Metal interconnection method and semiconductor device
By using a self-integrated monolayer and a copper-manganese layer to form a silicon-manganese interface layer in semiconductor processes, the problems of contact resistance and electromigration caused by the reduction of barrier layer thickness are solved, achieving low resistance and high reliability of metal interconnects.
Patent Information
- Application Number
- PCT/CN2026/093857
- Authority / Receiving Office
- WO · WO
- Patent Type
- Applications
- Current Assignee / Owner
- Priority Date
- 2025-05-16
- Filing Date
- 2026-04-29
- Publication Date
- 2026-11-19
AI Technical Summary
In the prior art, reducing the thickness of the barrier layer to decrease the contact resistance of the metal interconnect leads to a decrease in the reliability of the barrier layer, which in turn causes serious problems of electromigration.
A self-integrated single-layer cover is used to cover the front-end metal part to avoid the deposition of a barrier layer on it, and a copper-manganese layer is deposited on the via wall to form a silicon-manganese interface layer as a diffusion barrier layer to reduce metal atom diffusion and improve electromigration resistance reliability.
This effectively reduces the contact resistance of metal interconnects, while mitigating electromigration and improving chip reliability and performance.
Smart Images

Figure CN2026093857_19112026_PF_FP_ABST
Abstract
Description
Metal interconnection methods and semiconductor devices Technical Field
[0001] This application belongs to the field of semiconductor process technology, specifically relating to a metal interconnection method and a semiconductor device. Background Technology
[0002] As chip feature sizes continue to shrink, the resistance, capacitance, delay, and electromigration of back-end metal interconnects are among the key issues affecting the performance and reliability of interconnected devices within a chip. Device interconnects within a chip are accomplished using metal interconnect processes. Metal interconnect processes (such as copper interconnects and aluminum interconnects) can employ physical vapor deposition (PVD) or chemical vapor deposition (CVD) processes to sequentially deposit a barrier layer, a wetting layer, and a seed layer within vias in the dielectric layer. Among these, the barrier layer is crucial for filling the vias in the dielectric layer.
[0003] However, the presence of the barrier layer occupies a significant portion of the conductor volume within the via, leading to increased contact resistance in subsequent metal interconnects. Reducing the barrier layer thickness to decrease contact resistance results in via sidewall coverage issues, impacting the reliability of the barrier layer's function. Decreased barrier layer reliability, in turn, leads to severe electromigration. Summary of the Invention
[0004] This application discloses a metal interconnect method and a semiconductor device to solve the problem of decreased barrier layer reliability caused by reducing the contact resistance of subsequent metal interconnects in the metal interconnect process of related technologies by reducing the thickness of the underlying barrier layer.
[0005] To solve the above-mentioned technical problems, this application provides the following technical solution:
[0006] In a first aspect, embodiments of this application disclose a metal interconnection method, the disclosed metal interconnection method comprising:
[0007] A semiconductor substrate is provided, the semiconductor substrate including a first metal portion and a dielectric layer located on the first metal portion, and the dielectric layer having a through hole, the first metal portion being exposed at the bottom of the through hole;
[0008] A self-integrated monolayer covering the first metal portion is deposited in the through-hole;
[0009] A barrier layer is deposited on the wall of the through-hole, and the self-integrating monolayer is used to inhibit the deposition of the barrier layer on the self-integrating monolayer;
[0010] Remove the self-integrated single layer;
[0011] A wetting layer is deposited in the through-hole;
[0012] A copper-manganese layer is formed on the impregnation layer;
[0013] The through hole is filled with a second metal portion.
[0014] In a second aspect, embodiments of this application disclose a semiconductor device, which is fabricated using the metal interconnection method described in the first aspect. The semiconductor device includes a semiconductor substrate, a barrier layer, a wetting layer, a second metal portion, and a copper-manganese layer.
[0015] The semiconductor substrate includes a first metal portion and a dielectric layer located on the first metal portion; a through-hole is provided in the dielectric layer, and the first metal portion is located at the bottom of the through-hole;
[0016] The barrier layer is located on the wall of the through hole, and there is a gap between the barrier layer and the first metal part;
[0017] The wetting layer covers the barrier layer, the first metal portion, and the gap;
[0018] The copper-manganese layer covers the impregnation layer;
[0019] The second metal portion fills the space enclosed by the copper-manganese layer.
[0020] The metal interconnect method disclosed in this application deposits a copper-manganese layer on the wetting layer. This copper-manganese layer not only serves as a seed layer to prepare for the filling of the second metal portion, but also provides good anti-diffusion functionality, thereby mitigating electromigration phenomena occurring on the via walls where the barrier layer does not cover the area. At a preset process temperature, the copper-manganese layer has a higher chemical potential than pure copper with the dielectric layer. Therefore, the diffusion rate of manganese in copper is higher than the natural diffusion rate of copper. Consequently, before a significant reaction occurs with silicon at the interface between copper and the dielectric layer, manganese atoms migrate to the interface earlier and combine with oxygen atoms in the dielectric layer to form stable oxides. Simultaneously, due to the absence of a barrier layer, manganese atoms in the copper-manganese layer, driven by temperature, more easily penetrate the wetting layer region corresponding to the unblocked area on the via wall and combine with oxygen atoms at the interface, thus forming a silicon-manganese interface layer (MnSixOy) at the interface between the copper-manganese layer and the dielectric layer. The silicon-manganese interface layer has an amorphous structure, which is an advantageous diffusion barrier layer structure that can reduce the diffusion of metal atoms in the second metal part, thereby improving the reliability of electromigration resistance. Attached Figure Description
[0021] Figure 1 is a partial schematic diagram of the chip involved in the related technology;
[0022] Figure 2 is a schematic diagram of the structure after depositing a self-integrated monolayer in a through-hole in a related technology;
[0023] Figure 3 is a schematic diagram of the structure after further deposition of a barrier layer based on the structure in Figure 2 in the related technology;
[0024] Figure 4 is a schematic diagram of the structure after removing the self-integrated single layer in Figure 3 in the related technology;
[0025] Figure 5 is a schematic diagram of the structure after the wetting layer is deposited on the basis of Figure 4 in the related technology;
[0026] Figure 6 is a schematic flowchart of the metal interconnection method disclosed in an embodiment of this application;
[0027] Figure 7 is a schematic diagram of the structure after depositing a copper-manganese layer in the through-hole based on Figure 10e in the embodiment of this application;
[0028] Figure 8 is a schematic diagram of the structure of the semiconductor device disclosed in the embodiment of this application after filling the through hole with a second metal portion based on Figure 7;
[0029] Figure 9 is a schematic diagram of the structure of a semiconductor device disclosed in one embodiment of this application;
[0030] Figure 10a is a schematic diagram of the structure after the semiconductor substrate is provided in the embodiment of this application;
[0031] Figure 10b is a schematic diagram of the structure after depositing a self-integrated monolayer in a through-hole according to an embodiment of this application;
[0032] Figure 10c is a schematic diagram of the structure after a barrier layer is further deposited on the basis of the structure in Figure 10b in the embodiment of this application.
[0033] Figure 10d is a schematic diagram of the structure after removing the self-integrated monolayer in Figure 10c in the embodiment of this application;
[0034] Figure 10e is a schematic diagram of the structure after the wetting layer is deposited based on Figure 10d in the embodiment of this application.
[0035] Explanation of reference numerals in the attached figures: 001-Dielectric layer, 002-Back-end metal interconnect, 003-Upper barrier layer, 004-Lower barrier layer, 01-Dielectric layer, 05-Front-end metal interconnect, 06-Gap, 0121-Through hole, 020-Self-integrated monolayer, 030-Barrier layer, 040-Wetting layer, 10-Semiconductor substrate, 11-First metal portion, 12-Dielectric layer, 13-First portion, 14-Second portion, 16-Gap, 121-Through hole, 101-First dielectric sublayer, 102-Etching stop layer, 103-Second dielectric sublayer, 20-Self-integrated monolayer, 30-Barrier layer, 40-Wetting layer, 50-Copper-manganese layer, 60-Second metal portion, 70-Manganese-ruthenium stack, 80-Silicon-manganese interface layer. Detailed Implementation
[0036] To make the objectives, technical solutions, and advantages of this application clearer, the technical solutions of this application will be clearly and completely described below in conjunction with specific embodiments and corresponding drawings. Obviously, the described embodiments are only a part of the embodiments of this application, and not all of them. All other embodiments obtained by those skilled in the art based on the embodiments of this application without creative effort are within the scope of protection of this application.
[0037] The technical solutions disclosed in the various embodiments of this application are described in detail below with reference to the accompanying drawings.
[0038] As shown in Figure 1, this technical solution reduces the contact resistance of the subsequent metal interconnect 002 by decreasing the thickness of the lower barrier layer 004, thereby improving the resistance-capacitance delay phenomenon. With the continuous miniaturization of chip feature sizes, the barrier layer occupies a significant portion of the conductor volume in the via of the dielectric layer 001, thus significantly increasing the contact resistance of the subsequent metal interconnect 002 and exacerbating the resistance-capacitance delay. The barrier layer includes an upper barrier layer 003 and a lower barrier layer 004. The lower barrier layer 004 is located below the upper barrier layer 003 in the via. The contact resistance R of the subsequent metal interconnect 002... c The contact resistance R is formed by connecting the resistance R1 of the downstream metal interconnect 002 and the resistance R2 of the upper barrier layer 003 in parallel, and then connecting this parallel resistance to the resistance R3 of the lower barrier layer 004 in series. Since the resistance R2 of the upper barrier layer 003 is much greater than the resistance R1 of the downstream metal interconnect 002, the contact resistance R of the downstream metal interconnect 002 is... c It can be approximated that: R c = R1 + R3. Therefore, if it is necessary to reduce the contact resistance R of the downstream metal interconnect 002... c This can be achieved by reducing the resistance R3 of the lower blocking layer 004.
[0039] In some embodiments, the metal interconnect process is a copper interconnect process. In this case, the subsequent metal interconnect is essentially a subsequent copper wire.
[0040] To reduce the contact resistance R of the downstream metal interconnect 002 c The relevant technology uses a simple method to reduce the resistance R3 of the lower barrier layer 004 by reducing its thickness. However, reducing the thickness of the lower barrier layer 004 can lead to sidewall coverage problems in the via, affecting the reliability of the barrier layer's function. A decrease in the reliability of the barrier layer can lead to severe electromigration.
[0041] Specifically, since both the upper barrier layer 003 and the lower barrier layer 004 are formed simultaneously during the deposition of the barrier layer, reducing the thickness of the lower barrier layer 004 means that the thickness of the upper barrier layer 003 will also be reduced accordingly. This reduces the blocking ability of the upper barrier layer 003 attached to the hole wall of the via in the dielectric layer 001, ultimately leading to more severe electromigration through the upper barrier layer 003. Obviously, this will result in poor chip performance.
[0042] To mitigate the electromigration phenomenon exacerbated by the reduced thickness of the barrier layer, and to simultaneously reduce the contact resistance of the subsequent metal interconnect 002, referring to Figures 2 to 5, the metal interconnect process involved in this technical solution deposits a self-integrated monolayer 020 on the front-end metal interconnect 05 exposed at the bottom of the via 0121 in the dielectric layer 01. Simultaneously, the self-integrated monolayer 020 covers the front-end metal interconnect 05 exposed at the bottom of the via 0121. The self-integrated monolayer 020 is deposited on the front-end metal interconnect 05 and does not deposit on the via wall of the via 0121. Specifically, the self-integrated monolayer 020 does not bond to the dielectric layer 01 forming the via 0121.
[0043] Then, a barrier layer 030 is deposited on the wall of the via 0121, with the self-integrated monolayer 020 acting as a barrier. Specifically, the self-integrated monolayer 020 prevents the barrier layer 030 from depositing on the front-end metal interconnect 05, thus ensuring that the barrier layer 030 is fully deposited on the wall of the via 0121 without covering the front-end metal interconnect 05. Therefore, this technical solution does not produce the aforementioned lower barrier layer 04. In this case, there is no thickness limitation on the barrier layer 30 deposited on the wall of the via 0121, allowing it to be deposited to a sufficient thickness on the wall of the via 0121. After the barrier layer 030 is deposited, the self-integrated monolayer 020 covering the front-end metal interconnect 05 is removed, exposing the front-end metal interconnect 05 in the via 0121, thus preparing for subsequent processes.
[0044] As can be seen from the above process, the self-integrated monolayer 020 acts as a temporary barrier, preventing the barrier layer 030 from depositing on the front-end metal interconnect 05 during the deposition process, while not affecting the sufficient thickness of the barrier layer 030 deposited on the via wall of the via 0121. The barrier layer 030 can be deposited to a sufficiently thick thickness, equivalent to a sufficiently large thickness of the upper barrier layer 003 in the technical solution shown in Figure 1, thereby mitigating the electromigration phenomenon through the via wall that is exacerbated by the small barrier layer thickness in related technologies. At the same time, the self-integrated monolayer 020 prevents the deposition of the barrier layer 030 on the front-end metal interconnect 05, thus effectively eliminating the lower barrier layer 004 described in the technical solution shown in Figure 1. Specifically, this solution is equivalent to reducing the thickness of the lower barrier layer 004 in the technical solution shown in Figure 1 to zero, which can effectively reduce the contact resistance of the back-end metal interconnect 002. The technical solutions shown in Figures 2 to 5 can not only reduce the contact resistance of the back-end metal interconnect 002, but also eliminate the need to reduce the thickness of the barrier layer 030 (i.e., the upper barrier layer 003 in the technical solution shown in Figure 1) deposited on the wall of the via 0121, thereby avoiding the serious problem of electromigration caused by the decrease in the reliability of the barrier layer.
[0045] However, the inventors of this application discovered during the research and development process that after removing the self-integrated monolayer 020, the portion of the via wall 0121 that was originally covered by the self-integrated monolayer 020 (which is also the portion not covered by the barrier layer 030, hereinafter referred to as the first portion) is exposed, and a gap 06 is formed between the barrier layer 030 and the first metal part 011. As shown in Figure 4, because this first portion is not blocked by the barrier layer 030, it still faces the risk of electromigration after the subsequent deposition of the wetting layer 040, thereby affecting the reliability of the chip.
[0046] Based on this, referring further to Figures 6-8, this application discloses a metal interconnection method, which includes the following steps:
[0047] S101. Provide a semiconductor substrate 10, please refer to Figure 10a.
[0048] As shown in Figure 10a, in this step, the semiconductor substrate 10 includes a first metal portion 11 and a dielectric layer 12, with the dielectric layer 12 located on the first metal portion 11. The dielectric layer 12 has a via 121. Specifically, the via 121 can be formed on the dielectric layer 12 by an etching process. The first metal portion 11 is exposed at the bottom of the via 121.
[0049] In some embodiments, the first metal portion 11 may be made of copper. In other embodiments, the first metal portion 11 may also be made of other metals commonly used in metal interconnect processes (e.g., aluminum). This application does not limit the specific type of the first metal portion 11.
[0050] It should be noted that, in this document, the dielectric layer 12 described in the embodiments of this application can be equivalent to the dielectric layer 01 in the technical solutions shown in Figures 2 to 5. The first metal portion 11 described in the embodiments of this application can be equivalent to the front-end metal interconnect 05 in the technical solutions shown in Figures 2 to 5. Similarly, in the following text, the structures described in the embodiments of this application can all be equivalent to the corresponding structures in the technical solutions shown in Figures 2 to 5, and will not be repeated here.
[0051] In some embodiments, the dielectric layer 12 in the semiconductor substrate 10 may be made of at least silicon oxide.
[0052] In some embodiments, as shown in FIG9, the dielectric layer 12 may include a first dielectric sublayer 101, an etch stop layer 102, and a second dielectric sublayer 103. The etch stop layer 102 and the second dielectric sublayer 103 are sequentially stacked on the first dielectric sublayer 101. A first metal portion 11 is located in the first dielectric sublayer 101. The etch stop layer 102 and the second dielectric sublayer 103 together form a via 121.
[0053] S102. Deposit a self-integrated monolayer 20 covering the first metal part 11 in the through hole 121, please refer to FIG10b.
[0054] The self-integrated monolayer 20 is used to suppress the deposition of the barrier layer 30 mentioned below on the self-integrated monolayer 20.
[0055] The self-integrated monolayer 20 is selectively deposited on the first metal portion 11 at the bottom of the via 121. As shown in FIG10b, after step S102, the hole wall of the via 121 can be divided into a first portion 13 covered by the self-integrated monolayer 20 (i.e., equivalent to the aforementioned first portion) and a second portion 14 not covered by the self-integrated monolayer 20.
[0056] In some embodiments, step S102 may be performed by chemical vapor deposition or impregnation to deposit a self-integrated monolayer 20 in the via 121.
[0057] In some embodiments, the material of the self-assembled monolayer 20 is a SAM (Self-assembled monolayer) material. Specifically, the head groups of the SAM molecules are hydrophilic, making it easier for them to form chemical bonds with the first metal portion 11 and thus cover the first metal portion 11. Simultaneously, the head groups of the SAM molecules are difficult to bond to the surface of the dielectric layer 12. Therefore, SAM molecules can selectively grow on the first metal portion 11 without forming on the surface of the dielectric layer 12. Specifically, SAM molecules are deposited on the first metal portion 11 and not on the pore walls of the vias 121 of the dielectric layer 12.
[0058] Meanwhile, the tail of the SAM molecule is a hydrophobic group, and the van der Waals forces between the tail chains of the SAM molecule can inhibit the adsorption and nucleation of the precursor on the surface of the self-integrated monolayer 20 during the subsequent deposition of the barrier layer 30. Therefore, the barrier layer 30 can be selectively deposited on the pore walls of the via 121 that are not covered by the self-integrated monolayer 20, and will not be deposited on the self-integrated monolayer 20. It should be noted that the selective deposition principle of the self-integrated monolayer 20 in this embodiment is a well-known technology and will not be described further here.
[0059] In some embodiments, the SAM material can be a chain alkane. Specifically, in some embodiments, the SAM material can be octadecyltrichlorosilane, octadecyl mercaptan, benzotriazole, etc., and the embodiments of this application do not limit the specific type of SAM material.
[0060] In some embodiments, the length of the SAM molecule is typically 0.5 nm to 4 nm.
[0061] It should be noted that all numerical ranges in this article include the extreme values.
[0062] In some embodiments, to improve process quality, after providing the semiconductor substrate 10 and before the semiconductor substrate 10 enters the process chamber for self-integrated monolayer 20 deposition (i.e., between steps S101 and S102), the metal interconnect method disclosed in this application may further include at least one of a degassing process and a plasma pre-cleaning process for the semiconductor substrate 10. Therefore, the metal interconnect method disclosed in this application can ensure that the oxide layer and residues covering the first metal portion 11 can be thoroughly removed before the self-integrated monolayer 20 is deposited, which is beneficial for strengthening the bonding strength between metals after metal interconnection and reducing the resistance between metal interconnect lines.
[0063] S103. Deposit a barrier layer 30 on the wall of the through hole 121, as shown in Figure 10c.
[0064] The barrier layer 30 is used to prevent the diffusion of metal elements (e.g., copper) from the subsequent second metal portion 60 into the dielectric layer 12. Due to the effect of the self-integrated monolayer 20 formed in step S102, the barrier layer 30 will not be deposited on the self-integrated monolayer 20, and therefore will not be deposited on the first metal portion 11; the barrier layer 30 will only be deposited on the hole wall of the via 121. As shown in FIG10c, after step S103, the barrier layer 30 is deposited on the second portion 14 of the hole wall of the via 121. At the same time, since the first portion 13 of the hole wall of the via 121 is covered by the self-integrated monolayer 20, the barrier layer 30 will not be deposited on the first portion 13 of the hole wall of the via 121.
[0065] In some embodiments, this step may employ an atomic layer deposition process to deposit a barrier layer 30 on the wall of the via 121.
[0066] In some embodiments, the material of the barrier layer 30 may be tantalum nitride, and its precursor may be penta(dimethylamino)tantalum (PDMAT), tris(diethylamino)tert-butamide tantalum, etc. The embodiments of this application do not limit the specific material of the barrier layer 30.
[0067] S104. Remove the self-integrated single layer 20. Please refer to Figure 10d.
[0068] In some embodiments, step S104 may use hydrogen plasma, thermal annealing, or hydrogen free radicals to break the bond formed between the head group of the SAM molecule and the first metal part 11, thereby causing the SAM molecule to desorb from the surface of the first metal part 11, thereby exposing the first metal part 11 back to the bottom of the through hole 121.
[0069] As shown in Figure 10d, after removing the self-integrated monolayer 20, the first portion 13 on the hole wall of the through hole 121, which was originally covered by the self-integrated monolayer 20, is exposed again, thereby forming a gap 16 between the barrier layer 30 and the first metal part 11. Step S104 occurs after step S103, so the first portion 13, which was originally covered by the self-integrated monolayer 20, will not be covered by the barrier layer 30.
[0070] In some embodiments, as described above, the length of SAM molecules is generally 0.5 nm to 4 nm. Therefore, the height of the first portion 13 (which can also be considered as the width of the gap 06 in the related art) on the wall of the via 121 covered by the self-integrated monolayer 20 is 0.5 nm to 4 nm.
[0071] S105. Deposit the wetting layer 40 in the through hole 121, please refer to Figure 10e.
[0072] In some embodiments, step S105 may deposit a wetting layer 40 on the hole wall of the through hole 121 by means of physical vapor deposition or chemical vapor deposition.
[0073] In some embodiments, the wetting layer 40 may cover the wall of the through hole 121. In other embodiments, the wetting layer 40 may also cover the first metal portion 11.
[0074] It should be noted that the wetting layer 40 will cover the barrier layer 30 and also the first part 13 of the through hole 121 that is not covered by the barrier layer 30 after the removal of the self-integrated monolayer 20.
[0075] In some embodiments, step S105 may form the wetting layer 40 by depositing at least one of ruthenium, cobalt and tantalum.
[0076] In some embodiments, step S105 may form the wetting layer 40 by using Ta, Ta and Co, Ta and Ru, Ta, Co and Ru, or Ta, Ru and Co. Of course, in other embodiments, step S105 may also form the wetting layer 40 by depositing other materials that can serve as the wetting layer 40, and this application embodiment is not limited thereto.
[0077] As described above, the wetting layer 40 covers the hole wall of the through-hole 121. That is, the wetting layer 40 covers the second portion 14 of the through-hole 121 that is covered by the barrier layer 30. Simultaneously, the wetting layer 40 also covers the first portion 13 of the through-hole 121 that was originally covered by the self-integrated monolayer 20 but not by the barrier layer 30. The first portion 13, which was originally covered by the self-integrated monolayer 20 and exposed after the self-integrated monolayer 20 was removed, is at risk of electromigration because it is not covered by the barrier layer 30.
[0078] In some embodiments, between step S104 and step S105, the metal interconnect method disclosed in this application may further include: purging the process chamber to remove byproducts formed during the removal of the self-integrated monolayer 20. Because byproducts can be removed, a better process environment is provided for subsequent processes, avoiding adverse effects of byproducts on process performance.
[0079] S106. A copper-manganese layer 50 is formed on the impregnation layer 40, as shown in Figure 7.
[0080] In step S106, a copper-manganese layer 50 is deposited on the impregnation layer 40 as a seed layer for filling the second metal part 60 in the subsequent step S107.
[0081] In some embodiments, step S106 may employ a vapor deposition process to deposit a copper-manganese layer 50 on the wetting layer 40.
[0082] In some embodiments, the atomic ratio of manganese in the copper-manganese layer 50 may be 0.1%-5%.
[0083] In some embodiments, the thickness of the copper-manganese layer 50 can be 1 nm to 5 nm.
[0084] It should be noted that the embodiments of this application do not limit the atomic ratio of manganese in the copper-manganese layer 50, nor do they limit the thickness of the copper-manganese layer 50.
[0085] It should be noted that, in this article, the atomic ratio of manganese refers to the ratio of the number of manganese atoms in the copper-manganese layer 50 to the total number of metal atoms in the copper-manganese layer 50.
[0086] In step S106, the copper-manganese layer 50 covers the wetting layer 40 in the via 121, and also covers the first portion 13 on the via wall that is not covered by the barrier layer 30. This first portion 13 then acts as a diffusion barrier layer (i.e., it blocks metal diffusion), thus mitigating the electromigration phenomenon caused by the first portion not being shielded by the barrier layer 30. Specifically, at a preset process temperature, the copper-manganese layer 50 has a higher chemical potential with the dielectric layer 12 compared to pure copper. Therefore, the diffusion rate of manganese in copper is higher than the natural diffusion rate of copper. Thus, before a significant reaction occurs between the copper in the copper-manganese layer 50 and the silicon at the interface of the dielectric layer 12, the manganese atoms in the copper-manganese layer 50 migrate to the interface earlier and combine with oxygen atoms in the dielectric layer 12 to form a stable oxide. Meanwhile, since there is no barrier layer 30 covering it, manganese atoms in the copper-manganese layer 50 can more easily pass through the wetted layer 40 region corresponding to the part of the hole wall of the through hole 121 that is not covered by the barrier layer 30 under temperature drive and combine with oxygen atoms at the interface, thereby forming a silicon-manganese interface layer (MnSixOy)80 at the interface between the copper-manganese layer 50 and the dielectric layer 12.
[0087] There are various methods for forming the copper-manganese layer 50 on the wetting layer 40. In some embodiments, forming the copper-manganese layer 50 on the wetting layer 40 may include:
[0088] Step A1: Deposit a copper-manganese layer 50 on the wetting layer 40.
[0089] In some embodiments, step A1 can be performed by depositing the copper-manganese layer 50 using a vapor deposition process.
[0090] In other embodiments, to improve the coverage effect of the copper-manganese layer 50 on the wall of the through-hole 121, the formation of the copper-manganese layer 50 on the wetting layer 40 may further include step A2. Specifically, step A2 may be included after step A1. Wherein:
[0091] Step A2: Perform a copper-manganese reflow process on the copper-manganese layer 50. This step uses a reflow process to reflow the copper-manganese layer 50, thereby enabling the copper-manganese layer 50 to better cover the hole wall of the via 121, and thus better form a diffusion barrier layer (i.e., silicon-manganese interface layer 80) on the part of the hole wall not covered by the barrier layer 30.
[0092] In some embodiments, when performing a copper-manganese reflow process on the copper-manganese layer 50, the reflow process temperature can be 100℃-400℃, and the reflow time can be 10s-300s.
[0093] In some embodiments, a copper-manganese layer 50 may be deposited on the wetting layer 40. In other embodiments, multiple copper-manganese layers 50 may be deposited on the wetting layer 40. It should be noted that the number of copper-manganese layers 50 depends on process requirements and is not limited in the embodiments of this application.
[0094] S107. Fill the through hole 121 with the second metal part 60, please refer to Figure 8.
[0095] In step S107, a second metal portion 60 is filled into the through-hole 121. This second metal portion 60 serves as the downstream metal interconnect 002 described in the technical solution shown in FIG1. The second metal portion 60 fills the through-hole 121, thereby achieving interconnection between the second metal portion 60 and the first metal portion 11.
[0096] The metal interconnect method disclosed in this application deposits a copper-manganese layer 50 on the wetting layer 40. The copper-manganese layer 50 not only serves as a seed layer to prepare for the filling of the second metal portion 60, but also provides good anti-diffusion functionality, thereby mitigating electromigration phenomena occurring on the via wall of the via 121 in areas not covered by the barrier layer 30. At a preset process temperature, the copper-manganese layer 50 has a higher chemical potential than pure copper with the dielectric layer 12. Therefore, the diffusion rate of manganese in copper is higher than the natural diffusion rate of copper. Consequently, before a significant reaction occurs between silicon and copper at the interface of the dielectric layer 12, manganese atoms migrate to the interface earlier and combine with oxygen atoms in the dielectric layer 12 to form stable oxides. Simultaneously, due to the absence of the barrier layer 30, manganese atoms in the copper-manganese layer 50, driven by temperature, more easily penetrate the wetting layer 40 region corresponding to the area on the via wall of the via 121 not covered by the barrier layer 30 and combine with oxygen atoms at the interface, thereby forming a silicon-manganese interface layer 80 at the interface between the copper-manganese layer 50 and the dielectric layer 12. The silicon-manganese interface layer 80 has an amorphous structure, which is an advantageous diffusion barrier layer (i.e., a layer that can block metal diffusion) structure. This structure can reduce the diffusion of metal atoms in the second metal part 60, thereby improving the reliability of electromigration resistance.
[0097] In some embodiments, when the wetting layer 40 is formed using ruthenium, the ruthenium-formed wetting layer 40 has a high resistivity, which can be compensated by stacking a thin manganese-based barrier layer on the ruthenium. Under temperature, some manganese atoms of the copper-manganese layer 50 can migrate to the first portion 13 on the hole wall not covered by the barrier layer 30 to form the silicon-manganese interface layer 80 described above, while others will interact with the ruthenium-formed wetting layer 40 to form a manganese-ruthenium stack 70. Alloying between the manganese-ruthenium stack 70 can shrink the wetting layer 40 (e.g., shrink it by 1 nm), thereby increasing the volume of the second metal portion 60 in the same-sized via 121, thus avoiding the formation of voids in the second metal portion 60, which helps to reduce the resistance of the second metal portion 60.
[0098] In some embodiments, the manganese-ruthenium stack 70 may be formed on the surface of the impregnation layer 40 corresponding to the first portion 13, the second portion 14 and the first metal portion 11 facing the copper-manganese layer 50.
[0099] In the embodiments of this application, there are various ways to fill the through hole 121 with the second metal part 60, and the embodiments of this application do not limit it.
[0100] In some embodiments, step S107 may include the following steps:
[0101] Step B1: Fill the through hole 121 with copper material using an electroplating process.
[0102] In some embodiments, step B1 can be performed in a chemical electroplating copper machine to fill the through hole 121 with copper material.
[0103] Step B2: Anneal the copper material in the through hole 121 to form the second metal part 60.
[0104] In some embodiments, in step B2, the annealing temperature can be 150°C-600°C, and the annealing time can be 1 minute-120 minutes.
[0105] In other embodiments, in order to better fill the second metal portion 60 in the through hole 121, step S107 may include the following steps:
[0106] Step C1: Deposit copper-manganese material in via 121. This step C1 essentially involves further depositing copper-manganese material on top of the copper-manganese layer 50 deposited in S106. The additional copper-manganese material deposited in step C1 is primarily used to fill via 121.
[0107] Step C2: Perform a copper-manganese reflow process on the copper-manganese material so that the copper-manganese material reflows and fills the through hole 121 to form the second metal part 60.
[0108] In step C2, the additional deposited copper-manganese material is gradually refluxed to the bottom of the through-hole 121 through a reflow process, thereby gradually filling the through-hole 121. The filler formed by the reflowed additional copper-manganese material is essentially the second metal part 60. In this embodiment, the material of the second metal part 60 is essentially copper-manganese material.
[0109] In some embodiments, when performing a copper-manganese reflux process on copper-manganese materials, the reflux process temperature can be 100℃-400℃, and the reflux time can be 10s-300s.
[0110] Compared to using electroplating to fill the through hole 121, using a reflow process to fill the through hole 121 results in a better filling effect and is less restricted by the aspect ratio of the through hole 121.
[0111] In some other embodiments, filling the through hole 121 with the second metal portion 60 may include:
[0112] Step D1: Deposit copper material in through hole 121.
[0113] In some embodiments, step D1 may employ a vapor deposition process to deposit copper material in the via 121. Specifically, in some embodiments, step D1 deposits copper material on the copper-manganese layer 50 using a vapor deposition process.
[0114] In some embodiments, a layer of copper material may be deposited on the copper-manganese layer 50. In other embodiments, multiple layers of copper material may also be deposited on the copper-manganese layer 50, the number of copper material layers depending on process requirements (e.g., the via 121 needs to be filled by reflow in a subsequent copper reflow process), and this application embodiment does not impose any limitations.
[0115] Step D2: Perform a copper reflow process on the copper material so that the copper material reflows and fills the through hole 121 to form the second metal part 60.
[0116] In some embodiments, when performing a copper reflow process on copper materials, the reflow process temperature can be 100℃-400℃, and the reflow time can be 10s-300s.
[0117] Based on the metal interconnect process disclosed in the embodiments of this application, this application discloses a semiconductor device fabricated using the metal interconnect method described above. As shown in Figures 8 and 9, the disclosed semiconductor device includes a semiconductor substrate 10, a barrier layer 30, a wetting layer 40, a copper-manganese layer 50, and a second metal portion 60. The semiconductor substrate 10 includes a first metal portion 11 and a dielectric layer 12 located on the first metal portion 11. A through-hole 121 is provided in the dielectric layer 12. The first metal portion 11 is located at the bottom of the through-hole 121.
[0118] The barrier layer 30 is located on the wall of the through hole 121. The portion of the hole wall between the barrier layer 30 and the first metal part 11 is the first portion 13. The first portion 13 is not covered by the barrier layer 30, that is, there is a gap 16 between the barrier layer 30 and the first metal part 11. The portion of the hole wall covered by the barrier layer 30 is the second portion 14.
[0119] The wetting layer 40 covers the barrier layer 30, the first metal portion 11, and the gap 16. Specifically, the wetting layer 40 covering the gap essentially covers the first portion 13 of the hole wall. Due to the rapid migration of manganese atoms, a silicon-manganese interface layer 80 is formed between the first portion 13 and the wetting layer 40. At the preset process temperature, compared to pure copper, the copper-manganese layer 50 has a higher chemical potential with the dielectric layer 12. Therefore, the diffusion rate of manganese in copper is higher than the natural diffusion rate of copper. Thus, before the silicon at the interface between copper and dielectric layer 12 reacts significantly, manganese atoms migrate to the interface earlier and combine with oxygen atoms in dielectric layer 12 to form stable oxides. At the same time, due to the absence of the barrier layer 30, manganese atoms in the copper-manganese layer 50 can more easily pass through the wetting layer 40 region corresponding to the portion of the hole wall of the via 121 not covered by the barrier layer 30 under temperature drive and combine with oxygen atoms at the interface, thereby forming a silicon-manganese interface layer 80 at the interface between the copper-manganese layer 50 and dielectric layer 12. The silicon-manganese interface layer 80 has an amorphous structure, which is an advantageous diffusion barrier layer (i.e., a layer that can block metal diffusion) structure. This structure can reduce the diffusion of metal atoms in the second metal part 60, thereby improving the reliability of electromigration resistance.
[0120] In some embodiments, the dielectric layer 12 is made of at least silicon oxide. At the location where the wall of the via 121 is located in the gap 16 (i.e., the first location 13), a silicon-manganese interface layer 80 is formed at the interface between the dielectric layer 12 and the copper-manganese layer 50.
[0121] The second metal part 60 fills the space enclosed by the copper-manganese layer 50, thus filling the space completely.
[0122] Since the semiconductor devices disclosed in the embodiments of this application can be fabricated using the metal interconnect process disclosed in the embodiments of this application, the corresponding structural parts can be referred to the corresponding description in the metal interconnect process, and will not be repeated here.
[0123] Meanwhile, it should be noted that due to the high-speed migration of manganese atoms in the copper-manganese layer 50, and the relatively low proportion of manganese atoms in the copper-manganese layer 50, the number of manganese atoms in the copper-manganese layer 50 will be even less, or even non-existent, in the semiconductor device formed after the metal interconnect process. Of course, the remaining structure after the manganese atoms migrate from the copper-manganese layer 50 will fill the via 121 together with the second metal part 60.
[0124] In some embodiments, as described above, the wetting layer 40 can be formed by depositing at least one of ruthenium, cobalt, and tantalum. When the wetting layer 40 is formed using ruthenium, the ruthenium-formed wetting layer 40 has a high resistivity, which can be compensated by stacking a thin manganese-based barrier layer on the ruthenium. Under the influence of temperature, some manganese atoms in the copper-manganese layer 50 can migrate to the portion of the hole wall not covered by the barrier layer 30 to form the silicon-manganese interface layer 80 described above, while others will interact with the ruthenium-formed wetting layer 40 to form a manganese-ruthenium stack 70. Alloying between the manganese-ruthenium stack 70 can shrink the wetting layer 40 (e.g., shrink it by 1 nm), thereby increasing the volume of the second metal portion 60 in the via 121 of the same size. Based on this, in some embodiments, the material of the wetting layer 40 is ruthenium, and the surface of the wetting layer 40 facing the copper-manganese layer 50 has a manganese-ruthenium stack 70 formed thereon. The above embodiments of this application focus on describing the differences between the various embodiments. As long as the different features of the various embodiments are not contradictory, they can be combined to form more specific embodiments. For the sake of brevity, they will not be described in detail here.
[0125] The embodiments of this application have been described above with reference to the accompanying drawings. However, this application is not limited to the specific embodiments described above. The specific embodiments described above are merely illustrative and not restrictive. Those skilled in the art can make many other forms under the guidance of this application without departing from the spirit and scope of the claims, and all of these forms are within the protection scope of this application.
Claims
1. A metal interconnection method, wherein, include: A semiconductor substrate (10) is provided, the semiconductor substrate (10) including a first metal portion (11) and a dielectric layer (12) located on the first metal portion (11), and the dielectric layer (12) is provided with a through hole (121), the first metal portion (11) being exposed at the bottom of the through hole (121); A self-integrated monolayer (20) covering the first metal portion (11) is deposited in the through hole (121); A barrier layer (30) is deposited on the wall of the through hole (121), and the self-integrated monolayer (20) is used to inhibit the deposition of the barrier layer (30) on the self-integrated monolayer (20); Remove the self-integrated single layer (20); A wetting layer (40) is deposited in the through hole (121); A copper-manganese layer (50) is formed on the impregnation layer (40); The second metal portion (60) is filled into the through hole (121).
2. The method according to claim 1, wherein, The dielectric layer (12) is made of at least silicon oxide; wherein, the formation of the copper-manganese layer (50) on the wetting layer (40) includes: In the portion of the via (121) where the hole wall was originally covered by the self-integrated monolayer (20), a silicon-manganese interface layer (80) is formed at the interface between the dielectric layer (12) and the copper-manganese layer (50).
3. The method according to claim 1, wherein, The atomic percentage of manganese in the copper-manganese layer (50) is 0.1%-5%; and / or, The thickness of the copper-manganese layer (50) is 1nm-5nm.
4. The method according to any one of claims 1 to 3, wherein, The process of filling the through hole (121) with the second metal portion (60) includes: The through hole (121) is filled with copper material using an electroplating process; The copper material in the through hole (121) is annealed to form the second metal part (60).
5. The method according to claim 4, wherein, When annealing the copper material in the through hole (121), the annealing temperature is between 150℃ and 600℃, and the annealing time is between 1 minute and 120 minutes.
6. The method according to any one of claims 1 to 3, wherein, The process of filling the through hole (121) with the second metal portion (60) includes: Copper-manganese material is deposited in the through hole (121); The copper-manganese material is subjected to a copper-manganese reflux process so that the copper-manganese material is refluxed and filled in the through hole (121) to form the second metal part (60).
7. The method according to claim 6, wherein, When performing a copper-manganese reflux process on the copper-manganese material, the reflux temperature is 100℃-400℃ and the reflux time is 10s-300s.
8. The method according to any one of claims 1 to 3, wherein, The formation of the copper-manganese layer (50) on the impregnation layer (40) includes: The copper-manganese layer (50) is deposited on the impregnation layer (40).
9. The method according to claim 8, wherein, The formation of the copper-manganese layer (50) on the impregnation layer (40) further includes: After depositing the copper-manganese layer (50) on the impregnation layer (40), the copper-manganese layer (50) is subjected to a copper-manganese reflux process.
10. The method according to claim 9, wherein, When performing a copper-manganese reflow process on the copper-manganese layer (50), the reflow process temperature is 100℃-400℃ and the reflow time is 10s-300s.
11. The method according to any one of claims 1 to 3, wherein, The process of filling the through hole (121) with the second metal portion (60) includes: Copper material is deposited in the through hole (121); The copper material is subjected to a copper reflow process so that the copper material is reflowed and filled in the through hole (121) to form the second metal part (60).
12. The method according to claim 11, wherein, When performing a copper reflow process on the copper material, the temperature of the copper reflow process is 100℃-400℃, and the reflow time is 10s-300s.
13. A semiconductor device, wherein, The semiconductor device is fabricated using the metal interconnect method according to any one of claims 1-12, wherein the semiconductor device comprises: A semiconductor substrate (10) includes a first metal portion (11) and a dielectric layer (12) located on the first metal portion (11); a through hole (121) is provided in the dielectric layer (12), and the first metal portion (11) is located at the bottom of the through hole (121); A barrier layer (30) is located on the wall of the through hole (121), and a gap (16) is formed between the barrier layer (30) and the first metal part (11); A wetting layer (40) covers the barrier layer (30), the first metal portion (11), and the gap; A copper-manganese layer (50) covers the impregnation layer (40); The second metal part (60) fills the space enclosed by the copper-manganese layer (50).
14. The semiconductor device according to claim 13, wherein, The wetting layer (40) is made of ruthenium, and a manganese-ruthenium stack (70) is formed on the surface of the wetting layer (40) facing the copper-manganese layer (50).
15. The semiconductor device according to claim 13 or 14, wherein, The dielectric layer (12) is made of at least silicon oxide; wherein, the semiconductor device further includes: A silicon-manganese interface layer (80) is formed at a location corresponding to the hole wall of the through hole (121) and the gap (16), and is located at the interface between the dielectric layer (12) and the copper-manganese layer (50).