Method for manufacturing laminated substrate
The method of film formation, bonding, and sequential vacancy formation in laminated substrates addresses design limitations and misalignment issues, improving efficiency and reliability in manufacturing laminated substrates.
Patent Information
- Application Number
- PCT/JP2026/015057
- Authority / Receiving Office
- WO · WO
- Patent Type
- Applications
- Current Assignee / Owner
- Priority Date
- 2025-05-15
- Filing Date
- 2026-04-13
- Publication Date
- 2026-11-19
AI Technical Summary
Existing methods for manufacturing laminated substrates, such as printed circuit boards, face limitations in design freedom due to the thickness of glass layers, require multiple steps, and are prone to misalignment of via layers, leading to inefficiencies and potential defects.
A method involving film formation, bonding, thinning, and sequential vacancy formation steps, including sandblasting or laser processing for voids, allows for improved design freedom and reduces misalignment by forming voids after bonding, using dielectric materials like quartz glass and silicon, and direct bonding techniques.
This approach reduces manufacturing steps, enhances design flexibility, and minimizes misalignment, resulting in a more reliable and efficient production process for laminated substrates.
Smart Images

Figure JP2026015057_19112026_PF_FP_ABST
Abstract
Description
Manufacturing method for multilayer substrates
[0001] This invention relates to a method for manufacturing a laminated substrate.
[0002] It is known that laminated substrates having a laminated structure are applied to various industrial products. Depending on the application, such laminated substrates may be provided with through-holes that penetrate the laminated substrate in the stacking direction. As an example of a laminated substrate having through-holes, a printed circuit board has been proposed that includes: a first glass layer; a first wiring layer and a second wiring layer embedded above and below the first glass layer, respectively; a first via layer that penetrates the first glass layer and is connected to the first and second wiring layers; a second glass layer disposed on the upper surface of the first glass layer; a third wiring layer embedded above the second glass layer; and a second via layer that penetrates the second glass layer and is connected to the first and third wiring layers (see Patent Document 1). In the printed circuit board described in Patent Document 1, the first via layer and the second via layer are electrically connected to each other and function as through-holes that penetrate the printed circuit board in the stacking direction. The printed circuit board described in Patent Document 1 is manufactured by separately preparing a first glass layer and a second glass layer, providing a first wiring layer, a second wiring layer and a first via layer on the first glass layer, and providing a third wiring layer and a second via layer on the second glass layer, and then joining the first glass layer and the second glass layer so that the first via layer and the second via layer are electrically connected.
[0003] Japanese Patent Publication No. 2024-162954
[0004] In the method for manufacturing a printed circuit board described in Patent Document 1, through holes are formed in each of the first and second glass layers, and via layers are provided within these through holes. The size of the through holes that can be formed in the glass layer is limited by its relationship to the thickness of the glass layer, which may reduce the design freedom of the through hole size. Furthermore, since the first glass layer with the first via layer and the second glass layer with the second via layer are joined together after the via layers are provided in each of the first and second glass layers, it is difficult to reduce the number of steps in the manufacturing method of the printed circuit board, and there is a risk of misalignment between the first via layer and the second via layer in the printed circuit board. The main object of the present invention is to provide a method for manufacturing a laminated substrate that can reduce the number of steps, improve the design freedom of the sizes of the first and second holes, and suppress misalignment between the first and second holes.
[0005] [1] A method for manufacturing a laminated substrate according to an embodiment of the present invention includes a first film formation step, a bonding step, a thinning step, a first vacancy formation step, and a second vacancy formation step. In the first film formation step, a first conductive layer is formed on one side of the first dielectric substrate in the thickness direction. In the bonding step, a second dielectric substrate is bonded to the first dielectric substrate via the first conductive layer. In the thinning step, at least one of the first dielectric substrate and the second dielectric substrate is thinned. In the first vacancy formation step, a first vacancy is formed on the first dielectric substrate from the side opposite to the second dielectric substrate, recessed toward the second dielectric substrate. In the second vacancy formation step, a second vacancy is formed on the second dielectric substrate from the side opposite to the first dielectric substrate, communicating with the first vacancy. [2] In the method for manufacturing a laminated substrate described in [1] above, the first vacancy may penetrate the first dielectric substrate and the first conductor layer and reach the interior of the second dielectric substrate. [3] In the thinning step included in the method for manufacturing a laminated substrate described in [1] or [2] above, the first dielectric substrate may be thinned to form a functional layer. In this case, the second dielectric substrate functions as a support substrate that supports the functional layer via the first conductor layer. [4] In the first vacancy formation step included in the method for manufacturing a laminated substrate described in [1] to [3] above, the first vacancy may be formed by sandblasting or laser processing. In the second vacancy formation step, the second vacancy may be formed by etching. [5] In the method for manufacturing a laminated substrate described in any of [1] to [4] above, the first dielectric substrate may contain quartz glass. The second dielectric substrate may contain silicon. [6] The method for manufacturing a laminated substrate described in any of [1] to [5] above may further include a second film formation step. The second film formation step is performed after the second void formation step. In the second film formation step, a second conductive layer is formed on the surface of the first dielectric substrate opposite to the first conductive layer. [7] In the second film formation step included in the method for manufacturing a laminated substrate described in [6] above, a third conductive layer may be formed on the surface of the second dielectric substrate opposite to the first dielectric substrate.[8] In the second film formation step included in the method for manufacturing a laminated substrate described in [7] above, via conductor layers that electrically connect the second conductor layer and the third conductor layer may be formed on the inner surfaces of the first void and the second void, respectively.
[0006] According to embodiments of the present invention, it is possible to reduce the number of man-hours while improving the degree of freedom in designing the sizes of the first and second voids, and to suppress misalignment of the first and second voids.
[0007] Figure 1 is a schematic diagram illustrating a first film formation step and a bonding step included in a method for manufacturing a laminated substrate according to one embodiment of the present invention. Figure 2 is a schematic diagram illustrating a thinning step following the bonding step in Figure 1. Figure 3 is a schematic diagram illustrating a first void formation step following the thinning step in Figure 2. Figure 4 is a schematic diagram illustrating a second void formation step following the first void formation step in Figure 3. Figure 5 is a schematic diagram illustrating a second film formation step following the second void formation step in Figure 4. Figure 6 is a schematic perspective view of a laminated substrate manufactured by a method for manufacturing a laminated substrate according to one embodiment of the present invention. Figure 7 is a schematic cross-sectional view of a first modified example of the laminated substrate in Figure 6. Figure 8 is a schematic cross-sectional view of a second modified example of the laminated substrate in Figure 6. Figure 9 is a schematic cross-sectional view of a third modified example of the laminated substrate in Figure 6. Figure 10 is a schematic cross-sectional view of a fourth modified example of the laminated substrate in Figure 6. Figure 11 is a schematic cross-sectional view of a fifth modified example of the laminated substrate in Figure 6. Figure 12 is a schematic cross-sectional view of a sixth modified example of the laminated substrate shown in Figure 6. Figure 13 is a schematic cross-sectional view of a seventh modified example of the laminated substrate shown in Figure 6.
[0008] Embodiments of the present invention will be described below with reference to the drawings, but the present invention is not limited to these embodiments. Furthermore, in order to clarify the explanation, the drawings may schematically represent the width, thickness, shape, etc., of each part compared to the embodiments; however, these are merely examples and do not limit the interpretation of the present invention.
[0009] A. Schematic Figure 1 of the manufacturing method for a laminated substrate is a schematic diagram illustrating the first film formation step and bonding step included in the manufacturing method for a laminated substrate according to one embodiment of the present invention; Figure 2 is a schematic diagram illustrating the thinning step following the bonding step in Figure 1; Figure 3 is a schematic diagram illustrating the first void formation step following the thinning step in Figure 2; and Figure 4 is a schematic diagram illustrating the second void formation step following the first void formation step in Figure 3. In one embodiment, the manufacturing method for a laminated substrate includes a first film formation step, a bonding step, a thinning step, a first void formation step, and a second void formation step. As shown in Figure 1, in the first film formation step, a first conductive layer 3 is formed on one side in the thickness direction of the first dielectric substrate 1. In the bonding step, the second dielectric substrate 2 is bonded to the first dielectric substrate 1 via the first conductive layer 3. As shown in Figure 2, in the thinning step, at least one of the first dielectric substrate 1 and the second dielectric substrate 2 is thinned. As shown in Figure 3, in the first void formation step, a first void 10 is formed in the first dielectric substrate 1 from the side opposite to the second dielectric substrate 2, recessing toward the second dielectric substrate 2. As shown in Figure 4, in the second void formation step, a second void 20 is formed in the second dielectric substrate 2 from the side opposite to the first dielectric substrate 1, connecting to the first void 10. Hereinafter, the first void 10 and the second void 20 that connect to each other may be referred to as a through-hole 40. According to this method, after joining the first dielectric substrate 1 and the second dielectric substrate 2 via the first conductive layer 3, the first dielectric substrate 1 and / or the second dielectric substrate 2 are thinned to sequentially form the first void 10 and the second void 20. Compared to the case where voids are formed in each of the first and second dielectric substrates before joining them via the first conductive layer, this method reduces the number of steps required to manufacture the laminated substrate 100, while also improving the design flexibility of the sizes of the first void 10 and the second void 20, and suppressing misalignment of the first void 10 and the second void 20.
[0010] As shown in Figure 5, in one embodiment, the method for manufacturing a laminated substrate further includes a second film deposition step. The second film deposition step is performed after the second void formation step. In the second film deposition step, a second conductive layer 4 is deposited on the surface of the first dielectric substrate 1 opposite to the first conductive layer 3.
[0011] In one embodiment, after the thinning process, a third conductive layer 5 may be formed on the surface of the second dielectric substrate 2 opposite to the first dielectric substrate 1. The third conductive layer 5 may be formed in a process different from the second film deposition process, or it may be formed together with the second conductive layer 4 in the second film deposition process. In the illustrated example, the third conductive layer 5 is formed in the second film deposition process on the surface of the second dielectric substrate 2 opposite to the first dielectric substrate 1. This reduces the number of steps in the manufacturing of the laminated substrate 100 comprising the second conductive layer 4 and the third conductive layer 5.
[0012] In one embodiment, after the second void formation step, a via conductor layer 6 may be formed on the inner surfaces of the first void 10 and the second void 20 (the inner surfaces of the through-holes 40). When conductor layers are provided on the inner surfaces of voids formed in the first dielectric substrate and the second dielectric substrate, their surfaces must be smoothed by polishing beforehand in order to join them. As a result, crystal damage may occur on the polished surfaces of the first dielectric substrate and the second dielectric substrate, and / or variations in thickness and steps may occur due to differences in the materials of the conductor layer and the dielectric substrate exposed at the joining surface, or steps near the voids created during void formation. In these cases, the bonding strength between the first dielectric substrate and the second dielectric substrate may decrease, potentially adversely affecting the characteristics and reliability of the manufactured laminated substrate. In contrast, according to one embodiment, the first dielectric substrate 1 and the second dielectric substrate 2 are joined together, and after the first void 10 and the second void 20 are formed, a via conductor layer 6 is formed on their inner surfaces. Therefore, before joining the first dielectric substrate 1 and the second dielectric substrate 2, it is not necessary to smooth the surfaces of the first dielectric substrate 1 and the second dielectric substrate 2 by simultaneously polishing different materials. As a result, in the laminated substrate 100 equipped with the via conductor layer 6, the bonding strength between the first dielectric substrate 1 and the second dielectric substrate 2 can be improved, and desired characteristics and reliability can be stably expressed.
[0013] The via conductor layer 6 may be formed in a process different from the second film deposition process, or it may be formed together with the second conductor layer 4 and the third conductor layer 5 in the second film deposition process. In the illustrated example, the via conductor layer 6 is deposited on the inner surface of the through-hole 40 in the second film deposition process. The via conductor layer 6 electrically connects the second conductor layer 4 and the third conductor layer 5. This reduces the number of steps in the manufacturing of the laminated substrate 100 comprising the second conductor layer 4, the third conductor layer 5, and the via conductor layer 6.
[0014] B. Details of Method for Manufacturing Laminated Substrate Next, details of a method for manufacturing a laminated substrate according to one embodiment will be described with reference to FIGS. 1 to 5. In one embodiment, the method for manufacturing a laminated substrate includes a first film formation step, a bonding step, a thinning step, a first pore formation step, a second pore formation step, and a second film formation step in this order.
[0015] B-1. First Film Formation Step As shown in FIG. 1, in the first film formation step, first, a first dielectric substrate 1 and a second dielectric substrate 2 are prepared. Each of the first dielectric substrate 1 and the second dielectric substrate 2 contains a dielectric material. The dielectric material is arbitrarily and appropriately selected according to the use of the laminated substrate 100. The dielectric constant of the dielectric material at 100 GHz to 10 THz is, for example, 1.0 to 20, preferably 2.0 to 15. Examples of the dielectric material include inorganic materials and organic materials. Specific examples of inorganic materials include single-crystal quartz, amorphous quartz, spinel (MgAl 2 O 4 ), aluminum nitride (AlN), sapphire, silicon carbide (SiC), magnesium oxide (MgO), aluminum oxide (Al 2 O 3 ), silicon (Si), indium phosphide (InP), glass, sialon (Si 3 N 4 -Al 2 O 3 ), mullite (3Al 2 O 3 ·2SiO 2 , 2Al 2 O 3 ·3SiO 2 ), gallium nitride (GaN), silicon nitride (Si 3 N 4 ), gallium oxide (Ga 2 O 3 ), and diamond. Specific examples of organic materials include polyimide, fluororesin, cycloolefin polymer (COP), and liquid crystal polymer (LCP). The dielectric materials may be used alone or in combination. The first dielectric substrate 1 and the second dielectric substrate 2 may contain the same dielectric material as each other, or may contain different dielectric materials from each other.
[0016] Next, a first conductive layer 3 is formed on one side of the first dielectric substrate 1 in the thickness direction. More specifically, the first conductive layer 3 is formed on one side of the first dielectric substrate 1 in the thickness direction by a film formation method using a conductive material. The conductive material is arbitrarily and appropriately selected according to the function of the first conductive layer 3. Examples of conductive materials include metals and transparent electrode materials. Specific examples of metals include chromium (Cr), nickel (Ni), copper (Cu), gold (Au), silver (Ag), palladium (Pd), and titanium (Ti). Specific examples of transparent electrode materials include zinc oxide, indium oxide, and tin oxide. Among the conductive materials, metals are preferred, and gold (Au) and copper (Cu) are more preferred. The conductive materials can be used alone or in combination. Examples of film formation methods include plating, sputtering, vapor deposition, printing, and CVD (chemical vapor deposition), with sputtering being preferred.
[0017] In one embodiment, the first conductor layer 3 is in direct contact with the first dielectric substrate 1. The first conductor layer 3 may have a single-layer structure, or it may have a laminated structure in which two or more layers are stacked to improve adhesion or prevent oxidation. In the illustrated example, the first conductor layer 3 has a single-layer structure. The first conductor layer 3 has any appropriate configuration depending on the application of the laminated substrate 100. The first conductor layer 3 may be partially formed on one side in the thickness direction of the first dielectric substrate 1, or it may be formed on the entire surface of one side in the thickness direction of the first dielectric substrate 1. The thickness of the first conductor layer 3 is, for example, 1 μm or more, preferably 4 μm or more. On the other hand, the thickness of the first conductor layer 3 is, for example, 20 μm or less, preferably 10 μm or less.
[0018] B-2. Bonding Process Next, in the bonding process, the first dielectric substrate 1 and the second dielectric substrate 2 are bonded via the first conductive layer 3. In one embodiment, the first dielectric substrate 1, on which the first conductive layer 3 is provided, and the second dielectric substrate 2 are directly bonded. In this specification, "direct bonding" means that two layers or substrates are bonded without the interposition of an organic material (typically an organic adhesive). The form of direct bonding can be appropriately set according to the configuration of the layers or substrates to be bonded to each other. Furthermore, the interface of direct bonding is typically amorphous. In other words, an amorphous layer is formed at the interface of direct bonding. Therefore, the thermal resistance of the bonding interface can be dramatically reduced compared to resin bonding. With such a configuration, when an external device is connected to the laminated substrate 100, even if heat generated from the external device is transferred to the first dielectric substrate 1 and / or the second dielectric substrate 2, such heat can be smoothly dissipated from the first dielectric substrate 1 and / or the second dielectric substrate 2 to the package. As a result, the laminated substrate 100 can be efficiently heated, and the degradation of the characteristics of external devices can be suppressed.
[0019] Examples of direct bonding methods include surface activation by a carbonation beam, surface activation by radicals, surface activation by an ion beam, atomic diffusion, plasma bonding, hydrophilic bonding, and anodic bonding, with surface activation by a carbonation beam being preferred. In the surface activation by a carbonation beam, for example, in a high vacuum chamber (e.g., 1 × 10⁻⁶ -6At approximately Pa, a neutralization beam is irradiated onto each bonding surface of the components (layers or substrates) to be bonded. More specifically, the neutralization beam is irradiated onto the surface of the first conductive layer 3 opposite to the first dielectric substrate 1 and one side in the thickness direction of the second dielectric substrate 2. The neutralization beam is sometimes referred to as a fast atomic beam (FAB). In one embodiment, when performing surface activation with a neutralization beam, an inert gas is introduced into a chamber, and a high voltage is applied from a DC power supply to electrodes placed in the chamber. With this method, electrons move due to the electric field generated between the electrode (positive electrode) and the chamber (negative electrode), and a beam of atoms and ions from the inert gas is generated. Of the beam that reaches the grid, the ion beam is neutralized at the grid, so a beam of neutral atoms is emitted from the fast atomic beam source. The atomic species constituting the beam are preferably inert gas elements (e.g., argon (Ar), nitrogen (N)). The voltage during activation by beam irradiation is, for example, 0.5 kV to 2.0 kV, and the current is, for example, 50 mA to 200 mA. This activates the materials present on each junction surface, more specifically on the beam irradiation surface (the conductive material in the first conductive layer 3 and the dielectric material in the second dielectric substrate 2). Next, the activated junction surfaces are brought into contact with each other in a vacuum atmosphere at room temperature (25°C). The load during this joining is, for example, 100 N to 20000 N.
[0020] As shown in Figure 2, the first conductor layer 3 and the second dielectric substrate 2 are joined together to prepare a laminate 99 having the configuration of first dielectric substrate 1 / first conductor layer 3 / second dielectric substrate 2. In this specification, the laminate 99 refers to the laminate substrate before voids are formed, and is distinguished from the laminate substrate 100 in which voids are formed. In the illustrated example of the laminate 99, an amorphous layer 32 is formed between the first conductor layer 3 and the second dielectric substrate 2. The amorphous layer 32 contains a conductor material derived from the first conductor layer 3 and / or a dielectric material derived from the second dielectric substrate 2. The amorphous layer 32 formed in the surface activation method using the carbonation beam described above typically contains a conductor material derived from the first conductor layer 3 and a dielectric material derived from the second dielectric substrate 2.
[0021] In the bonding process, in addition to the first conductor layer 3, the first dielectric substrate 1 and the second dielectric substrate 2 may be directly bonded via a bonding layer (not shown). In this case, first, a bonding layer is formed on at least one of the surfaces of the first conductor layer 3 opposite to the first dielectric substrate 1, and one of the surfaces in the thickness direction of the second dielectric substrate 2, by a film deposition method using an inorganic material. As the inorganic material, for example, silicon dioxide (SiO₂) 2 Examples include amorphous silicon and tantalum oxide. The bonding layer is planarized by polishing (e.g., CMP polishing) as needed. Thereafter, the first dielectric substrate 1 and the second dielectric substrate 2 are directly bonded via the first conductor layer 3 and the bonding layer by the direct bonding method described above (preferably a surface activation method using a carbonation beam). This prepares a laminate 99 having the configuration of first dielectric substrate 1 / first conductor layer 3 / bonding layer (not shown) / second dielectric substrate 2. In this case, the amorphous layer 32 contains at least an inorganic material derived from the bonding layer. The thickness of the bonding layer is, for example, 0.001 μm to 10 μm, preferably 0.01 μm to 3 μm.
[0022] These laminates 99 are heat-treated as needed. This can improve the bonding strength between the first dielectric substrate 1 and the second dielectric substrate 2. The heating temperature is, for example, 60°C to 200°C, preferably 80°C to 150°C. The heating time is, for example, 10 minutes to 20 hours, preferably 1 hour to 10 hours.
[0023] B-3. Thinning Process Next, in the thinning process, the first dielectric substrate 1 and / or the second dielectric substrate 2 are thinned in the laminate 99. In the thinning process, only the first dielectric substrate 1 may be thinned, only the second dielectric substrate 2 may be thinned, or both the first dielectric substrate 1 and the second dielectric substrate 2 may be thinned. Hereinafter, the thinned dielectric substrate (first dielectric substrate 1 and / or second dielectric substrate 2) may be referred to as a functional layer, and the dielectric substrate that was not thinned may be referred to as a support substrate. Examples of methods for thinning the dielectric substrate include grinding, chemical mechanical polishing (CMP), etching, ion implantation, ultrasonic peeling, and laser peeling.
[0024] In one embodiment, the first dielectric substrate 1 is thinned to form a functional layer 1a, and the second dielectric substrate 2 is not thinned but functions as a support substrate 2a. The support substrate 2a supports the functional layer 1a via the first conductor layer 3. According to such a method, it is possible to sufficiently reduce the thickness of the functional layer 1a while suppressing damage to the functional layer 1a. Hereinafter, the dielectric material constituting the functional layer may be referred to as a first dielectric material, and the dielectric material constituting the support substrate may be referred to as a second dielectric material to distinguish them from each other in some cases.
[0025] The functional layer (the functional layer 1a in the illustrated example) contains a first dielectric material. The relative permittivity ε of the first dielectric material at 300 GHz is, for example, 12.0 or less, preferably 10.0 or less, and more preferably 5.0 or less. On the other hand, the lower limit of the relative permittivity ε of the first dielectric material at 300 GHz is typically 3.5. The dielectric loss tangent (dielectric loss) tanδ of the first dielectric material is preferably as small as possible. The dielectric loss tangent (dielectric loss) tanδ of the first dielectric material at 300 GHz is, for example, 0.0030 or less, preferably 0.0020 or less, and more preferably 0.0015 or less. When the relative permittivity ε and the dielectric loss tangent (dielectric loss) tanδ of the first dielectric material are within such ranges, the dielectric loss in the laminated substrate 100 can be reduced. Therefore, when the laminated substrate 100 is applied to a waveguide element, the propagation loss in the waveguide element can be reduced. The relative permittivity ε and the dielectric loss tangent (dielectric loss) tanδ are measured by, for example, terahertz time-domain spectroscopy. In addition, in this specification, when there is no reference to the measurement frequency regarding the relative permittivity and the dielectric loss tangent, it means the relative permittivity and the dielectric loss tangent at 300 GHz.
[0026] Examples of the first dielectric material include single-crystal quartz (relative permittivity 4.5, dielectric loss tangent 0.0013), amorphous quartz (quartz glass, relative permittivity 3.8, dielectric loss tangent 0.0010), spinel (relative permittivity 8.3, dielectric loss tangent 0.0020), aluminum nitride (relative permittivity 8.5, dielectric loss tangent 0.0015), sapphire (relative permittivity 9.4, dielectric loss tangent 0.0030), silicon carbide (relative permittivity 9.8, dielectric loss tangent 0.0022), magnesium oxide (relative permittivity 10.0, dielectric loss tangent 0.0012), and silicon (relative permittivity 11.7, dielectric loss tangent 0.0016). Among these inorganic materials, amorphous quartz (quartz glass) is preferred. In the illustrated example, the functional layer 1a (first dielectric substrate 1) contains amorphous quartz (quartz glass). When the functional layer contains amorphous quartz (quartz glass), the propagation loss in a waveguide device to which the laminated substrate 100 is applied can be stably reduced. Furthermore, since the dielectric constant is higher than that of a resin-based substrate, the substrate size can be reduced, and since the dielectric constant is relatively low among inorganic materials, it is advantageous for achieving low delay.
[0027] The thermal expansion coefficient (linear expansion coefficient) of the functional layer is, for example, 10×10 -6 / K or less, preferably 8×10 -6 / K or less. When the thermal expansion coefficient falls within such a range, thermal deformation (typically, warpage) of the laminated substrate 100 can be stably suppressed. The thermal expansion coefficient is measured, for example, in conformity with JIS standard R1618.
[0028] In one embodiment, the thickness of the functional layer satisfies the following formula (1). In the illustrated example, the thickness of the thinned functional layer 1a of the first dielectric substrate 1 satisfies the following formula (1). (In the formula, t represents the thickness of the functional layer. λ represents the wavelength of the electromagnetic wave incident on the functional layer. ε represents the relative permittivity of the first dielectric material at 300 GHz. a represents a value of 3 or greater.) If the thickness of the functional layer satisfies formula (1), the induction of slab modes and / or the occurrence of substrate resonance can be suppressed even when high-frequency electromagnetic waves are incident on the functional layer. Furthermore, since the first conductor layer is located between the functional layer and the support substrate, even if the thickness of the functional layer satisfies formula (1), leakage of electromagnetic waves incident on the functional layer to the support substrate can be suppressed.
[0029] In the above formula (1), a preferably represents a value of 6 or more. With this configuration, even when high-frequency electromagnetic waves are incident on the functional layer, the loss of electromagnetic waves in the functional layer can be stably reduced.
[0030] The thickness of the functional layer is, for example, 1 μm or more, preferably 2 μm or more, more preferably 10 μm or more, and even more preferably 20 μm or more. On the other hand, the thickness of the functional layer is, for example, 1700 μm or less, preferably 500 μm or less, more preferably 200 μm or less, and even more preferably 100 μm or less. A laminated substrate 100 having a functional layer having such thicknesses can realize a waveguide element with low propagation loss over a wide frequency range (i.e., broadband).
[0031] The support substrate (support substrate 2a in the illustrated example) contains a second dielectric material. The relative permittivity ε of the second dielectric material at 300 GHz is, for example, 2.0 to 20, preferably 3.0 to 15. The dielectric loss tangent (dielectric loss) tanδ of the second dielectric material at 300 GHz is, for example, 0.1 or less, preferably 0.01 or less. Examples of the second dielectric material include indium phosphide (InP), silicon (Si), glass, and SiAlON (Si 3 N 4 - Al 2 O 3 ), mullite (3Al 2 O 3 ・2SiO 2 , 2Al 2 O 3 3SiO 2), aluminum nitride (AlN), magnesium oxide (MgO), aluminum oxide (Al 2 O 3 ), spinel (MgAl 2 O 4 ), sapphire, quartz, crystal, gallium nitride (GaN), silicon carbide (SiC), silicon nitride (Si 3 N 4 ), gallium oxide (Ga 2 O 3 Examples include diamond. Among these second dielectric materials, silicon (Si) is preferred. In the illustrated example, the support substrate 2a (second dielectric substrate 2) contains silicon. When the support substrate contains silicon, the second vacancies can be formed with high precision in the second vacancy formation step.
[0032] The linear expansion coefficient of the second dielectric material is preferably as close as possible to that of the first dielectric material. The linear expansion coefficient of the second dielectric material is, for example, in the range of 50% to 150% of that of the first dielectric material. With such a configuration, thermal deformation (typically warping) of the composite substrate can be suppressed.
[0033] The thermal conductivity of the support substrate is, for example, 150 W / Km or more. In one embodiment, the thickness of the support substrate is greater than the thickness of the functional layer. The thickness of the support substrate is, for example, 1.1 to 30 times, preferably 1.5 to 10 times, the thickness of the functional layer. The thickness of the support substrate is, for example, 50 μm or more, preferably 100 μm or more, and more preferably 150 μm or more. On the other hand, the thickness of the support substrate is, for example, 3000 μm or less, preferably 2000 μm or less, and more preferably 300 μm or less. Having such a thickness for the support substrate can improve the mechanical strength of the laminated substrate 100, and when the laminated substrate 100 is applied to a waveguide element, propagation loss can be stably reduced.
[0034] B-4. First void formation step Next, as shown in Figure 3, in the first void formation step, a first void 10 is formed in the laminate 99. More specifically, the first void 10 is formed on the first dielectric substrate 1 from the side opposite to the second dielectric substrate 2 toward the second dielectric substrate 2. In the illustrated example, the first void 10 is formed on the functional layer 1a from the side opposite to the support substrate 2a toward the support substrate 2a.
[0035] Examples of methods for forming the first void 10 include sandblasting, laser processing, wet etching, and dry etching. The methods for forming the first void 10 can be used individually or in combination. In one embodiment, the first void 10 is formed in the laminate 99 by sandblasting or laser processing. This allows for the precise formation of the first void 10. Furthermore, by selecting sandblasting or laser processing as the method for forming the first void 10, it is possible to reduce the number of steps and improve the freedom of material selection without being hindered by materials present at the interface between dielectric substrates, as is the case with etching. In particular, sandblasting allows for the smooth and precise formation of the first void 10, and enables stable adjustment of the surface roughness of the inner wall of the first void 10 to a range described later.
[0036] In sandblasting, a suitable material is typically projected onto a first dielectric substrate 1. Examples of materials projected onto the first dielectric substrate in sandblasting (hereinafter sometimes referred to as "projection material") include glass, silicon, zircon, alumina, and silicon carbide. The projection material has a particle shape. The average primary particle diameter of the projection material is, for example, 2 μm to 100 μm, preferably 3 μm to 50 μm, and more preferably 4 μm to 30 μm. By using such a projection material, the processing rate, micro-processing, and surface roughness can be appropriately adjusted.
[0037] In laser processing, a suitable laser beam is typically irradiated onto the first dielectric substrate 1. The laser beam is typically pulsed. The pulse duration is, for example, 290 fs (femtoseconds) to 100 ps (picoseconds), preferably 700 fs to 50 ps. The wavelength of the laser beam is, for example, 343 nm (nanometers) to 515 nm, and also, for example, 900 nm to 1200 nm. Using such a laser beam suppresses modification of the substrate material due to thermal effects during laser irradiation, as well as unwanted deposits such as dross (molten material) and burrs, and allows for the processing of a wide range of materials at once with high pulse energy.
[0038] The first void 10 extends from the surface of the first dielectric substrate 1 opposite to the second dielectric substrate 2 to any suitable position. Hereinafter, the surface of the first dielectric substrate 1 opposite to the second dielectric substrate 2 may be referred to as the upper surface 11 of the first dielectric substrate 1. In the first void formation step, the deepest part of the first void 10 may be located inside the first dielectric substrate 1, inside the first conductive layer 3, between the first dielectric substrate 1 and the first conductive layer 3, between the first conductive layer 3 and the second dielectric substrate 2, or inside the second dielectric substrate 2.
[0039] In one embodiment, the deepest part of the first void 10 is located inside the second dielectric substrate 2. In the illustrated example, the deepest part of the first void 10 is located inside the support substrate 2a. In other words, the first void 10 penetrates the first dielectric substrate 1 (functional layer 1a) and the first conductor layer 3 to reach the interior of the second dielectric substrate 2 (support substrate 2a). With this configuration, in the second void formation process, it is easy to form the communication portion between the first void 10 and the second void 20 inside the second dielectric substrate 2. This makes it possible to smoothly manufacture a laminated substrate 100 that can suppress bonding delamination.
[0040] The dimensions (depth) of the first void 10 in the thickness direction of the first dielectric substrate 1 are, for example, 0.8 times or more, preferably 2 times or more, the thickness of the first dielectric substrate 1. On the other hand, the depth of the first void 10 is, for example, 10 times or less, preferably 6 times or less, and more preferably 3 times or less, the thickness of the first dielectric substrate 1.
[0041] The first void 10 has any suitable shape when viewed from the upper surface 11 side of the first dielectric substrate 1. Examples of the shape of the first void 10 when viewed from the upper surface 11 side include a circular shape, an elliptical shape, a polygonal shape such as a quadrilateral, and a circular shape is preferred. When the first void 10 has a circular shape, the inner diameter of the first void 10 on the upper surface 11 of the first dielectric substrate 1 is, for example, 20 μm to 200 μm, and preferably 30 μm to 100 μm.
[0042] In one embodiment, the first void 10 has a tapered shape, becoming smaller in diameter as it moves away from the upper surface 11 of the first dielectric substrate 1. With this configuration, a via conductor layer 6 can be easily formed on the inner surface of the first void 10, and the strength of the laminated substrate 100 can be improved. The taper angle of the first void 10 is, for example, 70° to 90°, and preferably 75° to 85°.
[0043] The surface roughness (more specifically, the arithmetic mean height Sa) of the inner wall of the first void 10 is, for example, 0.01 μm to 20 μm, preferably 0.05 μm to 10 μm, and more preferably 0.1 μm to 5 μm. When the surface roughness of the inner wall of the first void 10 is within this range, the adhesion of the via conductor layer 6 to the inner wall of the first void 10 can be improved. The arithmetic mean height Sa is measured, for example, in accordance with the international standard ISO 25178.
[0044] In one embodiment, multiple such first voids 10 are formed at intervals from one another. In the illustrated example, multiple first voids 10 are arranged at intervals from one another in a plane direction perpendicular to the thickness direction of the first dielectric substrate 1 (see Figure 6). The pitch of the multiple first voids 10 (the distance between the centers of adjacent first voids 10) is, for example, 40 μm or more, preferably 60 μm or more. On the other hand, the pitch of the multiple first voids 10 is, for example, 600 μm or less, preferably 400 μm or less, and more preferably 200 μm or less.
[0045] B-5. Second void formation step Next, as shown in Figure 4, a second void 20 is formed in the laminate 99 in the second void formation step. More specifically, a second void 20 is formed on the side of the second dielectric substrate 2 opposite to the first dielectric substrate 1, and is connected to the first void 10. In the illustrated example, the second void 20 is formed on the side of the support substrate 2a opposite to the functional layer 1a, toward the first void 10. Examples of methods for forming the second void 20 include etching, laser processing, and sandblasting. The methods for forming the second void 20 can be used individually or in combination. In one embodiment, the second void 20 is formed by etching. This allows for the accurate formation of the second void 20. Examples of etching methods include dry etching and wet etching, preferably dry etching, and more preferably deep etching by the BOSCH method. Dry etching allows for the smooth formation of the second void 20. In particular, when the second dielectric substrate 2 contains silicon, by employing the BOSCH method, which allows the taper angle to be controlled to almost vertical, a through-hole 40 can be realized by adjusting the depth (processing time) of the second void 20, even if the taper angle and depth of the first void 10 are different. This improves the design and / or manufacturing process flexibility of the laminated substrate 100. Furthermore, since the processing accuracy of the second void 20 can be improved, the pitch of multiple second voids 20 can be reduced when forming multiple second voids 20, and as a result, the laminated substrate 100 can be miniaturized.
[0046] The second void 20 extends from the surface of the second dielectric substrate 2 opposite to the first dielectric substrate 1 to any suitable position and communicates with the first void 10. Hereinafter, the surface of the second dielectric substrate 2 opposite to the first dielectric substrate 1 may be referred to as the bottom surface 21 of the second dielectric substrate 2. The deepest part of the first void 10 (the end opposite to the top surface 11) and the deepest part of the second void 20 (the end opposite to the bottom surface 21) are in communication. The communication portion between the first void 10 and the second void 20 may be located inside the first dielectric substrate 1, inside the first conductive layer 3, between the first dielectric substrate 1 and the first conductive layer 3, between the first conductive layer 3 and the second dielectric substrate 2, or inside the second dielectric substrate 2.
[0047] In the illustrated example, the first void 10 and the second void 20 are in communication within the second dielectric substrate 2. With this configuration, delamination of the bond in the laminated substrate 100 can be suppressed compared to the case where the communication portion between the first void 10 and the second void 20 is located between the first dielectric substrate 1 or the second dielectric substrate 2 and the first conductor layer 3.
[0048] The dimensions (depth) of the second void 20 in the thickness direction of the first dielectric substrate 1 are, for example, 0.3 to 1.2 times the thickness of the second dielectric substrate 2, and preferably 0.5 to 1.0 times.
[0049] The second void 20 has any suitable shape when viewed from the lower surface 21 of the second dielectric substrate 2. Examples of the shape of the second void 20 when viewed from the lower surface 21 include a circular shape, an elliptical shape, a polygonal shape such as a quadrilateral, and a circular shape is preferred. When the second void 20 has a circular shape, the inner diameter of the second void 20 on the lower surface 21 of the second dielectric substrate 2 is, for example, 40 μm to 200 μm, preferably 60 μm to 120 μm. The inner diameter of the second void 20 on the lower surface 21 of the second dielectric substrate 2 is, for example, 2.0 times or less the depth of the second void 20, preferably 1.0 times or less, and more preferably 0.5 times or less. On the other hand, the inner diameter of the second void 20 on the lower surface 21 of the second dielectric substrate 2 is, for example, 0.2 times or more the depth of the second void 20, and also, for example, 0.5 times or more. The inner diameter of the second void 20 on the lower surface 21 of the second dielectric substrate 2 is, for example, 0.8 times or more, preferably 1.2 times or more, the inner diameter of the first void 10 on the upper surface 11 of the first dielectric substrate 1. On the other hand, the inner diameter of the second void 20 on the lower surface 21 of the second dielectric substrate 2 is, for example, 4.0 times or less, preferably 2.0 times or less, the inner diameter of the first void 10 on the upper surface 11 of the first dielectric substrate 1. When the inner diameter of the second void 20 on the lower surface 21 of the second dielectric substrate 2 is within this range, multiple connected first and second voids can be arranged periodically at narrow intervals, thereby achieving miniaturization of elements through circuit integration, suppression of electrical signal leakage due to gaps between adjacent voids, and improved heat dissipation.
[0050] In one embodiment, the second void 20 has a tapered shape, becoming smaller in diameter as it moves away from the lower surface 21 of the second dielectric substrate 2. With this configuration, a via conductor layer 6 can be easily formed on the inner surface of the second void 20, and the strength of the laminated substrate 100 can be improved. The taper angle of the second void 20 is typically smaller than the taper angle of the first void 10. The taper angle of the second void 20 is, for example, 80° to 90°, preferably 82° to 87°. The inner diameter of the deepest part of the second void 20 (the end opposite to the lower surface 21) is, for example, 0.9 times or less, preferably 0.7 times or less, the inner diameter of the second void 20 on the lower surface 21 of the second dielectric substrate 2. On the other hand, the inner diameter of the deepest part of the second void 20 is, for example, 0.2 times or more, preferably 0.4 times or more, the inner diameter of the second void 20 on the lower surface 21 of the second dielectric substrate 2. If the inner diameter of the deepest part of the second cavity 20 is within this range, the design freedom of the laminated substrate 100 having the through-hole 40 can be improved.
[0051] The surface roughness (more specifically, the arithmetic mean height Sa) of the inner wall of the second void 20 is, for example, 0.0001 μm to 10 μm, preferably 0.0005 μm to 0.1 μm, and more preferably 0.001 μm to 0.05 μm. When the surface roughness of the inner wall of the second void 20 is within this range, the adhesion of the via conductor layer to the inner wall can be improved, and conductor loss of high-frequency signals due to surface roughness can be suppressed.
[0052] In one embodiment, a step 30 is formed in the communication portion between the first cavity 10 and the second cavity 20. The center of the deepest part of the first cavity 10 (the end opposite the top surface 11) and the center of the deepest part of the second cavity 20 (the end opposite the bottom surface 21) may substantially coincide or may be offset from each other. The distance between the center of the deepest part of the first cavity 10 and the center of the deepest part of the second cavity 20 is, for example, 0 μm to 30 μm. In the illustrated example, the center of the deepest part of the first cavity 10 (the end opposite the top surface 11) and the center of the deepest part of the second cavity 20 (the end opposite the bottom surface 21) substantially coincide, and the inner diameter of the deepest part of the first cavity 10 (the end opposite the top surface 11) and the inner diameter of the deepest part of the second cavity 20 (the end opposite the bottom surface 21) are different from each other. When the center of the deepest part of the first void 10 and the center of the deepest part of the second void 20 substantially coincide, the distance between their centers is, for example, less than 0.5 μm.
[0053] In the illustrated example, the inner diameter of the deepest part of the first void 10 is smaller than the inner diameter of the deepest part of the second void 20. The inner diameter of the deepest part of the first void 10 is, for example, 0.9 times or less, preferably 0.8 times or less, the inner diameter of the first void 10 on the upper surface 11 of the first dielectric substrate 1. On the other hand, the inner diameter of the deepest part of the first void 10 is, for example, 0.4 times or more, preferably 0.5 times or more, the inner diameter of the deepest part of the first void 10 on the upper surface 11 of the first dielectric substrate 1. The inner diameter of the deepest part of the first void 10 is, for example, 0.9 times or less, preferably 0.7 times or less, the inner diameter of the deepest part of the second void 20. On the other hand, the inner diameter of the deepest part of the first void 10 is, for example, 0.2 times or more, preferably 0.4 times or more, the inner diameter of the deepest part of the second void 20. The inner diameter of the deepest part of the first void 10 is, for example, 20 μm to 70 μm, preferably 30 μm to 50 μm. Having the inner diameter of the deepest part of the first void 10 within this range can further improve the design freedom of the laminated substrate 100 having the through-hole 40.
[0054] Typically, the same number of such second voids 20 are formed as the number of first voids 10. Therefore, if multiple first voids 10 are formed in the laminate 99 during the first void formation step, multiple second voids 20 will be formed during the second void formation step. The range of the pitch of the multiple second voids 20 (the distance between the centers of adjacent second voids 20) is, for example, the same as the range of the pitch of the multiple first voids 10 described above.
[0055] This allows for the manufacture of a laminated substrate 100 having a through-hole 40 formed by the communication between the first void 10 and the second void 20. More specifically, the laminated substrate 100 comprises the first dielectric substrate 1 described above, the second dielectric substrate 2 described above, the first conductive layer 3 described above, and the through-hole 40 described above.
[0056] B-6. Second Film Formation Process As shown in Figure 5, in one embodiment, the second film formation process is performed after the second void formation process. In the illustrated second film formation process, the second conductor layer 4, the third conductor layer 5, and the via conductor layer 6 are formed together. More specifically, a conductor thin film is formed on the upper surface 11 of the first dielectric substrate 1, the lower surface 21 of the second dielectric substrate 2, and the inner surface of the through-hole 40 by a film formation method using a conductor material. Examples of conductor materials used in the second film formation process include the same conductor material as used in the first film formation process. Preferably, copper (Cu) is used as the conductor material used in the second film formation process. Examples of film formation methods for the second film formation process include the same film formation method as used in the first film formation process, preferably sputtering. Next, a resist is applied to any appropriate position on the conductor thin film, and the resist is patterned by photolithography so as to expose the portion to be removed from the conductor thin film and mask the other portion. Subsequently, the conductive thin film exposed from the resist is removed, for example, by wet etching (more specifically, with ferric chloride solution). As a result, a second conductive layer 4 is formed on the upper surface 11 of the first dielectric substrate 1, a third conductive layer 5 is formed on the lower surface 21 of the second dielectric substrate 2, and a via conductive layer 6 is formed on the inner surface of the through-hole 40.
[0057] In one embodiment, the second conductor layer 4 is in direct contact with the upper surface 11 of the first dielectric substrate 1. The second conductor layer 4 may have a single-layer structure or a laminated structure in which two or more layers are stacked. The thickness range of the second conductor layer 4 is, for example, the same as the thickness range of the first conductor layer 3.
[0058] The second conductor layer 4 has any suitable configuration depending on the application of the laminated substrate 100. Examples of the second conductor layer 4 include a coplanar electrode, a microstrip electrode, and a differential line. As shown in Figure 6, in one embodiment, the second conductor layer 4 includes a coplanar electrode 4a. In the illustrated example, the coplanar electrode 4a comprises a signal electrode 41, a first ground electrode 42, and a second ground electrode 43. With such a configuration, electromagnetic waves can be coupled with the electric field generated between the signal electrode 41 and the ground electrodes 42 and 43 and propagated through the first dielectric substrate 1 (functional layer 1a) (see Figure 5). When the second conductor layer 4 includes a coplanar electrode 4a, the first conductor layer 3 typically functions as a ground electrode.
[0059] The signal electrode 41 has a linear shape extending in a direction perpendicular to the thickness direction of the first dielectric substrate 1. In the illustrated example, the signal electrode 41 extends over the entire laminated substrate 100, but the lengthwise dimension of the signal electrode 41 can be arbitrarily and appropriately adjusted. In addition, multiple signal electrodes 41 may be arranged in parallel on the laminated substrate 100. The width of the signal electrode 41 (dimension perpendicular to the lengthwise direction) is, for example, 2 μm to 200 μm, preferably 20 μm to 150 μm. The first ground electrode 42 is positioned in a direction intersecting (preferably perpendicular to) the lengthwise direction of the signal electrode 41, so as to form a predetermined gap between it and the signal electrode 41. The second ground electrode 43 is positioned on the opposite side of the signal electrode 41 from the first ground electrode 42 in a direction intersecting (preferably perpendicular to) the lengthwise direction of the signal electrode 41, so as to form a predetermined gap between it and the signal electrode 41. The gap extends in the lengthwise direction of the signal electrode 41. The width of the above-mentioned void (gap) is, for example, 2 μm to 100 μm, and preferably 5 μm to 80 μm.
[0060] As shown in Figure 5, in one embodiment, the third conductor layer 5 is in direct contact with the lower surface 21 of the second dielectric substrate 2. The third conductor layer 5 may have a single-layer structure or a laminated structure in which two or more layers are stacked. The thickness range of the third conductor layer 5 is, for example, the same as the thickness range of the first conductor layer 3. The third conductor layer 5 has any suitable configuration depending on the application of the laminated substrate 100. The third conductor layer 5 may be partially formed on the lower surface 21 of the second dielectric substrate 2 or may be formed on the entire lower surface 21 of the second dielectric substrate 2.
[0061] In one embodiment, the via conductor layer 6 is in direct contact with the inner surface of the through-hole 40. The via conductor layer 6 may be partially formed on the inner surface of the through-hole 40, or it may be formed over the entire inner surface of the through-hole 40. In the illustrated example, the via conductor layer 6 is formed over the entire inner surface of the through-hole 40, including the step 30. The via conductor layer 6 electrically connects the second conductor layer 4 and the third conductor layer 5. In the illustrated example, the via conductor layer 6 electrically connects the first ground electrode 42 or the second ground electrode 43 to the third conductor layer 5. The via conductor layer 6 may be in contact with the first conductor layer 3. In this way, the via conductor layer 6 electrically connects the first conductor layer 3 to the second conductor layer 4 and the third conductor layer 5, respectively. More specifically, the via conductor layer 6 electrically connects the first conductor layer 3 to the first ground electrode 42 or the second ground electrode 43, and electrically connects the first conductor layer 3 to the third conductor layer 5. The thickness range of the via conductor layer 6 is, for example, the same as the thickness range of the first conductor layer 3.
[0062] Furthermore, the internal space of the through-hole 40 may be filled with the conductive material described above, if necessary. Filling the internal space of the through-hole 40 with conductive material can improve the strength of the laminated substrate 100.
[0063] As described above, a laminated substrate 100 further comprising a second conductor layer 4, a third conductor layer 5, and a via conductor layer 6 is manufactured. In other words, the laminated substrate 100 in the illustrated example comprises the first dielectric substrate 1 described above, the second dielectric substrate 2 described above, the first conductor layer 3 described above, the through-hole 40 described above, the second conductor layer 4 described above, the third conductor layer 5 described above, and the via conductor layer 6 described above.
[0064] C. Laminated Substrate Such a laminated substrate 100 can be applied to various industrial products. Examples of applications for the laminated substrate 100 include waveguides, interposers, and miniature antennas. In one embodiment, the laminated substrate 100 is applied to a waveguide capable of guiding electromagnetic waves. In this case, the laminated substrate 100 preferably comprises a second conductor layer 4 including coplanar electrodes and / or microstrip electrodes. The frequency of the electromagnetic waves guided by the waveguide is, for example, 30 GHz or more and 20 THz or less. In other words, the waveguide is capable of guiding electromagnetic waves from millimeter waves to terahertz waves. Millimeter waves are typically electromagnetic waves with frequencies of about 30 GHz to 300 GHz; terahertz waves are typically electromagnetic waves with frequencies of about 300 GHz to 20 THz. In particular, the waveguide element to which the laminated substrate 100 is applied can guide electromagnetic waves with frequencies of 30 GHz or more and 2 THz or less (especially electromagnetic waves with frequencies of 30 GHz or more and 1 THz or less) with excellent propagation loss.
[0065] D. Modified Example In the laminated substrate 100 shown in Figure 5, the communication portion between the first void 10 and the second void 20 is located inside the second dielectric substrate 2. The arrangement of the communication portion between the first void 10 and the second void 20 is not particularly limited, as described above. As shown in Figure 7, the communication portion between the first void 10 and the second void 20 may be located inside the first dielectric substrate 1. As shown in Figure 8, the communication portion between the first void 10 and the second void 20 may be located at the interface between the first conductor layer 3 and the second dielectric substrate 2.
[0066] In the laminated substrate 100 shown in Figure 5, the second void 20 has a tapered shape, becoming smaller in diameter as it moves away from the lower surface 21 of the second dielectric substrate 2. The shape of the second void 20 is not limited to this. As shown in Figure 9, the inner surface of the second void 20 may extend substantially parallel to the thickness direction of the second dielectric substrate 2. In this case, when the thickness direction of the second dielectric substrate 2 is 90°, the inner surface of the second void 20 extends, for example, in the 85° to 90° direction. With such a configuration, high integration of through-holes 40 can be achieved. As shown in Figure 10, the second void 20 may have a tapered shape, becoming larger in diameter as it moves away from the lower surface 21 of the second dielectric substrate 2. With such a configuration, the via conductor layer 6 can be formed with fewer defects.
[0067] In the laminated substrate 100 shown in Figure 5, the inner diameter of the deepest part of the first void 10 is smaller than the inner diameter of the deepest part of the second void 20. The relationship between the inner diameters of the deepest parts of the first void 10 and the second void 20 is not limited to this. As shown in Figure 11, the inner diameter of the deepest part of the first void 10 may be larger than the inner diameter of the deepest part of the second void 20. As shown in Figure 12, the inner diameter of the deepest part of the first void 10 and the inner diameter of the deepest part of the second void 20 may be substantially the same. In this case, no step 30 is formed in the communication portion between the first void 10 and the second void 20.
[0068] In the laminated substrate 100 shown in Figure 5, the center of the deepest part of the first void 10 and the center of the deepest part of the second void 20 substantially coincide. However, the configuration of the communication portion between the first void 10 and the second void 20 is not limited to this. As shown in Figure 13, the centers of the deepest part of the first void 10 and the centers of the deepest part of the second void 20 may be offset from each other. In this case, the distance between the centers of the deepest part of the first void 10 and the centers of the deepest part of the second void 20 is, for example, 0.5 μm to 30 μm.
[0069] The laminated substrate according to the embodiment of the present invention can be used in a wide range of fields such as waveguides, next-generation high-speed communications, sensors, laser processing, and solar power generation, and can be particularly suitable for use as a waveguide for millimeter-wave to terahertz waves.
[0070] 1. First dielectric substrate 2. Second dielectric substrate 3. First conductor layer 4. Second conductor layer 5. Third conductor layer 6. Via conductor layer 10. First void 20. Second void 40. Through-hole 100. Laminated substrate
Claims
1. A method for manufacturing a laminated substrate, comprising: a first film formation step of forming a first conductive layer on one surface in the thickness direction of a first dielectric substrate; a bonding step of joining a second dielectric substrate to the first dielectric substrate via the first conductive layer; a thinning step of thinning at least one of the first dielectric substrate and the second dielectric substrate; a first vacancy formation step of forming a first vacancy that is recessed toward the second dielectric substrate from the side of the first dielectric substrate in the first dielectric substrate; and a second vacancy formation step of forming a second vacancy that is connected to the first vacancy from the side of the second dielectric substrate in the second dielectric substrate.
2. The method for manufacturing a laminated substrate according to claim 1, wherein the first void penetrates the first dielectric substrate and the first conductor layer and reaches the interior of the second dielectric substrate.
3. The method for manufacturing a laminated substrate according to claim 1, wherein in the thinning step, the first dielectric substrate is thinned to form a functional layer, and the second dielectric substrate functions as a support substrate that supports the functional layer via the first conductive layer.
4. The method for manufacturing a laminated substrate according to claim 3, wherein in the first void formation step, the first void is formed by sandblasting or laser processing, and in the second void formation step, the second void is formed by etching.
5. The method for manufacturing a laminated substrate according to claim 4, wherein the first dielectric substrate contains quartz glass and the second dielectric substrate contains silicon.
6. A method for manufacturing a laminated substrate according to any one of claims 1 to 5, further comprising a second film formation step of forming a second conductive layer on the surface of the first dielectric substrate opposite to the first conductive layer after the second void formation step.
7. The method for manufacturing a laminated substrate according to claim 6, wherein in the second film formation step, a third conductive layer is formed on the surface of the second dielectric substrate opposite to the first dielectric substrate.
8. The method for manufacturing a laminated substrate according to claim 7, wherein in the second film formation step, via conductor layers are formed on the inner surfaces of the first void and the second void, respectively, to electrically connect the second conductor layer and the third conductor layer.