Chemical mechanical polishing device
By incorporating a temperature control device and a heating source into the chemical mechanical polishing (CMP) apparatus, the problem of temperature instability was solved, enabling precise control of the wafer surface temperature, improving polishing uniformity and efficiency, and making it suitable for high-precision semiconductor manufacturing.
Patent Information
- Application Number
- PCT/CN2026/093826
- Authority / Receiving Office
- WO · WO
- Patent Type
- Applications
- Current Assignee / Owner
- Priority Date
- 2025-05-12
- Filing Date
- 2026-04-29
- Publication Date
- 2026-11-19
AI Technical Summary
Existing chemical mechanical polishing (CMP) equipment suffers from unstable temperature control during the polishing process, leading to temperature deviations on the wafer surface and affecting polishing uniformity and efficiency. This is especially problematic in high-precision semiconductor manufacturing where it is difficult to meet the requirements for precise temperature control.
A temperature control device, including a temperature sensor and a heating source, is installed in the hollow space of the grinding head. Combined with heat pipes and temperature-conducting mesh lines, the controller enables precise regulation of the wafer surface temperature. A heating source is also placed on the grinding table to preheat the grinding slurry, ensuring temperature uniformity.
Stable control of wafer surface temperature was achieved, improving grinding uniformity and efficiency, and ensuring high-precision planarization, especially reducing surface defects and flatness errors during copper planarization.
Smart Images

Figure CN2026093826_19112026_PF_FP_ABST
Abstract
Description
A chemical mechanical grinding apparatus
[0001] This application claims priority to Chinese Patent Application No. 202510607523.0, filed on May 12, 2025, entitled “A Chemimechanical Grinding Apparatus”, the entire contents of which are incorporated herein by reference. Technical Field
[0002] This disclosure relates to the field of wafer processing technology, and in particular to a chemical mechanical polishing apparatus. Background Technology
[0003] In semiconductor manufacturing technology, surface planarization is a crucial technique for high-density photolithography. A flat surface without any unevenness is essential to prevent exposure scattering and achieve precise pattern transfer. As wafer fabrication technology advances and the dimensions of wires and gates shrink, the requirements for the flatness of the wafer surface in photolithography become increasingly stringent, placing ever stricter demands on the planarization process. Chemical mechanical polishing (CMP) is an acceptable planarization method. Also known as chemical mechanical polishing, it's a process that combines chemical reactions with mechanical abrasion. The principle is a processing technique that combines chemical etching and mechanical removal. The specific process is as follows: The wafer to be polished is fixed face-down on a polishing pad and then pressed onto the polishing pad under pressure. After the wafer and pad are in contact, a polishing slurry containing chemical reagents and abrasives is added at a controlled flow rate. The surface material reacts chemically with the reagents in the slurry, forming a removable thin reaction layer. Then, the mechanical abrasive action between the polishing pad and the wafer peels off this reaction layer. Finally, the peeled-off material is carried away by the flowing slurry, exposing a new surface. The new surface reacts again, and the process is repeated until global planarization is achieved. Based on the different objects being ground, grinding is mainly divided into: metal grinding and non-metal grinding, such as silicon grinding (Poly CMP), silicon oxide grinding (Silicon Oxide CMP), silicon carbide grinding (Silicon Carbide CMP), tungsten grinding (W CMP), and copper grinding (Cu CMP). Grinding equipment typically includes: grinding fluid, grinding pad, grinding plate, cleaning brush, and chemical cleaning and protective agents.
[0004] In CMP processes, both chemically-related variables (such as initial reaction conditions and chemical reaction rates) and mechanically-related variables (such as the surface friction coefficient and viscoelasticity of the polishing pad) are highly temperature-dependent. To improve reaction speed and polishing effect, high-temperature polishing is often used, such as increasing the temperature of the polishing zone or using high-temperature polishing slurries. However, a significant difference remains between the actual and set temperatures, making it difficult to precisely control the operating temperature of the CMP apparatus. Furthermore, the polishing slurry undergoes complex chemical reactions with the thin film on the wafer surface during polishing, generating substantial heat. Simultaneously, the abrasive particles in the slurry mechanically polish the wafer surface to remove surface film materials and chemical reaction products, also generating significant heat. As polishing time increases, the surface temperature of the polishing pad gradually rises. These factors all contribute to a gradual increase in polishing temperature, leading to changes in the polishing rate. Unstable polishing rates can easily result in incomplete or excessive wafer polishing. Furthermore, the deviation in grinding rate caused by temperature often varies at different locations on the wafer. This leads to poor in-plane grinding uniformity, increasing the difficulty of precisely controlling the CMP process, narrowing the process window, reducing the repeatability of consecutive grinding operations, and lowering product yield. As semiconductor process nodes continue to shrink (especially below 10nm), higher demands are placed on the precision and uniformity of wafer surface treatment. The requirements for grinding stability and uniformity are becoming increasingly stringent. Particularly during copper planarization, temperature control becomes one of the key factors affecting material removal rate (MRR) and surface quality. Therefore, it is urgent to solve the problem of temperature instability during the grinding process.
[0005] It should be noted that the information disclosed in the background section above is only used to enhance the understanding of the background of this disclosure, and therefore may include information that does not constitute prior art known to those skilled in the art. Summary of the Invention
[0006] To address the shortcomings of existing technologies, this disclosure provides a chemical mechanical polishing (CMP) apparatus that ensures temperature control during processing, improves the flatness and uniformity of the wafer surface, solves the problem of temperature deviation on the wafer surface in existing CMP processes leading to poor uniformity of in-wafer polishing, and improves etching efficiency.
[0007] To achieve the above objectives, the technical solution is as follows: A chemical mechanical grinding apparatus, comprising:
[0008] A rotating shaft that moves along an axis under the action of an external power source;
[0009] A grinding table is disposed at the end of the rotating shaft and fixedly connected to the rotating shaft;
[0010] The grinding pad is in close contact with the grinding table;
[0011] A polishing slurry supply device is used to supply polishing slurry to the surface of a polishing pad;
[0012] The grinding head has a built-in hollow accommodating space, and a wafer retaining ring is set inside the hollow accommodating space to fix the wafer to be ground;
[0013] A force-applying device acts on the grinding head to control the force applied to the grinding head;
[0014] The hollow accommodating space is equipped with a temperature control device to adjust the wafer surface temperature. The chemical mechanical polishing apparatus with the above structure can precisely control the wafer surface temperature and improve polishing uniformity. Specifically, by setting a temperature control device in the hollow accommodating space—specifically, by uniformly setting temperature sensors on the inner wall of the hollow accommodating space or on the inner wall of the hollow accommodating space and the wafer holding ring—combined with a heating source uniformly set on the inner wall of the hollow accommodating space, the local temperature of the wafer surface can be directly adjusted.
[0015] In one embodiment, the grinding table is provided with a heating source for heating the grinding fluid.
[0016] In one embodiment, the grinding head is provided with a grinding fluid temperature measuring device to measure the temperature of the grinding fluid in the vicinity of the grinding head.
[0017] In one embodiment, the grinding fluid temperature measuring device is a temperature sensor.
[0018] In one embodiment, the temperature control device includes a temperature sensor and a heating source, the heating source being uniformly arranged around the wafer holding ring.
[0019] In one embodiment, the heating source is an infrared lamp, and a heat-conducting pipe is wound around the periphery of the wafer holding ring.
[0020] In one embodiment, the heating source is an infrared lamp, and a heat-conducting mesh is wound around the periphery of the wafer holding ring. Using an infrared lamp as the heating source and distributing heat evenly around the entire wafer holding ring via heat pipes or heat-conducting mesh effectively avoids localized overheating, ensures uniform temperature on the wafer surface, and achieves high-precision temperature control.
[0021] In one embodiment, a controller is also included, which is electrically connected to the rotating shaft, the force application device, the grinding table, the grinding fluid supply device, and the temperature control device. This configuration enables a high degree of automation and intelligence in operation, simplifying the operation process and improving the system's response speed and stability.
[0022] In one embodiment, when the device is operating, the wafer surface temperature is 0.5-2°C higher than the polishing slurry temperature. Preferably, the wafer surface temperature is 0.5-1°C higher than the polishing slurry temperature, and more preferably, the wafer surface temperature is 0.5-0.8°C higher than the polishing slurry temperature. Extensive experimentation and innovative analysis have verified that this temperature difference setting optimizes the balance between the chemical reaction rate and the physical removal process, further improving polishing quality and consistency. This temperature difference range is particularly suitable for fine processing with high temperature requirements, such as wafer surface copper planarization. This setting ensures efficient removal of excess copper layers while minimizing surface defects and planarity errors.
[0023] In one embodiment, a chemical mechanical polishing apparatus is also provided for the planarization of copper on a wafer surface. When using this apparatus to planarize copper on a wafer, a relatively stable wafer polishing temperature can be maintained, and the wafer surface polishing consistency is good.
[0024] This CMP apparatus significantly improves the quality and efficiency of wafer surface treatment through a series of innovative designs. It not only solves the common temperature control challenges in traditional CMP equipment but also introduces an intelligent management system to enhance operational flexibility and reliability. Simultaneously, the temperature control device on the wafer holding ring precisely adjusts the wafer surface temperature, crucial for maintaining optimal chemical reaction conditions and reducing surface inhomogeneity caused by temperature fluctuations. The heating source on the polishing table ensures the polishing slurry reaches the ideal temperature before entering the polishing area, contributing to temperature stability throughout the polishing process and optimizing the slurry's chemical activity. A temperature measuring device on the polishing head monitors and provides real-time feedback on the actual operating temperature of the polishing slurry. This instant feedback mechanism allows the system to dynamically adjust the temperature control strategy based on actual conditions, ensuring optimal polishing conditions. Through the coordinated implementation of these various technologies, the temperature stability of the CMP apparatus, especially in the wafer polishing area, is greatly improved. In some embodiments, the anti-fogging layer has a thickness of 1-50 nm and is uniformly distributed on the transparent substrate and mask pattern inside the photomask protection frame.
[0025] It should be understood that the above general description and the following detailed description are exemplary and explanatory only, and are not intended to limit this disclosure. Attached Figure Description
[0026] The accompanying drawings, which are incorporated in and form part of this specification, illustrate embodiments consistent with this disclosure and, together with the description, serve to explain the principles of this disclosure. It is obvious that the drawings described below are merely some embodiments of this disclosure, and those skilled in the art can obtain other drawings based on these drawings without any inventive effort.
[0027] Figure 1 is a schematic diagram of the structure of a chemical mechanical grinding apparatus according to an embodiment of the present disclosure;
[0028] Figure 2 is a schematic diagram of the hollow accommodating space in the grinding head of a chemical mechanical grinding apparatus according to an embodiment of this disclosure.
[0029] Reference numerals: 101. Chemical mechanical polishing apparatus; 1. Polishing table; 2. Controller; 3. Rotating shaft; 4. Heating wire; 5. Polishing pad; 6. Polishing slurry supply device; 7. Temperature sensor; 8. Wafer; 9. Hollow accommodating space; 10. Heating source; 11. Polishing head; 12. Wafer holding ring; 13. Force application device; 15. Heat pipe; 16. Temperature control device; 17. Polishing slurry temperature measuring device. Detailed Implementation
[0030] Exemplary embodiments will now be described more fully with reference to the accompanying drawings. However, these exemplary embodiments can be implemented in many forms and should not be construed as limited to the embodiments set forth herein; rather, they are provided so that this disclosure will be thorough and complete, and will fully convey the concept of the exemplary embodiments to those skilled in the art. The same reference numerals in the drawings denote the same or similar structures, and therefore detailed descriptions of them will be omitted. Furthermore, the drawings are merely illustrative of this disclosure and are not necessarily drawn to scale.
[0031] Although relative terms such as "up" and "down" are used in this specification to describe the relative relationship of one component of an icon to another, these terms are used only for convenience, such as according to the orientation of the examples shown in the accompanying drawings. It is understood that if the device of the icon is flipped upside down, the component described as "up" will become the component described as "down." When a structure is "up" of another structure, it may mean that the structure is integrally formed on the other structure, or that the structure is "directly" mounted on the other structure, or that the structure is "indirectly" mounted on the other structure through another structure.
[0032] The terms “a,” “one,” “the,” “the,” and “at least one” are used to indicate the presence of one or more elements / components / etc.; the terms “including” and “having” are used to indicate an open-ended inclusion and to mean that there may be other elements / components / etc. in addition to the listed elements / components / etc.; the terms “first” and “second” are used only as markers and are not a limitation on the number of objects.
[0033] In certain chemical mechanical polishing (CMP) processes, such as tungsten CMP and copper CMP, the polishing slurries are highly sensitive to temperature. Temperature changes alter the rate of chemical reactions, leading to deviations in the polishing rate. Unstable polishing rates can result in incomplete or excessive polishing of the silicon wafer, especially at the contact points between the area to be polished and the polishing slurry, where temperature variations have a more significant impact on the polishing process. While some CMP machines are equipped with polishing end cooling devices, such as cooling water circulating beneath the polishing table or precise temperature control of the polishing slurry, the rotational effect means that simply circulating cooling water or adjusting the slurry temperature, while effective in lowering the temperature, cannot precisely control the temperature of the polishing table, particularly the wafer polishing area.
[0034] To address the above issues, the most common solutions are as follows: the mainstream approach is to maximize the temperature stability within the grinding chamber. For example, Jinghe employs a chemical mechanical polishing (CMP) device that includes a temperature control module. After obtaining the real-time grinding temperature of the grinding pad surface, the temperature control module sends a target value for the first set temperature to the grinding slurry supply module and a target value for the second set temperature to the coolant supply module. The grinding slurry supply module sprays the grinding slurry with the first set temperature onto the grinding pad, and the coolant supply module outputs the coolant with the second set temperature into the coolant circulation channel within the pressure plate. This achieves real-time adjustment of the grinding temperature, which helps improve grinding stability and grinding accuracy. Huahong Grace Semiconductor has improved the temperature control system for the polishing pad. This system includes a temperature sensor and an air compressor temperature control system during chemical mechanical polishing (CMP). The air compressor temperature control system comprises an air compressor and a gas pipeline, which are interconnected to form a closed loop. The gas pipeline is positioned between the polishing pad and an independent platform located below it. By controlling the temperature of the polishing pad, the temperature of the wafer during the CMP process is controlled, maintaining the chemical properties of the polishing slurry, such as selectivity and removal rate, at optimal values. This extends the lifespan of the polishing pad and improves the flatness and stability of the wafer. The system also improves the circulation system of the polishing slurry. Furthermore, it discloses a CMP apparatus including a thermostat with a thermostat fluid, connected to the hollow space within the polishing head via a first and second circulation pipeline; and a thermostat controller electrically connected to the thermostat and used to control the temperature of the thermostat. Temperature control of the grinding head and the wafer to be ground is achieved through the circulation of the constant-temperature liquid in the constant-temperature device. The temperature of the constant-temperature device is adjusted by the constant-temperature controller to precisely control the rate of chemical mechanical polishing (CMP). Yangtze Memory Technologies Co., Ltd. has improved temperature control and setting by proposing a grinding pad temperature control method. Before grinding the sample, the surface temperature of the grinding pad is set to the initial grinding temperature. During the grinding process, the surface temperature of the grinding pad is monitored. If the temperature change exceeds a preset threshold, the surface temperature of the grinding pad is adjusted back to the initial grinding temperature. Setting the surface temperature of the grinding pad to the optimal temperature before grinding the sample facilitates precise control of the grinding rate. During the grinding process, the surface temperature of the grinding pad is monitored in real time. If the temperature change exceeds a preset threshold, a grinding control plate is used to bring the surface temperature of the grinding pad back to the optimal temperature for grinding the sample. Precise control of the grinding pad surface temperature improves the stability and efficiency of CMP.Onsteel Technology has disclosed an electrothermal temperature-controlled chemical mechanical polishing platform, including a temperature controller and a heater. A groove is formed on the upper surface of the polishing disc base, within which a ceramic disc is placed. A spiral groove is formed on the ceramic disc, and a heating wire is placed within the spiral groove. A thermocouple and connecting wire are also placed within the groove, and the thermocouple and connecting wire are connected to two sets of metal rings. The temperature controller uses the thermocouple to measure and control the heater in real time to adjust the surface temperature of the polishing disc, thereby keeping the polishing disc at the desired temperature and achieving precise control of the polishing temperature.
[0035] While some existing solutions have improved the consistency of grinding and polishing through temperature control in the CMP process, and real-time monitoring of wafer surface temperature and polishing slurry temperature is also implemented, overall temperature adjustment and control in the CMP process has not been achieved. This fails to ensure the continuous stability of the reaction temperature during wafer surface grinding in the CMP process. Furthermore, without a control and detection mechanism, the temperature of each area, especially the wafer surface temperature undergoing grinding and polishing, cannot be made uniform during the polishing process. This can easily lead to temperature deviations in the wafer during grinding and polishing, such as heating up during rapid friction and local cooling when in contact with the polishing slurry, resulting in reduced uniformity of surface polishing. Therefore, achieving consistent wafer surface polishing is a major problem that urgently needs to be solved in chemical mechanical polishing equipment.
[0036] Therefore, it is necessary to provide a chemical mechanical polishing (CMP) apparatus to ensure temperature control during the processing, solve the problem of wafer surface temperature deviation in the existing CMP process, and improve the stability and efficiency of the CMP process.
[0037] In one embodiment, please refer to Figure 1, which is a schematic diagram of the chemical mechanical polishing (CMP) apparatus of this disclosure. The CMP apparatus 101 includes: a rotating shaft 3, which moves along its axis under external power; a polishing table 1, disposed at the end of the rotating shaft and fixedly connected to the rotating shaft 3; a heating wire 4 in the polishing table for heating the polishing slurry; a polishing pad 5, which is tightly attached to the polishing table for polishing a wafer; a polishing slurry supply device 6 for supplying polishing slurry to the surface of the polishing pad 5; a polishing head 11, having a built-in hollow accommodating space 9, inside which a wafer holding ring 12 is disposed for fixing the wafer 8 to be polished; a force application device 13, which acts on the polishing head 11 to control the force on the polishing head; and a temperature control device 16 in the hollow accommodating space for adjusting the wafer surface temperature. The polishing head is provided with a polishing slurry temperature measuring device 17 for measuring the polishing slurry temperature in the area near the polishing head. The polishing slurry temperature measuring device can be a temperature sensor, such as an infrared thermometer.
[0038] The rotating shaft 3, as the core of the power transmission of the entire device, moves along its axis under the action of external power, providing the necessary rotational kinetic energy for the entire grinding system. To ensure stability, the rotating shaft is made of a high-rigidity, low-friction coefficient material and equipped with a precision bearing system, ensuring smoothness and reliability under high-speed operation. The external power source can be a high-precision motor, connected to the rotating shaft 3 via a coupling. The motor speed can be precisely controlled by the controller 2, realizing dynamic adjustment of the rotating shaft 3's speed. The grinding table 1 is located at the end of the rotating shaft 3, directly connected to the rotating shaft, and rotates with the rotating shaft. The connection between the rotating shaft and the grinding table is fixed. A heating wire 4 is embedded inside the grinding table to preheat the grinding fluid to the ideal working temperature. The heating wire is selected from either iron-chromium-aluminum heating wire or nickel-chromium heating wire, which can work stably for a long time in high-temperature environments, adapting to the heat changes that may occur during the grinding process; at the same time, it has excellent thermal conductivity and a stable temperature coefficient of resistance, facilitating precise control of heating power, realizing precise adjustment of the grinding fluid temperature, and rapidly converting electrical energy into heat energy and uniformly transferring it to the grinding fluid. The heating wire 4 is spirally and evenly wound inside the grinding table 1, ensuring that the grinding slurry is heated evenly within the grinding table 1 and avoiding localized overheating or undercooling. This provides a stable temperature environment for the grinding slurry as it flows through the grinding pad 5, which is beneficial for maintaining optimal conditions for the chemical reaction. Furthermore, it increases the contact area between the heating wire and the grinding slurry, improving heating efficiency and enabling the grinding slurry to be heated to the required temperature quickly.
[0039] The design of preheating the polishing slurry and polishing space by incorporating heating wires inside the polishing table not only helps to activate the active ingredients in the polishing slurry, but also reduces the impact of thermal stress caused by temperature differences on the wafer.
[0040] A polishing pad 5 is placed in close contact with the polishing table. The polishing pad is the part that directly contacts the wafer to be polished, removing material from the wafer surface through mechanical friction. It determines the final surface finish and smoothness. The polishing pad used in this chemical mechanical polishing apparatus has good wear resistance and moderate hardness, which can effectively remove excess material while avoiding surface damage caused by excessive wear.
[0041] The slurry supply device 6 is responsible for supplying an appropriate amount of slurry to the grinding area to maintain proper lubrication and promote chemical reactions. This device can precisely adjust the flow rate according to actual needs, ensuring optimal working conditions throughout the grinding process. The slurry supply device 6 includes components such as a storage tank, pump body, flow control valve, and temperature regulation module. The controller 2 precisely controls the slurry supply device 6 based on temperature data. When the temperature rises, the slurry flow rate is increased to accelerate heat removal, while the slurry temperature is adjusted to maintain it within a suitable range. When the temperature drops, the flow rate is reduced accordingly, and the temperature is adjusted to maintain the stability of the grinding process. The slurry supply device is equipped with a preheating component, ensuring the slurry is close to the grinding processing temperature before being sprayed out. A dual-temperature zone flow channel, i.e., a main / auxiliary dual-flow channel system, can be implemented within the slurry supply device. The main flow channel uses a 316L stainless steel tube (φ6mm) equipped with a PID temperature controller, while the auxiliary flow channel uses a polytetrafluoroethylene capillary tube (φ1mm) for rapid thermal compensation.
[0042] The grinding head 11 is a key component, containing a hollow accommodating space 9 to hold the wafer 8 to be ground and secure it with a wafer retaining ring 12. Furthermore, the grinding head integrates various temperature control devices, such as a temperature sensor 7 and a heating source 10. These devices work together to achieve precise control of the wafer surface temperature. The dimensions of the hollow accommodating space 9 can be precisely matched to the specifications of the wafer 8 to be ground, ensuring that the wafer can be stably placed within it. The wafer retaining ring 12 is located inside the hollow accommodating space 9 to fix the wafer 8 to be ground. The wafer retaining ring 12 is typically made of a material with a certain degree of rigidity and wear resistance, such as stainless steel. Its inner wall is in close contact with the edge of the wafer, fixing the wafer through vacuum adsorption or mechanical clamping to prevent displacement or shaking of the wafer during the grinding process.
[0043] The force application device 13 controls the magnitude of friction during the grinding process by adjusting the pressure applied to the grinding head, thereby indirectly affecting the temperature change of the wafer surface. The force application device 13 can be a pneumatic or hydraulic system, and the pressure applied to the grinding head 11 is precisely controlled by the controller 2. When it is necessary to increase the grinding rate, the pressure can be appropriately increased to improve the friction; when the temperature is too high, the pressure is reduced to reduce the friction, thereby reducing heat generation and ensuring that the grinding process is carried out under suitable pressure conditions to achieve the best processing effect.
[0044] The temperature control device 16 includes a temperature sensor and a heating source. The heating source is uniformly arranged around the wafer holding ring. The temperature control device 16 is installed inside the polishing head to maintain the wafer surface temperature within an ideal range. The polishing slurry temperature measuring device 17 is located near the polishing head and is specifically used to monitor the actual working temperature of the polishing slurry so as to provide timely feedback to the control system for adjustment. Compared with conventional wafer temperature measuring devices, the above-mentioned setup of this disclosure provides more accurate temperature measurement and faster temperature control. The temperature control device 16 may also include components such as a semiconductor cooling chip or a heating film, which, through linkage with the controller 2, achieves precise control of the wafer surface temperature. When it is necessary to increase the wafer surface temperature, the heating function of the temperature control device 16 is activated; when it is necessary to decrease the temperature, the cooling function is activated, thereby maintaining the wafer surface temperature within the set range.
[0045] The heating source 10 can be a heating wire or a heating lamp, such as an infrared lamp. In one embodiment, the heating source 10 is an infrared lamp, which is uniformly arranged on the upper surface of the hollow accommodating space 9 and uniformly distributed around the wafer holding ring 12. Infrared lamps have the characteristics of fast heating speed and high thermal radiation efficiency, which can quickly increase the ambient temperature around the wafer. Furthermore, due to their uniform layout, they can maintain a relatively stable ambient temperature around the wafer, avoiding uneven grinding of the wafer surface due to uneven temperature.
[0046] In one embodiment, referring to Figure 2, the grinding head of the chemical mechanical polishing apparatus 101 of this disclosure may further include a temperature sensor 7 and a heating source 10 disposed within the hollow accommodating space 9 of the grinding head. The temperature sensor is used to measure the wafer surface temperature. The heating source 10 is uniformly disposed on the upper surface of the hollow accommodating space and uniformly disposed around the wafer holding ring, which can maintain a relatively stable ambient temperature around the wafer. The temperature sensor 7 may be disposed on the inner wall of the hollow accommodating space or simultaneously disposed on the inner wall of the hollow accommodating space and the wafer holding ring, so as to achieve accurate measurement of the wafer surface temperature during polishing, and can further regulate the wafer surface temperature by controlling the heating source 10 and the heating wire 4 through the controller 2 based on the information of the temperature sensor 7.
[0047] In one embodiment, a heat-conducting pipe 15 is wound around the periphery of the wafer holding ring. This heat-conducting pipe further enables rapid heat transfer from the wafer surface, achieving a uniform temperature distribution and reducing surface unevenness caused by temperature fluctuations. The heat-conducting pipe, wound around the wafer holding ring 12, is made of a metal tube with excellent thermal conductivity, such as copper, silver, or aluminum. These metal tubes have good thermal conductivity, enabling rapid heat transfer from the wafer surface and achieving a uniform temperature distribution. The diameter and wall thickness of the heat-conducting pipe 15 are rationally designed to ensure good heat conduction while withstanding the pressure during the grinding process. Its winding method involves tightly wrapping around the wafer holding ring 12, forming an efficient heat transfer channel that rapidly dissipates the heat generated during grinding, reducing surface unevenness caused by temperature fluctuations.
[0048] In one embodiment, the wafer retaining ring may be uniformly wound with thermally conductive mesh lines. These mesh lines can be made of thermally conductive metals such as copper, aluminum, or metal alloys, or they can be prepared by coating thermally conductive ceramics such as aluminum nitride (AlN), boron nitride (BN), or silicon carbide (SiC). In one embodiment, the mesh lines are made of copper and have a mesh structure. This mesh structure increases the thermally conductive area, further promoting uniform heat diffusion, making the temperature distribution on the wafer surface more uniform, and improving the stability of the grinding process. The heat pipes and the thermally conductive mesh lines can be simultaneously placed on the wafer retaining ring or close to its periphery for faster heat transfer.
[0049] In one embodiment, the chemical mechanical polishing apparatus 101 further includes a controller 2, which is the core control unit of the entire apparatus. The controller 2 is electrically connected to components such as the rotating shaft 3, the force application device 13, the polishing table 1, the polishing slurry supply device 6, and the temperature control device 16. It receives temperature data from various temperature sensors, processes and analyzes it in the form of electrical signals, and then issues control commands to each execution component to achieve dynamic regulation of the polishing process. For example, it measures the temperature of the wafer surface, the polishing slurry, and other locations, collects data on the corresponding operating parameters of each component, and transmits the data to the controller 2 in the form of electrical signals. Based on the collected temperature data, the controller 2 dynamically adjusts the rotation speed of the rotating shaft 3. When the temperature rises, it appropriately reduces the rotation speed to reduce frictional heat generated during polishing; when the temperature falls, it increases the rotation speed to ensure that polishing efficiency is not affected. Simultaneously, by adjusting the pressure applied to the wafer by the force application device 13, the controller 2 can control the frictional force during polishing. When the temperature is too high, it reduces the pressure to reduce friction, thereby reducing heat generation; when the temperature is too low, it appropriately increases the pressure to ensure the polishing effect. Controller 2 precisely controls the polishing slurry supply device 6, including adjusting the flow rate and temperature of the polishing slurry. When the temperature rises, the flow rate of the polishing slurry is increased to accelerate heat removal, while the temperature of the polishing slurry is adjusted to maintain it within a suitable range; when the temperature drops, the flow rate is reduced accordingly and the temperature is adjusted. Controller 2 operates the temperature control device 16 based on temperature data, maintaining the temperature stability of the polishing head by heating or cooling it, thereby affecting the wafer surface temperature and ensuring that the entire CMP process operates under optimal conditions.
[0050] Taking the copper planarization and polishing of a wafer surface as an example, the working process of this device is explained in detail:
[0051] (I) Preparation Stage
[0052] Place the wafer 8 to be ground into the hollow receiving space 9 inside the grinding head 11 and fix it with the wafer retaining ring 12, ensuring that the surface of the wafer to be ground is in adjacent contact with the grinding pad 5 and that the position is accurate. Install the grinding pad 5 on the grinding table 1 and check the flatness and installation firmness of the grinding pad. Add an appropriate amount of grinding slurry to the storage tank of the grinding slurry supply device 6 and set the initial temperature and flow rate of the grinding slurry. Turn on the controller 2 and initialize the working parameters of each component, such as the initial rotation speed of the shaft 3, the initial pressure of the force application device 13, and the initial power of the heating wire 4 and the heating source 10.
[0053] (II) Grinding Stage
[0054] An external power source drives the rotating shaft 3 to rotate, causing the grinding table 1 and the grinding pad 5 to rotate together.
[0055] The slurry supply device 6 begins supplying slurry to the surface of the polishing pad 5, and the force application device 13 applies a set initial pressure to the polishing head 11, generating friction between the wafer and the polishing pad 5, thus initiating the polishing process. The temperature sensor 7 measures the wafer surface temperature in real time, and the slurry temperature measuring device 17 measures the slurry temperature in the area near the polishing head, transmitting the temperature data to the controller 2 in the form of an electrical signal.
[0056] Based on the collected temperature data, controller 2 dynamically adjusts the rotational speed of the spindle 3, the pressure of the force application device 13, the flow rate and temperature of the polishing slurry, the power of the heating wire 4 and the heating source 10, and the temperature control device 16 according to a preset control strategy and algorithm. For example, when the wafer surface temperature is detected to be lower than the polishing slurry temperature, controller 2 increases the power of the heating source 10 and appropriately increases the spindle speed and the applied pressure to increase frictional heat, gradually raising the wafer surface temperature to 1°C higher than the polishing slurry temperature and maintaining it stable. During the polishing process, the heat pipe 15 and the heat-conducting mesh continuously and evenly transfer heat from the wafer surface, ensuring a uniform temperature distribution on the wafer surface.
[0057] (III) Monitoring and Adjustment Phase
[0058] The controller 2 monitors the working status and temperature data of each component in real time, and displays the current speed, pressure, temperature, flow rate and other parameters through a human-machine interface (such as a display screen), so that operators can keep track of the grinding process in real time.
[0059] Operators can manually adjust the settings according to the actual grinding effect and process requirements, such as modifying the wafer surface temperature setting value and the grinding fluid flow rate. Controller 2 will automatically adjust the working status of each execution component according to the new settings.
[0060] When a temperature fluctuation exceeds the allowable range or an abnormal situation occurs (such as heating wire failure, temperature sensor malfunction, etc.), the controller 2 will issue an alarm and automatically take corresponding protective measures, such as stopping the shaft rotation and turning off the heating source, to ensure the safety of the device and the wafer.
[0061] (iv) Conclusion
[0062] Once the copper planarization grinding on the wafer surface is complete, the controller 2 issues a command to stop the rotation of the spindle 3 and shut off the grinding slurry supply device 6 and the heating source 10.
[0063] The force application device 13 releases the pressure on the grinding head 11, lifts the grinding head 11, and removes the ground wafer 8.
[0064] Clean and maintain the equipment, check the working status of each component, and prepare for the next grinding.
[0065] Measurements of the wafer surface temperature during copper planarization using the chemical mechanical polishing apparatus of this disclosure revealed that the wafer surface temperature remained constant throughout the polishing process, with a temperature difference of no more than 0.3°C. Through the coordinated operation of the various components, the apparatus can maintain the stability of the wafer surface temperature during the copper planarization polishing process, improve the consistency of the material removal rate, and achieve high-precision planarization.
[0066] In summary, the chemical mechanical polishing (CMP) apparatus of this disclosure integrates multiple advanced control and measurement technologies, aiming to improve the precision, uniformity, and efficiency of wafer surface treatment. Temperature control devices located in the hollow accommodating space and on the wafer holding ring can precisely adjust the wafer surface temperature, maintaining optimal conditions for the chemical reaction. A heating source on the polishing table ensures the polishing slurry reaches the ideal temperature before entering the polishing area, helping to maintain temperature stability throughout the polishing process and optimizing the chemical activity of the slurry. A temperature measuring device on the polishing head can monitor and provide real-time feedback on the actual working temperature of the polishing slurry. Combined with the overall control system, this dynamically adjusts the temperature control strategy, ensuring optimal polishing conditions and maintaining the stability of the wafer surface temperature during polishing, improving the consistency of material removal rates, and reducing surface inhomogeneity caused by temperature fluctuations. With the rapid development of the semiconductor industry, the requirements for the precision and uniformity of wafer surface treatment are becoming increasingly stringent. The CMP apparatus of this disclosure integrates multiple advanced technologies, meeting the needs of high-end semiconductor manufacturing and possessing broad application prospects in wafer manufacturing, integrated circuit production, and other industries. In the future, with the continuous advancement of technology, this device can be further integrated with other smart devices and systems to achieve more efficient and precise semiconductor manufacturing processes.
[0067] The foregoing has provided a detailed description of a chemical mechanical grinding apparatus. The above description, in conjunction with specific preferred embodiments, further elaborates on this disclosure and should not be construed as limiting the specific implementation of this disclosure to these descriptions. For those skilled in the art, the architecture of this disclosure can be flexibly varied without departing from its conceptual framework, leading to the development of a series of products. Any simple deductions or substitutions should be considered as falling within the patent protection scope defined by the submitted claims.
[0068] Other embodiments of this disclosure will readily occur to those skilled in the art upon consideration of the specification and practice of the invention disclosed herein. This disclosure is intended to cover any variations, uses, or adaptations of this disclosure that follow the general principles of this disclosure and include common knowledge or customary techniques in the art not disclosed herein. The specification and examples are to be considered exemplary only, and the true scope and spirit of this disclosure are indicated by the appended claims.
Claims
1. A chemical mechanical grinding apparatus (101), comprising: A rotating shaft (3) moves along its axis under the action of an external power source; A grinding table (1) is disposed at the end of the rotating shaft (3) and fixedly connected to the rotating shaft (3); The grinding pad (5) is attached tightly to the grinding table (1); A polishing slurry supply device (6) is used to supply polishing slurry to the surface of the polishing pad (5); The grinding head (11) has a built-in hollow accommodating space (9), and a wafer holding ring (12) is provided inside the hollow accommodating space (9) to fix the wafer (8) to be ground; A force-applying device (13) acts on the grinding head (11) to control the force on the grinding head (11); The hollow accommodating space (9) is characterized by being equipped with a temperature control device (16) for adjusting the surface temperature of the wafer (8).
2. The chemical mechanical polishing apparatus (101) according to claim 1, characterized by The grinding table (1) is equipped with a heating source (10) for heating the grinding fluid.
3. The chemical mechanical polishing apparatus (101) according to claim 1, characterized by The grinding head (11) is equipped with a grinding fluid temperature measuring device (17) to measure the temperature of the grinding fluid in the vicinity of the grinding head.
4. The chemical mechanical polishing apparatus (101) according to claim 3, characterized by The temperature measuring device is a temperature sensor (7).
5. The chemical mechanical polishing apparatus (101) according to claim 1, characterized by The temperature control device (16) includes a temperature sensor (7) and a heating source (10), which is uniformly arranged around the wafer holding ring (12).
6. The chemical mechanical polishing apparatus (101) according to claim 5, characterized by The heating source (10) is an infrared lamp, and a heat-conducting tube (15) is wound around the periphery of the wafer holding ring (12).
7. The chemical mechanical polishing apparatus (101) according to claim 5, wherein The heating source (10) is an infrared lamp, and the wafer holding ring (12) is surrounded by a heat-conducting mesh.
8. The chemical mechanical polishing apparatus (101) according to Claim 1, characterized by It also includes a controller (2), which is electrically connected to the rotating shaft (3), the force application device (13), the grinding table (1), the grinding fluid supply device (6), and the temperature control device (16).
9. The chemical mechanical polishing apparatus (101) according to any one of claims 1 to 8, characterized in that, When the device is in operation, the surface temperature of the wafer (8) is 0.5-2℃ higher than the temperature of the polishing slurry.
10. Use of a chemical mechanical polishing apparatus (101) as claimed in claim 9, characterized in that This device is used for copper planarization on the surface of a wafer (8).