Method for manufacturing heat sink

The method addresses fin height inconsistencies in heat sinks by applying uniform stress to achieve plastic deformation, ensuring consistent fin heights and improved cooling efficiency.

WO2026239713A1PCT designated stage Publication Date: 2026-11-19RESONAC CORP
View PDF 0 Cites 0 Cited by

Patent Information

Application Number
PCT/JP2026/006848
Authority / Receiving Office
WO · WO
Patent Type
Applications
Current Assignee / Owner
Priority Date
2025-05-14
Filing Date
2026-02-25
Publication Date
2026-11-19

AI Technical Summary

Technical Problem

Existing heat sinks with varying fin heights after molding face issues such as reduced cooling efficiency due to incomplete fin joining and potential coolant leakage, exacerbated by springback during conventional fin height correction methods.

Method used

A method involving a straightening process that applies uniform stress to all fins, extending beyond the elastic deformation region to the plastic deformation region, ensuring all fins undergo plastic deformation, thereby achieving uniform fin heights.

Benefits of technology

Ensures consistent fin heights post-straightening, preventing springback and ensuring uniform fin integration, thus enhancing cooling efficiency and preventing coolant leakage.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure JP2026006848_19112026_PF_FP_ABST
    Figure JP2026006848_19112026_PF_FP_ABST
Patent Text Reader

Abstract

This method for manufacturing a heat sink provided with a base part and a plurality of fins protruding from one surface of the base part includes at least: a molding step of obtaining, using a molding material, a heat sink molded body including the base part and the plurality of fins; and a correction step of, when the plurality of fins of the heat sink molded body have at least two different protrusion heights, applying stress to all the fins to reduce the protrusion heights to a height at which the fin having the lowest protrusion height is plastically deformed, thereby performing correction such that all the fins have a uniform protrusion height.
Need to check novelty before this filing date? Find Prior Art

Description

Method for manufacturing heat sink

[0001] The present invention relates to a method for manufacturing a heat sink. This application claims priority based on Japanese Patent Application No. 2025-080888 filed in Japan on May 14, 2025, the content of which is incorporated herein by reference.

[0002] Heat sinks are widely used as heat dissipation means for radiating heat generated by members constituting electronic devices and home electric appliances to the outside. Such heat sinks are mainly made of aluminum alloy due to their high thermal conductivity and ease of molding.

[0003] In order to improve heat dissipation efficiency, many heat sinks are composed of a base part joined to an object to be cooled, and a plurality of fins erected, for example, in a direction perpendicular to the base part. By arranging and forming such a plurality of fins at narrow intervals, the surface area is increased and the heat dissipation efficiency is improved.

[0004] Such heat sinks are generally molded by die molding, die forging, die casting, cutting, or the like, but many of the molded heat sink bodies after molding have variations such as different heights of individual fins, that is, different tip positions.

[0005] When there is variation in the height of the fins as described above, for example, when the entire plurality of fins are accommodated in a coolant tank through which a coolant flows and the tips of the fins are joined to the bottom surface of the coolant tank, some fins with a height lower than the designed value are not joined, which causes a problem that the cooling efficiency is lowered. In addition, there is a concern that some fins with a height higher than the designed value may cause the molded heat sink body to lift from the coolant tank, creating gaps and the like, leading to coolant leakage.

[0006] For this reason, a step of correcting the height of the fins is also known in order to make all the heights of the plurality of fins of the molded heat sink body after molding uniform. For example, Patent Document 1 discloses that the tip height of the plurality of pin fins is corrected by pressing the tips of the plurality of pin fins in the length direction of the pin fins while melting the tips with the heat of a punch heated to a temperature equal to or higher than the melting point of the constituent material of the pin fins.

[0007] Japanese Patent Publication No. 2020-072107

[0008] However, when correcting fins by pressing the flat surface of a correction jig against multiple fins to lower the height of the taller fins, there was a problem in that the fins whose height had been corrected in the elastic deformation region would return to their original height due to springback, resulting in the height of not all fins being uniform even after correction.

[0009] For example, if you correct multiple fins so that the shortest fin is slightly lower than the others, the tallest fin will undergo plastic deformation due to its larger deformation, resulting in a roughly uniform amount of springback after correction. However, the shortest fin will undergo smaller deformation, and in the case of deformation within the elastic deformation range, its springback after correction will be less than that of a fin corrected to the plastic deformation range. Thus, if there are differences in the amount of springback after correction among the fins, there is a concern that the fin heights will not be uniform even after correction.

[0010] The present invention has been made in view of the above circumstances, and aims to provide a method for manufacturing a heat sink that can suppress changes in fin height after the straightening stress is removed when straightening a plurality of fins of different heights to a constant height.

[0011] To solve the above problems, the present invention provides the following means.

[0012] (1) A method for manufacturing a heat sink according to one aspect of the present invention is a method for manufacturing a heat sink comprising a base portion and a plurality of fins protruding from one surface of the base portion, comprising at least a molding step of obtaining a heat sink molded body comprising the base portion and the plurality of fins using a molding material, and a correcting step of, if the protrusion heights of the plurality of fins of the heat sink molded body are at least two stages, applying stress to all the fins to a height at which the fin with the lowest protrusion height undergoes plastic deformation to reduce the protrusion height so that all the fins have a uniform protrusion height.

[0013] (2) In the method for manufacturing the heat sink described in (1) above, the straightening step is a step of applying uniform stress to all the fins by the flat surface of the straightening jig.

[0014] (3) In the heat sink manufacturing method of (1) or (2) above, the straightening step is a step of applying uniform stress to all the fins in two or more stages using the straightening jig.

[0015] (4) In any one of the heat sink manufacturing methods described in (1) to (3) above, the straightening step is performed by heating the heat sink molded body to a temperature range that is higher than room temperature and 50°C or more lower than the melting point of the molding material of the heat sink molded body.

[0016] (5) In the method for manufacturing a heat sink according to any one of (1) to (4) above, the heat sink is made of an aluminum alloy.

[0017] According to the present invention, it is possible to provide a method for manufacturing a heat sink that can suppress changes in fin height after the straightening stress is removed when straightening multiple fins of different heights to a constant height.

[0018] This is an external perspective view showing an example of a heat sink manufactured by the heat sink manufacturing method of the present invention. This is a schematic cross-sectional view showing the straightening process in steps in the heat sink manufacturing method of the first embodiment of the present invention. This is a graph showing the relationship between applied stress and strain to the fin with the lowest protrusion height and the fin with the highest protrusion height in the straightening process of the present invention. This is a graph showing the relationship between applied stress and strain to the fin with the lowest protrusion height and the fin with the highest protrusion height in a conventional straightening process. This is a schematic cross-sectional view showing the straightening process in the heat sink manufacturing method of the second embodiment of the present invention. This is a schematic cross-sectional view showing the straightening process in the heat sink manufacturing method of the third embodiment of the present invention.

[0019] The following describes in detail a method for manufacturing a heat sink according to an embodiment of the present invention, with appropriate reference to the drawings. The drawings used in the following description may show enlarged versions of characteristic parts for convenience in order to clearly illustrate the features of the present invention, and the dimensional ratios of each component may differ from those of the actual components. The materials, dimensions, etc., exemplified in the following description are examples only, and the present invention is not limited to them; it can be modified as appropriate within the scope of achieving its effects.

[0020] [Heat sink] Figure 1 is an external perspective view showing an example of a heat sink that can be manufactured by a heat sink manufacturing method according to one embodiment of the present invention. The heat sink 1, after undergoing the straightening process described later, is integrally molded from, for example, an aluminum alloy with excellent thermal conductivity. The heat sink 1 of this embodiment is a fin-type heat sink and comprises a base portion (foundation) 11 and a plurality of fins 12, 12... erected vertically from one surface 11a of the base portion 11. The plurality of fins 12, 12... are straightened so that the height of the protrusion along the vertical direction from one surface 11a is constant.

[0021] [Method for Manufacturing a Heat Sink: First Embodiment] The method for manufacturing a heat sink in this embodiment first involves forming a heat sink molded body before the straightening process using various processing methods such as mold forming, die forging, die casting, and cutting (forming process). In such a heat sink molded body immediately after forming, the heights of the multiple fins may be uneven, and it is necessary to correct the heights.

[0022] Next, the heat sink molded body is straightened so that the height of the multiple fins constituting the heat sink is constant, thereby obtaining a heat sink 1 with a constant fin height (straightening step). In this embodiment, as a heat sink molded body before the straightening step, an example is given in which three fins molded at three different heights are straightened to a constant height. Figure 2 is a schematic cross-sectional view showing the straightening step in the heat sink manufacturing method of this embodiment in stages.

[0023] As illustrated in Figure 2(a), the molded heat sink body 10 has three fins 12a, 12b, and 12c that are erected vertically from the base portion 11. The height (projection height) of each fin from one surface 11a of the base portion 11 to the top of each fin is such that fin 12b is the lowest, fin 12c is the highest, and fin 12a is in between.

[0024] In the straightening process, for example, the fin height is straightened using a straightening jig 20 equipped with a flat surface 21. The straightening jig 20 only needs to be equipped with a pressing means such as a hydraulic device that can press it toward the heat sink molded body 10 with any stress to any position.

[0025] In the straightening process, as shown in Figure 2(b), the straightening method involves pressing the flat surface 21 of the straightening jig 20 against the three fins 12a, 12b, and 12c with equal stress, compressing them until the fin heights of all three fins 12a, 12b, and 12c reach a predetermined height h1.

[0026] At this time, stress is applied to all fins 12a, 12b, and 12c to reduce their protrusion heights until the fin 12b with the lowest protrusion height undergoes plastic deformation, thereby achieving a uniform protrusion height h1 for all fins 12a, 12b, and 12c.

[0027] Figure 3 is a graph showing the relationship between applied stress and strain for the fin with the lowest protrusion height and the fin with the highest protrusion height during this straightening process. In the straightening process of this embodiment, if stress is applied to the fin 12b with the lowest protrusion height, extending beyond the elastic deformation region to the plastic deformation region to reduce its protrusion height, then stress will also be applied to the plastic deformation region of fins 12a and 12c, which have higher protrusion heights before straightening.

[0028] This makes it possible to make the springback amount of all fins 12a, 12b, and 12c uniform. As a result, as shown in Figure 2(b), even after stopping the stress application by the straightening jig 20, all fins 12a, 12b, and 12c spring back from a predetermined height h1 by a uniform springback amount Δh. Therefore, the protruding height of all fins 12a, 12b, and 12c after straightening can be made uniform at a protruding height h2, which is h1 + Δh.

[0029] On the other hand, if stress is applied only up to the elastic deformation region to the fin with the lowest protrusion height, as in the conventional straightening process, as shown in Figure 4, the highest fin will be plastically deformed, but the lowest fin will not. As a result, when the pressure from the straightening jig is released, the amount of springback will differ between the highest and lowest fins before straightening, resulting in uneven height distribution among the fins after straightening.

[0030] In the straightening process of this embodiment, it is also preferable to preheat the heat sink molded body 10 whose protrusion height is to be straightened. If the heat sink molded body 10 to be straightened is heated to a temperature higher than room temperature and at least 50°C lower than the melting point of the molding material of the heat sink molded body 10, for example, an aluminum alloy, then the straightening can be performed with lower stress compared to when the heat sink molded body 10 is straightened by applying stress at room temperature.

[0031] Therefore, the protruding height of the fins 12a, 12b, and 12c can be corrected at low cost using simpler straightening equipment. In this embodiment, the heat sink molded body 10 made of aluminum alloy was heated at a temperature lower than the melting point of the aluminum alloy and sufficient to reduce the applied stress, for example, 500°C, to perform the straightening process.

[0032] Furthermore, in this straightening process, when applying stress to all fins 12a, 12b, and 12c using the straightening jig 20, it is preferable to lower the straightening jig 20 in multiple stages, for example, two stages, rather than continuously lowering it to a predetermined height h1.

[0033] By lowering the straightening jig 20 in multiple stages, it is possible to more reliably prevent buckling or bending from occurring while the fins 12a, 12b, and 12c are being shortened to a predetermined height h1.

[0034] As described above, according to the heat sink manufacturing method of one embodiment of the present invention, in the straightening process, if stress is applied to the fin with the lowest protrusion height, extending beyond the elastic deformation region to the plastic deformation region, thereby reducing the protrusion height, then stress will also be applied to all fins with a higher protrusion height than this one before straightening, extending to the plastic deformation region.

[0035] This allows for a uniform amount of springback in all fins. As a result, even after the stress application by the straightening jig is stopped, all fins will spring back by the same amount, making it possible to straighten all fins to a uniform protrusion height after correction.

[0036] [Method for Manufacturing a Heat Sink: Second Embodiment] Figure 5 is a schematic cross-sectional view showing the straightening process of the heat sink manufacturing method in the second embodiment. In this embodiment, the heat sink molded body 10 before correction is placed on a stage 32 whose height is fixed. The heat sink molded body 10 is then pressed against the stage 32 by a height adjustment jig 33 to the extent that the heat sink molded body 10 does not deform. After that, the straightening jig 30 is lowered toward the heat sink molded body 10. Then, the multiple fins 12 of the heat sink molded body 10 are pressed against the flat surface 31 of the straightening jig 30 to straighten them so that the protruding height of the fins 12 is uniform (straightening process).

[0037] The height adjustment jig 33 used in this embodiment only needs to be formed so that its thickness matches the corrected height of the fin 12. The thickness of this height adjustment jig 33 is set to a thickness that allows stress to be applied to the fin 12b with the lowest protrusion height, extending beyond the elastic deformation region to the plastic deformation region.

[0038] In the straightening process of this embodiment, as in the first embodiment, stress is applied to the fin 12b with the lowest protrusion height, extending beyond the elastic deformation region to the plastic deformation region to reduce its protrusion height. This also applies stress to all other fins 12a and 12c, which have higher protrusion heights before straightening, extending to the plastic deformation region. As a result, the amount of springback of all fins 12a, 12b, and 12c becomes uniform, and all fins 12a, 12b, and 12c after straightening can be made to have a uniform protrusion height.

[0039] [Method for Manufacturing a Heat Sink: Third Embodiment] Figure 6 is a schematic cross-sectional view showing the straightening process of the method for manufacturing a heat sink in the third embodiment. In this embodiment, the straightening jig 40 used in the straightening process comprises a flat surface 41 and a height adjustment part 43 extending downward from the end of the flat surface 41.

[0040] The amount of protrusion downward from the flat surface 41 of the height adjustment section 43 is set to an amount that allows stress to be applied to the fin 12b with the lowest protrusion height, extending beyond the elastic deformation region to the plastic deformation region. In this embodiment, the straightening jig 40 is lowered to a position where the lower end of the height adjustment section 43 contacts the stage 42 on which the heat sink molded body 10 is placed, thereby straightening the fins 12 so that their protrusion heights are uniform (straightening process).

[0041] In the straightening process of this embodiment, as in the first embodiment, stress is applied to the fin 12b with the lowest protrusion height, extending beyond the elastic deformation region to the plastic deformation region to reduce its protrusion height. This also applies stress to all other fins 12a and 12c, which have higher protrusion heights before straightening, extending to the plastic deformation region. As a result, the amount of springback of all fins 12a, 12b, and 12c becomes uniform, and all fins 12a, 12b, and 12c after straightening can be made to have a uniform protrusion height.

[0042] Although one embodiment of the present invention has been described above, these embodiments are presented as examples and are not intended to limit the scope of the invention. These embodiments can be carried out in various other forms, and various omissions, substitutions, and modifications can be made without departing from the spirit of the invention. These embodiments and their variations are included in the scope and spirit of the invention, as well as in the claims and their equivalents.

[0043] 1... Heat sink 10... Heat sink molded body 11... Base part 12... Fin 20... Straightening jig 21... Flat surface

Claims

1. A method for manufacturing a heat sink comprising a base portion and a plurality of fins protruding from one surface of the base portion, comprising at least a molding step of obtaining a heat sink molded body comprising the base portion and the plurality of fins using a molding material, and a correcting step of, if the protrusion heights of the plurality of fins of the heat sink molded body are at least two or more stages, applying stress to all the fins to reduce the protrusion height to a height at which the fin with the lowest protrusion height undergoes plastic deformation, thereby correcting the fins so that all of them have a uniform protrusion height.

2. The method for manufacturing a heat sink according to claim 1, wherein the straightening step is a step of applying uniform stress to all the fins by the flat surface of a straightening jig.

3. The method for manufacturing a heat sink according to claim 2, wherein the straightening step is a step of applying uniform stress to all the fins in two or more stages using the straightening jig.

4. The method for manufacturing a heat sink according to any one of claims 1 to 3, wherein in the straightening step, the heat sink molded body is heated to a temperature range that is higher than room temperature and 50°C or more lower than the melting point of the molding material of the heat sink molded body.

5. The method for manufacturing a heat sink according to any one of claims 1 to 3, wherein the heat sink is made of an aluminum alloy.