[3,2-d]pyrimidine (abbreviation: 8(βN2)-4mDBtPBfpm), 2,2'-(pyridine-2,6-diyl)bis(4-phenylbenzo[h]quinazoline) (abbreviation: 2,6(P-Bqn)2Py), 2,2'-(pyridine-2,6-diyl)bis{4-[4-(2-naphthyl)phenyl]-6-phenylpyrimidine} (abbreviation: 2,6(NP-PPm)2Py), 6-(biphenyl-3-yl)-4-[3,5-Bis(9H-carbazole-9-yl)phenyl]-2-phenylpyrimidine (abbreviation: 6mBP-4Cz2PPm), 2,4-Bis[4-(1-naphthyl)phenyl]-6-[4-(3-pyridyl)phenyl]pyrimidine (abbreviation: 2,4NP-6PyPPm), 4-[3,5-bis(9H-carbazole-9-yl)phenyl]-2-phenyl-6-(biphenyl-4-yl)pyrimidine (abbreviation: 6BP-4Cz2PPm), 7-[4-(9-phenyl-9H-carbazole-2-yl)quinazoline-2-yl]-7H-dibenzo[c,g]cal Organic compounds having a diazine skeleton, such as Bazole (abbreviation: PC-cgDBCzQz), 2-[3'-(9,9-dimethyl-9H-fluoren-2-yl)biphenyl-3-yl]-4,6-diphenyl-1,3,5-triazine (abbreviation: mFBPTZn), 2-(biphenyl-4-yl)-4-phenyl-6-(9,9'-spirobio[9H-fluoren]-2-yl)-1,3,5-triazine (abbreviation: BP-SFTZn), 2-{3-[3-(benzo[b]naphtho[1,2-d]furan-8-yl)phenyl]phenyl}-4,6-diphenyl-1 ,3,5-triazine (abbreviation: mBnfBPTZn), 2-{3-[3-(benzo[b]naphtho[1,2-d]furan-6-yl)phenyl]phenyl}-4,6-diphenyl-1,3,5-triazine (abbreviation: mBnfBPTZn-02), 9-[4-(4,6-diphenyl-1,3,5-triazine-2-yl)phenyl]-9'-phenyl-3,3'-bi-9H-carbazole (abbreviation: PCCzPTZn), 9-[3-(4,6-diphenyl-1,3,5-triazine-2-yl)phenyl]-9'-phenyl-2,3'-bi-9H-carbazole (abbreviation: mPCCzPTZn-02), 5-[3-(4,6-diphenyl-1,3,5-triazine-2-yl)phenyl]-7,7-dimethyl-5H,7H-indeno[2,1-b]carbazole (abbreviation: mINc(II)PTZn), 2-{3-[3-(dibenzothiophen-4-yl)phenyl]phenyl}-4,6-diphenyl-1,3,5-triazine (abbreviation: mDBtBPTZn), 2,4,6-tris[3'-(pyridine-3-yl)biphenyl-3-yl]-1,3,5-triazine (abbreviation: TmPPPyTz), 2-[3-(2,6-dimethyl-3-pyridinyl)-5-(9-phenanthryl)phenyl]-4,6-diphenyl-1,3,5-triazine (abbreviation: mPn-mDMePyPTZn), 11-[4-(biphenyl-4-yl)-6-phenyl-1,3,5-triazine-2-yl]-11,12-dihydro-12-phenylindoro[2,3-a]carbazole (abbreviation: BP-Icz(II)TZn), 2-[3'-(triphenylene-2-yl)biphenyl-3-yl]-4,6-diphenyl-1,3 Examples of organic compounds having a triazine skeleton include 5-triazine (abbreviated as mTpBPTZn), 3-[9-(4,6-diphenyl-1,3,5-triazine-2-yl)-2-dibenzofuranyl]-9-phenyl-9H-carbazole (abbreviated as PCDBfTZn), and 2-(biphenyl-3-yl)-4-phenyl-6-{8-[(1,1':4',1''-terphenyl)-4-yl]-1-dibenzofuranyl}-1,3,5-triazine (abbreviated as mBP-TPDBfTZn). Among the above, organic compounds containing a heteroaromatic ring having a diazine skeleton, organic compounds containing a heteroaromatic ring having a pyridine skeleton, and organic compounds containing a heteroaromatic ring having a triazine skeleton are preferred due to their good reliability. In particular, organic compounds containing heteroaromatic rings with a diazine (pyrimidine and pyrazine) skeleton, and organic compounds containing heteroaromatic rings with a triazine skeleton, exhibit high electron transport properties and contribute to reducing the driving voltage.

[0272] Furthermore, the electron transport layers (114, 114a, 114b) may be not only a single layer, but also two or more layers made of the above material stacked together.

[0273] Furthermore, a layer for controlling the movement of electron carriers may be provided between the electron transport layers (114, 114a, 114b) and the light-emitting layers (113, 113a, 113b). This layer is made by adding a small amount of a substance with high electron-trapping properties to the electron-transporting material described above, and it is possible to adjust the carrier balance by suppressing the movement of electron carriers. Such a configuration is highly effective in suppressing problems that occur when electrons penetrate the light-emitting layer (for example, a decrease in device lifespan).

[0274] ≪Electron injection layer≫ The electron injection layer (115, 115a, 115b) has the function of promoting electron injection by reducing the electron injection barrier from the second electrode 102.

[0275] Furthermore, for example, Group 1 metals, Group 2 metals, or their oxides, halides, carbonates, etc., can be used. Also, composite materials of the electron-transporting material and an electron-donating material can be used. Examples of electron-donating materials include Group 1 metals, Group 2 metals, or their oxides. Specifically, lithium fluoride (LiF), sodium fluoride (NaF), cesium fluoride (CsF), calcium fluoride (CaF) 2 ), lithium oxide (LiO x Alkali metals, alkaline earth metals, or compounds thereof, such as ) can be used. Also, erbium fluoride (ErF) can be used. 3 Rare earth metal compounds such as ) can be used. Alternatively, an electride may be used in the electron injection layer 115. Examples of such electrides include a substance obtained by adding electrons to a mixed oxide of calcium and aluminum at a high concentration. Furthermore, the electron injection layers (115, 115a, 115b) may be made of a substance that can be used in the electron transport layers (114, 114a, 114b).

[0276] Furthermore, a composite material obtained by mixing an organic compound and an electron donor may be used in the electron injection layers (115, 115a, 115b). Such a composite material has excellent electron injection and electron transport properties because electrons are generated in the organic compound by the electron donor. In this case, the organic compound is preferably a material that is excellent in transporting the generated electrons, and specifically, for example, the substance that constitutes the electron transport layer 114 described above (metal complex, or heteroaromatic compound, etc.) can be used. As the electron donor, any substance that exhibits electron-donating properties to the organic compound is acceptable. Specifically, alkali metals, alkaline earth metals, or rare earth metals are preferred, such as lithium, sodium, cesium, magnesium, calcium, erbium, and ytterbium. Alkali metal oxides or alkaline earth metal oxides are also preferred, such as lithium oxide, calcium oxide, and barium oxide. Lewis bases such as magnesium oxide can also be used. Furthermore, organic compounds such as tetrathiafulvalene (abbreviated as TTF) can also be used.

[0277] Furthermore, organic compounds that can be used in the electron injection layer include 4,7-di-1-pyrrolidinyl-1,10-phenanthroline (abbreviation: Pyrrd-Phen), 1,1'-pyridine-2,6-diyl-bis(1,3,4,6,7,8-hexahydro-2H-pyrimido[1,2-a]pyrimidine) (hpp2Py), and 1,1'-(9,9'-spirobi[9H-fluorene]-2 Organic compounds such as ,7-diyl)bis(1,3,4,6,7,8-hexahydro-2H-pyrimido[1,2-a]pyrimidine) (abbreviated as 2,7hpp2SF) and 1-(9,9'-spirobi[9H-fluoren]-2-yl)-1,3,4,6,7,8-hexahydro-2H-pyrimido[1,2-a]pyrimidine (abbreviated as 2hppSF) can be used.

[0278] The light-emitting layer, hole injection layer, hole transport layer, electron transport layer, and electron injection layer described above can be formed by methods such as vapor deposition (including vacuum deposition), inkjet printing, coating, and gravure printing, respectively. In addition to the materials described above, inorganic compounds such as quantum dots or polymer compounds (oligomers, dendrimers, polymers, etc.) may also be used for the light-emitting layer, hole injection layer, hole transport layer, electron transport layer, and electron injection layer.

[0279] Furthermore, the quantum dots may include colloidal quantum dots, alloy quantum dots, core-shell quantum dots, core quantum dots, etc. Quantum dots containing elemental groups from groups 2 and 16, 13 and 15, 13 and 17, 11 and 17, or 14 and 15 may also be used. Alternatively, quantum dots containing elements such as cadmium (Cd), selenium (Se), zinc (Zn), sulfur (S), phosphorus (P), indium (In), tellurium (Te), lead (Pb), gallium (Ga), arsenic (As), and aluminum (Al) may be used.

[0280] <Pair of electrodes> The first electrode 101 and the second electrode 102 function as the anode or cathode of the light-emitting device. The first electrode 101 and the second electrode 102 can be formed using metals, alloys, conductive compounds, mixtures thereof, or laminates.

[0281] Preferably, one of the first electrode 101 or the second electrode 102 is formed of a conductive material having the function of reflecting light. Examples of such conductive materials include aluminum (Al) or alloys containing Al. Examples of alloys containing Al include alloys containing Al and L (where L represents one or more of titanium (Ti), neodymium (Nd), nickel (Ni), and lanthanum (La)), such as alloys containing Al and Ti, or Al, Ni, and La. Aluminum has low resistance and high light reflectivity. In addition, since aluminum is abundant in the Earth's crust and inexpensive, using aluminum can reduce the manufacturing cost of light-emitting devices. In addition, alloys containing silver (Ag), or Ag and N (where N represents one or more of yttrium (Y), Nd, magnesium (Mg), ytterbium (Yb), Al, Ti, gallium (Ga), zinc (Zn), indium (In), tungsten (W), manganese (Mn), tin (Sn), iron (Fe), Ni, copper (Cu), palladium (Pd), iridium (Ir), or gold (Au) may be used. Examples of silver-containing alloys include alloys containing silver, palladium, and copper; alloys containing silver and copper; alloys containing silver and magnesium; alloys containing silver and nickel; alloys containing silver and gold; and alloys containing silver and ytterbium. Other transition metals such as tungsten, chromium (Cr), molybdenum (Mo), copper, and titanium can also be used.

[0282] Furthermore, the light emitted from the light-emitting layer is extracted through one or both of the first electrode 101 and the second electrode 102. Therefore, it is preferable that at least one of the first electrode 101 and the second electrode 102 be made of a conductive material that has the function of transmitting light. The conductive material has a visible light transmittance of 40% to 100%, preferably 60% to 100%, and a resistivity of 1 × 10⁻¹⁶. −2 Examples include conductive materials with a conductivity of Ω·cm or less.

[0283] Furthermore, the first electrode 101 and the second electrode 102 may be formed from a conductive material having the function of transmitting light and the function of reflecting light. The conductive material has a visible light reflectance of 20% to 80%, preferably 40% to 70%, and a resistivity of 1 × 10⁻⁶. −2 Examples of conductive materials include those with a conductivity of Ω·cm or less. For example, they can be formed using one or more types of conductive metals, alloys, or conductive compounds. Specifically, metal oxides such as indium tin oxide (ITO), indium tin oxide containing silicon or silicon oxide (ITSO), indium zinc oxide, indium tin oxide containing titanium, indium titanium oxide, and indium oxide containing tungsten and zinc oxide can be used. In addition, a thin metal film that transmits light (preferably with a thickness of 1 nm to 30 nm) can be used. As a metal, for example, Ag can be used. As an alloy, alloys such as Ag and Al, Ag and Mg, Ag and Au, Ag and Yb can be used.

[0284] In this specification, a material having the function of transmitting light is any material that has the function of transmitting visible light and is conductive, and may include, for example, oxide conductors represented by ITO as described above, oxide semiconductors, or organic conductors containing organic matter. Examples of organic conductors containing organic matter include composite materials obtained by mixing an organic compound with an electron donor, and composite materials obtained by mixing an organic compound with an electron acceptor. Inorganic carbon-based materials such as graphene may also be used. The resistivity of the material is preferably 1 × 10⁻⁶. 5 Ω·cm or less, more preferably 1 × 10⁻⁶ 4 It is less than or equal to Ω·cm.

[0285] Alternatively, one or both of the first electrode 101 and the second electrode 102 may be formed by stacking multiple of the above materials.

[0286] Furthermore, to improve light extraction efficiency, a material with a refractive index higher than that of the electrode may be formed in contact with an electrode that has the function of transmitting light. Such a material can be any material that has the function of transmitting visible light, and may or may not be conductive. For example, in addition to the oxide conductors mentioned above, oxide semiconductors and organic materials can be used. Examples of organic materials include the materials exemplified in the light-emitting layer, hole injection layer, hole transport layer, electron transport layer, or electron injection layer. Inorganic carbon-based materials or thin metal films that transmit light to a certain extent can also be used, and multiple layers of several nanometers to tens of nanometers may be stacked.

[0287] When the first electrode 101 or the second electrode 102 functions as a cathode, it is preferable to use a material with a small work function (3.8 eV or less). For example, elements belonging to Group 1 or Group 2 of the periodic table (alkali metals such as lithium, sodium, and cesium; alkaline earth metals such as calcium and strontium; magnesium, etc.), alloys containing these elements (e.g., Ag and Mg, Al and Li), rare earth metals such as europium (Eu) and Yb, alloys containing these rare earth metals, alloys containing aluminum and silver, etc. can be used.

[0288] Furthermore, when using the first electrode 101 or the second electrode 102 as an anode, it is preferable to use a material with a large work function (4.0 eV or more).

[0289] Furthermore, the first electrode 101 and the second electrode 102 may be laminates of a conductive material having the function of reflecting light and a conductive material having the function of transmitting light. In that case, the first electrode 101 and the second electrode 102 are preferable because they can have a function to adjust the optical distance so that the light from each light-emitting layer can resonate at a desired wavelength and intensify the light of that wavelength.

[0290] The first electrode 101 and the second electrode 102 can be formed using methods such as sputtering, vapor deposition, printing, coating, MBE (Molecular Beam Epitaxy), CVD, pulsed laser deposition, ALD (Atomic Layer Deposition), etc., as appropriate.

[0291] ≪Charge Generation Layer (Intermediate Layer)≫ The charge generation layer 106 has the function of injecting electrons into the organic compound layer 103a and holes into the organic compound layer 103b when a voltage is applied between the first electrode (anode) 101 and the second electrode (cathode) 102. The charge generation layer 106 may be a configuration in which an electron acceptor is added to a hole transport material (also called a P-type layer), or a configuration in which an electron donor is added to an electron transport material (also called an electron injection buffer layer). Furthermore, both of these configurations may be laminated. In addition, an electron relay layer may be provided between the P-type layer and the electron injection buffer layer. By forming the charge generation layer 106 using the materials described above, it is possible to suppress the increase in driving voltage when an organic compound layer including an emissive layer is laminated.

[0292] In the charge generation layer 106, when an electron acceptor is added to a hole-transporting material which is an organic compound (P-type layer), the hole-transporting material shown in this embodiment can be used. Furthermore, as the electron acceptor, 7,7,8,8-tetracyano-2,3,5,6-tetrafluoroquinodimethane (abbreviated as F) can be used. 4 Examples include -TCNQ), chloranil, etc. Also, oxides of metals belonging to groups 4 through 8 of the periodic table can be used. Specifically, examples include vanadium oxide, niobium oxide, tantalum oxide, chromium oxide, molybdenum oxide, tungsten oxide, manganese oxide, and rhenium oxide. The above-mentioned acceptor materials may also be used. Furthermore, the materials constituting the P-type layer may be used as a mixed film, or single films containing each material may be laminated.

[0293] Furthermore, in the charge generation layer 106, if an electron donor is added to the electron transport material (electron injection buffer layer), the electron transport material may be the electron transport material shown in this embodiment.

[0294] Furthermore, alkali metals, alkaline earth metals, rare earth metals, or metals belonging to groups 2 and 13 of the periodic table, as well as their oxides and carbonates, can be used as electron donors. Specifically, lithium (Li), cesium (Cs), magnesium (Mg), calcium (Ca), ytterbium (Yb), indium (In), lithium oxide (Li) 2 It is preferable to use o), cesium carbonate, etc. Alternatively, an organic compound such as tetrathianaphthalene may be used as an electron donor.

[0295] In the charge generation layer 106, when an electron relay layer is provided between the P-type layer and the electron injection buffer layer, the electron relay layer contains at least an electron-transporting material and has the function of preventing interaction between the electron injection buffer layer and the P-type layer and smoothly transferring electrons. Preferably, the LUMO level of the electron-transporting material included in the electron relay layer is between the LUMO level of the acceptor material in the P-type layer and the LUMO level of the electron-transporting material included in the electron transport layer in contact with the charge generation layer 106. The specific energy level of the LUMO level of the electron-transporting material used in the electron relay layer is preferably -5.0 eV or higher, more preferably -5.0 eV or higher and -3.0 eV or lower. Preferably, as the electron-transporting material used in the electron relay layer, a phthalocyanine-based material or a metal complex having a metal-oxygen bond and an aromatic ligand is used.

[0296] Although Figure 5D shows a configuration in which two organic compound layers 103 are stacked, a stacked structure including three or more light-emitting layers may be used by providing a charge generation layer between different light-emitting layers.

[0297] <<Capping Layer>> Although not shown in Figures 5A to 5E, a capping layer may be provided on the second electrode 102 of the light-emitting device. For example, a material with a high refractive index can be used for the capping layer. By providing a capping layer on the second electrode 102, the extraction efficiency of light emitted from the second electrode 102 can be improved.

[0298] Specific examples of materials that can be used in the cap layer include 5,5'-diphenyl-2,2'-di-5H-[1]benzothieno[3,2-c]carbazole (abbreviated as BisBTc) and 4,4',4''-(benzene-1,3,5-triyl)tri(dibenzothiophene) (abbreviated as DBT3P-II).

[0299] <Substrate> Furthermore, a light-emitting device according to one aspect of the present invention may be manufactured on a substrate made of glass, plastic, or the like. The order in which the components are manufactured on the substrate may be either by stacking them sequentially from the first electrode 101 side, or by stacking them sequentially from the second electrode 102 side.

[0300] In addition, as a substrate on which a light-emitting device according to one aspect of the present invention can be formed, for example, glass, quartz, or plastic can be used. A flexible substrate may also be used. A flexible substrate is a substrate that can be bent (flexible), and examples include plastic substrates made of polycarbonate or polyarylate. Films, inorganic vapor-deposited films, etc., can also be used. In addition, other materials are acceptable as long as they function as a support in the manufacturing process of the light-emitting device and optical element. Alternatively, any material that has the function of protecting the light-emitting device and optical element is acceptable.

[0301] For example, in this specification and the like, light-emitting devices can be formed using various substrates. The type of the substrate is not particularly limited. Examples of the substrate include a semiconductor substrate (e.g., a single crystal substrate such as a silicon substrate), an SOI substrate, a glass substrate, a quartz substrate, a plastic substrate, a metal substrate, a stainless steel substrate, a substrate including stainless steel foil, a tungsten substrate, a substrate including tungsten foil, a flexible substrate, a laminated film, cellulose nanofiber (CNF) containing a fibrous material, paper, or a base material film, and the like. Examples of the glass substrate include barium borosilicate glass, aluminoborosilicate glass, soda lime glass, and the like. Examples of the flexible substrate, the laminated film, the base material film and the like include the following. For example, plastics typified by polyethylene terephthalate (PET), polyethylene naphthalate (PEN), polyethersulfone (PES), and polytetrafluoroethylene (PTFE) can be given. Alternatively, an example thereof includes an acrylic resin or the like. Alternatively, examples thereof include polypropylene, polyester, polyvinyl fluoride, polyvinyl chloride, and the like. Alternatively, examples thereof include resins such as polyamide, polyimide, aramid, or epoxy, an inorganic deposited film, papers, and the like.

[0302] Alternatively, a flexible substrate may be used as the substrate, and the light-emitting device may be formed directly over the flexible substrate. Alternatively, a separation layer may be provided between the substrate and the light-emitting device. The separation layer can be used to separate the light-emitting device from the substrate after part or the whole of the light-emitting device is completed thereover, and transfer the light-emitting device to another substrate. At that time, the light-emitting device can be transferred to a substrate having poor heat resistance or a flexible substrate. Note that for the above-described separation layer, for example, a stacked structure of an inorganic film of a tungsten film and a silicon oxide film, a structure in which a resin film such as polyimide is formed over a substrate, or the like can be used.

[0303] That is, a light-emitting device may be formed using a certain substrate, and then the light-emitting device may be transferred to another substrate, so that the light-emitting device is arranged over the another substrate. Examples of the substrate to which the light-emitting device is transferred include, in addition to the above-described substrate, a cellophane substrate, a stone substrate, a wood substrate, a cloth substrate (including natural fibers (silk, cotton, hemp), synthetic fibers (nylon, polyurethane, polyester), or recycled fibers (acetate, cupro, rayon, recycled polyester), and the like), a leather substrate, a rubber substrate, and the like. By using these substrates, a light-emitting device that is not easily broken, a light-emitting device with high heat resistance, a lightweight light-emitting device, or a thin light-emitting device can be obtained.

[0304] Alternatively, for example, a field-effect transistor (FET) may be formed over the above-described substrate, and the light-emitting device may be fabricated over an electrode electrically connected to the FET. Accordingly, an active matrix display device in which driving of the light-emitting device is controlled by the FET can be fabricated.

[0305] Note that one embodiment of the present invention was described in this embodiment. Alternatively, one embodiment of the present invention will be described in another embodiment. Note that one embodiment of the present invention is not limited thereto. That is, since various aspects of the invention are described in this embodiment and other embodiments, one embodiment of the present invention is not limited to a specific aspect. For example, although the example where one embodiment of the present invention is applied to a light-emitting device is described, one embodiment of the present invention is not limited thereto. For example, depending on cases or circumstances, one embodiment of the present invention does not necessarily need to be applied to a light-emitting device.

[0306] The structure described in this embodiment can be combined as appropriate with any of the structures described in the other embodiments.

[0307] (Embodiment 2) In this embodiment, modified examples of the cross-sectional view of the unit 30 illustrated in FIG. 1B in Embodiment 1 will be described with reference to FIGS. 6A to 6D. A method for manufacturing the unit 30 will also be described.

[0308] In the cross-sectional view shown in Figure 6A, in addition to the configuration shown in Figure 1B, an inorganic film 21 is included. The inorganic film 21 has a portion located within the opening of the partition wall 20, between the side surface of the partition wall 20 and the side surface of any of the color conversion layer 12R, color conversion layer 12G, and layer 12B; a portion located between the substrate 40 and any of the color conversion layer 12R, color conversion layer 12G, and layer 12B; and a portion located on the partition wall 20. In this case, since the side and top surfaces of the partition wall 20 are covered by the inorganic film 21 and inorganic film 22, the diffusion of constituent elements from the side surface of the partition wall 20 can be prevented. Therefore, the effect of suppressing the deterioration of the color conversion layer 12R, color conversion layer 12G, and layer 12B can be further enhanced. Thus, an even more reliable display device can be made.

[0309] Furthermore, in the configuration shown in Figure 6A, it can be said that in each subpixel, the inorganic film 21, the color conversion layer 12R, the color conversion layer 12G, or layer 12B, and the inorganic film 22 overlap each other. Also, between each subpixel, the partition wall 20, the inorganic film 21, and the inorganic film 22 overlap each other. Furthermore, in each subpixel, it can be said that the color conversion layer 12R, the color conversion layer 12G, or layer 12B is located between the inorganic film 21 and the inorganic film 22. Also, between each subpixel, the inorganic film 21 is located between the partition wall 20 and the inorganic film 22. Regardless of these expressions, the structure can be described by referring to the drawings. The same applies to other drawings.

[0310] The cross-sectional view shown in Figure 6B shows a configuration that includes an inorganic film 23 in addition to the configuration shown in Figure 6A. The inorganic film 23 has a configuration that includes a portion located between the substrate 40 and the partition wall 20, and a portion located between the substrate 40 and the inorganic film 21. By having a configuration that includes an inorganic film 23, the periphery of the partition wall 20 is surrounded by inorganic films 21, 22, and 23. Therefore, even if constituent elements are released from the side of the partition wall 20, these constituent elements can be contained in the region surrounded by inorganic films 21, 22, and 23, thereby reliably preventing them from diffusing into the surroundings. Consequently, the effect of suppressing the degradation of the color conversion layer 12R, color conversion layer 12G, and layer 12B can be further enhanced. Thus, an even more reliable display device can be made.

[0311] Furthermore, in the configuration shown in Figure 6B, it can be said that in each subpixel, the inorganic film 23, inorganic film 21, color conversion layer 12R, color conversion layer 12G, or layer 12B, and inorganic film 22 are all overlapping each other. Also, between each subpixel, the inorganic film 23, partition wall 20, inorganic film 21, and inorganic film 22 are all overlapping each other. Furthermore, in each subpixel, it can be said that either color conversion layer 12R, color conversion layer 12G, or layer 12B is located between inorganic film 21 and inorganic film 22. Also, in each subpixel, inorganic film 21 is located between inorganic film 23 and either color conversion layer 12R, color conversion layer 12G, or layer 12B. Furthermore, between each subpixel, inorganic film 21 is located between partition wall 20 and inorganic film 22. Regardless of these expressions, the structure can be described by referring to the drawings. The same applies to other drawings.

[0312] The inorganic films 21 and 23 can be made from materials similar to those used for the inorganic film 22. Furthermore, it is preferable that the film thicknesses of the inorganic films 21 and 23 be the same as those of the inorganic film 22.

[0313] The cross-sectional view shown in Figure 6C shows a configuration in which layer 12B is not provided, as in the configuration shown in Figure 6A. For example, if the sub-pixel 11B is a blue sub-pixel and the light-emitting device 110 emits blue light, then it is not necessary to convert the color of the light emitted by the light-emitting device 110 with layer 12B, and therefore layer 12B does not need to be provided on the sub-pixel 11B. In this case, it is preferable that the inorganic film 21 and the inorganic film 22 are in contact in region 24. In this case, it is possible to prevent the constituent elements of the partition wall 20 from diffusing from the partition wall 20, and thus the effect of suppressing the deterioration of the color conversion layer 12R and the color conversion layer 12G by the inorganic film 21 and the inorganic film 22 can be further enhanced.

[0314] The cross-sectional view shown in Figure 6D shows a configuration in which, in addition to the configuration shown in Figure 6B, a colored layer 14R that transmits red light is provided on the sub-pixel 11R, a colored layer 14G that transmits green light is provided on the sub-pixel 11G, and a colored layer 14B that transmits blue light is provided on the sub-pixel 11B. Specifically, colored layers of each color (colored layer 14R, colored layer 14G, colored layer 14B) are provided between the substrate 40 and the inorganic film 23. Some of the light emitted by the light-emitting device may be transmitted directly without being converted by the color conversion layer. By extracting the light that has been transmitted through the color conversion layer via the colored layer, light other than the desired color can be absorbed by the colored layer, thereby increasing the color purity of the light exhibited by the sub-pixel.

[0315] Each colored layer can use one or more of the following materials: metal, resin, pigment, or dye. Furthermore, each colored layer can be formed at a desired position using methods such as printing, inkjet printing, or photolithography etching.

[0316] This embodiment can be combined with other embodiments as appropriate.

[0317] (Embodiment 3) In this embodiment, an example of the configuration of a light-emitting device according to one aspect of the present invention and an example of a method for manufacturing the same will be described.

[0318] One aspect of the present invention is a display device having light-emitting devices (also called light-emitting elements). The display device has two or more light-emitting devices with different emission colors. Each light-emitting device has a pair of electrodes and an organic compound layer between them. Preferably, the light-emitting devices are organic electroluminescent devices (organic electroluminescent devices). For example, a full-color display device can be realized by having three types of light-emitting devices that emit red (R), green (G), or blue (B) light, respectively.

[0319] A partition wall is provided between two adjacent light-emitting devices (a first light-emitting device and a second light-emitting device) to divide the organic compound layer. This partition wall is a conductive structure with an inverse tapered shape. The partition wall can also be described as having a shape where its upper part protrudes laterally more than its lower part. The partition wall is formed so as to be located between two adjacent pixel electrodes. The partition wall is also provided so as to surround one pixel electrode. When the organic compound layer of the first light-emitting device is deposited, a step is created by the partition wall.

[0320] In this specification, "step breakage" refers to the phenomenon in which a layer, film, electrode, etc., is divided due to the shape of the surface on which it is formed (for example, a step or other difference in height).

[0321] Next, the upper electrode is formed by covering the organic compound layer and the partition wall. At this time, the upper electrode is formed by a film deposition method that provides higher step coverage than the organic compound layer. This allows a configuration in which a part of the upper electrode covers the edge of the organic compound layer and also contacts a part of the partition wall. Next, a protective layer is formed to cover the upper electrode and the partition wall. The protective layer is preferably formed by atomic layer deposition (ALD), which provides extremely high step coverage. This makes it possible to obtain a good protective film with few defects such as pinholes.

[0322] Below, we will explain more specific examples with reference to the diagrams.

[0323] [Configuration Example] Figure 7 shows a schematic top view of a unit 31 of the display device 100, which includes transistors and light-emitting devices. The unit 31 has a plurality of transistors 150 and a plurality of light-emitting devices 110. In Figure 7, the X and Y directions, which are orthogonal to each other, are indicated by arrows.

[0324] The light-emitting devices 110 are arranged in a matrix. Figure 7 shows a so-called stripe arrangement, where light-emitting devices of the same color are arranged in the Y direction. Note that the arrangement method of the light-emitting devices is not limited to this, and other arrangement methods such as S-stripe arrangement, delta arrangement, zigzag arrangement may be applied, or a pentile arrangement may be used.

[0325] As the light-emitting device 110, it is preferable to use an EL element such as an OLED (Organic Light Emitting Diode) or a QLED (Quantum-dot Light Emitting Diode). Examples of light-emitting materials for the EL element include fluorescent materials, phosphorescent materials, and thermally activated delayed fluorescence (TADF) materials. Not only organic compounds but also inorganic compounds (such as quantum dot (Q-dot) materials) can be used as light-emitting materials for the EL element.

[0326] Furthermore, partition walls 120 are provided between each light-emitting device 110. The partition walls 120 have a grid-like upper surface shape. It can also be said that the light-emitting devices 110 are provided in the area surrounded by the partition walls 120.

[0327] As shown in Figure 7, in a plan view, a gap is provided between the partition wall 120 and the light-emitting device 110. Figure 7 shows the gap Sx in the X direction and the gap Sy in the Y direction between the light-emitting device 110 and the partition wall 120.

[0328] Figure 8A is a schematic cross-sectional view of the display device 100 corresponding to the cutting line A-B shown in Figure 7. The display device 100 has a plurality of transistors 150 and a light-emitting device 110.

[0329] A transistor 150 is provided on a substrate 109. The transistor 150 has a semiconductor layer 151 on which a channel is formed, an insulating layer 152 that functions as a gate insulating layer, a conductive layer 153 that functions as a gate electrode, and a pair of conductive layers 154 that are in contact with the semiconductor layer 151 and function as a source electrode and a drain electrode. The conductive layers 154 are provided on an insulating layer 131 that covers the semiconductor layer 151, the insulating layer 152, and the conductive layers 153, and are in contact with the semiconductor layer 151 at an opening provided in the insulating layer 131.

[0330] It is preferable to use a metal oxide (also called an oxide semiconductor) that exhibits semiconductor properties as the semiconductor layer 151. As the oxide semiconductor, an oxide semiconductor such as indium oxide or In-Ga-Zn oxide (IGZO) can be used. Alternatively, the semiconductor layer of the transistor may have silicon. Examples of silicon include amorphous silicon and crystalline silicon (low-temperature polysilicon, single-crystal silicon, etc.).

[0331] In addition, metal oxides that can be used in the semiconductor layer 151 include tin oxide, zinc oxide, indium tin oxide, indium titanium oxide, indium gallium oxide, indium tungsten oxide, indium zinc oxide, indium gallium aluminum oxide, indium gallium tin oxide, gallium zinc oxide, aluminum zinc oxide, indium aluminum zinc oxide, indium tin zinc oxide, indium titanium zinc oxide, indium gallium zinc oxide, indium gallium tin zinc oxide, and indium gallium aluminum zinc oxide. Alternatively, silicon-containing indium tin oxide, gallium tin oxide, aluminum tin oxide, etc., can also be used.

[0332] In this example, transistor 150 is shown as a so-called top-gate type transistor, where the gate electrode is located on the upper side of the semiconductor layer, but it is not limited to this. For example, a bottom-gate type transistor, where the gate electrode is located below the semiconductor layer, can also be used.

[0333] An insulating layer 132 is provided to cover the conductive layer 154 and the insulating layer 131, and the light-emitting device 110 is provided over the insulating layer 132. The light-emitting device 110 includes an organic compound layer 103 between a first electrode 101 and a second electrode 102.

[0334] Each of the first electrodes 101 is provided over the insulating layer 132, and is connected to the conductive layer 154 in an opening provided in the insulating layer 132. Accordingly, each of the first electrodes 101 is connected to one of a source electrode and a drain electrode of the transistor 150.

[0335] The organic compound layer 103 included in the light-emitting device 110 contains at least a light-emitting organic compound that emits light. Note that the organic compound layer 103 may include one or more of an electron injection layer, an electron transport layer, an electron blocking layer, a hole injection layer, a hole transport layer, and a hole blocking layer, in addition to a layer containing a light-emitting substance (a light-emitting layer).

[0336] A conductive film having translucency to visible light is used for one of each first electrode 101 and the second electrode 102, and a conductive film having reflectivity is used for the other. By making each first electrode 101 light-transmissive and the second electrode 102 reflective, a bottom-emission type light-emitting device can be obtained. Conversely, by making each first electrode 101 reflective and the second electrode 102 light-transmissive, a top-emission type light-emitting device can be obtained. Note that by making both each first electrode 101 and the second electrode 102 light-transmissive, a dual-emission type display device can also be obtained.

[0337] Furthermore, a protective layer 135 is provided covering the second electrode 102. Each protective layer 135 can be, for example, a single-layer structure or a multi-layer structure including at least an inorganic insulating film. Examples of inorganic insulating films include oxide films or nitride films such as silicon oxide film, silicon oxide nitride film, silicon nitride film, silicon nitride film, aluminum oxide film, aluminum oxide nitride film, and hafnium oxide film. Alternatively, semiconductor materials such as indium gallium oxide and indium gallium zinc oxide may be used as the protective layer 135. Aluminum oxide and silicon nitride are particularly preferred due to their high barrier properties against water.

[0338] Furthermore, a laminated film of an inorganic insulating film and an organic insulating film can also be used as the protective layer 135. For example, it is preferable to have a configuration in which an organic insulating film is sandwiched between a pair of inorganic insulating films.

[0339] An insulating layer 133 is provided to cover the ends of each first electrode 101. The portion of the first electrode 101 that is not covered by the insulating layer 133 functions as the light-emitting region of the light-emitting device 110. The ends of the insulating layer 133 are preferably tapered. The insulating layer 133 may be omitted if it is not needed.

[0340] In this specification, an object is said to have a tapered shape if the angle between the side surface of the object and the contact surface between the object and the surface to be formed (also called the taper angle) is greater than 0 degrees and less than 90 degrees, and the cross-sectional shape has a thickness that increases continuously from the end. On the other hand, an object is said to have an inverse tapered shape if the angle between the side surface of the object and the contact surface between the object and the surface to be formed is greater than 90 degrees and less than 180 degrees.

[0341] The insulating layer 133 preferably contains an organic resin. By using an organic resin as the insulating layer 133, adhesion with the organic compound layer 103 can be improved, thereby improving the manufacturing yield. Furthermore, by using an organic resin in the insulating layer 133, its surface can be made flat or gently curved. Therefore, the coverage of the film formed on the insulating layer 133 can be improved.

[0342] Examples of materials that can be used for the insulating layer 133 include acrylic resin, polyimide resin, epoxy resin, polyamide resin, polyimidoamide resin, siloxane resin, benzocyclobutene resin, phenol resin, and precursors of these resins.

[0343] Each organic compound layer 103 has a region in contact with the upper surface of the first electrode 101 and a region in contact with the surface of the insulating layer 133. The ends of each organic compound layer 103 are located on the insulating layer 133.

[0344] A partition wall 120 is provided on the insulating layer 133. The partition wall 120 is conductive and has an inverse tapered shape. An organic compound layer 103a may also be formed on the partition wall 120. The organic compound layer 103a has the same structure as the organic compound layer 103.

[0345] Figure 9A shows two light-emitting devices 110, a partition wall 120 located between them, and an enlarged view of the vicinity thereof. The organic compound layer 103 has its ends located on the insulating layer 133. The second electrode 102 covers the ends of the organic compound layer 103 and is in contact with the upper surface of the insulating layer 133 and a portion of the side surface of the partition wall 120.

[0346] Since the second electrode 102 is in contact with the conductive partition wall 120, it can also be said that it is connected via the partition wall 120. Furthermore, as shown in Figure 7, the partition wall 120 is provided in a grid pattern so as to weave between the light-emitting devices 110, so the second electrode 102 of all light-emitting devices 110 is connected via the partition wall 120. In addition, the partition wall 120 also functions as wiring that supplies potential to the second electrode 102 of each light-emitting device 110.

[0347] As shown in Figure 9A, the insulating layer 133 has its end located on the first electrode 101. The gap Sx corresponds to the space between the end of the insulating layer 133 and the end of the most protruding part of the partition wall 120. The presence of the gap Sx allows the end of the organic compound layer 103, which is stepped off by the partition wall 120 during film formation, to be formed on the insulating layer 133 and not on the first electrode 101. For example, if the end of the organic compound layer 103 is located on the first electrode 101, the second electrode 102 covering the organic compound layer 103 may come into contact with the first electrode 101, potentially causing an electrical short circuit. Therefore, it is important to provide a gap Sx between the end of the insulating layer 133 and the partition wall 120 in order to ensure that the end of the organic compound layer 103 is reliably located on the insulating layer 133. The same applies to the gap Sy.

[0348] Preferably, the height h of the partition wall 120 is greater than the thickness of the organic compound layer 103. Furthermore, the taper angle θ of the partition wall 120 can be greater than 90 degrees and less than 180 degrees. The closer the taper angle θ is to 90 degrees, the easier it is for the partition wall 120 and the second electrode 102 to come into contact during the formation of the second electrode 102. However, the smaller the gap between the end of the organic compound layer 103 and the partition wall 120, the less space may be available for the second electrode 102 and the partition wall 120 to come into contact. Also, the closer the taper angle θ is to 180 degrees, the more likely the organic compound layer 103 is to break in steps, while making it difficult to bring the second electrode 102 and the partition wall 120 into contact. Therefore, the taper angle θ should be, for example, 95 degrees or more and 150 degrees or less, preferably 100 degrees or more and 135 degrees or less. Furthermore, if the coverage of the second electrode 102 is sufficiently high, an even larger taper angle θ can be used. For example, the taper angle θ can be set to 105 degrees or more and 175 degrees or less, preferably 120 degrees or more and 170 degrees or less.

[0349] Here, the taper angle θ is shown as the angle between the bottom and side surfaces of the partition wall 120. However, as shown in Figure 9A, it can also be expressed as the angle (taper angle θ') between the side surface of the partition wall 120 and the upper surface of the underlayment (insulating layer 133 in this case) that does not come into contact with the partition wall 120. In that case, it can be expressed as θ' ​​= 180 degrees - θ (both θ and θ' are between 0 and 180 degrees). That is, the preferred range for the taper angle θ' can be expressed as 30 degrees to 85 degrees, preferably 45 degrees to 80 degrees, or 5 degrees to 75 degrees, preferably 10 degrees to 60 degrees. When deciding which angle to use to express the taper angle, one should choose the one that is easier to measure, taking into account the surface shape of the underlayment (e.g., insulating layer 133).

[0350] The partition wall 120 can be made of various conductive materials. For example, metals, alloys, oxide conductive materials, nitride conductive materials, etc., can be used. For example, metallic materials such as gold, silver, platinum, magnesium, nickel, tungsten, chromium, molybdenum, iron, cobalt, copper, palladium, titanium, aluminum, yttrium, zirconium, and tantalum, or alloy materials containing such metallic materials, can be used.

[0351] Furthermore, it is preferable that the partition wall 120 contains an oxide conductive material containing indium. This is preferable because it can reduce the contact resistance with the second electrode 102. For example, an oxide conductive material such as indium tin oxide can be used. Other materials that can be used include indium oxide, indium zinc oxide, indium titanium oxide, indium gallium zinc oxide, indium tin zinc oxide, indium titanium zinc oxide, and indium gallium tin zinc oxide. Alternatively, indium tin oxide containing silicon can also be used. In addition, an oxide conductive material that does not contain indium, such as zinc oxide, may be used.

[0352] This configuration allows for the creation of distinct organic compound layers between adjacent light-emitting devices, substantially eliminating leakage current through the organic compound layers compared to cases where the organic compound layers are in contact with each other or where a common organic compound layer is used. This prevents unintended light emission, resulting in a display device with high contrast and high display quality. Furthermore, since the organic compound layer 103 is covered by the second electrode 102 and the protective layer 135 within the region surrounded by the partition wall 120, it prevents the diffusion of impurities such as moisture into the organic compound layer 103, resulting in a highly reliable display device. Moreover, this configuration does not require the use of a metal mask, and all processing of the organic compound layer 103, etc., can be performed using photolithography, making it easier to achieve high resolution and high aperture ratio compared to cases where a metal mask is used.

[0353] Figure 8A and others show an example in which the partition wall 120 is provided on the insulating layer 133, but the insulating layer 133 does not need to be provided. Figure 8B shows an example in which the insulating layer 133 is not provided. In Figure 8B, the partition wall 120 is provided in contact with the upper surface of the insulating layer 132, similar to the first electrode 101. Also, the ends of each organic compound layer 103 are located on the insulating layer 132, and each second electrode 102 is in contact with the insulating layer 132 and the partition wall 120.

[0354] Furthermore, in Figures 8 and 9, the height of the partition wall 120 is depicted as being greater than its width, but in reality, the cross-sectional width may be formed to be greater than the height.

[0355] Furthermore, while Figures 8 and 9A show an example where the second electrode 102 is continuous from the side to the top of the partition wall 120 without being stepped by the partition wall 120, the second electrode 102 may be stepped. Figure 9B shows an example where the second electrode 102 is stepped. In this case, the partition wall 120 has a conductive layer 102a that covers the side and top surfaces of the organic compound layer 103a. The conductive layer 102a contains the same material as the second electrode 102. The protective layer 135 also has portions that are in contact with the side surfaces of the partition wall 120. With this configuration, the entire second electrode 102, including its end, can be covered by the protective layer 135 and the partition wall 120. This prevents water and other substances from diffusing into the light-emitting device 110 from the outside via the second electrode 102, and prevents the second electrode 102 itself from deteriorating.

[0356] The partition wall 120 shown in Figure 9A, etc., is an example having an inverse tapered shape. The shape of the partition wall 120 exemplified in Figure 9A, etc., can also be described as having a roughly trapezoidal shape in cross-section, where the length of the upper base is longer than the length of the lower base. However, the shape of the partition wall 120 is not limited to this, and various shapes can be taken as long as the organic compound layer 103 can be stepped. The partition wall 120 can also have a symmetrical shape in cross-section. If the upper surface of the partition wall 120 is flat, the shape of the partition wall 120 in cross-section will be a polygon with an even number of corners. Examples of other cross-sectional shapes of the partition wall 120 will be described below.

[0357] The examples shown in Figures 10A and 10B are examples in which the side surface of the partition wall 120 has a curved shape. In Figure 10A, it has a concave curved surface, and in Figure 10B, it has a convex curved surface.

[0358] When the side surface of the partition wall 120 has a curved shape, it is difficult to uniquely determine the taper angle θ. In such cases, as shown in Figures 10A and 10B, a straight line connecting the point of the widest part of the partition wall 120 in a cross-sectional view and the point of the end of the contact surface between the partition wall 120 and the underlayment (insulating layer 133) can be assumed to be a hypothetical side surface of the partition wall 120, and the angle between this straight line and the contact surface between the partition wall 120 and the underlayment (insulating layer 133) can be defined as the taper angle θ.

[0359] Here, the partition wall 120 only needs to have a tapered shape in a portion including at least the part that is in contact with the substrate film, and the shape of the part above that is not specified. As shown in Figure 10C, the partition wall 120 can be divided into a lower part 120B (also called the first part) which has a tapered shape, and an upper part 120T (also called the second part) which is located above the lower part 120B. Since the upper part 120T can take various shapes, its shape is not explicitly shown here and is indicated by a dashed line. Below, examples of upper parts 120T with different shapes will be described.

[0360] Figure 10D shows an example where the upper part 120T has a rectangular shape in cross-section. Figures 10E and 10F show examples where the upper part 120T has a trapezoidal shape in cross-section, where the length of the upper side (also called the upper base) is shorter than the length of the lower side (also called the lower base). Figure 10E shows an example where the height of the upper part 120T is smaller than the lower part 120B, and Figure 10F shows an example where the heights of the upper part 120T and the lower part 120B are roughly the same. The partition walls 120 shown in Figures 10D, 10E, and 10F can also be said to have a hexagonal shape in cross-section.

[0361] Figure 10G shows an example where the partition wall 120 has an octagonal shape in cross-sectional view. In Figure 10G, a portion of the side surface of the partition wall 120 is approximately perpendicular to the surface to be formed.

[0362] Figures 10H and 10I are modified examples of Figures 10A and 10B, respectively, and are examples having a curved lower part 120B and a trapezoidal upper part 120T in cross-sectional view.

[0363] Although the above shows that the side surface of the partition wall 120 has corners, depending on the processing method of the partition wall 120, the corners may be rounded. In particular, when the partition wall 120 is formed by an isotropic etching method such as wet etching, the corners tend to be rounded.

[0364] The above is an explanation of the example configuration.

[0365] [Example of Method for Manufacturing a Light-Emitting Device] Below, an example of a method for manufacturing a display device according to one aspect of the present invention will be described with reference to the drawings. Here, the display device 100 shown in the above configuration example will be used as an example. Figures 11A to 11F are schematic cross-sectional views of each step in the method for manufacturing the display device illustrated below.

[0366] Furthermore, thin films (insulating films, semiconductor films, conductive films, etc.) that constitute the display device can be formed using methods such as sputtering, chemical vapor deposition (CVD), vacuum deposition, pulsed laser deposition (PLD), and atomic layer deposition (ALD).

[0367] Furthermore, thin films (insulating films, semiconductor films, conductive films, etc.) that constitute the display device can be formed by methods such as spin coating, dip coating, spray coating, inkjet printing, dispensing, screen printing, offset printing, doctor knife coating, slit coating, roll coating, curtain coating, and knife coating.

[0368] Sputtering methods include RF sputtering, which uses a high-frequency power supply for sputtering; DC sputtering, which uses a DC power supply; and pulsed DC sputtering, which changes the voltage applied to the electrodes in pulses. For film deposition using insulating targets, RF sputtering is preferable. DC sputtering is mainly used when depositing films using conductive targets. In addition to forming conductive films, DC sputtering can also be used to form insulating films by reactive sputtering using pulsed DC sputtering. Specifically, pulsed DC sputtering can be used when depositing compounds such as oxides, nitrides, and carbides using reactive sputtering.

[0369] CVD methods can be classified into plasma-enhanced CVD (PECVD), which utilizes plasma; thermal CVD (TCD), which utilizes heat; and photo-CVD (Photo-CVD), which utilizes light. Furthermore, depending on the source gas used, they can be divided into metal CVD (MCCVD) and metal-organic CVD (MOCVD) methods.

[0370] Plasma CVD allows for the production of high-quality films at relatively low temperatures. Thermal CVD, on the other hand, does not use plasma, thus minimizing plasma damage to the workpiece. Furthermore, thermal CVD avoids plasma damage during film formation, resulting in films with fewer defects.

[0371] As ALD methods, thermal ALD, which carries out the reaction of the precursor and reactant using only thermal energy, and PEALD, which uses plasma-excited reactants, can be used.

[0372] Unlike sputtering, CVD and ALD are film deposition methods that are less affected by the shape of the workpiece and provide good step-level coverage. In particular, the ALD method is suitable for coating the surface of openings with high aspect ratios due to its excellent step-level coverage and excellent thickness uniformity. However, since the ALD method has a relatively slow deposition rate, it is sometimes preferable to use it in combination with other film deposition methods that have a faster deposition rate, such as the CVD method.

[0373] In CVD (Chemical Vapor Deposition), films of any composition can be deposited by changing the flow rate ratio of the raw material gases. For example, in CVD, by changing the flow rate ratio of the raw material gases while the film is being deposited, films with continuously changing compositions can be deposited. When depositing films while changing the flow rate ratio of the raw material gases, the time required for film deposition can be shortened compared to depositing films using multiple deposition chambers, because time spent on transport or pressure adjustment is eliminated. Therefore, it may be possible to increase the productivity of semiconductor devices.

[0374] In the ALD method, films of any composition can be deposited by simultaneously introducing multiple different types of precursors. Alternatively, when introducing multiple different types of precursors, films of any composition can be deposited by controlling the number of cycles for each precursor. Furthermore, similar to the CVD method, films with continuously changing compositions can be deposited.

[0375] Furthermore, the thin films constituting the display device can be processed using photolithography or other methods. Alternatively, the thin films may be processed by nanoimprint lithography, sandblasting, lift-off methods, etc. Island-like thin films may also be directly formed using a film deposition method with a shielding mask such as a metal mask. Induced self-assembly (DSA) methods may also be used.

[0376] There are two main methods of photolithography. One method involves forming a resist mask on the thin film to be processed, then processing the thin film by etching or other means, and removing the resist mask. The other method involves forming a photosensitive thin film, then exposing and developing it to process the thin film into the desired shape.

[0377] In photolithography, the light used for exposure can be, for example, i-line (wavelength 365 nm), g-line (wavelength 436 nm), h-line (wavelength 405 nm), or a mixture thereof. Other light sources such as ultraviolet light, KrF laser light, or ArF laser light can also be used. Exposure may also be performed using immersion lithography. Furthermore, extreme ultraviolet (EUV) light or X-rays may be used as the light source for exposure. An electron beam can also be used instead of the light source for exposure. Using extreme ultraviolet light, X-rays, or an electron beam is preferable because it enables extremely fine processing. Note that a photomask is not required when exposure is performed by scanning a beam such as the above-mentioned light or an electron beam.

[0378] Thin films can be etched using methods such as dry etching, wet etching, and sandblasting. Dry etching allows for isotropic or anisotropic etching by controlling the conditions. Wet etching allows for isotropic etching.

[0379] First, a substrate 109 is prepared, and the transistor 150, insulating layer 131, insulating layer 132, etc. are formed on it. Next, a conductive film is deposited on the insulating layer 132, and the first electrode 101 is formed by removing unnecessary parts by etching.

[0380] When using a conductive film that is reflective to visible light as each first electrode 101, it is preferable to use a material (for example, silver or aluminum) that has the highest possible reflectivity across the entire wavelength range of visible light. This not only improves the light extraction efficiency of the light-emitting device but also enhances color reproduction.

[0381] Next, an insulating layer 133 is formed by covering the ends of each first electrode 101 (Figure 11A). An organic insulating film or an inorganic insulating film can be used as the insulating layer 133. It is preferable that the ends of the insulating layer 133 be tapered in order to improve the step coverage of the subsequent EL film. In particular, when using an organic insulating film, it is preferable to use a photosensitive material because it is easier to control the shape of the ends depending on the exposure and development conditions.

[0382] Next, a conductive film 120f, which will later become the partition wall 120, is formed. It is preferable to use a material for the conductive film 120f that allows for a large selectivity ratio of etching rate with respect to each of the first electrodes 101. It is preferable to use different conductive materials for the conductive film 120f and the layer located at the top of the first electrodes 101. Alternatively, a film that functions as an etching stopper may be formed before the conductive film 120f, and this film located on the first electrodes 101 may be removed after etching of the conductive film 120f. In that case, the same conductive material can be used for the first electrodes 101 and the conductive film 120f.

[0383] Next, a resist mask 141 is formed on the conductive film 120f (Figure 11B). Subsequently, the portion of the conductive film 120f not covered by the resist mask 141 is removed by etching to form a partition wall 120, and then the resist mask 141 is removed (Figure 11C).

[0384] The conductive film 120f can be etched by an isotropic etching method. For example, a wet etching method or an isotropic dry etching method can be used. Wet etching is particularly preferable because it excels in isotropic etching and exhibits good processability even when the conductive film 120f is thin. By processing the conductive film 120f so that etching proceeds faster at the bottom than at the top, a partition wall 120 having an inverse tapered shape can be formed.

[0385] For example, by selecting materials such that the adhesion between the conductive film 120f and the insulating layer 133 is lower than the adhesion between the conductive film 120f and the resist mask 141, the etching rate at the bottom is improved compared to the top, and a reverse tapered partition wall 120 can be formed. For example, if a conductive oxide such as indium tin oxide is used for the conductive film 120f, an organic material with low adhesion to indium tin oxide (e.g., acrylic resin) can be used for the insulating layer 133.

[0386] Next, an organic compound layer 103 is formed on each of the first electrodes 101 and the partition walls 120 (Figure 11D). At this time, the organic compound is stepped by the partition walls 120, and an organic compound layer 103 is formed between the partition walls 120, and an organic compound layer 103a is formed on top of the partition walls 120. The organic compound layer 103 can be formed using, for example, vacuum deposition, sputtering, or both.

[0387] Next, the second electrode 102 is formed by covering the organic compound layer 103, etc. (Figure 11E). At this time, the second electrode 102 is formed so as to cover the edge of the organic compound layer 103 and to be in contact with at least a part of the side surface of the partition wall 120. The second electrode 102 can be formed using one or more of the following methods: vacuum deposition, sputtering, and CVD.

[0388] Next, a protective layer 135 is formed by covering the second electrode 102 (Figure 11F). The protective layer 135 is preferably formed by a film deposition method that provides high step coverage, and is preferably formed by CVD or ALD. The ALD method is particularly preferred because it causes less damage to the layer to be formed.

[0389] For example, an aluminum oxide film can be formed as the protective layer 135 by the ALD method. In this case, it is preferable to use trimethylaluminum, triethylaluminum, triisobutylaluminum, dimethylaluminum hydride, tris(dimethylamino)aluminum, tris(diethylamino)aluminum, or aluminum trichloride as the aluminum precursor. Furthermore, as the oxidizing agent, for example, ozone (O) 3 ), oxygen (O 2 ), water (H 2 O), Nitrogen dioxide (NO) 2 ), nitrous oxide (N 2 O), hydrogen peroxide (H 2 O 2 ) and others can be used, and two or more of these may be used.

[0390] Furthermore, the protective layer 135 may be a laminated structure of a film deposited by the ALD method and a film deposited by a film deposition method other than the ALD method (e.g., CVD method, sputtering method, etc.). While the ALD method has extremely high step coverage, its deposition rate is relatively slow compared to other film deposition methods. Therefore, by first depositing a film with very few defects using the ALD method, and then forming a thick insulating film using the CVD method or the like, the time required for the deposition process of the protective layer 135 can be shortened.

[0391] The display device 100 can be manufactured through the above process.

[0392] (Embodiment 4) This embodiment describes an example of the configuration of a display device according to one aspect of the present invention.

[0393] The display device of this embodiment can be a high-resolution display device or a large-screen display device. Therefore, the display device of this embodiment can be used in electronic devices with relatively large screens, such as television sets, desktop or notebook personal computers, computer monitors, digital signage, and large game machines such as pachinko machines, as well as in the display units of digital cameras, digital video cameras, digital photo frames, mobile phones, portable game consoles, smartphones, smartwatches, tablet devices, personal digital assistants, and audio playback devices.

[0394] [Display device 400A] Figure 12 shows a perspective view of the display device 400A, and Figure 13 shows a cross-sectional view of the display device 400A.

[0395] The display device 400A has a configuration in which substrate 452 and substrate 451 are bonded together. In Figure 12, substrate 452 is clearly indicated by a dashed line.

[0396] The display device 400A includes a display unit 462, a circuit 464, wiring 465, etc. Figure 12 shows an example in which IC 473 and FPC 472 are mounted on the display device 400A. Therefore, the configuration shown in Figure 12 can also be described as a display module having the display device 400A, an IC (integrated circuit), and an FPC.

[0397] For example, a scan line drive circuit can be used as circuit 464.

[0398] The wiring 465 has the function of supplying signals and power to the display unit 462 and the circuit 464. These signals and power are input to the wiring 465 from an external source via the FPC 472, or from the IC 473.

[0399] Figure 12 shows an example in which IC 473 is provided on the substrate 451 using the COG (Chip On Glass) method or the COF (Chip On Film) method. IC 473 can be an IC having, for example, a scan line drive circuit or a signal line drive circuit. Note that the display device 400A and the display module may be configured without an IC. Alternatively, the IC may be mounted on the FPC using the COF method or the like.

[0400] Figure 13 shows an example of a cross-section obtained by cutting a portion of the display device 400A, including the FPC 472, a portion of the circuit 464, a portion of the display unit 462, and a portion of the area including the end.

[0401] The display device 400A shown in Figure 13 has a transistor 201, a transistor 205, a light-emitting device 430a, a light-emitting device 430b, and a light-emitting device 430c, etc., between the substrate 451 and the substrate 452.

[0402] The light-emitting devices 430a, 430b, and 430c can be the light-emitting devices exemplified in Embodiment 1. Each light-emitting device 430 includes a pixel electrode 411a, 411b, or 411c, an island-shaped organic compound layer having a light-emitting layer, and an upper electrode.

[0403] Each protective layer 416 and the substrate 452 are bonded together via an adhesive layer 442. For sealing the light-emitting device, a solid encapsulation structure or a hollow encapsulation structure can be applied. In Figure 13, the space 443 surrounded by the substrate 452, the adhesive layer 442, and the substrate 451 is filled with an inert gas (such as nitrogen or argon), indicating a hollow encapsulation structure. The adhesive layer 442 may be provided overlapping the light-emitting device. Alternatively, the space 443 surrounded by the substrate 452, the adhesive layer 442, and the substrate 451 may be filled with a resin different from the adhesive layer 442.

[0404] The light-emitting devices 430a, 430b, and 430c have an optical adjustment layer between the pixel electrode and the organic compound layer. Light-emitting device 430a has an optical adjustment layer 426a, light-emitting device 430b has an optical adjustment layer 426b, and light-emitting device 430c has an optical adjustment layer 426c. Details of the light-emitting devices can be found in Embodiment 1. Each optical adjustment layer 426 has a different thickness. It is also preferable that each optical adjustment layer 426 is made of the same material that has light transmittance and conductivity. It is preferable to use a conductive metal oxide film containing indium or zinc as the optical adjustment layer 426.

[0405] The pixel electrodes 411a, 411b, and 411c are each connected to the conductive layer 222b of the transistor 205 through an opening provided in the insulating layer 214.

[0406] The edges of the pixel electrodes and the optical adjustment layer are covered by an insulating layer 421. The pixel electrodes contain a material that reflects visible light, and the counter electrodes contain a material that transmits visible light.

[0407] The light emitted by the light-emitting device is projected onto the substrate 452. It is preferable to use a material with high transparency to visible light for the substrate 452.

[0408] A partition wall 420 is provided on the insulating layer 421. The partition wall 420 can be described by referring to the partition wall 120 shown in Embodiment 1. The partition wall 420 is provided in a region that overlaps with the light-shielding layer 417, which also serves as a barrier separating the color conversion layer. On the partition wall 420, a layer is provided which includes a part of the upper electrodes of two adjacent light-emitting devices on either side of the partition wall 420, and a layer which includes the same material as the organic compound layer. In addition, a protective layer 416 is provided which covers the partition wall 420.

[0409] Both transistors 201 and 205 are formed on the substrate 451. These transistors can be manufactured using the same materials and the same process.

[0410] On the substrate 451, insulating layers 211, 213, 215, and 214 are provided in this order. A portion of insulating layer 211 functions as a gate insulating layer for each transistor. A portion of insulating layer 213 functions as a gate insulating layer for each transistor. Insulating layer 215 is provided covering the transistors. Insulating layer 214 is provided covering the transistors and functions as a planarization layer. The number of gate insulating layers and insulating layers covering the transistors are not limited and may be a single layer or two or more layers, respectively.

[0411] It is preferable to use a material that does not easily allow impurities such as water and hydrogen to diffuse into at least one layer of the insulating layer covering the transistor. This allows the insulating layer to function as a barrier layer. With such a configuration, the diffusion of impurities from the outside into the transistor can be effectively suppressed, thereby improving the reliability of the display device.

[0412] It is preferable to use inorganic insulating films for insulating layers 211, 213, and 215. Examples of inorganic insulating films that can be used include silicon nitride, silicon oxide nitride, silicon oxide, silicon nitride, aluminum oxide, and aluminum nitride. Alternatively, hafnium oxide, yttrium oxide, zirconium oxide, gallium oxide, tantalum oxide, magnesium oxide, lanthanum oxide, cerium oxide, and neodymium oxide may also be used. Furthermore, two or more of the above insulating films may be laminated together.

[0413] Here, organic insulating films often have lower barrier properties than inorganic insulating films. Therefore, it is preferable that the organic insulating film has an opening near the edge of the display device 400A. This prevents impurities from entering through the organic insulating film from the edge of the display device 400A. Alternatively, the organic insulating film may be formed so that its edge is inward from the edge of the display device 400A, so that the organic insulating film is not exposed at the edge of the display device 400A.

[0414] An organic insulating film is preferred for the insulating layer 214, which functions as a planarizing layer. Examples of materials that can be used as the organic insulating film include acrylic resins, polyimide resins, epoxy resins, polyamide resins, polyimidoamide resins, siloxane resins, benzocyclobutene resins, phenolic resins, and precursors of these resins.

[0415] In the region 228 shown in Figure 13, an opening is formed in the insulating layer 214. This prevents impurities from entering the display unit 462 from the outside through the insulating layer 214, even when an organic insulating film is used for the insulating layer 214. Therefore, the reliability of the display device 400A can be improved.

[0416] Transistors 201 and 205 have a conductive layer 221 that functions as a gate, an insulating layer 211 that functions as a gate insulating layer, conductive layers 222a and 222b that function as source and drain, a semiconductor layer 231, an insulating layer 213 that functions as a gate insulating layer, and a conductive layer 223 that functions as a gate. Here, the same hatching pattern is applied to multiple layers obtained by processing the same conductive film. The insulating layer 211 is located between the conductive layer 221 and the semiconductor layer 231. The insulating layer 213 is located between the conductive layer 223 and the semiconductor layer 231.

[0417] The transistor structure of the display device of this embodiment is not particularly limited. For example, planar transistors, staggered transistors, inverse staggered transistors, etc., can be used. Furthermore, either a top-gate or bottom-gate transistor structure may be used. Alternatively, gates may be provided above and below the semiconductor layer in which the channel is formed.

[0418] Transistors 201 and 205 are configured in which a semiconductor layer on which a channel is formed is sandwiched between two gates. The transistors may be driven by connecting the two gates and supplying them with the same signal. Alternatively, the threshold voltage of the transistors may be controlled by applying a potential to control the threshold voltage to one of the two gates and a potential to drive the other gate.

[0419] The crystallinity of the semiconductor material used in the transistor is not particularly limited; amorphous semiconductors, single-crystal semiconductors, or semiconductors with crystalline properties other than single crystals (microcrystalline semiconductors, polycrystalline semiconductors, or semiconductors with crystalline regions in part) may be used. Using a single-crystal semiconductor or a semiconductor with crystalline properties is preferable because it can suppress the degradation of transistor characteristics.

[0420] The semiconductor layer of the transistor preferably has a metal oxide (also called an oxide semiconductor). In other words, the display device of this embodiment preferably uses a transistor (hereinafter referred to as an OS transistor) that uses a metal oxide in the channel formation region. Alternatively, the semiconductor layer of the transistor may have silicon. Examples of silicon include amorphous silicon and crystalline silicon (low-temperature polysilicon, single-crystal silicon, etc.).

[0421] The semiconductor layer preferably contains a metal oxide containing indium. In particular, it is especially preferable that it contains indium oxide.

[0422] Furthermore, the semiconductor layer preferably comprises, for example, indium, M (where M is one or more selected from gallium, aluminum, silicon, boron, yttrium, tin, copper, vanadium, beryllium, titanium, iron, nickel, germanium, zirconium, molybdenum, lanthanum, cerium, neodymium, hafnium, tantalum, tungsten, and magnesium), and zinc. In particular, M is preferably one or more selected from aluminum, gallium, yttrium, and tin.

[0423] In particular, it is preferable to use an oxide containing indium (In), gallium (Ga), and zinc (Zn) (also written as IGZO) as the semiconductor layer.

[0424] When the semiconductor layer is an In-M-Zn oxide, it is preferable that the atomic ratio of In in the In-M-Zn oxide is equal to or greater than the atomic ratio of M. Examples of such In-M-Zn oxide atomic ratios of metal elements include compositions where In:M:Zn = 1:1:1 or nearby, In:M:Zn = 1:1:1.2 or nearby, In:M:Zn = 2:1:3 or nearby, In:M:Zn = 3:1:2 or nearby, In:M:Zn = 4:2:3 or nearby, In:M:Zn = 4:2:4.1 or nearby, In:M:Zn = 5:1:3 or nearby, In:M:Zn = 5:1:6 or nearby, In:M:Zn = 5:1:7 or nearby, In:M:Zn = 5:1:8 or nearby, In:M:Zn = 6:1:6 or nearby, In:M:Zn = 5:2:5 or nearby, and so on. Note that "nearby composition" includes a range of ±30% of the desired atomic ratio.

[0425] For example, when the atomic ratio is stated as In:Ga:Zn = 4:2:3 or nearby, it includes cases where, with In set to 4, Ga is between 1 and 3, and Zn is between 2 and 4. Also, when the atomic ratio is stated as In:Ga:Zn = 5:1:6 or nearby, it includes cases where, with In set to 5, Ga is greater than 0.5 and 2 or less, and Zn is between 5 and 7. Furthermore, when the atomic ratio is stated as In:Ga:Zn = 1:1:1 or nearby, it includes cases where, with In set to 1, Ga is greater than 0.5 and 2 or less, and Zn is greater than 0.5 and 2 or less.

[0426] The transistors in circuit 464 and the transistors in display unit 462 may have the same structure or different structures. The structures of the multiple transistors in circuit 464 may all be the same or there may be two or more different structures. Similarly, the structures of the multiple transistors in display unit 462 may all be the same or there may be two or more different structures.

[0427] A connection portion 204 is provided in the region of substrate 451 where substrate 452 does not overlap. At the connection portion 204, wiring 465 is electrically connected to FPC 472 via a conductive layer 466 and a connecting layer 242. The conductive layer 466 is shown as an example of a laminated structure consisting of a conductive film obtained by processing the same conductive film as the pixel electrode and a conductive film obtained by processing the same conductive film as the optical adjustment layer. The conductive layer 466 is exposed on the upper surface of the connection portion 204. This allows the connection portion 204 and FPC 472 to be electrically connected via the connecting layer 242.

[0428] On the surface of the substrate 452 facing the substrate 451, a light-shielding layer 417 and a color conversion layer 412 (color conversion layer 412R, color conversion layer 412G, and color conversion layer 412B) are provided. Furthermore, it is preferable that the insulating layer 418 between the color conversion layer 412 and the light-emitting device contains particles for scattering light. Various optical components can be arranged on the outside of the substrate 452. Examples of optical components include polarizing plates, phase difference plates, light diffusion layers (such as diffusion films), anti-reflective layers, and light-collecting films. Additionally, an antistatic film to suppress dust adhesion, a water-repellent film to prevent dirt from adhering, a hard coat film to suppress scratches during use, and an impact-absorbing layer may be arranged on the outside of the substrate 452.

[0429] By providing a protective layer 416 that covers the light-emitting device, it is possible to suppress the ingress of impurities such as water into the light-emitting device and improve the reliability of the light-emitting device.

[0430] In the region 228 near the edge of the display device 400A, it is preferable that the insulating layer 215 and the protective layer 416 are in contact with each other through an opening in the insulating layer 214. In particular, it is preferable that the inorganic insulating film of the insulating layer 215 and the inorganic insulating film of the protective layer 416 are in contact with each other. This makes it possible to suppress impurities from entering the display unit 462 from the outside through the organic insulating film. Therefore, the reliability of the display device 400A can be improved.

[0431] The protective layer 416 may have a laminated structure of an organic insulating film and an inorganic insulating film. In this case, it is preferable that the edges of the inorganic insulating film extend outward more than the edges of the organic insulating film.

[0432] Substrates 451 and 452 can be made of glass, quartz, ceramics, sapphire, resin, metal, alloy, semiconductor, etc., respectively. The substrate on the side that extracts light from the light-emitting device should be made of a material that transmits the light. Using flexible materials for substrates 451 and 452 can increase the flexibility of the display device. Alternatively, a polarizing plate may be used as substrate 451 or substrate 452.

[0433] As substrates 451 and 452, the following can be used: polyester resins such as polyethylene terephthalate (PET) and polyethylene naphthalate (PEN), polyacrylonitrile resin, acrylic resin, polyimide resin, polymethyl methacrylate resin, polycarbonate (PC) resin, polyethersulfone (PES) resin, polyamide resin (nylon, aramid, etc.), polysiloxane resin, cycloolefin resin, polystyrene resin, polyamide-imide resin, polyurethane resin, polyvinyl chloride resin, polyvinylidene chloride resin, polypropylene resin, polytetrafluoroethylene (PTFE) resin, ABS resin, cellulose nanofiber, etc. One or both of substrates 451 and 452 may be made of glass of a thickness sufficient to provide flexibility.

[0434] Furthermore, when a circular polarizing plate is superimposed on a display device, it is preferable to use a substrate with high optical isotropy for the substrate of the display device. A substrate with high optical isotropy has low birefringence (or a small amount of birefringence).

[0435] For substrates with high optical isotropy, the absolute value of the retardation (phase difference) is preferably 30 nm or less, more preferably 20 nm or less, and even more preferably 10 nm or less.

[0436] Examples of films with high optical isotropy include triacetylcellulose (TAC, also known as cellulose triacetate) film, cycloolefin polymer (COP) film, cycloolefin copolymer (COC) film, and acrylic film.

[0437] Furthermore, when using a film as the substrate, the film may absorb water, potentially causing wrinkles or other shape changes in the display panel. Therefore, it is preferable to use a film with low water absorption for the substrate. For example, it is preferable to use a film with a water absorption rate of 1% or less, more preferable to use a film with a water absorption rate of 0.1% or less, and even more preferable to use a film with a water absorption rate of 0.01% or less.

[0438] Various types of curing adhesives can be used as the adhesive layer, including UV-curing adhesives, reaction-curing adhesives, thermosetting adhesives, and anaerobic adhesives. Examples of these adhesives include epoxy resins, acrylic resins, silicone resins, phenolic resins, polyimide resins, imide resins, PVC (polyvinyl chloride) resins, PVB (polyvinyl butyral) resins, and EVA (ethylene vinyl acetate) resins. Materials with low moisture permeability, such as epoxy resins, are particularly preferred. Two-component mixed resins may also be used. Adhesive sheets may also be used.

[0439] As the connecting layer 242, an anisotropic conductive film (ACF), an anisotropic conductive paste (ACP), or the like can be used.

[0440] Materials that can be used for conductive layers such as the gate, source, and drain of transistors, as well as various wirings and electrodes that constitute display devices, include metals such as aluminum, titanium, chromium, nickel, copper, yttrium, zirconium, molybdenum, silver, tantalum, and tungsten, as well as alloys mainly composed of these metals. Films containing these materials can be used as single layers or in a multilayer structure.

[0441] Furthermore, conductive oxides such as indium oxide, indium tin oxide, indium zinc oxide, zinc oxide, and zinc oxide containing gallium, or graphene can be used as the light-transmitting conductive material. Alternatively, metallic materials such as gold, silver, platinum, magnesium, nickel, tungsten, chromium, molybdenum, iron, cobalt, copper, palladium, and titanium, or alloy materials containing such metallic materials, can be used. Alternatively, nitrides of such metallic materials (e.g., titanium nitride) may be used. When using metallic materials or alloy materials (or their nitrides), it is preferable to make them thin enough to be light-transmitting. In addition, a laminated film of the above materials can be used as a conductive layer. For example, using a laminated film of a silver-magnesium alloy and indium tin oxide is preferable because it can enhance conductivity. These can also be used as conductive layers for various wirings and electrodes that constitute a display device, and as conductive layers (conductive layers that function as pixel electrodes or common electrodes) in light-emitting devices.

[0442] Examples of insulating materials that can be used for each insulating layer include resins such as acrylic resin and epoxy resin, and inorganic insulating materials such as silicon oxide, silicon oxide nitride, silicon nitride, silicon oxide, and aluminum oxide.

[0443] [Display Device 400B] Figure 14A shows a cross-sectional view of the display device 400B. The perspective view of the display device 400B is the same as that of the display device 400A (Figure 13). Figure 14A shows an example of a cross-section of the display device 400B when a part of the area including the FPC 472, a part of the circuit 464, and a part of the display unit 462 are cut. In Figure 14A, an example of a cross-section is shown when a part of the display unit 462, in particular, including the light-emitting devices 430b and 430c, is cut. Note that explanations of parts that are the same as those of the display device 400A may be omitted.

[0444] The display device 400B shown in Figure 14A has transistors 202, 210, light-emitting device 430b, and light-emitting device 430c between substrates 453 and 454.

[0445] The substrate 454 and the protective layer 416 are bonded together via an adhesive layer 442. The adhesive layer 442 is provided in superimposed on the light-emitting devices 430b and 430c, respectively, and a solid encapsulation structure is applied to the display device 400B.

[0446] The substrate 453 and the insulating layer 212 are bonded together by an adhesive layer 455.

[0447] The method for manufacturing the display device 400B involves first bonding a fabricated substrate, on which an insulating layer 212, transistors, light-emitting devices, etc., are provided, to a substrate 454 on which a light-shielding layer 417 is provided, using an adhesive layer 442. Then, the fabricated substrate is peeled off and a substrate 453 is attached to the exposed surface, thereby transferring the components formed on the fabricated substrate to the substrate 453. It is preferable that both the substrate 453 and the substrate 454 are flexible. This increases the flexibility of the display device 400B.

[0448] The insulating layer 212 can be made of an inorganic insulating film that can be used for insulating layer 211, insulating layer 213, and insulating layer 215, respectively.

[0449] The pixel electrodes are connected to the conductive layer 222b of the transistor 210 through an opening in the insulating layer 214. The conductive layer 222b is connected to the low-resistance region 231n through openings in the insulating layers 215 and 225. The transistor 210 has the function of controlling the driving of the light-emitting device.

[0450] The ends of the pixel electrodes are covered by an insulating layer 421.

[0451] The light emitted by the light-emitting devices 430b and 430c is emitted towards the substrate 454. It is preferable to use a material with high transparency to visible light for the substrate 454.

[0452] A connection portion 204 is provided in the region of substrate 453 that does not overlap with substrate 454. At the connection portion 204, wiring 465 is electrically connected to FPC 472 via a conductive layer 466 and a connecting layer 242. The conductive layer 466 can be obtained by processing the same conductive film as the pixel electrode. This allows the connection portion 204 and FPC 472 to be electrically connected via the connecting layer 242.

[0453] Transistors 202 and 210 each have a conductive layer 221 that functions as a gate, an insulating layer 211 that functions as a gate insulating layer, a semiconductor layer having a channel forming region 231i and a pair of low-resistance regions 231n, a conductive layer 222a connected to one of the pair of low-resistance regions 231n, a conductive layer 222b connected to the other of the pair of low-resistance regions 231n, an insulating layer 225 that functions as a gate insulating layer, a conductive layer 223 that functions as a gate, and an insulating layer 215 covering the conductive layer 223. The insulating layer 211 is located between the conductive layer 221 and the channel forming region 231i. The insulating layer 225 is located between the conductive layer 223 and the channel forming region 231i.

[0454] The conductive layer 222a and the conductive layer 222b are each connected to the low-resistance region 231n via openings provided in the insulating layer 215. Of the conductive layer 222a and the conductive layer 222b, one functions as a source and the other functions as a drain.

[0455] Figure 14A shows an example in which the insulating layer 225 covers the top and sides of the semiconductor layer. The conductive layer 222a and the conductive layer 222b are connected to the low-resistance region 231n through openings provided in the insulating layer 225 and the insulating layer 215, respectively.

[0456] On the other hand, in the transistor 209 shown in Figure 14B, the insulating layer 225 overlaps with the channel formation region 231i of the semiconductor layer 231, but does not overlap with the low-resistance region 231n. For example, the structure shown in Figure 14B can be fabricated by processing the insulating layer 225 using the conductive layer 223 as a mask. In Figure 14B, an insulating layer 215 is provided covering the insulating layer 225 and the conductive layer 223, and the conductive layer 222a and conductive layer 222b are connected to the low-resistance region 231n, respectively, through openings in the insulating layer 215. Furthermore, an insulating layer 218 covering the transistor may also be provided.

[0457] Furthermore, the substrate 452 is provided with a colored layer 415R, a colored layer 415G, and a colored layer 415B between it and the color conversion layer 412. Here, the light-shielding properties can be further enhanced by the superposition of the colored layers 415R, 415G, and 415B in the region overlapping with the light-shielding layer 417. In addition, a planarization film is provided on the colored layers 415R, 415G, and 415B. In Figure 14, the insulating layer 413 and the insulating layer 414 function as the planarization film. Also, if the light-emitting device 430c is blue and the colored layer 415B is blue, a color conversion layer does not necessarily have to be provided between the light-emitting device 430c and the colored layer 415B. In Figure 14A, the color conversion layer that is blue is omitted, but a color conversion layer may be provided in the same way as the color conversion layer 412G provided between the colored layer 415G and the light-emitting device 430b.

[0458] The configuration examples illustrated in this embodiment, and the corresponding drawings, etc., can be appropriately combined with other configuration examples or drawings, etc., at least in part.

[0459] This embodiment can be implemented in appropriate combination with other embodiments described herein, at least in part.

[0460] (Embodiment 5) This embodiment describes an electronic device according to one aspect of the present invention.

[0461] The electronic device of this embodiment has a light-emitting device according to one aspect of the present invention in its display unit. The light-emitting device according to one aspect of the present invention is highly reliable and easily capable of high-definition and high-resolution displays. Therefore, it can be used in the display units of various electronic devices.

[0462] Examples of electronic devices include television sets, desktop or notebook personal computers, computer monitors, digital signage, large game machines such as pachinko machines, and other electronic devices with relatively large screens, as well as digital cameras, digital video cameras, digital photo frames, mobile phones, portable game consoles, personal digital assistants, and audio playback devices.

[0463] In particular, since the light-emitting device according to one aspect of the present invention can increase resolution, it can be suitably used in electronic devices having a relatively small display area. Examples of such electronic devices include wristwatch-type and bracelet-type information terminals (wearable devices), as well as wearable devices that can be attached to the head, such as VR devices such as head-mounted displays, AR devices such as glasses, and MR (Mixed Reality) devices.

[0464] A light-emitting device according to one aspect of the present invention preferably has an extremely high resolution such as HD (1280 x 720 pixels), FHD (1920 x 1080 pixels), WQHD (2560 x 1440 pixels), WQXGA (2560 x 1600 pixels), 4K (3840 x 2160 pixels), or 8K (7680 x 4320 pixels). In particular, a resolution of 4K, 8K, or higher is preferred. Furthermore, the pixel density (resolution) of the light-emitting device according to one aspect of the present invention is preferably 100 ppi or more, preferably 300 ppi or more, more preferably 500 ppi or more, more preferably 1000 ppi or more, more preferably 2000 ppi or more, more preferably 3000 ppi or more, more preferably 5000 ppi or more, and even more preferably 7000 ppi or more. By using a light-emitting device having high resolution and / or high detail, it is possible to further enhance the sense of presence and depth. Furthermore, there are no particular limitations on the aspect ratio of the light-emitting device according to one embodiment of the present invention. For example, the light-emitting device can accommodate various aspect ratios such as 1:1 (square), 4:3, 16:9, and 16:10.

[0465] The electronic device of this embodiment may have sensors (including those with the function of detecting, detecting, or measuring force, displacement, position, velocity, acceleration, angular velocity, rotational speed, distance, light, liquid, magnetism, temperature, chemical substances, sound, time, hardness, electric field, current, voltage, power, radiation, flow rate, humidity, gradient, vibration, odor, or infrared radiation).

[0466] The electronic device of this embodiment can have a variety of functions. For example, it can have a function to display various information (still images, videos, text images, etc.) on the display unit, a touch panel function, a function to display a calendar, date or time, a function to execute various software (programs), a wireless communication function, a function to read programs or data recorded on a recording medium, and so on.

[0467] Figures 15A to 15D illustrate an example of a wearable device that can be worn on the head. These wearable devices have at least one of the following functions: a function to display AR content, a function to display VR content, a function to display SR (Substantial Reality) content, and a function to display MR content. By having an electronic device that has the function to display at least one of the following content types, such as AR, VR, SR, and MR, it is possible to enhance the user's sense of immersion.

[0468] The electronic device 700A shown in Figure 15A and the electronic device 700B shown in Figure 15B each include a pair of display panels 751, a pair of housings 721, a communication unit (not shown), a pair of mounting units 723, a control unit (not shown), an imaging unit (not shown), a pair of optical members 753, a frame 757, and a pair of nose pads 758.

[0469] A light-emitting device according to one embodiment of the present invention can be applied to the display panel 751. Therefore, a highly reliable electronic device can be made.

[0470] Electronic devices 700A and 700B can project an image displayed on the display panel 751 onto the display area 756 of the optical element 753. Because the optical element 753 is translucent, the user can see the image displayed on the display area superimposed on the transmitted image visible through the optical element 753. Therefore, electronic devices 700A and 700B are electronic devices capable of AR display.

[0471] Electronic devices 700A and 700B may be equipped with cameras capable of capturing images of the area in front of them as imaging units. Furthermore, electronic devices 700A and 700B may each be equipped with acceleration sensors such as gyro sensors to detect the orientation of the user's head and display an image corresponding to that orientation in the display area 756.

[0472] The communications unit has a wireless communication device, which can supply, for example, a video signal. Alternatively, instead of the wireless communication device, or in addition to the wireless communication device, it may be equipped with a connector to which a cable for supplying video signals and power potential can be connected.

[0473] Furthermore, electronic devices 700A and 700B are equipped with batteries that can be charged wirelessly, wired, or both.

[0474] The housing 721 may be equipped with a touch sensor module. The touch sensor module has the function of detecting when the outer surface of the housing 721 is touched. The touch sensor module can detect the user's tap or slide operations and perform various processes. For example, a tap operation can be used to pause or resume the video, and a slide operation can be used to fast forward or rewind. Furthermore, by providing a touch sensor module in each of the two housings 721, the range of operations can be expanded.

[0475] Various types of touch sensors can be applied to the touch sensor module. For example, various methods such as capacitive, resistive, infrared, electromagnetic induction, surface acoustic wave, or optical sensors can be used. In particular, it is preferable to apply capacitive or optical sensors to the touch sensor module.

[0476] When using an optical touch sensor, a photoelectric conversion device (also called a photoelectric conversion element) can be used as the light-receiving device. The active layer of the photoelectric conversion device can be made of either an inorganic semiconductor or an organic semiconductor, or both.

[0477] The electronic device 800A shown in Figure 15C and the electronic device 800B shown in Figure 15D each include a pair of display units 820, a housing 821, a communication unit 822, a pair of mounting units 823, a control unit 824, a pair of imaging units 825, and a pair of lenses 832.

[0478] A light-emitting device according to one embodiment of the present invention can be applied to the display unit 820. Therefore, a highly reliable electronic device can be made.

[0479] The display unit 820 is located inside the housing 821 in a position visible through the lens 832. Furthermore, by displaying different images on a pair of display units 820, a three-dimensional display using parallax can be achieved.

[0480] Electronic devices 800A and 800B can each be described as electronic devices for VR. A user wearing either electronic device 800A or electronic device 800B can view the image displayed on the display unit 820 through the lens 832.

[0481] It is preferable that electronic devices 800A and 800B each have a mechanism that allows adjustment of the left and right positions of the lens 832 and the display unit 820 so that they are in the optimal position according to the user's eye position. It is also preferable that they have a mechanism that adjusts the focus by changing the distance between the lens 832 and the display unit 820.

[0482] The attachment portion 823 allows the user to attach the electronic device 800A or 800B to their head. Note that, for example, in Figure 15C, it is illustrated as having a shape similar to the temples (or arms, etc.) of eyeglasses, but it is not limited to this. The attachment portion 823 only needs to be wearable by the user; for example, it may be helmet-shaped or band-shaped.

[0483] The imaging unit 825 has the function of acquiring external information. The data acquired by the imaging unit 825 can be output to the display unit 820. An image sensor can be used in the imaging unit 825. In addition, multiple cameras may be provided to accommodate multiple angles of view, such as telephoto and wide-angle.

[0484] Although an example with an imaging unit 825 is shown here, any distance measuring sensor (hereinafter also referred to as a detection unit) capable of measuring the distance to an object can be provided. In other words, the imaging unit 825 is one form of a detection unit. As the detection unit, for example, an image sensor or a distance image sensor such as LiDAR (Light Detection and Ranging) can be used. By using the image obtained by the camera and the image obtained by the distance image sensor, more information can be acquired, enabling more accurate gesture control.

[0485] The electronic device 800A may have a vibration mechanism that functions as a bone conduction earphone. For example, a configuration having such a vibration mechanism can be applied to one or more of the display unit 820, housing 821, and mounting unit 823. This eliminates the need for separate audio equipment such as headphones, earphones, or speakers, allowing users to enjoy video and audio simply by wearing the electronic device 800A.

[0486] Electronic devices 800A and 800B may each have input terminals. Cables can be connected to the input terminals to supply video signals from video output devices, etc., and power for charging batteries provided in the electronic devices.

[0487] An electronic device according to one aspect of the present invention may have a function for wireless communication with an earphone 750. The earphone 750 has a communication unit (not shown) and has a wireless communication function. The earphone 750 can receive information (e.g., voice data) from the electronic device through its wireless communication function. For example, the electronic device 700A shown in Figure 15A has a function for transmitting information to the earphone 750 through its wireless communication function. Also, for example, the electronic device 800A shown in Figure 15C has a function for transmitting information to the earphone 750 through its wireless communication function.

[0488] Furthermore, the electronic device may have an earphone section. The electronic device 700B shown in Figure 15B has an earphone section 727. For example, the earphone section 727 and the control unit can be connected to each other by a wire. Part of the wiring connecting the earphone section 727 and the control unit may be located inside the housing 721 or the mounting section 723.

[0489] Similarly, the electronic device 800B shown in Figure 15D has an earphone unit 827. For example, the earphone unit 827 and the control unit 824 can be connected to each other by a wire. Part of the wiring connecting the earphone unit 827 and the control unit 824 may be located inside the housing 821 or the mounting unit 823. Also, the earphone unit 827 and the mounting unit 823 may have magnets. This allows the earphone unit 827 to be fixed to the mounting unit 823 by magnetic force, which is preferable as it facilitates storage.

[0490] Furthermore, the electronic device may have an audio output terminal to which earphones or headphones can be connected. The electronic device may also have an audio input terminal and / or an audio input mechanism. For example, a microphone or other sound-collecting device can be used as the audio input mechanism. By having an audio input mechanism, the electronic device may be given the function of a so-called headset.

[0491] Thus, as one embodiment of the present invention, both eyeglass-type (electronic devices 700A and 700B, etc.) and goggle-type (electronic devices 800A and 800B, etc.) are preferred as electronic devices.

[0492] Furthermore, an electronic device according to one aspect of the present invention can transmit information to earphones via wired or wireless means.

[0493] The electronic device 6500 shown in Figure 16A is a portable information terminal that can be used as a smartphone.

[0494] The electronic device 6500 includes a housing 6501, a display unit 6502, a power button 6503, a button 6504, a speaker 6505, a microphone 6506, a camera 6507, and a light source 6508, etc. The display unit 6502 has a touch panel function.

[0495] A light-emitting device according to one embodiment of the present invention can be applied to the display unit 6502. Therefore, a highly reliable electronic device can be made.

[0496] Figure 16B is a schematic cross-sectional view of the housing 6501 including the end on the microphone 6506 side.

[0497] A light-transmitting protective member 6510 is provided on the display side of the housing 6501, and the display panel 6511, optical member 6512, touch sensor panel 6513, printed circuit board 6517, and battery 6518 are arranged in the space enclosed by the housing 6501 and the protective member 6510.

[0498] The protective member 6510 is fixed to the display panel 6511, the optical member 6512, and the touch sensor panel 6513 by an adhesive layer (not shown).

[0499] In the area outside the display unit 6502, a portion of the display panel 6511 is folded back, and the FPC 6515 is connected to this folded portion. IC 6516 is mounted on the FPC 6515. The FPC 6515 is connected to terminals provided on the printed circuit board 6517.

[0500] A light-emitting device according to one embodiment of the present invention can be applied to the display panel 6511. This makes it possible to realize an extremely lightweight electronic device. Furthermore, because the display panel 6511 is extremely thin, it is possible to incorporate a large-capacity battery 6518 while keeping the thickness of the electronic device low. In addition, by folding back a part of the display panel 6511 and placing the connection part with the FPC 6515 on the back of the pixel section, an electronic device with a narrow bezel can be realized.

[0501] Figure 16C shows an example of a television system. The television system 7100 has a display unit 7000 incorporated into a housing 7171. Here, the housing 7171 is shown to be supported by a stand 7173.

[0502] A light-emitting device according to one embodiment of the present invention can be applied to the display unit 7000. Therefore, a highly reliable electronic device can be made.

[0503] The television device 7100 shown in Figure 16C can be operated using the operation switches on the housing 7171 and a separate remote control unit 7151. Alternatively, the display unit 7000 may be equipped with a touch sensor, and the television device 7100 can be operated by touching the display unit 7000 with a finger or the like. The remote control unit 7151 may have a display unit that displays information output from the remote control unit 7151. Channels and volume can be controlled and the image displayed on the display unit 7000 can be controlled using the operation keys or touch panel on the remote control unit 7151.

[0504] The television system 7100 is configured to include a receiver and a modem, etc. The receiver can receive general television broadcasts. Furthermore, by connecting to a wired or wireless communication network via the modem, it is possible to perform one-way (from sender to receiver) or two-way (between sender and receiver, or between receivers, etc.) information communication.

[0505] Figure 16D shows an example of a notebook personal computer. The notebook personal computer 7200 has a casing 7211, a keyboard 7212, a pointing device 7213, and an external connection port 7214, etc. A display unit 7000 is incorporated into the casing 7211.

[0506] A light-emitting device according to one embodiment of the present invention can be applied to the display unit 7000. Therefore, a highly reliable electronic device can be made.

[0507] Figures 16E and 16F show examples of digital signage.

[0508] The digital signage 7300 shown in Figure 16E includes a housing 7301, a display unit 7000, and a speaker 7303, etc. Furthermore, it may include LED lamps, operation keys (including a power switch or operation switch), connection terminals, various sensors, a microphone, etc.

[0509] Figure 16F shows a digital signage 7400 mounted on a cylindrical column 7401. The digital signage 7400 has a display unit 7000 that is provided along the curved surface of the column 7401.

[0510] In Figures 16E and 16F, a light-emitting device according to one embodiment of the present invention can be applied to the display unit 7000. Therefore, a highly reliable electronic device can be made.

[0511] The larger the display area 7000, the more information can be provided at once. Furthermore, a larger display area 7000 is more eye-catching, which can, for example, enhance the effectiveness of advertising.

[0512] Applying a touch panel to the display unit 7000 is preferable because it not only displays images or videos on the display unit 7000, but also allows users to operate it intuitively. Furthermore, when used for purposes such as providing route information or traffic information, intuitive operation can enhance usability.

[0513] Furthermore, as shown in Figures 16E and 16F, it is preferable that the digital signage 7300 or digital signage 7400 can be linked wirelessly with an information terminal 7311 or information terminal 7411 such as a smartphone owned by the user. For example, the advertising information displayed on the display unit 7000 can be displayed on the screen of the information terminal 7311 or information terminal 7411. Also, the display on the display unit 7000 can be switched by operating the information terminal 7311 or information terminal 7411.

[0514] Furthermore, the digital signage 7300 or digital signage 7400 can be used to run games using the screen of the information terminal 7311 or information terminal 7411 as the control device (controller). This allows an unspecified number of users to participate in and enjoy the game simultaneously.

[0515] The electronic device shown in Figures 17A to 17G includes a housing 9000, a display unit 9001, a speaker 9003, operation keys 9005 (including a power switch or operation switch), connection terminals 9006, a sensor 9007 (including a function to detect, detect, or measure force, displacement, position, velocity, acceleration, angular velocity, rotational speed, distance, light, liquid, magnetism, temperature, chemical substances, sound, time, hardness, electric field, current, voltage, power, radiation, flow rate, humidity, gradient, vibration, odor, or infrared radiation), a microphone 9008, etc.

[0516] The electronic devices shown in Figures 17A to 17G have various functions. For example, they may have functions to display various information (still images, videos, text images, etc.) on a display unit, a touch panel function, a function to display a calendar, date or time, a function to control processing by various software (programs), a wireless communication function, a function to read and process programs or data recorded on a recording medium, etc. However, the functions of electronic devices are not limited to these and can have various functions. Electronic devices may have multiple display units. Furthermore, electronic devices may be equipped with a camera, etc., and have functions to capture still images or videos and save them to a recording medium (external or built into the camera), a function to display the captured images on a display unit, etc.

[0517] Details of the electronic equipment shown in Figures 17A to 17G will be explained below.

[0518] Figure 17A is a perspective view showing a personal information terminal 9171. The personal information terminal 9171 can be used, for example, as a smartphone. The personal information terminal 9171 may also be equipped with a speaker 9003, a connection terminal 9006, or a sensor 9007. Furthermore, the personal information terminal 9171 can display text and image information on multiple surfaces. Figure 17A shows an example where three icons 9050 are displayed. Information 9051, indicated by a dashed rectangle, can also be displayed on other surfaces of the display unit 9001. Examples of information 9051 include notifications of incoming emails, SNS messages, phone calls, etc., the title of emails or SNS messages, the sender's name, date and time, time, battery level, signal strength, etc. Alternatively, icons 9050, etc., may be displayed in the position where the information 9051 is displayed.

[0519] Figure 17B is a perspective view showing the personal digital assistant (PDA) 9172. The PDA 9172 has the function of displaying information on three or more sides of the display unit 9001. Here, an example is shown in which information 9052, information 9053, and information 9054 are displayed on different sides. For example, a user can check information 9053, which is displayed in a position that can be observed from above the PDA 9172, while the PDA 9172 is stored in the breast pocket of their clothing. The user can check the display without taking the PDA 9172 out of their pocket and decide, for example, whether or not to answer a call.

[0520] Figure 17C is a perspective view showing the tablet terminal 9173. The tablet terminal 9173 can run various applications, such as mobile phone calls, email, document viewing and creation, music playback, internet communication, and computer games. The tablet terminal 9173 has a display unit 9001, a camera 9002, a microphone 9008, and a speaker 9003 on the front of the housing 9000. The left side of the housing 9000 has operation keys 9005 as buttons for operation, and the bottom has connection terminals 9006.

[0521] Figure 17D is a perspective view showing a wristwatch-type personal information terminal 9200. The personal information terminal 9200 can be used, for example, as a smartwatch (registered trademark). The display unit 9001 has a curved display surface, allowing it to display information along the curved surface. The personal information terminal 9200 can also make hands-free calls by communicating with, for example, a wireless communication headset. Furthermore, the personal information terminal 9200 can transmit data to other information terminals and be charged via a connection terminal 9006. The charging operation may be performed by wireless power supply.

[0522] Figures 17E to 17G are perspective views showing a foldable portable information terminal 9201. Figure 17E shows the portable information terminal 9201 in an unfolded state, Figure 17G shows it in a folded state, and Figure 17F shows a perspective view of the state in between, transitioning from one of Figures 17E or 17G to the other. The portable information terminal 9201 offers excellent portability in its folded state and excellent readability of the display due to its seamless, wide display area in its unfolded state. The display unit 9001 of the portable information terminal 9201 is supported by three housings 9000 connected by hinges 9055. For example, the display unit 9001 can be bent with a radius of curvature of 0.1 mm to 150 mm.

[0523] This embodiment can be appropriately combined with other embodiments or examples. Furthermore, if multiple configuration examples are shown within a single embodiment in this specification, these configuration examples can be appropriately combined.

[0524] In this embodiment, the Pz and GSP_slope of an organic compound film that can be used in a light-emitting device in a display device according to one aspect of the present invention were calculated.

[0525] Specifically, the following can be used as host materials for fluorescent luminescent substances: 7-[4-(10-phenyl-9-antryl)phenyl]-7H-dibenzo[c,g]carbazole (abbreviation: cgDBCzPA), shown in structural formula (400); 2-(10-phenyl-9-antryl)benzo[b]naphtho[2,3-d]furan (abbreviation: Bnf(II)PhA), shown in structural formula (401); 9-[4-(10-phenyl-9-antryl)phenyl]-9H-carbazole (abbreviation: CzPA), shown in structural formula (402); and 1-[10-(phenyl-2,3,4,5,6-d] 5 The Pz and GSP_slope of the membrane of )-9-antryl[b]...

Claims

A display device having a first color conversion layer, a second color conversion layer, a first light-emitting device, and a second light-emitting device, wherein the first color conversion layer is located on the first light-emitting device. The second light-emitting device has the second color conversion layer, A partition wall is provided between the first light-emitting device and the second light-emitting device. The first light-emitting device and the second light-emitting device are A layer of organic compound is provided between a pair of electrodes. The organic compound layer has a first light-emitting layer and a second light-emitting layer. The first light-emitting layer comprises a fluorescent light-emitting material and a first organic compound. The second light-emitting layer comprises a phosphorescent material and a second organic compound. The difference between the maximum peak wavelength in the PL spectrum of the fluorescent material and the maximum peak wavelength in the PL spectrum of the phosphorescent material is 30 nm or less. The GSP_slope of the film made of the first organic compound is 20 mV / nm or more and 100 mV / nm or less. A display device in which the GSP_slope of a film made of the second organic compound is 20 mV / nm or more and 100 mV / nm or less.   In claim 1, A display device in which the difference between the GSP_slope of a film made of the first organic compound and the GSP_slope of a film made of the second organic compound is 10 mV / nm or less.   A display device having a first color conversion layer, a second color conversion layer, a first light-emitting device, and a second light-emitting device, The first light-emitting device has the first color conversion layer, The second light-emitting device has the second color conversion layer, A partition wall is provided between the first light-emitting device and the second light-emitting device. The first light-emitting device and the second light-emitting device are A layer of organic compound is provided between a pair of electrodes. The organic compound layer has a first light-emitting layer and a second light-emitting layer. The first light-emitting layer comprises a fluorescent light-emitting material and a first organic compound. The second light-emitting layer comprises a phosphorescent material and a second organic compound. The difference between the maximum peak wavelength in the PL spectrum of the fluorescent material and the maximum peak wavelength in the PL spectrum of the phosphorescent material is 30 nm or less. A display device in which the difference between the GSP_slope of a film made of the first organic compound and the GSP_slope of a film made of the second organic compound is 10 mV / nm or less.   In any one of claims 1 to 3, The lowest triplet excitation energy level of the fluorescent material is higher than the lowest triplet excitation energy level of the first organic compound. A display device wherein the lowest triplet excitation energy level of the phosphorescent material is lower than the lowest triplet excitation energy level of the second organic compound.   In claim 4, The first organic compound is an organic compound having a polycyclic aromatic hydrocarbon, The second organic compound is an organic compound having a heteroaromatic ring, which is a display device.   In claim 1 or claim 2, The second light-emitting layer has a third organic compound, The GSP_slope of the film made of the third organic compound is 20 mV / nm or more and 100 mV / nm or less. The second organic compound is an organic compound having a π-electron-deficient heteroaromatic ring, The third organic compound is a display device having a π-electron-rich heteroaromatic ring.   In claim 6, A display device in which the second and third organic compounds are a combination that forms an excited complex.   In any one of claims 1 to 3, The pair of electrodes comprises a first electrode formed on a substrate and a second electrode. The first light-emitting layer is located between the first electrode and the second light-emitting layer in a display device.   In any one of claims 1 to 3, The pair of electrodes comprises a first electrode formed on a substrate and a second electrode. The end of the first electrode is covered with an insulator. The first electrode is electrically connected to the transistor, The first light-emitting layer is located between the first electrode and the second light-emitting layer in a display device.   In any one of claims 1 to 3 The first light-emitting layer and the second light-emitting layer are in contact with each other in a display device.   In any one of claims 1 to 3, The aforementioned fluorescent material has a maximum peak in its PL spectrum in the wavelength range of 440 nm to 520 nm. The phosphorescent material is a display device having the maximum peak in the PL spectrum in the wavelength range of 440 nm to 520 nm.