Method and system for recovering polysilicon slurry
By treating polycrystalline silicon slag slurry to remove aluminum and titanium, and combining it with cracking, distillation, concentration and hydrolysis processes, the problem of low conversion efficiency of high-boiling-point substances was solved, and efficient recovery of chlorosilanes and efficient utilization of resources were achieved.
Patent Information
- Application Number
- PCT/CN2026/110878
- Authority / Receiving Office
- WO · WO
- Patent Type
- Applications
- Current Assignee / Owner
- Priority Date
- 2025-05-15
- Filing Date
- 2026-07-15
- Publication Date
- 2026-11-19
AI Technical Summary
In the existing polysilicon production process, the high-boiling-point catalytic cracking process has problems such as low conversion efficiency and high energy consumption, making it difficult to efficiently recover high-boiling-point substances from polysilicon slag slurry.
The method for recovering polycrystalline silicon slag slurry includes aluminum removal, titanium removal, cracking reaction, distillation, concentration and hydrolysis. Impurities are removed by aluminum removal evaporation kettle and titanium removal evaporation tower, and cracking reaction is carried out by hydrogen chloride to finally obtain highly efficient chlorosilane recovery.
It achieves efficient removal of impurities from polysilicon slurry, improves resource utilization, achieves a chlorosilane recovery rate of over 98%, and reduces chlorine consumption in polysilicon production.
Smart Images

Figure CN2026110878_19112026_PF_FP_ABST
Abstract
Description
A method and system for recycling polycrystalline silicon slag slurry
[0001] This application claims priority to Chinese Patent Application No. 202510625550.0, filed on May 15, 2025, entitled "A Method and System for Recycling Polycrystalline Silicon Slag Slurry", the entire contents of which are incorporated herein by reference. Technical Field
[0002] This invention relates to a method and system for recovering polycrystalline silicon slag slurry, belonging to the field of chemical separation technology. Background Technology
[0003] With increasing demand, the photovoltaic and integrated circuit industries have experienced rapid development. Polysilicon is a core raw material for both industries, leading to a surge in polysilicon production by various companies.
[0004] Currently, almost all polysilicon manufacturers use the modified Siemens process, which generates a large amount of slurry during polysilicon production. This slurry mainly consists of polychlorosilanes, silicon powder, metal chlorides, silicon tetrachloride, trichlorosilane, and dichlorosilane. After separation to remove silicon powder and metal chlorides, and recovering some silicon tetrachloride, trichlorosilane, and dichlorosilane, the remaining slurry contains polychlorosilanes with boiling points higher than silicon tetrachloride and trichlorosilane, i.e., high-boiling-point substances. This portion of the material needs to be recovered and reused through catalytic cracking.
[0005] Currently, there are two main catalytic cracking processes for high-boiling-point substances. One is to use liquid-phase catalysts to catalytically crack high-boiling-point substances in a reactor. However, this method is a batch reaction, and the gas phase is unevenly distributed in the liquid phase, resulting in low conversion efficiency and high energy consumption. The other is to use solid-phase resin catalysts to catalytically crack high-boiling-point substances in a tower reactor. However, this method has a low single-pass conversion rate.
[0006] Therefore, it is necessary to provide a method that can efficiently recover high-boiling-point substances. Summary of the Invention
[0007] This invention provides a method for recycling polycrystalline silicon slag slurry, which can efficiently recover high-boiling-point substances from polycrystalline silicon slag slurry and improve resource utilization.
[0008] This invention provides a recycling system for polycrystalline silicon slag slurry. This recycling system is used to implement the above-mentioned recycling method. The recycling system has a simple structure and is suitable for widespread application.
[0009] This invention provides a method for recycling polycrystalline silicon slag slurry, comprising:
[0010] Aluminum removal and titanium removal treatments are performed on the high-boiling-point substances produced by slurry processing to obtain intermediate high-boiling-point substances.
[0011] The intermediate high-boiling-point substance is subjected to a cracking reaction with hydrogen chloride to obtain cracking products and residual liquid;
[0012] The pyrolysis products were subjected to distillation to obtain gaseous chlorosilanes and low-boiling substances;
[0013] The residual liquid was concentrated to obtain gaseous chlorosilane and concentrated product;
[0014] The concentrated product is subjected to a first hydrolysis treatment to obtain hydrogen gas and waste liquid.
[0015] The method for recycling polycrystalline silicon slag slurry as described above, wherein the aluminum removal treatment includes:
[0016] The high-boiling-point substance is subjected to a first aluminum removal treatment using an aluminum removal evaporator to obtain a first gas phase and a first liquid phase; the first gas phase is subjected to a second aluminum removal treatment using an aluminum removal evaporator to obtain a gas phase to be titanium removed and a second liquid phase.
[0017] The polycrystalline silicon slag recovery method described above further includes: the second liquid phase participating in the first aluminum removal treatment.
[0018] The method for recovering polycrystalline silicon slag slurry as described above, wherein the titanium removal treatment includes: performing a first titanium removal treatment on the gas phase to be titanium removed using a titanium removal evaporator to obtain a second gas phase and a third liquid phase; and performing a second titanium removal treatment on the second gas phase using a titanium removal evaporator to obtain an intermediate high-boiling substance and a fourth liquid phase.
[0019] The method for recycling polycrystalline silicon slag slurry as described above further includes: the fourth liquid phase participating in the first titanium removal treatment.
[0020] The method for recycling polycrystalline silicon slag slurry as described above further includes: performing a second hydrolysis treatment on the first liquid phase and / or the third liquid phase.
[0021] In the polycrystalline silicon slag recovery method described above, the temperature in the first aluminum removal treatment is 150-200℃, and the pressure is 0.05-0.15 MPaG; and / or,
[0022] In the second aluminum removal process, the temperature is 80-180℃ and the pressure is 0.03-0.15 MPaG; and / or,
[0023] In the first titanium removal treatment, the temperature is 150-200℃ and the pressure is 0.05-0.15 MPaG; and / or,
[0024] In the second titanium removal treatment, the temperature is 130-180℃ and the pressure is 0.05-0.15 MPaG; and / or,
[0025] In the second hydrolysis treatment, the temperature is 50-80℃ and the pressure is 0.02-0.06MPaG.
[0026] The method for recovering polycrystalline silicon slag slurry as described above, wherein the pyrolysis reaction is carried out at a temperature of 140-180℃ and a pressure of 0.05-0.15 MPaG; and / or,
[0027] In the distillation process, the temperature is 60–130°C and the pressure is 0.05–0.15 MPaG.
[0028] In the polycrystalline silicon slag slurry recovery method described above, the concentration treatment is performed at a temperature of 130–180°C and a pressure of 0.05–0.15 MPaG; and / or,
[0029] In the first hydrolysis treatment, the temperature is 50-80℃ and the pressure is 0.02-0.06MPaG.
[0030] The present invention provides a recycling system for implementing the polycrystalline silicon recycling method described above, comprising: an aluminum removal unit, a titanium removal unit, a cracking unit, a distillation unit, a concentration unit, and a hydrolysis unit;
[0031] The outlet of the aluminum removal unit is connected to the inlet of the titanium removal unit, the outlet of the titanium removal unit is connected to the inlet of the pyrolysis unit, the first outlet of the pyrolysis unit is connected to the inlet of the distillation unit, the second outlet of the pyrolysis unit is connected to the inlet of the concentration unit, and the outlet of the concentration unit is connected to the inlet of the hydrolysis unit.
[0032] This invention provides a method for recycling polycrystalline silicon slag slurry, which can efficiently recover high-boiling-point substances from polycrystalline silicon slag slurry and improve resource utilization.
[0033] This invention provides a polycrystalline silicon slag slurry recovery system. By organically combining an aluminum removal unit, a titanium removal unit, a cracking unit, a distillation unit, a concentration unit, and a hydrolysis unit, it can be used to implement the above-mentioned recovery method. The recovery system has a simple structure and is suitable for widespread application. Attached Figure Description
[0034] To more clearly illustrate the technical solutions in the embodiments of the present invention or related technologies, the accompanying drawings used in the description of the embodiments of the present invention or related technologies are briefly introduced below. Obviously, the drawings described below are merely some embodiments of the present invention. For those skilled in the art, other drawings can be obtained based on these drawings without creative effort.
[0035] Figure 1 is a process flow diagram of aluminum removal treatment for high boiling points in some embodiments of the present invention;
[0036] Figure 2 is a process flow diagram of titanium removal treatment for high-boiling-point substances in some embodiments of the present invention;
[0037] Figure 3 is a process flow diagram of high-boiling-point pyrolysis in some embodiments of the present invention;
[0038] Figure 4 is a process flow diagram of high-boiling-point pyrolysis residue treatment in some embodiments of the present invention.
[0039] Explanation of reference numerals in the attached drawings: 1: Aluminum removal evaporator; 2: Aluminum removal evaporation tower; 3: Aluminum removal residue hydrolysis tank; 4: Aluminum removal agent feeding tank; 5: Aluminum removal reflux tank; 6: Aluminum removal residue recovery tank; 7: Aluminum removal agent buffer tank; 8: Aluminum removal reflux pump; 9: Hydrolysate circulation pump; 10: First condenser; 11: Titanium removal evaporator; 12: Titanium removal evaporation tower; 13: Second condenser; 14: Titanium removal agent tank; 15: Titanium removal reflux tank; 16: Titanium removal reflux pump; 17: Titanium removal buffer tank; 18: Hydrolysate cooler; 21: High-boiling reaction vessel; 22: High-boiling distillation column; 23: Catalyst tank; 24: First cooler; 25: Second cooler; 26: High-boiling distillation column reflux tank; 27: High-boiling reflux pump; 31: Catalyst concentration vessel; 32: Conversion residue neutralization vessel. Detailed Implementation
[0040] The technical solutions of the embodiments of the present invention will be clearly and completely described below with reference to the accompanying drawings. Obviously, the described embodiments are only some embodiments of the present invention, and not all embodiments. Based on the embodiments of the present invention, all other embodiments obtained by those skilled in the art without creative effort are within the scope of protection of the present invention.
[0041] Figure 1 is a process flow diagram of aluminum removal treatment for high-boiling-point substances in some embodiments of the present invention; Figure 2 is a process flow diagram of titanium removal treatment for high-boiling-point substances in some embodiments of the present invention; Figure 3 is a process flow diagram of pyrolysis treatment for high-boiling-point substances in some embodiments of the present invention; Figure 4 is a process flow diagram of pyrolysis residue treatment for high-boiling-point substances in some embodiments of the present invention. As shown in Figures 1-4, the first aspect of the present invention provides a method for recycling polycrystalline silicon slag slurry, comprising: aluminum removal treatment and titanium removal treatment of high-boiling-point substances generated from slag slurry treatment to obtain intermediate high-boiling-point substances;
[0042] The intermediate high-boiling-point substance is subjected to a cracking reaction with hydrogen chloride to obtain cracking products and residual liquid;
[0043] The pyrolysis products were subjected to distillation to obtain gaseous chlorosilanes and low-boiling substances;
[0044] The residual liquid was concentrated to obtain gaseous chlorosilane and concentrated products;
[0045] The concentrated product is subjected to a first hydrolysis treatment to obtain hydrogen gas and waste liquid.
[0046] In this invention, the high-boiling-point substances generated from slurry treatment mainly include Si2Cl6, Si2OCl6, AlCl3, SiCl4, SiHCl3, iron-containing chlorides, titanium-containing chlorides, and boron-containing chlorides. Specifically, the mass percentage of Si2Cl6 is 55-70%, the mass percentage of Si2OCl6 is 3-8%, the mass percentage of AlCl3 is 0.01-0.08%, the mass percentage of SiCl4 is 15-25%, the mass percentage of SiHCl3 is 0.5-3%, the mass percentage of iron-containing chlorides is no higher than 80 ppm, the mass percentage of titanium-containing chlorides is no higher than 30 ppm, and the mass percentage of boron-containing chlorides is no higher than 30 ppm.
[0047] The method for recycling polycrystalline silicon slag slurry of the present invention specifically includes: performing aluminum removal treatment on high-boiling substances to remove aluminum impurities from the high-boiling substances, and then performing titanium removal treatment on the high-boiling substances after removing aluminum impurities to remove titanium impurities from the high-boiling substances, thereby obtaining intermediate high-boiling substances after removing aluminum and titanium.
[0048] Then, under the action of a catalyst, the intermediate high-boiling substance can be cracked with hydrogen chloride to obtain cracking products including silicon tetrachloride and trichlorosilane, as well as residual liquid including chlorosilane, polysiloxane and spent catalyst.
[0049] The cracking products, including silicon tetrachloride and trichlorosilane, are then subjected to distillation to obtain high-boiling gaseous chlorosilanes and low-boiling substances. The obtained gaseous chlorosilanes can be recycled, and the obtained low-boiling substances can be returned to participate in the cracking reaction.
[0050] The residual liquid is concentrated, during which the chlorosilanes in the residual liquid will volatilize, thereby obtaining gaseous chlorosilanes and concentrated products including waste catalysts and polysiloxanes. The obtained gaseous chlorosilanes can be recycled.
[0051] The concentrated product undergoes a first hydrolysis treatment to obtain hydrogen gas and waste liquid. The hydrogen gas can be recycled and reused, while the waste liquid has lower toxicity and can be directly discharged into the main wastewater pipe.
[0052] The method for recovering polycrystalline silicon slag slurry of the present invention can efficiently remove impurities from high-boiling substances generated during polycrystalline silicon slag slurry treatment, realize the recovery of chlorosilanes in polycrystalline silicon slag slurry, and improve resource utilization.
[0053] In some embodiments of the present invention, the aluminum removal process includes:
[0054] The high-boiling-point substance is subjected to a first aluminum removal treatment using an aluminum removal evaporator 1 to obtain a first gas phase and a first liquid phase; the first gas phase is subjected to a second aluminum removal treatment using an aluminum removal evaporator 2 to obtain a gas phase to be titanium removed and a second liquid phase.
[0055] It is understandable that aluminum removers can be added during the aluminum removal process.
[0056] Specifically, the high-boiling-point substances generated from the slurry treatment undergo a first aluminum removal treatment in the aluminum removal evaporator 1. After the first aluminum removal treatment, a first gas phase mainly consisting of Si2Cl6, Si2OCl6, SiCl4, SiHCl3, iron-containing chlorides, titanium-containing chlorides, and boron-containing chlorides, and a first liquid phase mainly consisting of AlCl3, aluminum removal agent, and unreacted high-boiling-point substances are obtained.
[0057] The first gas phase is output from the gas phase outlet of the aluminum removal evaporator 1 and enters the aluminum removal evaporator 2 through the inlet of the aluminum removal evaporator 2. The gas phase undergoes a second aluminum removal treatment in the aluminum removal evaporator 2 to obtain a titanium-removing gas phase containing Si2Cl6, Si2OCl6, iron-containing chlorides, titanium-containing chlorides, and boron-containing chlorides, as well as a second liquid phase containing SiCl4 and SiHCl3.
[0058] Since the aluminum removal evaporator 2 has a higher separation efficiency, this invention can more efficiently remove Al impurities from high-boiling substances by sequentially using the aluminum removal evaporator 1 and the aluminum removal evaporator 2, thereby reducing the aluminum impurity content in the recovered chlorosilane and improving resource utilization.
[0059] Furthermore, the second liquid phase can participate in the first aluminum removal process to further save materials and achieve better aluminum removal, thereby improving resource utilization efficiency.
[0060] In some embodiments of the present invention, the titanium removal process includes: performing a first titanium removal process on the gas phase to be removed using a titanium removal evaporator 11 to obtain a second gas phase and a third liquid phase; and performing a second titanium removal process on the second gas phase using a titanium removal evaporator 12 to obtain an intermediate high-boiling substance and a fourth liquid phase.
[0061] It is understandable that titanium removal agents can be added during titanium removal treatment.
[0062] Specifically, the titanium removal evaporator 11 is used to perform a first titanium removal treatment on the gas phase to be titanium removed, which includes Si2Cl6, Si2OCl6, iron-containing chloride, titanium-containing chloride and boron-containing chloride, to obtain a second gas phase mainly including Si2Cl6, Si2OCl6, SiCl4, SiHCl3, iron-containing chloride and boron-containing chloride, and a third liquid phase mainly including titanium removal agent, titanium-containing chloride and unreacted high-boiling substances;
[0063] Then, the second gas phase is subjected to a second titanium removal treatment using a titanium removal evaporator 12 to obtain an intermediate high-boiling product including Si2Cl6 and Si2OCl6, and a fourth liquid phase including SiCl4, SiHCl3 and a small amount of titanium chloride.
[0064] Since the titanium removal evaporator 12 has a higher separation efficiency, this invention can more efficiently remove Ti impurities from the gas phase to be titanium removed by sequentially using the titanium removal evaporator 11 and the titanium removal evaporator 12 to remove aluminum from high-boiling substances, thereby reducing the titanium impurity content in the recovered chlorosilane and further improving resource utilization.
[0065] Furthermore, the fourth liquid phase can be involved in the first titanium removal process to further save materials and achieve better titanium removal, thereby improving resource utilization efficiency.
[0066] In some embodiments of the present invention, a second hydrolysis treatment is further performed on the first liquid phase and / or the third liquid phase.
[0067] In some embodiments, lime milk (a lime milk aqueous solution with a mass percentage of 3-10%) can be added during the second hydrolysis treatment. The first liquid phase and / or the third liquid phase undergo hydrolysis under the action of lime milk. The wastewater obtained from hydrolysis enters the wastewater main pipe, and the tail gas (HCl, H2, water) obtained enters the tail gas tower for treatment. This can further achieve efficient waste removal of high-boiling polysilicon and improve resource utilization efficiency.
[0068] The present invention can further select the parameters of the first aluminum removal treatment, the second aluminum removal treatment, the first titanium removal treatment, and the second titanium removal treatment to further improve the effectiveness of the aluminum removal and titanium removal treatments, obtain intermediate high-boiling substances with higher purity, and promote subsequent processing. Exemplarily, in some embodiments of the present invention, in the first aluminum removal treatment, the temperature is 150-200°C, and the pressure is 0.05-0.15 MPaG; and / or,
[0069] In the second aluminum removal process, the temperature is 80-180℃ and the pressure is 0.03-0.15 MPaG; and / or,
[0070] In the first titanium removal treatment, the temperature is 150-200℃ and the pressure is 0.05-0.15 MPaG; and / or,
[0071] In the second titanium removal process, the temperature is 130-180℃ and the pressure is 0.05-0.15 MPaG; and / or,
[0072] In the second hydrolysis treatment, the temperature is 50-80℃ and the pressure is 0.02-0.06MPaG.
[0073] The inventors also discovered that by selecting the parameters of the pyrolysis reaction, the efficiency of the pyrolysis reaction can be further improved, yielding pyrolysis products and residual liquid. For example, in the pyrolysis reaction, the temperature is 140-180°C and the pressure is 0.05-0.15 MPaG.
[0074] In some embodiments of the present invention, when the temperature is 60-130°C and the pressure is 0.05-0.15 MPaG during distillation, the gaseous chlorosilanes in the cracking products can be separated from low-boiling substances more efficiently while saving energy, thereby achieving efficient recovery and utilization of high-boiling substances.
[0075] Furthermore, when the concentration process is carried out at a temperature of 130–180°C and a pressure of 0.05–0.15 MPaG, the efficiency of the concentration process can be improved, as well as the yield and purity of gaseous chlorosilanes.
[0076] When the temperature is 50-80℃ and the pressure is 0.02-0.06MPaG in the first hydrolysis treatment, the efficiency of the first hydrolysis treatment can be further improved while saving energy consumption. This allows the polysiloxane in the concentrated product to be more fully converted into hydrogen and waste liquid, achieving efficient treatment of waste in the slurry and improving the efficiency of resource recycling.
[0077] A second aspect of the present invention provides a recycling system for implementing the above-described polysilicon recycling method, comprising: an aluminum removal unit, a titanium removal unit, a cracking unit, a distillation unit, a concentration unit, and a hydrolysis unit;
[0078] The outlet of the aluminum removal unit is connected to the inlet of the titanium removal unit, the outlet of the titanium removal unit is connected to the inlet of the pyrolysis unit, the first outlet of the pyrolysis unit is connected to the inlet of the distillation unit, the second outlet of the pyrolysis unit is connected to the inlet of the concentration unit, and the outlet of the concentration unit is connected to the inlet of the hydrolysis unit.
[0079] Specifically, after the high-boiling-point substance undergoes aluminum removal treatment in the aluminum removal unit, a titanium-removing gas phase is obtained, in which aluminum impurities have been removed. This titanium-removing gas phase is output from the outlet of the aluminum removal unit and enters the titanium removal unit through the inlet. In the titanium removal unit, it undergoes titanium removal treatment, resulting in an intermediate high-boiling-point substance with titanium impurities removed. This intermediate high-boiling-point substance is output from the outlet of the titanium removal unit and enters the cracking unit through the inlet. In the cracking unit, it undergoes a cracking reaction with hydrogen chloride to obtain cracking products and residual liquid. The cracking products are output from the first outlet of the cracking unit and enter the distillation unit through the inlet to undergo distillation treatment, obtaining gaseous chlorosilanes and low-boiling-point substances. The residual liquid is output from the second outlet of the cracking unit and enters the concentration unit through the inlet. In the concentration unit, it undergoes concentration treatment to obtain gaseous chlorosilanes and concentrated products. The concentrated products are output from the outlet of the concentration unit and enter the hydrolysis unit through the inlet. In the hydrolysis unit, it undergoes a first hydrolysis treatment to obtain hydrogen and waste liquid.
[0080] The method for recovering polycrystalline silicon slag slurry of the present invention can efficiently remove impurities from high-boiling substances generated during polycrystalline silicon slag slurry treatment, realize the recovery of chlorosilanes in polycrystalline silicon slag slurry, and improve resource utilization.
[0081] The technical solution of the present invention will be further described below with reference to specific embodiments.
[0082] Example 1
[0083] The polycrystalline silicon slag slurry recovery system of this embodiment is shown in Figures 1-4, including: an aluminum removal evaporator 1, an aluminum removal evaporation tower 2, an aluminum removal residual liquid hydrolysis tank 3, an aluminum removal agent feeding tank 4, an aluminum removal residual liquid recovery tank 6, an aluminum removal reflux tank 5, an aluminum removal agent buffer tank 7, a hydrolysis tank cooler, a hydrolysis liquid circulation pump 9, an aluminum removal reflux pump 8, a first condenser 10, a titanium removal evaporator 11, a titanium removal evaporation tower 12, a second condenser 13, a titanium removal agent tank 14, a titanium removal reflux tank 15, a titanium removal reflux pump 16, a titanium removal buffer tank 17, a hydrolysis liquid cooler 18, a high-boiling reaction vessel 21, a high-boiling distillation tower 22, a catalyst tank 23, a first cooler 24, a second cooler 25, a high-boiling distillation tower reflux tank 26, a high-boiling reflux pump 27, a catalyst concentration vessel 31, and a conversion residual liquid neutralization vessel 32;
[0084] The outlet of the aluminum removal agent feeding tank 4 is connected to the inlet of the aluminum removal agent buffer tank 7. The outlet of the aluminum removal agent buffer tank 7 is connected to the inlet of the aluminum removal evaporator 1. The gas phase outlet of the aluminum removal evaporator 1 is connected to the inlet of the aluminum removal evaporation tower 2. The top outlet of the aluminum removal evaporation tower 2 is connected to the inlet of the first condenser 10. The outlet of the first condenser 10 is connected to the inlet of the aluminum removal reflux tank 5. The outlet of the aluminum removal reflux tank 5 is connected to the inlet of the aluminum removal reflux pump 8. The outlet of the aluminum removal reflux pump 8 is connected to the inlet of the aluminum removal evaporation tower 2. The bottom outlet of the aluminum removal evaporation tower 2 is connected to the inlet of the aluminum removal evaporator 1.
[0085] The liquid phase outlet of the aluminum removal evaporator 1 is connected to the inlet of the aluminum removal residual liquid recovery tank 6, the outlet of the aluminum removal residual liquid recovery tank 6 is connected to the inlet of the aluminum removal residual liquid hydrolysis tank 3, the liquid phase outlet of the aluminum removal residual liquid hydrolysis tank 3 is connected to the inlet of the hydrolysis liquid circulation pump 9, the outlet of the hydrolysis liquid circulation pump 9 is connected to the cold source inlet of the hydrolysis tank cooler, and the gas phase outlet of the aluminum removal residual liquid hydrolysis tank 3 is connected to the heat source inlet of the hydrolysis liquid cooler 18.
[0086] The outlet of the aluminum removal residual liquid recovery tank 6 is connected to the inlet of the aluminum removal evaporator 1;
[0087] The outlet of the aluminum removal reflux tank 5 is connected to the inlet of the titanium removal buffer tank 17, the outlet of the titanium removal agent tank 14 is connected to the inlet of the titanium removal buffer tank 17, the outlet of the titanium removal agent tank 14 is connected to the inlet of the titanium removal evaporator 11, the gas phase outlet of the titanium removal evaporator 11 is connected to the inlet of the titanium removal evaporator 12, the top outlet of the titanium removal evaporator 12 is connected to the inlet of the second condenser 13, the outlet of the second condenser 13 is connected to the inlet of the titanium removal reflux tank 15, the outlet of the titanium removal reflux tank 15 is connected to the inlet of the titanium removal reflux pump 16, the outlet of the titanium removal reflux pump 16 is connected to the inlet of the titanium removal evaporator 12, and the bottom outlet of the titanium removal evaporator 12 is connected to the inlet of the titanium removal evaporator 11.
[0088] The liquid phase outlet of the titanium removal evaporator 11 is connected to the inlet of the aluminum removal residual liquid recovery tank 6, the outlet of the aluminum removal residual liquid recovery tank 6 is connected to the inlet of the aluminum removal residual liquid hydrolysis tank 3, the liquid phase outlet of the aluminum removal residual liquid hydrolysis tank 3 is connected to the inlet of the hydrolysis liquid circulation pump 9, the outlet of the hydrolysis liquid circulation pump 9 is connected to the cold source inlet of the hydrolysis liquid cooler 18, and the gas phase outlet of the aluminum removal residual liquid hydrolysis tank 3 is connected to the heat source inlet of the hydrolysis liquid cooler 18.
[0089] Except that the outlet of the titanium reflux pump 16 is connected to the high-boiling feed inlet of the high-boiling reactor 21, the outlet of the catalyst tank 23 is connected to the catalyst feed inlet, the high-boiling reactor 21 has an HCl feed inlet; the cracking product outlet of the high-boiling reactor 21 is connected to the feed inlet of the high-boiling distillation column 22, the bottom outlet of the high-boiling distillation column 22 is connected to the inlet of the high-boiling reactor 21, the top outlet of the high-boiling distillation column 22 is connected to the heat source inlet of the first cooler 24, circulating water enters the first cooler 24 through the cold source inlet of the first cooler 24, the heat source outlet of the first cooler 24 is connected to the heat source inlet of the second cooler 25, ethylene glycol enters the second cooler 25 through the cold source inlet of the second cooler 25, the heat source outlet of the second cooler 25 is connected to the inlet of the high-boiling distillation column reflux tank 26, and the outlet of the high-boiling distillation column reflux tank 26 is connected to the high-boiling reflux pump 27;
[0090] The outlet of the high-boiling reactor 21 is connected to the inlet of the catalyst concentration reactor 31, and the outlet of the concentrated product of the catalyst concentration reactor 31 is connected to the inlet of the conversion residue neutralization reactor 32.
[0091] Example 2
[0092] The method for recycling polycrystalline silicon slag slurry in this embodiment uses the system from Embodiment 1, and specifically includes:
[0093] 1) The aluminum removal agent is fed into the aluminum removal agent buffer tank 7 through the aluminum removal agent feeding tank 4, and then into the aluminum removal evaporator 1 through the aluminum removal agent buffer tank 7. The high boiling point and the aluminum removal agent are subjected to the first aluminum removal treatment in the aluminum removal evaporator 1. After the first aluminum removal treatment, the first liquid phase and the first gas phase are obtained.
[0094] The first gas phase is output from the outlet of the aluminum removal evaporator 1 and enters the aluminum removal evaporator 2 through the inlet. The second aluminum removal process is carried out in the aluminum removal evaporator 2. The titanium-removing gas phase obtained after the second aluminum removal process is output from the top outlet of the aluminum removal evaporator 2 and enters the first condenser 10 through the inlet. After condensation in the first condenser 10, liquid chlorosilane is obtained. The liquid chlorosilane is output from the outlet of the first condenser 10 and enters the aluminum removal reflux tank 5 through the inlet. Part of the liquid chlorosilane in the aluminum removal reflux tank 5 is output from the outlet of the aluminum removal reflux tank 5 and enters the aluminum removal reflux pump 8 through the inlet. The outlet of the aluminum removal reflux pump 8 is connected to the inlet of the aluminum removal evaporator 2, and the bottom outlet of the aluminum removal evaporator 2 is connected to the inlet of the aluminum removal evaporator 1.
[0095] The first liquid phase is output from the liquid phase outlet of the aluminum removal evaporator 1, and enters the aluminum removal residual liquid recovery tank 6 through the inlet of the aluminum removal residual liquid recovery tank 6. The liquid phase in the aluminum removal residual liquid recovery tank 6 is output from the outlet of the aluminum removal residual liquid recovery tank 6, and enters the aluminum removal residual liquid hydrolysis tank 3 through the inlet of the aluminum removal residual liquid hydrolysis tank 3. In the aluminum removal residual liquid hydrolysis tank 3, it undergoes a second hydrolysis treatment with 8% lime milk to obtain wastewater and tail gas.
[0096] Part of the exhaust gas is cooled by the hydrolysate cooler 18 and then re-enters the aluminum removal residual hydrolysate tank 3, while part of the exhaust gas enters the exhaust gas tower for treatment.
[0097] Part of the wastewater enters the wastewater main pipe, and part of the wastewater is connected to the inlet of the hydrolysate circulation pump 9. Then, it is transported to the hydrolysis tank cooler through the outlet of the hydrolysate circulation pump 9, serving as the cold source of the hydrolysate cooler 18 to cool the exhaust gas.
[0098] 2) The liquid chlorosilane output from the aluminum removal reflux tank 5 enters the titanium removal buffer tank 17 through the titanium removal buffer tank 17, and the titanium removal agent enters the titanium removal buffer tank 17 through the titanium removal agent tank 14. Then, the premix of the titanium removal agent and the liquid chlorosilane output from the aluminum removal reflux tank 5 enters the titanium removal evaporator 11 through the titanium removal buffer tank 17, so that the liquid chlorosilane output from the aluminum removal reflux tank 5 and the titanium removal agent undergo the first titanium removal treatment in the titanium removal evaporator 11. After the first titanium removal treatment, the third liquid phase and the second gas phase are obtained.
[0099] The second gas phase is output from the outlet of the titanium removal evaporator 11 and enters the titanium removal evaporator 12 through the inlet. After being processed by the titanium removal evaporator 12, the intermediate high-boiling product is output from the top outlet of the titanium removal evaporator 12 and enters the second condenser 13 through the inlet. After being condensed by the second condenser 13, liquid chlorosilane is obtained. The liquid chlorosilane is output from the outlet of the condenser 3 and enters the titanium removal reflux tank 15 through the inlet. Part of the liquid chlorosilane in the titanium removal reflux tank 15 is output from the outlet of the titanium removal reflux tank 15 and enters the titanium removal reflux pump 16 through the inlet. The outlet of the titanium removal reflux pump 16 is connected to the inlet of the titanium removal evaporator 12, and the bottom outlet of the titanium removal evaporator 12 is connected to the inlet of the titanium removal evaporator 11.
[0100] The third liquid phase is output from the liquid phase outlet of the titanium removal evaporator 11, and enters the aluminum removal residual liquid recovery tank 6 through the inlet of the aluminum removal residual liquid recovery tank 6. The liquid phase in the aluminum removal residual liquid recovery tank 6 is output from the outlet of the aluminum removal residual liquid recovery tank 6, and enters the aluminum removal residual liquid hydrolysis tank 3 through the inlet of the aluminum removal residual liquid hydrolysis tank 3. In the aluminum removal residual liquid hydrolysis tank 3, it undergoes a second hydrolysis treatment with 8% lime milk to obtain wastewater and tail gas.
[0101] Part of the exhaust gas is cooled by the hydrolysate cooler 18 and then re-enters the aluminum removal residual hydrolysate tank 3, while part of the exhaust gas enters the exhaust gas tower for treatment.
[0102] Part of the wastewater enters the wastewater main pipe, and part of the wastewater is connected to the inlet of the hydrolysate circulation pump 9. Then, it is transported to the hydrolysis tank cooler through the outlet of the hydrolysate circulation pump 9, serving as the cold source of the hydrolysate cooler 18 to cool the exhaust gas.
[0103] 3) Add catalyst to catalyst tank 23, so that the catalyst is output from the outlet of catalyst tank 23 and enters high-boiling reactor 21 through catalyst inlet. Liquid chlorosilane output from titanium removal reflux pump 16 enters high-boiling substance inlet into high-boiling reactor 21. HCl enters high-boiling reactor 21 through HCl inlet. Under the action of catalyst in high-boiling reactor 21, HCl and high-boiling substance in liquid chlorosilane output from titanium removal reflux pump 16 undergo cracking reaction to obtain cracking products and residual liquid.
[0104] The cracking products are output through the cracking product outlet and enter the high-boiling distillation column 22 through the feed inlet. In the high-boiling distillation column 22, the cracking products are distilled to obtain gaseous chlorosilanes and low-boiling substances. The low-boiling substances are output through the bottom outlet of the high-boiling distillation column 22 and enter the high-boiling reactor 21 through the inlet to participate in the cracking reaction.
[0105] A gaseous chlorosilane is introduced into the first cooler 24 through its heat source inlet, and circulating water is introduced into the first cooler 24 through its cold source inlet. In the first cooler 24, the gaseous chlorosilane is subjected to a first cooling treatment using circulating water to obtain intermediate chlorosilane. The intermediate chlorosilane is then output through the heat source outlet of the first cooler 24 and enters the second cooler 25 through its heat source inlet. Ethylene glycol is introduced into the second cooler 25 through its cold source inlet. In the second cooler 25, the intermediate chlorosilane is subjected to a second cooling treatment using ethylene glycol to obtain liquid chlorosilane. The liquid chlorosilane is then output through the heat source outlet of the second cooler 25 and enters the high-boiling-point distillation column reflux tank 26 through its inlet. It is stored in the high-boiling-point distillation column reflux tank 26 and then pumped out of the high-boiling-point distillation column reflux tank 26 using a high-boiling-point reflux pump 27 for reuse.
[0106] 4) The residual liquid output from the high-boiling reactor 21 enters the catalyst concentration reactor 31 for concentration treatment to obtain gaseous chlorosilane and concentrated products;
[0107] The gaseous chlorosilane is fed into the high-boiling distillation column 22 for distillation.
[0108] The concentrated product is introduced into the conversion residue neutralization vessel 32. In the conversion residue neutralization vessel 32, a first hydrolysis treatment is carried out using an aqueous sodium hydroxide solution to obtain hydrogen gas and waste liquid.
[0109] Hydrogen gas is introduced into the tail gas scrubbing tower for scrubbing treatment, and the resulting waste liquid is sent to the wastewater treatment facility for treatment.
[0110] The high-boiling compounds include: Si2Cl6, Si2OCl6, AlCl3, SiCl4, SiHCl3, iron-containing chlorides, titanium-containing chlorides, and boron-containing chlorides, with the following mass percentages: Si2Cl6 66.29%, Si2OCl6 6.4%, AlCl3 0.03%, SiCl4 24.7%, SiHCl3 1.4%, iron-containing chloride 20 ppm, titanium-containing chloride 6 ppm, and boron-containing chloride 4 ppm.
[0111] The aluminum removal agent is a compound salt, and the addition amount of the aluminum removal agent is 16 kg / t of high boiling point.
[0112] Except for aluminum evaporator 1, the temperature is 184℃ and the pressure is 0.06MPaG;
[0113] Except for aluminum evaporator 2, the temperature is 112℃ and the pressure is 0.04MPaG;
[0114] In the aluminum residue hydrolysis tank 3, the temperature is 45℃ and the pressure is 0.05MPaG;
[0115] The titanium removal agent is a composite ester, and the addition amount of the titanium removal agent is 0.3 kg / t of high-boiling-point substance;
[0116] Except for the titanium evaporator 11, the temperature is 152℃ and the pressure is 0.07MPaG;
[0117] Except for titanium evaporator 12, the temperature is 142℃ and the pressure is 0.04MPaG;
[0118] In the titanium residue hydrolysis tank, the temperature is 45℃ and the pressure is 0.05MPaG;
[0119] The catalyst is tri-n-butylamine;
[0120] The pyrolysis reaction was carried out at a temperature of 145℃ and a pressure of 0.05 MPaG.
[0121] During the distillation process, the temperature was 61℃ and the pressure was 0.045 MPaG;
[0122] The reflux ratio of the high-boiling-point distillation column 22 is 1.2:1;
[0123] During the concentration process, the temperature was 156℃ and the pressure was 0.05 MPaG;
[0124] The sodium hydroxide aqueous solution has a mass percentage of 20% and a flow rate of 10 m³ / h.
[0125] In the first hydrolysis treatment, the temperature was 55℃ and the pressure was 0.06 MPaG.
[0126] The polysilicon slag slurry recovery method in this embodiment has a high conversion rate of over 90% for high-boiling substances and a recovery rate of over 98% for chlorosilanes. Most of the chlorosilanes in the polysilicon slag slurry can be recovered and reused, effectively reducing the chlorine consumption in polysilicon production to 0.1 or even lower, thus saving costs.
[0127] The various embodiments in this specification are described in a related manner. Similar or identical parts between embodiments can be referred to interchangeably. Each embodiment focuses on its differences from other embodiments. The above are merely preferred embodiments of the present invention and are not intended to limit the scope of protection of the present invention. Any modifications, equivalent substitutions, improvements, etc., made within the spirit and principles of the present invention are included within the scope of protection of the present invention.
Claims
1. A method for recovering a polysilicon slurry, characterized by, include: Aluminum removal and titanium removal treatments are performed on the high-boiling-point substances produced by slurry processing to obtain intermediate high-boiling-point substances. The intermediate high-boiling-point substance is subjected to a cracking reaction with hydrogen chloride to obtain cracking products and residual liquid; The pyrolysis products were subjected to distillation to obtain gaseous chlorosilanes and low-boiling substances; The residual liquid was concentrated to obtain gaseous chlorosilane and concentrated product; The concentrated product is subjected to a first hydrolysis treatment to obtain hydrogen gas and waste liquid.
2. The method for recovering the polysilicon slurry according to claim 1, characterized in that, The aluminum removal process includes: The high-boiling-point substance is subjected to a first aluminum removal treatment using an aluminum removal evaporator to obtain a first gas phase and a first liquid phase; the first gas phase is subjected to a second aluminum removal treatment using an aluminum removal evaporator to obtain a gas phase to be titanium removed and a second liquid phase.
3. The method for recovering the polysilicon slurry according to claim 2, characterized in that, Also includes: The second liquid phase participates in the first aluminum removal process.
4. The recovery method of polysilicon slurry according to claim 2 or 3, characterized in that, The titanium removal process includes: performing a first titanium removal process on the gas phase to be titanium removed using a titanium removal evaporator to obtain a second gas phase and a third liquid phase; and performing a second titanium removal process on the second gas phase using a titanium removal evaporator to obtain an intermediate high-boiling substance and a fourth liquid phase.
5. The method for recovering the polysilicon slurry according to claim 4, characterized in that, Also includes: The fourth liquid phase participates in the first titanium removal process.
6. The method of recovering polysilicon slurry according to any one of claims 4-5, wherein Also includes: The first liquid phase and / or the third liquid phase are subjected to a second hydrolysis treatment.
7. The method of recovering polysilicon slurry according to claim 6, wherein In the first aluminum removal process, the temperature is 150-200℃ and the pressure is 0.05-0.15 MPaG; and / or, In the second aluminum removal process, the temperature is 80-180℃ and the pressure is 0.03-0.15 MPaG; and / or, In the first titanium removal treatment, the temperature is 150-200℃ and the pressure is 0.05-0.15 MPaG; and / or, In the second titanium removal treatment, the temperature is 130-180℃ and the pressure is 0.05-0.15 MPaG; and / or, In the second hydrolysis treatment, the temperature is 50-80℃ and the pressure is 0.02-0.06MPaG.
8. The method of recovering polysilicon slurry according to any one of claims 1 to 7, characterized in that, In the pyrolysis reaction, the temperature is 140-180℃ and the pressure is 0.05-0.15 MPaG; and / or, In the distillation process, the temperature is 60–130°C and the pressure is 0.05–0.15 MPaG.
9. The method of recovering polysilicon slurry according to any one of claims 1 to 4, characterized in that, In the concentration process, the temperature is 130–180°C and the pressure is 0.05–0.15 MPaG; and / or, In the first hydrolysis treatment, the temperature is 50-80℃ and the pressure is 0.02-0.06MPaG.
10. A recovery system for carrying out the recovery method of the polycrystalline silicon according to any one of claims 1 to 9, characterized by, include: Aluminum removal unit, titanium removal unit, cracking unit, distillation unit, concentration unit, and hydrolysis unit; The outlet of the aluminum removal unit is connected to the inlet of the titanium removal unit, the outlet of the titanium removal unit is connected to the inlet of the pyrolysis unit, the first outlet of the pyrolysis unit is connected to the inlet of the distillation unit, the second outlet of the pyrolysis unit is connected to the inlet of the concentration unit, and the outlet of the concentration unit is connected to the inlet of the hydrolysis unit.