Nicotine granulates with increased storage stability
A chemically bonded ceramic system with low free water content in nicotine granulates addresses TSNA formation and discolouration, ensuring stability and aesthetic appeal in nicotine pouches.
Patent Information
- Application Number
- PCT/EP2026/064020
- Authority / Receiving Office
- WO · WO
- Patent Type
- Applications
- Current Assignee / Owner
- Priority Date
- 2025-05-13
- Filing Date
- 2026-05-13
- Publication Date
- 2026-11-19
AI Technical Summary
Nicotine-containing pouches face challenges in avoiding the formation of tobacco-specific nitrosamines (TSNAs) and discolouration during storage, which are harmful and reduce product aesthetic appeal.
A novel granulate comprising a solid, porous chemically bonded ceramic system based on calcium sulphate or calcium silicate with minimal free water content, typically less than 1%, is used to minimize TSNA formation and discolouration by reducing oxidation.
The granulate exhibits enhanced stability, reducing TSNA formation and discolouration, maintaining product appearance and safety over extended storage periods.
Smart Images

Figure EP2026064020_19112026_PF_FP_ABST
Abstract
Description
[0001] NICOTINE GRANULATES WITH INCREASED STORAGE STABILITY
[0002] Field of the invention
[0003] The invention relates to a nicotine-containing granulate and nicotine pouches that are capable of storing and releasing nicotine. The invention also relates to methods of manufacturing a nicotine granulate and a pouched product. The nicotine-containing granulates and pouches may be used in intraoral delivery of nicotine, such as in recreational use products. The granulates and pouches may also be employed in aiding smoking cessation, treating nicotine dependence or alleviating the symptoms of nicotine dependence.
[0004] Background
[0005] Tobacco-free nicotine products are used by individuals to provide pleasurable sensations resulting from nicotine uptake. They are also useful as nicotine replacement therapy products. Intraoral products that are used in this way include nicotine pouches. These are a convenient and safer alternative to cigarettes as they offer a source of nicotine which does not expose the user to some of the risks associated with cigarette smoking, such as harmful substances found in cigarette smoke (e.g. carbon monoxide, benzene and formaldehyde) and in the cigarette itself (e.g. vinyl chloride that is used in cigarette filters).
[0006] Nicotine pouches, often referred to as "white pouches" are pre-portioned pouches containing either tobacco-derived nicotine or synthetic nicotine, potentially in salt form, but no tobacco leaf, ground tobacco (i.e. dust), or tobacco stem. They are described as either similar to snus, or a tobacco-free version of snus. Non-tobacco-based nicotine pouches are commercially available, and one of the first examples of this was ZYN®, a product marked by Swedish Match® (N. Plurphanswat et al., The American Journal on Addictions, 29: 279-286, 2020; Lunell E., et al., Nicotine & Tobacco Research, 2020, 1757-1763).
[0007] Nicotine pouches have been approved by e.g. the Norwegian Medicines Agency for smoking cessation and are sold as a nicotine replacement therapy. Nicotine pouches are also increasingly used recreationally as an alternative to tobacco products such as cigarettes and snus.To use a nicotine pouch, the user puts a pouch in contact with the inside surface of the mouth, typically between the upper lip and gum, behind the lower lip or against the cheek, and leaves it there while the nicotine and taste is being released, much like portion snus. The pouch is typically kept in the mouth for a period of from five minutes to one hour and are then disposed of when finished.
[0008] Nicotine pouches are typically purchased in a ready-to-use form by the end user. Pouches are usually supplied for sale in pocket-sized containers that each hold around 20 pouches. A challenge in relation to such pouches is the avoidance of forming significant levels of unwanted substances such as tobacco-specific nitrosamines (TSNAs) during storage.
[0009] TSNAs are a group of molecules formed through nitrosation of nicotine or nicotine related substances. TSNAs comprise the most important groups of carcinogens in tobacco products, thus their formation should be eliminated wherever possible. There are some indicative limits to the N-nitrosonornicotine (NNN) and 4- methylnitrosamino)-l-(3-pyridyl)-l-butanone (NNK) amounts in smokeless tobacco products and "snusliknande" products, for example the FDA 21 CFR Part 1132 sets a limit of NNN <1 pg / g in smokeless tobacco products, and the LIVSFS 2024:2 sets a limit of NNN + NNK <2 pg / g
[0010] We have now devised a novel granulate containing nicotine or a salt thereof that has advantageous properties and addresses one or more of the challenges above.
[0011] The listing or discussion of an apparently prior-published document in this specification should not necessarily be taken as an acknowledgement that the document is part of the state of the art or is common general knowledge.
[0012] Disclosure of the Invention
[0013] According to a first aspect of the invention, there is provided a novel granulate comprising a solid, porous chemically bonded ceramic system and nicotine or a salt thereof, wherein the chemically bonded ceramic system is based on a calcium sulphate, a calcium silicate or a combination thereof, and wherein the amount of free water in the granulate is less than 1% by weight of the granulate.
[0014] These granulates are hereinafter referred to as "granulates of the invention".Granulates of the invention may be combined with other ingredients, such as flavours and pH regulating agents, to form an intraoral formulation. The intraoral formulation may be placed in a pouch (such as a permeable, sealed bag as described elsewhere herein) which can then be used by a user simply placing it in their mouth. These intraoral formulations and pouches are referred to herein as "formulations of the invention" and "pouches of the invention", respectively.
[0015] Granulates of the invention have been found to exhibit excellent stability characteristics, as shown in the examples. The granulates may be used to provide a store of nicotine for intraoral pouches, particularly fabric pouches of the sort used commercially in nicotine pouches, and these granulates and pouches are less prone to forming TSNAs during storage. Nicotine is prone to oxidation, during which the nicotine is transformed into other substances, including the 'related substances' described in the European pharmacopoeia as well as some of the tobacco specific nitrosamines (TSNAs). Some of these oxidised substances have a yellow colour and may contribute to discolouration of the granulate and / or the pouch. Without wishing to be bound by theory, it is believed that the presence of free water in the granulate contributes to, or accelerates, the oxidation of nicotine. TSNAs are a group of molecules formed through nitrosation of nicotine or nicotine related substances. TSNAs comprise the most important groups of carcinogens in tobacco products, thus their formation should be eliminated wherever possible. There are some indicative limits to the NNN and NNK amounts in smokeless tobacco products and "snusliknande" products, for example the FDA 21 CFR Part 1132 sets a limit of NNN <1 pg / g in smokeless tobacco products, and the LIVSFS 2024:2 sets a limit of NNN+NNK <2 pg / g.
[0016] We have also surprisingly found that discolouration of granulates and, in particular, pouches during normal storage is greatly reduced when the amount of free water in the granulate is reduced. Discolouration is undesirable because it reduces the product's aesthetic appeal to the end user. The reduction of the amount of free water in the granulate may allow the pouch to maintain an appearance (e.g. colour) similar to that of a freshly-manufactured nicotine pouch over a significant period of time, e.g. at least one week.
[0017] The term "free water" refers to water that is intermixed with the chemically bonded ceramic system (e.g. during its formation) and that may be removed (e.g. evaporated). The term does not include "chemically bound water" in said system.Chemically bonded ceramic systems based on a calcium sulphate, a calcium silicate or a combination thereof are typically formed using water and a suitable inorganic precursor (as is described elsewhere herein), so that the system comprise a hydrated form of calcium sulphate and / or a hydrated form of calcium silicate. Water therefore forms part of the chemical structure of these chemically bonded ceramic systems, generally through forming coordination bonds with metal ions. This water may be referred to as "chemically bound water".
[0018] Not all of the water present during the formation of the chemically bonded ceramic system will necessarily become part of the chemical structure of that system. Some of the water may instead become intermixed with the chemically bonded ceramic system. This intermixed water is typically (e.g. exclusively) located in pores and spaces of the chemically bonded ceramic system. The term "free water" may therefore be understood to refer to this water. A portion of this intermixed water can be evaporated relatively easily compared to chemically bound water, however it is also known that a portion of the water held in pores of porous materials can bind quite strongly to the pore walls and this water may thereby appear trapped in said system (e.g. in the pores of said system) because evaporation is hindered (e.g. under the conditions described herein). This water is referred to herein as "trapped water". Without wishing to be bound by theory, it is believed that this trapping occurs due to capillary forces.
[0019] The free water content in granulates may be measured by methods described elsewhere herein, such as Karl Fischer titration. These methods measure the total amount of intermixed water in the granulates, including both "trapped water" and water that is easily evaporated. For the avoidance of doubt, chemically bound water is not measured by these methods.
[0020] Granulates
[0021] Granulates of the invention comprise a chemically bonded ceramic system based on a calcium sulphate, a calcium silicate or a combination thereof and nicotine or a salt thereof. The chemically bonded ceramic system is typically formed from a precursor material (as is described hereinafter) and water. Thus, in one embodiment, the granulate of the invention comprises (or consists essentially of) a chemically bonded ceramic system based on a calcium sulphate, a calcium silicate or a combination thereof, nicotine or a salt thereof, water and optionally the precursor(s) to the chemically bonded ceramic system, though typically the amount of precursor remainingis small. In this context, the use of "consisting essentially of" will be understood to mean that the granulate may contain substances, such as flavours, that do not materially affect the release of nicotine from the granules.
[0022] The granulates are typically formed by mixing a suitable precursor material (as is described hereinafter) and water in a granulator. In one embodiment, the granulate of the invention is obtained by wet granulation. The individual granules in the granulates of the invention may be predominantly spherical or at least round in shape, and so are distinguishable from crush ceramics where the particles are more rugged. This morphology significantly enhances the flowability and packing efficiency of the material compared to powders, and particularly powders of chemically bonded ceramic systems obtained by crushing larger hardened masses of chemically bonded ceramic material. The relatively smooth, and uniform surfaces of granules (compared to powders) reduces internal friction, and allows the particles to move past each other more easily and settle into a denser, more compact arrangement.
[0023] Advantageously, at least a portion of the nicotine (or a salt thereof) may be present during the granulation (e.g. wet granulation) process so that the final granules contain both the nicotine and the chemically bonded ceramic system. When nicotine is present during the formation of the chemically bonded ceramic system, nicotine may thereby become located in pores in the chemically bonded ceramic system as is described elsewhere herein. Other salts of nicotine may also be formed in small amounts, such as nicotine sulphate in the case of a chemically bonded ceramic system based on calcium sulphate.
[0024] Production of the granulate using wet granulation has been shown to yield granulate material that is capable of providing rapid release, uptake and sensory experience of nicotine when placed in the mouth. Wet granulation also facilitates the rapid production of high volumes (i.e. greater than 1kg per batch) of granulate material under conditions that enable control of the granulate product characteristics such as granulate size and nicotine loading. Thus, in one embodiment, the granulate is obtained by wet granulation.
[0025] Granulation (e.g. wet granulation) imparts advantageous characteristics to the granulate, including increased flowability which results in the granulate being easier to handle and process; increased uniformity of the particle size distribution thus ensuring more consistent mixing of active pharmaceutical ingredients and excipients.The granulate comprising (or consisting essentially of) the chemically bonded ceramic system and nicotine (or salt thereof) may be formed by mixing together the chemically bonded ceramic material, or precursor(s) thereto, and the nicotine (or salt thereof), along with, or in, a liquid, such as an aqueous solvent (e.g. water), so providing a granulate. In this context, the use of "consisting essentially of" will be understood to mean that the granulate may contain a small amount (e.g. less than 5%, such as less than 1% by weight of the granulate) of the solid starting materials used to form the chemically bonded ceramic system, i.e. the chemically bonded ceramic precursor, in addition to the chemically bonded ceramic system, nicotine (or salt thereof) and water. The term will be understood to mean that the granulate may contain substances, such as flavours, that do not materially affect the release of nicotine from the granules. In one embodiment, the precursor for the chemically bonded ceramic system is a calcium sulphate, e.g. a calcium sulphate hemihydrate. In one embodiment, the granulate consists essentially of a solid, porous chemically bonded ceramic system (e.g. formed from a calcium sulphate), nicotine or a salt thereof and water.
[0026] The granulates of the invention comprise free water where the amount of free water in the granulate is less than 1% by weight of the granulate. In one embodiment, the granulate comprises free water where the amount of free water in the granulate is less than about 0.95%, less than about 0.9%, less than about 0.85%, less than about 0.8%, less than about 0.75%, or less than about 0.7% by weight of the granulate. In a further embodiment, the amount of free water in the granulate is less than 0.7% by weight of the granulate, preferably from 0.2% to 0.6% (most preferably 0.3% to 0.5%) by weight of the granulate. It has been found that reducing water content to this level is achievable in an efficient manner that can be used to prepare granulates at scale (e.g. in multi-kilogram batches). Furthermore, the remaining water does not appear to affect the formation ofTSNAs (or discolouration) to a significant extent. Lower water content may be achievable, but significant heating during drying has been found necessary.
[0027] The amount of free water in the granulate may be measured by techniques known in the art, including, but not limited to, IR-balance, a drying chamber or Karl-Fischer titration.
[0028] The IR-balance measuring technique, also known as infrared moisture analysis, is used to determine the moisture content of a sample by utilizing infrared radiation. In this technique, the sample is placed on a balance and exposed to infrared heat, which causes the moisture (typically free water in the granulate) within the sample toevaporate. The balance measures the weight loss of the sample as the moisture evaporates, and this change represents the amount of moisture that has been evaporated.
[0029] The drying chamber technique is used to measure water content by creating a controlled environment where the sample is dried, and the loss of moisture is determined. The process involves placing the sample in a drying chamber, which is equipped with temperature and humidity controls. The sample may be heated to accelerate moisture evaporation, but drying chambers are advantageous in that they can dry the granulate to the required degree without any need for heating. Avoiding heating minimises the risk of unwanted changes in the material, such as loss of chemically bound water from the chemically bonded ceramic system itself. Moisture is typically removed from the atmosphere by way of a dessicant, such as silica gel, in the chamber. The weight of the sample is measured before and after the drying process, and the difference in weight is used to calculate the water content.
[0030] An alternative method for measuring the free water in the granulate is the Karl Fischer water measurement method. This is a widely used technique for determining the water content in various substances. This method is based on the Karl Fischer reaction, which involves the quantitative reaction of water with iodine and sulphur dioxide in the presence of an alcohol and a base. Thus, in one embodiment, the amount of free water in the granulate of the invention is less than 1% by weight of the granulate (or any of the other values discussed herein) as measured by Karl Fischer titration.
[0031] Individual granule sizes in the granulates of the invention may vary, so granule sizes are typically described in terms of a particle size distribution. Particle size distributions obtained in the granulation process may be determined using techniques which are known to the skilled person. Suitable analytical techniques include laser diffraction techniques. Where granules are separated by sieving methods, the particle size distribution may alternatively be characterised by reference to the sieves used. Other methods include analytical sieving, e.g. according to USP<786>.
[0032] Suitable mean granule sizes in the granulates disclosed herein are in the range of about 50 to about 1000 pm (e.g. about 100 to about 1000 pm, or about 200 to about 1000 pm), which values may be determined by sieving. In one embodiment, the granulate comprises granules, and at least 50% (e.g. at least about 60%, at least about 70%, at least about 80%, or at least about 90%) by weight of said granules have a size from 200 to 1000 pm. In another embodiment, at least about 50% by weight of thechemically bonded ceramic system is provided in the form of granules having a size of from 200 to 800 pm. For the avoidance of doubt, in such embodiments, the granulate of the invention may contain granules that are larger and / or smaller than the specified range, provided the proportion (by weight) is relatively low (e.g. less than 50%, less than 40%, less than 30%, less than 20% or less than 10%).
[0033] However, if granules are too large, this can inhibit rapid nicotine release or cause difficulties with pouch loading. Thus, in yet another embodiment, at least about 50% (e.g. at least about 60%, at least about 70%, at least about 80%, or at least about 90%) by weight of the granules containing the chemically bonded ceramic have a size of from about 200 to about 900 pm (e.g. about 200 to about 800 pm).
[0034] Average granule sizes may also be described using a particle size volume distribution, e.g. when measurements are made using laser diffraction techniques.
[0035] Granules comprising the chemically bonded ceramic system and the nicotine (or salt thereof) may have a particle size distribution characterised by one or more (e.g. all) of the following:
[0036] (i) a D (v, 0.1) of at least about 200 pm,
[0037] (ii) a D (v, 0.1) of at least about 220 pm,
[0038] (iii) a D (v, 0.5) of from 250 pm to 450 pm,
[0039] (iv) a D (v, 0.5) of from 280 pm to 400 pm,
[0040] (v) a D (v, 0.9) of less than about 1000 pm, and
[0041] (vi) a D (v, 0.9) of less than about 900 pm.
[0042] According to a second aspect of the invention, there is provided a process for preparing a granulate comprising a solid, porous chemically bonded ceramic system based on a calcium sulphate, a calcium silicate or a combination thereof, and nicotine or a salt thereof;
[0043] wherein the process comprises:
[0044] (i) combining a precursor for a chemically bonded ceramic system, water and nicotine or a salt thereof in a granulator;
[0045] (ii) mixing said combination to form a granulate;
[0046] (iii) drying said granulate such that the amount of free water in the granulate is less than 1% by weight of the granulate.
[0047] In step (i), the ingredients may be combined in any order and in any form. For example, the nicotine (or salt thereof) may be supplied in the form of a solid (e.g. asolid nicotine bitartrate salt), but preferably it is supplied in the form of a solution (e.g. an aqueous solution).
[0048] Step (ii) typically comprises wet granulation as hereinbefore described. In one embodiment, the granulate obtained in step (ii) is sieved to obtain the desired size distribution before being subjected to step (iii). Sieving may be performed using any method known in the art in order to obtain a desired particle size distribution, such as one of the particle size distributions described elsewhere herein.
[0049] The granulate obtained in step (ii) will gradually harden as the chemically bonded ceramic system 'cures'. This process may take several hours, depending on the conditions. Hardening may be largely or fully completed before any sieving takes place. Alternatively, sieving may be performed before the granulate is fully hardened.
[0050] Both the timing of the drying and the degree of drying are important aspects of the present invention as both can help to reduce TSNA formation. Drying step (iii) is preferably performed after the granulate is largely or fully hardened. For example, the granulate may be left to harden for at least one hour before being subjected to drying conditions. However, shortening the time between the formation of the granulate (e.g. the hardened granulate) in step (ii) and the drying in step (iii) is believed to be advantageous. It is believed that TSNAs and other degradation products of nicotine start to form immediately after granulation, and the rate of formation slows significantly once the granulate has been sufficiently dried. It is also hypothesised that these degradation products contribute to, or induce, discolouration of granulates and pouches during storage. Thus, minimising the time period between forming the granulate and drying is believed to reduce discolouration in the final product. In one embodiment, the drying step according to step (iii) of the second invention is commenced at least one hour after the production of the granulate in step (ii). In another embodiment, the drying step according to step (iii) of the second invention is commenced up to 20 days, up to 15 days, up to 14 days, up to 13 days, up to 12 days, up to 11 days, up to 10 days, up to 9 days, up to 8 days, up to 7 days, up to 6 days, up to 5 days, up to 4 days, up to 3 days, up to 2 days or up to 1 day after the production of the granulate in step (ii). In one embodiment, the drying step according to step (iii) of the second invention is commenced not more than 7 days after the production of the granulate in step (ii). In a particular embodiment, the drying step according to step (iii) of the second invention is commenced not more than 1 day after the production of the granulate in step (ii).Drying said granulate can be performed by any drying method known to the person skilled in the art. Notable drying methods include vacuum drying, oven drying, fluid bed drying or drying at room temperature in low humidity (e.g. below 30% relative humidity, preferably below 20% relative humidity).
[0051] Vacuum drying involves drying the granulates under reduced pressure, typically in a vacuum chamber. This method lowers the boiling point of solvents, allowing them to evaporate more rapidly and / or at a lower temperature. Vacuum drying may also be carried out in combination with a heat source. As the evaporation that occurs during drying will tend to lower the temperature of the material being dried, the heat source can facilitate efficient drying by maintaining the granulate at room temperature or an elevated temperature (e.g. up to 45 °C).
[0052] Oven drying involves heating the materials, e.g. at a controlled temperature, to accelerate the evaporation of moisture. It is typically carried out using standard drying ovens known to the person skilled in the art, such as convection drying ovens or vacuum drying ovens.
[0053] In fluid bed drying, the granulates are lifted or suspended in a stream of heated air or gas. The granulates are placed on a perforated bed plate through which the air or gas is passed. The particles are lifted and agitated by the upward flow of air, creating a fluid-like state. This ensures uniform drying as the air or gas comes into direct contact with each particle, allowing efficient removal of moisture.
[0054] Vacuum drying has been found to be particularly advantageous (in comparison to other methods mentioned above) as it typically enables an adequate reduction of the water level to be achieved without a significant loss of nicotine.
[0055] Drying the granulate at room temperature in low humidity (e.g. below 30% relative humidity, preferably below 20% relative humidity) has been shown to be effective at removing free water. It has also been found that the moisture content of a dried granulate stored at around 30 % RH will not change.
[0056] A water content of around 0.3% by weight of the granulate can advantageously be achieved without the need for significant heating. Excessively heating the raw granulates to dry them may be undesirable as it can disproportionately accelerate evaporation of nicotine from the granulate. The benefit of water evaporation arisesfrom heating is likely to be outweighed by the loss of nicotine in these circumstances. Drying should hence be performed at as low temperatures as possible.
[0057] In addition, it is of high importance to ensure that any heat used during drying does not impact crystalline water in the calcium sulphate. Chemically bonded ceramic systems formed from calcium sulphate are primarily composed of calcium sulphate dihydrate, however dehydration of the dihydrate to form the hemihydrate can occur at relatively low temperatures, such as around 45 °C (Krejsova, J., eta / . Mater Struct 57, 128 (2024)). However, it has been found that granulates containing a chemically bonded ceramic system formed from calcium sulphate can retain their chemically bound water for short periods (e.g. at least up to one hour) when heated to 60 °C. For example, moisture studies have shown that the amount of water removed during drying at 60 °C over short periods was the same as that removed during drying at room temperature, indicating that chemically bound water was not being lost during drying at 60 °C.
[0058] In one embodiment, the temperature of the granulate does not exceed 60 °C, and preferably does not exceed 45 °C, during drying. In another embodiment, the temperature of the granulate is maintained at between ambient temperature and 60 °C, particularly between ambient temperature and 45 °C, during drying.
[0059] In one embodiment of the second aspect of the invention, the granulate is dried in step (iii) such that the amount of free water in the granulate is less than 0.7% by weight of the granulate, preferably from 0.2% to 0.6% by weight of the granulate.
[0060] Nicotine and Nicotine salts
[0061] The granulates of the invention are intended for use in the intraoral delivery of nicotine, which may be for therapeutic or recreational purposes. They are useful in this respect because they may be used in a pouch for releasing nicotine or a salt thereof when said pouch is placed in a user's mouth. The granulate may be used in the manufacture of intraoral pouches that offer an alternative to tobacco products (such as cigarettes and tobacco-containing snus) and so can be used to reduce a user's exposure to many of the potentially toxic components found in tobacco products. The granulates are also useful in the manufacture of products that may be useful in medicine, e.g. in nicotine replacement therapy. Nicotine is typically obtained from tobacco products, e.g. tobacco oil and other extracts. For example, the nicotine can be provided as a free base, anicotine salt (e.g., as nicotine bitartrate), as a resin complex of nicotine (e.g., nicotine polacrilex), or as a solvate or other suitable form.
[0062] The amount of nicotine (or salt thereof) present in the intraoral pouches may be varied according to its intended use and the intended release profile. As is mentioned elsewhere, the nicotine-containing granulate of the invention may be one of several components in an intraoral formulation. Typically, an intraoral formulation according to the invention comprises said nicotine or salt thereof in an amount of up to 1.67% (calculated as the nicotine free base), however higher quantities are possible. For example, the formation may comprise said nicotine or salt thereof from 0.1% to 10% (e.g. from 0.2% to 5%, such as from 0.4% to 1.67%) by weight of the formulation (calculated as the nicotine free base). For example, each individual pouches of the invention may contain nicotine or a salt thereof at from 1 to 20 mg (calculated as the nicotine free base). Larger amounts of nicotine may be incorporated into the formulations without significantly reducing the release characteristics of the formulation. In embodiments of the invention in which the intraoral formulation is provided in a pouch, each pouch may contain nicotine (or a salt thereof) in a total amount of about 1 mg, about 2 mg, about 3 mg, about 4 mg, about 5 mg, about 6 mg, about 7 mg, about 8 mg, about 9 mg, about 10 mg, about 11 mg, about 12 mg, about 13 mg, about 14 mg, about 15 mg, about 16 mg, about 17 mg and about 18 mg. For the avoidance of doubt, these values refer to nicotine calculated as the free base, regardless of the form in which the nicotine is present.
[0063] Preferably, some or all of the nicotine is present in the formulations of the invention as a water-soluble form of nicotine. In this context, the term "water-soluble form" is understood as referring to a form of nicotine having a solubility in water of at least 10 g thereof per 100 mL water under ambient conditions, including temperature of 25°C, atmospheric pressure, and pH of 7. The nicotine present in the formulations of the invention is believed to exist as an (at least largely) amorphous material, particularly when the chemically bonded ceramic system is formed in the presence of a crystalline salt of nicotine. Without wishing to be bound by theory, it is believed that the incorporation of the nicotine into the chemically bonded ceramic system helps the nicotine to dissolve (e.g. in saliva) more rapidly in use.
[0064] In one embodiment, the formulation of the invention is prepared using a salt of nicotine, such as a nicotine bitartrate salt (e.g. nicotine bitartrate dihydrate). This salt may be used as a solid or as an aqueous solution in the processes described herein. Other suitable salt forms include nicotine ascorbate, nicotine aspartate, nicotinebenzoate, nicotine monotartrate, nicotine chloride (e.g., nicotine hydrochloride and nicotine dihydrochloride), nicotine citrate, nicotine fumarate, nicotine gentisate, nicotine lactate, nicotine mucate, nicotine laurate, nicotine levulinate, nicotine malate, nicotine perchlorate, nicotine pyruvate, nicotine salicylate, nicotine sorbate, nicotine succinate, nicotine zinc chloride, nicotine sulphate, nicotine tosylate and hydrates thereof (e.g., nicotine zinc chloride monohydrate). For the avoidance of doubt, where a formulation of the invention is prepared using a salt of nicotine, the nicotine may be present in the final formulation as nicotine free base, a salt of nicotine (e.g. nicotine bitartrate) or a mixture thereof.
[0065] As is described elsewhere herein, the formulations of the invention may be used in nicotine-containing pouches, similar to snus. Snus typically contains ground tobacco. However, in particular embodiments, these pouches do not contain ground tobacco (e.g. they may not contain any particles of tobacco dust, leaf or stem). In a further embodiment, the pouches are tobacco-free. Similarly, in particular embodiments, the granulates of the invention are tobacco-free, as are mixture (e.g. formulations) containing those granulates.
[0066] Chemically bonded ceramic systems
[0067] The granulates of the invention comprise a chemically bonded ceramic system. The use of a chemically bonded ceramic system is advantageous as such systems are typically porous and those pores can store nicotine (or a salt thereof) for release in the mouth. A high degree of loading of nicotine (or a salt thereof) in pores of the chemically bonded ceramic system can be achieved whilst still enabling the granulate to release the nicotine so that it can be transported through the oral mucosa at a satisfactory rate and to a satisfactory extent once in the mouth. The granulates of the invention (as well as pouches containing the granulates) are therefore intended for intraoral use, and may be supplied to the end user in any of the final product forms described herein, particularly when combined with a pH regulating agent in cases where the chemically bonded ceramic carrier is not capable of acting as a source of alkalinity.
[0068] By the use of the term "chemically bonded ceramic system" (or similar) we refer to materials that are capable of being formed at room temperature or at slightly elevated temperature (e.g. less than about 200 °C). These systems act as carriers in the formulations of the invention as they contain pores within which the nicotine (or salt thereof) may be located.The term "chemically bonded ceramic" typically refers to a system formed from a self¬ setting precursor material. Chemically bonded ceramic systems include non-hydrated, partly hydrated or fully hydrated ceramics. Therefore, in an embodiment of the invention, the chemically bonded ceramic system in the granulate is based on a ceramic material that is formed from a self-setting precursor ceramic. Examples of chemically bonded ceramic systems include those formed from calcium sulphates, calcium silicates, and combinations thereof. Preferred granulates include those based on chemically bonded ceramic systems, which following hydration of one or more appropriate precursor substances consume a controlled amount of water to form a network. Precursor substances that may be mentioned in this respect include (CaO)3(SiC>2), (CaO CSiCh), and, particularly, calcium sulphate (e.g. calcium sulphate hemihydrate). Other chemically bonded ceramic systems may be added alongside the calcium sulphate and / or calcium silicate systems according to the first aspect of the invention. Suitable examples of other chemically bonded ceramic systems include materials which can act as a source of alkalinity, such as chemically bonded ceramic systems formed from calcium phosphates and calcium aluminates. Precursor substances that may be mentioned in this respect include CaOAhOs, (CaO)i2(Al2O3)?, (CaOXAhC ), (CaO)(Al2O3)2, alpha-tricalcium phosphate, and tetracalcium phosphate (Ca4(PO4)2O). These substances are all capable of reacting with water at room temperature to form a chemically bonded ceramic system. Water may be provided in liquid form, or the precursor substance may be exposed to a humid atmosphere for a sufficient amount of time for the material to cure and harden.
[0069] However, in a further embodiment, the chemically bonded ceramic materials in the granulate (or formulations) of the invention are not formed from calcium phosphates. In a yet further embodiment, the chemically bonded ceramic materials in the granulate (or formulations) of the invention are exclusively formed from a calcium sulphate, a calcium silicate, or a combination thereof.
[0070] In one embodiment, the water-to-cement ratio (w / c) in step (i) of the process according to the second aspect of the invention is about 0.2 to about 0.8 g / g. However, when forming granulates that comprise a chemically bonded ceramic system based on a calcium sulphate, the liquid(water)-to-cement weight ratio used in the process may be in the region of about 0.2 to about 0.4 (g / g), such as about 0.25 (g / g). In one embodiment, the water-to-cement ratio (w / c) is preferably about 0.25 to about 0.3 g / g. This ratio is lower than that typically used when working with cast calciumsulphates (i.e. when calcium sulphate hemihydrate is mixed with water to form a paste which is then hardened to form a block that is crushed to produce a powder).
[0071] Other particular systems available are those based on silicates, which consume a great amount of water. Phases such C2S and C3S in crystalline or amorphous state (C= CaO, SiOz = S, according to common cement terminology) may be used, which are readily available. The calcium silicate phases may be used as separate phases or as mixtures of phases. The above-mentioned phases, all in non-hydrated form, act as the binder phase (the cement) in the carrier when hydrated. The liquid(water)-to-cement weight ratio is typically in the region of 0.2 to 0.5, preferably in the region of 0.3 to 0.4.
[0072] The water-to-cement ratio during manufacturing, particularly for chemically bonded ceramic systems formed from calcium silicates, is important for the pore size and pore volume. If the W / C ratio is increased above the ratio that gives complete hydration, any excess water present will result in an increased pore volume and, to some extent, increased pore size. For calcium silicates, the permissible range of water content is quite wide, i.e. it is possible to increase the W / C ratio far above the theoretic value needed for complete hydration and still have a hardened body with sufficient structural integrity.
[0073] Particular materials that may be employed as the chemically bonded ceramic precursor include those based upon a sulphate, such as a calcium sulphate. Particular examples of such substances include alfa or beta phase calcium sulphate hemihydrate (the end product of which is calcium sulphate dihydrate). In one embodiment, the chemically bonded ceramic system is based on a calcium sulphate (e.g. it is formed from a calcium sulphate hemihydrate).
[0074] As will be apparent to the skilled person, the precursor(s) to the chemically bonded ceramic system may not be fully used up during the formation of the latter, and so a small proportion of the precursor(s) may remain in the final product (i.e. the granulate). For example, in embodiments in which the chemically bonded ceramic system is formed from a calcium sulphate (e.g. calcium sulphate hemihydrate), the granulate may contain a small amount of calcium sulphate hemihydrate in addition to the primary hydrated product, i.e. calcium sulphate dihydrate.
[0075] The use of the chemically bonded ceramic systems described herein may be particularly beneficial for a user's oral health because they contain calcium. Chemically bondedceramic systems that are capable of releasing calcium (e.g. in the form of solubilised calcium ions) into saliva are capable of remineralisation and so can, for example, contribute to mineral growth on the surfaces of teeth. Materials that allow excess ions (e.g. calcium ions, hydroxide ions and possibly also phosphate ions) to diffuse into surrounding saliva under physiological conditions (e.g. at the pH and temperature typically found in the mouth) may be particularly suited for this, but saliva itself can act as a source of phosphate ions so chemically bonded ceramic system that are capable of releasing calcium into saliva may thereby contribute to the growth of minerals, such as apatite, on teeth.
[0076] The intraoral formulations of the invention may contain any amount of the granulate that is sufficient to hold and deliver the intended amount of nicotine in use. In one embodiment of the invention, the granulate is present at from about 40% to about 98% (such as from about 70% to about 95%) by weight of the intraoral formulation. When the formulation is incorporated into a pouch, the granulate may be present at from about 40% to about 98% (such as from about 70% to about 95%) by weight of the contents of the pouch. The final products that are provided to users, as described elsewhere herein (e.g. nicotine pouches), typically have a mass not exceeding 2 grams, such as up to 1 g or up to 0.5 g. In an embodiment of the invention, the granulate is present at from about 40% to about 98% (such as from about 70% to about 95%) by weight of the nicotine pouch.
[0077] The chemically bonded ceramic systems used in the granulates of the invention may be loaded with nicotine or a salt thereof by first forming the chemically bonded ceramic system as a granulate (e.g. by mixing the precursor and water in a granulator). In a second step that granulate may be soaked in a liquid containing the nicotine or its salt, or the nicotine may be combined through any other method which facilitates the drawing up of that substance into the pores of the system via capillary forces (including spraying, brushing, rolling, dip coating, powder coating, misting or vacuum enhanced loading).
[0078] However, preferably the nicotine (or salt thereof) is present when the chemically bonded ceramic system granulate is formed. When compared to other loading methods such as soaking, this allows for greater control over the extent to which the pores in the chemically bonded ceramic system are filled with the nicotine, and so allows greater control over the release characteristics of the final product. In particular, this loading method enables the total amount of nicotine that is stored in, and released from, the chemically bonded ceramic system to be more reliably controlled.In examples in which the formulation of the invention also contains a pH regulating agent, it is preferred that the pH regulating agent is not present during the process of loading the chemically bonded ceramic system with nicotine (or salt thereof). The pH regulating agent may instead be added to the granulate after it is formed.
[0079] As is hereinbefore described, the chemically bonded ceramic system is formed from a suitable precursor material, such as a calcium sulphate (e.g. calcium sulphate hemihydrate), which is typically provided in a powdered form for hydration. The mean grain size of any precursor powder particles may be below about 500 pm, e.g. below about 100 pm, preferably between about 1 pm and about 30 pm. This is to enhance hydration. Such precursor material may be transformed into a nano-size microstructure during hydration (e.g. when brought into contact with liquid water or a humid atmosphere). This reaction involves dissolution of the precursor material and repeated subsequent precipitation of nano-size hydrates in the water (solution) and upon remaining non-hydrated precursor material. This reaction favourably continues until precursor materials have been transformed and / or until a pre-selected porosity determined by partial hydration using the time and temperature, as well as the H2O in liquid and / or humidity, is measured.
[0080] The total porosity of the chemically bonded ceramic system may be from about 10% to about 70%, such as from about 20% to about 40%. Porosities and average pore sizes may be measured by methods known to the skilled person, for example the mercury intrusion method, the BET (Brunauer, Emmet, and Teller) method, and N2-adsorption techniques.
[0081] In the granulates of the invention in which the nicotine (or salt thereof) is present when the chemically bonded ceramic system is formed, the nicotine (or salt thereof) may be described as being co-formedly interspersed in pores in the chemically bonded ceramic system. This means that, whatever process is employed to form the chemically bonded ceramic system, it must also necessarily form pores in which the nicotine is interspersed. Chemically bonded ceramic systems are particularly suited for this because the process by which the porous carrier (the chemically bonded ceramic system) and its pore network is formed does not require very high temperatures, in contrast to sintered ceramics.
[0082] The nicotine (or salt thereof) may be mixed with precursor(s) to the chemically bonded ceramic system using a variety of techniques, such as dry powder mixing. Wetgranulation requires mixing of the nicotine or salt thereof with precursor(s) to the chemically bonded ceramic system in a suitable liquid, as is described elsewhere herein. Alternatively, the nicotine (or salt thereof) and precursor(s) may be mixed by way of a sol-gel process, as a solution, or as a slurry, a paste or a putty of, for example, particles, granules or pellets of said precursor(s), in the presence of an appropriate liquid (e.g. an aqueous or organic solvent). This mixing step is followed by some sort of "curing" process to form the chemically bonded ceramic system, which comprises pores in which the nicotine resides. Chemically bonded ceramic systems that are formed in this way may be said to be pre-loaded with the nicotine.
[0083] The pores in the chemically bonded ceramic systems are themselves a three- dimensional network of channels or voids within the solid network, containing (e.g. particles of) nicotine or a salt thereof.
[0084] In such instances, the chemical reagents may be mixed together with the nicotine prior to or during preparation of the chemically bonded ceramic system. However, such secondary pores are not necessarily formed in this way, and bonding together of primary particles of chemically bonded ceramic material may also be physical and / or mechanical, or may be formed during the production of a three-dimensional, chemically bonded ceramic network as described hereinbefore, in the presence of the nicotine.
[0085] Preferably, the precursors for the chemically bonded ceramic system are mixed with the nicotine (or salt thereof) prior to the hardening process taking place. The nicotine is then present at the moment when pore formation occurs with the result that the nicotine becomes located in these pores of the chemically bonded ceramic system. In such systems, the chemically bonded ceramic system may be said to be formed in the presence of the nicotine or salt thereof (e.g. nicotine bitartrate or a hydrate thereof). Excellent control over the total amount of nicotine loaded into the granulate can be achieved by processing in this way. Therefore, in one embodiment, at least a portion of the nicotine (or salt thereof) is located in pores of the (hardened) chemically bonded ceramic system. By this, we mean that at least 20% (e.g. at least 30%, or at least 40%) by weight of the nicotine (or salt thereof) in the intraoral formulation of the invention is located in pores of the chemically bonded ceramic system. In another embodiment, the nicotine or salt thereof in the granulate or formulation of the invention is predominantly located in pores of the chemically bonded ceramic system. By this, we mean that at least 50% (e.g. at least 60%, at least 70%, or at least 80%) by weight of the nicotine (or salt thereof) in the granulate or formulation of the invention is located in pores of the chemically bonded ceramic system. In another embodiment,essentially all of the nicotine (or salt thereof) in the granulate or formulation is located in pores of the chemically bonded ceramic system. By this, we mean that at least 90% (e.g. at least 95%, preferably at least 98%) by weight of the nicotine (or salt thereof) in the granulate or formulation of the invention is located in pores of the chemically bonded ceramic system. In a preferred embodiment, at least 80% by weight of the nicotine or salt thereof in the granulate is located in pores in the chemically bonded ceramic system.
[0086] According to a third aspect of the invention, there is provided an intraoral formulation comprising a granulate according to the first aspect of the invention or a granulate obtainable by the process according to the second aspect of the invention. The granulate according to the first aspect of the invention or granulate obtainable by the process of the second aspect of the invention may be present in the intraoral formulation at from about 40% to about 98% by weight of the formulation.
[0087] The intraoral formulation according to the third aspect of the invention may comprise one or several additional ingredients alongside the granulate, such as a flavour or a pH regulating agent.
[0088] In one embodiment, the formulation further comprises an organic liquid, a low melting organic solid or a polymer. Said substances are referred to herein as "stabilising agents". The term "low-melting solid" in this context refers to a substance that melts at or below 50°C, e.g. at or below body temperature. For the avoidance of doubt, the stabilising agent is not nicotine and is not water. Water-miscible liquids and water- miscible low-melting solids are particularly advantageous as they are easy to process and may readily dissolve in saliva. Suitable substances are known in the art, and include propylene glycol ("PG", E1520), glycerol polyethylene glycol (PEG), triacetin, and MCT oil (medium chain triglycerides (e.g. C8-C10), typically obtained from coconut oil or palm kernel oil). Preferred molecular weights for PEG are those ranging from about 200 to about 1000 g / mol, particularly from about 200 to about 800 g / mol (e.g. from about 200 to about 400 g / mol), such as about 200 or about 400 g / mol. However, other molecular weights for PEG may be selected to achieve the desired effect.
[0089] Polymers (including co-polymers and polymer blends) may alternatively be used if they can be dissolved or suspended in volatile solvent (such as water, ethanol, propanol or similar) for use in the method of the invention. The solubility of the polymer is preferably at least 1g per 100 g solvent (e.g. at 25°C or at 50°C) to facilitate efficient and scalable manufacture. The polymer should also be permeable to nicotine to asufficient extent that, during use (i.e. following placement of the intraoral formulation in the mouth of a user), the nicotine can be released and taken up into the body. Suitable polymers for stabilising agents include polyvinyl pyrrolidone (PVP), Eudragit®, hydroxypropyl cellulose (HPC), hydroxypropyl methylcellulose (HPMC) and sodium alginate (E401). Polymers marketed under the trade mark Eudragit® are neutral methacrylic polymers with acid or alkaline groups, typically with pH-responsive properties (Eudragit® S100, a methacrylic acid-methyl methacrylate copolymer (1:2), is a suitable example). PEG with a molecular weight above 1000 g / mol (e.g. up to 2000 g / mol) may also achieve the desired effect.
[0090] In one embodiment, the organic liquid, or low melting organic solid is selected from the group consisting of propylene glycol, polyethylene glycol, triacetin and MCT oil (medium chain triglycerides), preferably propylene glycol.
[0091] The organic liquid, low melting organic solid or polymer may be mixed with the granulate using any method known in the art, e.g. through manual shaking or mechanical mixing. The amount of organic liquid, low melting organic solid or polymer present in the intraoral formulation of the invention may be between about 0.1% and about 10% (such as from about 0.3% to about 6%, e.g. from about 0.5% to about 4% or from about 1% to about 4%) by weight of the formulation. Higher amounts of said substance may be used if an adequate nicotine release profile can be maintained. This may be advantageous in helping to bind the smallest particles together to minimise the formation of fine dust, which can travel through, or block pores in, the sort of non¬ woven fabrics typically used in the manufacture of nicotine pouches.
[0092] In one embodiment of the second aspect of the invention, the method includes the step of adding a stabilising agent (e.g. propylene glycol) to the granulate of step (iii). The product thereby obtained may be described as granules coated with the stabilising agent. By this, we mean that the stabilising agent may substantially or completely cover the external surface of the granules.
[0093] pH Regulating Agent
[0094] The intraoral formulations according to the third aspect of the invention may further comprise a pH regulating agent. The addition of a pH regulating agent may enhance the rate and extent of transmucosal uptake of nicotine. Tomar S. L. et al. (Tobacco Control 1997;6:219-225) reported that increased alkalinity promotes the absorption of nicotine and increases its physiological effects. The term “pH regulating agent"refers to any substance capable of altering the pH of normal saliva at the site of absorption. Nicotine will predominantly be absorbed through the mucosa in the non¬ protonated form. Therefore, it is preferable to provide a local pH which results in a high fraction of the nicotine being non-protonated. For this reason, alkaline conditions enhance transport / uptake of nicotine across the oral mucosa and into the bloodstream, and so it is preferred that the pH regulating agent is an alkaline agent, i.e. a substance capable of increasing the pH of saliva above 7.
[0095] Suitable pH regulating agents are known to the skilled person, and particular agents that may be mentioned include sodium bicarbonate and, most particularly, sodium carbonate. These and other suitable pH regulating agents (particularly alkaline agents) are disclosed in international patent applications WO 2023 / 187223 and WO 2023 / 187224 together with methods by which these agents may be incorporated into a formulation. For example, in embodiments of the present invention that contain a pH regulating agent, the chemically bonded ceramic system is formed (i.e. allowed to harden and set) without the pH regulating agent being present. This reduces loss of nicotine during manufacture.
[0096] In an embodiment, the pH regulating agent is selected from the group consisting of carbonates (including hydrogen carbonates), silicates, aluminates, acetates, glycinates, phosphates, glycerophosphates, citrates, borates, hydroxides and mixtures thereof. Further examples of pH regulating agents that may be used include calcium aluminates, calcium silicates, calcium phosphates and calcium carbonates, as well as chemically bonded ceramic systems made from any of these calcium salts (as described elsewhere herein), and mixtures thereof.
[0097] In an embodiment of the invention, the intraoral formulation comprises said pH regulating agent in an amount of at least 0.1%, particularly at least 0.5%, by weight of the formulation. For example, the formulation may comprise said pH regulating agent (e.g. sodium carbonate or sodium bicarbonate) in an amount of from 0.1% to 20% by weight of the intraoral formulation (i.e. by weight of the pouch contents), e.g. from about 1% to about 10% by weight of the intraoral formulation (i.e. by weight of the pouch contents).
[0098] In certain embodiments in which the intraoral formulation of the invention also contains a pH regulating agent, the pH regulating agent is not present during the process of loading the chemically bonded ceramic system with nicotine (or salt thereof). In a further embodiment, the pH regulating agent is not present when the stabilising agentis mixed with the granulate. The pH regulating agent may instead be introduced into the formulation after the stabilising agent and granulate have been mixed together. Without wishing to be bound by theory, it is believed that this order of mixing may be advantageous because nicotine salts are typically more stable than nicotine in the free base form. When nicotine or a salt thereof is placed in a slightly alkaline environment, a greater proportion of the nicotine will exist in the free base form compared to nicotine in a neutral or acidic environment. By bringing the granulate and the stabilising agent together before the pH regulating agent is introduced, the nicotine (or salt thereof) is less likely to be exposed to an alkaline environment. The pH regulating agent and the one or more flavours may be added in any order.
[0099] Flavours
[0100] The intraoral formulations according to the third aspect of the invention may further comprise a flavour, optionally wherein (i) the flavour includes an ingredient selected from the group consisting of sugar, a sugar alcohol, and an artificial sweetener; and / or (ii) the flavour includes an ingredient is selected from the group consisting of menthol, peppermint, Wintergreen, sweet mint, spearmint, vanillin, chocolate, black cherry, coffee, cinnamon, clove, tobacco, citrus, fruit flavour and mixtures thereof.
[0101] In this context, the term "flavour" is used to refer to a substance that imparts a specific taste, such as a sweetener, a salt or a flavouring agent.
[0102] Sweeteners include sugars (such as sucrose, glucose, dextrose, maltose and / or fructose), sugar alcohols (such as mannitol, xylitol, sorbitol, maltitol and / or isomalt), or artificial sweeteners (such as sucralose, cyclamates, aspartame, acesulfame K and / or saccharin). Sweeteners are particularly useful for masking the taste of the nicotine in the formulation. Such sweeteners may be present in an amount of at least 0.1%, and preferably not more than 5%, by weight of the intraoral formulation of the invention.
[0103] Flavouring agents that may be used include menthol, peppermint, Wintergreen, sweet mint, spearmint, vanillin, chocolate, black cherry, coffee, cinnamon, clove, tobacco, citrus, fruit flavour and mixtures thereof. In one embodiment, the flavouring agent is not tobacco. The formulations of the invention may be used with any flavour or combination of flavours. Such flavours may each be present in an amount of at least 0.1%, and preferably not more than 10% (e.g. not more than 5%), by weight of the formulation of the invention.Substances that give a cooling mouthfeel, such as sugar alcohols (e.g. erythritol), may be used in the intraoral pouches disclosed herein.
[0104] Other flavours that may be used include sialagogues such as salt (NaCI). Sialagogues are advantageous because they increase saliva production. Other such substances are known in the art, including sweeteners (e.g. xylitol) and acidic substances (such as malic acid and ascorbic acid). Thus, in a further embodiment, the formulation of the invention includes a sialagogue. The nicotine in the granulate and elsewhere in the formulation is able to dissolve in saliva and is then be absorbed through the oral mucosa. Flavouring agents in the formulation are also transported by saliva to taste buds in the oral cavity. The incorporation of a substance that increases saliva production improves the experience for the user by ensuring that the sensations arising from the nicotine and flavouring agents in the product can occur more quickly. A sialagogue may be present in an amount of at least 0.1%, and preferably not more than 5%, by weight of the formulation.
[0105] Intraoral formulations of the invention may also contain one or more preservatives. Substances that may be used as preservatives include sodium benzoate and potassium sorbate as well as other substances known in the art to have similar functionality.
[0106] In embodiments in which multiple flavours are present, the flavours (as well as any pH regulating agent or preservative that may be present) may be added together or separately, and may be added in any order. Each such component may be individually provided as a dry solid, a liquid, or a solution. For example, some flavouring agents are typically sourced as a mixture with glycerol.
[0107] In a particular embodiment, the formulation of the invention comprises nicotine or a salt thereof, a chemically bonded ceramic system, a pH regulating agent, a sweetener, a sialagogue, and one or more flavouring agents. Furthermore, the formulation is obtainable by (or obtained by) the method of the second aspect of the invention.
[0108] In a further particular embodiment, the formulation of the invention comprises nicotine or a salt thereof, a chemically bonded ceramic system, sodium carbonate, acesulfame-K, sodium chloride, and one or more flavouring agents. In a particular embodiment, the chemically bonded ceramic system is formed from a calcium sulphate hemihydrate precursor.Nicotine pouches
[0109] The granulates and intraoral formulations of the invention are capable of providing both immediate and sustained release of nicotine, but are particularly suited for products (e.g. nicotine pouches) intended for slow and / or sustained nicotine release upon exposure to moisture in the mouth. The intraoral formulations may therefore be used in the manufacture of final products, such as nicotine pouches (similar to snus).
[0110] Intraoral formulations that are capable of providing a sustained release of nicotine allow the user to obtain a long-lasting sensory experience using a minimal number of formulations per day. Where the intraoral formulation is intended to be used as part of a therapeutic method of treating nicotine dependence, this characteristic improves patient compliance and minimises interference with the individual's lifestyle.
[0111] The intraoral formulations of the invention are particularly suited for transmucosal administration whereby the formulation (e.g. in a pouch) is placed in contact with the lip, gum or cheek for an extended period (several minutes) while the nicotine is released. As increased alkalinity in saliva enhances the rate and extent of transmucosal uptake of nicotine, the formulation of the invention is preferably able to give a pH of at least 8 upon contact with saliva.
[0112] The terms "pouch" and "nicotine pouch" as used herein refer to a pouch or bag that is fully or partially loaded with an intraoral formulation of the invention. A nicotine pouch containing the intraoral formulation of the invention may be described as a tobacco- free version of snus. In such systems, the pouch or bag contains a specific amount of the formulation, and thereby a specific amount of nicotine, but typically does not include any tobacco dust, leaf or stem.
[0113] In one embodiment, the formulation is designed to release at least 50% by weight of the nicotine within a period of 30 minutes when in contact with oral saliva. The formulations of the invention may also be capable of increasing the concentration of nicotine in the blood plasma of an average subject by at least 3 ng / mL when held in the subject’s mouth for a period of 30 minutes.
[0114] The intraoral formulations of the invention may be capable of achieving a nearly constant rate of release over an interval of from about 10 minutes to about 1 hour, potentially longer. In one embodiment, the granulates and formulations are capable of achieving a nearly constant rate of uptake over an interval of from about 10 to 30minutes. What is meant by this is that nicotine release from the product continually occurs (at a non-zero rate) over the specified time interval. Constant release may further be defined as a granulate or formulation being capable of maintaining a steady state concentration in a body fluid not deviating more than about 20% (e.g. about 10%) from the mean value during the dose interval.
[0115] The intraoral formulations of the invention, when held in the mouth, may advantageously be capable of releasing a relatively high proportion of the material held in the pores. By this we mean that, when the intraoral formulation is held in the mouth for an extended period of time (e.g. at least 10 minutes or preferably at least 20 minutes or at least 30 minutes), at least 30% (e.g. at least 40%, or at least 50%) of the nicotine stored in the pores of the chemically bonded ceramic system is released (from said pores) and made available for absorption across the mucosa to the user. This characteristic allows the user to know more accurately how much nicotine is absorbed into the body, which may be advantageous when dosing a patient for therapeutic purposes.
[0116] The term "sustained-release" is employed herein synonymously with the term "controlled-release", and will be understood by the skilled person to include formulations that provide, and / or are adapted to provide, for a "sustained", a "prolonged" and / or an "extended" release of nicotine (in which nicotine is released at a sufficiently retarded rate to produce a therapeutic response or give a pleasurable experience over an extended period of time compared to pouch formulations currently on the market).
[0117] The total amount of nicotine that is delivered by a single pouch during use is preferably from about 0.5 mg to about 20 mg, 0.5 mg to about 18 mg, e.g. from about 1 mg to about 10 mg. For example, a single pouch may deliver from about 1 mg to about 8 mg, from about 1.5 mg to about 7.5 mg, from about 2 mg to about 5 mg, from about 2.5 mg to about 5 mg, from about 3 to about 10 mg, from about 3 to about 7.5 mg or from about 3 mg to about 5 mg nicotine to the user. The above values refer to the amount of nicotine in the free base form that can be delivered from each pouch, irrespective of whether the nicotine is present as the free base, a salt, a mixture thereof, or in any other form. The amount of nicotine released from a used pouch can be determined by determining the amount of nicotine contained in the pouch both prior to, and after, use.The intraoral formulations of the invention are suitable for use in conventionally sized nicotine pouches that are intended to be used by holding the pouch in the mouth under the lip. Typically, such pouches are rectangular and have a length of about 25 to about 35 mm, and a width of about 10 to about 15 mm.
[0118] The granulates of the invention may also provide a relatively concentrated form of nicotine, thus enabling the manufacture of small pouches that still contain a conventional amount of nicotine and have advantageous release properties as described herein. Formulations of the invention may contain at least 5 mg (such as least 10 mg, at least 20 mg or at least 30 mg) nicotine (calculated as the free base) per gram of formulation. By way of an example, 15 mg of nicotine (calculated as free base) may be incorporated into a chemically bonded ceramic system to give a granulate with a total mass of up to 0.6 g (e.g. from 0.4 g to 0.6 g), preferably no more than 0.4 g. In this context, small pouches may have no dimension larger than about 25 mm, preferably no dimension larger than about 21 mm. Typically, small pouches are rectangular and have a length of about 10 to about 15 mm, and a width of about 8 to about 10 mm. Larger pouches may be about 28 mm in length and may contain between 0.7 and 0.9 g of the formulation. Unless otherwise specified, pouches typically have a width of about 14-15 mm. In one embodiment, pouches are rectangular and have dimensions of about 21 mm and about 15 mm, and optionally contain about 0.4 g of the formulation.
[0119] The amount of nicotine contained in the intraoral formulation prior to use may exceed the amount of nicotine that is intended to be delivered to the user. This is because a proportion of the nicotine may be trapped in the chemically bonded ceramic system in such a way that complete release of the nicotine is not possible within the likely time period of use. However, preferably the intraoral formulation is capable of releasing substantially all of the nicotine or salt thereof upon contact with an aqueous liquid (e.g. saliva). By this, we mean that, upon contact with an aqueous liquid, the intraoral formulation is capable of releasing at least 80% (e.g. at least 90%) by weight of the nicotine or salt thereof.
[0120] In a fourth aspect, the invention relates to a permeable, sealed bag containing a granulate according to the first aspect of the invention or an intraoral formulation according to the third aspect of the invention. Such a product may be referred to as a "nicotine pouch". The bag is typically made of a permeable material that encloses a cavity. The intraoral formulation is held in the cavity, and soluble components of the formulation are able to pass through the bag material when the bag is exposed towater (e.g. saliva). Suitable materials for nicotine pouches are known to the skilled person, and include paper of the sort used in tea bags, filter paper, and the like. Other materials include heat-sealable non-woven cellulose, such as long fiber paper, cotton, silk and vinyl-based plastics. In one embodiment, the bag material is a cellulose-based product, e.g. a non-woven cellulose-based fabric.
[0121] Although, in some embodiments, the formulation within the nicotine pouch contains a pH regulating agent, a quantity of pH regulating agent may alternatively or additionally be present and associated with the bag material itself. For example, particles of a pH regulating agent (e.g. sodium carbonate and / or sodium bicarbonate) may be embedded within the permeable material of the bag so that this pH regulating agent is readily able to dissolve upon contact with saliva. The pH regulating agent associated with the bag material may be the same as or different from any pH regulating agent in the formulation.
[0122] For the avoidance of doubt, it is not essential for all of the nicotine in the final product to be located in pores of the chemically bonded ceramic system. Some of the nicotine may be located outside of the pores. For example, where the final product is a pouch containing the intraoral formulation, a portion of the nicotine (e.g. from 1 to 50%, from 5 to 40% or from 10 to 30% by weight of the total amount of nicotine (or salt thereof) in the final product) may be mixed with granulated chemically bonded ceramic system (which may itself comprise pores containing an amount of nicotine or salt thereof) prior to being placed in the pouch.
[0123] In a further example, where the final product is provided in the form of a pouch containing the formulation, a portion of the nicotine in the product may be associated with the material that forms the pouch, i.e. a portion of the nicotine (e.g. from 0.1 to 30%, from 0.5 to 20% or from 1 to 10% by weight of the total amount of nicotine (or salt thereof) in the final product) is not located within the cavity of the bag (as is described elsewhere herein) but is instead bound to or incorporated within the walls of the bag itself. This may be achieved e.g. by soaking the pouch material in a solution containing nicotine (as base or dissolved nicotine salt) and then allowing the solvent (e.g. water or another appropriate solvent) to evaporate leaving nicotine or a salt thereof incorporated into the pouch material.
[0124] In an embodiment of the invention in which the intraoral formulation is contained within a pouch, the total weight of the loaded pouch is from 0.2 to 3 g, such as from 0.4 to 2 g. In another embodiment, the nicotine pouch has a weight and / or volume similar tocommercially available portion snus products and nicotine pouches. In a further embodiment of the invention, the formulation is contained within a small pouch having a total weight of from 0.1 to 0.7 g, (e.g. from 0.1 to 0.5 g, such as from 0.1 to 0.4 g). Small pouches are discussed elsewhere herein and the utility of such low weight products is possible thanks to the fact that the chemically bonded ceramic systems referred to herein are capable of providing a very compact and stable storage of nicotine whilst maintaining a suitable release profile.
[0125] Nicotine pouches may be manufactured using methods known to those skilled in the art, particularly those methods used for the manufacture of snus and commercially available nicotine pouches (such as ZYN®). For example, the contents for the pouch (i.e. the intraoral formulation of the invention) may be made using the methods described herein, and the formulation may then be then loaded into sealable bags, e.g. heat-sealable bags. Such bags should be water insoluble and permeable to saliva. Suitable materials for nicotine pouches are described hereinbefore, and are also known to the skilled person, for example from US patent no. 9,161,908. Heat-sealable non¬ woven cellulose, such as long fiber paper, offers a particularly suitable material for use in nicotine pouches. Typically, pouches are prepared from a ribbon of material by folding and partially-sealing (e.g. heat-sealing) the ribbon so as to form an open pouch. Once a prescribed amount of the granulate-containing formulation is filled into the open pouch (e.g. by way of a gravity-fed loading process), it is maintained in the pouch by sealing (e.g. heat-sealing) the opening. Thus, in a further embodiment of the second aspect of the invention, the method further comprises the step of loading the granulate into a bag (e.g. a heat-sealable non-woven cellulose pouch) and sealing said bag.
[0126] TSNAs are potent carcinogens and their formation is consequently undesirable.
[0127] Granulates of the invention have been shown to be less prone to the production of TSNAs compared to granulates that contain higher amounts of free water. This improvement is demonstrated in the following examples where lower TSNA levels are measured for the granulates of the invention after several weeks of storage. Without wishing to be bound by theory, it is believed that TSNA formation arises, in part, as a result of oxidation of the nicotine. It is also believed that free water in the granulate accelerates the oxidation of nicotine. Thus, drying the granulate sufficiently rapidly and / or thoroughly after its formation reduces the amount of free water therein, and thereby reduces the rate of TSNA formation during storage.In one embodiment, granulates of the invention produce TSNAs (e.g. NNN or NNK) at a reduced rate compared to a similar nicotine granulate (i.e. comprising the same solid, porous chemically bonded ceramic system and the same form of nicotine) and that has not been dried after manufacture. Such a reduction may be detectable by measuring TSNA levels in the granulate after storage for a period of at least 1 week (e.g. at least 2 weeks, at least 3 weeks, at least 4 weeks, at least 6 weeks, at least 10 weeks, at least 11 weeks, or at least 12 weeks) under ambient temperature and atmospheric conditions (e.g. in the absence of light). Granulates of the invention may also be characterised on the basis of their TSNA content after storage. For example, granulates of the invention may be characterised as containing a lower amount of TSNAs (e.g. NNN or NNK) after storage for at least 1 week (e.g. at least 2 weeks, at least 3 weeks, at least 4 weeks, at least 6 weeks, at least 10 weeks, at least 11 weeks, or at least 12 weeks) under the above-mentioned conditions when compared to a similar nicotine granulate that is not dried after manufacture.
[0128] In one embodiment, after 6 weeks of storage, the TSNA content of a granulate (or formulation) of the invention may be 20% lower (e.g. 50% lower) than the TSNA content of a similar nicotine granulate that is not dried after manufacture. Alternatively, or additionally, after 11 weeks of storage, the TSNA content of a granulate (or formulation) of the invention may be 60% lower (e.g. 90% lower) than the TSNA content of a similar nicotine granulate that is not dried after manufacture.
[0129] TSNA levels may be measured using the techniques described elsewhere herein, e.g. using LC-MS / MS.
[0130] Discolouration of nicotine pouches is an unwanted change that reduces the visual appeal of the product for the end user. Pouches containing granulates of the invention have been shown to have enhanced stability in this respect compared to pouches containing granulates that comprise higher amounts of free water. This enhanced stability is demonstrated in the following examples where yellowing is shown to be reduced in pouches containing the granulates of the invention. Without wishing to be bound by theory, it is believed that yellowing arises, in part, as a result of oxidation of the nicotine. It is also believed that free water in the granulate accelerates the oxidation of nicotine. Thus, drying the granulate sufficiently rapidly and / or thoroughly after its formation reduces the amount of free water therein, and thereby reduces the extent to which nicotine is oxidised. In turn, discolouration of filled pouches during storage is reduced, and the shelf-life of the product is extended.In one embodiment, changes in the appearance (e.g. colour) of a nicotine pouch containing a granulate of the invention during storage are reduced compared to a pouch containing a nicotine granulate that has not been dried to the same extent. Such a reduction may be detectable when the storage is for a period of at least 1 day (e.g. at least 2 days, at least 3 days, at least 4 days, at least 5 days, at least 6 days or at least 7 days, at least 2 weeks, at least 3 weeks, at least 4 weeks, at least 6 weeks, or at least 8 weeks) under ambient temperature and atmospheric conditions (e.g. in the absence of light).
[0131] Changes in colour may be measured using the techniques described elsewhere herein, e.g. in the Examples. In one embodiment, the colour change of a nicotine pouch containing a formulation of the invention during storage as measured using such methods may be reduced by at least around 20%, such as by at least around 50%.
[0132] Furthermore, the granulates and formulations of the invention are advantageous as they provide a safe storage means for nicotine (or a salt thereof). Pure nicotine is classified as having acute toxicity and it is a skin and eye irritant. Manufacture and handling of pure nicotine is challenging and end-user products which risk exposing the user to the liquid during use (e.g. during refilling) are highly undesirable. The granulates and formulations of the invention overcome these risks by providing a diluted, solid form of nicotine. In this form, the nicotine can be handled easily and the risk of the user being exposed to the nicotine is greatly reduced. The granulates and formulations of the invention also have an improved safety profile over other solid forms of nicotine, such as nicotine-loaded microcrystalline cellulose as the latter is prone to releasing the nicotine (often in salt form) as a dust. In contrast, the granulates and formulations of the invention are much more effective at binding the nicotine in the carrier to avoid release prior to the intended time.
[0133] Unless the context clearly requires otherwise, throughout the description and the claims, the words "comprise", "comprising", and the like are to be construed in an inclusive sense as opposed to an exclusive or exhaustive sense; that is to say, in the sense of "including, but not limited to".
[0134] The term 'consisting essentially of' will be understood to mean that the scope of this (and only this) aspect of the invention is limited to the specified essential features mentioned immediately thereafter, along with other features that do not materially affect the basic and novel characteristic(s) of this aspect of the invention.Wherever the word "about" is employed herein in the context of dimensions (e.g. values, temperatures, pressures (exerted forces), relative humidities, sizes and weights, particle or grain sizes, pore sizes, timeframes etc.), amounts (e.g. relative amounts (e.g. numbers or percentages) of particles, individual constituents in a formulation or a component of a formulation and absolute amounts, such as amount of nicotine, numbers of particles, etc.), deviations (from constants, degrees of degradation, etc.) it will be appreciated that such variables are approximate and as such may vary by ± 10%, for example ± 5% and preferably ± 2% (e.g. ± 1%) from the numbers specified herein.
[0135] Figures
[0136] Figure 1 shows the colour changes during storage for pouches tested according to Example 7a;
[0137] Figure 2 shows the colour changes during storage for pouches tested according to Example 7b.
[0138] Examples
[0139] Example 1 - Preparation of Strong Nicotine Granulate (Granulate Batch 1)
[0140] A nicotine-loaded granulate formed from calcium sulphate was made by the following method.
[0141] Materials
[0142] USP grade nicotine bitartrate dihydrate
[0143] water
[0144] (CSH) BP, DAB grade calcium sulphate hemihydrate
[0145] Manufacturing of CBC-based nicotine pouches
[0146] The manufacturing was made in steps first producing a nicotine-containing chemically bonded ceramic (CBC) granulate which is then dried and sieved. The quantity of nicotine used was chosen to produce a granulate that contained approximately 30 mg of nicotine per gram of granulate.Step 1:
[0147] 249 g of nicotine bitartrate dihydrate was dissolved in 555 ml of water. 2300 g of calcium sulphate hemihydrate was weighed into the steel drum of an intensive mixer type granulator. The granulator was started at a speed of 16 m / s (Speed setting I for both mixing arm and drum) and the nicotine / water solution was poured in during 20 s. The granulator was on for another 160 s whereafter the granulator was turned off and the granulate poured out onto a stainless-steel tray. The granulate was left to cool off until the temperature in the granulate was below 25 °C.
[0148] Step 2:
[0149] The granulate was left to harden over two nights in an environment where the relative humidity was low (approximately 14%).
[0150] Step 3:
[0151] The dried granulate was sieved using a "ZEUS" Industrial circular sieve shaker FTI-0550 A to obtain granules ("nicotine granules") in the range of 200 - 710 pm.
[0152] Example 2 - Preparation of Strong Nicotine Granulate (Granulate Batch 2)
[0153] A nicotine-loaded granulate formed from calcium sulphate was made by the following method (same ingredients as Example 1). The quantity of nicotine used was chosen to produce a granulate that contained approximately 30 mg of nicotine per gram of granulate.
[0154] Step 1:
[0155] 249 g of nicotine bitartrate dihydrate was dissolved in approx. 540 ml of water. 2300 g of calcium sulphate hemihydrate was weighed into the steel drum of an intensive mixer type granulator. The granulator was started at a speed of 16 m / s (Speed setting I for both mixing arm and drum) and the nicotine / water solution was poured in during 20 s. The granulator was on for another 160 s whereafter the granulator was turned off and the granulate poured out onto a stainless-steel tray. The granulate was left to cool off until the temperature in the granulate was below 25 °C.
[0156] Step 2:
[0157] The granulate was sieved using a "ZEUS" Industrial circular sieve shaker FTI-0550 A to obtain granules ("nicotine granules") in the range of 200 - 710 pm. The granulate was then stored for 20 days in a closed polyethene container in a fridge at around 4-8 °C.Step 3:
[0158] Half of the sieved nicotine granulate obtained in step 2 was dried in a convection oven at room temperature overnight. The other half of the sieved nicotine granulate was kept undried for analysis of the nicotine and moisture content.
[0159] Example 3 - Preparation of 15 mg / g Nicotine Granulate (Batch 3)
[0160] A nicotine-loaded granulate formed from calcium sulphate was made by the following method (same ingredients as Example 1). The quantity of nicotine used was chosen to produce a granulate that contained approximately 15 mg of nicotine per gram of granulate.
[0161] Step 1:
[0162] 152 g of nicotine bitartrate dihydrate was dissolved in approx. 535 ml of water. 2300 g of calcium sulphate hemihydrate was weighed into the steel drum of an intensive mixer type granulator. The granulator was started at a speed of 16 m / s (Speed setting I for both mixing arm and drum) and the nicotine / water solution was poured in during 20 s. The granulator was on for another 160 s whereafter the granulator was turned off and the granulate poured out onto a stainless-steel tray. The granulate was left to cool off until the temperature in the granulate was below 25 °C.
[0163] Step 2:
[0164] The granulate was sieved using a Retsch® AS 200 Basic sieve shaker stack with certified analytical sieves to obtain granules ("nicotine granules") in the range of 200 - 710 pm.
[0165] Step 3:
[0166] Following a 10-day storage period, the sieved nicotine granules obtained in step 2, were dried in a convection oven, set at 30°C, for up to 24 hours. After 0, 1, 2 and 3 hours of drying, samples were collected for analysis.
[0167] Comparative Example 4 - Preparation of Undried 30 mg / g Nicotine Granulate (Batch 4)
[0168] A nicotine-loaded granulate formed from calcium sulphate was made by the following method which did not include a drying step (same ingredients as Example 1). The quantity of nicotine used was chosen to produce a granulate that contained approximately 30 mg of nicotine per gram of granulate.Step 1:
[0169] 249 g of nicotine bitartrate dihydrate was dissolved in 565 ml of water. 2300 g of calcium sulphate hemihydrate was weighed into the steel drum of an intensive mixer type granulator. The granulator was started at a speed of 16 m / s (Speed setting I for both mixing arm and drum) and the nicotine / water solution was poured in during 20 s. The granulator was on for another 160 s whereafter the granulator was turned off and the granulate poured out onto a stainless-steel tray. The granulate was left to cool off until the temperature in the granulate was below 25 °C.
[0170] Step 2:
[0171] The granulate was sieved using a "ZEUS" Industrial circular sieve shaker FTI-0550 A to obtain granules ("nicotine granules") in the range of 200 - 710 pm.
[0172] The sieved nicotine granulate was kept undried for analysis of the nicotine and moisture content.
[0173] Comparative Example 5 - Open Air Curing (Batch 5)
[0174] Nicotine bitartrate water solution was granulated together with calcium sulphate hemihydrate powder to form nicotine granules with a nicotine concentration of around 16-17 mg / g. The corresponding amounts were as follows:
[0175] Nicotine bitartrate: 1679 g
[0176] Water: 6341 g
[0177] Calcium sulfate hemihydrate (CASH): 25000 g
[0178] The granulation was preformed using a high speed granulator (maximum filling volume: 40 L). First, the CASH powder was added to the granulator and the granulator was started. The liquid was added to the container at a steady rate for approximately 65 seconds after which the high-speed mixing was continued for approximately another 160 seconds.
[0179] The finished product was placed on metallic trays and left under ambient conditions for 24 hours for final curing.
[0180] Example 6 - Nicotine measurement
[0181] The nicotine content of the granulates of the preceding examples was measured using HPLC-UV in water. Briefly, 0.10-0.15 g of the nicotine granulate, as prepared inExamples 1, 2 and 3 was dispersed in 50 mL distilled water and stirred at 360 rpm for 30 minutes. An aliquot (1.5 mL) was added to an HPLC vial, and the same was analysed. The UV absorption at 254 nm was detected and allowed the nicotine concentration to be determined using a reference standard. Results are in Table 1.
[0182] Table 1 - nicotine content of batch 1 and 2 nicotine granulates
[0183] Granulate Batch Nicotine Content (mg / g) 1 28.3
[0184] 2 (undried) 27.7
[0185] 2 (dried) 26.0
[0186] 4 28.9
[0187]
[0188] The results outlined in Table 1 show that the nicotine content was between 25-30 mg / g.
[0189] The nicotine content was also measured for each of the samples of batch 3 taken after 0, 1, 2 and 3 hours of drying, according to the method of Example 3. The measurement was taken immediately after drying. Results are in Table 2.
[0190] Table 2 - nicotine content of batch 3 nicotine granulates
[0191] Drying time (h) Nicotine Content (mg / g) 0 9.326
[0192] 1 8.413
[0193] 2 8.450
[0194] 3 7.750
[0195]
[0196] The data shows that minimal changes in the nicotine content occur during drying.
[0197] Example 7 - Moisture measurement
[0198] The moisture content of the nicotine granulates prepared in Examples 1, 2, 3 and 5 was measured. Moisture measurements were made using either an IR-balance or a drying chamber. For IR balance measurements, the granulate was slowly heated to 60°C, and the weight change was monitored in real time. The sample was heated until the weight change stabilised (which typically required 5 to 10 minutes). The percentage of free water in the granulate was calculated using the following equation:
[0199] [Weight loss]
[0200] % Free water in granulate = 100% x - - - - - — - [Initial granulate weight]For measurements in a drying chamber, the granulate was placed in a chamber with silica gel and the weight change after 48 hours was noted. Both methods have been shown to give the same results.
[0201] Batch 1 moisture measurements were made 6-7 weeks after drying. Batch 2 and 5 moisture measurements were made within 24 hours of drying. For batch 5, three samples were taken from one tray, one from the right, left and middle of the tray, and all were collected from the top of the tray. Typical moisture content following 5 weeks of storage with no drying is 2-5%. Results are in Table 3.
[0202] Table 3 - Summary of the moisture content of batch 1 and 2 nicotine granulates.
[0203] Granulate Batch Moisture Content (wt%) 1 0.54
[0204] 2 (undried) 3.89
[0205] 2 (dried) 0.34
[0206] 5 (open air curing) 3.17, 2.55, 3.58 (individual measurements)
[0207] 3.1 ± 0.5 (average)
[0208]
[0209] The results outlined in Table 3 show that the moisture content of dried granules was below 0.6%.
[0210] The moisture content was also measured for each of the samples of batch 3 nicotine granulates taken after 0, 1, 2 and 3 hours of drying. The measurement was taken using an IR-balance immediately after drying. Results are in Table 4.
[0211] Table 4 - Summary of the moisture content of batch 3 nicotine granulates measured.
[0212] Drying time (h) Moisture Content (wt%) 0 2.02
[0213] 1 1.36
[0214] 2 0.70
[0215] 3 0.35
[0216]
[0217] The results show that within 2 hours, the moisture content was below 1% and within 3 hours the moisture content was below 0.5%.Example 8 - Filled Pouches
[0218] Nicotine granulates made in each of Examples 1 to 4 were mixed with other ingredients according to the two recipes in Table 5 to form two powder formulations for each granulate batch - one designated MINT, and one designated CITRUS.
[0219] Table 5 - Recipes for Pouch Contents
[0220] Ingredient Mass (g)
[0221] MINT CITRUS
[0222] Nicotine granules 50 50
[0223] NazCOs 2.5 2.5
[0224] NaCI 1 1
[0225] Acesulfa me-K 0.2 0.2
[0226] Aroma ICE COOL 1.6 - Aroma CHINESE QUINCE - 1.6
[0227] Aroma COOLING 0.5 0.5
[0228] Aroma PEPPERMINT 0.5 0.5
[0229]
[0230] The ingredients were combined, and the mixture was homogenized by Turbula mixing for 30 minutes at 50 rpm, before the granule powder was pouched into nicotine pouches (width: approx. 13-14 mm; length: approx. 25 mm). Pouches were made of non-woven cellulose material containing a binder to facilitate sealing by heat-welding.
[0231] Example 9 - Discolouration testing
[0232] The pouches of Example 8 were stored for 8 weeks. The pouch appearance was recorded immediately following preparation (0 weeks) and again after 2, 4, 6 and 8 weeks of storage.
[0233] Storage
[0234] The pouches were placed into plastic, cylindrical storage cans. The storage can dimensions were 67 mm (diameter) and 16 mm (height). Each can contained at least 5 pouches in a randomly scattered orientation.
[0235] The storage cans were kept closed (i.e. no light exposure) and stored at room¬ temperature (around 20 °C) and with an ambient atmosphere between measurements.Cans were opened at each test-point (start and 2, 4, 6 and 8 weeks) for colour measurements.
[0236] Analysis
[0237] The appearance of the pouches in each can was recorded in images taken using a Lightbox Ortospectra OS60-4 (setting D - daylight). Images were subjected to colour scoring analysis.
[0238] Colour Scoring
[0239] Once all images had been obtained, an average colour measurement was determined for each test batch at each time point according to the following method.
[0240] As yellowing occurred most strongly at the seams, only the end-seams of the pouches were analysed. Within each study, the images (figures 1 and 2) obtained at all time points were taken together, and the pouch region with the darkest yellow colour across all images was identified by eye to determine the maximum colour score. The RGB24 colour for that region / pixel was determined by identifying the pixel colour on a digital colour palate. The average RGB24 colour for freshly-sealed pouches (i.e. the starting colour) was similarly determined using only the time-zero images. These two colours (i.e. the darkest yellow colour and the starting colour) were designated scores of "10" and "0" respectively. When mapped on a colour chart, the yellow colours for the test pouches all fell on the colour chart between these two extreme colours, so the colourspace between these extremes was divided into equal-sized regions to enable scores spanning 0 to 10 to be assigned accordingly. A single yellowness score for each image was then obtained by assigning a yellowness score to a representative region / spot of each observable seam in each image and then determining the median score. Table 6 summarises the discolouration scoring for pouches made with granulates of batches 1 and 4. Table 7 summarises the discolouration scoring for pouches prepared using batch 2 granulates, both dried and undried.
[0241] Table 6 - discolouration scores for batches 1 and 4
[0242] Pouch containing Batch 4 Pouch containing Batch 1
[0243] Mint Citrus Mint Citrus
[0244] 0 weeks 0 0 0 0
[0245] 8 weeks 9 9 1 1
[0246]
[0247] Table 7 - discolouration scores for batch 2 (dried and undried)
[0248] Batch 2 - undried Batch 2 - dried
[0249] Mint Citrus Mint Citrus
[0250] 0 weeks 0 0 0 0
[0251] 8 weeks 10 10 3 4
[0252]
[0253] These data show that discolouration of the pouches is significantly reduced when the granulate has been dried.
[0254] The result observed for batch 1 was particularly surprising because discolouration is normally obvious after 2-4 weeks in pouches containing approx. 30 mg / g nicotine where no drying has taken place.
[0255] Example 10 - Tobacco specific nitrosamines (TSNA) measurements
[0256] Samples were analysed for their TSNA content using LC-MS / MS. The analysis was performed by Eurofins Food and Feed Testing Sweden (Lidkbping).
[0257] In the following discussion:
[0258] NNN is N-nitrosonornicotine
[0259] NNK is 4-methylnitrosamino)-l-(3-pyridyl)-l-butanone
[0260] Nicotine granulate of batch 1, prepared according to Example 1, had a NNN content of <0.01 pg / g (estimated to be 0.0016 pg / g). At the date of testing the granulate was approximately 6 weeks old.
[0261] TSNA content was not measured for formulations containing batch 2 nicotine granulates. Prior analyses of formulations containing nicotine granulates made analogously to batch 4 (i.e. without drying) have shown that, after six weeks of storage, the NNN content is typically between 0.01 and 0.05 pg / g.
[0262] The TSNA content was also measured for each of the samples of batch 3 nicotine granulate taken after 0, 1, 2 and 3 hours of drying. Separate measurements were taken approximately 6 and 11 weeks after drying. Table 8 Summarises the TSNA content of batch 3 nicotine granulates.Table 8 - TSNA content of batch 3 nicotine granulates
[0263] Drying time (h) 6 weeks 11 weeks
[0264] NNN NNK NNN NNK
[0265] (pg / g) (pg / g) (pg / g) (pg / g)
[0266] 0 0.0520 0.0051 0.1300 0.0130
[0267] 1 0.0530 0.0100 0.0780 0.0130
[0268] 2 0.0050 0.0038 0.0059 0.0045
[0269] 3 0.0055 0.0033 0.0055 0.0050
[0270]
[0271] The results presented herein indicate that drying of the nicotine granulate both decreases the amount of TSNAs in the material and reduces the discolouration of the final product. The results further indicate that immediate drying is preferred over drying after 10-20 days. It seems that TSNAs start to form immediately after granulation and only stops or slows down when the material is sufficiently dried.
Claims
Claims1. A granulate comprising a solid, porous chemically bonded ceramic system and nicotine or a salt thereof;wherein the chemically bonded ceramic system is based on a calcium sulphate, a calcium silicate or a combination thereof; andwherein the amount of free water in the granulate is less than 1% by weight of the granulate.
2. The granulate according to Claim 1, wherein the amount of free water in the granulate is less than 0.7% by weight of the granulate, preferably from 0.2% to 0.6% by weight of the granulate.
3. The granulate according to Claim 1 or Claim 2, wherein the chemically bonded ceramic system is formed in the presence of the nicotine or salt thereof.
4. The granulate according to any one of the preceding claims, wherein at least 80% by weight of the nicotine or salt thereof is located in pores in the chemically bonded ceramic system.
5. The granulate according to any one of the preceding claims, wherein the salt of nicotine is a nicotine bitartrate salt, such as nicotine bitartrate dihydrate.
6. The granulate according to any one of the preceding claims, wherein the chemically bonded ceramic system is based on a calcium sulphate.
7. The granulate according to any one of the preceding claims, wherein the granulate is obtained by wet granulation.
8. The granulate according to any one of the preceding claims, wherein the granulate comprises granules, and at least about 50% (e.g. at least about 90%) by weight of said granules have a size of from 200 to 1000 pm, optionally wherein at least about 50% by weight of the chemically bonded ceramic system is provided in the form of granules having a size of from 200 to 800 pm.
9. A process for preparing a granulate comprising a solid, porous chemically bonded ceramic system based on a calcium sulphate, a calcium silicate or a combination thereof, and nicotine or a salt thereof;wherein the process comprises:(i) combining a precursor for a chemically bonded ceramic system, water and nicotine or a salt thereof in a granulator;(ii) mixing said combination to form a granulate;(iii) drying said granulate such that the amount of free water in the granulate is less than 1% by weight of the granulate.
10. The process according to Claim 9, wherein the granulate is dried in step (iii) such that the amount of free water in the granulate is less than 0.7% by weight of the granulate, preferably from 0.2% to 0.6% by weight of the granulate.
11. The process according to Claim 9 or Claim 10, wherein the precursor for a chemically bonded ceramic system is calcium sulphate hemihydrate.
12. The process according to any one of Claims 9 to 11, wherein the water to cement ratio (w / c) in step (i) is about 0.2 to about 0.8 g / g, such as about 0.2 to about 0.4 g / g.
13. The process according to any one of Claims 9 to 12, wherein step (iii) is commenced not more than 7 days after the production of the granulate in step (ii).
14. An intraoral formulation comprising a granulate according to any one of Claims 1 to 8, or a granulate obtainable by the process of any one of Claims 9 to 13.
15. The intraoral formulation according to Claim 14, further comprising an organic liquid, a low-melting organic solid or a polymer.
16. The intraoral formulation according to Claim 14 or Claim 15, wherein the organic liquid, or low-melting organic solid is selected from the group consisting of propylene glycol, glycerol, polyethene glycol, triacetin, and MCT oil (medium chain triglycerides), preferably propylene glycol.
17. The intraoral formulation according to any one of Claims 14 to 16, further comprising a pH regulating agent.
18. The intraoral formulation according to Claim 17, wherein the pH regulating agent is selected from the group consisting of carbonates (including hydrogencarbonates), silicates, aluminates, acetates, glycinates, phosphates, glycerophosphates, citrates, borates, hydroxides and mixtures thereof.
19. The intraoral formulation according to any one of Claims 14 to 18, further comprising a flavour, optionally wherein:(i) the flavour includes an ingredient selected from the group consisting of sugar, a sugar alcohol, and an artificial sweetener; and / or(ii) the flavour includes an ingredient is selected from the group consisting of menthol, peppermint, Wintergreen, sweet mint, spearmint, vanillin, chocolate, black cherry, coffee, cinnamon, clove, tobacco, citrus, fruit flavour and mixtures thereof.
20. The intraoral formulation according to any one of Claims 14 to 19, wherein the granulate is present at from about 40% to about 98% by weight of the formulation.
21. A permeable, sealed bag containing a granulate as defined in any one of Claims 1 to 8 or an intraoral formulation as defined in any one of Claims 14 to 20.