Decorative composite
The decorative composite with a thin metal layer on a plastic carrier addresses processing difficulties and mechanical weaknesses of conventional foils, offering a durable, visually appealing, and environmentally friendly decorative solution for furniture surfaces.
Patent Information
- Application Number
- PCT/EP2026/062825
- Authority / Receiving Office
- WO · WO
- Patent Type
- Applications
- Current Assignee / Owner
- Priority Date
- 2025-05-13
- Filing Date
- 2026-05-05
- Publication Date
- 2026-11-19
AI Technical Summary
Conventional metal foils used for decorative coatings on structural elements like furniture are difficult to process, show substrate irregularities, and are mechanically weak, leading to visual defects and reduced lifespan.
A decorative composite comprising a thin metal decorative layer on a plastic carrier layer, bonded with adhesives, allowing low-pressure application and improved impact resistance, with optional protective layers for enhanced durability.
The composite provides a homogeneous, durable, and mechanically resilient decorative coating that reduces substrate visibility and environmental impact, while being easier to process and maintain.
Smart Images

Figure EP2026062825_19112026_PF_FP_ABST
Abstract
Description
[0001] May 5, 2026
[0002] Decorative composite
[0003] DESCRIPTION
[0004] The invention relates to a decorative composite for producing a decorative coating on surfaces of a structural element of furniture and other surfaces of structural elements in the visible area of a user, comprising a carrier layer and a decorative layer arranged adhering to the carrier layer, wherein the decorative layer is a film made of a metal.
[0005] In current technology, metal foils are frequently used to provide high-quality metallic surfaces on structural elements such as furniture. However, these conventional foils present significant processing difficulties. Particularly when applied to substrates that are not perfectly flat, such as particleboard, the underlying structure shows through. This results in undesirable irregularities in the visible surface.
[0006] Furthermore, conventional metal foils are sensitive to impact, which can lead to dents, cracks, or peeling under mechanical stress, especially in everyday use. These disadvantages negatively affect both the visual appearance and the lifespan of the coated components.
[0007] Against this background, there is a need for a decorative composite that is easy and durable to process, offers a homogeneous visible surface and is also mechanically resilient, without exhibiting the structural weaknesses of conventional metal foils.
[0008] The present invention is therefore based on the objective of providing a decorative composite that enables a high-quality decorative coating on the surfaces of structural elements, wherein the composite has improved processability, increased impact resistance and reduced susceptibility to showing through of substrate structures compared to conventional metal foils.
[0009] The invention is solved by a decorative composite according to claim 1. Advantageous embodiments are specified in the dependent claims. May 5, 2026
[0010] According to the invention, a decorative composite for producing a decorative coating on the surfaces of a structural element of furniture and other surfaces of structural elements in the visible area of a user is being used. The composite comprises a carrier layer and a decorative layer adhered to the carrier layer, wherein the decorative layer is a foil made of a metal. The coatings according to the invention are preferably used on structural elements of furniture or other elements in the visible area of a viewer. Such structural elements are typically substructures made of OSB (oriented strand board), particleboard, MDF (medium-density fiberboard), HDF (high-density fiberboard), and other wood and / or composite materials.
[0011] According to the invention, a decorative layer is arranged in an adhesive manner on the carrier layer. The carrier layer has a bottom side facing the surface to be coated and a top side facing the decorative layer. The decorative layer is arranged on the top side of the carrier layer.
[0012] A key advantage of the invention is that the composite is suitable for bonding to surfaces, particularly wooden surfaces, using low-pressure methods. Pure metal foils of comparable thickness (e.g., 80 µm) cannot be bonded, or at best only with disadvantages unacceptable for a decorative surface, to elements commonly used for substructures, such as chipboard or MDF panels, because the structure of the substrate presses into the metal foil and causes plastic deformation.
[0013] In previously used metal foils, adhesives are not typically employed. Instead, to prevent unwanted texturing, the metal foils are pressed against phenolic resin papers and / or melamine resin papers (HPL (High Pressure Laminate) or CPL (Continuous Pressure Laminate)). To avoid textural imprints, very thick anodized metal foils have been used, such as aluminum foils with layer thicknesses exceeding 250 µm or stainless steel foils with layer thicknesses exceeding 200 µm. This results in a high weight for such conventional coatings. Furthermore, such conventional metal foils are very difficult to process, and ultimately, the use of unnecessarily high metal content, especially aluminum, is detrimental to sustainability, particularly when considering the use of [May 5, 2026].
[0014] Primary aluminum, i.e., newly produced, not recycled aluminum. The decorative composite according to the invention reduces the amount of CO2 generated during production compared to conventional films of greater thickness.
[0015] The very thin layer thickness achievable with a metal foil of a composite according to the invention also allows for the simpler implementation of desired mechanical and chemical properties compared to thicker metal foils. The laminate structure of the composite according to the invention particularly improves the resistance of the coated surface to impacts (during processing / manufacturing and everyday use).
[0016] Finally, the composite according to the invention also allows the processing of the metal-based films in the laminating-gluing process, in particular in roll laminating devices or vacuum pressing devices.
[0017] In a preferred embodiment, the carrier layer is a film made of a plastic, in particular a rigid or stiff film, wherein the film is preferably made of a plastic from the group consisting of polyimide (PI), polyethylene terephthalate (PET), polycarbonate (PC), polymethyl methacrylate (PMMA), polyvinyl chloride (PVC), acrylonitrile butadiene styrene (ABS), or polyester. In a particularly preferred embodiment, the carrier layer is designed as a plastic film made of polyethylene terephthalate (PET).
[0018] PET is particularly suitable as a substrate material, as such films form a hard base and are therefore well-suited for coating textured surfaces. In principle, other plastics besides those listed can also be used for the substrate layer. With regard to sustainability, the use of materials containing recycled content for the substrate layer and / or the decorative layer is also being considered.
[0019] A particularly lightweight composite with very good mechanical and chemical properties can be achieved if the decorative layer is an aluminum foil. One variant therefore envisions the decorative layer being an aluminum foil.
[0020] In one embodiment, it is envisaged that the carrier layer has a thickness in the range of 100 pm to 300 pm. It is further preferably provided that the
[0021] ,.. / 45 May 2026
[0022] The carrier layer has a thickness in the range of 100 g / m to 180 g / m, and more preferably in the range of 125 g / m to 150 g / m. A particularly preferred embodiment is one in which the carrier layer has a thickness of less than or equal to 125 g / m.
[0023] With regard to the metal layer forming the decorative layer, it is intended that the decorative layer (14) has a thickness in the range of 50 g / m to 150 g / m. It is further preferably provided that the decorative layer has a thickness in the range of 60 g / m to 100 g / m, and even more preferably in the range of 70 g / m to 100 g / m. A particularly preferred embodiment is one in which the decorative layer has a thickness of less than or equal to 80 g / m.
[0024] Improved protection of the composite according to the invention can be achieved by arranging a first protective layer above the decorative layer, in particular a protective layer comprising a decorative protective varnish.
[0025] A decorative protective coating can be either inorganic or organic. Coatings containing both organic and inorganic components can also be used. For example, UV acrylates, which are special acrylic monomers or oligomers that cure quickly using UV light (ultraviolet light) or electron beam curing (EBC), can be used as protective coatings. Epoxy, polyurethane, polyester, and melamine coatings are also suitable options. Inorganic components used in protective coatings can include silica gels (silicates) or corundum. Such a decorative protective coating can have various desired decorative and / or protective properties. For example, the coating can have a specific color or texture.Furthermore, a suitably selected protective coating can provide UV or weather protection, or, for example, an antibacterial effect.
[0026] In a preferred embodiment, the first protective layer is thought to have a thickness in the range of 5 gm to 100 gm.
[0027] A high level of protection, particularly during processing and / or storage of the decorative composite, can be achieved if the surface facing away from the substrate layer is coated.
[0028] ...May 155, 2026
[0029] A protective film is arranged on the side of the decorative layer. In one embodiment, a protective film is arranged above the decorative layer. In particular, it can be provided that the protective film is arranged above a previously described first protective layer. This protective film is a temporary protective layer that is removed during or after the application of the composite to a surface. The protective film protects the composite from external mechanical and / or chemical influences that could affect it during handling, processing, and storage. Such a protective film generally consists of a substrate film acting as a carrier and an adhesive layer. The adhesive layer must be selected so that it is removed without leaving any residue when peeled off the composite.
[0030] Regarding the film thickness, it is intended that the protective film has a thickness in the range of 50 pm to 150 pm. A particularly preferred embodiment is one in which the protective film has a thickness of less than or equal to 100 pm.
[0031] According to one embodiment, the decorative layer is bonded to the carrier layer by means of an adhesive layer, in particular by means of an adhesive from the group consisting of 2-component polyurethane, hot melt (air-penetrating), UV adhesive, or rubber adhesive. It is intended that the adhesive layer bonding the decorative layer to the carrier layer has a thickness in the range of 1 pm to 30 pm, preferably in the range of 8 pm to 20 pm.
[0032] The joining of the composite according to the invention with the surface of a structural element can be facilitated by the composite having an adhesive layer on its underside, designed for bonding to the surface of the structural element. The underside of the composite, i.e., the side of the carrier layer facing away from the decorative layer, can thus be prepared for bonding to a surface to be coated. Preferably, the adhesive layer is a pressure-sensitive adhesive (for example, PSA adhesive or hot melt), preferably made of a material from the group consisting of polyurethane (PU), acrylates, rubber, or ethylene vinyl acetate (EVA), and the adhesive layer has a thickness in the range of 5 pm to 250 pm. The adhesive can also be a silicone-based adhesive.
[0033] ...May 165, 2026
[0034] Preferably, the adhesive layer has a thickness in the range of 100 µm to 200 g / m. A particularly preferred embodiment is one in which the adhesive layer has a thickness in the range of 150 g / m to 175 g / m, so that it can adapt uniformly to any unevenness.
[0035] To protect the adhesive layer before the composite is used, a removable covering layer can be arranged on the free surface of the adhesive layer. This covering layer is preferably a polyolefin- or silicone-based film or paper, and preferably has a thickness in the range of 20 g / m² to 100 g / m². A particularly preferred embodiment has a covering layer thickness of 35 g / m² or less.
[0036] According to the invention, a method for producing a decorative coating on the surface of a structural element with a decorative composite according to one of the preceding claims is also included, comprising the step of bonding the decorative composite to the surface of the structural element. In particular, it is intended that the decorative composite is bonded to the surface of the structural element by means of a low-pressure process.
[0037] According to a preferred embodiment, the composite is bonded to the surface by means of lamination, wherein the lamination particularly comprises one or more of the following steps: applying adhesive to the surface of the structural element; applying the composite (10) to the surface (28) coated with the adhesive; drying and / or curing the composite (10) applied to the surface (28) coated with the adhesive. Applying adhesive to the surface of the structural element can be omitted if the composite already has an adhesive layer on its underside intended for bonding to the structural element.
[0038] The drying step typically involves treatment with temperature or heat. The curing step usually includes treatment by radiation (e.g., electron beam curing (ESC)) and / or a chemical reaction or cross-linking (e.g., with moisture penetration).
[0039] ,.. / 75 May 2026
[0040] With regard to lamination, it may be specifically intended to use flat or roll lamination, for which a flat or roll laminator is used.
[0041] For bonding the decorative composite to the surface of the structural element, the pressing pressure (e.g., the contact pressure of the roller pair) can range from 2 bar to 8 bar. Higher pressure may be necessary for thicker or textured materials.
[0042] If thermal activation of the bond between the composite and the surface is necessary, the temperature for adhesive activation can range from 80 °C to 130 °C (depending on the adhesive type). When using rollers, the roller temperature can range from 30 °C to 80 °C (often temperature-controlled to promote adhesive reaction or prevent waviness).
[0043] Laminating speeds range from 10 m / min to 100 m / min (depending on the material, adhesive, and drying time). The drying temperature can range from 60 °C to 120 °C, especially when using solvent-based adhesives or dispersion adhesives.
[0044] The processing parameters for flat / roll laminating machines depend heavily on the material used (e.g., paper, films, textiles), the adhesive system (e.g., solvent-based, solvent-free, hot melt, dispersion adhesive), and the machine configuration. Based on experience, the following guidelines can be assumed: The amount of adhesive to be applied for the adhesive application step to the surface of the structural element can vary depending on the material, ranging from 1 g / m². 2 up to 250 g / m² 2 High grammages, for example in the range of 50 g / m², are particularly common when coating highly textured surfaces such as plywood. 2 up to 250 g / m² 2 It is used to compensate for unevenness and structural depressions. For example, the adhesive can be applied using a doctor blade roller, engraving roller, rubber roller, or by spray application.
[0045] For applying the composite to the surface, the material tension, i.e., the web tension, can be selected and adjusted according to the material used and other parameters. Tension control is usually achieved via dancer rollers or brakes. Steel rollers are frequently used as laminating rollers, often in contrast to rubber or silicone rollers.
[0046] ,.. / 85. May 2026
[0047] It is also conceivable that the composite is bonded to the surface by vacuum pressing, wherein the vacuum pressing process comprises, in particular, one or more of the following steps: arranging the composite on the surface of the structural element in a position intended for coating; placing the structural element together with the composite arranged on its surface in a vacuum pressing device; generating a vacuum in the vacuum pressing device; curing the bond between the surface of the structural element and the composite. During or after generating a vacuum, it may be possible to apply pressure to the structural element bearing the composite by means of a press ram or the like, in order to press the composite onto the surface of the structural element.
[0048] In particular, if no adhesive layer for bonding to the surface of the structural element has yet been arranged on the underside of the composite according to the invention, the method comprises the following step before arranging the composite: preparing the surface of the structural element and / or an underside of the composite to be bonded to the surface of the structural element, wherein a suitable adhesive is applied to the surface of the structural element and / or to the underside of the composite.
[0049] The vacuum pressing device can be designed, for example, as a vacuum press or a vacuum bag. A vacuum pressing device typically consists of a flexible, airtight bag or chamber that completely encloses the workpiece.
[0050] When creating a vacuum, a vacuum or suitable negative pressure is generated by extracting gas within the vacuum press. The extraction of air creates a negative pressure that causes the surrounding air to exert a uniform pressure on the workpiece. This results in an even distribution of the adhesive and a bubble-free bond between the adhesive and the surface of the structural element.
[0051] Depending on the adhesive used and the surface material of the structural element, the curing of the bond can take place at room temperature or with the application of additional heat.
[0052] ...May 195, 2026
[0053] The combination of pressure and possibly heat ensures a permanent and stable bond.
[0054] Vacuum lamination in furniture manufacturing is a precise process in which materials such as wood, veneers, or plastics are bonded together under uniform pressure. This method offers numerous advantages, especially for complex shapes or delicate surfaces. The vacuum pressure generated during lamination ensures even pressure across the entire surface, which is particularly beneficial for large or irregular shapes. Both flat and three-dimensional workpieces can be laminated, enabling the production of curved or shaped furniture components. Since no mechanical presses are used, the method is especially gentle on sensitive surfaces and materials. The uniform distribution of the adhesive and the controlled curing process result in high quality with minimal material waste.
[0055] The vacuum pressure is selected, for example, in the range of -0.8 bar to -0.95 bar (relative to ambient pressure). The aim is to ensure uniform contact pressure across the entire surface to prevent air bubbles and uneven adhesion.
[0056] The temperature is selected, for example, in the range of 60 °C to 120 °C, depending particularly on the type of adhesive used (e.g., polyvinyl acetate (PVAc), polyurethane (PUR), urea-formaldehyde (UF)) or the material's sensitivity to heat. The aim is to activate the adhesive and accelerate the curing process.
[0057] The pressing time is selected, for example, in the range of 10 to 30 minutes, depending particularly on the type of adhesive used and its curing time, or on the material thickness and type. The aim is to ensure a complete and permanent bond between the materials.
[0058] The residual moisture content of the surface material of the structural element is chosen to be around 8%, for example, to prevent deformation or delamination. To ensure good adhesion between the composite and the surface of the structural element,
[0059] ,.. / 105 May 2026
[0060] Care must be taken to apply the adhesive evenly and sufficiently between the bond and the surface.
[0061] The invention is explained in more detail using figures. They show
[0062] Fig. 1 shows a schematic representation of a composite according to the invention with a carrier layer and a decorative layer,
[0063] Fig. 2 shows a schematic representation of a composite according to the invention with a specific layer structure,
[0064] Fig. 3 shows a schematic representation of a composite according to the invention with a specific layer structure in one variant,
[0065] Fig. 4 shows a schematic representation of a composite according to the invention with a specific layer structure in a further variant,
[0066] Fig. 5 shows a schematic representation of a composite according to the invention with a specific layer structure in one variant, and
[0067] Fig. 6 shows a schematic representation of a composite according to the invention arranged on a surface of a structural element.
[0068] Figure 1 shows a schematic cross-section through a decorative composite 10 for producing a decorative coating on the surface 28 of a structural element 26 (see Fig. 6) in a first embodiment. The decorative composite 10 has a carrier layer 12 on the upper surface of which a decorative layer 14 is arranged. The carrier layer 12 forms the mechanical framework of the decorative composite 10 and serves to receive the decorative design elements of the decorative layer 14.
[0069] In the specific embodiment shown in Figure 2, a protective layer 16 is additionally arranged on the decorative layer 14, which can serve in particular to protect against mechanical damage, abrasion and / or UV radiation. The protective layer can also be colored or textured. Other properties are also conceivable, such as providing an antibacterial surface.
[0070] ... / ll5 May 2026
[0071] The protective layer is, for example, an organic or inorganic lacquer, or a lacquer with organic and inorganic components. The decorative layer 14 is bonded to the carrier layer 12 by means of a first adhesive layer 20. The decorative composite 10 thus consists of a carrier layer 12, a decorative layer 14 attached by means of adhesive layer 20, and a protective layer 16 placed on top of it.
[0072] The specific embodiment shown in Figure 3, in addition to the components of Figure 2, includes a protective film 18 arranged on the protective layer 16. This protective film 18 serves in particular to provide temporary protection for the protective layer 16 during transport, storage or processing of the composite 10 and can be removed before or after coating the surface 28 of the structural element 26.
[0073] Figure 4 shows a further embodiment of the decorative composite 10 according to the invention, in which a further adhesive layer 22 is applied to the underside of the composite 10, i.e., to the side of the carrier layer 12 facing the surface 28 of the structural element 26 to be coated. This further adhesive layer 22 has a surface 30 via which the composite 10 can be applied to the surface 28 of the structural element 26 and bonded to it. The adhesive layer 22 can, for example, be designed as a pressure-sensitive or heat-activated adhesive.
[0074] In the embodiment according to Figure 5, in addition to the structure shown in Figure 4, a cover layer 24 is provided, which is arranged on the surface 30 of the further adhesive layer 22. The cover layer 24 protects the adhesive layer 22 until the decorative composite 10 is applied to the surface 28 of the structural element 26 and is removed immediately before application.
[0075] Figure 6 shows an application of the decorative composite 10 in its state applied to a surface 28 of a structural element 26. The adhesive bond is achieved, for example, by means of the previously described adhesive layer 22.
[0076] ,.. / 125 May 2026
[0077] REFERENCE MARK LIST
[0078] 10 Decorative Composite
[0079] 12 Carrier layer
[0080] 14 decorative layer
[0081] 16 Protective layer
[0082] 18 protective film
[0083] 20 adhesive layers
[0084] 22 adhesive layer
[0085] 24 Cover layer
[0086] 26 Construction element
[0087] 28 Surface of the structural element 30 Surface of the adhesive layer
Claims
May 5, 2026 REQUIREMENTS 1. Decorative composite (10) for producing a decorative coating on surfaces (28) of a structural element (26) of furniture or other surfaces (28) of structural elements (26) in the visible area of a user, comprising a carrier layer (12) and a decorative layer (14) arranged adhering to the carrier layer, wherein the decorative layer is a film made of a metal.
2. Decorative composite (10) according to claim 1, characterized in that the carrier layer (12) is a film made of a plastic, in particular a rigid or stiff film, wherein the film is preferably made of a plastic from the group consisting of polyimide (PI), polyethylene terephthalate (PET), polycarbonate (PC), polymethyl methacrylate (PMMA), polyvinyl chloride (PVC), acrylonitrile butadiene styrene (ABS) or polyester, wherein the carrier layer (12) is preferably a film made of polyethylene terephthalate (PET).
3. Decorative composite (10) according to one of claims 1 or 2, characterized in that the decorative layer (14) is an aluminum foil.
4. Decorative composite (10) according to one of the preceding claims, characterized in that the carrier layer (12) has a layer thickness in the range of 100 pm to 300 pm.
5. Decorative composite (10) according to one of the preceding claims, characterized in that the decorative layer (14) has a layer thickness in the range of 50 pm to 150 pm.
6. Decorative composite (10) according to one of the preceding claims, characterized in that a first protective layer (16) is arranged above the decorative layer (14), in particular a protective layer (16) having a decorative protective lacquer.
7. Decorative composite (10) according to claim 6, characterized in that the first protective layer (16) has a layer thickness in the range of 5 pm to 100 pm. 5 May 2026 8. Decorative composite (10) according to one of the preceding claims, characterized in that a protective film (18) is arranged above the decorative layer (14).
9. Decorative composite (10) according to claim 8 and one of claims 6 or 7, characterized in that the protective film (18) is arranged above the first protective layer (16).
10. Decorative composite (10) according to one of the preceding claims, characterized in that the decorative layer (14) is bonded to the carrier layer (12) by means of an adhesive layer (20), in particular by means of an adhesive from the group consisting of 2K polyurethane, hot melt (IK-air-penetrating), UV adhesive or rubber adhesive.
11. Decorative composite (10) according to one of the preceding claims, characterized in that the composite (10) has on its underside an adhesive layer (22) designed for bonding to the surface (28) of the construction element (26).
12. Decorative composite (10) according to claim 11, characterized in that the adhesive layer (22) is a pressure-sensitive adhesive (for example, PSA adhesive or hot melt), preferably made of a material from the group consisting of polyurethane (PU), acrylates, rubber or ethylene vinyl acetate (EVA), and wherein the adhesive layer (22) has a layer thickness in the range of 5 pm to 250 pm.
13. Decorative composite (10) according to claim 12, characterized in that a release liner (24) covering the adhesive layer (22) is arranged on the free surface (30) of the adhesive layer (22), wherein the release liner (24) is preferably a polyolefin or silicone-based film or paper, and wherein the release liner (24) preferably has a thickness in the range of 20 pm to 100 pm.
14. Method for producing a decorative coating on surfaces (28) of a structural element (26) with a decorative composite (10) according to one of the preceding claims, comprising the step:
5. May 2026 Bonding the decorative composite (10) to the surface (28) of the construction element (26).
15. Method according to claim 14, characterized in that the composite (10) is bonded to the surface (28) by means of lamination, wherein the lamination in particular comprises one or more of the following steps: Applying adhesive to the surface (28) of the structural element (26); applying the composite (10) to the surface (28) coated with adhesive; drying and / or curing the composite (10) applied to the surface (28) coated with adhesive.
16. Method according to claim 14, characterized in that the composite (10) is bonded to the surface (28) by means of vacuum pressing, wherein the vacuum pressing in particular comprises one or more of the following steps: Arranging the composite (10) on the surface of the structural element in a position intended for coating; Placing the construction element (26) together with the composite (10) arranged on the surface of the construction element (26) in a vacuum pressing device; Creating a vacuum in the vacuum press device; Curing of the bond between the surface (28) of the structural element (26) and the composite (10).