Autogenous laser welding system and method
By using the detection and intelligent control modules of the laser self-fusion welding system to evaluate weld quality in real time, the problem of existing equipment being unable to quickly assess weld quality is solved, thus improving welding efficiency and quality.
Patent Information
- Application Number
- PCT/CN2025/133708
- Authority / Receiving Office
- WO · WO
- Patent Type
- Applications
- Current Assignee / Owner
- Priority Date
- 2025-05-16
- Filing Date
- 2025-11-10
- Publication Date
- 2026-11-19
AI Technical Summary
Existing laser welding equipment cannot quickly assess weld quality, resulting in low work efficiency.
A laser self-fusion welding system is adopted, including a laser welding execution module, a detection module, a database module, and an intelligent control module. The system analyzes the weld information by acquiring interference spectra in real time and compares it with preset thresholds to determine the weld quality.
It enables rapid assessment of weld quality, improves welding efficiency, and allows for timely detection and repair of potential defects, ensuring processing quality.
Smart Images

Figure CN2025133708_19112026_PF_FP_ABST
Abstract
Description
A laser self-fusion welding system and method Technical Field
[0001] This application relates to the field of welding technology, and in particular to a laser autofusion welding system and method. Background Technology
[0002] Laser autofusion welding offers advantages such as high energy density, concentrated heating, minimal thermal damage to materials, a large weld depth-to-width ratio, low residual stress in the weld joint, and high welding precision. In recent years, its application in the aerospace titanium alloy processing field has become increasingly widespread. For example, laser autofusion welding is commonly used in this field to process titanium alloy frame beam structural parts for aircraft.
[0003] Titanium alloy structural components are extremely valuable, requiring very high yield rates. However, titanium alloys themselves are prone to laser reflection, and the plasma generated during welding further reduces laser power, making them susceptible to defects during the welding process. Therefore, post-weld quality assessment is necessary to address potential defects promptly. However, existing laser welding equipment cannot quickly assess weld quality, resulting in low efficiency. Summary of the Invention
[0004] The main purpose of this application is to provide a laser autofusion welding system and method, which aims to solve the problems of existing laser welding equipment being unable to quickly assess weld quality and having low work efficiency.
[0005] To achieve the above objectives, this application provides a laser self-fusion welding system, which includes a laser welding execution module, a detection module, a database module, and an intelligent control module. The laser welding execution module is used to weld the workpiece to be welded. The detection module is connected to the laser welding execution module and is used to acquire interference spectra in real time. The interference spectra include interference spectra of the bottom signal of the molten pool keyhole and interference spectra of the weld morphology. The database module is used to store preset thresholds, including the thickness of the workpiece plate to be welded, the range of weld width after welding, and the range of weld reinforcement after welding. The intelligent control module is electrically connected to the detection module, the database module, and the laser welding execution module. The intelligent control module is used to analyze the interference spectra to obtain weld information and to judge the quality of the weld after welding based on the comparison result of the weld information and the preset thresholds. The weld information includes the depth of the molten pool keyhole obtained by analyzing the interference spectrum of the bottom signal of the molten pool keyhole, and the weld width and weld reinforcement after welding obtained by analyzing the interference spectrum of the weld morphology.
[0006] Optionally, the database module is further used to store welding process information, and the preset threshold further includes the range of weld width and the range of weld step difference before welding; the weld information also includes the weld width and weld step difference before welding obtained by the interference spectrum analysis of the weld morphology; the intelligent control module is further used to match the corresponding welding process information based on the comparison result of the weld width and the weld step difference before welding with the preset threshold and output a first control signal to the laser welding execution module, wherein the first control signal is used to instruct the laser welding execution module to perform welding based on the corresponding welding process information.
[0007] Optionally, the preset threshold also includes the center position of the weld trajectory; the weld information also includes the center position of the weld obtained by analyzing the interference spectrum of the weld morphology; the intelligent control module is further used to determine the trajectory deviation value based on the center position of the weld and the center position of the weld trajectory and output a second control signal to the laser welding execution module, wherein the second control signal is used to instruct the laser welding execution module to realize the welding trajectory offset.
[0008] Optionally, the laser welding execution module includes a laser welding head and an execution mechanism. The laser welding head is connected to the detection module; the execution mechanism is connected to the laser welding head and electrically connected to the intelligent control module; wherein, the execution mechanism is used to drive the laser welding head to perform welding.
[0009] Optionally, the detection module includes a light source, an optical detection module, and an optical measurement module. The optical detection module has a first measurement optical fiber interface, a second measurement optical fiber interface, and a reference optical fiber interface on its outer periphery. The first measurement optical fiber interface is connected to the light source through a measurement optical fiber, and the reference optical fiber interface is connected to the light source through a reference optical fiber. The optical measurement module has a third measurement optical fiber interface on its outer periphery, and the third measurement optical fiber interface is connected to the second measurement optical fiber interface through the measurement optical fiber. The optical measurement module is connected to the laser welding head.
[0010] Optionally, the first measurement optical fiber interface is perpendicular to the second measurement optical fiber interface, and the second measurement optical fiber interface is parallel to the reference optical fiber interface; the optical detection module includes a first cavity, a first dichroic mirror, a grating, a focusing lens, and a camera. The first dichroic mirror is disposed in the first cavity and located in the measurement optical path direction of the first measurement optical fiber interface; in the measurement optical path direction of the second measurement optical fiber interface and the reference optical path direction of the reference optical fiber interface, the first cavity is provided with a grating, a focusing lens, and a camera sequentially moving away from the first dichroic mirror; wherein, both the first measurement optical fiber interface and the second measurement optical fiber interface are located on the side of the first dichroic mirror opposite to the grating.
[0011] Optionally, the optical measurement module includes a second cavity, a second dichroic mirror, and a oscillating galvanometer. The second cavity is connected to the laser welding head, and the third measurement optical fiber interface is located on the side of the second cavity away from the laser welding head. In the measurement optical path direction of the third measurement optical fiber interface, the second cavity is provided with a second dichroic mirror and an oscillating galvanometer sequentially away from the third measurement optical fiber interface. The laser welding head is provided with a channel for the light path reflected by the oscillating galvanometer to intersect with the workpiece to be welded. A plane reflecting mirror is provided on one side of the second dichroic mirror in a first direction, and the first direction is perpendicular to the measurement optical path direction of the third measurement optical fiber interface.
[0012] Furthermore, to achieve the above objectives, this application also provides a laser autofusion welding method applied to the aforementioned laser autofusion welding system. The method is executed by an intelligent control module and includes: real-time acquisition of interference spectra, wherein the interference spectra include interference spectra of the molten pool keyhole bottom signal and interference spectra of the weld morphology; determination of weld information based on the interference spectra, wherein the weld information includes the molten pool keyhole depth obtained by analyzing the molten pool keyhole bottom signal interference spectrum, and the post-weld weld width and post-weld weld reinforcement height obtained by analyzing the weld morphology interference spectrum; acquisition of preset thresholds, wherein the preset thresholds include the thickness of the workpiece plate to be welded, the range of post-weld weld width, and the range of post-weld weld reinforcement height; and judgment of the post-weld weld quality based on the comparison result between the weld information and the preset thresholds.
[0013] Optionally, before determining the weld information based on the interference spectrum, the method further includes: analyzing the interference spectrum of the weld morphology to obtain the pre-weld weld width and pre-weld weld step difference; obtaining the pre-weld weld width range, the pre-weld weld step difference range, and welding process information; comparing the pre-weld weld width with the pre-weld weld width range; comparing the pre-weld weld step difference with the pre-weld weld step difference range; if the pre-weld weld width is within the pre-weld weld width range and the pre-weld weld step difference is within the pre-weld weld step difference range, then matching the corresponding welding process information and outputting a first control signal to the laser welding execution module, wherein the first control signal is used to instruct the laser welding execution module to perform welding based on the corresponding welding process information.
[0014] Optionally, before determining the weld information based on the interference spectrum, the method further includes obtaining the center position of the weld trajectory; determining the center position of the weld based on the interference spectrum of the weld morphology; determining the trajectory deviation value based on the center position of the weld trajectory and the center position of the weld, and outputting a second control signal to the laser welding execution module, wherein the second control signal is used to instruct the laser welding execution module to realize the welding trajectory offset.
[0015] Optionally, determining the weld information based on the interference spectrum includes determining whether the interference spectrum of the bottom signal of the molten pool keyhole is obtained; if the interference spectrum of the bottom signal of the molten pool keyhole is not obtained, the weld has been fully melted after welding, and the depth of the molten pool keyhole is a fixed value and less than the thickness of the workpiece plate to be welded; if the interference spectrum of the bottom signal of the molten pool keyhole is obtained, the depth of the molten pool keyhole is determined based on the interference spectrum of the bottom signal of the molten pool keyhole, and the weld width and weld reinforcement height after welding are determined based on the interference spectrum of the weld morphology.
[0016] Optionally, judging the quality of the post-weld weld based on the comparison result of the weld information and the preset threshold includes judging whether the post-weld weld has penetrated based on the comparison result of the molten pool keyhole depth and the thickness value of the workpiece plate to be welded; judging whether the post-weld weld width is qualified based on the comparison result of the post-weld weld width and the range of post-weld weld width; judging whether the post-weld weld height is qualified based on the comparison result of the weld height and the range of weld height; if the post-weld weld has penetrated, the post-weld weld width is qualified, and the post-weld weld height is qualified, then the quality of the post-weld weld is qualified; if the post-weld weld has not penetrated, or the post-weld weld width is unqualified, or the post-weld weld height is unqualified, then the quality of the post-weld weld is unqualified.
[0017] Optionally, determining whether the weld has penetrated after welding based on the comparison result between the keyhole depth of the molten pool and the thickness of the workpiece plate to be welded includes comparing the keyhole depth of the molten pool with the thickness of the workpiece plate to be welded; if the keyhole depth of the molten pool is greater than or equal to the thickness of the workpiece plate to be welded, then the weld has penetrated after welding; if the keyhole depth of the molten pool is less than the thickness of the workpiece plate to be welded, then the weld has not penetrated.
[0018] Optionally, determining whether the post-weld weld width is qualified based on the comparison result between the post-weld weld width and the post-weld weld width range includes comparing the post-weld weld width with the post-weld weld width range; if the post-weld weld width is within the post-weld weld width range, then the post-weld weld width is qualified; if the post-weld weld width is outside the post-weld weld width range, then the post-weld weld width is unqualified.
[0019] Optionally, determining whether the weld reinforcement height is qualified based on the comparison result between the weld reinforcement height and the weld reinforcement height range includes comparing the weld reinforcement height with the weld reinforcement height range; if the weld reinforcement height is within the weld reinforcement height range, then the weld reinforcement height is qualified; if the weld reinforcement height is outside the weld reinforcement height range, then the weld reinforcement height is unqualified.
[0020] This application proposes a laser self-fusion welding system. During the workpiece welding process by the laser welding execution module, the detection module acquires the interference spectrum of the signal at the bottom of the keyhole of the molten pool and the interference spectrum of the weld morphology in real time. The intelligent control module analyzes the interference spectrum of the signal at the bottom of the keyhole of the molten pool and the interference spectrum of the weld morphology to obtain the depth of the keyhole of the molten pool, the width of the weld after welding, and the height of the weld after welding. The depth of the keyhole of the molten pool, the width of the weld after welding, and the height of the weld after welding are compared with the corresponding preset thresholds stored in the database module. If the weld after welding has been fully fused, the width of the weld after welding is qualified, and the height of the weld after welding is qualified, then the quality of the weld after welding is qualified. If the weld after welding has not been fully fused, or the width of the weld after welding is unqualified, or the height of the weld after welding is unqualified, then the quality of the weld after welding is unqualified. In this way, the quality assessment of the weld after welding can be completed quickly, so that timely repair welding can be performed at the corresponding position, which greatly improves the welding efficiency.
[0021] Attached Figure Description
[0022] Figure 1 is a schematic diagram of the overall structure of a laser autofusion welding system provided in this application.
[0023] Figure 2 is a schematic diagram of the structure of the optical detection module implemented in this application;
[0024] Figure 3 is a schematic diagram of the structure of the optical measurement module implemented in this application;
[0025] Figure 4 is a flowchart of a laser autofusion welding method provided in an embodiment of this application;
[0026] Figure 5 is a flowchart of the process adaptive matching implementation in an embodiment of this application;
[0027] Figure 6 is a flowchart of the pre-welding positioning and weld tracking implementation in an embodiment of this application;
[0028] Figure 7 is a flowchart of the weld penetration determination process according to an embodiment of this application;
[0029] Figure 8 is a flowchart for determining the weld width and weld quality after welding according to an embodiment of this application.
[0030] In the diagram: 11. Light source; 12. Optical detection module; 121. First measurement optical fiber interface; 122. First dichroic mirror; 123. Grating; 124. Focusing lens; 125. Second measurement optical fiber interface; 126. Reference optical fiber interface; 127. First cavity; 128. Camera; 129. First water-cooling connector; 13. Optical measurement module; 131. Plane reflecting mirror; 132. Oscillating galvanometer; 133. Second dichroic mirror; 134. Second cavity; 135. Third measurement optical fiber interface; 136. Second water-cooling connector; 14. Measurement optical fiber; 15. Reference optical fiber; 2. Database module; 3. Intelligent control module; 31. Optical signal cable; 41. Laser welding head; 42. Actuator.
[0031] The realization of the purpose, functional features and advantages of this application will be further explained in conjunction with the embodiments and with reference to the accompanying drawings. Embodiments of the present invention
[0032] The technical solutions of the embodiments of the present invention will be clearly and completely described below with reference to the accompanying drawings. Obviously, the described embodiments are only a part of the embodiments of the present invention, and not all of the embodiments. Based on the embodiments of the present invention, all other embodiments obtained by those of ordinary skill in the art without creative effort are within the scope of protection of the present invention.
[0033] It should be noted that all directional indications (such as up, down, left, right, front, back, etc.) in the embodiments of the present invention are only used to explain the relative positional relationship and movement of each component in a certain specific posture (as shown in the figure). If the specific posture changes, the directional indication will also change accordingly.
[0034] In this invention, unless otherwise explicitly specified and limited, the terms "connection," "fixed," etc., should be interpreted broadly. For example, "fixed" can mean a fixed connection, a detachable connection, or an integral part; it can mean a mechanical connection or an electrical connection; it can mean a direct connection or an indirect connection through an intermediate medium; it can mean the internal communication of two components or the interaction between two components, unless otherwise explicitly limited. Those skilled in the art can understand the specific meaning of the above terms in this invention according to the specific circumstances.
[0035] Furthermore, if the embodiments of this invention involve descriptions such as "first" or "second," these descriptions are for descriptive purposes only and should not be construed as indicating or implying their relative importance or implicitly specifying the number of technical features indicated. Therefore, a feature defined with "first" or "second" may explicitly or implicitly include at least one of those features. Additionally, the meaning of "and / or" throughout the text includes three parallel solutions; for example, "A and / or B" includes solution A, solution B, or a solution where both A and B are satisfied simultaneously. Furthermore, the technical solutions of the various embodiments can be combined with each other, but this must be based on the ability of those skilled in the art to implement them. When the combination of technical solutions is contradictory or impossible to implement, it should be considered that such a combination of technical solutions does not exist and is not within the scope of protection claimed by this invention.
[0036] Referring to Figures 1-3, this application provides a laser self-fusion welding system. The system may include a laser welding execution module, a detection module, a database module 2, and an intelligent control module 3. The laser welding execution module is used to weld the workpiece to be welded. The detection module is connected to the laser welding execution module and is used to acquire interference spectra in real time. The interference spectra may include the interference spectrum of the signal at the bottom of the molten pool keyhole and the interference spectrum of the weld morphology. The database module 2 is used to store preset thresholds, which may include the thickness of the workpiece plate, the range of the weld width after welding, and the range of the weld reinforcement height after welding. The intelligent control module 3 is electrically connected to the detection module, the database module 2, and the laser welding execution module. The intelligent control module 3 is used to analyze the interference spectrum to obtain weld information and judge the quality of the weld after welding based on the comparison result between the weld information and the preset thresholds. The weld information may include the depth of the molten pool keyhole obtained by analyzing the interference spectrum of the signal at the bottom of the molten pool keyhole, and the weld width and weld reinforcement height after welding obtained by analyzing the interference spectrum of the weld morphology.
[0037] This application proposes a laser self-fusion welding system. During the workpiece welding process by the laser welding execution module, the detection module acquires the interference spectrum of the signal at the bottom of the keyhole of the molten pool and the interference spectrum of the weld morphology in real time. The intelligent control module 3 analyzes the interference spectrum of the signal at the bottom of the keyhole of the molten pool and the interference spectrum of the weld morphology to obtain the depth of the keyhole of the molten pool, the width of the weld after welding, and the height of the weld after welding. The depth of the keyhole of the molten pool, the width of the weld after welding, and the height of the weld after welding are compared with the corresponding preset thresholds in the storage and database module 2. If the weld after welding has been fully melted, the width of the weld after welding is qualified, and the height of the weld after welding is qualified, then the quality of the weld after welding is qualified. If the weld after welding has not been fully melted, or the width of the weld after welding is unqualified, or the height of the weld after welding is unqualified, then the quality of the weld after welding is unqualified. In this way, the quality assessment of the weld after welding can be completed quickly, so that timely re-welding can be performed at the corresponding position, which greatly improves the welding efficiency.
[0038] The intelligent control module 3 automatically acquires the interference spectrum detected by the detection module and the preset threshold in the database module 2.
[0039] It should be noted that when the weld has been fully melted after welding, the keyhole of the molten pool may completely penetrate the workpiece. This will prevent the detection module from acquiring the interference spectrum of the signal at the bottom of the keyhole of the molten pool. In this case, the intelligent control module 3 can determine that the weld has been fully melted after welding.
[0040] It should be understood that the intelligent control module 3 includes an industrial computer and a set of intelligent welding software. The intelligent control module 3 is electrically connected to the detection module through an optical signal cable 31. The industrial computer is equipped with a CPU and a GPU. The CPU is used for system feature algorithm calculation, and the GPU is used for parallel calculation of the algorithm to realize high-speed real-time processing of interference signals.
[0041] In an exemplary embodiment, the database module 2 is further used to store welding process information. The preset threshold may also include the range of weld width and the range of weld step before welding. The weld information may also include the weld width and the weld step before welding obtained by analyzing the interference spectrum of the weld morphology. The intelligent control module 3 is further used to match the corresponding welding process information based on the comparison result between the weld width and the weld step before welding and the preset threshold, and output a first control signal to the laser welding execution module. The first control signal is used to instruct the laser welding execution module to perform welding based on the corresponding welding process information.
[0042] Specifically, before welding begins, the detection module acquires the interference spectrum of the weld morphology. Then, the intelligent control module 3 analyzes the interference spectrum to obtain the pre-weld width and pre-weld step difference. Based on the range of the pre-weld width and the range of the pre-weld step difference, the intelligent control module 3 determines whether the pre-weld width and pre-weld step difference are qualified. If both the pre-weld width and pre-weld step difference are qualified, appropriate welding process information is matched and the first control signal is output to the laser welding execution module. If the pre-weld width or pre-weld step difference is unqualified, the module should prompt the reassembly of the workpiece to be welded.
[0043] Specifically, if the weld width before welding is within the range of the weld width before welding, then the weld width before welding is qualified; otherwise, it is unqualified. If the weld step difference before welding is within the range of the weld step difference before welding, then the weld step difference before welding is qualified; otherwise, it is unqualified.
[0044] It should be understood that once the workpiece to be welded is assembled and qualified, the intelligent control module 3 can send the corresponding welding process information to the laser welding execution module based on the pre-weld weld width and pre-weld weld step difference of the workpiece to be welded, so as to instruct the laser welding execution module to perform automatic welding. In this way, for different workpieces to be welded, the pre-weld weld width and pre-weld weld step difference can be automatically measured and the welding process parameters can be automatically matched, reducing the time required for manual measurement and judgment, improving processing efficiency. Furthermore, combined with the above scheme, the welding quality can be automatically judged after welding is completed, which can further improve the welding work efficiency.
[0045] For example, after automatic welding is completed, the welding quality is judged. If the weld reinforcement is not up to standard, the intelligent control module 3 can match the corresponding process information to control the laser welding execution module to perform repair welding to make the weld reinforcement up to standard. In this way, the weld quality can be quickly judged, and repair welding measures can be taken in time for potential defects to ensure the reliability of processing.
[0046] In addition, the database storage module is mainly used to store welding process information such as laser power, welding speed, oscillation mode, and oscillation frequency.
[0047] In an exemplary embodiment, the preset threshold may further include the center position of the weld trajectory; the weld information may further include the center position of the weld obtained by analyzing the interference spectrum of the weld morphology; the intelligent control module 3 is further used to determine the trajectory deviation value based on the center position of the weld and the center position of the weld trajectory and output a second control signal to the laser welding execution module, wherein the second control signal is used to instruct the laser welding execution module to realize the welding trajectory offset.
[0048] Specifically, the intelligent control module 3 compares the center position of the weld with the center position of the weld trajectory to obtain the trajectory deviation value, and converts the trajectory deviation value into an analog signal to output to the laser welding execution module, so as to control the laser welding execution module to realize the trajectory offset, realize the pre-welding positioning and welding tracking functions of conventional welds or long-distance narrow welds, and has strong versatility, which can be adapted to complex parts and fixtures of different shapes.
[0049] Referring to FIG1, in an exemplary embodiment, the laser welding execution module may include a laser welding head 41 and an execution mechanism 42. The laser welding head 41 is connected to the detection module; the execution mechanism 42 is connected to the laser welding head 41 and electrically connected to the intelligent control module 3; wherein, the execution mechanism 42 is used to drive the laser welding head 41 to perform welding.
[0050] Specifically, the laser welding head 41 can be a oscillating galvanometer welding laser head, and the actuator 42 can be a six-axis robot. The laser welding head 41 is connected to the actuator 42 through a mounting flange, so that the actuator 42 can drive the laser welding head 41 to perform welding operations.
[0051] Referring to Figures 1 and 2, in an exemplary embodiment, the detection module may include a light source 11, an optical detection module 12, and an optical measurement module 13. The optical detection module 12 is provided with a first measurement optical fiber interface 121, a second measurement optical fiber interface 125, and a reference optical fiber interface 126 on its outer periphery. The first measurement optical fiber interface 121 is connected to the light source 11 through a measurement optical fiber 14, and the reference optical fiber interface 126 is connected to the light source 11 through a reference optical fiber 15. The optical measurement module 13 is provided with a third measurement optical fiber interface 135 on its outer periphery. The third measurement optical fiber interface 135 is connected to the second measurement optical fiber interface 125 through a measurement optical fiber 14. The optical measurement module 13 is connected to the laser welding head 41.
[0052] It should be noted that the light source 11 can be a laser, and the spectral range of the light source 11 is 600-700nm, with a center wavelength of 650±100nm. The measurement optical fiber 14 and the reference optical fiber 15 are respectively led out from the light source 11 and connected to the optical detection module 12. The optical detection module 12 and the optical measurement module 13 are also connected through the measurement optical fiber 14.
[0053] Referring to Figure 2, in an exemplary embodiment, the first measurement optical fiber interface 121 is perpendicular to the second measurement optical fiber interface 125, and the second measurement optical fiber interface 125 is parallel to the reference optical fiber interface 126. The optical detection module 12 may include a first cavity 127, a first dichroic mirror 122, a grating 123, a focusing lens 124, and a camera 128. The first dichroic mirror 122 is disposed within the first cavity 127 and is located in the measurement optical path direction of the first measurement optical fiber interface 121. In the measurement optical path direction of the second measurement optical fiber interface 125 and the reference optical path direction of the reference optical fiber interface 126, the first cavity 127 is provided with a grating 123, a focusing lens 124, and a camera 128 arranged sequentially away from the first dichroic mirror 122. The first measurement optical fiber interface 121 and the second measurement optical fiber interface 125 are both located on the side of the first dichroic mirror 122 away from the grating 123.
[0054] Among them, camera 128 is a linear CCD camera.
[0055] It should be noted that the first dichroic mirror 122 and the focusing mirror 124 are installed using mounting brackets. The mounting brackets have built-in water-cooling channels, and each lens is cooled by circulating cooling water. A first water-cooling connector 129 is located outside the cavity, connecting to a Φ6 water-cooling pipe via a quick-connect fitting. The focal length of the focusing mirror is 150mm. The linear CCD camera has a measurement range of 600-700nm and a sampling frequency ≥250kHz.
[0056] Referring to FIG3, in an exemplary embodiment, the optical measurement module 13 may include a second cavity 134, a second dichroic mirror 133, and a oscillating galvanometer 132. The second cavity 134 is connected to the laser welding head 41, and the third measurement optical fiber interface 135 is located on the side of the second cavity 134 away from the laser welding head 41. In the measurement optical path direction of the third measurement optical fiber interface 135, the second cavity 134 is provided with the second dichroic mirror 133 and the oscillating galvanometer 132 sequentially away from the third measurement optical fiber interface 135. The laser welding head 41 is provided with a channel so that the light path reflected by the oscillating galvanometer 132 intersects with the workpiece to be welded. The second dichroic mirror 133 is provided with a planar reflecting mirror 131 on one side in the first direction, and the first direction is perpendicular to the measurement optical path direction of the third measurement optical fiber interface 135.
[0057] The first measurement optical fiber interface 121, the second measurement optical fiber interface 125, the reference optical fiber interface 126, and the third measurement optical fiber interface 135 mentioned above are all FC interfaces; among them, the second cavity 134 can be connected to the laser welding head 41 by bolts.
[0058] It should be noted that the second dichroic mirror 133, the oscillating galvanometer 132, and the plane reflecting mirror 131 are all installed in the second cavity 134 through mounting brackets. The mounting brackets have built-in water-cooling channels, and each mirror is cooled by circulating cooling water. A second water-cooling connector 136 is provided outside the second cavity 134. The second water-cooling connector 136 is connected to a water-cooling pipe with an outer diameter of Φ6 through a quick-connect fitting.
[0059] Specifically, during system operation, a detection laser with a wavelength of 650nm is first emitted by the laser. This detection laser travels along the measurement optical fiber 14 to the optical detection module 12. After being reflected by the first dichroic mirror 122, it travels back along the measurement optical fiber 14 to the optical measurement module 13. The detection laser, after passing through the second dichroic mirror 133, passes through the oscillating mirror 132 and then through the optical path of the laser welding head 41 to illuminate the surface of the object being welded. After reflection, it returns along the original optical path, passing through the first dichroic mirror 122 to reach the grating 123. The detection laser, after being reflected by the second dichroic mirror 133, illuminates the plane reflecting mirror 131 and is reflected back along the original optical path, passing through the first dichroic mirror 122 to reach the grating 123. The laser emits a reference laser with a similar composition to the detection laser, which reaches the grating 123 via the reference optical fiber 15. The reflected detection laser and the reference laser interfere at the grating 123, spreading out according to wavelength to form an interference pattern. The image is sampled by the camera 128 after the focusing lens 124 to obtain a one-dimensional interference spectrum, which is then transmitted to the intelligent control module 3 in the form of the interference spectrum.
[0060] Before welding begins, the surface of the workpiece to be welded is scanned by a detection laser. The interference spectrum of the weld morphology is obtained through the detection module. After the intelligent control module 3 analyzes the interference spectrum, it obtains the height information of different positions on the workpiece surface. This allows it to obtain the weld width and weld step difference before welding, thereby determining whether the assembly is qualified.
[0061] Before and during welding, the detection laser scans the weld seam in real time. The detection module obtains the interference spectrum of the weld seam morphology. After the intelligent control module 3 analyzes the interference spectrum, it calculates the center position of the weld seam. The center position of the weld seam is compared with the center position of the weld seam trajectory set in the database module 2 to calculate the trajectory deviation value. The deviation value is converted into an analog signal and output to the laser welding execution module, so that the laser welding execution module can realize the trajectory offset. It can realize the pre-weld positioning and welding tracking functions for conventional weld seams or long-distance narrow weld seams. It has strong versatility and can be adapted to complex parts and fixtures of different shapes.
[0062] Existing off-axis tracking systems have a weld recognition accuracy >0.2mm when the distance to the titanium alloy butt weld exceeds 300mm from the workpiece, which does not meet the welding requirements of complex titanium alloy structural parts. To ensure recognition accuracy, the system must be installed at the front end of the welding head, occupying a large installation space and easily interfering with the parts. If interference occurs, the off-axis tracking system must be removed, and welding must be completed through manual teaching, reducing processing efficiency. As shown in Figure 3, the measurement end, i.e., the optical measurement module 13, is installed on the laser welding head 41, allowing the measurement optical path of this system to be coaxial with the welding laser optical path. That is, both the detection laser and the welding laser are ultimately emitted from the channel on the laser welding head 41 to the workpiece to be welded, and the detection laser and the welding laser overlap. In this way, the detection module occupies less space, which can greatly avoid interference between this system and the workpiece or the clamping fixture of the workpiece during the welding process. In addition, with the aforementioned pre-weld positioning and welding tracking functions, this system can achieve a recognition accuracy of 0.1mm at a distance of 300mm-400mm from the workpiece, meeting the welding requirements of complex titanium alloy structural parts.
[0063] During welding, a detection laser scans the keyhole of the weld pool in real time. The detection module obtains the interference spectrum of the signal at the bottom of the keyhole. The intelligent control module 3 analyzes the interference spectrum and calculates the real-time keyhole depth. If no valid depth signal is returned, meaning the detection module has not acquired the interference spectrum of the signal at the bottom of the keyhole, it is determined that the keyhole has completely penetrated the workpiece, and the weld has been fully melted. If a valid depth signal is returned, the depth of the keyhole is compared with the workpiece plate thickness. If the keyhole depth is greater than the workpiece plate thickness, the weld is determined to be fully melted; if the keyhole depth is less than or equal to the workpiece plate thickness, the weld is determined to be incompletely melted, thus achieving weld penetration determination.
[0064] After welding is completed, the weld seam formed by laser scanning is inspected. The interference spectrum of the weld seam morphology is obtained through the detection module. After the intelligent control module 3 analyzes the interference spectrum, the weld seam width and weld seam reinforcement height after welding are obtained. Based on this, it is determined that the weld seam width and weld seam reinforcement height after welding are unqualified.
[0065] Among them, by utilizing the characteristics of titanium alloy laser self-fusion welding, such as easy laser reflection and welding plasma to reduce laser power, and based on conditions such as weld penetration, qualified weld width, and qualified weld reinforcement, the quality of the weld can be quickly determined.
[0066] Referring to Figures 4 to 8, based on the above embodiments, this application also provides a laser autofusion welding method applied to the above-mentioned laser autofusion welding system. The method is executed by the intelligent control module 3, and the method may specifically include the following steps:
[0067] S100. Real-time acquisition of interference spectra, wherein the interference spectra may include interference spectra of signals at the bottom of the keyhole of the molten pool and interference spectra of weld morphology;
[0068] S200. Determine weld information based on interference spectrum, wherein the weld information may include the depth of the molten pool keyhole obtained by interference spectrum analysis of the signal at the bottom of the molten pool keyhole, and the weld width and weld reinforcement obtained by interference spectrum analysis of the weld morphology.
[0069] S300. Obtain a preset threshold, wherein the preset threshold may include the thickness of the workpiece plate to be welded, the range of the weld width after welding, and the range of the weld height after welding.
[0070] S400. Determine the quality of the weld after welding based on the comparison results between the weld information and the preset threshold.
[0071] In step S100, the interference spectrum is obtained by detecting the laser-scanned workpiece in the detection module.
[0072] In step S300, the preset threshold can be set in advance in the database module 2 and then obtained by the intelligent control module 3.
[0073] In step S400, the depth of the keyhole in the molten pool and the thickness of the workpiece plate can be used to quickly determine whether the weld is fully penetrated. The width of the weld after welding and its range can be used to quickly determine whether the width of the weld after welding is acceptable. The height of the weld after welding and its range can be used to quickly determine whether the height of the weld after welding is acceptable. Based on these criteria, the weld quality can be quickly determined, effectively improving welding efficiency.
[0074] Referring to FIG5, in an exemplary embodiment, prior to step S200, the method may further include the following steps:
[0075] S110. Based on the interference spectrum analysis of weld morphology, the weld width and weld step difference before welding are obtained.
[0076] S120. Obtain the pre-weld weld width range, the pre-weld weld step range, and welding process information.
[0077] S130. Compare the weld width before welding with the range of weld width before welding.
[0078] S140. Compare the weld step difference before welding with the range of weld step difference before welding.
[0079] S150. If the weld width before welding is within the range of the weld width before welding and the weld step difference before welding is within the range of the weld step difference before welding, then the corresponding welding process information is matched and a first control signal is output to the laser welding execution module. The first control signal is used to instruct the laser welding execution module to perform welding based on the corresponding welding process information.
[0080] In step S120, the pre-weld weld width range, pre-weld weld step range, and welding process information can all be set in advance in the database module 2 and then obtained by the intelligent control module 3.
[0081] In step S150, if the weld width before welding is within the range of the weld width before welding and the weld step difference before welding is within the range of the weld step difference before welding, the intelligent control module 3 will match the welding process information corresponding to the weld width before welding and the weld step difference before welding, store it in the first control signal and send it to the laser welding execution module to instruct the laser welding execution module to perform welding according to the corresponding welding process information, complete the automatic matching of welding process, and realize automatic welding.
[0082] In addition, if the weld width before welding is not within the range of the weld width before welding or the weld step difference before welding is not within the range of the weld step difference before welding, the assembly of the workpiece to be welded is unqualified. The intelligent control module 3 can provide a prompt for reassembly. The specific prompting method is not limited here. It can issue an audio prompt or add a display screen to directly display relevant information about the assembly failure.
[0083] Referring to FIG6, in an exemplary embodiment, prior to step S200, the method may further include the following steps:
[0084] S160, Obtain the center position of the weld trajectory;
[0085] S170. The center position of the weld is determined based on the interference spectrum analysis of the weld morphology.
[0086] S180. Determine the trajectory deviation value based on the weld trajectory center position and the weld center position, and output a second control signal to the laser welding execution module. The second control signal is used to instruct the laser welding execution module to realize the welding trajectory offset.
[0087] In step S160, the center position of the weld trajectory is also stored in the database module 2 and matches the welding process information set in advance in the database module 2. The intelligent control module 3 obtains the center position of the welding trajectory corresponding to the welding process information.
[0088] In step S180, the actuator 42 receives the first control signal to offset the motion trajectory of the laser welding head 41, ensuring that the center position of the weld seam coincides with the center position of the weld seam trajectory in real time, thereby realizing pre-welding positioning and welding tracking. The actuator 42 is a six-axis robot.
[0089] Referring to FIG7, in an exemplary embodiment, step S200 may specifically include the following steps:
[0090] S210. Determine whether the interference spectrum of the signal at the bottom of the keyhole of the molten pool has been obtained;
[0091] S220. If the interference spectrum of the signal at the bottom of the keyhole of the molten pool is not obtained, then the weld has been melted through the keyhole of the molten pool to a fixed depth that is greater than the thickness of the workpiece plate to be welded.
[0092] S230. If the interference spectrum of the signal at the bottom of the keyhole of the molten pool is obtained, the depth of the keyhole of the molten pool is determined based on the interference spectrum of the signal at the bottom of the keyhole of the molten pool, and the weld width and weld reinforcement after welding are determined based on the interference spectrum of the weld morphology.
[0093] In step S210, during the welding process, when the weld is fully penetrated, the keyhole of the molten pool may completely penetrate the workpiece, so the detection module cannot obtain the signal interference spectrum at the bottom of the keyhole of the molten pool; therefore, it is necessary to determine whether the detection module has obtained the signal interference spectrum at the bottom of the keyhole of the molten pool.
[0094] In step S220, if the interference spectrum of the signal at the bottom of the molten pool keyhole is not obtained, a virtual molten pool keyhole depth can be obtained, and this depth is greater than the thickness of the workpiece plate to be welded.
[0095] In an exemplary embodiment, step S400 may specifically include the following steps:
[0096] S410. Determine whether the weld is fully penetrated after welding based on the comparison result between the keyhole depth of the molten pool and the thickness of the workpiece plate to be welded.
[0097] S420. Determine whether the weld width is qualified based on the comparison results between the weld width after welding and the range of weld width after welding.
[0098] S430. Determine whether the weld reinforcement is qualified after welding based on the comparison results between the weld reinforcement height and the weld reinforcement height range.
[0099] S440. If the weld has been fully penetrated, the weld width is qualified, and the weld reinforcement is qualified, then the quality of the weld is qualified.
[0100] S450. If the weld is not fully penetrated after welding, or the weld width or weld reinforcement is not up to standard after welding, then the quality of the weld is not up to standard.
[0101] In steps S440 and S450, the quality of the weld is qualified only when the weld has been fully penetrated, the weld width is qualified, and the weld reinforcement is qualified. Otherwise, the quality of the weld is unqualified and re-welding is required.
[0102] Referring to FIG7, in an exemplary embodiment, step S410 may specifically include the following steps:
[0103] S411. Compare the keyhole depth of the molten pool with the thickness of the workpiece plate to be welded.
[0104] S412. If the keyhole depth of the molten pool is greater than or equal to the thickness of the workpiece plate to be welded, then the weld has been fully fused after welding.
[0105] S413. If the depth of the keyhole in the molten pool is less than the thickness of the workpiece plate to be welded, the weld is not fully penetrated.
[0106] In step 412, when the interference spectrum of the signal at the bottom of the molten pool keyhole is not obtained, the depth of the molten pool keyhole is recorded as being greater than the thickness of the workpiece plate to be welded, that is, the weld has been fully melted.
[0107] In step S413, if the weld is not fully penetrated, it can be repaired by welding to ensure full penetration.
[0108] Referring to FIG8, in an exemplary embodiment, step S420 may specifically include the following steps:
[0109] S421. Compare the weld width after welding with the range of weld width after welding.
[0110] S422. If the width of the weld after welding is within the range of the weld width after welding, then the width of the weld after welding is qualified.
[0111] S423. If the width of the weld after welding is outside the range of weld width after welding, then the width of the weld after welding is unqualified.
[0112] In step S423, if the weld width is not up to standard after welding, the weld can be repaired to make the weld width within the range of the weld width after welding.
[0113] Referring to FIG8, in an exemplary embodiment, step S430 may specifically include the following steps:
[0114] S431. Compare weld reinforcement height with weld reinforcement height range;
[0115] S432. If the weld reinforcement is within the range of weld reinforcement height, then the weld reinforcement height is qualified.
[0116] S433. If the weld reinforcement is outside the weld reinforcement range, the weld reinforcement is unqualified.
[0117] In step S433, if the weld reinforcement height is not up to standard after welding, the weld can be repaired to ensure that the weld reinforcement height is within the weld width range.
[0118] Among them, the characteristic parameters in Figure 8 refer to the weld width and weld reinforcement height after welding, the range of weld width after welding, and the range of weld reinforcement height after welding; and the weld width after welding corresponds to the range of weld width after welding, and the weld reinforcement height after welding corresponds to the range of weld reinforcement height after welding.
[0119] The above are merely preferred embodiments of this application and do not limit the patent scope of this application. Any equivalent structural or procedural transformations made using the content of this application's specification and drawings, or direct or indirect applications in other related technical fields, are similarly included within the patent protection scope of this application.
Claims
1. A laser self-fusion welding system, characterized by, include: Laser welding execution module, used for welding workpieces; A detection module is connected to the laser welding execution module. The detection module is used to acquire interference spectra in real time, wherein the interference spectra include the interference spectrum of the signal at the bottom of the molten pool keyhole and the interference spectrum of the weld morphology. Database module (2) is used to store preset thresholds, wherein the preset thresholds include the thickness of the workpiece plate to be welded, the range of weld width after welding, and the range of weld height after welding. The intelligent control module (3) is electrically connected to the detection module, the database module (2) and the laser welding execution module. The intelligent control module (3) is used to analyze the interference spectrum to obtain weld information and judge the quality of the weld after welding based on the comparison result of the weld information and the preset threshold. The weld information includes the depth of the molten pool keyhole obtained by analyzing the interference spectrum of the signal at the bottom of the molten pool keyhole, and the width of the weld after welding and the height of the weld after welding obtained by analyzing the interference spectrum of the weld morphology.
2. The laser self-welding system of claim 1, wherein, The database module (2) is also used to store welding process information, and the preset threshold also includes the range of weld width before welding and the range of weld step difference before welding. The weld information also includes the weld width and weld step difference before welding, obtained by analyzing the interference spectrum of the weld morphology. The intelligent control module (3) is also used to match the corresponding welding process information based on the comparison results of the pre-weld weld width, the pre-weld weld step difference and the preset threshold, and output a first control signal to the laser welding execution module, wherein the first control signal is used to instruct the laser welding execution module to perform welding based on the corresponding welding process information.
3. The laser self-welding system of claim 1, wherein, The preset threshold also includes the center position of the weld trajectory; The weld information also includes the weld center position obtained by analyzing the interference spectrum of the weld morphology; The intelligent control module (3) is also used to determine the trajectory deviation value based on the weld center position and the weld trajectory center position and output a second control signal to the laser welding execution module, wherein the second control signal is used to instruct the laser welding execution module to realize the welding trajectory offset.
4. The laser self-welding system of claim 1, wherein, The laser welding execution module includes: The laser welding head (41) is connected to the detection module; The actuator (42) is connected to the laser welding head (41), and the actuator (42) is electrically connected to the intelligent control module (3); The actuator (42) is used to drive the laser welding head (41) to perform welding.
5. The laser self-welding system of claim 4, wherein, The detection module includes: Light source (11); The optical detection module (12) is provided with a first measurement optical fiber interface (121), a second measurement optical fiber interface (125) and a reference optical fiber interface (126) on its outer periphery. The first measurement optical fiber interface (121) is connected to the light source (11) through a measurement optical fiber (14), and the reference optical fiber interface (126) is connected to the light source (11) through a reference optical fiber (15). The optical measurement module (13) has a third measurement optical fiber interface (135) on its outer periphery. The third measurement optical fiber interface (135) is connected to the second measurement optical fiber interface (125) through the measurement optical fiber (14). The optical measurement module (13) is connected to the laser welding head (41).
6. The laser self-welding system of claim 5, wherein, The first measurement optical fiber interface (121) is perpendicular to the second measurement optical fiber interface (125), and the second measurement optical fiber interface (125) is parallel to the reference optical fiber interface (126); the optical detection module (12) includes: First cavity (127); The first dichroic mirror (122) is disposed in the first cavity (127) and located in the measurement optical path direction of the first measurement optical fiber interface (121); In the measurement optical path direction of the second measurement optical fiber interface (125) and the reference optical path direction of the reference optical fiber interface (126), the first cavity (127) is provided with a grating (123), a focusing lens (124) and a camera (128) that are sequentially moved away from the first dichroic mirror (122). The first measurement optical fiber interface (121) and the second measurement optical fiber interface (125) are both located on the side of the first dichroic mirror (122) away from the grating (123).
7. The laser self-welding system of claim 5, wherein, The optical measurement module (13) includes: The second cavity (134) is connected to the laser welding head (41), and the third measurement optical fiber interface (135) is located on the side of the second cavity (134) away from the laser welding head (41); In the direction of the measurement optical path of the third measurement optical fiber interface (135), the second cavity (134) is provided with a second dichroic mirror (133) and a oscillating galvanometer (132) that are sequentially moved away from the third measurement optical fiber interface (135). The laser welding head (41) is provided with a channel so that the optical path reflected by the oscillating galvanometer (132) intersects with the workpiece to be welded. The second dichroic mirror (133) has a planar reflective mirror (131) on one side of the first direction, and the first direction is perpendicular to the measurement optical path direction of the third measurement optical fiber interface (135).
8. A laser self-welding method, characterized by, Applied to the laser autofusion welding system according to any one of claims 1 to 7, the method is executed by the intelligent control module (3), and the method includes: Real-time acquisition of interference spectra, wherein the interference spectra include interference spectra of signals at the bottom of the keyhole of the molten pool and interference spectra of weld morphology; Weld information is determined based on the interference spectrum, wherein the weld information includes the depth of the keyhole of the molten pool obtained by analyzing the interference spectrum of the signal at the bottom of the keyhole of the molten pool, and the weld width and weld reinforcement obtained by analyzing the interference spectrum of the weld morphology. Obtain a preset threshold, wherein the preset threshold includes the thickness of the workpiece plate to be welded, the range of the weld width after welding, and the range of the weld reinforcement height after welding; The quality of the weld after welding is determined based on the comparison between the weld information and the preset threshold.
9. The laser autogenous welding method of claim 8 wherein, Before determining the weld information based on the interference spectrum, the method further includes: Based on the interference spectrum analysis of the weld morphology, the weld width and weld step difference before welding are obtained; Obtain the pre-weld weld width range, pre-weld weld step range, and welding process information; Compare the pre-weld weld width with the pre-weld weld width range; Compare the pre-weld weld step difference with the pre-weld weld step difference range; If the pre-weld width is within the range of the pre-weld width and the pre-weld step is within the range of the pre-weld step, then the corresponding welding process information is matched and a first control signal is output to the laser welding execution module, wherein the first control signal is used to instruct the laser welding execution module to perform welding based on the corresponding welding process information.
10. The laser self-welding method of claim 8, wherein, Before determining the weld information based on the interference spectrum, the method further includes: Obtain the center position of the weld trajectory; The location of the weld center was determined based on the interference spectrum analysis of the weld morphology. Based on the center position of the weld trajectory and the center position of the weld, a trajectory deviation value is determined, and a second control signal is output to the laser welding execution module, wherein the second control signal is used to instruct the laser welding execution module to realize the welding trajectory offset.
11. The laser autogenous welding method of claim 8 wherein, The determination of weld information based on the interference spectrum includes: Determine whether the interference spectrum of the signal at the bottom of the keyhole of the molten pool has been obtained; If the interference spectrum of the signal at the bottom of the keyhole of the molten pool is not obtained, the weld seam after welding has been fully melted, and the depth of the keyhole of the molten pool is a fixed value and less than the thickness of the workpiece plate to be welded. If the interference spectrum of the signal at the bottom of the keyhole of the molten pool is obtained, the depth of the keyhole of the molten pool is determined based on the interference spectrum of the signal at the bottom of the keyhole of the molten pool, and the weld width and weld reinforcement height after welding are determined based on the interference spectrum of the weld morphology.
12. The laser self-welding method of claim 8, wherein, The step of determining the quality of the weld after welding based on the comparison result between the weld information and the preset threshold includes: The weld penetration is determined based on the comparison between the depth of the keyhole in the molten pool and the thickness of the workpiece plate to be welded. The weld width after welding is judged to be qualified based on the comparison result between the weld width after welding and the range of weld width after welding. The weld reinforcement height after welding is judged to be qualified based on the comparison result between the weld reinforcement height and the weld reinforcement height range. If the weld has been fully penetrated, the weld width is acceptable, and the weld reinforcement is acceptable, then the quality of the weld is acceptable. If the weld is not fully penetrated, or the weld width or weld reinforcement is not up to standard, then the weld quality is not up to standard.
13. The laser self-welding method of claim 12, wherein, The determination of whether the weld has penetrated after welding based on the comparison result between the keyhole depth of the molten pool and the thickness of the workpiece plate to be welded includes: Compare the depth of the molten pool keyhole with the thickness of the workpiece plate to be welded; If the depth of the keyhole in the molten pool is greater than or equal to the thickness of the workpiece plate to be welded, then the weld seam has been fully melted after welding. If the depth of the keyhole in the molten pool is less than the thickness of the workpiece plate to be welded, then the weld is not fully penetrated.
14. The laser self-welding method of claim 12, wherein, The step of determining whether the post-weld weld width is qualified based on the comparison result between the post-weld weld width and the post-weld weld width range includes: Compare the weld width after welding with the range of weld width after welding; If the width of the weld after welding is within the range of the width of the weld after welding, then the width of the weld after welding is qualified. If the width of the weld after welding is outside the range of the specified weld width, then the width of the weld after welding is unqualified.
15. The laser self-welding method of claim 12, wherein, The step of determining whether the weld reinforcement is qualified based on the comparison result between the weld reinforcement height and the weld reinforcement height range includes: Compare the weld reinforcement height with the weld reinforcement height range; If the weld reinforcement is within the specified range, then the weld reinforcement is qualified. If the weld reinforcement is outside the specified range, then the weld reinforcement is unqualified.