Capacitor

The capacitor design addresses thermal stress-induced warpage by equally distributing stress across both substrate surfaces through symmetrical grooves and layering, improving structural stability and capacitance.

WO2026239569A1PCT designated stage Publication Date: 2026-11-19NISSAN MOTOR CO LTD
View PDF 0 Cites 0 Cited by

Patent Information

Application Number
PCT/JP2025/017756
Authority / Receiving Office
WO · WO
Patent Type
Applications
Current Assignee / Owner
Filing Date
2025-05-15
Publication Date
2026-11-19

AI Technical Summary

Technical Problem

Conventional capacitors experience thermal stress differences between the front and back surfaces of the substrate, leading to substrate warpage due to grooves being provided only on one surface.

Method used

The capacitor design includes grooves on both main surfaces of the substrate, with alternating dielectric and conductive layers stacked on each groove, ensuring equal thermal stress distribution by spacing and symmetrical arrangement of grooves on both sides.

Benefits of technology

This design effectively eliminates thermal stress differences and suppresses substrate warpage by balancing thermal stress across both surfaces, enhancing structural integrity and capacitance density.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure JP2025017756_19112026_PF_FP_ABST
    Figure JP2025017756_19112026_PF_FP_ABST
Patent Text Reader

Abstract

A capacitor (100) comprises: a substrate (1); a first groove (3) formed in a first main surface (2) of the substrate (1); a first laminated structure (40) which is formed on the surfaces of the first main surface (2) and the first groove (3) and in which dielectric layers (4a, 4b, 4c) and electroconductive layers (5a, 5b, 5c) are alternately laminated; a second groove (7) formed in a second main surface (6) facing the first main surface (2) of the substrate (1); and a second laminated structure (42) which is formed on the surfaces of the second main surface (6) and the second groove (7) and in which dielectric layers (8a, 8b, 8c) and electroconductive layers (9a, 9b, 9c) are alternately laminated. The first groove (3) and the second groove (7) are disposed apart from each other.
Need to check novelty before this filing date? Find Prior Art

Description

Capacitor

[0001] The present invention relates to a capacitor.

[0002] Conventionally, a capacitor in which a dielectric layer and an electrode layer are stacked on a substrate is disclosed in Patent Document 1. In the capacitor disclosed in Patent Document 1, the dielectric layer and the electrode layer are embedded inside a groove provided on one surface of the substrate.

[0003] Japanese Unexamined Patent Publication No. 2021-57374

[0004] However, in the above-described conventional capacitor, the groove is provided only on one surface of the substrate, and the dielectric layer and the electrode layer are embedded inside the groove, so there is a problem that a difference in thermal stress occurs between the front surface and the back surface of the substrate, causing warpage of the substrate.

[0005] The present invention has been made in view of the above problems, and an object thereof is to provide a capacitor that can eliminate the difference in thermal stress between the front surface and the back surface of a substrate and suppress warpage occurring in the substrate.

[0006] A capacitor according to one aspect of the present invention includes: a first groove formed in a first main surface of a substrate; a first stacked structure formed on the first main surface and a surface of the first groove, in which dielectric layers and conductive layers are alternately stacked; a second groove formed in a second main surface of the substrate; and a second stacked structure formed on the second main surface and a surface of the second groove, in which dielectric layers and conductive layers are alternately stacked, wherein the first groove and the second groove are arranged spaced apart from each other.

[0007] According to the present invention, the difference in thermal stress between the front surface and the back surface of the substrate can be eliminated, and warpage occurring in the substrate can be suppressed.

[0008] Figure 1 is a plan view showing the arrangement of grooves in a capacitor according to the first embodiment. Figure 2 is a cross-sectional view taken along line A-A in Figure 1, showing the structure of a capacitor according to the first embodiment. Figure 3A is a first step diagram illustrating the manufacturing method of a capacitor according to the first embodiment. Figure 3B is a second step diagram illustrating the manufacturing method of a capacitor according to the first embodiment. Figure 3C is a third step diagram illustrating the manufacturing method of a capacitor according to the first embodiment. Figure 3D is a fourth step diagram illustrating the manufacturing method of a capacitor according to the first embodiment. Figure 3E is a fifth step diagram illustrating the manufacturing method of a capacitor according to the first embodiment. Figure 3F is a sixth step diagram illustrating the manufacturing method of a capacitor according to the first embodiment. Figure 3G is a seventh step diagram illustrating the manufacturing method of a capacitor according to the first embodiment. Figure 3H is an eighth step diagram illustrating the manufacturing method of a capacitor according to the first embodiment. Figure 3I is a ninth step diagram illustrating the manufacturing method of a capacitor according to the first embodiment. Figure 4 is a plan view showing the arrangement of grooves in a capacitor according to the second embodiment. Figure 5 is a plan view showing the arrangement of grooves in a capacitor according to the third embodiment. Figure 6 is a plan view showing the arrangement of grooves in a capacitor according to the fourth embodiment. Figure 7 is a plan view showing the arrangement of grooves in a capacitor according to the fifth embodiment.

[0009] The embodiments will be described below with reference to the drawings. In the drawings, the same parts are denoted by the same reference numerals, and detailed explanations are omitted. However, the drawings are schematic, and some aspects, such as the relationship between thickness and planar dimensions, and the ratio of the thickness of each layer, may differ from reality. Furthermore, there may be differences in the dimensional relationships and ratios between different drawings.

[0010] (First Embodiment) Figure 1 is a plan view showing the arrangement of grooves in a capacitor according to this embodiment, and Figure 2 is a cross-sectional view taken along A-A in Figure 1 showing the structure of the capacitor. As shown in Figures 1 and 2, the capacitor 100 comprises a substrate 1, a first groove 3 formed on a first main surface 2 of the substrate 1, and a first laminated structure 40 formed on the surfaces of the first main surface 2 and the first groove 3, in which dielectric layers 4a to 4c and conductive layers 5a to 5c are alternately laminated.

[0011] Furthermore, the capacitor 100 includes a second groove 7 formed on a second main surface 6 facing the first main surface 2 of the substrate 1, and a second laminated structure 42 formed on the surfaces of the second main surface 6 and the second groove 7, in which dielectric layers 8a to 8c and conductive layers 9a to 9c are alternately stacked. In addition, the capacitor 100 includes interlayer films 10, 11, insulating films 12, 13, low-potential electrodes 14, 15, and high-potential electrodes 16, 17.

[0012] The substrate 1 is a conductive substrate, with a first groove 3 formed on the first main surface 2, which is the front side of the substrate 1, and a second groove 7 formed on the second main surface 6, which is the back side of the substrate 1. In other words, grooves are formed on both sides of the substrate 1. Furthermore, since the shape of the first groove 3 is the same as the shape of the second groove 7, the surface area of ​​the first groove 3 is the same as the surface area of ​​the second groove 7. Therefore, the sum of the surface areas of the first grooves 3 and the sum of the surface areas of the second grooves 7 formed on the substrate 1 is the same. This eliminates the difference in thermal stress between the front and back sides of the substrate 1, and suppresses warping that occurs in the substrate 1.

[0013] The first groove 3 and the second groove 7 are spaced apart as shown in Figures 1 and 2. In particular, the first groove 3 and the second groove 7 are spaced apart horizontally. However, the first groove 3 and the second groove 7 may overlap horizontally if they can be spaced apart vertically by reducing their depth. The depth of the first groove 3 and the second groove 7 does not need to penetrate the substrate 1.

[0014] As shown in Figure 1, in this embodiment, on the substrate 1, first groove regions 20A and 20B, in which a plurality of first grooves 3 are formed, and second groove regions 21A and 21B, in which a plurality of second grooves 7 are formed, are arranged alternately in the horizontal direction. Therefore, since the first groove regions 20A and 20B and the second groove regions 21A and 21B are arranged symmetrically, the first grooves 3 and the second grooves 7 are also arranged symmetrically. Furthermore, since the number of first groove regions 20A and 20B on the substrate 1 is the same as the number of second groove regions 21A and 21B, the number of first grooves 3 and the number of second grooves 7 formed on the substrate 1 are the same.

[0015] The first groove 3 and the second groove 7 have an aspect ratio of groove depth to groove width that is greater than a predetermined value. Similarly, the first groove 3 and the second groove 7 have an aspect ratio of groove length to groove width that is greater than a predetermined value. In other words, the first groove 3 and the second groove 7 are elongated rectangles in the vertical and horizontal directions, respectively. This allows for a larger surface area of ​​the grooves, thereby increasing the volume density of the grooves.

[0016] Furthermore, the longitudinal direction of the first groove 3 is the same as the longitudinal direction of the second groove 7, and the grooves are formed parallel to each other and at equal intervals.

[0017] In the capacitor 100 shown in Figure 1, the first groove 3 and the second groove 7 are positioned perpendicular to one side surface 44 of the rectangular substrate 1. Therefore, when the substrate 1 is a silicon wafer, the longitudinal direction of the first groove 3 and the longitudinal direction of the second groove 7 are positioned perpendicular to the orientation flat of the silicon wafer.

[0018] As shown in Figure 2, the dielectric layer 4c formed on the surface side of the substrate 1 is formed on the surface of the first main surface 2 and on the interior surface of the first groove 3, and the dielectric layers 4a and 4b are formed on the surfaces of the conductive layers 5b and 5c, respectively. The conductive layers 5a to 5c are formed on the surfaces of the dielectric layers 4a to 4c, respectively. Therefore, a first laminated structure 40 in which dielectric layers 4a to 4c and conductive layers 5a to 5c are alternately stacked is formed on the surface of the first main surface 2 and on the interior surface of the first groove 3.

[0019] Similarly, the dielectric layer 8c formed on the back side of the substrate 1 is formed on the surface of the second main surface 6 and on the inner surface of the second groove 7, and the dielectric layers 8a and 8b are formed on the surfaces of the conductive layers 9b and 9c, respectively. The conductive layers 9a to 9c are formed on the surfaces of the dielectric layers 8a to 8c, respectively. Therefore, a second laminated structure 42 in which dielectric layers 8a to 8c and conductive layers 9a to 9c are alternately stacked is formed on the surface of the second main surface 6 and on the inner surface of the second groove 7.

[0020] The interlayer film 10 is formed on the surface of the conductive layer 5a, which forms the surface of the first laminated structure 40, and is also formed inside the first groove 3. Similarly, the interlayer film 11 on the back side is formed on the surface of the conductive layer 9a, which forms the surface of the second laminated structure 42, and is also formed inside the second groove 7.

[0021] The insulating film 12 is formed on the surface of the interlayer film 10 and also on the sides of the contact holes 23a, 23b, 24a, and 24b. Similarly, the insulating film 13 on the back side is formed on the surface of the interlayer film 11 and also on the sides of the contact holes 25a, 25b, 26a, and 26b.

[0022] The low-potential electrode 14 is formed on the surface of the insulating film 12, bonded to the substrate 1 via a contact hole 23a, and bonded to the conductive layer 5b via a contact hole 23b. Similarly, the low-potential electrode 15 on the back side is formed on the surface of the insulating film 13, bonded to the substrate 1 via a contact hole 25a, and bonded to the conductive layer 9b via a contact hole 25b.

[0023] The high-potential electrode 16 is formed on the surface of the insulating film 12 and is bonded to the conductive layer 5c via a contact hole 24a and to the conductive layer 5a via a contact hole 24b. Similarly, the high-potential electrode 17 on the back side is formed on the surface of the insulating film 13 and is bonded to the conductive layer 9c via a contact hole 26a and to the conductive layer 9a via a contact hole 26b.

[0024] When a positive voltage is applied to the high-potential electrode 16 and a negative voltage is applied to the low-potential electrode 14 of the capacitor 100 configured in this way, positive charges are accumulated in the high-potential conductive layers 5a to 5c and negative charges are accumulated in the low-potential conductive layers. At this time, polarization occurs inside the dielectric layers 4a to 4c, capacitance is generated, and the capacitor functions.

[0025] Similarly, when a positive voltage is applied to the high-potential electrode 17 and a negative voltage is applied to the low-potential electrode 15 of capacitor 100, positive charges are accumulated in the high-potential conductive layers 9a to 9c and negative charges are accumulated in the low-potential conductive layers. At this time, polarization occurs inside the dielectric layers 8a to 8c, generating capacitance and allowing it to function as a capacitor.

[0026] In this embodiment, the case where the substrate 1 is a conductive substrate has been described, but the substrate 1 may also be an insulating substrate or a semiconductor substrate. In this case, the contact holes 23a and 25a and the dielectric layers 4c and 8c may be removed, or a conductive layer may be further formed on the substrate 1 side of the dielectric layers 4c and 8c.

[0027] Next, an example of a manufacturing method for the capacitor 100 according to this embodiment will be described with reference to Figures 3A to 3I.

[0028] First, a conductive substrate 1 is prepared, and a mask material is formed on the front and back surfaces of the substrate 1. A silicon oxide film can be used as the mask material, and ALD (Atomic Layer Deposition), thermal CVD, or plasma CVD can be used as the deposition method.

[0029] Next, a resist is patterned onto the mask material formed on the front and back surfaces of substrate 1. A general photolithography method can be used for patterning.

[0030] Next, the patterned resist is used as a mask, and the mask material is etched. Etching methods include wet etching using hydrofluoric acid and dry etching such as reactive ion etching. Once the mask material is etched, the resist is removed using oxygen plasma, sulfuric acid, or the like.

[0031] When the substrate 1 is etched by dry etching using the mask material formed in this manner, a first groove 3 is formed on the first main surface 2 of the substrate 1, and a second groove 7 is formed on the second main surface 6, as shown in Figures 3A and 3B. Figure 3A is a cross-sectional view taken along line A-A in Figure 1, and Figure 3B is a cross-sectional view taken along line B-B in Figure 1.

[0032] Next, as shown in Figure 3C, a dielectric layer 4c is deposited on the front side of the substrate 1, and a dielectric layer 8c is deposited on the back side. Alumina (aluminum oxide) films can be used for the dielectric layers 4c and 8c, and the ALD method can be used as an example of the deposition method. As a result, the dielectric layer 4c is formed on the surface of the first main surface 2 and the first groove 3, and at the same time, the dielectric layer 8c is formed on the surface of the second main surface 6 and the second groove 7.

[0033] Next, conductive layers 5c and 9c are deposited on the surfaces of dielectric layers 4c and 8c. Ruthenium (Ru) can be used as an example, but other metallic materials such as platinum (Pt), titanium nitride (TiN), and indium tin oxide (ITO), as well as conductive oxide films, can also be used. The ALD method can be used for depositing ruthenium.

[0034] Then, by repeating this process three times, three dielectric layers 4a to 4c are formed on the surface of the first main surface 2 and the first groove 3, and conductive layers 5a to 5c are formed on the surfaces of the dielectric layers 4a to 4c, respectively. Similarly, three dielectric layers 8a to 8c are formed on the surface of the second main surface 6 and the second groove 7, and conductive layers 9a to 9c are formed on the surfaces of the dielectric layers 8a to 8c, respectively.

[0035] Next, as shown in Figure 3D, an interlayer film 10 is deposited on the surface of a first laminated structure 40 in which dielectric layers 4a to 4c and conductive layers 5a to 5c are alternately stacked, and at the same time, an interlayer film 11 is deposited on the surface of a second laminated structure 42 in which dielectric layers 8a to 8c and conductive layers 9a to 9c are alternately stacked. At this time, the interlayer film 10 is also formed inside the first groove 3, and the interlayer film 11 is also formed inside the second groove 7. Silicon oxide films can be used for the interlayer films 10 and 11.

[0036] Next, as shown in Figure 3E, contact holes 23a, 23b, 24a, 24b, 25a, 25b, 26a, and 26b are formed on the surfaces of the interlayer films 10 and 11. First, a mask material (not shown) is formed on the surfaces of the interlayer films 10 and 11, and this mask material is patterned to form a contact hole formation pattern. A photoresist can be used as the mask material. Then, the interlayer films 10 and 11, dielectric layers 4a-4c, 8a-8c, and conductive layers 5a-5c, 9a-9c are etched by dry etching to form contact holes 23a, 23b, 24a, 24b, 25a, 25b, 26a, and 26b.

[0037] Next, as shown in Figure 3F, insulating films 12 and 13 are deposited on the surfaces of the interlayer films 10 and 11 and on the inner surfaces of the contact holes 23a, 23b, 24a, 24b, 25a, 25b, 26a, and 26b.

[0038] Next, as shown in Figure 3G, the insulating films 12 and 13 formed on the bottom surfaces of the contact holes 23a, 23b, 24a, 24b, 25a, 25b, 26a, and 26b are removed. First, a mask material (not shown) is formed on the surface of the insulating films 12 and 13, and this mask material is patterned to form an insulating film removal pattern. A photoresist can be used as the mask material. Then, the insulating films 12 and 13 are etched by dry etching to remove the insulating films 12 and 13 formed on the bottom surfaces of the contact holes 23a, 23b, 24a, 24b, 25a, 25b, 26a, and 26b.

[0039] Next, as shown in Figure 3H, electrode layers 31 and 32 are deposited so as to cover the surfaces of the insulating films 12 and 13. Here, Ti / Al is used as an example. Sputtering, electron beam (EB) deposition, and ALD methods can be used to form the electrode layers 31 and 32.

[0040] Next, as shown in Figure 3I, low-potential electrodes 14, 15 and high-potential electrodes 16, 17 are formed. First, a mask material (not shown) is formed on the surface of the electrode layers 31, 32. This mask material is patterned using a general photolithography method, and the electrode layers 31, 32 are etched by dry etching to form the low-potential electrodes 14, 15 and high-potential electrodes 16, 17. In this way, the capacitor 100 according to this embodiment can be manufactured, and the manufacturing method of the capacitor 100 is completed.

[0041] As described in detail above, the capacitor 100 according to this embodiment comprises a substrate 1, a first groove 3 formed on the first main surface 2 of the substrate 1, and a first laminated structure 40 formed on the surfaces of the first main surface 2 and the first groove 3, in which dielectric layers 4a to 4c and conductive layers 5a to 5c are alternately stacked. The capacitor 100 also comprises a second groove 7 formed on the second main surface 6 of the substrate 1, and a second laminated structure 42 formed on the surfaces of the second main surface 6 and the second groove 7, in which dielectric layers 8a to 8c and conductive layers 9a to 9c are alternately stacked, with the first groove 3 and the second groove 7 being spaced apart.

[0042] Accordingly, since grooves are formed on both surfaces of the substrate 1, thermal stress generated after laminating the dielectric layer and the conductive layer occurs on both surfaces of the substrate 1, and the thermal stress from the front surface of the substrate 1 can be offset by the thermal stress from the back surface of the substrate 1. Therefore, the difference in thermal stress between the front surface and the back surface of the substrate 1 is eliminated, and warpage occurring in the substrate 1 can be suppressed.

[0043] Further, in the capacitor 100 according to the present embodiment, the total surface area of the first grooves 3 formed in the substrate 1 is equal to the total surface area of the second grooves 7. Thereby, the total amount of thermal stress generated after laminating the dielectric layer and the conductive layer can be made equal on the front surface side and the back surface side of the substrate 1. Therefore, the difference in thermal stress between the front surface and the back surface of the substrate 1 is eliminated, and warpage occurring in the substrate 1 can be suppressed.

[0044] Furthermore, in the capacitor 100 according to the present embodiment, the number of the first grooves 3 formed in the substrate 1 is equal to the number of the second grooves 7. Thereby, the total amount of thermal stress generated after laminating the dielectric layer and the conductive layer can be made equal on the front surface side and the back surface side of the substrate 1. Therefore, the difference in thermal stress between the front surface and the back surface of the substrate 1 is eliminated, and warpage occurring in the substrate 1 can be suppressed.

[0045] Further, in the capacitor 100 according to the present embodiment, the longitudinal direction of the first grooves 3 is arranged in the same direction as the longitudinal direction of the second grooves 7. Thereby, the directions of thermal stress generated on both surfaces of the substrate 1 can be aligned, so that the thermal stress from the front surface of the substrate 1 can be offset by the thermal stress from the back surface of the substrate 1. Therefore, the difference in thermal stress between the front surface and the back surface of the substrate 1 is eliminated, and warpage occurring in the substrate 1 can be suppressed.

[0046] Further, in the capacitor 100 according to the present embodiment, the first grooves 3 and the second grooves 7 are set such that the aspect ratio of the groove depth to the groove width is greater than or equal to a predetermined value. Thereby, the surface area of the grooves can be increased, so that the capacitance density of the grooves can be increased.

[0047] Further, in the capacitor 100 according to the present embodiment, the first groove 3 and the second groove 7 are set such that the aspect ratio of the groove length to the groove width is greater than or equal to a predetermined value. As a result, the surface area of the grooves can be increased, so that the capacitance density of the grooves can be increased.

[0048] Further, in the capacitor 100 according to the present embodiment, when the substrate 1 is a silicon wafer, the longitudinal direction of the first groove 3 and the longitudinal direction of the second groove 7 are arranged perpendicular to the orientation flat of the silicon wafer. As a result, the grooves can be formed by dry etching, so that grooves with a high aspect ratio can be formed.

[0049] (Second Embodiment) Hereinafter, a second embodiment to which the present invention is applied will be described with reference to the drawings. In the description of the drawings, the same reference numerals are assigned to the same parts, and detailed description thereof will be omitted.

[0050] FIG. 4 is a plan view showing the arrangement of grooves in the capacitor 100 according to the present embodiment. As shown in FIG. 4, in the present embodiment, the first grooves 3 and the second grooves 7 are periodically arranged in the horizontal direction.

[0051] In particular, the first grooves 3 and the second grooves 7 are alternately arranged in the horizontal direction and are spaced apart from each other in the horizontal direction. That is, the first grooves 3 and the second grooves 7 are arranged symmetrically in the horizontal direction. Further, since the shape of the first groove 3 is the same as the shape of the second groove 7, the surface area of the first groove 3 is the same as the surface area of the second groove 7. Furthermore, the number of first grooves 3 and the number of second grooves 7 formed on the substrate 1 are the same. Therefore, the total sum of the surface areas of the first grooves 3 formed on the substrate 1 is the same as the total sum of the surface areas of the second grooves 7.

[0052] In addition, the longitudinal direction of the first grooves 3 is arranged in the same direction as the longitudinal direction of the second grooves 7, and the grooves are formed parallel to each other at equal intervals. The cross-sectional structure of the capacitor 100 is the same as that of FIG. 2 shown in the first embodiment, so detailed description thereof will be omitted.

[0053] In the capacitor 100 shown in Figure 4, the first groove 3 and the second groove 7 are positioned perpendicular to one side surface 44 of the rectangular substrate 1. Therefore, when the substrate 1 is a silicon wafer, the longitudinal direction of the first groove 3 and the longitudinal direction of the second groove 7 are positioned perpendicular to the orientation flat of the silicon wafer.

[0054] As described in detail above, in the capacitor 100 according to this embodiment, the first groove 3 and the second groove 7 are periodically arranged in the horizontal direction. As a result, the thermal stress from the surface of the substrate 1 and the thermal stress from the back surface of the substrate 1 act in a symmetrical manner, so that the thermal stress from the surface of the substrate 1 can be canceled out by the thermal stress from the back surface of the substrate 1. Therefore, the difference in thermal stress between the surface and back surface of the substrate 1 can be eliminated, and warping that occurs in the substrate 1 can be suppressed.

[0055] (Third Embodiment) A third embodiment to which the present invention is applied will be described below with reference to the drawings. In the drawings, the same parts are denoted by the same reference numerals, and detailed descriptions are omitted.

[0056] Figure 5 is a plan view showing the arrangement of grooves in the capacitor 100 according to this embodiment. As shown in Figure 5, in this embodiment, the first groove 3 and the second groove 7 are arranged symmetrically with respect to the center line C passing through the center of the substrate 1.

[0057] The first groove 3 and the second groove 7 are spaced apart horizontally. Furthermore, since the shape of the first groove 3 is identical to that of the second groove 7, the surface area of ​​the first groove 3 is the same as that of the second groove 7. Additionally, the number of first grooves 3 and second grooves 7 formed on the substrate 1 are the same. Therefore, the sum of the surface areas of the first grooves 3 and the sum of the surface areas of the second grooves 7 formed on the substrate 1 are the same.

[0058] In addition, the longitudinal direction of the first groove 3 is the same as the longitudinal direction of the second groove 7, and the grooves are formed parallel to each other and at equal intervals. The cross-sectional structure of the capacitor 100 is the same as that shown in Figure 2 of the first embodiment, so a detailed explanation is omitted.

[0059] In the capacitor 100 shown in Figure 5, the first groove 3 and the second groove 7 are positioned perpendicular to one side surface 44 of the rectangular substrate 1. Therefore, when the substrate 1 is a silicon wafer, the longitudinal direction of the first groove 3 and the longitudinal direction of the second groove 7 are positioned perpendicular to the orientation flat of the silicon wafer.

[0060] As described in detail above, in the capacitor 100 according to this embodiment, the first groove 3 and the second groove 7 are arranged symmetrically with respect to the center line C passing through the center of the substrate 1. As a result, the thermal stress from the surface of the substrate 1 and the thermal stress from the back surface of the substrate 1 act symmetrically, so that the thermal stress from the surface of the substrate 1 can be canceled out by the thermal stress from the back surface of the substrate 1. Therefore, the difference in thermal stress between the surface and back surfaces of the substrate 1 can be eliminated, and warping that occurs in the substrate 1 can be suppressed.

[0061] (Fourth Embodiment) A fourth embodiment to which the present invention is applied will be described below with reference to the drawings. In the drawings, the same parts are denoted by the same reference numerals, and detailed descriptions are omitted.

[0062] Figure 6 is a plan view showing the arrangement of grooves in the capacitor 100 according to this embodiment. As shown in Figure 6, in this embodiment, the first groove 3 and the second groove 7 are arranged at an angle, rotated by 45° with respect to the center of the rectangular substrate 1. The first groove 3 and the second groove 7 are arranged symmetrically with respect to the center line C passing through the center of the substrate 1.

[0063] The first grooves 3 and the second grooves 7 are arranged alternately in the horizontal direction and spaced apart horizontally. That is, the first grooves 3 and the second grooves 7 are arranged periodically in the horizontal direction. Furthermore, since the shape of the first groove 3 is the same as the shape of the second groove 7, the surface area of ​​the first groove 3 is the same as the surface area of ​​the second groove 7. In addition, the number of first grooves 3 and the number of second grooves 7 formed on the substrate 1 are the same. Therefore, the total surface area of ​​the first grooves 3 and the total surface area of ​​the second grooves 7 formed on the substrate 1 are the same.

[0064] In addition, the longitudinal direction of the first groove 3 is the same as the longitudinal direction of the second groove 7, and the grooves are formed parallel to each other and at equal intervals. The cross-sectional structure of the capacitor 100 is the same as that shown in Figure 2 of the first embodiment, so a detailed explanation is omitted.

[0065] In the capacitor 100 shown in Figure 6, the first groove 3 and the second groove 7 are positioned diagonally to one side surface 44 of the rectangular substrate 1. Therefore, when the substrate 1 is a silicon wafer, the longitudinal directions of the first groove 3 and the second groove 7 are positioned in directions that are not perpendicular to the orientation flat of the silicon wafer.

[0066] As a result, in the capacitor 100 according to this embodiment, the grooves can be formed by wet etching, making it possible to manufacture the capacitor 100 at a low cost.

[0067] (Fifth Embodiment) A fifth embodiment to which the present invention is applied will be described below with reference to the drawings. In the drawings, the same parts are denoted by the same reference numerals, and detailed descriptions are omitted.

[0068] Figure 7 is a plan view showing the arrangement of grooves in the capacitor 100 according to this embodiment. As shown in Figure 7, in this embodiment, the longitudinal direction of the first groove 3 and the longitudinal direction of the second groove 7 are arranged diagonally with respect to one side surface 44 of the rectangular substrate 1.

[0069] The first grooves 3 and the second grooves 7 are arranged alternately in the horizontal direction and spaced apart horizontally. That is, the first grooves 3 and the second grooves 7 are arranged periodically in the horizontal direction. Furthermore, since the shape of the first groove 3 is the same as the shape of the second groove 7, the surface area of ​​the first groove 3 is the same as the surface area of ​​the second groove 7. In addition, the number of first grooves 3 and the number of second grooves 7 formed on the substrate 1 are the same. Therefore, the total surface area of ​​the first grooves 3 and the total surface area of ​​the second grooves 7 formed on the substrate 1 are the same.

[0070] In addition, the longitudinal direction of the first groove 3 is the same as the longitudinal direction of the second groove 7, and the grooves are formed parallel to each other and at equal intervals. The cross-sectional structure of the capacitor 100 is the same as that shown in Figure 2 of the first embodiment, so a detailed explanation is omitted.

[0071] Here, since the first groove 3 and the second groove 7 are arranged diagonally, when the substrate 1 is a silicon wafer, the longitudinal direction of the first groove 3 and the longitudinal direction of the second groove 7 are arranged in directions that are not perpendicular to the orientation flat of the silicon wafer.

[0072] As a result, in the capacitor 100 according to this embodiment, the grooves can be formed by wet etching, making it possible to manufacture the capacitor 100 at a low cost.

[0073] As described above, embodiments of the present invention have been presented, but the statements and drawings that constitute part of this disclosure should not be understood as limiting the invention. Various alternative embodiments, examples, and operational techniques will become apparent to those skilled in the art from this disclosure.

[0074] 1 Substrate 2 First main surface 3 First grooves 4a, 4b, 4c, 8a, 8b, 8c Dielectric layer 5a, 5b, 5c, 9a, 9b, 9c Conductive layer 6 Second main surface 7 Second grooves 10, 11 Interlayer film 12, 13 Insulating film 14, 15 Low potential electrodes 16, 17 High potential electrodes 20A, 20B First groove region 21A, 21B Second groove region 23a, 23b, 24a, 24b, 25a, 25b, 26a, 26b Contact holes 31, 32 Electrode layer 40 First laminated structure 42 Second laminated structure 44 Side capacitor 100 C Center line

Claims

1. A capacitor comprising: a substrate; a first groove formed on a first main surface of the substrate; a first laminated structure formed on the surface of the first main surface and the first groove, in which dielectric layers and conductive layers are alternately stacked; a second groove formed on a second main surface of the substrate facing the first main surface; and a second laminated structure formed on the surface of the second main surface and the second groove, in which dielectric layers and conductive layers are alternately stacked, wherein the first groove and the second groove are spaced apart.

2. The capacitor according to claim 1, wherein the sum of the surface areas of the first grooves formed on the substrate and the sum of the surface areas of the second grooves are the same.

3. The capacitor according to claim 1, wherein the number of first grooves formed on the substrate and the number of second grooves are the same.

4. The capacitor according to any one of claims 1 to 3, wherein the longitudinal direction of the first groove is arranged in the same direction as the longitudinal direction of the second groove.

5. The capacitor according to any one of claims 1 to 4, wherein the first groove and the second groove are periodically arranged in the horizontal direction.

6. The capacitor according to any one of claims 1 to 4, wherein the first groove and the second groove are each arranged symmetrically with respect to a center line passing through the center of the substrate.

7. The capacitor according to any one of claims 1 to 6, wherein the aspect ratio of the groove depth to the groove width is set to be greater than or equal to a predetermined value for the first groove and the second groove.

8. The capacitor according to any one of claims 1 to 6, wherein the aspect ratio of the length of the groove to the width of the groove is set to be greater than or equal to a predetermined value for the first groove and the second groove.

9. The capacitor according to any one of claims 1 to 8, wherein, when the substrate is a silicon wafer, the longitudinal direction of the first groove and the longitudinal direction of the second groove are arranged perpendicular to the orientation flat of the silicon wafer.

10. The capacitor according to any one of claims 1 to 8, wherein, when the substrate is a silicon wafer, the longitudinal direction of the first groove and the longitudinal direction of the second groove are arranged in a direction not perpendicular to the orientation flat of the silicon wafer.